Composite part with a thermoplastic matrix, particularly profiled, and its manufacturing process

The method of agglomerating cords with a thermoplastic sheath forms a composite part with improved mechanical properties and efficient fiber distribution, addressing the inefficiencies of existing methods by using simpler and less costly tooling.

FR3131863B1Active Publication Date: 2024-09-27CQFD COMPOSITES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022000389
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-01-18
Publication Date
2024-09-27
Estimated Expiration
2042-01-18

AI Technical Summary

Technical Problem

Existing methods for manufacturing composite parts with a thermoplastic matrix are costly, require complex and expensive tooling, and have limitations in impregnation and fiber distribution, leading to inefficiencies in production and mechanical properties.

Method used

A method involving cords with a core of reinforcing fibers coated in a first thermoplastic material, where the cords are heated and agglomerated through shaping means to form a composite part, with a second thermoplastic material sheath melting to create a matrix, allowing for simpler and less expensive tooling and improved fiber distribution.

Benefits of technology

This process enables the production of composite parts with enhanced mechanical properties and flexibility in section design, using inexpensive tooling and minimizing material loss, while maintaining high fiber density and distribution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000019_0000
    Figure 00000019_0000
  • Figure 00000019_0001
    Figure 00000019_0001
  • Figure 00000019_0002
    Figure 00000019_0002
Patent Text Reader

Abstract

According to a process for manufacturing composite parts with a thermoplastic matrix: - a plurality of cords (30) are used, each having a core (301) with reinforcing fibers embedded in a first matrix of a first thermoplastic material (3011), and furthermore a sheath (302) of a second thermoplastic material around the core (301); - in an agglomeration step, the plurality of cords (30) are heated and then agglomerated by passing them together through forming means (22) under tension to form the part (3). The heating of the plurality of cords (30) is carried out to reach a temperature higher than the melting temperature of the second thermoplastic material, such that the second thermoplastic material forms a second matrix around the cores (301) after agglomeration and hardening. Part and element thus manufactured. Figure for the abbreviation: Fig. 1
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Composite part with thermoplastic matrix, in particular profile, and its manufacturing process Technical field

[0001] The invention relates to a composite part comprising continuous fibers and a thermoplastic matrix. It also relates to its manufacturing method. Prior art

[0002] It is known to produce profiles from composite material comprising continuous fibers coated in a matrix of synthetic material. The fibers are, for example, glass fibers, carbon fibers, synthetic material or plant fibers. Such profiles are known for being light and of good strength. The use of a thermoplastic matrix makes it possible to benefit from specific physical or chemical properties of thermoplastic materials, for example to subsequently transform the profiles by softening or melting the material and giving them a new shape. It also makes it easier to recycle objects constructed with these profiles.

[0003] One of the known methods for manufacturing such profiles is pultrusion, which consists of pulling a bundle of unidirectional fibers through a die making it possible to impregnate said fibers with a polymerizable resin and to polymerize the resin in the die to form a composite profile at the outlet of said die, consisting of the reinforcing fibers and a matrix incorporating the fibers. The resins used are mainly of the thermosetting type but can also be of the thermoplastic type. The bundle of fibers is typically a grouping of strands, each strand being composed of a multitude of fibers, for example glass fibers, placed side by side without intersecting. A strand is also called a "roving" in the case of glass or designated by the English term "roving".

[0004] In a particular case, the polymerization of precursors (monomers and oligomers) to obtain thermoplastic polymers can take place in situ in the pultrusion tooling. The precursors used are then generally of low viscosity, which has the advantage of allowing the use of very high reinforcement rates while having excellent and very homogeneous impregnation of the fibers. The existing reactive systems for pultrusion are mainly based on polymerization mechanisms by ring opening of monomers / oligomers such as ε-caprolactam for polyamide 6 (PA6), lauryl-lactam for polyamide 12 (PA12), cyclic oligomers of butylene terephthalate for poly(butylene terephthalate) (PBT) or radical polymerization as for poly(methyl methacrylate) (PMMA), from methyl methacrylate.

[0005] In the remainder of the document, the mixture of precursors which will form the polymer and the matrix after the reaction will be formally called resin.

[0006] The profile comes out of a pultrusion die which integrates an impregnation zone followed by the polymerization zone which also acts as a calibration zone since it gives the desired shape to the profile, so that the profile comes out in its final shape, generally in the solid state, that is to say at a temperature below the melting point of the thermoplastic material which composes it. These tools are extremely expensive due to their dimensions. Indeed, the size of the tool is determined by the time required for polymerization and by the compromise between the length of the die and the tensile forces generated on the profile. Note that, even if the polymerization speed can be accelerated by the addition of dedicated components, it remains limited by the need to maintain a low viscosity, the time to transfer the resin mixture into the tool and to wet the fiber bundle.

[0007] Document US 5,310,600 shows a technique for manufacturing a composite based on a polyamide matrix and continuous fibers, according to which a bundle of fibers is first impregnated with reactive resin and then coated in a thermoplastic sheath. The polymerization reaction occurs in the sheath by bringing it to a temperature sufficient for the polymerization reaction. The bead thus formed is then cut into granules, with or without removal of the sheath to serve as an injection molding material. This technique has the advantage of simplifying the tooling since it is no longer necessary to calibrate the bead during the polymerization phase. The sheath serves as mechanical support and as a barrier against the risk of evaporation of the resin monomers during the polymerization phase.This approach allows for simpler tooling and increased production rates since the tool size can be increased without increasing pulling forces.

[0008] Document WO 2011 / 156693 A2 shows a method for producing profiles comprising mainly two steps. In a first step, ribbons are produced from continuous fibers which are coated with molten thermoplastic material. These ribbons are then assembled in a stack and the assembly passes through a die while the thermoplastic material is melted again. This produces a profile with a rectangular section. The technique of coating fibers with molten thermoplastic material has never been convincing, because the material remains too viscous and can only impregnate a small section of fibers and with a low fiber density. Statement of the invention

[0009] The invention aims to provide a method for manufacturing composite parts with a thermoplastic matrix offering simplicity of implementation, having good productivity and using inexpensive tooling. It also aims to provide composite profiles with a thermoplastic matrix having new properties.

[0010] With these objectives in view, the invention relates to a method for manufacturing composite parts with a thermoplastic matrix according to which: - a plurality of cords are used comprising a core with reinforcing fibers taken in a first matrix made of a first thermoplastic material; - in an agglomeration step, the plurality of cords are heated and then the cords are agglomerated by passing them together through tensile shaping means to form the part, characterized in that at least one of the cords among the plurality of cords further comprises a sheath in a second thermoplastic material around the core, the heating of the plurality of cords in the agglomeration step being done to reach a temperature higher than the melting temperature of the second thermoplastic material, such that the second thermoplastic material forms a second matrix around the cores after agglomeration and hardening.

[0011] By providing the cords with a thermoplastic sheath, material is provided which will melt and then bind the cores of the cords together, forming the second matrix. Such an assembly makes it possible to produce parts of various sections with specific, inexpensive tooling. Indeed, in the case of a profiled part, it is sufficient to produce a die which will allow the agglomeration specific to the profile and to adapt the number of cords which feed the die to produce a specific section. It has been found that such a die is short and inexpensive. It generates reasonable drawing forces, which allows the use of simple drawing means and does not generate risks of fiber breakage or jamming in the die. Other shaping means are also possible, for example with a combination of rollers or chains of looped shells.These means can perform the pulling function or be supplemented by dedicated pulling means that act on the part downstream of its shaping and hardening. In general, all the beads have a sheath, although it is possible to mix beads with sheaths and beads without sheaths, the important thing being that the quantity of material for the second matrix is ​​sufficient and distributed. The beads can have various cross-sectional shapes, whether circular, elliptical, oblong, polygonal, rectangular, hexagonal or any other shape. In the case of amorphous or semi-crystalline materials, the melting temperature is understood to be a temperature above the glass transition temperature to obtain softening. complete material. In the case of PMMA, for example, this temperature is 100 to 150K higher than the glass transition temperature.

[0012] According to one embodiment, during the agglomeration step, the plurality of cords are heated to a temperature higher than the respective melting temperatures of the first and second materials. Thus, the cross-section of the core can be shaped to adapt it to the final cross-section to be obtained in the part. It could be advantageous in certain cases to have a melting temperature of the sheath which is higher than that of the thermoplastic material of the core. This may have the advantage of solidifying more quickly after agglomeration the peripheral part of the produced part consisting essentially of the material from the sheath.

[0013] According to one embodiment, during the agglomeration step, the melting temperature of the second thermoplastic material being lower than that of the first thermoplastic material, the plurality of cords are heated to a temperature lower than the melting temperature of the first thermoplastic material. Thus, the cores of the cords remain hard and do not deform and retain their section, while the second thermoplastic material melts to form the second matrix.

[0014] According to one embodiment, the cords are produced by reactive pultrusion, the core comprising continuous fibers. The cords obtained by pultrusion are well suited for the production of elongated or continuous parts. Reactive pultrusion of thermoplastic material has the advantage of achieving excellent impregnation of the fibers by the resin before its transformation into thermoplastic material. It is thus possible to obtain cords with a high fiber density and a very good distribution of the first thermoplastic material in the fibers.

[0015] Reactive pultrusion produces the first thermoplastic material selected for example from a group comprising polyamide-6, polyamide-12, polymethyl methacrylate, polybutylene terephthalate and polyethylene terephthalate. Existing reactive systems for pultrusion are mainly based on ring-opening polymerization mechanisms of monomers / oligomers such as ε-caprolactam for polyamide 6 (PA6), lauryl-lactam for polyamide 12 (PA 12), cyclic oligomers of butylene terephthalate for poly(butylene terephthalate) (PBT) or radical polymerization as for poly(methyl methacrylate) (PMMA), from methyl methacrylate.

[0016] According to an improvement, the agglomeration step is preceded by a reinforcement step in which a reinforcing layer is deposited on or around at least part of the plurality of cords. This adds a significant reinforcement to the part making it possible to absorb transverse forces and increase the cohesion of the bundle of cords. The reinforcing layer is, for example, made up of one or more strips of woven or non-woven textile, pre-impregnated or not. It can also be a metal strip or a strand of continuous fibers, made of glass or carbon. The reinforcing layer may be around the entire plurality of cords. It may also be around only a portion of the cords. It may also be applied in a strip without completely surrounding the cords.

[0017] In one embodiment, the reinforcing layer is deposited by winding around the portion of the plurality of cords. The density of the reinforcing layer can be easily adapted by modulating the winding pitch. This adjusts the mechanical strength of the produced part according to requirements. In addition, the reinforcement is continuous around the entire periphery of the part, without breakage, which optimizes its mechanical contribution.

[0018] According to one embodiment, the composite part is a profiled part whose final section is greater than or equal to the sum of the sections of the beads entering the shaping means. Thus, all the material entering the shaping means leaves without loss. When the sums of the sections are equal, the beads are assembled without adding material or reflux, by feeding the shaping means with just the quantity necessary and sufficient to obtain the final section of the part.

[0019] According to an improvement, a third material is added to obtain the final section of the composite part. This allows for perfect control of the section of the part obtained, without loss of material and minimizing the risk of a lack of material in the part. The third complementary material is, for example, supplied by an extruder in the manner of coextrusion and also makes it possible to increase the pressure on the beads in order to better compact them and to coat the part with a surface layer, if necessary. This complementary material may be the same as that of the bead sheaths, or a separate material in order to provide specific surface properties, in particular resistance to aggressive environments and external appearance. During the material injection phase, the third thermoplastic material also compresses the plurality of beads, which ensures that the sheaths are agglomerated together.The contribution of additional material is typically less than 5% of the total volume of the part, preferably less than 2%.

[0020] According to a constructive arrangement, the shaping means comprise a drawing die in which the agglomeration step is carried out, the die comprising a grid followed by a compacting chamber and by a calibrator, the grid making it possible to guide the beads towards the compacting chamber, the calibrator making it possible to freeze the section of the part. The material which melts is thus enclosed in the compacting chamber. The section of the compacting chamber reduces downstream in order to force the beads against each other. The sheaths are fused together in such a way that they form a second single matrix. coating the cores of the cords. The calibrator makes it possible to give a precise section to the profile obtained, for example with cooling which allows the thermoplastic material to harden.

[0021] According to one embodiment, the composite part is a profiled part whose final volume is less than the sum of the volumes of the beads entering the shaping means, the shaping means comprising regulating means for regulating the pressure by allowing molten thermoplastic material to leak. In this case, the passage of the beads in the shaping means will create a reflux of molten material. Advantageously, the reflux of material is regulated in order to maintain a pressure which makes it possible to improve the compaction of the beads together. This method has the advantage of remaining simple in terms of tooling. The excess material is typically less than 2% of the section of the part.

[0022] According to an improvement, in the case where the composite part is a profiled part whose final section is greater than the sum of the sections of the beads entering the shaping means, the third thermoplastic material is injected into the compacting chamber. A profiled part is thus obtained without a lack of material. The third thermoplastic material is for example injected by an extruder. This method avoids any loss of material, which optimizes the consumption of raw material. The injection can be carried out at different locations in the compacting chamber, either very far upstream, or on the contrary further downstream.

[0023] According to an improvement, in the case where the composite part is a profiled part whose final section is greater than the sum of the sections of the beads entering the shaping means, the die further comprises an injection chamber located between the compacting chamber and the calibrator for injecting the third thermoplastic material. This ensures in this way that the section of the profiled part is perfectly determined. In addition, the injection pressure of the third thermoplastic material improves the compaction of the beads together.

[0024] According to one embodiment, the third thermoplastic material is identical to the second thermoplastic material.

[0025] According to one embodiment, the shaping means comprise a mold, by pressing in which the agglomeration step is carried out. The shape of the part is then not necessarily of constant section as in the case of a die. The mold can incorporate cooling means which make it possible to obtain the hardening of the part. Even if the pressing is carried out discontinuously, the mold can be mobile to follow the continuous supply of the beads and return upstream at each cycle. Alternatively, the mold is fixed and the drawing is carried out discontinuously. Here too, it is possible to regulate a reflux in an excess manner.

[0026] According to one embodiment, the shaping means form the curved part in order to produce a curved part. In the case of agglomeration in a die or using extrusion, the die has a curvature in the spinning direction, and the drawing means accompany the curvature of the profile. The production of curved profiles by this means is advantageous, because the fibers remain trapped in the cores and well distributed in the section of the part, despite the curvature which tends to bring the fibers closer to the intrados of the part.

[0027] The invention also relates to a composite part, characterized in that it is obtained with a method as described above, and in that it comprises a plurality of cords comprising a core with reinforcing fibers and a matrix made of a first thermoplastic material, the cores being arranged in a second matrix made of a second thermoplastic material. Such parts can incorporate cords with cores with optimized mechanical properties, in particular with a high fiber density, while being simple to manufacture. The second thermoplastic material can be chosen to be different from the first thermoplastic material for its own properties, in particular for its appearance and resistance to an aggressive environment. It can also be chosen for its thermal properties, in particular lower thermal conductivity than the core, in order to obtain a poorly conductive part.

[0028] According to an improvement, the melting temperature of the second material is lower than the melting temperature of the first material. Thus, during the manufacture of the part, the second thermoplastic material can be melted while the cores are still solid. The second thermoplastic material can then agglomerate to form a second matrix, the cores retaining their cross-section.

[0029] Alternatively, the first and second thermoplastic materials are identical. This results in a homogeneous, coherent and easy to recycle part.

[0030] According to an improvement, the second thermoplastic material is different from the first thermoplastic material and is treated to obtain an adhesion property on the first thermoplastic material. A part is thus obtained with good cohesion of the second matrix, while allowing the use of a second material which is normally incompatible, but which has other specific qualities.

[0031] According to a preferred choice, the first thermoplastic material is chosen from a group comprising polyamide-6, polyamide-12, polymethyl methacrylate, polybutylene terephthalate and polyethylene terephthalate. These thermoplastic materials can be used in reactive pultrusion which makes it possible to obtain cores of high mechanical quality, thanks to perfect impregnation of the fibers.

[0032] According to an advantageous combination, the first thermoplastic material is polyamide and the second material is acid-modified polypropylene. maleic acid. In the case of polypropylene and a core with a polyamide, the adhesion properties of one material to the other are weak. The addition of maleic acid to the polypropylene significantly modifies this adhesion capacity so that the polypropylene creates a second matrix of good quality. In addition, it adds its own qualities, in particular it creates a barrier against humidity with respect to the polyamide, both during storage of the sheathed cords and after the manufacture of the part. This eliminates the need for a drying step of the polyamide before the agglomeration step. It also makes it possible to provide an adhesion property to protrusions that can be molded over the part, particularly in polypropylene. The choice of treating the polypropylene with maleic acid to form the sheath is not a priori obvious, because acids are known to disrupt the anionic polymerization of polyamide.Tests have shown that this is not the case, and the bond between polyamide and polypropylene is strong.

[0033] According to an advantageous characteristic, the second thermoplastic material contains an electrically conductive filler. The composite part can thus more easily receive a coating by electrostatically assisted painting, by putting the part under tension.

[0034] According to advantageous characteristics, the average rate of fibers by volume is greater than 40%, preferably greater than 55%. This rate is for example calculated on a section, by calculating the ratio between the cumulative section of the fibers and that of the profile. A high rate of fibers allows significant mechanical resistance of the profile, in particular with high rigidity and resistance to breaking in bending or high traction.

[0035] According to advantageous characteristics, the fiber content of the cores of the cords by volume is greater than 50%, preferably greater than 60%.

[0036] According to advantageous characteristics, the continuous fibers of the core of the cords are chosen from a group comprising glass fibers, carbon fibers, plant fibers, metal fibers and aramid fibers.

[0037] According to an improvement, the part is a straight or curved profile having a constant section.

[0038] According to an improvement, the cords comprise at least one longitudinal cavity. In other words, the cords have a hollow section. These cavities are found on the part, in particular if during the agglomeration step, the first thermoplastic material is not melted. Such a part is lighter than a part with the same external section but without cavities. In addition, it is less thermally conductive, in particular for a heat flow in the transverse direction.

[0039] The invention also relates to an element comprising a part as defined above on which at least one protrusion is added by molding. over the part. The element thus comprises a part of essentially elongated shape, like a beam, on which is added the possibility of connection to an environment or of serving as a support for accessories. Molding over the part, or overmolding, consists of placing a part of the part in a mold and injecting molten thermoplastic material onto this part. The thermoplastic material then adheres to the part and forms the protrusion(s).

[0040] In the case of using a treated polypropylene as a second thermoplastic material, the protrusion is advantageously made of a fifth thermoplastic material which is polypropylene. A good bond is obtained between the part and the injected material of the protrusion. Brief description of the figures

[0041] The invention will be better understood and other features and advantages will appear on reading the description which follows, the description making reference to the appended drawings among which:

[0042] - [Fig.l] is a schematic view of a manufacturing installation implementing implements a method according to a first embodiment of the invention;

[0043] - [Fig.2] is a sectional view of a cord produced in an intermediate manner with the installation of [Fig.l];

[0044] - [Fig.3] is a sectional view of a first example of a profile produced with the installation of [Fig.l];

[0045] - [Fig.4] is a sectional view of a second example of a profile produced with the installation of [Fig.l];

[0046] - [Fig.5] is a schematic view of a manufacturing facility implementing implements a method according to a second embodiment of the invention;

[0047] - [Fig.6] is a sectional view of a third example of a profile produced with the installation of [Fig.5];

[0048] - [Fig.7] is a sectional view of a fourth example of profile;

[0049] - [Fig.8] is a sectional view of an agglomeration line;

[0050] - [Fig.9] is a schematic view of a manufacturing facility implementing implements a method according to a third embodiment of the invention;

[0051] - [Fig.10] is a schematic view of a manufacturing facility implementing implements a method according to a fourth embodiment of the invention, for producing curved profiles;

[0052] - [Fig.l 1] is a perspective view of an element produced with the installation of the [Fig.10] ;

[0053] - [Fig. 12] is a schematic view of a manufacturing facility featuring implements a method according to a fifth embodiment of the invention, for producing molded parts;

[0054] - [Fig.13] is a view similar to [Fig.8] of a die variant of agglomeration

[0055] - [Fig. 14] is a view similar to [Fig.2] of a cord according to a variant. Detailed description

[0056] A method for manufacturing composite parts with a thermoplastic matrix according to the invention is described in connection with an installation shown diagrammatically in [Fig.l].

[0057] A first part of the installation comprises a spinning device 1 for manufacturing cords 30 in a spinning step, while a second part concerns an agglomeration device 2 for implementing an agglomeration step. The spinning device 1 is in practice a pultrusion device 1 which successively comprises: a first reel support 10 for storing and unwinding reels of rovings 3010 of continuous fibers, a preheating unit 11 for the fibers 3010 which makes it possible to bring the glass fibers to a temperature close to the melting temperature of reactive monomers, i.e. approximately 80°C in the case of e-caprolactam. The fibers 3010 are heated by infrared ramps, not shown, under a nitrogen flow.The pultrusion device 1 further comprises an impregnation unit 12 receiving from an injection unit 13 reactive monomers or pre-polymers which form, after polymerization, a first thermoplastic material 3011. As illustrated, the components of the reactive system are metered separately and mixed just at the inlet of the impregnation unit 12, for example in a static mixer 14. A sheathing unit 15 comprises a first extruder 150 and an extrusion die 151 placed after the impregnation unit 12 which makes it possible to deposit a sheath 302 made of a second thermoplastic material around the impregnated strands, in a sheathing step. The device then comprises a polymerization oven 16 in which the cord 30 is maintained at temperature to allow the polymerization of the resin into the first thermoplastic material 3011, so that the impregnated wicks become a core 301 forming with the sheath 302 the cord 30.The pultrusion device 1 further comprises a first pulling unit 17 which makes it possible to simultaneously advance the cord 30 hardened by cooling and to unwind the strands 3010 by the propagation of the movement through the pultrusion device 1.

[0058] The cords 30 thus produced are wound onto other reels 18 in order to accumulate a sufficient number of cords 30 for the agglomeration step.

[0059] In a variant not shown, the cords are hollow, that is to say they have a longitudinal cavity within the core. They could also have several cavities separated by partitions.

[0060] The second part of [Fig. 1] shows the agglomeration device 2 comprising a second reel support 20 on which the reels 18 of cords 30 are placed to unwind the cords 30. A plurality of cords 30 is thus directed towards an oven 21 to heat the cords 30 to a temperature higher than the melting temperature of the second thermoplastic material 302. At the outlet of the oven 21, shaping means 22 assemble the plurality of cords 30 so that the sheaths 302 come into contact with each other and fuse. In this example, the shaping means 22 are an agglomeration die which determines the section of the profile 3 at the outlet. The agglomeration die 22 is provided with cooling means in order to obtain the hardening of at least a part of the profile 3 thus formed.A second pulling unit 23 exerts traction on the hardened profile 3 and causes the cords 30 to unwind by the propagation of the movement through the agglomeration device 2.

[0061] In a variant not shown, the pultruded cords 30 could directly supply the agglomeration device without going through a winding step.

[0062] In a first example, cords 30 were manufactured by pultrusion with a first matrix formed by the first thermoplastic material 3011, which is polyamide-6 obtained by the polymerization of ε-caprolactam monomer, and as fibers glass fibers in a rate of approximately 84% by mass. The section of the cores 301 of the cords 30 was circular and of diameter 3 mm, as shown in [Fig. 2]. The cores 301 were covered with a sheath 302 of polypropylene of thickness 0.2 to 0.5 mm. The melting temperature of polyamide-6 is 220 °C while that of polypropylene is 170 °C. Such cords 30 could be produced at a speed of the order of 2 m / min on a pilot installation limited in size.

[0063] In the agglomeration device 2, 15 cords 30 were used by passing them through the furnace 21 to raise the temperature of the cords 30 to 150°C, then to 200°C in the die. At this latter temperature, the sheath 302 was melted, but not the cores 301. The plurality of cords 30 was grouped in the agglomeration die 22 to form a profile 3 of rectangular section, as shown in [Fig. 3], in which the cores 301 are coated in a second matrix 32 formed by the second thermoplastic material from the sheaths 302. The fiber content of the cores 301 of the cords 30 by volume was 70%. Modular tooling made it possible to produce profiles with a section of 48 x 3.2 mm. The average fiber content by volume over the entire section varied around 48%. Such profiles 3 could be produced at a speed of around 0.5 m / min.

[0064] In a second example, cords 30 were manufactured in the same way as previously. In the agglomeration device 2, 15 cords 30 were used by passing them through the furnace 21 to raise the temperature of the cords 30 to 200°C, then through the die to 250°C. At this latter temperature, the sheath 302 and the first thermoplastic material 3011 were melted. The plurality of cords 30 was grouped in an agglomeration die 22 to form a profile 103 with a rectangular section of 50 x 2.5 mm, as shown diagrammatically in [Fig. 4], in which the cores 301 are coated in a second matrix 1032 formed by the second thermoplastic material from the sheaths 302. The temperature level reached made it possible to modify the section of the cores 301, to bring them together, to deform them and to compact them together.The fiber content of the 301 cores of the 30 cords by volume was 70% and the average fiber content by volume over the entire section was around 60%.

[0065] In a second embodiment of the invention, shown in [Fig. 5], the agglomeration device 2 further comprises a winding station 24 between the furnace 21 and the agglomeration die 22. The winding station 24 is fed by one or more reels 240 to provide a roving of continuous fibers 33 and deposit it by forming a winding around the plurality of cords 30. The nature of the fibers may be the same as that of the cores 301, or of a different nature. [Fig. 6] shows a section of profile 203 according to a third example which can be obtained in this way. The second thermoplastic material has passed through the fibers 33 of the winding and forms a matrix 2032 which impregnates the fibers of the winding.

[0066] In a variant of the method, the winding 33 is made around only a part of the cords 30a. The complementary part is consolidated with the other cords 30b after the winding 33 has been made. [Fig.7] shows a section according to a fourth example of profile 303 which can be obtained in this way.

[0067] In a variant of the method, not shown, the wick is coated in a third matrix of a fourth thermoplastic material prior to the reinforcement step, previously heated before introduction into the agglomeration die in order to melt the fourth thermoplastic material of the third matrix.

[0068] In the sectional view of an agglomeration die 22 of [Fig. 8], there is successively, in order from upstream to downstream, an inlet in the form of a grid 223 provided to guide the cords 30 to the inlet of the die 22, a compacting chamber 224 to finish melting the thermoplastic material and agglomerate all of the cords 30, and finally a sizer 225. The grid 223 has a hole for each of the cords 30 which enters the die 22 in order to control the relative arrangement of the beads 30 upon their entry. The compacting chamber 224 is temperature-regulated so as to finish melting the material which coats the beads 30 and the matrix of the beads 30 if applicable. The compacting chamber 224 further comprises a regulation channel 2240 provided with a valve 2241 in order to evacuate the excess thermoplastic material by regulating a pressure of this material. Finally, the calibrator 225 determines the section of the final part and cools it in order to at least partially freeze this section.

[0069] According to a third embodiment, shown in [Fig.9], the shaping means 22' comprise an extruder 221 and an agglomeration die 222, a third thermoplastic material prepared by the extruder being injected around the plurality of cords 30 in the agglomeration die 222.

[0070] The agglomeration die 222 for the embodiment of [Fig. 9] is shown in [Fig. 13]. It differs from the die shown in [Fig. 8] in that it comprises an injection chamber 2220 located between the compacting chamber 224 and the calibrator 225. The compacting chamber 224 no longer comprises a regulating channel. Into the injection chamber 2220, the extruder 220 injects the third thermoplastic material that is necessary to complete the section of the final part. The pressure supplied by the extruder to the third thermoplastic material also makes it possible to complete the compaction of the beads 30 carried out in the compacting chamber 224.

[0071] In a variant of the third embodiment, not shown, the agglomeration die is similar to that shown in [Fig.8], with an injection of the material supplied by the extruder just downstream of the grid 223. The third thermoplastic material thus injected makes it possible to supplement the lack of second material provided by the sheaths of the cords.

[0072] In a fourth embodiment, shown in [Fig. 10], the installation differs from that of the first embodiment in that the die 22'' is curved in the drawing direction and the drawing means 23” are adapted to draw a 3” profile whose main direction is curved. It is possible that only the calibrator 225 is curved.

[0073] [Fig. 11] schematically shows an element 503 forming a bumper crossmember type part for a motor vehicle. This crossmember 503 is produced from a 3” C-shaped profile resulting from the process of [Fig. 10] and on which two protrusions 5030 have been molded forming ears schematizing stiffeners made of a fifth thermoplastic material, namely polypropylene. In this 3” profile, the first thermoplastic material is polyamide, the second material is polypropylene treated with maleic acid.

[0074] In a fifth embodiment, shown in [Fig. 12], the shaping means comprise a mold 22”’ in which the agglomeration step is carried out by pressing, discontinuously. The mold 22’” comprises cooling means, not shown, in order to allow the hardening of the molded part 3’”. The mold 22”’ is mounted to move in translation by translation means 25 in the drawing direction to return cyclically to the outlet of the furnace and enclose the plurality of beads 30 upstream of the previously molded part. When the mold 22’” closes, the beads 30 which have been previously heated agglomerate. The drawing means 23’” operate continuously, in this example. In a variant not shown, the mold does not translate and the drawing is carried out intermittently.

[0075] In a variant shown in [Fig. 14], the cord 30' has a rectangular section, as do the core 301' and the sheath 302' which coats the core 301'. The core is composed of fibers 3010' coated in a first matrix 3011'. Such a section of the cord 30' may be more suitable for the manufacture of certain parts by allowing a more adjusted assembly of several cords 30' having such a section. It is also necessary in this case to manage the orientation of the section of the cords 30' when they enter the shaping means 22. A form factor is defined as being the ratio between the dimension of the largest section and the smallest dimension. The form factor may vary between 1 and 5, or even 10 or beyond. The cord 30' further comprises a longitudinal cavity 303 of also rectangular section.This arrangement allows it to confer specific properties to the reconstituted part, particularly in terms of thermal properties by reducing conductivity and mechanical properties by lightening the structure.

Claims

Claims

1. Method for manufacturing composite parts with a thermoplastic matrix according to which: - a plurality of cords (30) are used comprising a core (301) with reinforcing fibers taken in a first matrix made of a first thermoplastic material (3011);- in an agglomeration step, the plurality of cords (30) are heated and then the cords (30) are agglomerated by passing them together through shaping means (22) by traction to form the part (3), characterized in that at least one of the cords (30) of the plurality of cords further comprises a sheath (302) in a second thermoplastic material around the core (301), the heating of the plurality of cords (30) in the agglomeration step being done to reach a temperature higher than the melting temperature of the second thermoplastic material so as to change the second thermoplastic material from the solid state to the molten state, such that the second thermoplastic material forms a second matrix around the cores (301) after agglomeration and hardening.;

2. The method of claim 1, wherein, during the agglomeration step, the plurality of beads (30) are heated to a temperature above the respective melting temperatures of the first and second thermoplastic materials (3011, 32).

3. Method according to claim 1, according to which, during the agglomeration step, the melting temperature of the second thermoplastic material (32) being lower than that of the first thermoplastic material (3011), the plurality of beads (30) are heated to a temperature lower than the melting temperature of the first thermoplastic material (3011).

4. Method according to one of the preceding claims, according to which the cords (30) are produced in a reactive pultrusion step, the core comprising continuous fibers.

5. The method of claim 4, wherein the reactive pultrusion produces the first thermoplastic material (3011) selected from a group comprising polyamide-6, polyamide-12, polymethyl methacrylate and polybutylene terephthalate.

6. A method according to one of the preceding claims, wherein the agglomeration step is preceded by a reinforcement step in which a reinforcing layer (33) is deposited on or around at least part of the plurality of cords (30).

7. The method of claim 6, wherein the reinforcing layer (33) is deposited by wrapping around the portion of the plurality of cords (30).

8. Method according to one of the preceding claims, according to which the composite part is a profiled part whose final section is greater than or equal to the sum of the sections of the cords (30) entering the shaping means (22).

9. Method according to claim 8, according to which a third material is added to obtain the final section of the composite part.

10. Method according to one of the preceding claims, according to which the shaping means comprise a die (22) by drawing in which the agglomeration step is carried out, the die (22) comprising an inlet (223) followed by a compacting chamber (224) and by a calibrator (225), the calibrator (225) making it possible to freeze the section of the part.

11. A method according to claim 9 and 10 taken in combination, wherein the third thermoplastic material is injected into the compacting chamber.

12. A method according to claim 9 and 10 taken in combination, wherein the die further comprises an injection chamber (2220) located between the compacting chamber (224) and the sizer (225) for injecting the third thermoplastic material.

13. Method according to one of claims 10 to 12, according to which the inlet is a grid (223) allowing the cords (30) to be guided towards the compacting chamber (224).

14. Method according to one of claims 1 to 7, according to which the composite part is a part whose final volume is less than the sum of the volumes of the beads (30) entering the shaping means (22), the shaping means (22) comprising regulating means (2240, 2241) for regulating the pressure by allowing molten thermoplastic material to leak.

15. Method according to one of claims 1 to 8 or claim 14, according to which the shaping means comprise a mold (22”), by pressing in which the agglomeration step is carried out.

16. A method according to any preceding claim, wherein the shaping means (22”) forms the curved part to produce a curved part (3”).

17. Composite part, characterized in that it is obtained with a method according to one of the preceding claims, and in that it comprises a plurality of cords (30) comprising a core (301) with reinforcing fibers and a matrix made of a first thermoplastic material (3011), the cores (30) being arranged in a second matrix made of a second thermoplastic material (32).

18. The part of claim 17, wherein the first thermoplastic material (3011) is selected from a group comprising polyamide-6, polyamide-12, polymethyl methacrylate, polybutylene terephthalate, and polyethylene terephthalate.

19. Part according to one of claims 17 or 18, in which the second thermoplastic material (32) is different from the first thermoplastic material (3011) and is treated to obtain an adhesion property on the first thermoplastic material (3011).

20. A part according to claims 18 and 19 taken in combination, wherein the first thermoplastic material is polyamide and the second material is polypropylene modified with maleic acid.

21. Part according to one of claims 17 to 20, in which the melting temperature of the second material (32) is lower than the melting temperature of the first thermoplastic material (3011).

22. Part according to claim 17 or 18, characterized in that it is obtained with a method according to one of claims 1, 2, or 4 to 16, in which the first and second thermoplastic material (3011, 32) are identical.

23. Part according to one of claims 17 to 22, in which the second thermoplastic material contains an electrically conductive filler.

24. Part according to one of claims 17 to 23, in which the average rate of fibers by volume is greater than 40%, preferably greater than 55%.

25.

26.

27.

28.

29.

30. Part according to one of claims 17 to 24, in which the fiber content of the cores (301) of the cords (30) by volume is greater than 50%, preferably greater than 60%. Part according to one of claims 17 to 25, in which the reinforcing fibers of the core (301) of the cords (30) are chosen from a group comprising glass fibers, carbon fibers, plant fibers, metal fibers and aramid fibers. Part according to one of claims 17 to 26, characterized in that it is a straight (3) or curved (3”) profile having a constant section. Part according to one of claims 17 to 27, in which the cords comprise at least one longitudinal cavity. Element characterized in that it comprises a part according to one of claims 17 to 28, on which at least one protrusion (5030) is added by molding over the part (3”). The element of claim 29, wherein the protrusion (5030) is made of a fifth thermoplastic material which is polypropylene.