AI Technical Summary
Traditional RGB micro-light-emitting diode (μLED) arrays face challenges with high cost, low throughput, limited positional accuracy, poor reliability, and inefficiency due to pick-and-place methods and color conversion techniques, especially at small pixel pitches, and nanowire growth issues with poor light extraction efficiency and color gamut.
A monolithic native LED array is formed with overlapping light-emitting regions and controlled by varying gate voltage, using epitaxial quantum well structures and selective area growth on a wafer substrate, allowing for efficient, high-resolution, and densely integrated RGB pixels.
The solution enables smaller, more efficient, and less susceptible RGB pixels with controlled wavelength emission, suitable for high-resolution displays, overcoming the limitations of traditional methods by improving throughput and reducing degradation.
Abstract
Description
[Technical Field]
[0001] The present invention relates to light emitting diode (LED) device structures and methods of forming light emitting diode device structures, and in particular, but not exclusively, the present invention relates to voltage controllable wavelength of light emission from native LED devices. [Background technology]
[0002] Conventional red / green / blue (RGB) micro light-emitting diode (μLED) light-emitting pixel arrays are typically realized using pick-and-place techniques or by using color conversion materials deposited or embedded within standard planar light-emitting diode (LED) structures. However, as the pixel pitch of such arrays is reduced to extremely small pitches (e.g., less than 5 μm) to provide higher resolution arrays, several problems arise.
[0003] For example, using a pick-and-place method can be impractical due to the high cost, low throughput, and limited positional accuracy of transferring μLEDs. In the case of color conversion, the use of such techniques is limited by the size of the phosphors used for color conversion, which are typically larger than 10 μm (i.e., larger than the pixel pitch in arrays with very small pitches used for higher resolution). Furthermore, color conversion techniques can suffer from poor reliability and inefficiency due to the small absorption coefficients associated with quantum dots (QDs). For example, to sufficiently absorb the blue emission that excites the color-converting QD material, a thickness of the color-converting QD material greater than 10 μm is used, making the color-converting QD material unsuitable for arrays with very small pixel pitches.
[0004] To avoid the need to transfer LEDs and provide high-quality, efficient light emission, it is beneficial to provide a native array of LEDs on the same substrate. One approach to building a native array of LEDs on the same substrate relies on selective area growth of nanowires, which are arrays of individual structures grown substantially perpendicular to a patterned growth substrate to form light-emitting structures. In the light-emitting structures, the light-emitting surface is defined by the cross-sectional area of the nanowires, using a typical epitaxial quantum well structure grown between an epitaxial n-type doped layer and an epitaxial p-type doped layer. However, such nanowire growth is usually difficult to control and can be subject to severe limitations in achievable light efficiency and color gamut, for example, due to poor light extraction efficiency and impurity incorporation. Summary of the Invention [Means for solving the problem]
[0005] To alleviate at least some of the above problems, a light emitting diode structure is provided comprising: a p-type region, an n-type region, a gate contact; a first light emitting region for recombination of carriers injectable by the p-type and n-type regions; and a second light emitting region for recombination of carriers injectable by the p-type and n-type regions, the first light emitting region and the second light emitting region at least partially overlapping to form a light emitting surface associated with the first light emitting region and the second light emitting region, wherein the p-type region is at least partially formed in a first channel through the first light emitting region and the n-type region is at least partially formed in the second channel through the first light emitting region and the second light emitting region, and the light emitting device is configured such that the wavelength of light emitted by the light emitting surface is controllable by varying a gate voltage applied to one of the p-type and n-type regions by the gate contact to vary carrier injection into the first light emitting region by the p-type and n-type regions.
[0006] Also provided is a method of forming a light emitting diode device comprising: a p-type region; an n-type region; a gate contact; a first light emitting region for recombination of carriers injectable by the p-type and n-type regions; and a second light emitting region for recombination of carriers injectable by the p-type and n-type regions, the first light emitting region and the second light emitting region at least partially overlapping to form a light emitting surface associated with the first light emitting region and the second light emitting region, the method including at least partially forming a p-type region in a first channel through the first light emitting region and the second light emitting region; and at least partially forming an n-type region in the second channel through the first light emitting region and the second light emitting region, the light emitting device being configured such that a gate voltage applied to at least one of the p-type and n-type regions by the gate contact varies carrier injection into the first and second light emitting regions by the p-type and n-type regions, thereby enabling control of the wavelength of light emitted by the light emitting surface.
[0007] Advantageously, a sequence of monolithically grown native GaN-based light-emitting structures can improve space utilization in arrays because the light-emitting regions are effectively stacked rather than side-by-side. Advantageously, compared to color-converted pixels, native colors can be made into smaller, more efficient, and less susceptible to degradation. Advantageously, compared to pick-and-place assembly, such structures can be formed in arrays at much higher throughput by forming arrays on wafers rather than transferring millions of pixels onto a substrate.
[0008] Preferably, the light emitting diode device comprises a third light emitting region at least partially overlapping the first and second light emitting regions to form a light emitting surface, wherein a p-type region is at least partially formed in the first channel through the third light emitting region and an n-type region is at least partially formed in the second channel through the third light emitting region, and the light emitting device is configured such that the wavelength of light emitted by the light emitting surface is controllable by varying a gate voltage applied to at least one of the p-type and n-type regions by a gate contact to vary carrier injection by the p-type and n-type regions into the first, second, and third light emitting regions. Advantageously, the structure may be used to provide red, green, and blue light emission, making structures and arrays so formed suitable for use in full-color displays, such as high-resolution light emitting displays.
[0009] Preferably, the first channel or the second channel is a via that at least partially defines the periphery of the light-emitting surface. Advantageously, the use of vias that at least partially define the periphery means that no etching is required to electrically isolate pixels from one another. Advantageously, the cathode grid runs around the periphery of each pixel, and more preferably, each pixel is separated at the top and bottom by undoped material, such as undoped GaN, allowing for higher density pixel integration.
[0010] Preferably, the depletion depth in the first channel or the second channel is varied by varying the gate voltage. Advantageously, by controlling the gate voltage, different wavelengths of light can be emitted from the structure. Such color control can provide a multicolor display.
[0011] Preferably, the light emitting diode device is an epitaxial crystalline semiconductor structure, wherein at least one of the first light emitting region, the second light emitting region, and the third light emitting region includes one or more epitaxial crystalline semiconductor layers, and preferably at least one of the first light emitting region, the second light emitting region, and the third light emitting region includes at least one epitaxial crystalline semiconductor layer. The device comprises an epitaxial crystalline semiconductor structure including a quantum well layer. Advantageously, standard planar epitaxial growth / deposition processes can be applied to form MQWs, which offers higher internal quantum efficiency (IQE), compared to the formation of light-emitting nanowires. The planar nature of the device also lends itself to better light extraction using standard surface patterning techniques.
[0012] Preferably, the p-type and / or n-type regions comprise a planarization layer, which is advantageously used both to provide a base for subsequent growth and a common electrical path for use, for example, as a common electrode.
[0013] Preferably, the gate contact is a ring contact corresponding to the pixel defined by the light emitting surface, and preferably the ring contact forms either a polygonal or circular shaped contact. Advantageously, the ring contact allows for uniform electrical injection into the light emitting diode structure and therefore uniform light distribution from the associated pixel.
[0014] Preferably, the light emitted from the first light-emitting region has a different primary peak wavelength than the light emitted from the second light-emitting region. Advantageously, a polychromatic output is provided.
[0015] Preferably, the first and second light emitting regions are separated by an undoped region, which advantageously reduces carrier diffusion within the structure.
[0016] Also provided is an array of light emitting diode devices comprising a plurality of light emitting diode devices. Advantageously, an array of light emitting diode devices, each providing multiple wavelength outputs, means that a high resolution, densely integrated light emitting diode display is provided.
[0017] Preferably, the array comprises a plurality of pixels, each pixel corresponding to an emitting surface area of a light emitting diode device. Advantageously, a full-color light emitting display having a small size and a high density of pixels can be provided, thereby forming a high resolution display.
[0018] Preferably, the p-type or n-type regions of at least two of the plurality of light emitting diode devices are shared to form a common electrode, which is advantageously a growth layer that forms part of a high quality integrated growth while enhancing the electrical connection versatility of the structure.
[0019] Preferably, the common electrode is on the opposite side of the array from the gate contact. Advantageously, higher density pixel integration can be achieved.
[0020] Further aspects of the present invention will become apparent from the following description and the appended claims.
[0021] A detailed description of embodiments of the present invention will now be given, by way of example only, with reference to the drawings in which: [Brief explanation of the drawings]
[0022] [Figure 1A] FIG. 1A shows a cross-sectional view of the epitaxial structure. [Figure 1B] FIG. 1B shows a cross-sectional view of the epitaxial structure of FIG. 1A after further processing. [Figure 1C] FIG. 1C shows a cross-sectional view of the epitaxial structure of FIG. 1B after further processing. [Figure 1D] FIG. 1D shows a cross-sectional view of the epitaxial structure of FIG. 1C after further processing. [Figure 1E] FIG. 1E shows a cross-sectional view of the epitaxial structure of FIG. 1D after further processing. [Figure 1F] FIG. 1E shows a cross-sectional view of the epitaxial structure of FIG. 1D after further processing. [Figure 2] FIG. 2 shows a plan view of an array of light emitting devices. [Figure 3] FIG. 3 shows a cross-sectional view of carrier injection in the epitaxial structure of FIG. 1E. [Figure 4] FIG. 4 shows a cross-sectional view of carrier injection in the epitaxial structure of FIG. 1E. [Figure 5A] FIG. 5A shows a cross-sectional view of a mesa formed in an epitaxial structure. [Figure 5B] FIG. 5B shows a top view of the mesa of FIG. 5A. [Figure 5C] FIG. 5C shows a top view of a symbol-based display. [Figure 6A] FIG. 6A shows a cross-sectional view of the mesa of FIG. 5A after further processing. [Figure 6B] FIG. 6B shows a top view of the processed mesa of FIG. 6A. DETAILED DESCRIPTION OF THE INVENTION
[0023] Light-emitting diodes (LEDs) are typically formed by processing light-emitting structures grown by forming epitaxial crystalline layers on relatively large wafer substrates in reactors such as, for example, MOCVD (metal organic chemical vapor deposition) reactors, MBE (molecular beam epitaxy) reactors, or other chemical vapor deposition reactors. For the reasons discussed above, known methods for creating arrays of light-emitting devices, such as arrays of high-resolution micro LEDs, face problems in processing LEDs made by crystal growth on relatively large wafer substrates to provide micro LEDs for high-resolution arrays. Using nanowire LED arrays to overcome these processing problems leads to problems in controlling the growth process and generally inferior performance than seen with conventional growth of LEDs on relatively large wafer substrates.
[0024] This disclosure describes LEDs that can be formed as part of a monolithic, high-resolution array by processing light-emitting structures that can be grown on relatively large wafer substrates. Beneficially, native color pixels can be formed that are smaller, more efficient, and less susceptible to degradation compared to color-converted pixels. Compared to pick-and-place assembly, processing epitaxial structures grown directly on wafers means that forming arrays of pixels on wafers eliminates the need to transfer millions of pixels (and the associated defects in the transfer process), thus allowing for higher throughput. Compared to nanowires, standard planar epitaxial deposition layer growth processing means that multiple quantum wells (MQWs) can be formed, resulting in high-quality growth and therefore relatively high internal quantum efficiency (IQE). Furthermore, processing the epitaxial structures provides planar devices that are conducive to light extraction using standard surface patterning techniques.
[0025] Advantageously, as described with reference to FIGS. 1-6, an epitaxial layer structure is provided in which blue, green, and red light-emitting MQWs are stacked in sequence without the use of p-type cladding. In one example, n-type GaN grid vias that intersect the MQW regions and define the periphery of the pixel are provided by an etching and selective area growth process sequence. A p-GaN via is also provided by a similar process sequence. Electron and hole injection is achieved by lateral injection directly into the quantum wells (QWs). In one example, a dielectric insulating layer is deposited on the n-type GaN grid via to electrically isolate the n-type GaN grid from a ring gate deposited on the grid. The arrangement of the ring metal gate, dielectric, and n-type GaN via forms a ring-shaped metal-insulator-semiconductor field effect transistor (MIS-FET). The grid The n-type doping in the ring gate vias and the thickness of the insulator in the MIS-FET are such that a negative voltage applied between the ring gate contact and the cathode contact, which is in ohmic contact with the n-type GaN, gradually depletes free electrons from the n-type ring via. By controlling the gate voltage, current can be passed to different depths in the structure, thereby energizing MQWs at different depths in the structure. Therefore, the voltage applied to each of the ring gates can be used to independently tune the color of light emitted from each pixel.
[0026] Advantageously, stacking light-emitting regions associated with different emission wavelengths allows the same pixel to emit three colors, rather than having separate pixels emitting red, green, or blue light side by side, allowing pixels to be packed more densely together.
[0027] Further advantages arising from the described methods and structures will become apparent in the following description. A method for providing an array of micro LEDs is described below with reference to various processing steps (which may include both steps performed in a growth reactor and steps performed outside the growth reactor using other processing and / or growth equipment). The methods and structures are described with reference to III-V semiconductor materials. In particular, the methods and structures are described with reference to nitride structures, including gallium nitride (GaN)-based light-emitting structures, which are known to result in relatively high-efficiency light-emitting structures. However, in further examples, the methods and structures are applicable to light-emitting structures based on other materials, particularly compound semiconductor materials, such as other III-V compound semiconductor materials and II-VI compound semiconductor materials.
[0028] In the following drawings, like reference numerals are used to denote aspects of structure associated with the same or equivalent features provided by the same or similar processes.
[0029] FIG. 1A illustrates structure 100A, an epitaxial structure 100A that can form the basis of an LED pixel array. Such an LED pixel array has a plurality of individual pixels, which can be individually addressable based on how such an LED pixel array is connected to a power source (e.g., depending on the configuration of a backplane for the LED pixel array). Epitaxially grown structure 100A, formed from multiple region-defining layers, contains an effective stack of natively grown light-emitting regions configured to emit light of different wavelengths. By appropriately processing epitaxially grown structure 100A, pixels suitable for use in displays can be fabricated, with the pixels having a light-emitting surface that emits light at wavelengths that depend on appropriate voltage control of the processed light-emitting structure.
[0030] Structure 100A is a gallium nitride (GaN)-based epitaxial structure containing multiple quantum wells (MQWs) grown by metalorganic chemical vapor deposition (MOCVD), which is effectively a native LED structure. Advantageously, known techniques can be used to provide high quality material that can be processed to provide LED arrays.
[0031] 1A shows an n-doped (n-GaN) n-type region 104 on which an undoped region 106 (intentionally undoped GaN) is grown. The n-type region 104 is formed on a substrate 102 and is approximately 500 nm thick with a doping level of 8×10 18 at / cm 3 In a further example, n-type regions 104 have different thicknesses and / or doping levels. Substrate 102 is formed from sapphire. In a further example, alternative and / or additional substrates (such as silicon or native GaN substrates) are used to provide a basis for epitaxial growth of structure 100A.
[0032] On top of the undoped region 106 is an undoped aluminum gallium nitride (AlGaN) region. First, a GaN-based superlattice structure 110 is grown on a first barrier region 108. This layer is the AlGaN barrier region 108. On this first barrier region 108, a GaN-based superlattice structure 110 is grown. The superlattice structure is formed to maintain the crystalline quality of the subsequently grown layers, taking into account the composition of the subsequently grown layers and the strain introduced depending on the thickness and composition of the subsequently grown layers. In one example, the superlattice structure 110 has 20 repeats of a 1.5 nm InGaN (5% indium composition) layer and a 2.7 nm GaN layer. In further examples, alternative structures are used and / or the superlattice structure is not included or is included with different layers of different composition and / or thickness.
[0033] Above superlattice structure 110 is light emitting region 112 having a multiple quantum well (MQW). Above light emitting region 112 is a further barrier layer, second barrier region 114. Above second barrier region 114 is second light emitting region 116. Above second light emitting region 116 is a layer providing third barrier region 118. Above the third barrier region is third light emitting region 120, and above third light emitting region 120 is an undoped layer, such as undoped GaN. Structure 100A is terminated with an insulating region provided by dielectric layer 122. Dielectric layer 122 is an Al2O3 layer having a thickness of approximately 10 nm. In further examples, dielectric layer 122 is formed of a different thickness and / or material while providing the necessary insulating properties. In further examples, additional and / or alternative layers and / or materials are used in epitaxial structure 100A.
[0034] N-type region 104, undoped region 106, first barrier region 108, superlattice 110, light emitting region 112, second barrier region 114, second light emitting region 116, third barrier region 118, third light emitting region 120, and dielectric layer 122 are shown in cross section as multiple epitaxial layers grown on a substrate. In further examples, alternative and / or additional methods may be used to form structure 100A; for example, dielectric layer 122 may be deposited on an otherwise epitaxially grown compound crystal structure in further examples.
[0035] Light-emitting regions 112, 116, 120 are grown in the appropriate order depending on the final orientation of the light-emitting device and its associated light-emitting surface. Here, light is extracted through n-type region 104 of the structure described in FIG. 1A, as described with respect to FIG. 1F, with first light-emitting region 112 configured to emit light having a primary peak wavelength corresponding to blue light, second light-emitting region 116 configured to emit light having a primary peak wavelength corresponding to green light, and third light-emitting region 120 configured to emit light having a primary peak wavelength corresponding to red light. This means that when the structure is inverted, light of longer wavelengths will pass through the structure without being absorbed by subsequent light-emitting regions (e.g., because blue light is absorbed in the green- and red-emitting quantum wells, and green light is absorbed in the red-emitting quantum well).
[0036] First light-emitting region 112 comprises an MQW. Additionally or alternatively, light-emitting region 112 may comprise a single quantum well (SQW). Additionally or alternatively, light-emitting region 112 may include one or more quantum dots or other structures that enable carrier recombination and light emission. The quantum wells and quantum dots confine carriers and, in use, provide a light source based on radiative carrier recombination in the quantum structure following carrier injection, e.g., by n-type and p-type regions when connected to a cathode and an anode, respectively. Light-emitting region 112 is configured to emit light having a primary peak wavelength (approximately 450 nm) corresponding to blue light. In one example, first light-emitting region 112 is formed with one or more quantum wells of 3 nm thick InGaN with a 20% indium composition. In further examples, quantum wells of different numbers, thicknesses, and compositions are used.
[0037] Second light emitting region 116 comprises an MQW. Additionally or alternatively, second light emitting region 116 may comprise a single quantum well (SQW). Additionally or alternatively, second light emitting region 116 may comprise one or more quantum dots or other structures that enable carrier recombination and light emission. The quantum wells and quantum dots confine carriers and, in use, provide a light source based on radiative carrier recombination in the quantum structure following carrier injection, for example, by n-type and p-type regions when connected to a cathode and anode, respectively. Second light-emitting region 116 is configured to emit light having a primary peak wavelength (approximately 520 nm) corresponding to green light. In one example, second light-emitting region 116 is formed with one or more quantum wells of 3 nm thick InGaN with a 30% indium composition. In further examples, quantum wells of different numbers, thicknesses, and compositions are used.
[0038] Third light emitting region 120 comprises an MQW. Additionally or alternatively, third light emitting region 120 may comprise a single quantum well (SQW). Additionally or alternatively, third light emitting region 120 may comprise one or more quantum dots or other structures that enable carrier recombination and light emission. The quantum wells and quantum dots confine carriers and, in use, provide a light source based on radiative carrier recombination in the quantum structure following carrier injection, e.g., by n-type and p-type regions when connected to a cathode and anode, respectively. Third light emitting region 120 is configured to emit light having a primary peak wavelength (approximately 620 nm) corresponding to red light. In one example, third light emitting region 120 is formed with one or more quantum wells of 3 nm thick InGaN with a 40% indium composition. In further examples, quantum wells of different numbers, thicknesses, and compositions are used.
[0039] In structure 100A, the quantum wells are separated by 3 nm of undoped GaN. The quantum wells and barrier layers are separated by 3 nm of undoped GaN. In further examples, different thicknesses and materials are used in structure 100A while retaining at least some of the functionality described herein.
[0040] The first barrier region 108, which is an undoped AlGaN barrier region 108, blocks carrier diffusion away from the first light emitting region 112. The first barrier region 108 has a thickness of 20 nm and a composition of AlGaN with an aluminum composition of 20%. In further examples, the first barrier region 108 has a different thickness and / or composition and / or is formed from a different material while providing suitable electron blocking properties and enabling high-quality crystal growth. While the first barrier region 108 is shown to be an AlGaN barrier region 108, additionally or alternatively, the barrier region 108 is formed from a different material.
[0041] Second barrier region 114, which is an undoped AlGaN barrier region 114, blocks carrier diffusion between first light emitting region 112 and second light emitting region 116. Second barrier region 114 has a thickness of 20 nm and a composition of AlGaN with an aluminum composition of 20%. In a further example, second barrier region 114 has a different thickness and / or composition and / or is formed from a different material while providing suitable electron blocking properties and enabling high-quality crystal growth. Although second barrier region 114 is shown to be an AlGaN barrier region 114, additionally or alternatively, barrier region 114 is formed from a different material.
[0042] Third barrier region 118, which is an undoped AlGaN barrier region 118, blocks carrier diffusion between second light emitting region 116 and third light emitting region 120. Third barrier region 118 has a thickness of 20 nm and a composition of AlGaN with an aluminum composition of 20%. In a further example, third barrier region 118 has a different thickness and / or composition and / or is formed from a different material while providing suitable electron blocking properties and enabling high-quality crystal growth. Although third barrier region 118 is shown to be an AlGaN barrier region 118, additionally or alternatively, barrier region 118 is formed from a different material.
[0043] Although light emitting regions 112, 116, 120 include MQWs, in further examples, light emitting regions 112, 116, 120 may have single quantum wells (SQWs). Light emitting regions 112, 116, 120 include multiple material layers to form an active region. For example, light emitting regions 112, 116, 120 may include layers such as short period superlattices and / or undoped recovery layers, thereby providing high-quality crystalline material and light emission from light emitting regions 112, 116, 120. Additionally or alternatively, light emitting regions 112, 116, 120 may include one or more quantum dots. Quantum wells and quantum dots confine carriers and, in use, provide a light source based on carrier recombination in the quantum structure following carrier injection by n-type and p-type regions when connected to a cathode and anode, respectively.
[0044] N-type region 104 is typically formed on a substrate 102, although alternatively, n-type region 104 may itself be a free-standing substrate suitable for growth of subsequent crystalline layers. In one example, substrate 102 is a sapphire substrate. In further examples, alternative substrates such as silicon substrates or GaN substrates are used.
[0045] The epitaxial structure 100A is grown using an MOCVD reactor. Advantageously, such structure 100A may be optimized for MOCVD growth and provide high-quality growth for efficient light generation. Additionally or alternatively, other deposition and / or growth methods, such as molecular beam epitaxy (MBE), may be used to provide the epitaxial structure 100A.
[0046] N-type region 104 is formed from n-type gallium nitride. However, in further examples, n-type region 104 may be formed from and / or based on other materials, such as other semiconductor materials (e.g., other III-V compound semiconductor materials, II-VI compound semiconductor materials, or other suitable materials).
[0047] The barrier regions 108, 114, and 118 are formed from aluminum gallium nitride, e.g., AlGaN with a 20% aluminum composition. However, in further examples, the barrier regions 108, 114, and 118 may additionally or alternatively be formed from different materials, such as other semiconductor materials (e.g., other III-V compound semiconductor materials, II-VI compound semiconductor materials, or other suitable materials). The superlattice 110 is formed from a gallium nitride-based material. Additionally or alternatively, the superlattice 110 is formed from other materials, such as other semiconductor materials (e.g., other III-V compound semiconductor materials, II-VI compound semiconductor materials, or other suitable materials).
[0048] Light emitting regions 112, 116, 120 each include at least one quantum well. Additionally or alternatively, light emitting regions 112, 116, 120 each include additional quantum wells. Additionally or alternatively, light emitting regions 112, 116, 120 include quantum dots or other quantum structures. Light emitting regions 112, 116, 120 are gallium nitride-based regions, and at least the quantum wells in each light emitting region 112, 116, 120 are formed from a gallium nitride-based material such as indium gallium nitride (InGaN) or aluminum indium gallium nitride (AlNGaN). Additionally or alternatively, different materials are used, such as other semiconductor materials (e.g., other III-V compound semiconductor materials, II-VI compound semiconductor materials, or other suitable materials), depending on the structure being grown. The composition of the quantum wells in light-emitting regions 112, 116, 120 is determined based on the primary peak wavelength selected for emission from light-emitting regions 112, 116, 120. Although three light-emitting regions 112, 116, 120 are shown in the drawings, in further examples, a different number of light-emitting regions are implemented. For example, there may be two light-emitting regions, and structure 100A would be adapted accordingly.
[0049] The light emitting regions 112, 116, 120 do not contain any doping. The regions do not include silicon doping or magnesium doping due to intentional doping of the light emitting regions 112, 116, 120 during growth of structure 100A. In a further example, doping is used in the light emitting regions 112, 116, 120, but to a degree that does not affect carrier injection for light emission through the light emitting surfaces of the pixels defined by the vias through the light emitting regions 112, 116, 120, as described herein. In a further example, different semiconductor layers are grown or otherwise formed to provide a base structure for processing a monolithic array of micro LEDs.
[0050] 1A, one skilled in the art will understand that additional layers, omissions of layers, and alternative layers may be used to implement the concepts described herein depending on the particular needs of a particular implementation. A description of a layer being formed on another layer indicates a positional relationship with respect to the order of growth of the layers and does not necessarily exclude the presence of a layer between a first layer and a second layer that is described as being on the first layer.
[0051] Once the epitaxial structure 100A is provided, it may be treated to provide conductive regions through which carriers may be injected into the final structure.
[0052] Accordingly, FIG. 1B shows the processed epitaxial structure 100B. The epitaxial structure 100A of FIG. 1A is shown with a channel 124 formed through the epitaxial structure to contact the n-type region 104. The channel 124 is formed using a mask layer. A mask layer (not shown) is formed and processed using known techniques, including lithography techniques, to selectively create openings and expose underlying portions of the epitaxial structure 100A, such as the dielectric layer 122. Portions of the mask layer are selectively removed, followed by selective etching of the underlying epitaxial structure 100A. Such selective etching provides the channel 124 in the epitaxial structure 100A. The channel 124 (also referred to as a via 124) is also formed by removing material to leave a path through the remaining material. Depending on the shape of the exposed areas in the mask layer and the depth of the etch, the channels / vias formed will have a corresponding form, which in one example is that of a trench via or a cylindrical via. Channels / vias 124 are formed by etching material to leave trenches, holes, or other pathways, but in a further example, channels 124 / vias 124 are additionally or alternatively created by forming material such that the absence of material creates a via structure within another structure, as opposed to removing material.
[0053] In one example, the mask layer is silicon nitride. Additionally or alternatively, a different material, such as silicon dioxide, is used. Advantageously, silicon nitride is an effective and controllable mask layer for subsequent processing steps.
[0054] Channel / via 124 is shown etched all the way through epitaxial structure 100A down to n-type region 104. Advantageously, this means that any n-type material subsequently deposited within channel / via 124 can be contacted by n-type region 104 on one side of the device and the n-type region formed within channel / via 124. This allows for the provision of gate and cathode contacts, as described herein.
[0055] To etch the channels / vias 124, lithographic techniques are used to pattern a mask layer and to open openings in the mask layer to allow etching of material exposed by the openings formed in the mask. The channels / vias 124 are shown in cross section. In plan view, the channels / vias 124 are formed in a grid structure to define pixels, with the channels / vias 124 being separated by trench channels that separate each individual pixel. A perimeter of the light-emitting surface of each individual pixel is defined by etching through the light-emitting regions 112, 116, 120 to form the channel / via 124. In one example, the channel / via 124 is formed using a dry etching technique, such as a plasma-based technique. Preferably, a wet etching process is used to repair damage caused by etching the channel / via 124. Additionally or alternatively, any suitable etching technique may be used to form the channel / via 124.
[0056] FIG. 1C shows further processed epitaxial structure 100C having channel 124 etched through epitaxial structure 100A and then overgrown to form an n-type region through light emitting regions 112, 116, 120.
[0057] When the channel / via 124 is formed in the epitaxial structure 100A, a selective overgrowth of n-type material is formed. Such overgrowth or deposition of material in the channel / via 124 may be performed while the mask layer used to enable etching of the channel / via 124 remains in place, for example, so that no growth occurs on the dielectric layer 122. FIG. 1C shows the same basic structure 100C as shown in the epitaxial structures 100A and 100B of FIGS. 1A and 1B, but the structure 100C in FIG. 1C has been further processed. The processed epitaxial structure 100C in FIG. 1C shows the structure etched through to provide the channel / via 124 as shown in FIGS. 1A and 1B. The channel / via 124 has been etched vertically through the epitaxial structure 100A down to the doped n-type region 104. An n-type overgrowth 128 of n-doped GaN (n-GaN) is then formed in the channel / via 124 to provide a conductive region through the light emitting regions 112 , 116 , 120 .
[0058] While the lateral distances between the channels / vias 124 (and n-type overgrowth 128) in FIG. 1C relate to a cross-section of a single pixel, it is understood that the selective etching of the epitaxial structure 100A and the overgrowth of n-type material in the via trenches provided by the selective etching result in an n-type grid that is, in effect, a common electrode (in this case, a cathode) for all of the pixels defined by the n-type overgrowth 128 throughout the light-emitting regions 112, 116, and 120 of the epitaxial structure 100C. Advantageously, the selective area growth of n-type material is performed using a metalorganic chemical vapor deposition (MOCVD) reactor using relatively high temperatures. These relatively high temperatures anneal defects and passivate any open MQW surfaces. After processing, no dangling bonds remain at the MQW edges, and therefore no passivation is required. Beneficially, therefore, a significant reduction in non-radiative recombination is achieved in light emitting regions 112, 116, 120. In a further example, the n-type overgrowth is performed using a different technique, such as MBE.
[0059] The n-type overgrowth 128 is shown raised from the surface of the dielectric layer 122. This advantageously allows contact to the doped overgrowth through one side of the structure 100C, opposite the side that can also be contacted when the substrate 102 of the structure 100C is removed. The structure 100C is not shown to scale. However, in one example, the width of the channel / via 124 is 500 nm. In a further example, the size of the structure is determined, for example, by the technique used and the desired structure. For example, the crystal habit of the material used may determine the growth shape of the raised material surface of any mask layer. A grid can be formed by growing n-type material in the channel / via 124 by etching through openings exposed in the mask layer. The doping level of the n-type region formed by the n-type overgrowth 128 is less than the doping level of the planar n-type region 104 that forms part of the epitaxial structure 100A. Advantageously, the lower doping level helps make the change in the space charge region in the n-type overgrowth 128 more rapidly change with gate voltage, as described herein. In a further example, the doping level in the n-type overgrowth 128 is selected to provide light emission control at a predetermined rate.
[0060] Once an effective cathode provided by n-type overgrowth 128 is established within channel / via 128, an anode is established based on p-type overgrowth formed within further via 126. This is illustrated in relation to Figures 1D and 1E.
[0061] FIG. 1D shows a cross-sectional view of epitaxial structure 100D, which is further processed from epitaxial structure 100C of FIG. 1C. There is an additional channel / via 126, which is a centrally formed cylindrical channel / via 126 within the pixel periphery defined by channel / via 124 having n-type overgrowth 128 formed through light-emitting regions 112, 116, and 120. Additionally or alternatively, additional channel / via 126 may be located in any suitable location for providing light emission. The cross-sectional shape of additional channel / via 126, as viewed in plan view, is determined by the patterning and etching process used to provide additional channel / via 126. Channel / via 126 has a width of approximately 500 nm. In a further example, channel / via 126 has a width sized to meet preferred implementations for carrier injection and pixel configuration. The further channel / via 126 is realized by depositing a further mask layer, selectively patterning the further mask layer to form openings that expose the underlying structure, and etching through the mask layer to the active area provided by the light emitting regions 112, 116, 120 using known lithography and etching techniques.
[0062] The structure 100D of FIG. 1D is then further processed to provide the structure 100E of FIG. 1E, where a p-type overgrowth 130 is formed in the additional channel / via 126. The p-type overgrowth 130 has a doping level of 3×10 18 at / cm 3The light emitting regions 112, 116, 120 are formed of p-type doped GaN. In a further example, different materials and / or different doping levels are used to provide the p-type regions. Selective area growth of the p-type overgrowth material is performed using a metalorganic chemical vapor deposition (MOCVD) reactor using relatively high temperatures. Such relatively high temperatures anneal defects and passivate any open MQW surfaces. After processing, no dangling bonds remain at the MQW edges, and therefore passivation is not required. Beneficially, therefore, a significant reduction in non-radiative recombination in the light emitting regions 112, 116, 120 is achieved. In a further example, the p-type overgrowth is performed using a different technique, such as MBE.
[0063] N-type overgrowth 128 provides an n-type region, and p-type overgrowth 130 provides a p-type region, allowing carrier injection into light emitting regions 112, 116, 120, as described herein. N-type overgrowth 128 provides an effective cathode, and p-type overgrowth 130 provides an effective anode, which, when an appropriate power source is used, allows lateral injection of carriers into light emitting regions 112, 116, 120. Such lateral carrier injection in light emitting regions 112, 116, 120 results in more efficient carrier injection, including more efficient hole injection, and therefore more efficient light emission. Carrier injection into the light emitting regions 112, 116, 120 may be based on the carrier diffusion length of the carriers injected into the multiple quantum well structures of the light emitting regions 112, 116, 120 to provide light, which may be emitted through a light emitting surface defined by a pixel periphery formed by n-type overgrowth 128 in a channel / via 124 etched through the light emitting regions 112, 116, 120.
[0064] Advantageously, in comparison to known selective area growth techniques, only n-type and p-type regions can be overgrown, thereby eliminating the poor uniformity and component atomic tension that typically occurs when growing AlGaN and InGaN alloys on patterned surfaces. This will eliminate issues related to the idiosyncratic pull.
[0065] Although the channel / via 124 that passes through the light emitting regions 112, 116, 120 of the epitaxial structure to form trenches that define the light emitting surface of the pixels is shown based on etching the epitaxial structure, in further examples other techniques are used to form the light emitting regions through which the channel / via passes to define the periphery of the light emitting surface of the pixels in the pixel array.
[0066] Figure 1F shows a cross-sectional view of a processed light emitting structure 100F as described with respect to Figures 1A-1E. The processed light emitting structure 100F is provided by inverting the light emitting structure of Figure 1E to extract light through the n-type region 104 (with the substrate 102 removed), thus avoiding absorption due to the p-type contact 136 formed on the p-type overgrowth 130 in the further channel / via 126.
[0067] A gate contact 134 is shown associated with the n-type overgrowth 128. The gate contact 134 includes a dielectric region 132 between the conductive portion of the gate contact 134 and the n-type overgrowth 128 in the channel / via 124 formed through the light emitting regions 112, 116, 120. The gate contact 134 forms a metal-insulator-semiconductor contact as part of an effective metal-insulator-semiconductor field effect transistor (MIS-FET).
[0068] The gate contact 134 is formed as a ring contact around the periphery of the pixel associated with the p-type overgrowth 130, and the ring contact follows the grid defined by the n-type overgrowth channels / vias 124 to provide n-type regions through the light-emitting regions 112, 116, 120 of the structure 100A. This is illustrated in FIG. 2, which shows a plan view 200 of the metal-insulator-semiconductor gate contact 134 and ohmic anode p-type contact 136. The pattern is repeated in an array. While nine light-emitting pixels 202 are shown in the example of FIG. 2, an array may be formed with any number of light-emitting pixels 202. Emitting pixel 202 is shown with a width dimension 140 that relates to the distance between channels / vias 124 surrounding a further central channel / via 126 (thus plan view 200 is actually a plan view of the underside of emitting pixel 202 opposite light-emitting surface 128 as described with respect to FIG. 1F). Although ring gate contacts 134 are shown as square shaped that relate to square shaped emitting pixels, in further examples gate contacts 134 take any suitable shape that relates to the emitting pixels with which they are associated.
[0069] FIG. 1F also shows an insulating dielectric layer 122. The insulating dielectric layer 122 insulates the n-type overgrowth 128 from any connections used to contact the p-type overgrowth 130. Preferably, the insulating layer 122 is silicon dioxide. An ohmic p-type contact 136 is shown to which the anode of each pixel to be addressed, having a cross-sectional dimension 140, is connected. Further examples include additional and / or alternative layers. In one example, a mirror / barrier layer is provided configured to reflect light emitted from the light-emitting regions 112, 116, 120 out of a light-emitting surface 138 defined by the n-type overgrowth 128 in a channel / via 124 that defines the periphery of the pixel. Advantageously, the ohmic p-type contact 136 can be connected to a backplane such that the p-type contact 136 at each pixel in the array is contacted and independently addressable.
[0070] A metal grid 142 is shown designed to make ohmic contact to the common cathode n-type grid of the light-emitting array. Such metal grid 142 is aligned with the n-type overgrowths 128 in the channels / vias 124 to maximize light extraction and therefore such that, when viewed in plan, it may assume substantially the same configuration as the grid provided by the channels / vias 124 etched through the light-emitting regions 112, 116, 120 of epitaxial structure 100A. Advantageously, the ohmic cathode contact is on the opposite side of structure 100F from the gate contact 134 and ohmic anode p-type contact 136, thereby providing a This facilitates voltage control of carrier injection into light-emitting regions 112, 116, 120, increasing light output, while making efficient use of the limited space associated with the pixel.
[0071] The pixel formed by the periphery associated with n-type overgrowth 128 providing the n-type region may be the width of the pixel, having dimension 140 shown in FIG. 1F. The pixel's light-emitting surface 138 (above n-type region 104) is optionally patterned. In the example of FIG. 1F, light-emitting surface 138 is curved. In a further example, the light-emitting surface is planar or patterned in any suitable manner to provide a surface through which light from light-emitting regions 112, 116, 120 exits structure 100F.
[0072] A cathode contact of metal grid 142 is shown providing electrical connection to n-type region 104. The cathode contact is an ohmic metal contact and is shown following the periphery of the associated light-emitting pixel in a manner similar to gate contact 134. However, in further examples, the cathode contact may take any suitable form and be formed from any suitable material. For example, n-type region 104 may provide a common electrode and may be electrically connected in a suitable manner. In a further example, a transparent conductive material such as indium tin oxide (ITO) may be used to provide the common electrode.
[0073] While the above LED structures are described with respect to growth by MOCVD, in some instances growth by different and / or complementary techniques may be beneficial. For example, growth by MBE may allow for lower temperature growth and / or slower growth rates, which may have advantages with respect to the growth and processing steps described above. Those skilled in the art will appreciate that, although the above process steps are described in any order, in further instances, the process steps may be performed in any order suitable to achieve the target structure.
[0074] To provide control over the wavelength of light emitted by the light emitting structure described in connection with Figures 1-2, carrier injection into light emitting regions 112, 116, 120 by p-type overgrowth 130 and n-type region 128 by anode contact 136 and cathode contact 142, respectively, is varied by application of a voltage at gate contact 134. This is shown in Figures 3 and 4.
[0075] FIG. 3 shows a light-emitting diode device 300 according to a first example of carrier injection into one of light-emitting regions 120. Arrow 302 indicates lateral carrier injection into light-emitting region 120 by p-type overgrowth 130, and a further arrow 304 indicates lateral carrier injection into light-emitting region 120 by the n-type region. Varying the voltage at gate contact 134 changes the carrier injection into light-emitting regions 112, 116, 120. This is illustrated in a second example of a light-emitting diode device 400 in FIG. 4. FIG. 4 shows arrow 402 indicating lateral carrier injection into light-emitting region 116 by p-type overgrowth 130 and lateral carrier injection into light-emitting region 116 by the n-type region (arrow 404). The change in carrier injection is provided by application of a negative voltage to gate contact 134, the negative voltage being lower than the voltage on cathode metal grid 142. The gate voltage removes electrons from the cathode pillars formed by the n-type overgrowth 128, pushing the space charge region deeper. Further increasing the negative voltage pushes the space charge region deeper, ultimately resulting in carrier injection into the first light emitting region 112 rather than the second light emitting region 116. Thus, gate voltage control can control the proportion of light emitted by the light emitting regions 112, 116, 120. Thus, if the n-type overgrowth 128 surrounds the light emitting regions 112, 116, 120 of the active region of a light emitting diode device, the gate voltage controls the depletion layer depth of the via surrounding the active region.
[0076] Advantageously, the pixel having light-emitting surface 138 emits red-green-blue light in sequence as the gate voltage at gate contact 134 becomes more negative, forcing the electron current deeper and deeper into the structure.
[0077] 1-4 has a peripheral n-type region and a central p-type region, with a gate contact and cathode associated with the n-type region and an anode associated with the p-type region, but in a further example, the p-type region forms the periphery of the pixel and has the anode and gate contact associated with the anode, and the n-type region provides the central cathode contact. In such a complementary variation, control of the gate voltage also changes lateral carrier injection and the wavelength of light emitted by the light-emitting region.
[0078] The structures described in connection with Figures 1-4 can be implemented in an array of monolithically grown native LEDs to provide multicolor light output for pixels, each capable of emitting light at a different voltage-controllable wavelength. Such structures advantageously provide micro LED structures for high-resolution emissive displays.
[0079] While the use of n-type and p-type material formed into a channel through multiple light-emitting regions of different wavelengths can be used to provide pixels having a light-emitting surface defined by one of the n-type and p-type regions to electrically isolate the pixel, in further examples, different arrangements of n-type and p-type regions through multiple light-emitting regions of different wavelengths are used. Examples of different implementations are described in relation to Figures 5 and 6.
[0080] FIG. 5 illustrates an epitaxial structure including the layers described in connection with the epitaxial structure 100A of FIG. 1A. The epitaxial structure of FIG. 1A is shown patterned and etched to provide a mesa 500 having a periphery 502. The mesa 500 has a cross-sectional shape as shown in plan view 500A of FIG. 5B. The epitaxial structure 100A of FIG. 1A can be etched to provide multiple mesas, as shown in FIG. 5C, with mesas 502A-502G shown to provide a display. By providing channels / vias in the mesas and then overgrowing p-type and n-type materials, a light-emitting structure can be formed that can be used to control the voltage of an epitaxial stack of monolithic native multicolor LED layers in a manner similar to that described in connection with FIGS. 1-4.
[0081] FIG. 6A shows a cross-sectional view of structure 600A, in which the mesa 500 structure of FIG. 5A has been processed to provide an n-type region 602 in the channel through light emitting regions 112, 116, and 120 and a p-type region 604 in the channel through light emitting regions 112, 116, and 120. In the example of FIG. 6A, n-type region 602 and p-type region 604 through light emitting regions 112, 116, and 120 are formed in appropriate locations within the mesa depending on the desired light emission. However, in further examples, p-type region 604 and n-type region 602 are formed in any suitable shape, size, and location to provide the desired light emission. For example, one of p-type region 604 and n-type region 602 forms the periphery of the mesa structure. When appropriate anode, cathode, and gate contacts are formed, light emission can be controlled by varying the voltage applied to the gate contact in a manner similar to that described in connection with FIGS. 1-4.
[0082] 6B shows a top view 600B of an anode contact 606 associated with p-type region 604 and a gate contact 608, including a dielectric region, associated with n-type region 602. A cathode contact is formed on the top or bottom of the structure, as appropriate. Light emission is controlled in region 612 between p-type region 604 and n-type region 602 by lateral carrier injection and radiative recombination in light emitting regions 112, 116, 120, as indicated by arrows 610.
[0083] In a further example, the use of n-type and p-type regions 602, respectively, through the light emitting regions 112, 116, 120 of an epitaxially grown structure, such as structure 100A of FIG. 1A, along with appropriate anode, cathode, and gate contacts, provides voltage-controllable wavelength-dependent light emission without forming mesa 500. In such an example, pairs of n-type and p-type regions through the light emitting region are used such that each pair is spaced far enough apart to provide localized light emission in a controlled manner. will be done.
Claims
1. A p-type region; an n-type region; A gate contact; a first light emitting region for recombination of carriers injectable by the p-type region and the n-type region; a second light emitting region for recombination of carriers injectable by the p-type region and the n-type region, the first light emitting region and the second light emitting region at least partially overlapping to form a light emitting surface associated with the first light emitting region and the second light emitting region, light emitted from the first light emitting region having a different primary peak wavelength compared to light emitted from the second light emitting region, the first light emitting region and the second light emitting region being separated by an undoped region; and A light emitting diode device comprising:
11. A light emitting diode device, comprising: a first light emitting region and a second light emitting region, the first light emitting region and the second light emitting region being electrically connected to a first gate electrode and a second gate electrode and the second gate electrode being electrically connected to the first ... second gate electrode and the
2. 2. The light emitting diode device of claim 1, comprising: a third light emitting region at least partially overlapping the first and second light emitting regions to form the light emitting surface, the second and third light emitting regions being separated by an undoped region separate from the undoped region, the p-type region being formed at least partially in the first channel through the third light emitting region and the n-type region being formed at least partially in the second channel through the third light emitting region, the light emitting diode device being configured to enable a wavelength of light emitted by the light emitting surface to be controllable by varying a gate voltage applied to at least one of the p-type and n-type regions by the gate contact to vary carrier injection by the p-type and n-type regions into the first, second and third light emitting regions.
3. 3. A light emitting diode device according to claim 1 or 2, wherein the first channel or the second channel is a via that at least partially defines a periphery of the light emitting surface.
4. 4. A light emitting diode device according to claim 1, wherein the light emitting diode device is configured to vary a depletion depth in the first channel or the second channel by varying the gate voltage.
5. 3. The light emitting diode device of claim 2, comprising an epitaxial crystalline semiconductor structure, wherein at least one of the first light emitting region, the second light emitting region, and the third light emitting region includes one or more epitaxial crystalline semiconductor layers, preferably wherein at least one of the first light emitting region, the second light emitting region, and the third light emitting region includes at least one epitaxial quantum well layer.
6. The light emitting diode device of any one of claims 1 to 5, wherein the p-type region or the n-type region comprises a planar layer.
7. 7. A light emitting diode device according to any one of claims 1 to 6, wherein the gate contact is a ring contact corresponding to a pixel defined by the light emitting surface, preferably the ring contact forming either a polygonal or a circular shaped contact.
8. An array of light emitting diode devices comprising a plurality of light emitting diode devices according to any one of claims 1 to 7.
9. 9. The array of light emitting diode devices of claim 8 comprising a plurality of pixels, said pixels corresponding to light emitting surface areas of light emitting diode devices.
10. 10. The array of light emitting diode devices of claim 9, wherein the p-type region or the n-type region of at least two light emitting diode devices of the plurality of light emitting diode devices is shared to form a common electrode.
11. 11. The array of light emitting diode devices of claim 10, wherein the common electrode is on an opposite side of the array from the gate contact.
12. A p-type region; an n-type region; A gate contact; a first light emitting region for recombination of carriers injectable by the p-type region and the n-type region; a second light emitting region for recombination of carriers injectable by the p-type region and the n-type region, the first light emitting region and the second light emitting region at least partially overlapping to form a light emitting surface associated with the first light emitting region and the second light emitting region, light emitted from the first light emitting region having a different primary peak wavelength than light emitted from the second light emitting region, and the first light emitting region and the second light emitting region being separated by an undoped region; 11. A method of forming a light emitting diode device, comprising: forming the p-type region at least partially in a first channel through the first light emitting region and the second light emitting region; and forming the n-type region at least partially in a second channel through the first light emitting region and the second light emitting region; the device is configured to enable control of the wavelength of light emitted by the light emitting surface by varying a gate voltage applied to one of the p-type and n-type regions by the gate contact to vary carrier injection by the p-type and n-type regions into the first and second light emitting regions.
13. 13. The method of claim 12, comprising forming a third light emitting region at least partially overlapping the first and second light emitting regions to form the light emitting surface, the second and third light emitting regions being separated by an undoped region separate from the undoped region, at least partially forming the p-type region in the first channel through the third light emitting region, and at least partially forming the n-type region in the second channel through the third light emitting region, wherein the light emitting diode device is configured to enable a wavelength of light emitted by the light emitting surface to be controllable by varying a gate voltage applied to one of the p-type and n-type regions by the gate contact to vary carrier injection by the p-type and n-type regions into the first, second and third light emitting regions.
14. 14. The method of claim 12 or 13, comprising forming the first channel or the second channel as a via that at least partially defines a periphery of the light emitting surface.
15. 14. The method of claim 13, comprising forming an epitaxial crystalline semiconductor structure, wherein at least one of the first light emitting region, the second light emitting region, and the third light emitting region comprises one or more epitaxial crystalline semiconductor layers, and preferably at least one of the first light emitting region, the second light emitting region, and the third light emitting region comprises at least one epitaxial quantum well layer.
16. 16. A method according to any one of claims 12 to 15, comprising forming the gate contact as a ring contact corresponding to a pixel defined by the light emitting surface, preferably the ring contact forming either a polygonal or circular shaped contact.
17. A method of forming an array of light emitting diode devices comprising a plurality of light emitting diode devices according to any one of claims 12 to 16.
18. 20. A method for forming an array of light emitting diode devices according to claim 17, comprising forming a plurality of pixels, said pixels corresponding to light emitting surface areas of a light emitting diode device.
19. 20. The method for forming an array of light emitting diode devices of claim 18, wherein the p-type region or the n-type region of at least two light emitting diode devices of the plurality of light emitting diode devices is shared to form a common electrode.
20. 20. A method for forming an array of light emitting diode devices according to claim 19 including forming the common electrode on an opposite side of the array from the gate contact.