Infrared sensor and manufacturing method thereof
The infrared sensor design addresses performance limitations by using a polymer resin-based light absorption layer with nanoparticles and a reflective mirror structure to enhance sensitivity and prevent peeling, achieving efficient light-to-heat conversion.
Patent Information
- Application Number
- JP2023045026
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Existing infrared sensors face limitations in performance due to low temperature coefficient of resistance (TCR) with vanadium oxide, high resistance values with amorphous silicon, and issues with light absorption layer peeling when thickened for improved infrared absorption.
An infrared sensor design incorporating a polymer resin-based light absorption layer with dispersed nanoparticles, an infrared reflecting mirror, electrodes, and a metal thin film to enhance light-to-heat conversion efficiency, using a laminated substrate with a thermal isolation layer to prevent film peeling and improve sensitivity.
The design achieves efficient light-to-heat conversion with increased light absorption layer thickness, enhancing sensitivity and preventing film peeling, while maintaining device integrity and performance.
Smart Images

Figure 2024134696000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an infrared sensor and a method for manufacturing the same. [Background technology]
[0002] Infrared sensors have been actively applied to industry in recent years, due to their wide range of applications, including not only security cameras but also thermography of the human body, in-vehicle cameras, and inspection of structures, food, etc. In particular, there is a demand for the development of inexpensive, high-performance infrared sensors that can obtain biometric information in conjunction with IoT (Internet of Things).
[0003] In a non-cooled infrared sensor using the bolometer method, the temperature of the light receiving part is changed by absorbing the incident infrared rays, and the radiation intensity of the infrared rays is detected as an electrical signal from the resistance value change caused by the temperature change of the material placed on the light receiving part. Currently, vanadium oxide, amorphous silicon, etc. are mainly used as the element material of the bolometer (Patent Document 1). In addition, the use of carbon nanotubes (CNTs), which have a high absolute value of the temperature dependence of resistance change (temperature coefficient of resistance (TCR)), as the element material of the bolometer is also being considered (Patent Document 2). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 09-257565 [Patent Document 2] JP 2015-49207 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, vanadium oxide has a problem that its performance is limited by its low temperature dependence of resistance change (temperature coefficient of resistance (TCR)).In addition, amorphous silicon has a high resistance value, and it has not yet been able to achieve performance that exceeds that of vanadium oxide.
[0006] On the other hand, although CNTs have a high TCR, they do not absorb infrared rays sufficiently by themselves, so there are cases where it is necessary to provide an additional light absorbing layer on the bolometer element that efficiently absorbs the infrared rays that enter and converts them into heat, etc., and transmits them to the bolometer element. When inorganic materials such as SiN and SiO2 are used as the light absorbing layer, a film thickness of several μm or more is required to ensure sufficient infrared absorption, but there is a problem that the light absorbing layer peels off when the film is made too thick.
[0007] In view of the above problems, an object of the present invention is to provide an infrared sensor capable of efficient light-to-heat conversion by increasing the thickness of a light absorbing layer, and a method for manufacturing the same. [Means for solving the problem]
[0008] In order to achieve the above object, the present invention provides an infrared reflective mirror, a first light absorbing layer formed on the infrared reflective mirror and being a polymer resin layer in which light absorbing nanoparticles are dispersed; Two electrodes formed on the first light absorbing layer; a light detection unit that at least partially overlaps and is in electrical contact with the two electrodes; a second light absorbing layer formed on the light detection unit and being a polymer resin layer in which light absorbing nanoparticles are dispersed; a metal thin film formed on the second light absorbing layer; The infrared sensor includes:
[0009] The present invention also provides a method for manufacturing a semiconductor device comprising the steps of: preparing an infrared reflective mirror; dispersing light absorbing nanoparticles in a polymer resin to form a material for a first light absorbing layer; applying a material of the first light absorbing layer onto the infrared reflective mirror to form a first light absorbing layer; forming two electrodes on the first light absorbing layer; forming a light detection portion so as to at least partially overlap and be in electrical contact with the two electrodes; dispersing light absorbing nanoparticles in a polymer resin to form a material for a second light absorbing layer; applying a material of the second light absorbing layer onto the light detection portion to form a second light absorbing layer; forming a metal thin film on the second light absorbing layer; The present invention relates to a method for manufacturing an infrared sensor, Effect of the Invention
[0010] According to the present invention, it is possible to provide an infrared sensor capable of efficient light-to-heat conversion by increasing the thickness of a light absorbing layer, and a method for manufacturing the same. [Brief description of the drawings]
[0011] [Figure 1] 1 is a cross-sectional view showing an embodiment of an infrared sensor according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The infrared sensor of the present invention comprises: An infrared reflecting mirror; a first light absorbing layer formed on the infrared reflective mirror and being a polymer resin layer in which light absorbing nanoparticles are dispersed; Two electrodes formed on the first light absorbing layer; a light detection unit that at least partially overlaps and is in electrical contact with the two electrodes; a second light absorbing layer formed on the light detection unit and being a polymer resin layer in which light absorbing nanoparticles are dispersed; a metal thin film formed on the second light absorbing layer; The infrared sensor includes:
[0013] When infrared rays are incident on the metal thin film, part of the infrared rays is reflected by the metal thin film, but the other part passes through the metal thin film and travels toward the light absorbing layer and the light detection section. The infrared rays that pass through these are then reflected by the infrared reflection mirror and are incident on the light absorbing layer and the light detection section again.
[0014] The infrared sensor of the present invention has a first light absorbing layer and a second light absorbing layer made of a polymer resin in which light absorbing nanoparticles are dispersed. By using a polymer resin as a binder, it is possible to thicken the light absorbing layer without causing peeling of the film. Furthermore, by using light absorbing nanoparticles with desired light absorption characteristics as a light absorbing material, efficient light-to-heat conversion is possible. This configuration makes it possible to convert light into heat without leakage, leading to improved sensitivity.
[0015] Furthermore, the infrared sensor of the present invention has an infrared reflecting mirror and a thin metal film arranged above and below the element, which utilizes the interference effect to increase the amount of light absorption, and the upper thin metal film makes it possible to prevent moisture from entering the device.
[0016] The infrared sensor of the present invention preferably includes a substrate having a heat insulating surface below the infrared reflecting mirror, and the substrate is more preferably a laminated substrate in which a support substrate and a thermal isolation layer are laminated.
[0017] The detection wavelength is from 760 nm to 1 mm, preferably from 2.5 μm to 1 mm, and more preferably from 5 μm to 1 mm.
[0018] A cross-sectional view of one embodiment of an infrared sensor according to the present invention is shown in Fig. 1. An infrared sensor 10 of this embodiment includes, in this order, a thermal isolation layer 14, an infrared reflection mirror 16, a first light absorbing layer 18, two electrodes 20, a light detection section 22, a second light absorbing layer 24, and a metal thin film 26 on the surface of a support substrate 12. Each component of the infrared sensor of this embodiment will be described in detail below.
[0019] (Support substrate 12) The material constituting the support substrate 12 may be an inorganic material or an organic material, and any material used in the art may be used without particular limitation. Inorganic materials include, but are not limited to, glass, Si, SiO2, SiN, etc. Organic materials include, but are not limited to, plastics, rubber, etc., such as polyimide, polyethylene, polypropylene, polystyrene, polyvinyl chloride, polyethylene terephthalate, acrylonitrile styrene resin, acrylonitrile butadiene styrene resin, fluororesin, methacrylic resin, polycarbonate, etc.
[0020] (thermal separation layer 14) By covering the surface of the support substrate with a material having high thermal insulation (low thermal conductivity), it is possible to suppress the dissipation of heat from the light detection unit. The thermal conductivity of the material constituting the thermal isolation layer 14 is generally 0.3 W / mK or less, preferably 0.15 W / mK or less, and more preferably 0.1 W / mK or less in some cases. Since a lower thermal conductivity is preferable, the lower limit is not particularly limited, but is, for example, 0.02 W / mK or more, for example, 0.05 W / mK or more. In particular, it is preferable that the thermal conductivity of the thermal isolation layer at least in the vertical direction (stacking direction) is within the above range. In this specification, the thermal conductivity can be a value determined at 25°C according to a standard method (ASTM C177, ASTM E1461, etc.).
[0021] Materials constituting the thermal isolation layer 14 include, but are not limited to, parylene. Parylene is a general term for paraxylylene-based polymers, and has a structure in which benzene rings are linked via CH2. Examples of parylene include those formed from a dimer represented by the following formula:
[0022] [ka]
[0023] In the above formula, at least one hydrogen atom of at least one benzene ring may be substituted with a halogen atom. Examples of halogen include fluorine (F), chlorine (Cl), bromine (Br), and iodine (I), and chlorine is preferred. The number of substitutions by halogen is 8 or less, preferably 6 or less, and more preferably 4 or less.
[0024] Parylene includes Parylene N, Parylene C, Parylene D, Parylene HT, and ParyFree, among which Parylene C (thermal conductivity: 0.084 (W / mK)) is the most suitable because it has the lowest thermal conductivity. Parylene is chemically stable and has excellent moisture, chemical, and insulation barrier properties. Parylene coating also has excellent temperature stability, mechanical properties, and tensile strength.
[0025] The method of forming the thermal isolation layer is not particularly limited and can be appropriately selected according to the material used. For example, when parylene is used, a parylene film can be formed by coating parylene on a support substrate using a vacuum deposition apparatus. Specifically, when a solid dimer is heated under vacuum, it vaporizes and becomes a dimer gas. This gas is thermally decomposed to cleave the dimer and become a monomer form. In a deposition chamber at room temperature, this monomer gas polymerizes on all surfaces to form a thin and transparent polymer film. If necessary, the support substrate may be pretreated, cleaned, and areas that should not be deposited may be masked before the deposition process.
[0026] In order to ensure heat insulation, the thickness of the thermal isolation layer is preferably 20 μm or more, more preferably 60 μm or more. The upper limit is not particularly limited, but in order to reduce the size of the infrared sensor, the thickness is preferably 1000 μm or less, more preferably 300 μm or less.
[0027] (Infrared Reflecting Mirror 16) The infrared reflection mirror 16 is a layer that reflects light that has passed through the first light absorbing layer 18 and the second light absorbing layer 24 and the light detection unit 22, and that allows the light to be reabsorbed by the light absorbing layers and the light detection unit. Therefore, the infrared reflection mirror 16 is provided on the opposite side to the light incident side with respect to the light absorbing layers 18 and 24 and the light detection unit 22. The infrared reflection mirror 16 can be made of any material that is used as a light reflection layer in an infrared sensor, and generally includes metals such as titanium, gold, silver, and aluminum, and can be formed by vapor deposition, sputtering, plating, or the like.
[0028] The thickness of the infrared reflective mirror can be appropriately set depending on the material, but is preferably 0.05 to 1 μm, and more preferably 0.1 to 0.2 μm.
[0029] (First light absorbing layer 18) The first light absorbing layer is a polymer resin layer in which light absorbing nanoparticles are dispersed. The light absorbing nanoparticles can be mixed or milled into the polymer resin using conventional mixing and / or milling equipment. The material of the first light absorbing layer thus formed can be applied onto the infrared reflecting mirror, and the first light absorbing layer can be formed, for example, by applying, drying, or annealing.
[0030] The light-absorbing nanoparticles 28 of the present invention are preferably particles that have no absorption in the visible and near-infrared regions, and in particular have an absorption band at wavelengths of 5 μm or more. The light-absorbing nanoparticles 28 preferably selectively absorb infrared rays at least about 1000 times more selectively than visible light and near-infrared rays, and particularly preferably absorb infrared rays at least about 10,000 times more selectively than visible light and near-infrared rays. By selecting light-absorbing nanoparticles that do not absorb in the visible and near-infrared regions, degradation of the polymer resin due to carrier generation caused by light absorption in the visible and near-infrared regions does not occur, and it is possible to suppress deterioration of device performance.
[0031] In this specification, "visible light" refers to electromagnetic waves with a lower wavelength limit of 360 to 400 nm and an upper wavelength limit of 760 to 830 nm, "infrared light" refers to electromagnetic waves with a wavelength from the long wavelength end of visible light (760 to 830 nm) to 1 mm, and "near-infrared light" refers to infrared light with a wavelength close to that of visible light, and electromagnetic waves with a wavelength of 2.5 μm or less.
[0032] Examples of the light-absorbing nanoparticles 28 include, but are not limited to, silicon oxide, silicon nitride, and the like. The light-absorbing nanoparticles 28 may be crystalline or amorphous (non-crystalline), but are preferably crystalline. From the viewpoint of preventing Mie scattering, the particle size parameter πD / λ (D: average particle size, λ: detection wavelength) is preferably 1 or less, and more preferably 0.1 or less. For example, when the detection wavelength is 10 μm, the average particle size of the light-absorbing nanoparticles is preferably about 3 μm or less, and more preferably about 0.3 μm or less. The average particle size of the light-absorbing nanoparticles is particularly preferably in the range of, for example, 0.05 to 0.15 μm.
[0033] The polymer resin 30 of the present invention preferably has an absorptance of 0.1 or less for electromagnetic waves with a wavelength of 5 μm or less, more preferably 0.08 or less, and particularly preferably 0.06 or less. The polymer resin 30 of the present invention preferably has a transmittance of 50% or more for visible light and near-infrared light, more preferably 60% or more, and particularly preferably 70% or more. From the above viewpoint, the polymer resin is preferably a resin having a basic skeleton consisting only of carbon and hydrogen, such as polystyrene.
[0034] The weight ratio of the polymer resin to the light-absorbing nanoparticles in the first light-absorbing layer is preferably 80:20 to 20:80, more preferably 60:40 to 30:70. When the weight ratio of the polymer resin to the light-absorbing nanoparticles is within the above range, both the light absorption and the dispersibility of the light-absorbing nanoparticles can be achieved, and the first light-absorbing layer does not peel off. If the amount of the light-absorbing nanoparticles is small, the light absorption may be insufficient, and if the amount of the binder polymer resin is small, the first light-absorbing layer may peel off.
[0035] The thickness of the first light absorbing layer is preferably 500 nm to 5 μm, and more preferably 1 μm to 3 μm. If the thickness of the first light absorbing layer is within the above range, sufficient light absorbency can be obtained.
[0036] (electrode 20) The material of the electrode may be appropriately selected in consideration of the bonding property with the light detection unit, and for example, a single metal such as titanium, gold, platinum, aluminum, copper, silver, tungsten, cobalt, or an alloy containing at least one of these metals may be used alone or in combination. The method of manufacturing the electrode is not particularly limited, and for example, the electrode may be formed by deposition, sputtering, or printing. If necessary, masking of the area where the electrode is not to be formed may be performed in advance. The thickness of the electrode may be appropriately adjusted, but is preferably 30 nm to 300 nm, and more preferably 50 nm to 200 nm. The distance between the two electrodes is preferably 2 to 100 μm, and more preferably 2 to 10 μm for miniaturization of the infrared sensor. can.
[0037] (Light detection unit 22) Examples of materials for the light detection unit include, but are not limited to, carbon nanotubes, vanadium oxide, amorphous silicon, etc. The light detection unit is preferably a carbon nanotube. A carbon nanotube (CNT) film will be described in detail below as an example of the light detection unit 22.
[0038] The carbon nanotube film is a thin film composed of a plurality of carbon nanotubes that form a conductive path that electrically connects two electrodes 20. The carbon nanotubes can form structures such as parallel lines, fibers, and networks, but it is preferable that they form a three-dimensional network structure that is less prone to aggregation and provides a uniform conductive path.
[0039] Carbon nanotubes may be single-walled, double-walled or multi-walled, but when separating a semiconductor type, single-walled or several-walled (e.g., two-walled or three-walled) carbon nanotubes are preferred, and single-walled carbon nanotubes are more preferred. Carbon nanotubes preferably contain 80% by mass or more of single-walled carbon nanotubes, and more preferably contain 90% by mass or more (including 100% by mass).
[0040] From the viewpoint of increasing the band gap and improving the TCR, the diameter of the carbon nanotube is preferably between 0.6 and 1.5 nm, more preferably between 0.6 and 1.2 nm, and even more preferably between 0.7 and 1.1 nm. In one embodiment, a diameter of 1 nm or less may be particularly preferable. If the diameter is 0.6 nm or more, the production of the carbon nanotube is easier. If the diameter is 1.5 nm or less, the band gap can be easily maintained within an appropriate range, and a high TCR can be obtained.
[0041] In this specification, the diameter of the carbon nanotubes means that the diameters of about 100 points of the carbon nanotubes on the heat insulating layer or in the formed thin film are measured using an atomic force microscope (AFM), and 60% or more, preferably 70% or more, in some cases more preferably 80% or more, and more preferably 100% are within the range of 0.6 to 1.5 nm. Preferably, 60% or more, preferably 70% or more, in some cases more preferably 80% or more, and more preferably 100% are within the range of 0.6 to 1.2 nm, and even more preferably 0.7 to 1.1 nm. In one embodiment, 60% or more, preferably 70% or more, in some cases more preferably 80% or more, and more preferably 100% are within the range of 0.6 to 1 nm.
[0042] The length of the carbon nanotubes is preferably between 100 nm and 5 μm because they are easily dispersed and have excellent coating properties. From the viewpoint of the electrical conductivity of the carbon nanotubes, the length is preferably 100 nm or more. If the length is 5 μm or less, aggregation on the heat insulating layer and / or during film formation is easily suppressed. The length of the carbon nanotubes is more preferably 500 nm to 3 μm, and even more preferably 700 nm to 1.5 μm.
[0043] In this specification, the length of carbon nanotubes means that at least 60%, preferably at least 70%, in some cases more preferably at least 80%, and more preferably 100% of the length distribution of carbon nanotubes is within the range of 100 nm to 5 μm, as determined by observing and counting at least 100 tubes using an atomic force microscope (AFM). Preferably, at least 60%, preferably at least 70%, in some cases more preferably at least 80%, and more preferably 100% of the length is within the range of 500 nm to 3 μm. More preferably, at least 60%, preferably at least 70%, in some cases more preferably at least 80%, and more preferably 100% of the length is within the range of 700 nm to 1.5 μm.
[0044] When the diameter and length of the carbon nanotube are within the above ranges, the influence of the semiconducting properties becomes large and a large current value can be obtained, so that when used as a bolometer film, a high TCR value is likely to be obtained.
[0045] The light detection unit preferably uses semiconducting carbon nanotubes having a large band gap and carrier mobility. The content of semiconducting carbon nanotubes, preferably semiconducting single-walled carbon nanotubes, in the carbon nanotubes is generally 67% by mass or more, preferably 70% by mass or more, more preferably 80% by mass or more, particularly preferably 90% by mass or more, more preferably 95% by mass or more, and even more preferably 99% by mass or more (including 100% by mass).
[0046] The thickness of the carbon nanotube film is not particularly limited, but is, for example, 1 nm or more, for example, several nm to 100 μm, preferably in the range of 2 nm to 20 nm. In order to ensure the network path of the carbon nanotubes, it is necessary that the thickness is 2 nm or more. Furthermore, if the thickness of the carbon nanotube film is 100 nm or less, printing technology can be officially applied as a method for producing the carbon nanotube film, which is preferable from the viewpoint of simplifying the production method. The thickness of the carbon nanotube film can be calculated as the average value of thicknesses measured at any 10 points on the carbon nanotube film.
[0047] In order to obtain a good light absorption rate, the density of the carbon nanotube film is, for example, 0.3 g / cm. 3 or more, preferably 0.8 g / cm 3 More preferably, it is 1.1 g / cm 3 The upper limit is not particularly limited, but it is preferably the upper limit of the true density of the carbon nanotubes used (for example, about 1.4 g / cm 3 The density of the carbon nanotube film can be calculated from the weight, area, and thickness of the carbon nanotube film obtained above.
[0048] The content of carbon nanotubes in the carbon nanotube film can be appropriately selected, but is preferably 60 mass % or more based on the total mass of the carbon nanotube film.
[0049] An example of a method for producing a carbon nanotube film will now be described in detail.
[0050] A dispersion solution of carbon nanotubes is obtained. The carbon nanotubes may be used after removing impurities such as surface functional groups and amorphous carbon, catalysts, etc. by heat treatment in an inert atmosphere or vacuum. The heat treatment temperature can be appropriately selected, but is preferably 800 to 2000°C, more preferably 800 to 1200°C.
[0051] The method for obtaining a carbon nanotube dispersion solution is not particularly limited, and a conventionally known method can be applied. For example, a carbon nanotube mixture, a dispersion medium, and a nonionic surfactant are mixed to prepare a solution containing carbon nanotubes, and the solution is ultrasonicated to disperse the carbon nanotubes, thereby preparing a carbon nanotube dispersion solution (micelle dispersion solution). In addition to or instead of the ultrasonication, a carbon nanotube dispersion method using mechanical shearing force may be used. Mechanical shearing may be performed in the gas phase.
[0052] The dispersion medium is not particularly limited as long as it is a solvent that can disperse and suspend the carbon nanotubes during the separation process. For example, water, heavy water, an organic solvent, an ionic liquid, or a mixture thereof can be used, with water and heavy water being preferred.
[0053] The nonionic surfactant can be appropriately selected, but it is preferable to use one or more nonionic surfactants composed of a non-ionized hydrophilic portion and a hydrophobic portion such as an alkyl chain, such as a nonionic surfactant having a polyethylene glycol structure represented by polyoxyethylene alkyl ether, or an alkyl glucoside nonionic surfactant. As such a nonionic surfactant, a polyoxyethylene alkyl ether represented by formula (1) is preferably used. In addition, the alkyl portion may contain one or more unsaturated bonds.
[0054] C n H 2n+1 (OCH2CH2) m OH (1) (In the formula, n is preferably 12 to 18, and m is 10 to 100, preferably 20 to 100.)
[0055] In particular, nonionic surfactants defined as polyoxyethylene (n) alkyl ethers (n is 20 to 100, alkyl chain length is C12 to C18), such as polyoxyethylene (23) lauryl ether, polyoxyethylene (20) cetyl ether, polyoxyethylene (20) stearyl ether, polyoxyethylene (10) oleyl ether, polyoxyethylene (10) cetyl ether, polyoxyethylene (10) stearyl ether, polyoxyethylene (20) oleyl ether, and polyoxyethylene (100) stearyl ether, are more preferred. In addition, N,N-bis[3-(D-gluconamido)propyl]deoxycholamide, n-dodecyl β-D-maltoside, octyl β-D-glucopyranoside, and digitonin can also be used.
[0056] Examples of nonionic surfactants include polyoxyethylene sorbitan monostearate (molecular formula: C64H126O26, trade name: Tween 60, manufactured by Sigma-Aldrich Co., Ltd., etc.), polyoxyethylene sorbitan trioleate (molecular formula: C24H44O6, trade name: Tween 85, manufactured by Sigma-Aldrich Co., Ltd., etc.), octylphenol ethoxylate (molecular formula: C14H22O(C2H4O)n, n=1 to 10, trade name: Triton X-100, manufactured by Sigma-Aldrich Co., Ltd., etc.), polyoxyethylene (40) isooctylphenyl ether (molecular formula: C8H17C6H40(CH2CH20)40H, trade name: Triton Also usable are X-405, manufactured by Sigma-Aldrich, etc.), poloxamer (molecular formula: C5H10O2, trade name: Pluronic, manufactured by Sigma-Aldrich, etc.), and polyvinylpyrrolidone (molecular formula: (C6H9NO)n, n = 5 to 100, manufactured by Sigma-Aldrich, etc.).
[0057] The concentration of the surfactant in the liquid containing the dispersion medium and the nonionic surfactant is preferably the critical micelle concentration to 10% by mass, more preferably the critical micelle concentration to 3% by mass. If it is below the critical micelle concentration, it is not preferable because it cannot be dispersed. If it is below 10% by mass, carbon nanotubes with a sufficient density can be applied while reducing the amount of surfactant after separation. In this specification, the critical micelle concentration (CMC) refers to the concentration at which the surface tension is measured at a constant temperature by changing the concentration of the surfactant aqueous solution using a surface tensiometer such as a Wilhelmy surface tensiometer. In this specification, the "critical micelle concentration" is a value at atmospheric pressure and 25°C.
[0058] In the micellar dispersion of carbon nanotubes and a nonionic surfactant, the carbon nanotubes are preferably in an isolated state. Therefore, if necessary, ultracentrifugation may be used to remove bundles, amorphous carbon, impurity catalysts, and the like. During dispersion, the carbon nanotubes can be cut, and the length can be controlled by changing the crushing conditions, ultrasonic output, ultrasonic treatment time, and the like. For example, untreated carbon nanotubes can be crushed with tweezers, a ball mill, or the like to control the aggregate size. After these treatments, the length can be controlled to 100 nm to 5 μm by using an ultrasonic homogenizer at an output of 40 to 600 W, or in some cases 100 to 550 W, 20 to 100 KHz, and a treatment time of 1 to 5 hours, preferably 3 hours. If the time is shorter than 1 hour, the nanotubes may hardly be dispersed depending on the conditions, and may remain almost the same as their original length. In addition, 3 hours or less is preferable from the viewpoint of shortening the dispersion treatment time and reducing costs. This embodiment may also have the advantage that the cut is easily adjusted by using a nonionic surfactant. Another advantage is that it does not contain ionic surfactants, which are difficult to remove.
[0059] By dispersing and cutting the carbon nanotubes, surface functional groups are generated on the surface or ends of the carbon nanotubes. The functional groups generated include carboxyl groups, carbonyl groups, hydroxyl groups, etc. In the case of treatment in a liquid phase, carboxyl groups and hydroxyl groups are generated, and in the case of treatment in a gas phase, carbonyl groups are generated.
[0060] The concentration of carbon nanotubes in the cutting and dispersion process (weight of carbon nanotubes / (total weight of dispersion medium and surfactant)×100) is not particularly limited, but can be, for example, 0.0003 to 10 mass%, preferably 0.001 to 3 mass%, and more preferably 0.003 to 0.3 mass%.
[0061] After the above-mentioned carbon nanotube dispersion / cutting step and before the separation step described below, a centrifugation treatment may be performed to remove bundles, amorphous carbon, metal impurities, etc. from the carbon nanotube dispersion liquid. The centrifugal acceleration can be appropriately adjusted, but is preferably 10,000×g to 500,000×g, more preferably 50,000×g to 300,000×g, and may be 100,000×g to 300,000×g in some cases. The centrifugation time is preferably 0.5 hours to 12 hours, more preferably 1 to 3 hours. The centrifugation temperature can be appropriately adjusted, but is preferably 4°C to room temperature, more preferably 10°C to room temperature.
[0062] Carbon nanotubes can be separated, for example, by an electric field induced layer formation method (ELF method: see, for example, K.Ihara et al. J.Phys.Chem.C.2011,115,22827-22832, Japanese Patent No. 5717233, which are incorporated herein by reference). An example of a separation method using the ELF method will be described. Carbon nanotubes, preferably single-walled carbon nanotubes, are dispersed in a nonionic surfactant, and the dispersion is placed in a vertical separation device, and a voltage is applied to electrodes arranged above and below, to separate the nanotubes by carrier-free electrophoresis. The mechanism of separation can be estimated, for example, as follows. When carbon nanotubes are dispersed in a nonionic surfactant, the micelles of semiconducting carbon nanotubes have a negative zeta potential, while the micelles of metallic carbon nanotubes have a zeta potential of the opposite sign (positive) (in recent years, it has been considered that they have a slightly negative zeta potential or are almost uncharged). Therefore, when an electric field is applied to the carbon nanotube dispersion, the conductive carbon nanotube micelles electrophores toward the anode (+) and the metallic carbon nanotube micelles electrophores toward the cathode (-) due to the difference in zeta potential. Finally, a layer in which the semiconducting carbon nanotubes are concentrated near the anode and a layer in which the metallic carbon nanotubes are concentrated near the cathode are formed in the separation tank. The voltage for separation can be appropriately set in consideration of the composition of the dispersion medium and the charge amount of the carbon nanotubes, and is preferably 1V or more and 200V or less, and more preferably 10V or more and 200V or less. From the viewpoint of shortening the separation process time, 100V or more is preferable. Also, from the viewpoint of suppressing the generation of bubbles during separation and maintaining separation efficiency, 200V or less is preferable. The purity of the separation is improved by repeating the separation. The dispersion after separation may be reset to the initial concentration and the same separation operation may be performed. This can further increase the purity.
[0063] The above-mentioned carbon nanotube dispersion / cutting and separation steps can provide a dispersion liquid in which semiconducting carbon nanotubes having a desired diameter and length are concentrated. The semiconducting carbon nanotube dispersion liquid obtained by the separation step means a dispersion liquid containing semiconducting carbon nanotubes in an amount of generally 67% by mass or more, preferably 70% by mass or more, more preferably 80% by mass or more, particularly preferably 90% by mass or more, more preferably 95% by mass or more, and even more preferably 99% by mass or more (the upper limit may be 100% by mass) of the total amount of carbon nanotubes. The tendency of separation of metallic and semiconducting carbon nanotubes can be analyzed by microscopic Raman spectroscopy and ultraviolet-visible-near infrared absorptiometry.
[0064] The concentration of the surfactant in the carbon nanotube dispersion after separation can be appropriately controlled. The concentration of the surfactant in the carbon nanotube dispersion is preferably the critical micelle concentration to about 5 mass%, more preferably 0.001 mass% to 3 mass%, and particularly preferably 0.01 to 1 mass% in order to suppress re-aggregation after application.
[0065] The semiconducting carbon nanotube dispersion obtained by the above-mentioned process is applied to the two electrodes on the first light absorbing layer so that they at least partially overlap and are in electrical contact with each other, and then dried, and optionally heat-treated, to form a carbon nanotube film.
[0066] The method of applying the semiconductor carbon nanotube dispersion is not particularly limited, and examples thereof include a dropping method, spin coating, printing, inkjet, spray coating, dip coating, etc. From the viewpoint of reducing the manufacturing cost, a printing method is preferable. Examples of the printing method include application (dispenser, inkjet, etc.), transfer (microcontact printing, gravure printing, etc.), etc.
[0067] The surfactant and the solvent can be removed from the applied semiconducting carbon nanotube dispersion by heat treatment. The temperature of the heat treatment can be appropriately set to a temperature equal to or higher than the decomposition temperature of the surfactant, but is preferably 150 to 500°C, more preferably 200 to 500°C, for example 200 to 400°C. If it is 200°C or higher, it is more preferable because it is easy to suppress the residue of the decomposition product of the surfactant. In addition, if it is 500°C or lower, for example 400°C or lower, it is preferable because it is possible to suppress the decomposition and size change of the carbon nanotubes, the detachment of functional groups, and the like.
[0068] (Second light absorbing layer 24) The second light absorbing layer is a polymer resin layer in which light absorbing nanoparticles are dispersed. The light absorbing nanoparticles and polymer resin in the second light absorbing layer are the same as the light absorbing nanoparticles and polymer resin in the first light absorbing layer. The configurations of the first light absorbing layer and the second light absorbing layer of the present invention may be the same or different. The method for producing the second light absorbing layer is the same as the method for producing the first light absorbing layer.
[0069] The thickness of the second light absorbing layer is preferably 500 nm to 5 μm, and more preferably 1 μm to 3 μm. If the thickness of the second light absorbing layer is within the above range, sufficient light absorbency can be obtained.
[0070] The total thickness of the first light absorbing layer and the second light absorbing layer is preferably 2.5 μm to 10 μm, more preferably 2.5 μm to 3 μm. The ratio of the thickness of the first light absorbing layer to the thickness of the second light absorbing layer is preferably 15:75 to 50:50, more preferably 20:80 to 30:70. Within the above range, infrared rays can be efficiently absorbed and transmitted to the light detection unit.
[0071] (Metal Thin Film 26) The metal thin film 26 may be, but is not limited to, a metal such as gold, silver, copper, or aluminum. The thickness of the metal thin film may be appropriately set depending on the material, but is preferably 5 to 25 nm. The metal thin film 26 is provided on the surface opposite the infrared reflection mirror 16 with respect to the light absorption layer and the light detection unit. The metal thin film 26 is preferably disposed at a position where the distance d between the infrared reflection mirror 16 and the metal thin film 26 is an odd multiple of 1 / 4 of the wavelength λ of the infrared light to be detected. By forming the infrared reflection mirror and the metal thin film in this positional relationship, the infrared rays can be caused to interfere with each other, and the infrared rays can be efficiently transmitted to the light detection unit and the light absorption layer.
[0072] The infrared sensor of the present invention has a simple structure and can be manufactured partially or entirely by a printing process, which allows for low costs. Note that, in the method for manufacturing an infrared sensor of the present invention, a number of manufacturing steps are described in order, but the order does not limit the order in which the multiple manufacturing steps are performed. Therefore, when implementing the manufacturing method of the present invention, the order of the multiple manufacturing steps can be changed as long as it does not interfere with the content.
[0073] The present invention is not limited to the above-described embodiment. Various modifications that can be understood by those skilled in the art can be made to the configuration and details of the present invention within the scope of the present invention.
[0074] (Appendix 1) An infrared reflecting mirror; a first light absorbing layer formed on the infrared reflective mirror and being a polymer resin layer in which light absorbing nanoparticles are dispersed; Two electrodes formed on the first light absorbing layer; a light detection unit that at least partially overlaps and is in electrical contact with the two electrodes; a second light absorbing layer formed on the light detection unit and being a polymer resin layer in which light absorbing nanoparticles are dispersed; a metal thin film formed on the second light absorbing layer; An infrared sensor comprising: (Appendix 2) 2. The infrared sensor of claim 1, wherein the light absorbing nanoparticles are silicon oxide and / or silicon nitride. (Appendix 3) 3. The infrared sensor according to claim 1 or 2, wherein the particle size parameter πD / λ (D: particle size, λ: detection wavelength) of the light absorbing nanoparticles is 1 or less. (Appendix 4) 4. The infrared sensor according to claim 1, wherein the polymer resin has an absorptivity of 0.1 or less for electromagnetic waves having a wavelength of 5 μm or less. (Appendix 5) 4. The infrared sensor according to any of the preceding appendices, wherein the polymer resin has a visible light and near-infrared light transmittance of 50% or more. (Appendix 6) 13. The infrared sensor of any preceding claim, wherein the polymeric resin is polystyrene. (Appendix 7) 4. The infrared sensor according to any of the preceding claims, wherein the light detection portion is one or more selected from carbon nanotubes, vanadium oxide, and amorphous silicon. (Appendix 8) The infrared sensor according to any one of the preceding appendices, wherein the light absorbing nanoparticles have an average particle size of 0.05 to 0.15 μm. (Appendix 9) The infrared sensor according to any of the preceding appendices, wherein the total thickness of the first light absorbing layer and the second light absorbing layer is 2.5 μm to 10 μm. (Appendix 10) The infrared sensor according to any one of the preceding appendices, wherein the first light absorbing layer has a thickness of 500 nm to 5 μm. (Appendix 11) The infrared sensor according to any one of the preceding appendices, wherein the second light absorbing layer has a thickness of 500 nm to 5 μm. (Appendix 12) The infrared sensor according to any of the preceding appendices, wherein a ratio of a thickness of the first light absorbing layer to a thickness of the second light absorbing layer is 15:75 to 50:50. (Appendix 13) The infrared sensor according to any of the preceding appendices, wherein a weight ratio of polymer resin to light absorbing nanoparticles in the first light absorbing layer is 80:20 to 20:80. (Appendix 14) The infrared sensor according to any of the preceding appendices, wherein a weight ratio of polymer resin to light absorbing nanoparticles in the second light absorbing layer is 80:20 to 20:80. (Appendix 15) 13. The infrared sensor of claim 12, wherein the distance between the infrared reflecting mirror and the metal thin film is an odd multiple of ¼ of the detection wavelength. (Appendix 16) The infrared sensor according to any one of the preceding appendices, wherein the infrared reflective mirror has a thickness of 0.05 to 1 μm. (Appendix 17) An infrared sensor as described in any preceding claim, comprising a substrate below the infrared reflective mirror, the substrate having a thermally insulating surface. (Appendix 18) The infrared sensor according to any of the preceding appendices, wherein the substrate is a laminated substrate in which a support substrate and a thermal isolation layer are laminated. (Appendix 19) 13. The infrared sensor of any preceding claim, wherein the thermal isolation layer is parylene. (Appendix 20) The infrared sensor according to any one of the preceding appendices, wherein the infrared sensor has a detection wavelength of 760 nm to 1 mm. (Appendix 21) Providing an infrared reflective mirror; dispersing light absorbing nanoparticles in a polymer resin to form a material for a first light absorbing layer; applying a material of the first light absorbing layer onto the infrared reflective mirror to form a first light absorbing layer; forming two electrodes on the first light absorbing layer; forming a light detection portion so as to at least partially overlap and be in electrical contact with the two electrodes; dispersing light absorbing nanoparticles in a polymer resin to form a material for a second light absorbing layer; applying a material of the second light absorbing layer onto the light detection portion to form a second light absorbing layer; forming a metal thin film on the second light absorbing layer; A method for manufacturing an infrared sensor, comprising: [Explanation of symbols]
[0075] 10 Infrared Sensor 12 Support substrate 14 Thermal separation layer 16 Infrared reflecting mirror 18 First light absorbing layer 20 electrodes 22 Light detection unit 24 Second light absorbing layer 26 Metallic Thin Film 28 Light-absorbing nanoparticles 30 Polymer resin
Claims
1. An infrared reflecting mirror; a first light absorbing layer formed on the infrared reflective mirror and being a polymer resin layer in which light absorbing nanoparticles are dispersed; Two electrodes formed on the first light absorbing layer; a light detection unit that at least partially overlaps and is in electrical contact with the two electrodes; a second light absorbing layer formed on the light detection unit and being a polymer resin layer in which light absorbing nanoparticles are dispersed; a metal thin film formed on the second light absorbing layer; An infrared sensor comprising:
2. The infrared sensor of claim 1 , wherein the light absorbing nanoparticles are silicon oxide and / or silicon nitride.
3. 3. The infrared sensor according to claim 1, wherein the particle size parameter πD / λ (D: particle size, λ: detection wavelength) of the light absorbing nanoparticles is 1 or less.
4. 3. The infrared sensor according to claim 1, wherein the polymer resin has an absorptance of 0.1 or less for electromagnetic waves having a wavelength of 5 [mu]m or less.
5. 5. The infrared sensor according to claim 4, wherein the polymer resin is polystyrene.
6. 3. The infrared sensor according to claim 1, wherein the light detection portion is one or more selected from the group consisting of carbon nanotubes, vanadium oxide, and amorphous silicon.
7. 3. The infrared sensor according to claim 1, wherein the total thickness of the first light absorbing layer and the second light absorbing layer is 2.5 μm to 10 μm.
8. 3. The infrared sensor according to claim 1, wherein the distance between the infrared reflecting mirror and the thin metal film is an odd multiple of 1 / 4 of the detection wavelength.
9. 3. The infrared sensor according to claim 1, further comprising a substrate having a heat insulating surface below the infrared reflecting mirror.
10. Providing an infrared reflective mirror; dispersing light absorbing nanoparticles in a polymer resin to form a material for a first light absorbing layer; applying a material of the first light absorbing layer onto the infrared reflective mirror to form a first light absorbing layer; forming two electrodes on the first light absorbing layer; forming a light detecting portion so as to overlap at least a portion of the light detecting portion and to be in electrical contact with the two electrodes; dispersing light absorbing nanoparticles in a polymer resin to form a material for a second light absorbing layer; applying a material of the second light absorbing layer onto the light detection portion to form a second light absorbing layer; forming a metal thin film on the second light absorbing layer; A method for manufacturing an infrared sensor, comprising:
Citation Information
Patent Citations
Infrared sensor and infrared sensor device
CN104011518A
Systems and methods for radiative cooling and heating
JP2018526599A
Thermal image sensor with chalcogenide material and method of fabricating the same
US20120132804A1
Systems and methods for enhanced bolometer response
US20170082497A1
Sensor configured to sense heat or infrared light and electronic device including same
US20230026770A1