Living room facility

By using circularly polarized light and a 1/4λ plate with optically anisotropic films, the display light leakage issue is resolved, enhancing privacy and safety in vehicles by reducing external visibility of display content.

JP2024133991AInactive Publication Date: 2024-10-03FUJIFILM CORP

Patent Information

Application Number
JP2023044048
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-20
Publication Date
2024-10-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The issue of display light leakage from vehicles, particularly from rear seats, which compromises privacy and poses a safety risk by distracting other drivers, is not adequately addressed by existing technologies.

Method used

The implementation of living room equipment with a display that emits circularly polarized light and a window equipped with a linear polarizing plate and a 1/4λ plate, composed of optically anisotropic films, to absorb circularly polarized light, thereby reducing light leakage to the outside.

Benefits of technology

This configuration effectively blocks light leakage from the display to the outside, ensuring privacy and safety by minimizing light emission from various viewing angles, even when the positional relationship between the display and window changes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133991000001_ABST
    Figure 2024133991000001_ABST
Patent Text Reader

Abstract

To provide a living room facility capable of securing privacy of a living room by suitably shielding display light even from various observation angles.SOLUTION: A living room facility including: a display configured to emit light from a display surface; and a window facing outside a room, in which an emission amount I1 of the light from the display surface of the window is smaller than an incident amount I2 of the light from the display surface of the window, and light leakage of the light to outside the room is prevented.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] To provide a room facility that improves privacy by preventing the display light and contents of a display in a room from being seen from outside the room, while allowing a user to see the outside from inside the room through a window with sufficient brightness. [Background technology]

[0002] The introduction of thin and lightweight displays into automobiles is progressing due to both the evolution of displays such as LCD and OLED, and improvements in technology to make the interior of automobiles more comfortable. In addition to replacing car navigation systems and instrument panel instruments, displays for passengers have been introduced in recent years, and displays for rear seats in particular are becoming larger.

[0003] As a result, the display light and contents can easily be seen from outside the vehicle, which is becoming a problem in terms of privacy. Furthermore, the light from such displays distracts other drivers, creating an undesirable situation in terms of safe driving.

[0004] From the viewpoint of preventing light leakage from inside the room, although it is not directly related to display light, Patent Document 1 discloses an indoor equipment using a reflective polarizer and a circularly polarized light source, but the reflected light intensity from the window increases on both the inside and outside of the room, making it look like a mirror, which is not desirable from a design perspective and is a matter of personal preference. Also, when viewed from an oblique direction to the normal direction of the window, the 1 / 4λ condition is not met, so circular polarization compensation is not performed and a lot of light leakage is observed. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2011-144511 A Summary of the Invention [Problem to be solved by the invention]

[0006] The problem to be solved by the present invention is to provide a room equipment that can suitably block display light from various observation angles and ensure privacy in the room. [Means for solving the problem]

[0007] That is, the present inventors have found that the above problems can be solved by the following configuration.

[0008] [1] A room facility having a display that emits light from a display surface and a window facing the outside of the room, wherein the amount of light emitted from the display surface I2 is smaller than the amount of light incident from the display surface I1, thereby preventing leakage of the light to the outside of the room. [2] The room equipment according to [1], wherein the light emitted from the display is circularly polarized light, and the window is laminated with at least a linear polarizer and a 1 / 4λ plate to absorb the circularly polarized light from the display. [3] The room equipment according to [1] or [2], wherein the 1 / 4λ plate is a laminate composed of multiple optically anisotropic films. [4] The room equipment according to any one of [1] to [3], wherein at least one of the plurality of optically anisotropic films is made of a liquid crystal material with a fixed orientation. [5] The room equipment according to any one of [1] to [4], wherein the room equipment is an automobile interior equipment. [6] The interior equipment of an automobile, the display being a passenger-oriented display arranged behind the driver's seat, and the window being a rear side and / or rear window. The interior equipment of an automobile, as described in [5]. Effect of the Invention

[0009] According to the present invention, it is possible to provide room equipment that can block light leakage to the outside through a display window installed indoors, in particular room equipment that can effectively suppress light leakage in various directions and is also effective for installation in a vehicle. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic cross-sectional view of an embodiment of a room facility of the present invention. [Diagram 2] FIG. 1 is a schematic diagram showing a mechanism for preventing light leakage in a room facility of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The present invention will be described in detail below. The following description of the components may be based on representative embodiments of the present invention, but the present invention is not limited to such embodiments. In this specification, a numerical range expressed using "to" means a range that includes the numerical values ​​before and after "to" as the lower and upper limits. In the present specification, each component may be used alone or in combination of two or more substances corresponding to each component. When two or more substances are used in combination for each component, the content of the component refers to the total content of the substances used in combination, unless otherwise specified. In addition, in this specification, "(meth)acrylic" is a notation representing "acrylic" or "methacrylic", and "(meth)acryloyl" is a notation representing "acryloyl" or "methacryloyl". Next, the terms used in this specification will be explained.

[0012] In this specification, the slow axis is defined at 550 nm unless otherwise specified.

[0013] In this specification, Re(λ) and Rth(λ) respectively represent the in-plane retardation and the retardation in the thickness direction at a wavelength λ. Unless otherwise specified, the wavelength λ is 550 nm. In the present invention, Re(λ) and Rth(λ) are values ​​measured at a wavelength λ using an AxoScan (manufactured by Axometrics). By inputting the average refractive index ((nx+ny+nz) / 3) and the film thickness (d(μm)) into AxoScan, Slow axis direction (°) Re(λ) = R0(λ) Rth(λ)=((nx+ny) / 2-nz)×d is calculated. Note that R0(λ) is displayed as a numerical value calculated by AxoScan, but it means Re(λ).

[0014] In this specification, the refractive indices nx, ny, and nz are measured using an Abbe refractometer (NAR-4T, manufactured by Atago Co., Ltd.) and a sodium lamp (λ=589 nm) as a light source. In addition, when measuring wavelength dependency, it can be measured using a multi-wavelength Abbe refractometer DR-M2 (manufactured by Atago Co., Ltd.) in combination with an interference filter. In addition, values ​​from the Polymer Handbook (JOHN WILEY & SONS, INC.) and catalogs of various optical films can be used. The average refractive index values ​​of major optical films are shown below as examples: cellulose acylate (1.48), cycloolefin polymer (1.52), polycarbonate (1.59), polymethyl methacrylate (1.49), and polystyrene (1.59).

[0015] In this specification, the term "light" refers to actinic rays or radiation, such as the bright line spectrum of a mercury lamp, far ultraviolet rays represented by an excimer laser, extreme ultraviolet rays (EUV light: extreme ultraviolet), X-rays, ultraviolet rays, and electron beams (EB), etc. Among these, ultraviolet rays are preferred.

[0016] In this specification, the term "visible light" refers to light having a wavelength of 380 to 780 nm. In addition, in this specification, unless otherwise specified, the measurement wavelength is 550 nm. In this specification, the angular relationship (e.g., "perpendicular", "parallel", etc.) is assumed to include the range of error permitted in the technical field to which the present invention pertains. Specifically, this means that the angle is within a range of less than ±10° from the exact angle, and the error from the exact angle is preferably within a range of ±5° or less, and more preferably within a range of ±3° or less.

[0017] In this specification, the horizontal alignment of rod-like liquid crystal compounds refers to a state in which the major axes of the liquid crystal compounds are aligned parallel to and in the same direction as the layer surface. Here, "horizontal" does not necessarily mean strictly horizontal, but means an orientation in which the inclination angle between the average molecular axis of the liquid crystal compound in the layer and the layer surface is less than 20°. In addition, the same orientation does not require the orientation to be strictly the same, but rather means that when the orientations of the slow axes are measured at any 20 positions within the plane, the maximum difference between the slow axis orientations at the 20 positions (the difference between the two slow axis orientations with the largest difference among the 20 slow axis orientations) is less than 10°. The vertical alignment of a discotic liquid crystal compound refers to a state in which the disc axis of the liquid crystal compound is aligned perpendicular to and in the same direction as the layer surface. Here, the term "vertical" does not necessarily mean strictly vertical, but means an orientation in which the inclination angle between the disc plane of the liquid crystal compound in the layer and the layer surface is 70 to 110°. In addition, the same orientation does not require the orientation to be strictly the same, but rather means that when the orientations of the slow axes are measured at any 20 positions within the plane, the maximum difference between the slow axis orientations at the 20 positions (the difference between the two slow axis orientations with the largest difference among the 20 slow axis orientations) is less than 10°.

[0018] In this specification, the optically anisotropic layer refers to a layer in which aligned liquid crystal compounds are fixed. The "fixed" state is a state in which the alignment of the liquid crystal compound is maintained. Specifically, it is more preferable that the layer has no fluidity in a temperature range of usually 0 to 50° C., or under more severe conditions, −30 to 70° C., and that the alignment state is not changed by an external field or external force, and the fixed alignment state can be stably maintained.

[0019] [Prevents light leakage from the display] The living room equipment of the present invention has a display that emits light from its display surface and a window facing the outside of the living room, and the window has a smaller amount of light emitted I2 from the display surface than the amount of light incident I1 from the display surface, thereby preventing leakage of the light to the outside of the room. The room equipment of the present invention preferably comprises a display that emits circularly polarized light and a window that absorbs this circularly polarized light. This is preferable not only in an arrangement in which the normal direction of the display surface coincides with the normal direction of the window surface (one example is the rear display and rear window of an automobile interior equipment), but also in an arrangement in which the angle between the normal directions of the two is large (one example is the rear display and rear side window of an automobile interior equipment), as this can effectively suppress leakage of display light outside the passenger compartment. An example of interior equipment in which the relative angles of components change due to a display whose position and tilt angle change and a window that is not vertical is equipment inside an automobile.

[0020] [Suitable usage form] By sequentially laminating a linear polarizing plate and a 1 / 4 λ plate on the display surface side, the light emitted from the display can be made circularly polarized, which is preferable. If the display is a liquid crystal display or an organic EL display, this can also serve as the polarizing plate on the display surface side of the display. The viewer will see circularly polarized light instead of linearly polarized light, but the amount of light hardly changes, so it can be viewed in the same way as a conventional display. On the other hand, it is preferable to place a 1 / 4 λ plate on the window side at an axial angle that absorbs the circularly polarized light emitted from the display, thereby preventing light leakage to the outside. Specifically, when right (or left) circularly polarized light is emitted from the display, a left (or right) circular polarizing plate is placed on the window. More specifically, it is preferable that the absorption axis of the polarizing plate placed on the display and the window, respectively, and the in-plane slow axis of the component of the 1 / 4 λ plate are shifted by 90°. It is preferable to use an absorption type system, particularly a specific optical configuration in which a plurality of retardation plates are combined, since this makes it possible to effectively block light leakage even if the positional relationship between the display / window / observer changes. The window has an amount λ2 of light exiting from the display surface of the display that is smaller than an amount λ1 of light entering from the display surface of the display. λ2 / λ1 is preferably 0.1 or less, and more preferably 0.05 or less. The room equipment of the present invention can also be used with displays that do not emit polarized light, such as LEDs, but the amount of light is reduced by approximately half due to the polarizing plate placed on the display side.

[0021] From the viewpoint of reducing light leakage from displays, it is possible to increase the density of existing dark-tinted glass. However, in order to achieve compatibility with the original function of windows, which is to allow for a view of the outside and to check the surroundings, it is preferable to reduce the density of the dark-tinted glass.

[0022] [Polarizer] The polarizer of the display and the window may be any member capable of converting natural light into a specific linearly polarized light, and may be, for example, an absorptive polarizer. The type of polarizer is not particularly limited, and any commonly used polarizer can be used, such as an iodine-based polarizer, a dye-based polarizer using a dichroic dye, and a polyene-based polarizer. Iodine-based polarizers and dye-based polarizers are generally produced by adsorbing iodine or a dichroic dye to polyvinyl alcohol and stretching it. A protective film may be disposed on one or both sides of the polarizer.

[0023] In addition, as described in WO 2019 / 131943 and JP 2017-83843 A, a coating-type polarizer produced by coating a liquid crystal compound and a dichroic organic dye (for example, a dichroic azo dye used in the light-absorbing anisotropic film described in WO 2017 / 195833 A) without using polyvinyl alcohol as a binder may be used as the polarizer. In other words, the polarizer may be a polarizer formed using a composition containing a polymerizable liquid crystal compound. This coating type polarizer is a technology that utilizes the orientation of a liquid crystal compound to orient a dichroic organic dye. As described in JP 2012-83734 A, it is preferable for the polymerizable liquid crystal compound to exhibit smectic properties in terms of increasing the degree of orientation. Alternatively, as described in WO 2018 / 186503 A, it is also preferable to crystallize the dye in terms of increasing the degree of orientation. WO 2019 / 131943 A describes a structure of a polymer liquid crystal that is preferable for increasing the degree of orientation.

[0024] A polarizer in which a dichroic organic dye is oriented by utilizing the orientation of liquid crystals without stretching has the following characteristics: It has many advantages, such as the ability to make the layer extremely thin, at around 0.1 μm to 5 μm, the fact that cracks are unlikely to occur when the layer is bent and thermal deformation is small, as described in JP 2019-194685 A, and the fact that polarizers with high transmittance exceeding 50% have excellent durability, even in such polarizing plates, as described in JP 6483486 A. Taking advantage of these advantages, the film can be used in applications requiring high brightness, small size and light weight, fine optical systems, molding onto curved surfaces, and flexible surfaces. Of course, the film can also be used by peeling off the support and transferring the polarizer.

[0025] The configuration of the polarizer protective film is not particularly limited, and may be, for example, a transparent support or a coating layer, or may be a laminate of a transparent support and a coating layer. The coating layer may be a known layer, for example, a layer obtained by polymerizing and curing a polymer or a polyfunctional monomer. Examples of the polymer include (meth)acrylic polymers and cycloolefin polymers. Examples of the polymerizable monomer include radically polymerizable or cationic polymerizable compounds. The bonding surface between the polarizer and the protective film is not particularly limited. For example, the coating layer side of the transparent support and the coating layer may be bonded to the polarizer for the purpose of suppressing diffusion of potassium ions or iodine ions from the polarizer over time under moist heat conditions.

[0026] [1 / 4λ plate] The quarter plate may be a stretched polymer film or an optically anisotropic film in which a liquid crystal compound is fixed. Any polymer film is preferably used as long as it is made of a material having excellent transparency and inherent birefringence, and examples of such materials include general-purpose polymers such as PMMA, polycarbonate, polystyrene, polyester, polyolefin, polycycloolefin, polyethylene, polysulfone, and polyethersulfone. These films can be used by adjusting the stretching ratio so that the desired birefringence value is in the vicinity of 1 / 4λ. In addition, in order to reduce the viewing angle dependency, it is also effective to perform biaxial stretching in the in-plane or thickness direction. Furthermore, it is also possible to use an organized polymer in which the side chain structure is modified so that optical expression occurs in the direction perpendicular to the main chain by stretching, thereby controlling the refractive index in the three-dimensional direction and the wavelength dependency of the birefringence.

[0027] [Optically anisotropic film formed by fixing liquid crystal compounds] The optically anisotropic film constituting the ¼ λ plate of the present invention has an optically anisotropic layer in which an oriented liquid crystal compound is fixed. Here, liquid crystal compounds can be classified into rod-shaped and disc-shaped types based on their shape. Furthermore, each type can be classified into low molecular weight and high molecular weight types. High molecular weight generally refers to a compound with a degree of polymerization of 100 or more (Polymer Physics, Phase Transition Dynamics, Masao Doi, p. 2, Iwanami Shoten, 1992). In the present invention, any liquid crystal compound can be used, but rod-shaped or discotic liquid crystal compounds (discotic liquid crystal compounds) are preferred. Furthermore, liquid crystal compounds that are monomers or have a relatively low molecular weight with a degree of polymerization of less than 100 are preferred. In addition, from the viewpoint of fixing the alignment, it is preferable that the liquid crystal compound has a polymerizable group. Examples of such a polymerizable group include an acryloyl group, a methacryloyl group, an epoxy group, and a vinyl group. In the following, a liquid crystal compound having a polymerizable group is abbreviated to "polymerizable liquid crystal compound". By polymerizing such a polymerizable liquid crystal compound, the alignment of the liquid crystal compound can be fixed. After the liquid crystal compound is fixed by polymerization, it is no longer necessary for the liquid crystal compound to exhibit liquid crystallinity.

[0028] As the rod-shaped liquid crystal compound, azomethines, azoxys, cyanobiphenyls, cyanophenyl esters, benzoic acid esters, cyclohexane carboxylic acid phenyl esters, cyanophenylcyclohexanes, cyano-substituted phenylpyrimidines, alkoxy-substituted phenylpyrimidines, phenyldioxanes, tolanes, and alkenylcyclohexylbenzonitriles are preferably used. These rod-shaped liquid crystal compounds are fixed by introducing a polymerizable group into the end structure of the rod-shaped liquid crystal compound (similar to the discotic liquid crystal described later), and utilizing the polymerization and curing reaction. As a specific example, an example in which a polymerizable nematic rod-shaped liquid crystal compound is cured with ultraviolet light is described in JP-A-2006-209073. In addition to the above-mentioned low molecular weight liquid crystal compounds, polymeric liquid crystal compounds can also be used. Polymeric liquid crystal compounds are polymers having side chains corresponding to the above-mentioned low molecular weight liquid crystal compounds. An optical compensation sheet using a polymeric liquid crystal compound is described in JP-A-5-53016 and the like.

[0029] Examples of discotic liquid crystal compounds include benzene derivatives described in the research report by C. Destrade et al., Mol. Cryst., Vol. 71, p. 111 (1981), truxene derivatives described in the research report by C. Destrade et al., Mol. Cryst., Vol. 122, p. 141 (1985), and Physicslett, A, Vol. 78, p. 82 (1990), cyclohexane derivatives described in the research report by B. Kohne et al., Angew. Chem., Vol. 96, p. 70 (1984), and azacrown and phenylacetylene macrocycles described in the research report by JM Lehn et al., J. Chem. Commun., p. 1794 (1985), and the research report by J. Zhang et al., J. Am. Chem. Soc., Vol. 116, p. 2655 (1994).

[0030] The molecules of the discotic liquid crystal compound include compounds that exhibit liquid crystallinity in which linear alkyl groups, alkoxy groups, and substituted benzoyloxy groups are substituted radially as side chains of the mother nucleus at the center of the molecule. It is preferable that the molecule or the molecular aggregate is a compound that has rotational symmetry and can impart a certain orientation. The retardation layer formed from a composition containing a discotic liquid crystal compound does not need to exhibit liquid crystallinity when it is finally included in the retardation layer. For example, when a low-molecular discotic liquid crystal molecule having a group that reacts with heat or light is polymerized by heating or light irradiation to increase the molecular weight, it loses liquid crystallinity, but the retardation layer containing such a high-molecular compound can of course be used in the present invention. Preferred examples of the discotic liquid crystal compound include the compounds described in JP-A-8-50206. In addition, the polymerization of discotic liquid crystal molecules is described in JP-A-8-27284.

[0031] In order to fix the discotic liquid crystal molecules by polymerization, it is necessary to bond a polymerizable group as a substituent to the discotic core of the discotic liquid crystal molecule. The discotic core and the polymerizable group are preferably bonded to a compound via a linking group, which allows the alignment state to be maintained even during the polymerization reaction. For example, the compounds described in paragraphs

[0151] to

[0168] of JP-A-2000-155216 can be mentioned.

[0032] In terms of improving light leakage from oblique directions, it is preferable for an optically anisotropic film made of a liquid crystal compound to exhibit the function of a 1 / 4λ plate as a whole as a laminate consisting of two or more optically anisotropic films, rather than as a single layer. In the case of a two-layer structure, the in-plane retardation at a wavelength of 550 nm of the first optically anisotropic film closer to the polarizer is preferably from 200 to 280 nm, more preferably from 210 to 250 nm. In the present invention, the angle between the in-plane slow axis of the first optically anisotropic film and the absorption axis or transmission axis of the polarizer is preferably from 50 to 85°, more preferably from 65 to 85°. The in-plane retardation at a wavelength of 550 nm of the second optically anisotropic film farther from the polarizer is preferably from 100 to 180 nm, more preferably from 100 to 150 nm. In the present invention, the angle between the in-plane slow axis of the first optically anisotropic film and the absorption axis or transmission axis of the polarizer is preferably from 5 to 40°, more preferably from 5 to 25°. The liquid crystal materials constituting the first and second optically anisotropic films can be either rod-shaped liquid crystals or discotic liquid crystals, and when combining the two, it is preferable to use discotic liquid crystals for the first optically anisotropic film and rod-shaped liquid crystals for the second optically anisotropic film.

[0033] In order to improve the color seen from an oblique direction, it is also preferable to add a layer in which a positive or negative C plate or a twisted nematic alignment is fixed. It is also preferable to use a liquid crystal material or composition with so-called reverse wavelength dispersion, in which the in-plane retardation increases with increasing wavelength.

[0034] A preferred example of the former is a configuration in which a negative A plate made of discotic liquid crystal, a layer in which a twisted rod-shaped liquid crystal compound is fixed, and a positive C plate made of rod-shaped liquid crystal are sequentially laminated from the side closer to the polarizer. The in-plane retardation of the negative A plate at a wavelength of 550 nm is preferably 140 to 220 nm, and more preferably 150 to 200 nm. The angle between the in-plane slow axis of the negative A plate and the absorption axis or transmission axis of the polarizer is preferably 40 to 85°, more preferably 50 to 85°, and even more preferably 65 to 85°.

[0035] The value of the product Δnd of the refractive index anisotropy Δn of the optically anisotropic layer (B) in which the twisted and aligned rod-like liquid crystal compound is fixed at a wavelength of 550 nm and the thickness d of the optically anisotropic layer (B) is preferably 140 to 220 nm, more preferably 150 to 210 nm, and even more preferably 160 to 200 nm, in terms of suppressing black coloring. The twist angle of the liquid crystal compound (twist angle of the alignment direction of the liquid crystal compound) is preferably 90±30° (within the range of 60 to 120°), more preferably 90±20° (within the range of 70 to 110°), and even more preferably 90±10° (within the range of 80 to 100°), in terms of suppressing black coloring. The torsion angle is measured using an AxoScan (polarimeter) device manufactured by Axometrics Inc. and the device analysis software of the same company.

[0036] The in-plane retardation of the positive C plate at a wavelength of 550 nm is preferably from 0 to 10 nm, and more preferably from 0 to 5 nm. The retardation in the thickness direction of the positive C plate at a wavelength of 550 nm is preferably −120 to −20 nm, more preferably −110 to −30 nm, and still more preferably −100 to −40 nm.

[0037] [substrate] In the present invention, a substrate may be used for forming the 1 / 4 λ plate or for protecting it. The substrate is preferably a transparent substrate. The transparent substrate refers to a substrate having a visible light transmittance of 60% or more, preferably 80% or more, and more preferably 90% or more.

[0038] The retardation value (Rth(550)) in the thickness direction of the substrate at a wavelength of 550 nm is not particularly limited, but is preferably −110 to 110 nm, more preferably −80 to 80 nm. The in-plane retardation value (Re(550)) of the substrate at a wavelength of 550 nm is not particularly limited, but is preferably 0 to 50 nm, more preferably 0 to 30 nm, and further preferably 0 to 10 nm.

[0039] The material for forming the substrate is preferably a polymer having excellent optical properties such as transparency, mechanical strength, thermal stability, moisture barrier properties, and isotropy. Examples of polymer films that can be used as the substrate include cellulose acylate films (e.g., cellulose triacetate film (refractive index 1.48), cellulose diacetate film, cellulose acetate butyrate film, and cellulose acetate propionate film), polyolefin films such as polyethylene and polypropylene, polyester films such as polyethylene terephthalate and polyethylene naphthalate, polyethersulfone films, polyacrylic films such as polymethyl methacrylate, polyurethane films, polycarbonate films, polysulfone films, polyether films, polymethylpentene films, polyether ketone films, (meth)acrylonitrile films, and films of polymers having an alicyclic structure (norbornene-based resins (Arton: product name, manufactured by JSR Corporation, and amorphous polyolefins (Zeonex: product name, manufactured by Zeon Corporation)). Among these, the material for the polymer film is preferably triacetyl cellulose, polyethylene terephthalate, or a polymer having an alicyclic structure, and more preferably triacetyl cellulose.

[0040] The substrate may contain various additives (for example, an optical anisotropy adjusting agent, a wavelength dispersion adjusting agent, fine particles, a plasticizer, an ultraviolet protection agent, a deterioration inhibitor, a release agent, etc.).

[0041] The thickness of the substrate is not particularly limited, but is preferably 10 to 200 μm, more preferably 10 to 100 μm, and even more preferably 20 to 90 μm. The substrate may be made of a laminate of multiple sheets. In order to improve adhesion with a layer provided thereon, the surface of the substrate may be subjected to a surface treatment (e.g., glow discharge treatment, corona discharge treatment, ultraviolet (UV) treatment, flame treatment). In addition, an adhesive layer (undercoat layer) may be provided on the substrate. In addition, in order to impart slipperiness to the substrate during the transport process and to prevent sticking between the front and back surfaces after winding, a polymer layer containing inorganic particles having an average particle size of about 10 to 100 nm at a solid content ratio of 5 to 40 mass % may be placed on one side of the substrate.

[0042] The substrate may be a so-called temporary support, that is, after the antireflection film of the present invention is produced, the substrate may be peeled off from the optically anisotropic layer.

[0043] [Other functional layers] The display and window of the present invention may be provided with other functional layers such as an anti-reflection layer. In particular, the window surface may be provided with a hard coat layer, a slip layer, an anti-fouling layer, a coloring material (light reducing layer, color tone layer), a UV / IR absorbing layer, a heat shielding layer, etc., as required.

[0044] [Application] The room equipment of the present invention is preferably equipment inside an automobile. By using it as interior equipment for an automobile, it is possible to provide interior equipment that allows good visibility of the outside of the vehicle from inside the vehicle and does not look out of place in the design of the windows when viewed from inside the vehicle, which is preferable. In the case of an in-vehicle device, it is preferable that the display is a passenger-oriented display arranged behind the driver's seat, and the window is a rear side and / or rear window. EXAMPLES

[0045] The features of the present invention will be described in more detail below with reference to examples and comparative examples. The materials, amounts, ratios, processing contents, and processing procedures shown in the following examples can be appropriately changed without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be interpreted as being limited by the specific examples shown below.

[0046] [Example 1] <Preparation of cellulose acylate film (substrate)> The following composition was put into a mixing tank, stirred, and heated at 90°C for 10 minutes. The obtained composition was then filtered through a filter paper with an average pore size of 34 μm and a sintered metal filter with an average pore size of 10 μm to prepare a dope. The solid content concentration of the dope was 23.5% by mass, the amount of the plasticizer added was the ratio relative to the cellulose acylate, and the solvent of the dope was methylene chloride / methanol / butanol = 81 / 18 / 1 (mass ratio).

[0047] ------------------------------------------------------------------ Cellulose Acylate Dope ------------------------------------------------------------------ Cellulose acylate (acetyl substitution degree 2.86, viscosity average polymerization degree 310) 100 parts by mass Sugar ester compound 1 (shown in the following formula (S4)) 6.0 parts by mass Sugar ester compound 2 (shown in the following formula (S5)) 2.0 parts by mass Silica particle dispersion (AEROSIL R972, Nippon Aerosil Co., Ltd.) 0.1 part by mass Solvent (methylene chloride / methanol / butanol) ------------------------------------------------------------------

[0048] [ka]

[0049] [ka]

[0050] The dope prepared above was cast using a drum film-forming machine. The dope was cast from a die onto a metal support cooled to 0° C., and then the obtained web (film) was peeled off. The drum was made of SUS.

[0051] The web (film) obtained by casting was peeled off from the drum, and then dried for 20 minutes in a tenter apparatus, which clips both ends of the web with clips and transports the web at 30 to 40°C during film transport. The web was then post-dried by zone heating while being transported by rolls. The obtained web was knurled and then wound up. The obtained cellulose acylate film had a thickness of 40 μm, an in-plane retardation Re(550) at a wavelength of 550 nm of 1 nm, and a retardation in the thickness direction Rth(550) at a wavelength of 550 nm of 26 nm. (Alkaline saponification treatment) The above-mentioned cellulose acylate film was passed through a dielectric heating roll at a temperature of 60°C to raise the film surface temperature to 40°C, and then an alkaline solution having the composition shown below was applied to the band surface of the film using a bar coater in an amount of 14 ml / m 2 The plate was then conveyed for 10 seconds under a steam-type far-infrared heater manufactured by Noritake Co., Ltd., which had been heated to 110°C. Next, using the same bar coater, pure water was applied at a rate of 3 ml / m 2 Next, the film was washed with water using a fountain coater and then dried with an air knife three times, and then conveyed to a drying zone at 70° C. for 10 seconds to prepare an alkali saponified cellulose acylate film.

[0052] ---------------------------------------------------------------------------------- Alkaline solution ---------------------------------------------------------------------------------- Potassium hydroxide 4.7 parts by mass Water 15.8 parts by mass Isopropanol 63.7 parts by weight Surfactant: C 14 H 29 O(CH2CH2O) 20 H 1.0 parts by mass Propylene glycol 14.8 parts by weight ----------------------------------------------------------------------------------

[0053] <Formation of alignment film 1> An alignment layer coating solution having the following composition was continuously coated on the alkaline saponified surface of the cellulose acylate film using a wire bar #14, and then dried with hot air at 60° C. for 60 seconds and then with hot air at 100° C. for 120 seconds.

[0054] ---------------------------------------------------------------------------------- Alignment film coating solution ---------------------------------------------------------------------------------- 10 parts by weight of the following polyvinyl alcohol Water 371 parts by mass Methanol 119 parts by weight Glutaraldehyde (crosslinking agent) 0.5 parts by weight Citric acid ester (manufactured by Sankyo Chemical Co., Ltd.) 0.175 parts by mass ----------------------------------------------------------------------------------

[0055] Polyvinyl alcohol [ka]

[0056] <Formation of Optically Anisotropic Layer (A)> The above-prepared alignment film was subjected to continuous rubbing treatment. At this time, the longitudinal direction of the long film was parallel to the transport direction, and the angle between the longitudinal direction of the film (transport direction) and the rotation axis of the rubbing roller was 76°. The longitudinal direction of the film (transport direction) was set to 90°, and when observed from the film side, the film width direction was taken as the reference (0°) and the clockwise direction was expressed as a positive value, so the rotation axis of the rubbing roller was at -14°. In other words, the position of the rotation axis of the rubbing roller was rotated 76° counterclockwise with the longitudinal direction of the film as the reference.

[0057] On the above-mentioned rubbed alignment film, an optically anisotropic layer coating solution (1a) containing a discotic liquid crystal compound of the following composition was applied using a Giesser coater to form a composition layer. The obtained composition layer was then heated with hot air at 110°C for 2 minutes to dry the solvent and ripen the alignment of the discotic liquid crystal compound. The obtained composition layer was then irradiated with UV light (500 mJ / cm2) at 80°C. 2 ) was carried out to fix the alignment of the liquid crystal compound, thereby forming an optically anisotropic layer (1a) corresponding to the optically anisotropic layer (A). The thickness of the optically anisotropic layer (1a) was 1.5 μm. The retardation at 550 nm was 168 nm. The average inclination angle of the discotic surface of the discotic liquid crystal compound with respect to the film surface was 90°, and it was confirmed that the compound was aligned perpendicular to the film surface. The angle of the slow axis of the optically anisotropic layer (1a) was parallel to the rotation axis of the rubbing roller, and the slow axis was -14° when viewed from the optically anisotropic layer (1a) side, assuming that the width direction of the film is 0° (the longitudinal direction is 90° counterclockwise and -90° clockwise).

[0058] ---------------------------------------------------------------------------------- Composition for forming optically anisotropic layer (1a) ---------------------------------------------------------------------------------- 80 parts by weight of the following discotic liquid crystal compound 1 20 parts by weight of the following discotic liquid crystal compound 2 0.55 parts by weight of the following alignment film interface alignment agent 1 0.1 parts by mass of the following fluorine-containing compound A 0.05 parts by mass of the following fluorine-containing compound B 0.21 parts by mass of the following fluorine-containing compound C Ethylene oxide modified trimethylolpropane triacrylate (V#360, manufactured by Osaka Organic Chemical Co., Ltd.) 10 parts by mass Photopolymerization initiator (Irgacure 907, manufactured by BASF) 3.0 parts by mass Methyl ethyl ketone 200 parts by mass ----------------------------------------------------------------------------------

[0059] Discotic Liquid Crystal Compound 1 [ka]

[0060] Discotic Liquid Crystal Compound 2 [ka]

[0061] Alignment film interface alignment agent 1 [ka]

[0062] Fluorine-containing compound A (in the following formula, a and b represent the content (mass%) of each repeating unit relative to all repeating units, where a represents 90 mass% and b represents 10 mass%). [ka]

[0063] Fluorine-containing compound B (The numerical value in each repeating unit indicates the content (mass%) relative to all repeating units.) [ka]

[0064] Fluorine-containing compound C (the numerical value in each repeating unit indicates the content (mass%) relative to all repeating units.) [ka]

[0065] <Formation of a laminate of the optically anisotropic layer (C) and the optically anisotropic layer (B)> (Formation of Optically Anisotropic Layer (1c)) On the cellulose acylate film prepared above, the optically anisotropic layer coating solution (1c) containing the rod-shaped liquid crystal compound of the following composition was applied using a Giesser coater to form a composition layer. Then, both ends of the film were held, a cooling plate (9°C) was placed on the side of the film on which the coating film was formed so as to be 5 mm away from the film, and a heater (75°C) was placed on the side opposite to the side on which the coating film was formed so as to be 5 mm away from the film, and the film was dried for 2 minutes. Next, the sample was heated to 60°C for 1 minute with hot air, and then irradiated with a 365 nm UV-LED at a dose of 100 mJ / cm while purging with nitrogen to keep the oxygen concentration in the atmosphere at 100 ppm or less. 2 After that, it was annealed with hot air at 120°C for 1 minute to form a precursor layer. The obtained precursor layer was irradiated with UV light (ultra-high pressure mercury lamp; UL750; manufactured by HOYA) at room temperature through a wire grid polarizer at 7.9 mJ / cm. 2 By irradiating the film with light (wavelength: 313 nm), a composition layer having an alignment control ability was formed on the surface. The thickness of the composition layer formed was 0.5 μm. The in-plane retardation Re at a wavelength of 550 nm was 0 nm, and the retardation Rth in the thickness direction at a wavelength of 550 nm was −68 nm. The average tilt angle of the long axis direction of the rod-like liquid crystal compound with respect to the film surface was 90°, and it was confirmed that the compound was aligned perpendicular to the film surface. In this manner, an optically anisotropic layer (1c) corresponding to the optically anisotropic layer (C) was formed.

[0066] ---------------------------------------------------------------------------------- Composition for forming optically anisotropic layer (1c) ---------------------------------------------------------------------------------- 100 parts by weight of the following rod-shaped liquid crystal compound (A) Polymerizable monomer (A-400, manufactured by Shin-Nakamura Chemical Co., Ltd.) 4.0 parts by mass 5.0 parts by mass of the following polymerization initiator S-1 (oxime type) 3.0 parts by weight of the following photoacid generator D-1 2.0 parts by weight of the following polymer M-1 2.0 parts by weight of the vertical alignment agent S01 listed below 2.0 parts by mass of the photo-alignable polymer A-1 shown below Methyl ethyl ketone 42.3 parts by mass Methyl isobutyl ketone 627.5 parts by mass ----------------------------------------------------------------------------------

[0067] Rod-shaped liquid crystal compound (A) (hereinafter, a mixture of compounds) [ka]

[0068] Polymerization initiator S-1 [ka]

[0069] Photoacid generator D-1 [ka]

[0070] Polymer M-1 [ka]

[0071] Vertical alignment agent S01 [ka]

[0072] Photoalignable polymer A-1 (the numerical value in each repeating unit indicates the content (mass%) of each repeating unit relative to the total repeating units, and the repeating units from the left were 40 mass%, 25 mass%, and 35 mass%. The weight average molecular weight was 69,300.) [ka]

[0073] (Formation of Optically Anisotropic Layer (1b)) Next, the optically anisotropic layer coating solution (1b) containing a rod-shaped liquid crystal compound having the following composition was applied onto the optically anisotropic layer (1c) prepared above using a Giesser coater, and heated with hot air at 80°C for 60 seconds. Next, the obtained composition layer was irradiated with UV light (500 mJ / cm2) at 80°C. 2 ) was carried out to fix the alignment of the liquid crystal compound, thereby forming an optically anisotropic layer (1b) corresponding to the optically anisotropic layer (B). The optically anisotropic layer (1b) had a thickness of 1.2 μm, a Δnd at a wavelength of 550 nm of 164 nm, and a twist angle of the liquid crystal compound of 81°. When viewed from the optically anisotropic layer (1b) side, assuming that the width direction of the film is 0° (the longitudinal direction is 90°), the alignment axis angle of the liquid crystal compound was 14° on the air side and 95° on the side in contact with the optically anisotropic layer (1c). The alignment axis angle of the liquid crystal compound contained in the optically anisotropic layer is expressed as negative when clockwise (right-handed) and positive when counterclockwise (left-handed), with the width direction of the substrate being taken as the reference 0°, when observing the substrate from the surface side of the optically anisotropic layer. In addition, the twist angle of the liquid crystal compound is expressed by observing the substrate from the surface side of the optically anisotropic layer, and taking the orientation axis direction of the liquid crystal compound on the surface side (front side) as the reference, when the orientation axis direction of the liquid crystal compound on the substrate side (rear side) is clockwise (right-handed), it is negative, and when it is counterclockwise (left-handed), it is positive.

[0074] ---------------------------------------------------------------------------------- Composition for forming optically anisotropic layer (1b) ---------------------------------------------------------------------------------- 70 parts by mass of the above rod-shaped liquid crystal compound (A) 30 parts by weight of the following rod-shaped liquid crystal compound (B) Ethylene oxide modified trimethylolpropane triacrylate (V#360, manufactured by Osaka Organic Chemical Co., Ltd.) 4 parts by mass Photopolymerization initiator (Irgacure 819, manufactured by BASF) 3 parts by weight 0.50 parts by mass of the following left-twisted chiral agent (L1) 0.20 parts by mass of the following fluorine-containing compound D Methyl isobutyl ketone 126 parts by mass Ethyl propionate 126 parts by mass ----------------------------------------------------------------------------------

[0075] Rod-shaped liquid crystal compound (B) [ka]

[0076] Left-twisted chiral agent (L1) [ka]

[0077] Fluorine-containing compound D (the numerical value in each repeating unit indicates the content (% by mass) relative to all repeating units, the content of the repeating unit on the left side was 76% by mass, and the content of the repeating unit on the right side was 24% by mass.) [ka]

[0078] By the above procedure, a laminate (1c-1b) was prepared in which the optically anisotropic layer (1c) and the optically anisotropic layer (1b) were directly laminated on a long cellulose acylate film. When the surface of the optically anisotropic layer (1c) in contact with the optically anisotropic layer (1b) was confirmed by the above method, the presence of a photoalignable polymer was confirmed.

[0079] <Formation of a laminate of optically anisotropic layer (A), optically anisotropic layer (B) and optically anisotropic layer (C)> The surface side of the optically anisotropic layer (1a) formed on the long-length cellulose acylate film prepared above and the surface side of the optically anisotropic layer (1b) of the laminate (1c-1b) formed on the long-length cellulose acylate film prepared above were bonded to a continuous machine using a 5 μm-thick acrylic adhesive (NCF-D692, manufactured by Lintec Corporation). Then, the cellulose acylate film on the optically anisotropic layer (1a) side was peeled off to expose the surface of the optically anisotropic layer (1a) that had been in contact with the cellulose acylate film. In this manner, an optical film (1c-1b-1a) was obtained in which the optically anisotropic layer (1c), the optically anisotropic layer (1b), and the optically anisotropic layer (1a) were laminated in this order on the long cellulose acylate film.

[0080] <Preparation of Linear Polarizing Plate 1> The surface of the support of cellulose triacetate film TJ25 (manufactured by Fujifilm Corporation: thickness 25 μm) was subjected to an alkali saponification treatment. Specifically, the support was immersed in a 1.5N sodium hydroxide aqueous solution at 55° C. for 2 minutes, then washed in a water washing bath at room temperature, and further neutralized with 0.1N sulfuric acid at 30° C. After neutralization, the support was washed in a water washing bath at room temperature, and further dried with hot air at 100° C. to obtain a polarizer protective film. A rolled polyvinyl alcohol (PVA) film with a thickness of 60 μm was continuously stretched in the longitudinal direction in an iodine aqueous solution and dried to obtain a polarizer with a thickness of 13 μm. The luminous efficiency corrected single transmittance of the polarizer was 43%. At this time, the absorption axis direction of the polarizer coincided with the longitudinal direction. The above polarizer protective film was attached to one surface of the above polarizer using the following PVA adhesive to prepare a linear polarizing plate 1.

[0081] (Preparation of PVA adhesive) A PVA adhesive was prepared by dissolving 100 parts by mass of a polyvinyl alcohol resin having acetoacetyl groups (average degree of polymerization: 1200, degree of saponification: 98.5 mol%, degree of acetoacetylation: 5 mol%) and 20 parts by mass of methylol melamine in pure water at a temperature of 30°C to prepare an aqueous solution with a solids concentration of 3.7% by mass.

[0082] <Creating a window> The surface of the optically anisotropic layer (1a) of the long optical film (1c-1b-1a) and the surface of the polarizer of the long linear polarizing plate (opposite the polarizer protective film) were continuously bonded together using an ultraviolet-curing adhesive. The TJ25 side of the obtained film was bonded to a commercially available glass plate (thickness 2 mm) using a pressure-sensitive adhesive.

[0083] <Creating a display> The surface of the optically anisotropic layer (1a) of the long optical film (1c-1b-1a) prepared above was attached to the polarizing plate surface of a commercially available IPS-liquid crystal display device using a pressure-sensitive adhesive. The optical films D and E were arranged so that the coating directions of the films were perpendicular to the absorption axes of the polarizing plates.

[0084] [Various evaluations] [Display light leakage (Display and window perpendicular (vertical))] Assuming the relative position of the rear display and side window in an in-vehicle application, the normal directions of the display and window were arranged perpendicular to each other, and the display was observed through the window from a position where the observation angle with respect to each plane was 45°, and light leakage was evaluated. The absorption axis of the display's polarizing plate was vertical, and the absorption axis of the window's polarizing plate was horizontal. The white luminance of the display was 200cd / m 2 The environmental brightness was approximately 10 lux. A: The light leakage from the display is so small that it is not visible. B: The light leakage from the display is visible, and the presence of the display is obvious. C: Light leakage from the display is easily visible and the displayed content can be confirmed. A rating of A was judged to be an acceptable level. The results are shown in Table 1.

[0085] [Display light leakage (viewing angle change conditions)] Assuming that the relative position to the car and the display viewing environment would change, we further changed the observation angle from the above evaluation (horizontal: ±20°, vertical: +20 / -10°, display tilt angle: vertical to 20°). A: The light leakage from the display is very small and difficult to see. B: Light leakage from the display increases depending on the angle, but is not noticeable. C: Light leakage increases significantly depending on the angle, or is constantly visible and bothersome D: Light leakage is easily noticeable at any angle and is unacceptable A and B ratings were deemed to be acceptable levels. The results are shown in Table 1.

[0086] [Transmittance] In the present invention, the luminosity-corrected single transmittance of the polarizer is measured using an automatic polarizing film measuring device: VAP-7070 (manufactured by JASCO Corporation). The luminosity-corrected single transmittance can be measured as follows. A sample (5 cm x 5 cm) is prepared by attaching a polarizer to glass via an adhesive. At this time, a polarizing plate protective film is attached to the polarizer so that it is on the side opposite the glass (air interface). The glass side of this sample is set facing the light source and measured.

[0087] [Example 2] <Formation of alignment film 2> An alignment film 2 was obtained in the same manner as in Example 1, except that a long cellulose acylate film (TD80UL, manufactured by Fujifilm Corporation) was used as the substrate.

[0088] (Formation of Optically Anisotropic Layer D) The alignment film 2 thus prepared was continuously subjected to a rubbing treatment. At this time, the longitudinal direction of the long film was parallel to the transport direction, and the angle between the longitudinal direction of the film and the rotation axis of the rubbing roller was 72.5° (the film width direction was 0°, the film longitudinal direction was 90°, and the clockwise direction with the film width direction as the reference when observed from the alignment film 2 side was expressed as a positive value, so the rotation axis of the rubbing roller was -17.5°).

[0089] The optically anisotropic layer A coating solution containing a discotic liquid crystal compound of the following composition was continuously coated on the above-prepared alignment film 2 with a wire bar of #4.8. The film was conveyed at a speed of 26 m / min. In order to dry the solvent of the coating solution and to mature the alignment of the discotic liquid crystal compound, the coating film on the alignment film 2 was heated with 130°C hot air for 90 seconds, then with 100°C hot air for 60 seconds, and irradiated with 300 mJ / cm2 UV (ultraviolet rays) at 80°C to fix the alignment of the liquid crystal compound, thereby obtaining an optically anisotropic layer A. The thickness of the optically anisotropic layer D was 2.0 μm. It was confirmed that the discotic liquid crystal compound had a disc surface with respect to the film surface of 90° on average, and that the discotic liquid crystal compound was aligned perpendicular to the film surface. The angle of the slow axis was parallel to the rotation axis of the rubbing roller, and was -17.5° when the film width direction was taken as 0° (the film longitudinal direction is 90°, and the clockwise direction is expressed as a positive value based on the film width direction when observed from the optically anisotropic layer D side.) The in-plane retardation of the optically anisotropic layer D at a wavelength of 550 nm was 240 nm, and the optically anisotropic layer D exhibited forward wavelength dispersion.

[0090] ---------------------------------------------------------------------------------- Composition of coating solution for optically anisotropic layer D ---------------------------------------------------------------------------------- Discotic liquid crystal compound 1 80 parts by weight Discotic liquid crystal compound 2 20 parts by weight Alignment film interface alignment agent 1 2 parts by weight Fluorine-containing compound A 0.1 part by mass 0.2 parts by mass of the following fluorine-containing compound D 0.05 parts by mass of the following fluorine-containing compound E Ethylene oxide modified trimethylolpropane triacrylate 5 parts by mass Photopolymerization initiator (Irgacure 907, manufactured by BASF) 4 parts by weight Methyl ethyl ketone 200 parts by mass ----------------------------------------------------------------------------------

[0091] Fluorine-containing compound D [ka]

[0092] Fluorine-containing compound E [ka]

[0093] (Preparation of Optically Anisotropic Layer E) The alignment film 2 produced in Example 1 was continuously subjected to a rubbing treatment. At this time, the longitudinal direction of the long film was parallel to the transport direction, and the angle between the longitudinal direction of the film and the rotation axis of the rubbing roller was 77.5° (the film width direction was 0°, the film longitudinal direction was 90°, and the clockwise direction with the film width direction as the reference when observed from the alignment film 2 side was expressed as a positive value, so the rotation axis of the rubbing roller was 12.5°).

[0094] The optically anisotropic layer E coating solution containing the rod-shaped liquid crystal compound of the following composition was continuously coated on the alignment film 2 after rubbing treatment with a wire bar of #2.8. The film conveying speed (V) was 26 m / min. In order to dry the solvent of the coating solution and to mature the alignment of the rod-shaped liquid crystal compound, the coating film on the alignment film was heated with hot air at 60°C for 60 seconds and irradiated with UV at 60°C to fix the alignment of the liquid crystal compound, thereby forming an optically anisotropic layer C. The thickness of the optically anisotropic layer E was 1.0 μm. The average tilt angle of the long axis of the rod-shaped liquid crystal compound with respect to the film surface was 0°, and it was confirmed that the liquid crystal compound was aligned horizontally with respect to the film surface. In addition, the angle of the slow axis was -77.5°, perpendicular to the rotation axis of the rubbing roller, and the film width direction was 0° (the film longitudinal direction is 90°, and the clockwise direction is expressed as a positive value based on the film width direction when observed from the optically anisotropic layer E side). The in-plane retardation of the optically anisotropic layer E at a wavelength of 550 nm is 116 nm, and the optically anisotropic layer C exhibits normal wavelength dispersion.

[0095] ---------------------------------------------------------------------------------- Composition of coating solution for optically anisotropic layer E ---------------------------------------------------------------------------------- Mixture of rod-shaped liquid crystal compounds (A) 100 parts by weight Photopolymerization initiator (Irgacure 907, manufactured by BASF) 6 parts by weight ·Fluorine-containing compound D 0.25 parts by mass ·Fluorine-containing compound E 0.3 parts by mass Ethylene oxide modified trimethylolpropane triacrylate 8 parts by mass Methyl ethyl ketone 337 parts by weight ----------------------------------------------------------------------------------

[0096] Following the same procedure as in Example 1, a linear polarizing plate was prepared. <Creating a window> The surface of the optically anisotropic layer of the long-sized optical film D prepared above and the surface of the polarizer of the long-sized linear polarizing plate prepared above (the surface opposite to the polarizer protective film) were continuously bonded together using an ultraviolet-curing adhesive. Then, the alignment film 2 of the optical film D was peeled off, and an ultraviolet-curing adhesive was applied to the surface of the optically anisotropic layer, which was then continuously laminated to the optically anisotropic layer side of the optical film E. The TJ25 side of the obtained film was attached to a commercially available glass plate (thickness 2 mm) with a pressure-sensitive adhesive.

[0097] <Creating a display> The surface of the optically anisotropic layer of the long-length optical film D prepared above was bonded to the polarizing plate surface of a commercially available IPS-liquid crystal display device using a pressure-sensitive adhesive. The optical film was arranged so that the coating direction of the optical film was perpendicular to the absorption axis of the polarizing plate. The alignment film 2 of the optical film D was peeled off, and the optical film E was bonded thereto using a pressure-sensitive adhesive.

[0098] [Example 3] <Creating a window> The polarizing film on the surface of a commercially available organic EL television was carefully peeled off, and after removing any dirt such as adhesive, the outermost surface of the polarizing plate was attached to a commercially available glass plate (thickness 2 mm) with a pressure-sensitive adhesive. This polarizing film used a 1 / 4 λ plate made of highly stretched modified cycloolefin polymer and a linear polarizing plate (hereafter referred to as linear polarizing plate 2). <Creating a display> The polarizing plate obtained by peeling from the commercially available organic EL television was immersed in 80°C hot water for 2 hours to swell and dissolve the PVA polarizer in the polarizing plate, and only the above 1 / 4λ plate was obtained. The obtained 1 / 4λ plate was bonded to the polarizing plate surface of a commercially available IPS-LCD display device with a pressure-sensitive adhesive. At this time, the slow axis of the 1 / 4λ plate and the slow axis of the polarizing plate of the IPS LCD display device were bonded at an angle of 90° from the angle with the absorption axis of the polarizing plate when it was originally laminated on the organic EL television.

[0099] [Comparative Example 1] A window was created by attaching a light-reducing film with a transmittance of 26% to a commercially available glass plate (thickness 2 mm). A commercially available IPS-LCD display device was prepared as is.

[0100] [Comparative Example 2] A window was created by attaching a 3% light-reducing film to a commercially available glass plate (thickness 2 mm). A commercially available IPS-LCD display was prepared as is.

[0101] [Comparative Example 3] The linear polarizing plate 1 prepared above was attached to a commercially available glass plate (thickness 2 mm) with a pressure-sensitive adhesive to create a window. A commercially available IPS-liquid crystal display device was prepared as it was.

[0102] The measurement and evaluation results of Examples 1 to 3 and Comparative Examples 1 to 3 are shown in Table 1. [Table 1]

[0103] As shown in the results in Table 1, the room equipment of the present invention is effective in preventing light leakage from the display to the outside. In addition, it is considered that the robustness of light leakage against viewing angle and axial direction is improved by using multiple optically anisotropic layers, such as a combination of positive and negative birefringence as optical elements. [Explanation of symbols]

[0104] 10. Display 20 Display side film 21, 31 1 / 4λ plate 22, 32 Linear polarizer 30 Windows 33 Window materials (glass, etc.) 34 Observer 41 Absorption axis of polarizing plate 42 1 / 4λ plate alone, apparent slow axis direction 43 Light from the display surface

Claims

1. A room facility having a display that emits light from a display surface and a window facing the outside of the room, wherein the window has an amount I2 of light emitted from the display surface that is smaller than an amount I1 of light incident from the display surface, thereby preventing leakage of the light to the outside of the room.

2. 2. The room equipment according to claim 1, wherein the light emitted from the display is circularly polarized light, and at least a linear polarizing plate and a 1 / 4 .lambda. plate are laminated on the window to absorb the circularly polarized light from the display.

3. The room equipment according to claim 1 , wherein the ¼λ plate is a laminate composed of a plurality of optically anisotropic films.

4. The room equipment according to claim 1, wherein at least one of the plurality of optically anisotropic films is made of a liquid crystal material with a fixed orientation.

5. The room equipment according to any one of claims 1 to 4, wherein the room equipment is an automobile interior equipment.

6. The room equipment according to claim 5, wherein the room equipment is an automobile interior equipment, the display is a passenger-oriented display arranged behind a driver's seat, and the window is a rear side and / or a rear window.

Citation Information

Patent Citations

  • Habitable room equipment

    JP2011144511A

Cited By

  • Optical film, polarizing plate, and display device

    WO2026160427A1