PLASTIC CONTAINERS FOR LIQUIDS AND METHOD FOR MANUFACTURING A PLASTIC CONTAINER
Patent Information
- Application Number
- DE502020009647
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-10-31
- Filing Date
- 2020-09-25
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2040-09-25
AI Technical Summary
Existing plastic containers with multi-layer walls, particularly those with inner layers of polyethylene and outer layers of recycled materials, face challenges in forming compatible welded connections due to material incompatibility between the container nozzle and the connecting piece, often requiring removal of layers to achieve a weld, which affects the quality of the connection.
The design features a container socket with a conical cross-section where the welding contact surface is formed by an inner layer segment, allowing only the inner layer to participate in the welding process, preventing incompatible material contact and ensuring a high-quality welded connection through a two-stage expansion process during blow molding that maintains sufficient material thickness for the inner layer.
This approach enables the formation of a reliable and high-quality welded connection between the container nozzle and the connecting piece, ensuring compatibility and maintaining the structural integrity of the container while avoiding material incompatibility issues, thus enhancing the container's functionality and durability.
Description
[0001] The present invention relates to a plastic container for liquids, in particular a container for transport and storage containers for liquids, having an outer shell made of a latticework or sheet metal material and a pallet-like base frame, wherein the plastic container is formed as a blow-molded body by blow molding from a tubular preform in a blow mold and has, in a fitting connection area of a container wall, a container nozzle provided with a container opening for connecting a container fitting, which is connected to a connection flange of the container fitting via a welded connection, wherein the container wall has an inner layer formed from a first plastic material and an outer layer formed from a second plastic material.
[0002] EP 1 630 105 A1 discloses a plastic container of the type mentioned above, which has a container fitting connected to a container nozzle via a heated element butt weld. The known plastic container is manufactured using a blow molding process. To form a container nozzle serving to connect the container fitting, a protrusion is formed on a fitting connection area of the container wall simultaneously with the production of the blow molded body. A wall area of this protrusion is removed with the aid of a cutting tool to form a container opening in order to form the container nozzle. After use of the cutting tool, the container nozzle thus has a container opening with an outer edge that forms a welding contact surface in a plane parallel to the container wall.In the subsequent mirror welding or butt welding process, a heating mirror is arranged as a heating element between the container nozzle and an oppositely arranged connecting nozzle of the container fitting in order to heat both a welding contact surface formed on the container nozzle and a welding contact surface formed on the connecting nozzle of the container fitting to welding temperature, so that after removal of the heating mirror, the welding contact surfaces are pressed against each other under pressure and can cool down in this position to form the welded joint.
[0003] The method described above for producing a welded connection between the container nozzle of the plastic container and the connecting nozzle of the container fitting is particularly also used for plastic containers whose container walls have a multi-layer structure, wherein an inner layer made of polyethylene is combined with an outer layer made of regenerated material, separated, for example, by an EVOH barrier layer. Neither the EVOH layer nor the regenerated layer, which is made of recycled material, are weldable for connection to a container fitting regularly made of polyethylene, so that in the area of the outer edge of the container nozzle, the outer layer and the EVOH layer must first be removed in order to create a welded connection between the container nozzle and the container fitting.
[0004] EP 2 387 492 B1 discloses a plastic container for a fuel, wherein the plastic container is formed as a blow-molded body by blow molding from a tubular preform in a blow mold and has, in a fitting connection region of a container wall, a container nozzle provided with a container opening for connecting a container fitting, which is connected to a connection flange of the container fitting via a welded joint, wherein the container wall has an inner layer formed from a first plastic material and an outer layer formed from a second plastic material. The container nozzle or the container fitting serves to fill the plastic container with fuel. Fuel is withdrawn or an engine is supplied with the fuel via a line on an upper side of the plastic container by means of a pump arranged in an interior of the plastic container.The pump is also connected to the tank fitting via a line.
[0005] The present invention is therefore based on the object of proposing a plastic container and a method for producing a plastic container which has a multi-layer wall structure and can be provided with a container fitting in a simple manner by means of a welded connection, wherein the container fitting is designed as a withdrawal fitting.
[0006] To achieve this object, the plastic container according to the invention has the features of claim 1.
[0007] According to the invention, the container wall has an inner layer formed from a first plastic material and an outer layer formed from a second plastic material, and the container nozzle has a longitudinal cross-section that widens towards the container opening, such that an end face of the container nozzle is at least partially formed by an inner layer segment arranged opposite the outer layer, and a welding contact surface of the container nozzle is formed by the inner layer segment, wherein the container nozzle is conical in shape, such that the welding contact surface is formed by a lateral surface of an inner cone provided with the inner layer, which is welded to an outer cone formed on the connecting nozzle of the container fitting, wherein the container fitting is designed as a withdrawal fitting.
[0008] The term "front surface" in this context is to be understood as the surface projection of the container nozzle into a front plane of the plastic container, i.e., a plane parallel to the container wall having the container nozzle, such that the inner layer segment forms a surface projection into the front surface and thus forms the welding contact surface of the container nozzle when establishing a welding contact between the connecting nozzle of the container fitting and the container nozzle. Because the relative arrangement of the outer layer to the inner layer segment is determined such that the outer layer is arranged opposite the inner layer segment, i.e., facing away from the inner layer segment, welding contact between the connecting nozzle of the container fitting and the outer layer of the container wall is prevented during welding. Rather, due to the design according to the invention, the welding contact orThe formation of a weld contact surface on the vessel nozzle is limited to the inner layer segment. This ensures that weld contact cannot occur between materials that are incompatible with a weld joint, which could adversely affect the quality of the weld.
[0009] According to the invention, the container nozzle is conical in shape such that the welding contact surface is formed by a lateral surface of an inner cone provided with the inner layer, which is welded to an outer cone formed on the connecting nozzle of the container fitting.
[0010] In the method according to the invention, during the blow molding of the plastic container having a container wall with an inner layer formed from a first plastic material and an outer layer formed from a second plastic material, the container wall expands into an expanding wall recess of the blow mold to form the protuberance, such that the protuberance formed in the container wall has a cross-section that increases towards a cover wall, and after the cover wall has been separated to form the container opening, a welding contact surface formed by an inner layer segment is formed that extends to the container opening, wherein the expansion occurs into a conically expanding wall recess, wherein the container fitting is designed as a removal fitting. The welding method carried out below can be carried out in particular as a heating element butt welding method.Other welding processes that can be used advantageously are the well-known friction welding processes, such as rotation welding and vibration welding.
[0011] Such a manufacturing method ensures that the welding contact surface formed by the inner layer segment is arranged exposed in an end face of the container nozzle and thus, when a welding contact is made between the connecting nozzle of the container fitting and the container nozzle, a surface contact is formed between the inner layer segment and the connecting nozzle of the container fitting.
[0012] According to the invention, the expansion takes place in a conically widening wall recess, so that the conically shaped welding contact surface already discussed above is achieved with the resulting advantageous effects.
[0013] If the protrusion is formed in at least two expansion steps, such that a central region of the protrusion is formed in a first expansion step, followed by the formation of a conical wall region of the protrusion concentrically arranged with respect to the central region in a second expansion step, the maximum expansion occurring during the formation of the protrusion can be reduced compared to the formation of the protrusion in only one expansion step, so that the wall thickness reduction of the container wall resulting from the expansion is correspondingly limited. This ensures, in particular, that the inner layer segment has the material thickness necessary to form a high-quality welded joint.
[0014] It is particularly advantageous if the central area of the protrusion is cylindrical, so that a uniform wall thickness distribution can be achieved in the area of the cone.
[0015] Preferably, the formation of the central region of the protrusion can take place simultaneously with the formation of the blow-molded body, so that the execution of the two-stage expansion process does not involve a significant increase in the blow-molding times for producing the blow-molded body.
[0016] A preferred embodiment of the invention is explained in more detail below with reference to the drawing.
[0017] They show: Fig. 1 a perspective view of a liquid container designed as a pallet container with an inner container designed as a plastic container; Fig. 2 an enlarged view of a fitting connection area of the plastic container in a partially sectioned side view; Fig. 3a an enlarged detailed view of a welded joint formed between a tank nozzle and a connecting nozzle of the tank fitting; Fig.3b a front view of the Fig. 3a shown container nozzle; Fig. 4a a first manufacturing step for producing the container neck using the blow molding process; Fig. 4b one in which Fig. 4a the central region of a protuberance produced on the plastic container in the first manufacturing step shown for forming the container neck; Fig. 5a a second manufacturing step for producing the container nozzle; Fig. 5b the protrusion produced on the plastic container by means of the second manufacturing step to form the container neck; Fig. 5c which in Fig. 5b shown protrusion in a sectional view; Fig. 6a bis 6c a schematic representation of the connection of the vessel fitting to the vessel nozzle using a heating element butt welding process.
[0018] Fig. 1 shows a transport and storage container which can be used as a single-use and reusable container and which has a cuboid-shaped plastic container 10 which, in the present case, has a filler neck 15 provided with a lid 14 in a container wall 13 on an upper side of the plastic container 10 and a container neck 17 in a fitting connection area 16 of the container wall 13 on a front side of the plastic container 10 for connecting a container fitting 18 which, in the present case, is designed as a withdrawal fitting.
[0019] For the purpose of forming a transport and storage container, the plastic container 10 is arranged on a pallet-like base frame 19, which has a support base 20, in the present case designed as a flat base tray, for supporting the plastic container 10.
[0020] The plastic container 10 is produced by blow molding from a tubular preform, wherein the container neck 17 is produced together with the cuboid-shaped base body of the plastic container 10 by the blow molding process.
[0021] Fig. 2 shows a welded joint 52 between the container nozzle 17 and a connecting nozzle 21 of the container fitting 18, which was carried out after the plastic container 10 has been manufactured using the blow molding process. Fig. 2 can be seen, and also in particular in the enlarged representation in Fig. 3 As shown, the container wall 13 of the plastic container 10 has a multi-layer wall structure, wherein in the present case an inner layer 22, which consists of HDPE, is separated from an outer layer 24 by a barrier layer 23, which in the present case is formed of EVOH. Since increased demands are placed on the material quality of the inner layer 22 due to the direct contact with the liquid contained in the plastic container 10, particularly in the case of food contact, the inner layer is regularly made of a homogeneous material of defined composition, such as HDPE. In contrast, the material used for the outer layer 24 is regularly recycled, so-called regenerated material, which is produced by shredding and grinding the plastic material of used plastic containers.In addition, the plastic container 10, which in the present case is designed as an explosion-proof container, has an Ex layer 25 formed from an electrically conductive material as its outer surface.
[0022] The term "outer layer" refers here to a layer that, in contrast to the inner layer, is arranged towards the outside of the plastic container. The outer layer does not necessarily have to form the outermost layer of the plastic container, but can be provided with another layer arranged towards the outside of the plastic container, such as the explosion-proof layer mentioned above as an example, or another functional layer or a decorative layer. Preferably, the inner layer consists of a material used for the first time, and the outer layer consists of a material formed from regrind. The regrind can originate from production waste generated during the manufacture of blow-molded articles or from recycled plastic containers.
[0023] Deviating from the exemplary embodiment explained, the inner layer and the outer layer can also be arranged directly on top of one another. In the case of an intermediate functional layer, such as the barrier layer mentioned above as an example, adhesion promoters can also be provided between the functional layer and the adjacent layers.
[0024] As in the Fig. 6a bis 6c As shown, the execution of a function in the Fig. 2 and 3The heating element butt weld joint 52 shown between the container nozzle 17 and the connecting nozzle 21 of the container fitting 18 is formed in such a way that the welding contact surfaces 26, 27 on the container nozzle 17 and the connecting nozzle 21, which are to be welded together, are heated by means of a welding mirror 28 arranged between the oppositely arranged welding contact surfaces 26, 27 until a doughy consistency is reached. For this purpose, the welding contact surfaces 26, 27 are moved against heating surfaces 29, 30 of the welding mirror 28 and heated by heat conduction, as shown in Fig. 6b After reaching the required welding temperature in the welding contact surfaces 26, 27 or a corresponding melting of the container nozzle 17 and the connecting nozzle 21 in the area of the welding contact surfaces 26, 27, the welding mirror 28 is removed from its Fig. 6b shown intermediate position and the welding contact surfaces 26, 27 are, as shown in Fig. 6c shown, move against each other under pressure so that the weld joint 52 can form during subsequent cooling.
[0025] Since the production of a welded joint requires appropriate material compatibility in the area of the welding contact surfaces 26, 27, it is not possible to weld a container fitting 18 made of a PE material to a barrier layer 23 made of an EVOH material or to a non-material-compatible, electrically conductive Ex layer 25 of the container wall 13.
[0026] To ensure that the Fig. 6a bis 6c The welded connection, shown as an example as a heating element butt weld, can be made between the container wall 13, which in addition to the inner layer 22 also has the barrier layer 23, the outer layer 24 and the Ex layer 25, and the connecting piece 21, has, as shown in particular in the Fig. 2 und 3a is shown, the container neck 17 has a longitudinal cross-section widening towards a container opening 31 formed on the container neck 17, as in Fig. 3a shown so that a Fig. 3b shown end face 32 of the container nozzle 17, i.e. the one shown in Fig. 3b shown end view X of the container neck 17 projected into the drawing plane, has an inner layer segment 33 which, during the production of the butt weld connection 52 for forming the welding contact surface 26, is exposed for direct contact with the Fig. 3a shown welding contact surface 27 of the connecting piece 21. With such an arrangement of the inner layer segment 33 forming the contact surface 26 of the container piece 17, neither the barrier layer 23 nor the explosion-proof layer 25 can impair the production of the welded connection 52.
[0027] In the Fig. 2 and 3 In the embodiment shown, the container nozzle 17 is conical in shape, such that the welding contact surface 26 of the container nozzle 17 is formed by a lateral surface 34 of an inner cone 35 formed by the container nozzle 17, which is welded to an outer cone 36 formed on the connecting nozzle 21 of the container fitting 18.
[0028] With reference to the Fig. 4a bis 5c The following explains the manufacture of the container neck 17 formed on the container wall 13 by blow molding, wherein the formation of the container neck 17 is based on a protuberance 37 initially formed in the container wall 13. As a comparison of the Fig. 4a und 5a shows, the protrusion 37 is produced in two expansion steps, whereby, as Fig. 4a shows, a molding tool 40 is used which is arranged in a mold wall 38 of a blow mold at a wall recess 39 and which in the present case has a cylindrical inner slide 41 and an outer slide 42 arranged coaxially to the cylindrical inner slide 41, wherein both the inner slide 41 and the outer slide 42 with their slide bottoms 43 and 44 respectively form a mold bottom 46 of the wall recess 39 except for a radial edge region 45.
[0029] As the Fig. 4a und 5a show, the wall recess 39 is designed such that it widens in the direction of the mold base 46 into the mold wall 38 and thus forms an annular undercut 47 in the mold wall 38, such that the wall recess 39 is conical in shape overall.
[0030] How Fig. 4a shows, the inner slide 41 and the outer slide 42 assume a relative arrangement when carrying out the first expansion step, in which the inner slide 41 is located with its slide base 43 in the plane of the mold base 46 and the outer slide 42 is arranged with its slide base 44 substantially in the plane of a mold wall surface 48, such that the undercut 47 is covered by the outer slide 42 and a cylindrical mold space 49 is formed within the wall recess 39.
[0031] As can be seen from a summary of the Fig. 4a und 4b As can be seen, when the container wall 13 expands into the wall recess 39, a central region 50 of the protuberance 37 is first formed, i.e. a preform of the protuberance 37, which is then only subsequently formed in the Fig. 5a illustrated second expansion step is completed, wherein to carry out the second expansion step the outer slide 42, with its slide base 44, is moved into a flush arrangement with the slide base 43 of the inner slide, so that now both slide bases 43, 44 are arranged in the plane of the mold base 46 and a mold space 51 supplemented by the undercut 47 is formed.
[0032] In the second expansion step, the expansion of a circular wall region 53 of the valve connection region 16 of the container wall 13, which surrounds the central region 47 and which is still supported on the outer slide 42 in the first expansion step, takes place, wherein the wall region 53 has a surface area which corresponds to the sum of the surfaces of the slide base 44 of the outer slide and an inner wall surface 54 formed by a slide projection s of the outer slide 42 relative to the inner slide 41. Since this surface area is only slightly smaller than the partial surface of the wall recess 39, which is formed from the sum of the slide base 44 of the outer slide 42 and the surface of the undercut 47, the expansion leads in the Fig. 5a illustrated second expansion step essentially leads to a turning of the edge region 53 supported on the outer slide 42 into the radial edge region 45 of the mold base 46 and the adjacent undercut 47, so that the wall region 52 experiences only a limited expansion and the most expanded portion of the protuberance 37 is formed in the region of a cover wall 55 of the protuberance 37 lying against the mold base 46.
[0033] As in Fig. 5c As indicated by the dividing line, the cover wall 55 forms the part of the protuberance 37 which is removed by a separating cut to form the container opening 31 on the container nozzle 17, so that the finished container nozzle 17 does not have a reduction in wall thickness that would endanger the function of the container nozzle 17 compared to the surrounding fitting connection area 16 of the container wall 13.
Claims
1. A plastic container (10) for liquids, in particular an inner container for transport and storage containers for liquids comprising an outer jacket made of latticework or of sheet metal material and a pallet-type understructure, the plastic container (10) being realized as a blow-molded body by blow molding from a tubular preform in a blow mold and having a container socket (17) for connecting a container fitting (18) in a fitting connecting area (16) of a container wall (13), the container socket (17) being provided with a container opening (31) and being connected to a connecting flange (21) of the container fitting (18) via a welded joint (52), the container wall (13) having an inner layer (22) made of a first plastic material and an outer layer (24) made of a second plastic materi al, characterized in that the container socket (17) has a longitudinal cross section widening toward the container opening (31) in such a manner that an end face (32) of the container socket (17) is formed at least in part by an inner layer segment (33) disposed opposite the outer layer (24), and a welding contact surface (26) of the container socket (17) is formed by the inner layer segment (33) the container socket (17) being cone-shaped in such a manner that the welding contact surface (26) is formed by a wall surface (34) of an inner cone (35), the inner cone (35) being provided with the inner layer (22) and being welded to an outer cone (36) formed on a connecting piece (21) of the container fitting (18), the container fitting (18) being realized as a tap fitting.
2. A method for producing a plastic container (10) for liquids, in particular as an inner container for transport and storage containers for liquids comprising an outer jacket made of latticework or of sheet metal material and a pallet-type understructure, the plastic container (10) being realized as a blow-molded body by blow molding from a tubular preform in a blow mold and having a container socket (17) for connecting a container fitting (18), the container socket (17) being realized in a fitting connecting area (16) of a container wall (13) and being provided with a container opening (31), wherein, in order to produce the container socket (17), a bulge (37) of the container wall (13) closed by a covering wall (55) is realized in a wall recess (39) of the blow mold, then the container opening (31) is formed by cutting off the covering wall (55), and then the connection between the container socket (17) and a connecting piece (21) of the container fitting (18) is established in the form of a welded joint (52), the container wall (13) having an inner layer (22) made of a first plastic material and an outer layer (24) made of a second plastic materi al, characterized in that in order to form the bulge (37), the container wall (13) is expanded into a widening wall recess (39) of the blow mold during blow molding of the plastic container (10) in such a manner that the bulge (37) formed in the container wall (13) has a cross section increasing toward the covering wall (55) and, once the covering wall (55) has been cut off in order to form the container opening (31), a welding contact surface (26) formed by an inner layer segment (33) and extending toward the container opening (31) is formed, the expansion occurring in a conically expanded wall recess (39), the container fitting (18) being realized as a tap fitting.
3. The method according to claim 2, characterized in that the bulge (37) is formed in at least two expansion steps in such a manner that a central portion (50) of the bulge (37) is formed in a first expansion step and a conical wall portion (53) of the bulge disposed concentrically with the central portion is formed subsequently in a second expansion step.
4. The method according to claim 3, characterized in that the central portion (50) of the bulge (37) is cylindrical.
5. The method according to claim 3 or 4, characterized in that the central portion (50) of the bulge (37) and the blow-molded body are formed simultaneously.