BAG AND FOIL HOSE FOR MAKING SUCH A BAG
Patent Information
- Application Number
- DE502019012170
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-12-03
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2039-12-03
AI Technical Summary
Existing bags with tear strips for bulk material handling are unclean to open, as operators come into contact with contents, and the perforation process is prone to errors due to the lack of a secure and controlled opening mechanism.
A bag design featuring a longitudinal seam where the upper and lower weakening lines begin, with a flag at the tear strip's start that extends beyond the seam, allowing for easy gripping and opening without touching the contents, and a varnish applied in a grid pattern to weaken the seam's adhesion, enabling secure tearing along the weakening lines.
The design allows for a clean and controlled opening of the bag, preventing contact with the contents and ensuring accurate tearing, while the varnish and flag facilitate easy handling and pouring of bulk materials.
Description
[0001] The invention relates to a bag with a filling space for bulk material, which is defined by a lower base, a circumferential wall, and an upper filling space closure facing away from the lower base. The bag has a tear strip for releasing an opening area of the bag, which is defined by an upper weakening line and a lower weakening line. Both weakening lines run parallel to the upper filling space closure, and the upper weakening line is positioned between the upper filling space closure and the lower weakening line.
[0002] Such a sack is known, for example, from EP 0 620 157 B1. With the help of the tear strip, the entire area of the sack above the strip is separated from the lower part of the sack containing the contents. The weakening lines and also a front line that runs perpendicular to the two weakening lines and where the tear strip begins are each perforated. To open the tear strip, the front line perforation is pressed in with a finger of the person opening the sack. The tear strip is then grasped in this area from the inside and outside of the sack material with the thumb and index finger and is further torn open along the weakening lines. However, handling of the opening is sloppy because the operator comes into contact with the contents of the sack when tearing it open and, moreover, the perforation along the front line is not always pressed correctly.
[0003] Further bags are known from DE 38 36 227 A1, FR 2 951 439 A1, EP 0 779 222 A1, DE 20 2016 102623 U1, EP 2 059 456 A1, WO 91 / 06488 A1, WO 2016 / 100852 A1 and WO 00 / 43272 A1.
[0004] The invention is based on the object of providing a bag of the type mentioned above with improved opening options.
[0005] The invention is achieved by a sack according to claim 1, in which the sack has a longitudinal seam running transversely to the upper filling space closure, wherein the upper and lower weakening lines begin in the region of the longitudinal seam and the longitudinal seam is weaker in the region between the two weakening lines than above the upper weakening line and below the lower weakening line. The tear strip therefore adheres less strongly to the sack material located below the tear strip in the region of the longitudinal seam and can be easily fixed between the thumb and index finger of an operator, first removed from the sack material located below the tear strip in the region of the longitudinal seam and then torn open along the weakening lines. The operator's fingers do not touch the contents of the sack.
[0006] Advantageously, the bag has an interfering substance in the area of the longitudinal seam between the two weakening lines that impedes the welding process. This is particularly preferably formed by a lacquer that is applied in the area of the longitudinal seam between the weakening lines in the manner of a grid, either on the side of the tear strip facing the filling chamber or on the side of the bag material facing away from the filling chamber below the tear strip. The lacquer is preferably selected such that the adhesion of an additional melt to form the longitudinal seam is significantly weaker on the lacquer than on the remaining bag material in the area of the longitudinal seam.
[0007] In a particularly preferred embodiment of the invention, a flag is arranged at the beginning of the tear strip between the two weakening lines, which flag extends beyond the longitudinal seam in the opposite direction to the tearing direction and does not adhere to the material of the sack wall. With the help of the flag, an operator can particularly easily grip the beginning of the tear strip and open the tear strip in the tearing direction along the weakening lines. If the sack is formed from a film web that is folded over to form a film tube, with the two sides of the film web being placed on top of each other and connected with the longitudinal seam, the flag is particularly preferably formed by pulling the upper film slightly beyond the longitudinal seam in the circumferential direction over the lower film web. This creates a film strip along the longitudinal seam that is not connected to the film underneath.The two lines of weakness then also extend beyond the longitudinal seam to the lateral end of the upper film of the bag. However, the lines of weakness do not extend to the lower film in the area of the longitudinal seam. For the purposes of this invention, the positioning of the beginning of the lines of weakness in the area of the longitudinal seam is to be understood as meaning that the lines of weakness either begin where the longitudinal seam runs or, if the aforementioned flag is formed, extend slightly beyond the longitudinal seam in the opposite direction to the tear-open direction.
[0008] In a preferred embodiment of the invention, the bag material in the region of the ends of the weakening lines and the material and width of the tear strip are designed such that the resistance to tearing of the tear strip beyond the ends of the weakening lines is greater than the resistance to tearing of the tear strip from the bag. As a result, when the opening field is opened along the weakening lines, the bag can only be opened up to the end of the weakening lines and not beyond, since if the tear strip is pulled further, the bag does not open any further, but the tear strip tears off. The ends of the weakening lines are understood to be the side of the weakening lines towards which the tear strip is opened, releasing the opening field, when it is torn along the weakening lines.
[0009] In a particularly preferred embodiment of the invention, the bag consists of a film which can be constructed in one or more layers.
[0010] According to the invention, the sack is a side-gusseted sack with a front side and a back side, which are connected to one another via a first side wall and a second side wall, wherein the side walls are each formed by side gussets. The weakening lines extend transversely over at least 80% of the width of the front side or the width of the back side of the sack, in particular over the entire width of the front side or over the entire width of the back side. The area of the side gussets, however, remains free of the weakening lines. Due to this design, the desired V-shaped chute below the opening field is formed particularly advantageously in a side-gusseted sack due to the positioning of the lower weakening line.
[0011] Both emptying the bulk material contained in the bag and dosing it are difficult with the bag disclosed in EP 0 620 157 B1, since the person emptying the bag has to grasp the hand of their first arm below the bottom of the bag and place the upper part of the remaining bag over the forearm of the second arm and then tilt the bag using the hand of the first arm. To facilitate emptying, in a particularly preferred embodiment of the invention the upper filling chamber closure has a fingertip contact area on its inner side facing the filling chamber. The fingertip contact area is formed by a material fold between a first leg and a second leg of the bag, with the first leg extending from the upper weakening line to the material fold and the second leg adjoining it, starting from the material fold.The material fold can be formed either in a single-piece film by a fold or the introduction of a seam, or by two films being joined together with a sealed seam. The first leg and the second leg of the sack are each formed by the sack material surrounding the filling space. The sack is dimensioned and the tear strip positioned in such a way that, with the opening panel of a sack filled with product open, the two legs enclose an angle of no more than 135° when the sack is carried by reaching into the opening panel. The sack is carried, for example, by the hand of an operator, i.e. an operator reaches into the opening panel with one hand and the first leg rests on the operator's hand, while the sack hangs down from the hand.The dimensions of the bag are thus selected such that an angle of no more than 135° is formed in the aforementioned state of the bag. It has been shown that this design allows the bag to be carried safely by reaching into the open opening.
[0012] According to the invention, the distance between the upper weakening line and the material edge is 30 to 65 mm, particularly preferably 45 to 55 mm, and the distance between the lower weakening line and the upper weakening line is 15 to 25 mm. The peripheral wall of the bag has a front and a back, with both weakening lines being centered either on the front or on the back of the bag and extending over 15 to 35% of the bag circumference.
[0013] The bag is opened along the lines of weakness, with the position of the lines of weakness determining the position of the opening panel within the bag. When opened, the opening panel is shaped like a rectangle with a height corresponding to the distance between the lines of weakness and a length corresponding to the length of the two lines of weakness. The opening panel is centered either on the front or back of the bag and extends over 15 to 35% of the bag's circumference.
[0014] It has been found that when the opening panel is positioned in this way, using the aforementioned positioning of the two weakening lines, the bag material between the upper material fold and the upper weakening line, and thus the upper edge of the opening panel, together with the material of the upper material fold, can be used for the hand of the other arm of the person emptying the bag. The resulting handle is voluminous and at the same time strong enough to allow the bag to be emptied easily. If the upper weakening line, and thus the upper edge of the opening panel, is moved further towards the bottom of the bag, the fingers of the person being operated no longer additionally grip the upper material fold, which significantly reduces the handle's stability and the person emptying the bag loses control over the bag.However, if the opening area is moved further toward the upper material edge by shortening the distance between the upper weakening line and the material edge beyond the inventive limit, the handle becomes very narrow and uncomfortable. Especially with heavier bags, an operator would have to support the weight primarily with their fingertips rather than with their entire hand.
[0015] By centering the opening panel on the front or back of the bag, the weight of the bag can be more easily balanced during emptying. The 15 to 25 mm spacing of the two weakening lines and the resulting height of the opening panel, combined with the extension of the weakening lines and thus also of the opening panel over 15 to 35% of the bag's circumference, create a V-shaped chute along the lower edge of the opening panel. This chute results from the lower weakening line, allowing for precise dosing and pouring direction.
[0016] A person emptying the sack grasps the sack with the hand of the first arm below the bottom of the sack. With the hand of the second arm, the person reaches into the opening and grasps the sack material between the upper edge of the opening and the material edge, as well as the material edge itself, in a stable grip. As soon as the person holds the sack at an angle by lifting the bottom or lowering the opening, the lower edge of the opening forms a V-shaped, outward-facing chute, through which the bulk material can be dispensed very easily and precisely.
[0017] In a particularly preferred embodiment of the invention, the upper, former filling chamber closure is formed by a transverse seam, whereby the transverse seam also forms the material fold inside the bag. This embodiment is particularly present when the bag is a side-gusseted bag.
[0018] In an alternative design, the upper filling chamber closure is formed by an upper base, and the material fold is formed by the transition from the surrounding wall of the bag to the upper base. The material fold can either be a fold incorporated into a film or the bag material is additionally sealed in this area. This design is particularly common when the bag is a valve bag.
[0019] The invention is further achieved by a film tube according to claim 8 for producing sacks of the aforementioned type. The film tube has a plurality of tear strips arranged parallel to one another at equal intervals, each for releasing a respective opening field. The tear strips are each delimited by an upper weakening line and a lower weakening line. The film tube is formed from a film web that is folded over to form a tube, wherein the film tube has a longitudinal seam running longitudinally to the film tube, which connects the two superimposed lateral ends of the film web to one another, thereby forming the film tube. The wall of the aforementioned sacks is of course also designed circumferentially accordingly.By means of this design of the film tube, a bag according to the invention of the aforementioned type can be produced from the film tube, with the advantages mentioned in connection with the bags according to the invention.
[0020] In a particularly preferred embodiment of the invention, at the beginning of each tear strip of the film tube, between the two weakening lines associated with this tear strip, a flag is arranged. This flag extends beyond the longitudinal seam, counter to the tear direction, and does not adhere to the material of the film tube wall. The resulting bags according to the invention, made from the film tube according to the invention, thus exhibit the advantages described with the aforementioned flags in connection with the bags when opening the opening field.
[0021] According to the invention, the film tube has a plurality of material folding areas arranged at constant intervals transversely to the longitudinal extent of the film tube for introducing a material fold, each of which is assigned to a tear strip. The distance between the upper weakening line in each case and the assigned material folding area is 30 to 65 mm, in particular 45 to 55 mm, and the distance between the lower weakening line in each case and the upper weakening line of each tear strip is 15 to 25 mm. The weakening lines are arranged centrally on the film tube in its flat state and extend over 15 to 35% of the film tube circumference. Due to this design of the film tube, a sack of the aforementioned type can be produced from the film tube with the advantages already listed for this sack above.
[0022] In a preferred embodiment of the film tube according to the invention, the films of the film tube in the region of the ends of the weakening lines, and the material and width of the tear strip, are designed such that the resistance to tearing of the tear strip beyond the ends of the weakening lines is greater than the resistance to tearing of the tear strip from the film tube. Here, too, a sack of the aforementioned type can be produced with a film tube according to the invention designed in this way, with the advantages mentioned for this sack.
[0023] Further details and advantageous embodiments of the invention are explained below with reference to a schematically illustrated bag and a schematically illustrated section of a film tube according to the invention; they show: Fig. 1a bag according to the invention with a closed opening field, Fig. 2a bag according to the invention correspondingFig. 1 with tear strip torn along the weakening lines, Fig. 3 the article from Fig. 2 in pouring position, showing the handle and the V-shaped chute and Fig. 4 a section of a flattened film tube.
[0024] In the following, elements of the invention that have the same function will be provided with a common reference number where appropriate. In particular, elements of the bag according to the invention that are also found in the film tube according to the invention will be provided with a common reference number. The features of the invention explained below with reference to the exemplary embodiments can also be the subject of the invention individually or in combinations other than those shown in the exemplary embodiment.
[0025] Fig. 1 bis 3 show a sack 2 according to the invention with a filling space for bulk material, which is delimited by a lower base 4, a circumferential wall 6 and an upper filling space closure 8 facing away from the lower base 4. The sack 2 has a tear strip 10 for releasing an opening field 12 of the sack 2, which is delimited by an upper weakening line 14 and a lower weakening line 16. Both weakening lines 14, 16 run parallel to the upper filling space closure 8 and the upper weakening line 14 is positioned between the upper filling space closure 8 and the lower weakening line 16. The sack 2 has a longitudinal seam 18 running transversely to the upper filling space closure 8. The upper and lower weakening lines 14, 16 each begin in the area of the longitudinal seam 18. The longitudinal seam 18 is weaker in the area between the two weakening lines 14, 16 than above the upper weakening line 14 and below the lower weakening line 16.
[0026] At the beginning 20 of the tear strip 10 between the two weakening lines 14, 16, a flag 22 is arranged which extends beyond the longitudinal seam 18 in the opposite direction to the tearing direction, the tearing direction being indicated by the arrow 24 in the exemplary embodiment, and does not adhere to the material 26 of the wall 6 of the bag 2 in this area.
[0027] The bag material in the region of the ends 28 of the weakening lines 14, 16 and the material and the width of the tear strip 10 are designed such that the resistance to tearing of the tear strip 10 beyond the ends 28 of the weakening lines 14, 16 is greater than the resistance to tearing of the tear strip 10 from the bag 2.
[0028] In the illustrated embodiment, the bag 2 is a gusseted bag with a front side 30 and a rear side opposite the front side, which is not visible in the exemplary embodiment. The front side 30 and the rear side are connected to one another via a first side wall 32 and a second side wall, the position of which is indicated by arrow 34. The side walls 32, 34 are each formed by side gussets 36, and the weakening lines 14, 16 extend transversely across at least 80% of the width a of the front side 30. The area of the side gussets 36 is free of the weakening lines 14, 16.
[0029] The upper filling chamber closure 8 has a fingertip support area 38 on its inner side facing the filling chamber, which is formed by a material bevel 40 between a first leg 42 and a second leg, which is not visible in the figures but whose position is indicated by the arrow 44, of the bag 2. The first leg 42 extends from the upper weakening line 16 to the material bevel 40 and the second leg 44 adjoins it, starting from the material bevel 40. The two legs 42, 44 enclose an angle of no more than 135° when the opening field 12 of the bag 2 filled with filling material is open when the bag 2 is carried by engaging in the opening field 12. This holding position is approximately in Fig. 3 shown, where in Fig. 3 the bag 2 is additionally held by a second hand below the bag 2.
[0030] The distance b between the upper weakening line 14 and the material bevel 40 is 30 to 65 mm and particularly preferably 45 to 55 mm. The distance c between the lower weakening line 16 and the upper weakening line 14 is 15 to 25 mm. The peripheral wall 6 of the bag also has a front side 30 and a rear side (not visible in the exemplary embodiment), with both weakening lines 14, 16 being centered on the front side of the bag 2 and extending over 15 to 35% of the bag circumference.
[0031] In the exemplary embodiment, the upper filling chamber closure 8 is formed by a transverse seam 46 and the transverse seam 46 also forms the material fold 40 in the interior of the bag 2.
[0032] Fig. 4 shows a section of a film tube 48 according to the invention for producing the aforementioned bags 2 according to the invention. The film tube 48 has a plurality of tear-open strips 10 arranged parallel to one another at equal intervals, each of which releases an opening field 12, each of which is delimited by an upper weakening line 14 and a lower weakening line 16. The film tube 48 also has a longitudinal seam 18 running longitudinally to the film tube 48. The upper and lower weakening lines 14, 16 each begin in the region of the longitudinal seam 18, and the longitudinal seam 18 is weaker in the region between the upper and lower weakening lines 14, 16 assigned to a tear-open strip 10 than above the upper weakening line 14 and below the lower weakening line 16.
[0033] In the film tube 48 according to the invention, a flag 22 is arranged at the beginning 20 of each tear strip 10 between the two weakening lines 14, 16 assigned to this tear strip 10, which flag extends beyond the longitudinal seam 18 counter to the tear direction 24 and does not adhere to the material 26 of the wall 6 of the sack 2. The film tube 48 also has a plurality of material folding areas 52 arranged at constant intervals transversely to the longitudinal extent, represented by the arrow 50 of the film tube 48, for each introducing a material fold 40. The distance b of the upper weakening line 14 of the assigned tear strip 10 to the material folding area 52 is 30 to 65 mm and in particular 45 to 55 mm. The distance c between the lower weakening line 16 and the upper weakening line 14 of each tear strip is 15 to 25 mm. The weakening lines 14, 16 are shown on the film tube 48 in its flattened state, Fig. 4 , arranged centrally and extend over 15 to 35% of the film tube circumference.
[0034] The film of the film tube 48 in the region of the ends 28 of the weakening lines 14, 16 and the film and the width of the tear strip 10 are designed such that the resistance to tearing of the tear strip 10 beyond the ends 28 of the weakening lines 14, 16 is greater than the resistance to tearing of the tear strip 10 from the film tube 48. Reference numbers
[0035] 2Bag 4Lower base 6Wall 8Upper filling space closure 10Tear strip 12Opening field 14Upper weakening line 16Lower weakening line 18Longitudinal seam 20Start of tear strip 22Flag 24Tear direction 26Wall material 28End of weakening lines 30Front 32First side wall 34Second side wall 36Side gussets aWidth of front 38Fingertips on layer area 40Material fold 42First leg 44Second leg bDistance upper weakening line - material fold cDistance upper weakening line - lower weakening line 46Cross seam 48Film tube 50Longitudinal extension 52Material fold area
Claims
1. Bag (2) with a filling space for bulk material which is delimited by a lower base (4), a circumferential wall (6) and an upper filling space termination (8) facing away from the lower base (4), and with at least one tear-off strip (10) to release an opening field (12) of the bag (2) which is delimited by an upper tear line (14) and a lower tear line (16), wherein both tear lines (14, 16) run parallel to the upper filling space termination (8) and the upper tear line (14) is positioned between the upper filling space termination (8) and the lower tear line (16), wherein the bag (2) has a longitudinal seam (18) which opens transversely to the upper filling space termination (8), the upper and the lower tear line (14, 16) begin in the region of the longitudinal seam (18) and the longitudinal seam (18) is formed to be weaker in the region between the two tear lines (14, 16) than above the upper tear line (14) and below the lower tear line (16), wherein the bag (2) is a side gusset bag with a front side (30) and a rear side which are connected to one another via a first side wall (32) and a second side wall (34), wherein the side walls (32, 34) are formed in each case by side gussets (36), and the tear lines (14, 16) extend transversely over at least 80% of the width (a) of the front side (30) or the width of the rear side, in particular over the entire width (a) of the front side (30) or the entire width of the rear side, the region of the side gussets (36) is, however, free of the tear lines (14, 16), and wherein the upper filling space termination (8) has a fingertip bearing region (38) on its inside facing the filling space, which is formed by a material fold (40) between a first limb (42) and a second limb (44) of the bag (2), wherein the first limb (42) extends from the upper tear line (14) up to the material fold (40) and the second limb (44) adjoins this starting from the material fold (40), characterized in that the two limbs (42, 44) enclose, in the state with an opened opening field (12) of a bag (2) filled with filling material when carrying the bag (2) by engagement into the opening field (12), an angle of no more than 135 degrees, and that the distance (b) from the upper tear line (14) to the material fold (40) is 30 to 65 mm, the distance (c) from the lower tear line (16) to the upper tear line (14) is 15 to 25 mm and the circumferential wall (6) of the bag (2) has a front side (30) and a rear side, wherein both tear lines (14, 16) are arranged centred either on the front side (30) or on the rear side of the bag (2) and extend over 15 to 35% of the circumference of the bag.
2. Bag (2) according to Claim 1, characterized in that the bag (2) has a disruptive substance which hinders a welding process in the region of the longitudinal seam (18) between the two tear lines (14, 16).
3. Bag (2) according to any one of the preceding claims, characterized by a flag (22) which is arranged at the start of the tear-off strip (10) between the two tear lines (14, 16), goes beyond the longitudinal seam (18) counter to the tear-off direction (24) and does not adhere to the material of the wall (6) of the bag (2).
4. Bag (2) according to any one of the preceding claims, characterized in that the bag material in the region of the ends (28) of the tear lines (14, 16) and the material and the width of the tear-off strip (10) are formed in such a manner that the resistance to a tearing off of the tear-off strip (10) beyond the ends (28) of the tear lines (14, 16) is greater than the resistance to a tearing off of the tear-off strip (10) from the bag (2) .
5. Bag (2) according to any one of the preceding claims, characterized in that the bag (2) is composed of a film.
6. Bag (2) according to any one of the preceding claims, characterized in that the upper filling space termination (8) is formed by a transverse seam (46) and the transverse seam (46) also forms the material fold (40) inside the bag (2).
7. Bag (2) according to any one of the preceding claims, characterized in that the upper filling space termination (8) is formed by an upper base and the material fold (40) forms the transition of the circumferential wall (6) to the upper base.
8. Film tube (48) for producing bags (2) according to any one of the preceding claims, with a plurality of tear-off strips (10) arranged at constant distances parallel to one another for the release of in each case one opening field (12) which are delimited in each case by an upper tear line (14) and a lower tear line (16), wherein both tear lines (14, 16) run parallel to one another, with a longitudinal seam (18) running longitudinally with respect to the film tube (48), wherein the upper and the lower tear lines (14, 16) begin in each case in the region of the longitudinal seam (18) and the longitudinal seam (18) is formed to be weaker respectively in the region between the upper and lower tear line (14, 16) assigned to a tear-off strip (10) than above the upper tear line (14) and below the lower tear line (16) and with a plurality of material fold regions (52) arranged at constant distances in each case transversely to the longitudinal extent (50) of the film tube (48) for incorporation in each case of a material fold (40) which is assigned in each case to a tear-off strip (10), wherein the distance (b) between the upper tear line (14) of the assigned tear-off strip (10) and the material fold region (52) is 30 to 65 mm, the distance (c) between the lower tear line (16) and the upper tear line (14) of each tear-off strip (10) is 15 to 25 mm and the tear lines (14, 16) on the film tube (14), in its laid-flat state, are arranged in a centred manner and extend over 15 to 35% of the circumference of the film tube.
9. Film tube (48) according to Claim 8, characterized in that the film tube (48) has a disruptive connection which hinders a welding process in the region of the longitudinal seam (18) in each case between the upper and lower tear line (14, 16) assigned to a tear-off strip (10) .
10. Film tube (48) according to any one of preceding Claims 8 or 9, characterized by a flag (22) which is arranged at the start of each tear-off strip (10) between the two tear lines (14, 16) assigned to this tear-off strip (10), goes beyond the longitudinal seam (18) counter to the tear-off direction (24) and does not adhere to the material of the wall (6) of the film tube (48) .
11. Film tube (48) according to any one of Claims 8 to 10, characterized in that the film of the film tube (48) in the region of the ends (28) of the tear lines (14, 16) and the film and the width of the tear-off strip (10) are formed in such a manner that the resistance to a tearing off of the tear-off strip (10) beyond the ends (28) of the tear lines (14, 16) is greater than the resistance to a tearing off of the tear-off strip (10) from the film tube (28).
