METHOD FOR MANUFACTURING A WATCH COMPONENT FROM COMPOSITE MATERIAL

DE602022006776T2Active Publication Date: 2024-10-16DE LA MFG DHORLOGERIE AUDEMARS PIGUET & CIE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602022006776
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-04-19
Filing Date
2022-04-05
Publication Date
2024-10-16
Estimated Expiration
2042-04-05

AI Technical Summary

Technical Problem

Conventional ceramic matrix composite materials lack diversity in visual appearance and have inadequate scratch resistance and mechanical strength, while existing sintering processes like Spark Plasma Sintering (SPS) result in homogeneous ceramic parts.

Method used

A method involving the deposition of layers with randomly arranged ceramic powder and fibers in a mold, followed by FAST/SPS sintering, and subsequent machining to achieve a unique visual appearance and high mechanical resistance, using ceramic powders like Zirconia with Alumina matrix, and incorporating fibers such as carbon, basalt, or aramid for enhanced properties.

Benefits of technology

The method produces watch components with a unique and random visual appearance, high scratch resistance, and improved mechanical strength, allowing for reliable authentication through image comparison with a database.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

Technical field

[0001] The present invention relates to a method for manufacturing a watch component from a ceramic matrix composite material. The invention also relates to a method for authenticating or identifying a watch part. State of the art

[0002] Conventional composite materials, which have a polymer matrix and fibers, have good mechanical strength but low hardness and therefore average resistance to abrasion and scratch resistance. Forged composite materials, on the other hand, have an inhomogeneous and random aesthetic allowing the production of unique pieces. Forged composite materials such as carbon, aramid (kevlar ®< ) or glass fibers, sometimes combined and structured using a polymer resin, do not have very good scratch resistance and low hardness (<100HV).

[0003] Ceramics, such as zirconia or alumina, have high abrasion resistance and can be considered scratch-resistant. Ceramics are materials with a uniform and identical visual appearance from one piece to another, which has a negative impact on the diversity of the visual appearance of ceramic parts. Furthermore, ceramics have the disadvantage of being fragile due to their structure.

[0004] The use of a FAST / SPS (Spark Plasma Sintering) sintering process to increase the mechanical strength of ceramic materials is known from the state of the art.

[0005] For example, US8906498 discloses a method of manufacturing an impact-resistant material sandwich. The method includes a process of SPS (Spark Plasma Sintering) a ceramic powder to form a tile and coupling a ductile support layer to the tile. The ductile support layer may include a layer of polyethylene fibers.

[0006] Another example is disclosed in CN108299000A which describes a method for the low-temperature preparation of a SiC-type composite material. The method includes, in particular, cutting carbon fibers into a length of 1 to 3 mm and various steps to obtain a uniformly mixed powder. An SPS sintering operation of the powder, placed in a graphite matrix, is then carried out.

[0007] These processes have a negative impact on the diversity of the visual appearance of the ceramic pieces obtained, which are essentially homogeneous.

[0008] EP3795341 discloses a watch component made of a composite material composed of a polymer-based matrix and a reinforcement made of at least two different types of cut fibers, one of which is a polyazole.

[0009] EP3674816 discloses a decorative article, in particular a watch component made from a material comprising by weight: 60 to 90% of a metallic or ceramic material having a density greater than or equal to 5 g / cm3; 10 to 32% of a plastic material comprising a thermoplastic resin and a coupling agent; 0 to 8% of a reinforcement and 0 to 3% of a pigment.

[0010] An aim of the invention is to propose an alternative manufacturing method for a ceramic matrix composite material making it possible to produce watch components with a unique and random visual appearance from one piece to another.

[0011] Another aim of the invention is to propose a method for manufacturing a ceramic matrix composite material which has the advantage of being light and which has high scratch resistance as well as high mechanical strength. Brief summary of the invention

[0012] According to the invention, these aims are achieved in particular by a method for manufacturing a watch component made of ceramic matrix composite material. The manufacturing method comprises the following steps: depositing in a mold a succession of layers each comprising a ceramic powder, at least one layer of the succession of layers further comprising fibers mixed with the ceramic powder, the fibers being arranged randomly; carrying out a FAST / SPS sintering operation; demolding the sintered watch component comprising the succession of layers, and machining or finishing the sintered component to the final dimensions of the watch component in such a way that the fibers are partly visible on the surface of the watch component.

[0013] According to one embodiment, at least two layers of the succession of layers comprise fibers.

[0014] According to one embodiment, the at least two layers are separated by another layer of the succession of layers. The other layer does not comprise fibers.

[0015] According to one embodiment, the at least two layers are adjacent. The composition of one of the two adjacent layers is different from the composition of the other of the two adjacent layers.

[0016] According to one embodiment, all layers of the succession of layers comprise fibers. The composition of one of the layers is different from the composition of any of the other layers.

[0017] Sintering time is typically between 1 minute and 90 minutes.

[0018] Sintering temperatures are preferably between 800°C and 2000°C.

[0019] According to one embodiment, the ceramic powder is a composite selected from one of the following three composites: Alumina matrix zirconia (ZTA), Zirconia matrix alumina (ATZ) and Zirconia stabilized at least partially with Yttrium (Y-TZP).

[0020] The mass proportion of the fibers of said at least one layer comprising fibers is between 1.5% and 55%, preferably between 1.5% and 25%.

[0021] The fibers have a length between 2mm and 70mm, preferably between 3mm and 50mm.

[0022] According to one embodiment, the watch component is a component of a watch case, in particular a case middle, a case back, a bezel or a crown.

[0023] According to one embodiment, the watch component is a component of a watch movement, in particular a plate or a bridge.

[0024] A watch component manufactured by the method according to the invention has the advantage of being able to be identified or authenticated reliably, for example using a method comprising the following steps: capturing an image of the watch component of the timepiece having randomly distributed fibers on the surface; comparing this image to a database of images stored on a server, the database comprising a series of images of randomly distributed fibers, each image of said database being associated with another distinctive element of the timepiece, and authenticating or identifying the timepiece by matching the captured image to one of the images in the database.

[0025] The image database is created from a multitude of images captured for each watch component manufactured by the method according to the invention.

[0026] In one embodiment, the distinctive element is selected from a serial number, the production date and the caliber of the timepiece. Brief description of the figures

[0027] Examples of implementation of the invention are indicated in the description illustrated by the appended figures in which: there figure 1 is a schematic view of a section of a composite material composed of several layers of different natures according to an embodiment of the invention before the sintering operation; figure 2 is a schematic view of a section of the composite material according to the figure 1 after the sintering operation; the figure 3 is a schematic view of a section of a composite material composed of several layers of different natures according to another embodiment of the invention, and the figure 4 illustrates a schematic view of a section of a watch case, according to an embodiment of the invention, obtained by machining the composite material of the figure 2 to the final dimensions of the watch case. Example(s) of embodiment of the invention

[0028] The composite material watch component, as described later, is obtained by a manufacturing process including in particular a flash sintering operation, or “ Field Assisted Sintering Technique / Spark Plasma Sintering (FAST / SPS) » in English, which is a sintering process related to hot isostatic pressing but using the Joule effect to heat a pre-compacted powder in a mold between two graphite electrodes under an inert atmosphere or vacuum, the whole being subjected to a pressure of several megapascals under the action of a hydraulic press. A direct or alternating current of several kiloamperes, pulsed or not, is applied between the electrodes with a voltage of a few volts.

[0029] The manufacturing process of a watch component, for example a watch case 50 according to the figure 4 , in ceramic matrix composite material consists of depositing several successive layers 10, 20, 30, 40 in a mold (not shown).

[0030] In reference to the figure 1 , each of the successive layers 10, 20, 30, 40 of the composite material comprises a pre-compacted ceramic powder 12. The last layer 10 further comprises fibers 14 mixed with the ceramic powder. The fibers 14 are mixed with the ceramic powder 12 before the application of the last layer in the mold in order to obtain a last layer 10 where the fibers are arranged randomly.

[0031] The pre-compacted ceramic powder 12 of each layer forms a ceramic matrix.

[0032] The powder 12 constituting the ceramic matrix may, for example, be a composite selected from one of the following three composites: Alumina matrix zirconia (ZTA), Zirconia matrix alumina (ATZ) and Zirconia stabilized at least partially with Yttrium (Y-TZP).

[0033] According to another embodiment, the ceramic matrix 12 may comprise a mixture of the three aforementioned composites.

[0034] The fibers 14 arranged randomly in the ceramic matrix 12 of the layer 10 are, for example, fibers chosen from carbon fibers, basalt fibers, glass fibers and aramid fibers. The ceramic matrix may also incorporate a mixture of these different types of fibers. The mass proportion of the fibers in the layer 10 is generally between 1.5% and 55%, preferably between 1.5% to 25%, or even between 1.5% and 10%. Furthermore, the length of these fibers is between 2mm and 70mm, preferably between 3mm and 50mm, or even between 3mm and 6mm.

[0035] The other layers 20, 30, 40 of the composite material of the figure 1are made up of a ceramic matrix which may each include pigments 16, 17, 18 of different natures in order to give these layers different colors so that the watch component, obtained by a FAST / SPS sintering process and ground by machining in order to obtain the final dimensions of the component, has a visual appearance where the demarcation between the different layers is visible on the surface of the watch component.

[0036] The composite material according to the figure 1 then undergoes a FAST / SPS sintering operation. After the compression and sintering operation, the dimensions of the composite material are significantly reduced in one dimension as can be seen in figure 2 .

[0037] The sintering time and temperature depend on the composition of the different layers 10, 20, 30, 40, but also on the size and shape of the part to be sintered. The temperature range is between 800 and 2000°C, preferably between 900 and 1500°C while the sintering time (plateau time) is between 1 and 90 minutes, preferably between 2 and 45 minutes when each of the layers comprises a ceramic matrix.For example, for a watch case made up of a first layer of Yttrium-stabilized Zirconia with a thickness of 1 mm, green in color and comprising 5% by mass of carbon fibers, a second layer of Yttrium-stabilized Zirconia with a thickness of 2 mm and blue in color, a third layer of Yttrium-stabilized Zirconia with a thickness of 2 mm and green in color, and a fourth layer of Yttrium-stabilized Zirconia with a thickness of 1 mm, brown in color and comprising 10% by mass of carbon fibers, the sintering temperature is approximately 1050°C and the sintering time is approximately 12 minutes.

[0038] Once the FAST / SPS sintering operation is completed, the composite material is cooled and demolded. The sintered composite material is then machined to the final dimensions of the watch component in order to obtain, for example, a watch case shown in figure 4Alternatively, the part is not machined but finished, for example polished or decorated.

[0039] According to an embodiment illustrated by the figure 3 , the successive layers of the composite material 10, 20, 30, 40 with a ceramic matrix comprise a first and second layer 10, 30 each comprising fibers 14 arranged randomly. The arrangement of the fibers 14 of the first layer 10 is different from the arrangement of the fibers of the second layer 30. The first and second layers 10, 30 are separated by a third layer 20 which may comprise a certain type of pigment 16 in order to give this layer a particular visual appearance, in particular in terms of its color, which is different from the visual appearance of the first and second layers 10, 30.

[0040] According to another embodiment not illustrated, at least two adjacent layers of the succession of layers forming the composite material comprise fibers. The composition of one of the two adjacent layers is different from the composition of the other of the two layers.

[0041] According to an additional embodiment not illustrated, all of the layers of succession of layers forming the composite material comprise fibers. The composition of one of the layers is different from the composition of any of the other layers.

[0042] The watch component obtained by the FAST / SPS sintering manufacturing process according to the invention, for example the case 50 illustrated in figure 4, has the advantage of being light, having high scratch resistance as well as a unique and random visual appearance, that is to say that the visual appearance of the watch components obtained by this manufacturing process differs from one component to another.

[0043] Thanks to the unique visual appearance of the fibers, a watch component with a unique visual appearance is obtained, such as a watch case. This makes it possible to authenticate or identify a watch part comprising, for example, the watch case manufactured according to the method described above. The authentication or identification of the watch part can be carried out by comparing the visual appearance of the photographed part, or characteristics of this appearance, with reference photographs or databases of characteristics of reference parts.

[0044] For example, the method first comprises capturing an image of the watch component of the timepiece having randomly distributed fibers on the surface, for example a portion of the caseband. The captured image is then compared to a database of images stored on a server. The database comprises a series of randomly distributed fiber images created from a multitude of images captured for each watch component manufactured by the method according to the invention.

[0045] Authentication or identification of the watch piece is then carried out by matching the captured image to one of the images in the database.

Claims

1. Manufacturing process for a watch component (50) in a composite material with a ceramic matrix, comprising the following steps: - depositing in a mould a succession of layers (10, 20, 30, 40), each comprising a ceramic powder (12), at least one layer (10; 10, 30; 10, 20, 30, 40) of said succession of layers further comprising fibres (14) mixed with the ceramic powder (12), the fibres being arranged randomly; - performing a FAST / SPS sintering operation; - demoulding the sintered watch component comprising the succession of layers (10, 20, 30, 40), and - machining or finishing the sintered component to the final dimensions of the watch component (50) such as said fibres (14) are visible on the surface of the watch component (50).

2. Process according to claim 1, wherein at least two layers (10, 30) of said succession of layers (10, 20, 30, 40) comprise fibers (14).

3. Process according to the preceding claim, wherein said at least two layers (10, 30) are separated by another layer (20) of said succession of layers (10, 20, 30, 40), said another layer does not comprising fibers (14).

4. Process according to claim 2, wherein said at least two layers (10, 30) are adjacent, the composition of one of the two layers (10, 30) being different from the composition of the other of the two layers.

5. Process according to claim 1, wherein all layers of said succession of layers (10, 20, 30, 40) comprise fibres (14), the composition of one of the layers (10, 20, 30, 40) being different from the composition of any of the other layers.

6. Process according to any of claims 1 to 5, wherein the sintering time is between 1 and 90 minutes, preferably between 2 and 45 minutes.

7. Process according to any preceding claim, wherein the sintering temperatures are between 800°C and 2000°C, preferably between 900 and 1500°C.

8. Process according to any preceding claim, wherein said ceramic powder (12) is a composite selected from one of the following three composites: Zirconia with Alumina Matrix (ZTA), Alumina with Zirconia Matrix (ATZ) and Zirconia stabilized at least partially with Yttrium (Y-TZP).

9. Process according to any of claims 1 to 7, wherein said ceramic powder (12) is composed of a mixture of Zirconia with Alumina Matrix (ZTA), of Alumina with Zirconia Matrix (ATZ), and of Zirconia stabilized at least partially with Yttrium (Y-TZP).

10. Process according to any preceding claim, wherein the fibres (14) are selected from carbon fibres, basalt fibres, glass fibres and aramid fibres.

11. Process according to any preceding claim, wherein the proportion by mass of the fibres (14) in said at least one layer (10; 10, 30; 10, 20, 30, 40) comprising fibres is between 1.5% and 55%, preferably between 1.5% and 25%.

12. Process according to any preceding claim, wherein the fibres (14) have a length between 2mm and 70mm, preferably between 3mm and 50mm.

13. Process according to any preceding claim, wherein the watch component is a component of a watch case, in particular a case middle (50), a case back, a bezel or a crown.