Ceramic substrate, manufacturing method for the same, electrostatic chuck, substrate fixing device, and package for semiconductor device

JP2023141972A5Active Publication Date: 2024-10-09SHINKO ELECTRIC IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2022048585
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2022-03-24
Publication Date
2024-10-09
Estimated Expiration
2042-03-24

AI Technical Summary

Technical Problem

Conventional sintering processes for ceramic substrates with tungsten-based electrostatic chucks face challenges due to tungsten's high melting point, necessitating the use of sintering aids that require higher temperatures, which are difficult to manage and costly.

Method used

Incorporating a body-centered cubic lattice structure with copper dissolved in tungsten as the main component for the conductor pattern, allowing for sintering at lower temperatures, specifically around 1100°C, by adding copper oxide as a sintering aid.

Benefits of technology

Enables sintering of conductor patterns at approximately 150°C lower temperatures than conventional methods, improving sinterability and reducing processing complexity and costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
Patent Text Reader

Abstract

To make it possible to sinter a conductor pattern on a ceramic substrate at a lower temperature than before.SOLUTION: The ceramic substrate has a base body and a conductor pattern built into the base body. The base body is ceramic. The conductor pattern is mainly composed of a solid solution of tungsten with a body-centered cubic lattice structure in which copper is solidly dissolved in tungsten.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a ceramic substrate and a manufacturing method thereof, an electrostatic chuck, a substrate fixing device, and a package for a semiconductor device. [Background technology]

[0002] Conventionally, film deposition equipment and plasma etching equipment used in manufacturing semiconductor devices have a stage for precisely holding a wafer in a vacuum processing chamber. As such a stage, for example, a substrate fixing device has been proposed that attracts and holds a wafer using an electrostatic chuck mounted on a base plate.

[0003] The electrostatic chuck is made of a ceramic substrate having a base body, an electrostatic electrode built into the base body, etc. The electrostatic electrode is, for example, a sintered body containing tungsten as a main component and also containing nickel oxide, aluminum oxide, and silicon dioxide (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Publication No. 2020-43336 Summary of the Invention [Problem to be solved by the invention]

[0005] In the above-mentioned sintered body, ceramics and tungsten are sintered under the same conditions, but tungsten is difficult to sinter due to its high melting point (over 3300°C), making it necessary to add an appropriate sintering aid. Nickel oxide, aluminum oxide, and silicon dioxide function as sintering aids in the above-mentioned sintered body. The liquidus temperature changes depending on the sintering aid added, but there is a demand for sintering aids that can lower the liquidus temperature below conventional levels, allowing sintering at relatively low temperatures.

[0006] The present invention has been made in view of the above points, and has as its object to make it possible to sinter a conductor pattern on a ceramic substrate at a temperature lower than conventional temperatures. [Means for solving the problem]

[0007] This ceramic substrate has a base and a conductive pattern embedded in the base, the base being made of ceramic, and the conductive pattern having a body-centered cubic lattice structure as its main component, in which copper is solid-solved in tungsten. [Effects of the Invention]

[0008] According to the disclosed technology, the conductor pattern on the ceramic substrate can be sintered at a lower temperature than conventionally. [Brief explanation of the drawings]

[0009] [Figure 1] 1 is a cross-sectional view illustrating a simplified example of a substrate fixing device according to a first embodiment. [Figure 2] FIG. 2 is a simplified plan view illustrating the substrate fixing device according to the first embodiment. [Figure 3] 1A to 1C are perspective views (part 1) illustrating a manufacturing process of the electrostatic chuck according to the first embodiment. [Figure 4] 6A to 6C are perspective views (part 2) illustrating the manufacturing process of the electrostatic chuck according to the first embodiment. [Figure 5] This is the result of the investigation into the liquidus temperature (part 1). [Figure 6] This is the result of the investigation into the liquidus temperature (part 2). [Figure 7] This is the result of the investigation into the liquidus temperature (part 3). [Figure 8] FIG. 10 is a cross-sectional view illustrating a package for a semiconductor device according to a second embodiment. [Figure 9] FIG. 10 is a plan view illustrating a package for a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE INVENTION

[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings, the same components are denoted by the same reference numerals, and redundant explanations may be omitted.

[0011] First Embodiment [Structure of the substrate holding device] Fig. 1 is a simplified cross-sectional view illustrating a substrate fixing device according to a first embodiment. Referring to Fig. 1, the substrate fixing device 1 has, as its main components, a base plate 10 and an electrostatic chuck 20. The substrate fixing device 1 is a device that uses the electrostatic chuck 20 to attract and hold a substrate W (e.g., a semiconductor wafer) that is an object to be attracted.

[0012] The base plate 10 is a member on which the electrostatic chuck 20 is mounted. The thickness of the base plate 10 is, for example, about 20 to 40 mm. The base plate 10 is formed from, for example, a metal material such as aluminum or cemented carbide, or a composite material of such a metal material and a ceramic material, and can be used as an electrode for controlling plasma. For example, in view of ease of availability, ease of processing, and good thermal conductivity, a base plate made of aluminum or an alloy thereof with its surface anodized (insulating layer formed) is preferably used.

[0013] For example, by supplying a predetermined high-frequency power to the base plate 10, the energy for causing the generated ions in the plasma state to collide with the substrate W adsorbed on the electrostatic chuck 20 can be controlled, thereby enabling the etching process to be performed effectively.

[0014] A gas supply path may be provided inside the base plate 10 to introduce an inert gas for cooling the substrate W attracted to the electrostatic chuck 20. When an inert gas such as He or Ar is introduced from the outside of the substrate fixing device 1 into the gas supply path and the inert gas is supplied to the back surface of the substrate W attracted to the electrostatic chuck 20, the substrate W can be cooled.

[0015] A coolant flow path may be provided inside the base plate 10. The coolant flow path is, for example, a hole formed in a ring shape inside the base plate 10. A coolant such as cooling water or Galden is introduced into the coolant flow path from the outside of the substrate fixing device 1. By circulating the coolant through the coolant flow path to cool the base plate 10, the substrate W attracted to the electrostatic chuck 20 can be cooled.

[0016] The electrostatic chuck 20 is a part that attracts and holds the substrate W, which is an object to be attracted. The planar shape of the electrostatic chuck 20 is formed according to the shape of the substrate W, and is, for example, circular. The diameter of the wafer, which is an object to be attracted to the electrostatic chuck 20, is, for example, 8, 12, or 18 inches.

[0017] Note that a plan view refers to viewing the object from the normal direction of the upper surface 10a of the base plate 10, and a planar shape refers to the shape of the object viewed from the normal direction of the upper surface 10a of the base plate 10.

[0018] The electrostatic chuck 20 is provided on the upper surface 10a of the base plate 10 via an adhesive layer. The adhesive layer is, for example, a silicone adhesive. The thickness of the adhesive layer is, for example, about 0.1 to 2.0 mm. The adhesive layer not only bonds the base plate 10 and the electrostatic chuck 20 together, but also has the effect of reducing stress caused by the difference in thermal expansion coefficient between the ceramic electrostatic chuck 20 and the aluminum base plate 10. The electrostatic chuck 20 may be fixed to the base plate 10 with screws.

[0019] The electrostatic chuck 20 is a ceramic substrate having, as its main components, a base 21, an electrostatic electrode 22, and a heating element 24. The upper surface of the base 21 is a mounting surface 21a on which an object to be attracted is placed. The electrostatic chuck 20 is, for example, a Johnsen-Rahbek type electrostatic chuck. However, the electrostatic chuck 20 may also be a Coulomb force type electrostatic chuck.

[0020] The substrate 21 is a dielectric. The thickness of the substrate 21 is, for example, about 5 to 10 mm, and the relative dielectric constant (1 kHz) of the substrate 21 is, for example, about 9 to 10. The substrate 21 is a ceramic made of, for example, aluminum oxide (Al2O3), aluminum nitride (AlN), yttrium aluminum garnet (YAG), or the like. Among these, it is preferable to use ceramic made of aluminum oxide, which is easy to sinter, relatively low cost, and has high electrical resistance. Here, "ceramics made of aluminum oxide" means ceramics to which no inorganic components other than aluminum oxide are added.

[0021] The aluminum oxide purity of the substrate 21 is preferably 99.5% or higher. A purity of 99.5% or higher indicates that the substrate is formed without adding a sintering aid. A purity of 99.5% or higher also indicates that the substrate may contain impurities unintentionally present in the manufacturing process, etc. The relative density of the substrate 21 to the aluminum oxide is preferably 97% or higher. The average particle size of the aluminum oxide in the substrate 21 is preferably 1.0 μm or higher and 3.0 μm or lower.

[0022] The electrostatic electrode 22 is a thin-film electrode formed by a conductor pattern and is built into the base 21. In this embodiment, the electrostatic electrode 22 is a bipolar type and includes a first electrostatic electrode 22a and a second electrostatic electrode 22b. Note that a monopolar type consisting of a single electrostatic electrode may also be used as the electrostatic electrode 22. The electrostatic electrode 22 is mainly composed of a solid solution of tungsten and copper with a body-centered cubic lattice structure. Here, "main component" means a component that accounts for 50 wt% or more of the total material constituting the electrostatic electrode 22. In the electrostatic electrode 22, the ratio of copper to tungsten is preferably 0.05 wt% or more and 10 wt% or less.

[0023] The first electrostatic electrode 22a is connected to the positive electrode of a power supply 40a provided outside the substrate fixing device 1. The second electrostatic electrode 22b is connected to the negative electrode of a power supply 40b provided outside the substrate fixing device 1. The negative electrode of the power supply 40a and the positive electrode of the power supply 40b are connected outside the substrate fixing device 1, and the connection point is at ground potential.

[0024] A positive (+) voltage is applied to the first electrostatic electrode 22a from the power supply 40a, and a negative (-) voltage is applied to the second electrostatic electrode 22b from the power supply 40b. As a result, a positive (+) charge is applied to the first electrostatic electrode 22a, and a negative (-) charge is applied to the second electrostatic electrode 22b. Accordingly, a negative (-) charge is induced in the portion Wa of the substrate W corresponding to the first electrostatic electrode 22a, and a positive (+) charge is induced in the portion Wb of the substrate W corresponding to the second electrostatic electrode 22b.

[0025] If the substrate W, the electrostatic electrode 22, and the ceramic part 25 of the electrostatic chuck 20 (base 21) disposed therebetween are regarded as a capacitor, the ceramic part 25 corresponds to a dielectric layer. The substrate W is electrostatically attracted to the electrostatic chuck 20 by the Coulomb force generated between the electrostatic electrode 22 and the substrate W via the ceramic part 25. The attracting and holding force becomes stronger as the voltage applied to the electrostatic electrode 22 increases.

[0026] The heating element 24 is a heater built into the base 21, which generates heat when a current flows through it to heat the mounting surface 21a of the base 21 to a predetermined temperature. The heating element 24 is disposed below (on the base plate 10 side of) the first electrostatic electrode 22a and the second electrostatic electrode 22b. The heating element 24 is a conductor formed in a film shape. The heating element 24 is provided as a plurality of heater electrodes that can independently control the heating of a plurality of regions (heater zones) on the base 21 in a plane.

[0027] The heating element 24 may be provided as a single heater electrode. The heating element 24 is mainly composed of, for example, a solid solution of tungsten and copper with a body-centered cubic lattice structure.

[0028] When a current is supplied to the heating element 24 from a power source provided outside the substrate fixing device 1, the heating element 24 generates heat, thereby heating the electrostatic chuck 20. The temperature of the substrate W is controlled to a predetermined temperature by the temperature of the electrostatic chuck 20. The heating temperature of the electrostatic chuck 20 is set within a range of 50°C to 200°C, for example, to 150°C.

[0029] Fig. 2 is a simplified plan view illustrating the substrate holding device according to the first embodiment. Referring to Fig. 2, in the substrate holding device 1, an electrostatic chuck 20 is disposed on a disk-shaped base plate 10, and the peripheral portion of the base plate 10 is exposed around the electrostatic chuck 20. Mounting holes 11 for mounting the base plate 10 to a chamber of a semiconductor manufacturing device are arranged along the peripheral portion.

[0030] Furthermore, the electrostatic chuck 20 and the base plate 10 have a plurality of (three in FIG. 2 ) lift pin openings 12 in the center. Lift pins for moving the substrate W in the vertical direction are inserted into the lift pin openings 12. By lifting the substrate W above the mounting surface 21 a with the lift pins, the substrate W can be automatically transported by a transport device.

[0031] [Electrostatic chuck manufacturing method] Next, a description will be given of a manufacturing method of the electrostatic chuck 20. Figures 3 and 4 are perspective views illustrating the manufacturing process of the electrostatic chuck according to the first embodiment.

[0032] First, as shown in FIG. 3(a), a green sheet 51 made of a ceramic material and an organic material is prepared. The green sheet 51 is formed, for example, into a rectangular plate shape. The ceramic material of the green sheet 51 is made of aluminum oxide and does not contain a sintering aid. The organic components are removed from the green sheet 51, and the ceramic material is sintered and densified, thereby forming the base 21 on which the substrate W shown in FIG. 1 is mounted.

[0033] 3(b), a green sheet 52 made of the same material and having the same shape as the green sheet 51 is prepared, and a conductive paste is printed on the upper surface of the green sheet 52 by, for example, a printing method (screen printing) to form a conductor pattern 55. The conductor pattern 55 will become the electrostatic electrode 22 shown in FIG. 1 when fired in a step described later. The conductor pattern 55 may also be formed on the lower surface of the green sheet 51.

[0034] The conductive paste used to form the conductor pattern 55 contains, for example, tungsten as a main component and copper oxide. The conductive paste used to form the conductor pattern 55 may further contain an organic material, etc. The amount of copper oxide added is preferably, for example, 0.1 g to 10 g per 100 g of tungsten. That is, the ratio of copper oxide to tungsten in the conductive paste is preferably 0.1 wt% to 10 wt%. When the ratio of copper oxide to tungsten is 0.1 wt% or more, the liquidus temperature of the conductive paste can be approximately 1100°C.

[0035] Even if the ratio of copper oxide to tungsten is greater than 10 wt%, the liquidus temperature of the conductive paste remains approximately 1100°C. However, if the ratio of copper oxide to tungsten exceeds 10 wt%, the electrical characteristics of tungsten are less likely to be exhibited in the tungsten-copper solid solution produced by sintering the conductive paste. Therefore, it is preferable that the ratio of copper oxide to tungsten be 10 wt% or less. Furthermore, when co-firing the conductive paste and green sheet, it is preferable that the average particle size of tungsten be 0.5 μm or more and 3.0 μm or less.

[0036] Next, as shown in FIG. 3(c), a green sheet 53 made of the same material and shape as the green sheet 51 is prepared, and a conductive paste is printed on the upper surface of the green sheet 53 by, for example, a printing method (screen printing) to form a conductor pattern 57. The conductive paste for forming the conductor pattern 57 may be made of the same material as the conductive paste for forming the above-mentioned conductor pattern 55. The green sheet 53 is used for forming the heating element 24 shown in FIG. 1 when fired, and becomes the substrate 21 of the portion that is bonded to the base plate 10. The conductor pattern 57 becomes the heating element 24 when fired in a step described below. The conductor pattern 57 may also be formed on the lower surface of the above-mentioned green sheet 52.

[0037] Next, as shown in Fig. 4(a), the green sheets 51 to 53 are stacked to form a structure 71a. The green sheets 51 to 53 are bonded to one another by applying heat and pressure. Next, as shown in Fig. 4(b), the periphery of the structure 71a is cut to form a disk-shaped structure 71b.

[0038] Next, the structure 71b shown in FIG. 4(b) is fired to obtain the ceramic substrate 72a shown in FIG. 4(c). The firing temperature is, for example, 1600°C. In this process, the electrostatic electrode 22 is obtained by sintering the conductor pattern 55, and the heating element 24 is obtained by sintering the conductor pattern 57. The liquid phase temperature of the conductive paste in which copper oxide is added to tungsten is approximately 1100°C, so it is easily sintered at the temperature (for example, 1600°C) used to fire the ceramic substrate 72a. As a result, the electrostatic electrode 22 and the heating element 24 are formed, each of which is mainly composed of a solid solution of tungsten and copper with a body-centered cubic lattice structure.

[0039] Next, various processes are performed on the ceramic substrate 72a to complete the electrostatic chuck 20. For example, the upper and lower surfaces of the ceramic substrate 72a are polished to form a mounting surface and an adhesive surface. Also, the lift pin openings 12 shown in FIG. 1 are formed in the ceramic substrate 72a.

[0040] The substrate fixing device and the like will be explained in more detail below with reference to examples and comparative examples, but the present invention is not limited to these examples in any way.

[0041] [Consideration of liquidus temperature] First, as a comparative example, 1 g of nickel oxide, 1 g of aluminum oxide, and 1 g of silicon dioxide were added to 100 g of tungsten, and the mixture was fired in an atmosphere of nitrogen and hydrogen. The liquidus temperature was calculated using Fact Stage (manufactured by Computational Mechanics Research Center, Inc.) Fact Stage is software that quantitatively predicts the thermodynamic equilibrium state of a multi-component system.

[0042] The calculation results for the comparative example are shown in Figure 5. Note that Figure 5(b) is an enlarged view of the area surrounded by the dashed line in Figure 5(a). As shown in Figure 5, calculations confirmed that sintering the material according to the comparative example results in the formation of a solid solution with a body-centered cubic lattice structure in which nickel is solid-dissolved in tungsten. Furthermore, in the comparative example, the liquidus temperature was approximately 1330°C.

[0043] Next, as an example, the liquidus temperature when 1 g of copper oxide was added to 100 g of tungsten and adjusted in an atmosphere of nitrogen and hydrogen was calculated using Fact Stage.

[0044] The calculation results for the example are shown in Figure 6. Note that Figure 6(b) is an enlarged view of the area surrounded by the dashed line in Figure 6(a). As shown in Figure 6, it was confirmed by calculation that a solid solution with a body-centered cubic lattice structure in which copper is dissolved in tungsten is formed by sintering the material according to the example. Furthermore, in the example, the liquidus temperature was approximately 1100°C.

[0045] Next, we used FactStage to calculate whether the liquidus temperature changes depending on the amount of copper oxide added to tungsten. Figures 7(a) to 7(c) show the calculation results for the cases where 0.1 g, 2 g, and 10 g of copper oxide are added to 100 g of tungsten. As shown in Figures 7(a) to 7(c), even when 0.1 g of copper oxide is added to 100 g of tungsten, a liquid phase is formed, and the liquidus temperature is approximately 1100 °C. Furthermore, it was found that even if the amount of copper oxide added to 100 g of tungsten is increased, the amount of liquid phase simply increases, and the liquidus temperature remains constant at approximately 1100 °C. In other words, the calculation confirmed that when copper oxide is added to tungsten and then sintered, the liquidus temperature does not depend on the amount of copper oxide added.

[0046] In this way, when copper oxide is added to tungsten and then fired, the liquidus temperature can be raised to approximately 1100°C, making it possible to sinter the conductor pattern at a temperature approximately 150°C lower than in the conventional method (comparison example), thereby improving the sinterability of tungsten.

[0047] When aluminum oxide is used for the base, the sintering temperature is approximately 1500°C to 1600°C. Therefore, the liquidus temperature of the conductor pattern should be lower than this, but a lower temperature makes it easier to handle and also makes it possible to use materials other than aluminum oxide that sinter at lower temperatures. Furthermore, due to restrictions on the firing process of the base, the liquidus temperature of the conductor pattern is preferably 800°C or higher.

[0048] Second Embodiment In the second embodiment, an example of a package for a semiconductor device having the ceramic substrate described in the first embodiment is shown. Fig. 8 is a cross-sectional view illustrating the package for a semiconductor device according to the second embodiment. Fig. 9 is a plan view illustrating the package for a semiconductor device according to the second embodiment.

[0049] As shown in FIG. 8, the semiconductor device package 100 has a ceramic substrate 110, a heat sink 150, and external connection terminals 160, and the heat sink 150 is brazed to the ceramic substrate 110.

[0050] The ceramic substrate 110 has a plurality of laminated ceramic bases 111, 112, 113, and 114 (four in this embodiment), wiring patterns 121, 122, 123, and 124 which are examples of conductor patterns, and vias 132, 133, and 134 which penetrate the ceramic bases 112, 113, and 114. The via 132 connects the wiring patterns 121 and 122 to each other, the via 133 connects the wiring patterns 122 and 123 to each other, and the via 134 connects the wiring patterns 123 and 124 to each other. In the ceramic substrate 110, the ceramic bases 111 to 114 form a base.

[0051] 8 and 9, the ceramic substrate 110 is provided with a cavity 170 that penetrates the center of the ceramic bases 112, 113, and 114 and in which the semiconductor element 200 is mounted. The wiring pattern 121 is disposed on the upper surface of the ceramic base 112 so as to surround the cavity 170. The ceramic base 111 is formed with an opening 111X that exposes the wiring pattern 121.

[0052] The ceramic bases 111-114 are ceramics made of aluminum oxide, and the wiring patterns 121-124 are mainly composed of a solid solution of tungsten and copper with a body-centered cubic lattice structure. The vias 132-134 are sintered bodies containing, for example, molybdenum as a main component, nickel oxide, aluminum oxide, and silicon dioxide. The ceramic substrate 110 can be manufactured by the same manufacturing method as the electrostatic chuck 20 of the first embodiment.

[0053] In the semiconductor device package 100, the semiconductor element 200 is mounted on the heat sink 150. Pads of the semiconductor element 200 are electrically connected to the wiring pattern 121 of the ceramic substrate 110 by bonding wires or the like. As a result, the semiconductor element 200 is connected to the external connection terminal 160 via the wiring patterns 121 to 124 and the vias 132 to 134.

[0054] In the semiconductor device package 100, the wiring patterns 121 to 124 can be formed by sintering a conductive paste containing tungsten as the main component and copper oxide as an additive, which, like the first embodiment, allows the wiring patterns to be sintered at a temperature about 230°C lower than conventionally, improving the sinterability of tungsten.

[0055] Although the preferred embodiments have been described in detail above, the present invention is not limited to the above-described embodiments, and various modifications and substitutions can be made to the above-described embodiments without departing from the scope of the claims.

[0056] For example, in the first embodiment, the members included in the substrate fixing device and their arrangement may be changed as appropriate.

[0057] In the first embodiment, the heating element 24 may be disposed between the electrostatic chuck 20 and the base plate 10. Alternatively, the heating element 24 may be disposed inside the base plate 10. Alternatively, the heating element 24 may be attached externally below the electrostatic chuck.

[0058] The substrate fixing device according to the first embodiment is applied to a semiconductor manufacturing device, for example, a dry etching device (for example, a parallel plate type reactive ion etching (RIE) device).

[0059] Furthermore, examples of objects to be attracted by the substrate fixing device according to the first embodiment include glass substrates used in the manufacturing process of liquid crystal panels and the like, in addition to semiconductor wafers (silicon wafers and the like). [Explanation of symbols]

[0060] 1 Board fixing device 10 Base Plate 11 Mounting hole 12 Lift pin opening 20 Electrostatic Chuck 21 Base 22 Electrostatic Electrode 22a First electrostatic electrode 22b Second electrostatic electrode 24 Heating element 25 Ceramics Department 40a, 40b power supply 51, 52, 53 Green Sheets 55, 57 Conductor pattern 71a, 71b structure 72a Ceramic substrate 100 Semiconductor device package 110 Ceramic substrate 111~114 Ceramic substrate 121~124 Wiring pattern 132~134 Beer

Claims

1. a substrate; a conductive pattern embedded in the substrate, the substrate is ceramic, The conductive pattern is a ceramic substrate whose main component is a solid solution of tungsten and copper with a body-centered cubic lattice structure.

2. 2. The ceramic substrate according to claim 1, wherein the base is mainly composed of aluminum oxide.

3. 3. The ceramic substrate according to claim 2, wherein the aluminum oxide in the base has a purity of 99.5% or more.

4. 4. The ceramic substrate according to claim 2, wherein the base has a relative density of 97% or more with respect to aluminum oxide.

5. 5. The ceramic substrate according to claim 2, wherein the base has an average grain size of aluminum oxide of 1.0 μm or more and 3.0 μm or less.

6. A package for a semiconductor device, comprising the ceramic substrate according to any one of claims 1 to 5.

7. 6. The electrostatic chuck according to claim 1, wherein the conductive pattern is an electrostatic electrode.

8. A base plate and A substrate fixing device comprising: an electrostatic chuck according to claim 7 mounted on one surface of the base plate.

9. A method for manufacturing a ceramic substrate having a base and a conductor pattern embedded in the base, comprising: forming a conductor pattern on the upper surface of the green sheet using a conductive paste containing tungsten and copper oxide; and firing the green sheet and the conductor pattern to form the base and the conductor pattern.

10. 10. The method for manufacturing a ceramic substrate according to claim 9, wherein a ratio of the copper oxide to the tungsten in the conductive paste is 0.1 wt % or more and 10 wt % or less.