Integration of vapor deposition processes into plasma etching reactors.
Patent Information
- Application Number
- JP2023518343
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-10-23
- Filing Date
- 2021-10-22
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2041-10-22
AI Technical Summary
The challenge in semiconductor manufacturing is etching high aspect ratio features with narrow widths and deep depths in a uniform manner, particularly when combining plasma etching and vapor-based deposition processes in a single reactor, which leads to issues like unwanted condensation, residue formation, and conductance mismatches.
The solution involves a reactor design with adjustable flow conductance, separate gas paths for etching and deposition gases, and plasma cleaning mechanisms to minimize residue buildup and optimize conductance for both processes, allowing for variable and controlled gas flow to manage condensation and residue effectively.
This approach enhances processing efficiency by reducing unwanted deposits, improving throughput, and ensuring high-quality etching and deposition results by maintaining uniform gas flow and minimizing side reactions.
Smart Images

Figure 2022087365000001 
Figure 2022087365000002 
Figure 2022087365000003
Abstract
Description
Technical Field
[0001] Incorporation by Reference As part of this application, a PCT application form is filed simultaneously with this specification. Each application specified in the PCT application form filed simultaneously and for which this application claims benefit or priority is hereby incorporated by reference in its entirety for all purposes into this specification.
Background Art
[0002] One process frequently employed during the manufacture of semiconductor devices is to form cylindrical or other concave features etched into a dielectric material. Examples of situations in which such a process can be performed include memory applications such as DRAM and 3D NAND. As the semiconductor industry advances and device dimensions become smaller, it becomes increasingly difficult to etch such concave features, particularly high aspect ratio features having a narrow width and / or a deep depth, in a uniform manner.
[0003] The description of the background art presented herein is intended to generally present the content of the present disclosure. The research by the inventors named at the present time, within the scope described in this background art section, cannot be considered separately as prior art at the time of filing, in the same manner as aspects of the description that cannot be considered as prior art against the present disclosure, whether explicitly or implicitly.
Summary of the Invention
[0004] One embodiment includes an apparatus for processing a substrate, the apparatus including a processing chamber comprising an outer chamber and a reactor having an inlet and an outlet, the reactor being located within the outer chamber, a plasma generator configured to supply plasma to the reactor, and a substrate support, wherein during processing, gaseous species pass from the reactor through the outlet into the outer chamber, the flow conductance from the reactor into the outer chamber is changeable and controllable during processing, and when the apparatus is in a low flow conductance state, the flow conductance from the reactor into the outer chamber is about 0.2 sccm / mTorr or less.
[0005] In some embodiments, the device further includes a movable pressure control ring located near the outlet to the reactor, which is adjustable to change the flow conductance from the reactor into the outer chamber.
[0006] In some embodiments, the apparatus further includes a movable wall within the reactor, which is adjustable to change the fluid conductance from the reactor to the outer chamber.
[0007] In some embodiments, the substrate support is configured to be adjustable to change the flow conductance from the reactor to the outer chamber.
[0008] In various embodiments, when the apparatus is in a high-flow-conductance state, the flow-conductance from the reactor into the outer chamber is approximately 1 sccm / mTorr or greater. In some embodiments, the apparatus also includes a controller configured to switch the apparatus between a low-conductance state and a high-conductance state while processing substrates.
[0009] Another embodiment includes an apparatus for processing a substrate, the apparatus including a processing chamber comprising an outer chamber and a reactor having an inlet and an outlet, the reactor being located within the outer chamber, a plasma generator configured to supply plasma to the reactor and the outer chamber, and a substrate support, thereby allowing gaseous species to pass from the reactor through the outlet into the outer chamber during processing.
[0010] In some embodiments, the plasma generator is configured to provide direct plasma to the reactor, and the direct plasma is not confined to the reactor.
[0011] In some embodiments, the plasma generator is configured to generate remote plasma that is supplied to an outer chamber.
[0012] Another embodiment includes an apparatus for processing a substrate, the apparatus including a processing chamber, a substrate support, a bypass path having a flow conductance of about 1 sccm / mTorr or more, a showerhead including (i) a plurality of orifices for supplying gas to the processing chamber, and (ii) a bypass outlet for supplying gas to the bypass path, and a gas injection path configured to supply gas to the showerhead.
[0013] Another embodiment includes an apparatus for processing a substrate, the apparatus comprising: a processing chamber; a substrate support; a first inlet to the processing chamber for supplying at least a purge gas and a deposition gas phase to the processing chamber; an optional second inlet to the processing chamber, thereby supplying an etching gas to the processing chamber via the first inlet or the optional second inlet; a gas injection path configured to alternately supply at least a purge gas and a deposition gas phase to the first inlet; a purge gas supply path configured to supply a purge gas to the gas injection path; a deposition gas phase supply path configured to supply a deposition gas phase to the gas injection path; an etching gas supply path configured to supply an etching gas to the gas injection path or the optional second inlet; a bypass path fluidically coupled to the purge gas supply path and the deposition gas phase supply path via a valve, the bypass path not supplying gas to the processing chamber; and a controller configured to alternately flow the purge gas and the deposition gas phase into the processing chamber via the gas injection path, and to alternately flow the purge gas and the deposition gas phase into the bypass path.
[0014] Another embodiment includes an apparatus for processing a substrate, the apparatus including a processing chamber, a plasma generator configured to provide plasma to the processing chamber, a substrate support, a first inlet to the processing chamber configured to provide a deposition gas phase to the processing chamber, a second inlet to the processing chamber configured to provide an etching gas to the processing chamber, thereby preventing the deposition gas phase and the etching gas from mixing with each other before passing through the processing chamber, and an outlet to the processing chamber.
[0015] In any of the embodiments described above, the apparatus may also include a controller configured to cause any of the methods described herein.
[0016] These and other embodiments are described further below with reference to the drawings. [Brief explanation of the drawing]
[0017] [Figure 1] Figure 1 shows a flowchart related to a method for etching a substrate according to various embodiments of the present specification.
[0018] [Figure 2] Figure 2 shows a combined etching / deposition reactor that shows various problems that can occur.
[0019] [Figure 3] Figure 3 shows a combined etching / deposition reactor that uses a shared injection path for the deposition gas phase and the etching gas.
[0020] [Figure 4] Figure 4 shows a combined etching / deposition reactor that has separate injection paths for the deposition gas phase and the etching gas.
[0021] [Figure 5] Figure 5 shows a combined etching / deposition reactor that includes a bypass path that enables a high-flow purge.
[0022] [Figure 6A] Figure 6A shows a combined etching / deposition reactor that has a bypass path that is alternately used by the deposition gas phase and the purge gas. [Figure 6B] Figure 6B shows a combined etching / deposition reactor that has a bypass path that is alternately used by the deposition gas phase and the purge gas.
[0023] [Figure 7] Figure 7 shows a combined etching / deposition reactor that provides a controllable flow conductance using a pressure control ring.
[0024] [Figure 8] Figure 8 shows a combined etching / deposition reactor that provides a controllable flow conductance using a movable wall.
[0025] [Figure 9] Figure 9 shows a coupled etching / deposit reactor that provides controllable fluid conductance using an adjustable reactor gap.
[0026] [Figure 10] Figure 10 shows a coupled etching / deposit reactor with a movable lower reactor assembly that enables the formation of an unconfined plasma.
[0027] [Figure 11] Figure 11 shows a coupled etching / deposition reactor including a remote plasma source. [Modes for carrying out the invention]
[0028] The following description includes numerous specific details to provide a complete understanding of these embodiments. Embodiments of this disclosure may be carried out without some or all of these specific details. In other examples, well-known process behaviors are not described in detail so as not to unnecessarily obscure the embodiments of this disclosure. Embodiments of this disclosure are described in relation to specific embodiments. However, it will be understood that there is no intention to limit the embodiments of this disclosure.
[0029] The fabrication of various semiconductor devices involves etching features into a dielectric material using a plasma-based etching process. Often, the dielectric material is supplied as a stack of materials, which may include alternating layers of materials. For example, the stack may include any combination of silicon oxide, silicon nitride, and / or polysilicon. Additional layers may be present as desired for a particular application.
[0030] One technique for forming high aspect ratio features involves incorporating one or more deposition steps into an etching process. The deposition steps may be gas-phase based deposition steps, including supplying a deposition gas phase to a reactor. The film deposited by the deposition steps can facilitate passivation or etching at desired locations on the substrate. For example, the deposited film can passivate the upper sidewalls of a partially etched feature, thereby allowing etching at the bottom of the feature without etching the upper sidewalls laterally. The deposition steps provide good control with respect to step coverage, thickness, and selectivity for different substrates.
[0031] In the embodiments described herein, both the etching and deposition processes are performed in the same processing chamber. This eliminates the need to transport the substrate between separate etching and deposition chambers while features are being formed. The efficiency improvements achieved by avoiding substrate transport are particularly relevant when the deposition and etching processes are repeated several times during the etching process.
[0032] The use of coupled etching / deposit reactors can offer various advantages, such as reduced processing time and increased throughput. However, there are several engineering considerations that arise when coupling etching / deposit equipment. To realize the benefits of coupled etching / deposit reactors in packages that are practical for industrial microelectronics processing, embodiments herein address several potential conflicts between (1) reactor designs optimized for plasma etching and (2) reactor designs optimized for vapor-phase based deposition. Generally, plasma etching processes are typically performed at low pressure and high conductance (or variable conductance including high conductance), deposition dosing processes are typically performed at high pressure and low conductance, and purging processes are typically performed at high pressure and high conductance.
[0033] Embodiments herein present several innovations that enable a production-worthy process combining plasma etching and gas-phase based deposition in a single reactor. These innovations generally fall into the categories of (a) injection of deposition gas and etching gas into the processing chamber, (b) control of variable gas conductance over a wide range of conductances, (c) pumping and purging capabilities over a wide range of pump flow rates, and (d) control of unwanted deposit accumulation in the processing chamber. These innovations may be combined as desired for specific applications. Specific embodiments are described further below.
[0034] As used herein, the term “gas phase” is intended to refer to a gaseous species supplied to the processing chamber without the use of plasma. The term “deposited gaseous phase” is intended to refer to a gaseous reactant supplied to the processing chamber without the use of plasma during the deposition operation. Similarly, the term “gas-phase based deposition” is intended to refer to deposition that involves supplying a deposition gaseous phase to the processing chamber without the simultaneous use of plasma. Exemplary gas-phase based deposition schemes include, for example, molecular layer deposition, self-assembled monolayer deposition, thermally driven atomic layer deposition, and plasma-driven atomic layer deposition that involves supplying a deposition gaseous phase without exposure to plasma (e.g., in such cases, plasma is used to accelerate the reaction after the supply of the deposition gaseous phase has been stopped). The gaseous species used herein are typically based on chemicals with relatively low vapor pressures, making them impractical for use in conventional plasma etching gas supply systems including thermal mass flow controllers. Such chemicals are typically in liquid or solid form under ambient conditions. Therefore, unwanted condensation of the gaseous phase is a common problem. In contrast, the term “gas” is more generally used and may refer to a species supplied to the processing chamber with or without plasma. The term "etching gas" is intended to refer to the reactants supplied to the processing chamber during the etching operation. In most cases, the etching gas is supplied to the chamber while plasma is present. Commonly used etching gases typically have a vapor pressure high enough to allow the use of conventional thermal mass flow controllers.
[0035] As used herein, the term "low pressure" is intended to mean a pressure of approximately 800 mTorr or less unless otherwise specified. The term "high pressure" is intended to mean a pressure of approximately 1 Torr or more unless otherwise specified. The term "low conductance" is intended to mean a conductance of approximately 0.05 sccm / mTorr or less unless otherwise specified. The term "high conductance" is intended to mean a conductance of approximately 1 sccm / mTorr or more unless otherwise specified. I. Process Flow
[0036] Figure 1 shows a flowchart of a method for etching concave features according to various embodiments of this specification. The method in Figure 1 begins with operation 101, in which a substrate is received in a processing chamber. The substrate has a stack of material on it, the stack of which includes a dielectric material. The dielectric material may be silicon oxide and / or silicon nitride. Additional layers of material may be provided as desired for specific applications. Examples of material stacks are described further below. A patterned mask layer is provided on top of the dielectric material. The pattern of the mask layer defines the locations where features should be formed on the stack.
[0037] Next, in operation 103, etching gas is introduced into the processing chamber to generate plasma from the etching gas. The substrate is exposed to the plasma to partially etch features into the stack. Next, in operation 105, the processing chamber is optionally purged to remove excess etching gas and / or etching byproducts. The purging step helps reduce unwanted reactions between the etching gas and the deposited gas phase later introduced during processing. Purging may include supplying a purge gas and / or discharging the processing chamber. In various cases, the result of purging operation 105 may also be purging some or all of the supply lines used to supply the etching gas to the processing chamber, including any supply lines shared between the etching gas and the deposited gas phase.
[0038] In operation 107, the deposition gas phase is flowed into the processing chamber to deposit a film on the sidewalls of the partially etched features. Depending on the deposition mechanism, additional reactants may or may not be provided. For example, if the film is deposited as a self-assembled monolayer, additional reactants are not required. On the other hand, if the film is deposited by molecular layer deposition or atomic layer deposition, for example, the deposition gas phase and additional reactants may be provided to the processing chamber in a periodic manner. In some cases, the deposition is conformal. The film may or may not extend along the entire length of the sidewall. In some cases, the film is concentrated near the top of the sidewall, but is significantly thinner or absent near the bottom of the sidewall.
[0039] In operation 109, the process continues with another optional purge of the processing chamber to remove excess deposited reactants (e.g., the deposited gas phase and any additional reactants) and byproducts. In various cases, the result of the purge operation 109 may also be the purging of some or all of the supply lines used to supply the deposited gas phase to the processing chamber, including any supply lines shared between the etching gas and the deposited gas phase.
[0040] In operation 111, it is determined whether the features are close to their final target structure. If the features are close to the final target structure, the method continues in operation 113, flowing etching gas into the processing chamber, generating plasma from the etching gas, and finally etching the features. At this point, the method is complete. If it is determined in operation 111 that the features are not close to the final target structure, the method repeats from operation 103, performing another partial etching step. The operation in Figure 1 is repeated until the features reach their final target structure. II. Potential Risks and Focus
[0041] Figure 2 shows an apparatus used for both etching and deposition, illustrating some of the problems that can arise when these processes are combined on a single apparatus. The illustrated apparatus has a design that confines the etching plasma to an internal region of a vacuum chamber. This internal region is called the “reactor.” During processing, the substrate is placed on a substrate support and exposed to the conditions of the reactor. For example, during etching, the substrate is exposed to the etching plasma confined within the reactor. The portion outside the vacuum chamber is not exposed to the plasma and is called the “outer chamber.” This design is commonly used in capacitively coupled dielectric etching systems, such as Lam Research’s Flex® product family. For illustrative purposes, this configuration is assumed below. However, the techniques disclosed herein are not limited to this particular apparatus configuration. Such techniques may be applied to other apparatus configurations for plasma etching.
[0042] In the embodiment shown in Figure 2, the deposition gas phase and etching gas are selectively supplied to the processing chamber through a shared supply line. One potential problem is unwanted condensation of the deposition gas phase. The condensed deposition gas phase 210 may form liquid residue 220, for example, on the supply line and / or the plenum behind the showerhead. This condensation can occur because temporal and spatial fluctuations in the gas phase temperature and pressure can create conditions where the liquid state is more favorable than the gas state. This liquid residue 220 may hinder the efficient purging of the gas phase supply path. In some cases, the liquid residue 220 may form aerosolized droplets, which could lead to the formation of unwanted particles 230 that deposit on the substrate surface.
[0043] Another problem that may arise during processing is the formation of unwanted material on the surfaces of the processing apparatus (e.g., the reactor surface, the processing chamber surface, the supply line, the showerhead, etc.). Often, this unwanted material arises from the reaction between the etching gas and the deposition gas phase. For example, unwanted deposits 240 may form in the shared supply line that provides both the etching gas and the deposition gas phase to the processing chamber. Similarly, unwanted deposits 250 may form on the plenum on the back of the showerhead and / or in the holes of the showerhead (not shown). Unwanted deposits 240 and 250 are particularly likely to form in areas where both liquid residue 220 and etching gas are present, for example, on hardware shared by the deposition gas phase / etching gas. The deposition gas phase and etching gas are not actively introduced simultaneously. However, residual amounts of the gas phase or gas remain in the supply path in a gaseous and / or adsorbed or condensed state on the surface, which can lead to unwanted cross-reactions. In certain embodiments, unwanted deposits 240 and 250 may arise from a reaction between HBr (e.g., flowing into the reactor as an etching gas) and residues of the diamine deposition gas phase used in a preceding molecular layer deposition process.
[0044] Unwanted deposits 260 may also occur on the walls of the outer chamber. Unwanted deposits 260 may also be residues resulting from unwanted side reactions, such as (1) a reaction between the deposition gas phase and the etching gas, (2) a reaction between the deposition gas phase and a byproduct of the etching process / etching gas plasma, or (3) a reaction between the deposition gas phase and a byproduct of the deposition reaction. In some cases, the unwanted deposits 260 may be polymers, such as polymers resulting from molecular layer deposition reactions.
[0045] Based on the configuration of the confined plasma, conventional etching reactors used solely for etching operations typically produce little to no deposits on the outer chamber walls. Therefore, conventional etching equipment has no need or reason to include a mechanism for removing such deposits from the outer chamber walls. Instead, such reactors often feature plasma generators that can be used for automatic cleaning of the reactor surface. These automatic cleaning processes do not reach the outer chamber and therefore do not act to remove unwanted deposits in this area.
[0046] Another issue to address when performing both etching and deposition in the same reactor is optimizing the fluid conductance through the reactor for each process. For example, etching is typically performed over a tunable medium to high conductance range (e.g., between approximately 1 and 50 sccm / mTorr). Often, plasma etching is performed at relatively high conductance, while automated plasma cleaning of the reactor is performed at medium conductance. In contrast, deposition is typically performed at relatively low conductance (e.g., between approximately 0.001 and 0.03 sccm / mTorr), allowing for both high pressure and high doses in the reactor, as well as both low pressure and low doses in the outer chamber. The low conductance during deposition reduces the dose time in the reactor, allowing for more efficient use of the deposition gas phase. Additionally, the smaller dose in the outer chamber minimizes unwanted deposits in the outer chamber.
[0047] Thus, when both etching and deposition are performed in the same reactor, it is beneficial to ensure that the conductance through the reactor is variable and controllable over a wide range. This variable conductance is indicated by a series of downward arrows from the reactor to the outer chamber. When using variable conductance, it is also beneficial to ensure that the conductance can be changed quickly to maximize throughput. III. Etching
[0048] In general, embodiments of this specification should not be limited to specific etchant species or etching conditions, and the etching process may be carried out using conventional processing conditions. Exemplary processing conditions are described in U.S. Patents 9,384,998, 9,887,097, and 9,997,373, each of which is incorporated herein by reference in its entirety.
[0049] In some embodiments, the pressure during etching may be between approximately 10 and 200 mTorr (e.g., for capacitively coupled plasmas) or between approximately 1 and 120 mTorr (e.g., for inductively coupled plasmas). The exemplary flow rate of the etching gas may be between approximately 100 and 3000 sccm. A turbomechanical pump may be used to remove excess etching gas and etching byproducts from the processing chamber during etching, and the maximum turbomechanical pump flow rate is typically around 3000 sccm.
[0050] In many cases, etching involves generating a plasma from an etching gas and exposing the substrate to the plasma. The etching gas may include, for example, a chlorine source, a bromine source, a carbon source, a fluorine source, an oxygen source, and / or a hydrogen source. In various embodiments, various combinations of etching gases may be used. Exemplary gases that may be provided as etching gases include chlorine gas (Cl2), hydrogen chloride (HCl), carbonyl sulfide (COS), fluorocarbon (CxFy), and hydrofluorocarbon (C x H y F z ), chlorocarbon (C x Cl y ), hydrochlorocarbon (C x H y Cl z Examples of etching gases include, but are not limited to, nitrogen trifluoride (NF3), hydrogen bromide (HBr), trifluoroimethane (CF3I), oxygen (O2), and hydrogen (H2). The etching gas may also contain one or more inert gases.
[0051] To facilitate high-quality etching results, the etching / deposit reactor may be provided with specific features. These features may include any combination of (1) multi-zone gas injection to facilitate control of process uniformity, (2) showerhead gas injection for uniform gas supply, (3) corrosion-resistant gas line materials such as nickel-chromium-molybdenum alloy, and / or (4) controlled variable gas conductance (e.g., including both low and high conductance). Further details are provided in the following embodiments. IV. Deposition
[0052] Depending on the various embodiments, several different gas-phase-based deposition mechanisms may be used. In some cases, molecular layer deposition is used. In some cases, self-assembled monolayer deposition is used. In some cases, atomic layer deposition is used. When atomic layer deposition is used, the reaction may be thermally driven or plasma driven. If the reaction of atomic layer deposition is plasma driven, there is at least one step that includes supplying the deposited gas phase to the processing chamber without simultaneously generating plasma. Other gas-phase-based deposition mechanisms may be used as appropriate for specific applications.
[0053] The embodiments herein are not limited by any particular deposition gas phase or deposition conditions. The deposition process may be carried out using conventional deposition conditions. Often, the deposition process is designed to deposit a thin film having a known and controlled composition on a substrate, for example, on the sidewalls of a partially etched feature. Gas-phase based deposition processes are typically carried out at pressures between about 1 and 40 Torr. Relatively high deposition pressures result in high fluidity of the species reaching the substrate surface, thus relatively shortening the processing time. Conventional deposition reactors are typically capable of providing flow rates of 5 SLM or more at high pressure (e.g., above 2 Torr) to allow for rapid and effective purging. Purging is particularly beneficial when chemical exchanges are circulated amongst themselves, for example, to prevent unwanted reactions between the residual gas phase and subsequent reactants.
[0054] To facilitate high-quality deposition results, the etching / deposition reactor may be provided with several features. These features may include any combination of: (1) efficient high-pressure / high-flow purging with minimal dead legs in the gas phase path; (2) point-of-use valves that allow for rapid purging without dead legs; (3) heated point-of-use valves designed to minimize the risk of gas phase condensation in steady state and during switching; (4) controlled and progressively increasing wall temperatures along the deposition gas phase supply path from the deposition gas phase source to the processing chamber; (5) designs that avoid condensation by preventing rapid expansion of the gas phase, for example, by preventing it from flowing through small orifices; and (6) heated chamber walls that reduce unwanted deposits on these surfaces. When heated components are used, the temperature may be selected to reduce adsorption of the deposition gas phase or other reactants. On the other hand, when using organic reactants, for example, unwanted decomposition that may occur at temperatures above approximately 250°C may be avoided. These features may be combined with those listed above to facilitate high-quality etching results. Further details are provided in the following embodiments. V. Examples
[0055] Figures 3 to 11 illustrate several embodiments in accordance with the embodiments described herein. Various features will be described in relation to these embodiments. Features may be described in relation to specific embodiments. However, it will be understood that features may be combined as desired for specific applications. A. Co-injection of sediment gas phase and etching gas
[0056] Figure 3 shows a coupled etching / deposit reactor according to various embodiments. In this embodiment, there is an injection path 330 used to alternately supply the deposition gas phase and the etching gas. The deposition gas phase is generated from a gas phase source 350, and the etching gas is generated from an etching gas source 360. For ease of illustration, the gas phase source 350 and the etching gas source 360 are omitted from the rest of the figure. However, it is understood that the gas phase source 350 and the etching gas source 360 are included. Similarly, Figure 3 shows a plasma generator 370, which is omitted from the rest of the figure. However, it is understood that the plasma generator 370 is included. The plasma generator 370 may be configured to provide capacitively coupled plasma to the reactor. Other types of plasma may be provided in particular cases. Valve 310 controls the supply of the deposition gas phase, and valve 320 controls the supply of the etching gas. Valves 310 and 320 may be point-of-use valves. Exemplary valve structures are described in U.S. Patent Publication No. 2013 / 0333768, filed September 25, 2012, and U.S. Patent Publication No. 2019 / 0323125, filed April 18, 2018, each incorporated in its entirety by reference. The valve structures described in these publications enable rapid purging of the supply system without dead legs. In general, any of the valves described herein may be point-of-use valves.
[0057] In the embodiment shown in Figure 3, both the deposition gas phase and the etching gas are selectively injected into the reactor of the processing chamber via a single shared showerhead 340. Various alternatives are available. For example, the deposition gas phase may be supplied separately by a different supply system such as a gas ring, one or more nozzles, or a dual showerhead having separate supply paths for the deposition gas phase and the etching gas.
[0058] Furthermore, a controller 380 is shown in Figure 3. The controller 380 may be used to control the apparatus that causes the methods and operations described herein. The controller 380 is omitted from the remaining figures; however, it is understood that such a controller is typically present. The controller will be discussed further below.
[0059] One advantage of the embodiment shown in Figure 3 is its simplicity. Since only a single showerhead is used, the hardware cost is relatively low. Another advantage of the embodiment in Figure 3 is that, since both types are supplied via the showerhead, it provides the substrate with a highly uniform flow of both the deposition gas phase and the etching gas. This promotes a high degree of process uniformity. In the embodiment shown in Figure 3, there is a risk of unwanted side reactions occurring between the flowing deposition gas phase and the etching gas residue, or between the flowing etching gas and the deposition gas phase residue. To minimize these unwanted side reactions, relatively more substantial purging conditions, such as very long purging times longer than 5 seconds, may be used. B. Separate injection of the deposit gas phase and etching gas.
[0060] Figure 4 shows a coupled etching / deposit reactor according to various embodiments. In this embodiment, separate supply lines are provided to supply the deposition gas phase and etching gas to the reactor. The deposition gas phase supply path 410410 supplies the deposition gas phase to the plenum and gas ring 420420, while the etching gas supply path 430 supplies the etching gas to the plenum and showerhead 440440.
[0061] One advantage of the embodiment in Figure 4 is that the deposited gas phase and etching gas do not come into contact with each other before being supplied to the reactor, thereby minimizing the risk of unwanted side reactions occurring between the flowing deposited gas phase and the etching gas residue, and between the flowing etching gas and the deposited gas phase residue. The embodiment in Figure 4 may provide a less uniform flow of the deposited gas phase on the substrate compared to the embodiment in Figure 3, where the deposited gas phase is supplied via a showerhead. However, since the deposition mechanism is usually dependent on monolayer adsorption or otherwise self-limiting, even the less uniform flow provided in Figure 4 may be sufficient to provide high-quality deposition results.
[0062] In another embodiment similar to Figure 4, a dual showerhead may be provided. The dual showerhead provides separate, isolated paths for supplying the deposition gas phase and the etching gas. The deposition gas phase supply path 410 and the etching gas supply path 430 can each be supplied into separate ports of the dual showerhead, ensuring that the deposition gas phase and the etching gas remain physically separated until they reach the reactor. In another embodiment similar to Figure 4, the deposition gas phase may be injected into the reactor from the side of the reactor (rather than from the top, as shown in Figure 4). C. Bypass Purge Route
[0063] Figure 5 shows a coupled etching / deposit reactor according to various embodiments. In the embodiment of Figure 5, the deposition gas phase and etching gas are supplied to the reactor via a showerhead 530. The gas phase supply path 510 and the etching gas supply path 520 supply the deposition gas phase and etching gas into a single injection path that enters the showerhead 530. The purge gas is similarly supplied to the reactor via the showerhead 530 after passing through the deposition gas phase supply path 510 and an injection path shared by the deposition gas phase and the etching gas. In this embodiment, the showerhead 530 includes (1) several small orifices for supplying the etching gas, deposition gas phase, and purge gas to the reactor, and (2) two types of outlets, including a bypass outlet 540 for relatively fast removal of gas (e.g., purge gas) from the showerhead 530. The bypass outlet supplies a bypass path 550 connected to a large-capacity pump 560. The bypass path 550 is a high-conductance path (e.g., greater than 1 sccm / mTorr). The high-capacity pump 560 may support flow rates exceeding, for example, 3000 sccm. The valve 540 controls the flow through the bypass path 550.
[0064] If the bypass path 550 is not present, the showerhead 530 limits the maximum achievable flow rate of purge gas into the reactor. This limitation arises from the configuration of the showerhead 530, which has a small array of orifices resulting in relatively low conductance. In contrast, if the bypass path 550 and the large-capacity pump 560 are present, the purge gas can flow at very high speeds, limited only by the conductance of the bypass path 550 and the pumping capacity of the large-capacity pump 560.
[0065] Because the purge gas can flow at high speed, unwanted residues (e.g., from the deposition gas phase or etching gas) can be removed more efficiently. This can reduce purge time and improve throughput. The purge time that can be reduced includes purging between process steps based on the deposition gas phase and etching gas, as well as purging between process steps based on various deposition gas phases and / or additional reactants during deposition (e.g., when periodic deposition methods such as molecular layer deposition or atomic layer deposition are used). The embodiment in Figure 5, which includes valve 540, bypass path 550, and high-capacity pump 560, may add cost, power consumption, and complexity to the system. D. Bypass to minimize pressure loss
[0066] Figures 6A and 6B show coupled etching / deposit reactors according to various embodiments. In this embodiment, there is a bypass path 660 that is alternately shared between the deposition gas phase (supplied via the deposition gas phase supply path 610) and the purge gas (supplied via the purge gas supply path 620). For example, Figure 6A shows a valve configuration 630 that allows the deposition gas phase to flow through the bypass path 660 while the purge gas is supplied to the processing chamber. In contrast, Figure 6B shows a valve configuration 680 that allows the purge gas to flow through the bypass path 660 while the deposition gas phase is supplied to the processing chamber.
[0067] Pump 670 drives the flow along the bypass path 660. Pump 670 may be a high-capacity pump, as described in relation to Figure 5, or a turbomechanical pump. Similarly, the bypass path 660 may be a high-conductance path, as described in relation to Figure 5, or it may have lower conductance. A flow restrictor 650 may be provided in the bypass path 660. The flow restrictor 650 may be, for example, a fixed-size orifice or an adjustable needle valve. The flow restrictor 650 may be configured to change / control the flow conductance in the bypass path 660 so that the flow conductance in the bypass path 660 matches the flow conductance in the injection path 640, which alternately supplies the deposited gas phase / purge gas to the reactor in the processing chamber. The bypass path 660 allows the flow of the deposited gas phase and purge gas to be established / stabilized before being directed to the reactor in the processing chamber. This configuration minimizes local pressure fluctuations near valve 630 or 680 during the switch between the purge gas and the sediment gas phase. This prevents unwanted condensation of the sediment gas phase during the switch.
[0068] One advantage of the embodiments in Figures 6A and 6B is that the shared bypass path 660, with its controlled conductance and associated valve, minimizes local pressure fluctuations near valve 630 or 680 during the switching between the purge gas and the deposited gas phase. This reduces the risk of unwanted condensation of the deposited gas phase during the switching. With a lower risk of condensation, there is a lower possibility of unwanted side reactions occurring and generating unwanted particles on the substrate or reactor surface, as described in relation to Figure 2. The embodiments in Figures 6A and 6B, including the bypass path 660, the flow restrictor 650, and the pump 670, may add cost and complexity to the system. E. Pressure control ring for variable conductance
[0069] Figure 7 shows a coupled etching / deposit reactor according to various embodiments. This embodiment shows one mechanism that provides variable flow conductance 750 from the reactor to the outer chamber. The reactor is defined at least partially by a confinement shroud 710. A gaseous species passes from the reactor through an outlet 720 to the outer chamber. The outlet 720 may be formed as a slotted or otherwise perforated portion of the confinement shroud 710, as shown.
[0070] In Figure 7, the pressure control ring 730 is positioned close to the outlet 720. The height of the pressure control ring 730 is adjustable to provide a wide range of fluid conductance from the reactor to the outer chamber. For example, when the pressure control ring 730 is in an upper position (relatively close to the outlet 720), the flow from the reactor into the outer chamber is more restricted, resulting in lower fluid conductance. In contrast, when the pressure control ring 730 is in a lower position (relatively far from the outlet 720), the flow from the reactor into the outer chamber is less restricted, resulting in higher fluid conductance.
[0071] In this embodiment of the coupled etching / deposit reactor, when the pressure control ring 730 is positioned in an upper position, an elastomer seal 740 may be provided, for example, above the upper surface of the pressure control ring 730 (as shown in Figure 7) or below the lower surface of the reactor, to further reduce the flow conductance. The elastomer seal 740 may engage to block or substantially restrict the flow from the reactor to the outer chamber, resulting in a very low conductance state. This very low conductance state is particularly useful during gas phase deposition, for example, during the dose process in which the deposited gas phase is supplied to the reactor and adsorbed onto the substrate surface.
[0072] In various embodiments in which a pressure control ring is used, the conductance from the reactor to the outer chamber is adjustable over a wide range. For example, in some cases, the conductance may be adjusted to a low value of about 0.01 sccm / mTorr when the pressure control ring 730 is at its highest position, or to a high value of about 50 sccm / mTorr when the pressure control ring 730 is at its lowest position. During processing, the pressure control ring 730 may be positioned at a relatively high position (e.g., at the highest position) during certain deposition steps, for example, when a gas phase precursor is being introduced into the reactor. In contrast, the pressure control ring 730 may be positioned at a relatively low position (e.g., at the lowest position) during other processing steps such as etching and / or purging steps.
[0073] One advantage of the embodiment in Figure 7 is that the pressure control ring 730 allows for broad control of the fluid conductance from the reactor to the outer chamber. This makes it possible to perform the etching and deposition processes under substantially different processing conditions. Furthermore, very different conditions can be established simultaneously in the reactor and the outer chamber. For example, during the vapor deposition process, the pressure in the reactor may be significantly higher than the pressure in the outer chamber. In certain embodiments, the pressure in the reactor may be high, as described above, while the pressure in the outer chamber may be less than 20 mTorr. This configuration allows for efficient introduction of the deposited vapor phase onto the substrate and reduces the risk of unwanted deposition in the outer chamber by significantly reducing the dose amount in the outer chamber. Another advantage of the embodiment in Figure 7 is that by rapidly moving the pressure control ring 730, a fast transition from the dose process (low conductance is desirable) to the purge process (high conductance is desirable), or vice versa, is possible. In the embodiment shown in Figure 7, the entire reactor may be exposed to the chemicals of the vapor deposition process. F. Movable wall for variable conductance
[0074] Figure 8 shows a coupled etching / deposit reactor according to various embodiments. This embodiment illustrates another mechanism that provides variable flow conductance from the reactor to the outer chamber. The reactor is defined, at least partially, by a containment shroud 810. A movable wall or partition 840 divides the reactor into an internal reactor region (labeled "internal reactor" in Figure 8) and a peripheral reactor region (labeled "830" in Figure 8). The internal reactor region is radially inward of the movable wall 840, while the peripheral reactor region 830 is between the internal reactor region and the outer chamber. During processing, gaseous species pass from the internal reactor region, under the movable wall 840, through the peripheral reactor region 830, and through the outlet 820 into the outer chamber. In this embodiment, the outlet 820 is provided as a slotted or otherwise perforated portion of the containment shroud 810.
[0075] Notably, the movable wall 840 is movable up and down as desired. The movable wall 840 extends in a ring shape around the showerhead and substrate. In this embodiment, the lower part of the movable wall 840 engages with the upper surface of the substrate support 860 when the movable wall 840 is at its lowest position. In an alternative embodiment, the lower part of the movable wall 840 may engage with a portion of the containment shroud 810, for example, at a position radially inward of the outlet 820. When the movable wall 840 is relatively low, the flow from the internal reactor region to the peripheral reactor region is more restricted, and the associated flow conductance is lower. When the movable wall 840 is raised, part or all of the movable wall 840 retracts into the pocket 850, thereby removing / reducing the flow restriction and providing relatively high conductance.
[0076] In some embodiments, an elastomer seal (not shown) may be provided between the lower part of the movable wall 840 and the surface with which the movable wall 840 engages when it is in its lowest position. For example, such a seal may be provided below the lower surface of the movable wall 840, above the upper surface of the substrate support, or above the upper surface of the containment shroud 810. Similarly, in some embodiments, an elastomer seal (not shown) may be provided between the upper part of the movable wall 840 and the surface on the containment shroud 810 or pocket 850 with which the movable wall 840 engages when it is in its lowest position.
[0077] In various embodiments in which the movable wall 840 is used, the conductance from the reactor to the outer chamber is adjustable over a wide range. For example, in some cases, the conductance may be adjusted to a low value of about 0.01 sccm / mTorr when the movable wall 840 is at its lowest position, and to a high value of about 50 sccm / mTorr when the movable wall 840 is at its highest position. During processing, the movable wall 840 may be positioned at a relatively low position (e.g., lowest position) during certain deposition steps, for example, when a gas phase precursor is being introduced into the internal reactor region. In contrast, the movable wall 840 may be positioned at a relatively high position (e.g., highest position) during other processing steps, such as etching and / or purging steps.
[0078] One advantage of the embodiment in Figure 8 is that, similar to the embodiment in Figure 7, it provides broad control over fluid conductance. Furthermore, the embodiment in Figure 8 allows for the vapor deposition and etching processes to be carried out under substantially different processing conditions. Moreover, the embodiment in Figure 8 allows for the simultaneous establishment of very different processing conditions in the internal reactor region, the peripheral reactor region 830, and the outer chamber. Another advantage of this embodiment is that, because the internal reactor region is exposed to the vapor deposition process / chemicals, and the dose is very small in the peripheral reactor region and outer chamber, the risk of unwanted deposits forming in these regions is reduced. Consequently, this reduces the total amount of deposited vapor phase required to doze the substrate. Furthermore, when the movable wall 840 is at its lowest position, it effectively reduces the associated processing volume surrounding the substrate, thus reducing the dosing time and the duration of the purging process. Dosing time is the time required to reach the target pressure during the dosing process. Thus, a shorter dosing time correlates with a shorter dose duration for a given target dose. In the embodiment shown in Figure 8, it may take a relatively long time (for example, up to several seconds) to change the position of the movable wall 840 as desired between processes. G. Adjustable reactor gap for variable conductance
[0079] Figure 9 shows a coupled etching / deposit reactor according to various embodiments. This example illustrates another mechanism that provides variable flow conductance from the internal reactor region to the outer chamber. As described above, the reactor is defined at least partially by the confinement shroud 910. The upper reactor lip 940 and the lower reactor lip 950 divide the reactor into an internal reactor region (labeled "internal reactor" in Figure 9) and a peripheral reactor region (labeled "930" in Figure 9). The internal reactor region is radially inward of the upper reactor lip 940 and the lower reactor lip 950, while the peripheral reactor region is between the internal reactor region and the outer chamber. During processing, gaseous species pass from the internal reactor region, through the space between the upper reactor lip 940 and the lower reactor lip 950, into the peripheral reactor region 930, and through the outlet 920 into the outer chamber. In this embodiment, the outlet 920 is provided as a slotted or otherwise perforated portion of the containment shroud 910.
[0080] In this embodiment, the lower reactor assembly 960 has an adjustable height. This means that the height of the gap between the lower reactor assembly 960 and the showerhead is adjustable. The lower reactor assembly 960 includes at least a substrate support and a lower reactor lip 950. When the lower reactor assembly 960 is in a relatively low position, there is less restriction on flow from the internal reactor region to the peripheral reactor region and into the outer chamber, thereby providing relatively high fluid conductance. In contrast, when the lower reactor assembly 960 is in a relatively high position, the upper reactor lip 940 and the lower reactor lip 950 are closer to each other, thereby restricting flow from the internal reactor region to the peripheral reactor region and into the outer chamber, providing relatively low fluid conductance.
[0081] In various cases, the upper reactor lip 940 and the lower reactor lip 950 may be in contact with each other, thereby sealing the internal reactor region. In some embodiments, for the same reasons as described in relation to Figure 7, an elastomer seal (not shown) may be provided between the upper reactor lip 940 and the lower reactor lip 950. The elastomer seal may be provided on either or both of the upper reactor lip 940 and the lower reactor lip 950.
[0082] As shown in Figure 9, in various embodiments in which the movable lower reactor assembly 960 is used in combination with the upper reactor lip 940 and the lower reactor lip 950, the conductance from the internal reactor region to the external chamber is adjustable over a wide range. For example, in some cases, the conductance may be adjusted to a low level of about 0.01 sccm / mTorr when the movable lower reactor assembly 960 is at its highest position, and to a high level of about 50 sccm / mTorr when the movable lower reactor assembly 960 is at its lowest position. During processing, the movable lower reactor assembly 960 may be positioned at a relatively high position (e.g., the highest position) during certain deposition steps, for example, when a gas phase precursor is being introduced into the internal reactor region. In contrast, the movable lower reactor assembly 960 may be positioned at a relatively low position (e.g., the lowest position) during other processing steps, such as etching and / or purging steps.
[0083] One advantage of the embodiment in Figure 9 is that, as with the embodiments in Figures 7 and 8, it provides a wide range of control over fluid conductance. Similar to those embodiments, the embodiment in Figure 9 allows etching and deposition operations to be performed under different processing conditions. Similarly, this embodiment allows for the simultaneous establishment of very different processing conditions in the internal reactor region, the peripheral reactor region, and the outer chamber. For example, the gas-phase deposition process can operate at a much higher pressure in the internal reactor region compared to the lower pressure simultaneously established in the peripheral reactor region and the outer chamber. This minimizes dosing in the peripheral reactor region and the outer chamber, reducing the risk of unwanted deposit formation in these regions. Another advantage of this embodiment is that a smaller volume of the internal reactor region (compared to the entire reactor) can be filled and purged more quickly. In this embodiment, positioning the lower reactor assembly 960 each time it is moved may take a relatively long time (e.g., up to several seconds). H. Cleaning of the outer chamber with unconfined plasma
[0084] Figure 10 shows a coupled etching / deposit reactor according to various embodiments. In this embodiment, the lower reactor assembly 1010 has an adjustable height. The lower reactor assembly 1010 includes at least a substrate support. Figure 10 shows the lower reactor assembly 1010 in a relatively low position (e.g., the lowest position). In contrast, when the reactor assembly 1010 is in a relatively high position (e.g., the highest position), it may be similar to the apparatus shown in Figure 3 (for example, considering the relative height of the reactor and the lower reactor assembly).
[0085] When the lower reactor assembly 1010 is in its relatively high position, any plasma generated in the reactor is confined within the reactor. Such confined plasma is useful for processing the substrate, for example, during etching operations. This positioning is also useful for vapor deposition processes. In contrast, when the lower reactor assembly 1010 is in its relatively low position, plasma generated in the reactor (e.g., from a plasma-cleaning gas such as O2) is no longer confined within this volume. Instead, the plasma persists in both the reactor and the outer chamber. For example, plasma 1020 may be present in the outer chamber. Therefore, the plasma can reach and clean unwanted residues from the surface (e.g., walls) of the outer chamber. Conventional etching reactors did not substantially generate unwanted deposits on the surface of the outer chamber, so there was no need or reason to provide a mechanism for cleaning these surfaces. In contrast, when both etching and deposition are performed on the same substrate in the same reactor, such unwanted deposits can become a problem. In these cases, it is beneficial to periodically or intermittently clean the surface of the outer chamber.
[0086] One advantage of the embodiment shown in Figure 10 is the control of residue accumulation in the outer chamber. In this embodiment, the components of the outer chamber (e.g., the walls and any other exposed components) are exposed to the plasma, so such components should preferably be manufactured from materials suitable for plasma exposure. I. Cleaning of the outer chamber using remote plasma
[0087] Figure 11 shows a coupled etching / deposition reactor according to various embodiments. In this embodiment, a remote plasma source 1110 generates plasma that is supplied to the outer chamber as remote plasma 1130. Valve 1120 may be used to control the supply of plasma to the outer chamber. Compared to the plasma generated in the embodiment of Figure 10, the remote plasma of Figure 11 provides relatively high-density reactive radicals for chamber cleaning. The remote plasma 1130 may also provide relatively low-density ions.
[0088] One advantage of the embodiment shown in Figure 11 is that the accumulation of residue in the outer chamber can be controlled using a remote plasma 1130. In this embodiment, remote plasma cleaning may be less efficient than direct unconfined plasma (as used, for example, in Figure 10). Furthermore, since the components of the outer chamber are exposed to remote plasma conditions, they preferably need to be manufactured from materials that are suitable for exposure to remote plasma. Also, the remote plasma source may add cost and complexity to the system. J. Controller
[0089] Any apparatus described herein may include a controller. In some embodiments, the controller may be part of a system and may be part of the embodiments described above. Such a system may include a semiconductor processing apparatus comprising one or more processing tools, one or more chambers, one or more processing platforms, and / or specific processing components (such as a wafer pedestal, a gas flow system, etc.). These systems may be integrated with electronics for controlling system operation before, during, and after processing of semiconductor wafers or substrates. The electronics may be referred to as a “controller” and may control various components or sub-parts of one or more systems. Depending on the processing requirements and / or the type of system, the controller may be programmed to control any of the processes disclosed herein. Such processes include supplying processing gases, setting temperature (e.g., heating and / or cooling), setting pressure, setting vacuum, setting power, setting radio frequency (RF) generator, setting RF matching circuitry, setting frequency, setting flow rate, setting fluid supply, setting position and operation, loading and unloading wafers into and out of tools, and loading and unloading wafers into and out of other transport tools and / or load locks connected to or interlocked with a particular system.
[0090] In a broad sense, a controller may be defined as an electronic device having various integrated circuits, logic, memory, and / or software that receive and issue instructions, control operations, enable cleaning operations, enable endpoint measurements, etc. Integrated circuits may include chips in the form of firmware that store program instructions, chips defined as digital signal processors (DSPs), application-specific integrated circuits (ASICs), and / or one or more microprocessors, or microcontrollers that execute program instructions (e.g., software). Program instructions are instructions communicated to the controller in the form of various individual settings (or program files) that may define operational parameters for performing a particular process on or for a semiconductor wafer or for a system. In some embodiments, operational parameters are part of a recipe defined by a process engineer that may achieve one or more processing steps during the manufacturing of one or more layers, materials, metals, oxides, silicon, silicon dioxide, surfaces, circuits, and / or wafer dies.
[0091] In some embodiments, the controller may be integrated with the system, coupled to it, networked to the system, or a combination of both, or coupled to it as part of a computer. For example, the controller may reside in a “cloud” and may be all or part of a fab host computer system. This enables remote access to wafer processing. The computer may enable remote access to the system, monitor the current progress of manufacturing operations, investigate the history of past manufacturing operations, investigate trends or performance criteria from multiple manufacturing operations, modify parameters of the current process, set processing steps following the current process, or start a new process. In some embodiments, a remote computer (e.g., a server) can provide process recipes to the system over a network. Such a network may include a local network or the internet. The remote computer may include a user interface that enables the entry or programming of parameters and / or settings. Such parameters and / or settings are then communicated from the remote computer to the system. In some embodiments, the controller receives instructions in the form of data. Such data identifies parameters for each of the processing steps performed during one or more operations. It should be understood that the parameters may be specific to the type of process being performed and the type of tool that the controller is configured to integrate or control. Therefore, as described above, the controllers may be distributed, for example, by including one or more individual controllers that are networked together and cooperate toward a common purpose, such as the processes and controls described herein. An example of a distributed controller for such purposes is one or more integrated circuits on a chamber that communicate with one or more remotely located integrated circuits (such as at the platform level or as part of a remote computer) and are combined to control the processes on the chamber.
[0092] Exemplary systems may include, but are not limited to, plasma etching chambers or modules, deposition chambers or modules, spin rinse chambers or modules, metal plating chambers or modules, cleaning chambers or modules, bevel edge etching chambers or modules, physical vapor deposition (PVD) chambers or modules, chemical vapor deposition (CVD) chambers or modules, atomic layer deposition (ALD) chambers or modules, atomic layer etching (ALE) chambers or modules, ion implantation chambers or modules, tracking chambers or modules, and any other semiconductor processing systems related to or available for the fabrication and / or manufacture of semiconductor wafers.
[0093] As described above, depending on one or more process steps performed by the tool, the controller may communicate with one or more other tool circuits or modules, other tool components, cluster tools, other tool interfaces, adjacent tools, nearby tools, tools located throughout the factory, a main computer, another controller, or tools used for material transfer to and from tool locations and / or load ports within the semiconductor manufacturing plant. conclusion
[0094] The embodiments described above have been explained in some detail for the purpose of clarifying understanding. However, it will be apparent that certain changes and modifications may be made within the scope of the appended claims. It should be noted that there are many alternative ways of implementing the processes, systems, and apparatus of these embodiments. Therefore, these embodiments should be considered illustrative and not restrictive, and are not limited to the details given herein.
Claims
1. An apparatus for processing a substrate, comprising: The apparatus comprises: A processing chamber comprising: An outer chamber; and a reactor having an inlet and an outlet, the reactor being disposed within the outer chamber; a processing chamber comprising: a plasma generator configured to provide a plasma to the reactor; A substrate support; Equipped with During processing, gas phase species pass from the reactor, through the outlet, and into the outer chamber; a flow conductance from the reactor into the outer chamber is variable and controllable during processing; The apparatus, wherein when the apparatus is in a low flow conductance state, the flow conductance from the reactor into the outer chamber is about 0.2 sccm / mTorr or less.
2. 2. The apparatus of claim 1, The apparatus further comprising a movable pressure control ring proximate the outlet to the reactor, the movable pressure control ring being adjustable to vary the flow conductance from the reactor into the outer chamber.
3. 2. The apparatus of claim 1, The apparatus further comprising a movable wall within the reactor, the movable wall being adjustable to vary the flow conductance from the reactor to the outer chamber.
4. 2. The apparatus of claim 1, An apparatus, wherein the substrate support is configured to be adjustable to vary the flow conductance from the reactor to the outer chamber.
5. An apparatus according to any one of claims 1 to 4, The apparatus, wherein when the apparatus is in a high conductance state, the flow conductance from the reactor into the outer chamber is greater than or equal to about 1 sccm / mTorr.
6. 6. The apparatus of claim 5, The apparatus further comprising a controller configured to switch the apparatus between a low conductance state and the high conductance state during processing of the substrate.
7. An apparatus for processing a substrate, comprising: The apparatus comprises: A processing chamber comprising: An outer chamber; and a reactor having an inlet and an outlet, the reactor being disposed within the outer chamber; a processing chamber comprising: a plasma generator configured to provide a plasma to the reactor and the outer chamber; A substrate support; Equipped with During processing, gas phase species pass from the reactor, through the outlet, and into the outer chamber.
8. 8. The apparatus of claim 7, The apparatus, wherein the plasma generator is configured to provide a direct plasma to the reactor, the direct plasma not being confined to the reactor.
9. 8. The apparatus of claim 7, The apparatus, wherein the plasma generator is configured to generate a remote plasma that is delivered to the outer chamber.
10. An apparatus for processing a substrate, comprising: The apparatus comprises: a processing chamber; A substrate support; a bypass path having a flow conductance of about 1 sccm / mTorr or greater; (i) a showerhead including a plurality of orifices for providing gas to the processing chamber, and (ii) a bypass outlet for providing gas to the bypass path; a gas injection passage configured to provide gas to the showerhead; An apparatus comprising:
11. An apparatus for processing a substrate, comprising: The apparatus comprises: a processing chamber; A substrate support; a first inlet to the processing chamber for providing at least a purge gas and a deposition vapor to the processing chamber; an optional second inlet to the processing chamber, where an etching gas is provided to the processing chamber via the first inlet or via the optional second inlet; a gas injection path configured to alternately provide at least the purge gas and the deposition gas to the first inlet; a purge gas supply path configured to provide the purge gas to the gas injection path; a deposition vapor supply passage configured to provide the deposition vapor to the gas injection passage; an etching gas supply path configured to provide the etching gas to the gas injection path or the optional second inlet; a bypass path fluidly coupled to the purge gas supply path and the deposition vapor supply path via a valve, the bypass path not supplying gas to the processing chamber; a controller configured to (i) alternately flow the purge gas and the deposition vapor into the processing chamber through the gas injection path; and (ii) alternately flow the purge gas and the deposition vapor into the bypass path. An apparatus comprising:
12. An apparatus for processing a substrate, comprising: The apparatus comprises: a processing chamber; a plasma generator configured to provide a plasma to the processing chamber; A substrate support; a first inlet to the processing chamber, the first inlet configured to provide a deposition vapor to the processing chamber; a second inlet to the processing chamber, the second inlet configured to provide an etching gas to the processing chamber, the deposition gas and the etching gas not mixing with each other prior to passing through the processing chamber; an outlet to the processing chamber; An apparatus comprising:
13. An apparatus according to any one of claims 1 to 12, The apparatus further comprising a controller configured to cause any of the methods described herein.