Polymer electrolyte fuel cell

The cross-flow structure in the cathode-side separator and gas diffusion layer of polymer electrolyte fuel cells addresses performance issues by balancing humidity and preventing drying or flooding, improving fuel cell efficiency without humidification.

JP2024135301APending Publication Date: 2024-10-04KK TOYOTA CHUO KENKYUSHO +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023045924
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Polymer electrolyte fuel cells experience performance deterioration due to electrolyte membrane drying or flooding when operating without humidification, especially under fluctuating conditions.

Method used

A cross-flow structure is implemented in the cathode-side separator and gas diffusion layer, optimizing the average cross-flow amounts in different sections of the cathode gas flow path to balance humidity and prevent drying or flooding, while maintaining low pressure loss.

Benefits of technology

The cross-flow structure effectively suppresses electrolyte membrane drying and flooding, enhancing fuel cell performance without humidification, particularly in automotive applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135301000001_ABST
    Figure 2024135301000001_ABST
Patent Text Reader

Abstract

To provide a polymer electrolyte fuel cell in which deterioration in performance hardly occurs even when non-humidified cathode gas is supplied to a cathode side to generate electricity.SOLUTION: A polymer electrolyte fuel cell includes a membrane electrode assembly, an anode-side gas diffusion layer, a cathode-side gas diffusion layer, an anode-side separator, and a cathode-side separator, and the polymer electrolyte fuel cell is used to generate electricity by supplying non-humidified cathode gas to a cathode. The cathode-side separator and the cathode-side gas diffusion layer include a cross-flow structure, and the cross-flow structure satisfies Q1<Q2 and Q1<Q3, where Q1 represents an average cross-flow amount in a first section (inlet section); Q2 represents an average cross-flow amount in a second section (intermediate section); and Q3 represents an average cross-flow amount in a third section (outlet section).SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a polymer electrolyte fuel cell, and more particularly to a polymer electrolyte fuel cell whose performance is unlikely to deteriorate even when power is generated by supplying unhumidified cathode gas to the cathode side. [Background technology]

[0002] A polymer electrolyte fuel cell includes a membrane electrode assembly (MEA) in which electrodes (catalyst layers) are bonded to both sides of an electrolyte membrane made of a solid polymer electrolyte. In a polymer electrolyte fuel cell, a gas diffusion layer is generally disposed on the outside of the catalyst layer. The gas diffusion layer is for supplying reactant gas and electrons to the catalyst layer, and is made of carbon paper, carbon cloth, or the like. Furthermore, a separator having a gas flow path is disposed on the outside of the gas diffusion layer. A polymer electrolyte fuel cell usually includes a structure (fuel cell stack) in which a plurality of unit cells each consisting of such an MEA, gas diffusion layer, and separator are stacked.

[0003] In solid polymer fuel cells, the electrolyte membrane needs to maintain an appropriate water content in order to exhibit good proton conductivity. Therefore, if the temperature of the fuel cell during power generation is high or the water content in the supply gas is low, the electrolyte membrane dries out and performance decreases. On the other hand, when power is generated using a polymer electrolyte fuel cell, water is produced on the cathode side due to an electrode reaction. Therefore, when the temperature of the fuel cell is low and the water content in the supply gas is high, liquid water is likely to be produced in the gas diffusion layer on the cathode side. Excess liquid water inhibits oxygen transport and causes a decrease in the performance of the fuel cell.

[0004] In order to solve this problem, various proposals have been made in the past. For example, Patent Document 1 states: A flow path plate having a plurality of flow path holes formed therein and curved in a corrugated shape; A flat plate bonded to one side of the flow path plate and A porous separator plate for a fuel cell comprising: The same document states: (A) When the surface of the flow path plate is brought into close contact with the outer surface of the gas diffusion layer and a reactant gas is passed through the space between the plate and the gas diffusion layer, the reactant gas forms a turbulent flow and is transmitted to the gas diffusion layer; and (B) This increases the amount of gas diffusion and improves the performance of the fuel cell. is stated.

[0005] In Patent Document 2, A rib for dividing adjacent gas flow paths; a throttle portion provided on the rib for reducing a flow passage cross-sectional area of ​​the gas flow passage; a communication groove provided in the narrowed portion for communicating between adjacent gas flow paths; A fuel cell separator comprising: This document describes that by forming a communicating groove in the throttling portion, an increase in pressure loss of the reaction gas in the throttling portion can be suppressed.

[0006] Patent Document 3 states: A straight gas flow path with low gas flow resistance. Serpentine gas flow path with high gas flow resistance A fuel cell separator comprising: The same document states: (A) Water tends to accumulate in gas flow paths with high flow resistance, whereas little water remains in gas flow paths with low flow resistance; and (B) By providing gas flow paths with different flow resistance in the separator, gas can be supplied to the electrode catalyst layer through a gas flow path with low flow resistance even under highly humidified conditions. is stated.

[0007] Patent Document 4 states: It is composed of a laminate of an anode facing plate, an intermediate plate, and a cathode facing plate. An opening was provided on the fuel gas inlet side of the anode facing plate to allow the fuel gas to come into contact with the MEA. A separator for a fuel cell is disclosed. The same document states: (A) When an opening is provided at a position corresponding to the most downstream side of the cathode gas flow path, the produced water is transported to the opening through the MEA, and the fuel gas is humidified by the produced water; and (B) This allows the electrolyte membrane to self-humidify. is stated.

[0008] Patent document 5 discloses a solid polymer fuel cell in which the gas flow path length of the separator of a single cell located a long distance from the reactant gas supply pipe is made shorter than the gas flow path length of the separator of a single cell located a short distance from the reactant gas supply pipe. The same document states: (A) In the case where a reactant gas is distributed to each unit cell from a reactant gas supply pipe via a manifold, by shortening the gas flow path length of the separator as the distance from the reactant gas supply pipe to the unit cell becomes longer, the pressure loss in the gas flow path can be reduced as the distance from the reactant gas supply pipe to the unit cell becomes longer; and (B) This allows the reactant gas to be distributed uniformly to each unit cell. is stated.

[0009] Patent Document 1 describes that the use of a porous separator plate generates turbulence in the gas flow passage, thereby increasing the amount of gas diffusing into the gas diffusion layer. However, when turbulence is generated in the cathode flow channel, if the gas diffusion amount is too large, oxygen transport is promoted, but in a low humidity environment, the electrolyte membrane dries out, causing a decrease in performance. On the other hand, if the gas diffusion amount is too small, in a high humidity environment, the liquid water generated in the gas diffusion layer on the cathode side is not sufficiently discharged, hindering oxygen transport. In other words, simply generating turbulence is not enough to achieve a balance between the two.

[0010] In addition, in order to keep the electrolyte membrane in an appropriately wet state, a humidifier may be used to humidify the fuel gas and / or the oxidant gas, but the use of a humidifier increases the size of the fuel cell system and reduces its efficiency. On the other hand, when unhumidified reactant gas is supplied to a fuel cell, if the operating conditions of the fuel cell fluctuate significantly, the amount of liquid water in the fuel cell may be excessive or insufficient. Therefore, in a fuel cell system without a humidifier, the performance of the fuel cell is likely to deteriorate due to drying or flooding of the electrolyte membrane.

[0011] Furthermore, there has been no prior art example of a polymer electrolyte fuel cell that is less susceptible to degradation of fuel cell performance due to drying or flooding of the electrolyte membrane, even when generating electricity while supplying unhumidified cathode gas to the cathode in an environment where power generation conditions fluctuate greatly. [Prior art documents] [Patent documents]

[0012] [Patent Document 1] JP 2013-125744 A [Patent Document 2] Patent Publication No. 2022-169222 [Patent Document 3] JP 2011-150801 A [Patent Document 4] JP 2011-086519 A [Patent Document 5] JP 2005-056671 A Summary of the Invention [Problem to be solved by the invention]

[0013] An object of the present invention is to provide a polymer electrolyte fuel cell whose performance is unlikely to deteriorate even when power is generated by supplying unhumidified cathode gas to the cathode side. [Means for solving the problem]

[0014] In order to solve the above problems, a polymer electrolyte fuel cell according to the present invention has the following configuration. (1) The solid polymer fuel cell is a membrane electrode assembly in which an anode side catalyst layer and a cathode side catalyst layer are bonded to both sides of an electrolyte membrane; an anode-side gas diffusion layer disposed on the outer side of the anode-side catalyst layer; a cathode-side gas diffusion layer disposed on the outer side of the cathode-side catalyst layer; an anode-side separator disposed on the outer side of the anode-side gas diffusion layer; a cathode-side separator disposed on the outer side of the cathode-side gas diffusion layer; It is equipped with: (2) The solid polymer fuel cell is used to generate power by supplying unhumidified cathode gas to the cathode. (3) The cathode-side separator and the cathode-side gas diffusion layer have a structure (cross-flow structure) that generates a gas flow (cross flow) between the cathode gas flow channels through the cathode-side gas diffusion layer, The cross-flow structure satisfies the following formulas (1) to (3).

[0015] Q1 <Q2…(1) Q1 <Q3…(2) Q i (i=1, 2, 3)=ktΔP i / μw(cm 3 / min / cm) …(3)

[0016] however, Q1 is the average crossflow volume in the first section (inlet section) where 0≦x / L<0.15; Q2 is the average crossflow in the second section (middle section) where 0.15≦x / L<0.7; Q3 is the average crossflow in the third section (outlet section) where 0.7≦x / L≦1.0; L is the total length of the cathode gas channel, x is the distance from the inlet of the cathode gas channel, k is the in-plane permeability coefficient of the cathode gas diffusion layer, t is the thickness of the cathode side gas diffusion layer, ΔP i is the pressure P in the first cathode gas flow channel in the i-th section i1and a pressure P in a second cathode gas flow passage adjacent to the first cathode gas flow passage. i2 The absolute value of the difference between μ is the viscosity of the cathode gas, w is the width of a rib that separates the first cathode gas flow channel and the second cathode gas flow channel. Effect of the Invention

[0017] In the case where the cathode-side separator and the cathode-side gas diffusion layer have a crossflow structure, by making the average crossflow volume Q1 in the inlet section of the cathode gas flow channel smaller than the average crossflow volume Q2 in the middle section and the average crossflow volume Q3 in the outlet section, it is possible to suppress drying of the electrolyte membrane in the inlet section and flooding in the middle section and the outlet section, thereby suppressing a local decrease in current density in the plane of the electrolyte membrane. Furthermore, by optimizing the cross-flow rate from the inlet to the outlet of the cathode gas flow path, it is possible to improve the performance of a fuel cell without increasing pressure loss, even when operating a vehicle-sized fuel cell without humidification. [Brief description of the drawings]

[0018] [Figure 1] FIG. 1 is a schematic diagram of a separator having a structure in which the cross-sectional area ratio (S2in / S1in) of the inlet of a gas flow passage is different from the cross-sectional area ratio (S2out / S1out) of the outlet. [Diagram 2] FIG. 13 is a graph showing the relationship between the cross flow amount, the current density, and the amount of liquid water when the cell temperature is 40° C. [Diagram 3] FIG. 13 is a graph showing the relationship between the cross flow amount, the current density, and the amount of liquid water when the cell temperature is 60° C. [Figure 4] FIG. 13 is a graph showing the relationship between the crossflow amount and the current density when the cell temperature is 80° C.

[0019] [Diagram 5] FIG. 13 is a graph showing the relationship between the distance x from the flow path inlet and the relative humidity when the cell temperature is 80° C. [Figure 6] FIG. 13 is a graph showing the relationship between the distance x from the flow path inlet and the relative humidity when the cell temperature is 60° C. [Figure 7] FIG. 4 is a diagram showing the relationship between the total length L of the cathode gas flow channel and the sum of current values. [Figure 8] FIG. 13 is a diagram showing the relationship between the number of narrowed portions and pressure loss. [Figure 9] FIG. 13 is a diagram showing the relationship between the number of constrictions and performance. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] [Configuration 1] A polymer electrolyte fuel cell having the following configuration. (1) The solid polymer fuel cell is a membrane electrode assembly in which an anode side catalyst layer and a cathode side catalyst layer are bonded to both sides of an electrolyte membrane; an anode-side gas diffusion layer disposed on the outer side of the anode-side catalyst layer; a cathode-side gas diffusion layer disposed on the outer side of the cathode-side catalyst layer; an anode-side separator disposed on the outer side of the anode-side gas diffusion layer; a cathode-side separator disposed on the outer side of the cathode-side gas diffusion layer; It is equipped with: (2) The solid polymer fuel cell is used to generate power by supplying unhumidified cathode gas to the cathode. (3) The cathode-side separator and the cathode-side gas diffusion layer have a structure (cross-flow structure) that generates a gas flow (cross flow) between the cathode gas flow channels through the cathode-side gas diffusion layer, The cross-flow structure satisfies the following formulas (1) to (3).

[0021] Q1 <Q2…(1) Q1 <Q3…(2) Q i (i=1, 2, 3)=ktΔP i / μw(cm 3 / min / cm) …(3)

[0022] however, Q1 is the average crossflow volume in the first section (inlet section) where 0≦x / L<0.15; Q2 is the average crossflow in the second section (middle section) where 0.15≦x / L<0.7; Q3 is the average crossflow in the third section (outlet section) where 0.7≦x / L≦1.0; L is the total length of the cathode gas channel, x is the distance from the inlet of the cathode gas channel, k is the in-plane permeability coefficient of the cathode gas diffusion layer, t is the thickness of the cathode side gas diffusion layer, ΔP i is the pressure P in the first cathode gas flow channel in the i-th section i1 and a pressure P in a second cathode gas flow passage adjacent to the first cathode gas flow passage. i2 The absolute value of the difference between μ is the viscosity of the cathode gas, w is the width of a rib that separates the first cathode gas flow channel and the second cathode gas flow channel.

[0023] [Configuration 2] The cathode side separator is (a) A flow channel structure with a constriction. (b) an alternating occlusion type flow channel structure; and (c) End-narrowed flow channel structure 2. The polymer electrolyte fuel cell according to claim 1, comprising at least one structure selected from the group consisting of:

[0024] [Configuration 3] The cathode side separator is The first cathode gas flow channel and the second cathode gas flow channel are arranged in parallel with each other across the rib; a narrowed portion provided in the first cathode gas flow channel and / or the second cathode gas flow channel; Equipped with The cross-flow structure further satisfies the following formula (4) and / or formula (5): 3. The polymer electrolyte fuel cell according to claim 1 or 2. 0≦Q1≦Q2 / 10 …(4) Q2≧Q3…(5)

[0025] [Configuration 4] 4. The polymer electrolyte fuel cell according to any one of configurations 1 to 3, wherein the total length L of the cathode gas channel is 190 mm or more and 300 mm or less.

[0026] [Configuration 5] the cathode gas flow passage includes a narrowed portion, 5. The polymer electrolyte fuel cell according to any one of configurations 1 to 4, wherein the number n of the narrowed portions provided in one of the cathode gas channels is 5 or more and 9 or less.

[0027] An embodiment of the present invention will be described in detail below. [1. Polymer electrolyte fuel cell] The polymer electrolyte fuel cell according to the present invention comprises: a membrane electrode assembly in which an anode side catalyst layer and a cathode side catalyst layer are bonded to both sides of an electrolyte membrane; an anode-side gas diffusion layer disposed on the outer side of the anode-side catalyst layer; a cathode-side gas diffusion layer disposed on the outer side of the cathode-side catalyst layer; an anode-side separator disposed on the outer side of the anode-side gas diffusion layer; a cathode-side separator disposed on the outer side of the cathode-side gas diffusion layer; It is equipped with:

[0028] [1.1. Purpose] The polymer electrolyte fuel cell according to the present invention is used to generate power by supplying unhumidified cathode gas to the cathode. When generating electricity by supplying unhumidified cathode gas to a fuel cell, if the operating conditions of the fuel cell fluctuate significantly, the amount of liquid water in the fuel cell is likely to become excessive or insufficient. Therefore, in a fuel cell system without a humidifier, the performance of the fuel cell is likely to deteriorate due to drying or flooding of the electrolyte membrane. In contrast, in the present invention, the structure (cross-flow structure) of the cathode separator and the cathode gas diffusion layer is optimized, so that the performance degradation of the fuel cell due to drying or flooding of the electrolyte membrane is suppressed even under non-humidified conditions. Details of the cross-flow structure will be described later.

[0029] [1.2. Membrane electrode assembly] The membrane electrode assembly (MEA) is composed of a cathode catalyst layer and an anode catalyst layer bonded to both sides of an electrolyte membrane made of a solid polymer electrolyte. The cathode catalyst layer and the anode catalyst layer each consist of a composite of an electrode catalyst and a catalyst layer ionomer. In the present invention, the type of solid polymer electrolyte constituting the electrolyte membrane is not particularly limited, and an optimum material can be selected depending on the purpose. Similarly, the types of the electrode catalyst and catalyst layer ionomer contained in the catalyst layer are not particularly limited, and the most suitable materials can be selected depending on the purpose.

[0030] [1.3. Anode side gas diffusion layer] The anode side gas diffusion layer is disposed on the outer side of the anode side catalyst layer. In the present invention, the structure and material of the anode side gas diffusion layer are not particularly limited, and an optimum one can be selected depending on the purpose. The anode side gas diffusion layer is particularly A water-repellent treated substrate; a water-repellent layer formed on the catalyst layer side surface of the substrate; It is preferable that the above configuration is provided.

[0031] [1.4. Cathode side gas diffusion layer] The cathode side gas diffusion layer is disposed on the outer side of the cathode side catalyst layer. In the present invention, the structure and material of the cathode side gas diffusion layer are not particularly limited as long as they can generate a cross flow as described below, and the most suitable one is selected depending on the purpose. The cathode side gas diffusion layer is particularly A water-repellent treated substrate; a water-repellent layer formed on the catalyst layer side surface of the substrate; It is preferable that the above configuration is provided.

[0032] [1.5. Anode side separator] The anode-side separator is for extracting electrons from the anode-side catalytic layer and supplying an anode gas (fuel gas) to the anode-side catalytic layer. The anode-side separator is disposed on the outer side of the anode-side gas diffusion layer. The anode-side separator is provided with an anode gas flow path for allowing the anode gas to flow. In the present invention, the structure and material of the anode-side separator are not particularly limited, and an optimum one can be selected depending on the purpose.

[0033] [1.6. Cathode side separator] The cathode-side separator is for supplying electrons and cathode gas (oxidant gas) to the cathode-side catalyst layer. The cathode-side separator is disposed on the outer side of the cathode-side gas diffusion layer. The cathode-side separator is provided with a plurality of adjacent cathode gas flow paths for passing the cathode gas. In addition, the two adjacent cathode gas flow paths (first cathode gas flow path, second cathode gas flow path) are partitioned by a rib. In the present invention, the structure and material of the cathode-side separator are not particularly limited as long as they are capable of generating a crossflow, which will be described later, and the optimum structure and material can be selected depending on the purpose.

[0034] [1.7. Cross-flow structure] In the present invention, the cathode separator and the cathode gas diffusion layer have a cross-flow structure.

[0035] Here, the term "cross flow" refers to a gas flow between cathode gas flow channels through the cathode side gas diffusion layer. In other words, "cross flow" means that when the first cathode gas flow path and the second cathode gas flow path are arranged adjacent to each other with a rib in between, all or a part of the cathode gas flowing through either the first cathode gas flow path or the second cathode gas flow path flows to the other path through the cathode-side gas diffusion layer located immediately below the rib.

[0036] The term "crossflow structure" refers to a structure that can generate a predetermined crossflow amount at a predetermined position in the cathode gas flow channel. (a) the structure of the cathode-side separator (e.g., the cross-sectional area of ​​the cathode gas flow channel, the arrangement of the cathode gas flow channel, etc.), and / or (b) The structure of the cathode-side gas diffusion layer (e.g., the in-plane permeability coefficient of the cathode-side gas diffusion layer (particularly, the in-plane permeability coefficient of the cathode-side gas diffusion layer directly under the rib), the thickness of the cathode-side gas diffusion layer (particularly, the thickness of the cathode gas diffusion layer directly under the rib), etc.) It can be controlled by:

[0037] [1.7.1. Equations (1) to (3)] In the present invention, the cross-flow structure satisfies the following formulas (1) to (3), which is different from the conventional structure.

[0038] Q1 <Q2…(1) Q1 <Q3…(2) Q i (i=1, 2, 3)=ktΔP i / μw(cm 3 / min / cm) …(3)

[0039] however, Q1 is the average crossflow volume in the first section (inlet section) where 0≦x / L<0.15; Q2 is the average crossflow in the second section (middle section) where 0.15≦x / L<0.7; Q3 is the average crossflow in the third section (outlet section) where 0.7≦x / L≦1.0; L is the total length of the cathode gas channel, x is the distance from the inlet of the cathode gas channel, k is the in-plane permeability coefficient of the cathode gas diffusion layer, t is the thickness of the cathode side gas diffusion layer, ΔP i is the pressure P in the first cathode gas flow channel in the i-th section i1 and a pressure P in a second gas flow passage adjacent to the first cathode gas flow passage. i2 The absolute value of the difference between μ is the viscosity of the cathode gas, w is the width of a rib that separates the first cathode gas flow channel and the second cathode gas flow channel.

[0040] [A. Section 1, Section 2, Section 3] The "first section" refers to a section where x / L is equal to or greater than 0 and less than 0.15, that is, a section located in the vicinity of the inlet of the cathode gas flow channel. The "second section" refers to a section where x / L is equal to or greater than 0.15 and less than 0.7, that is, a section located in the middle of the cathode gas flow channel. The "third section" refers to a section where x / L is equal to or greater than 0.7 and less than 1.0, that is, a section in the vicinity of the outlet of the cathode gas flow channel.

[0041] When unhumidified cathode gas flows through the cathode gas flow channel, the humidity of the cathode gas flowing through the first section is low. However, water is generated in the cathode gas flow channel by an electrode reaction, and the generated water is carried downstream by the cathode gas. Therefore, the humidity of the cathode gas increases the closer it is to the outlet of the cathode gas flow channel.

[0042] The position of x / L=0.15 corresponds to the lower limit of the section where performance improvement can be expected by generating a relatively large cross flow. At the position of x / L=0.15, the cathode gas is sufficiently humidified by the generated water. For example, when power is generated by flowing unhumidified cathode gas through a cathode gas flow path having a total length L of 200 to 300 mm, the position of x / L=0.15 corresponds to the position where the relative humidity of the cathode gas is about 20% RH. On the other hand, at a position where x / L is less than 0.15, the relative humidity of the cathode gas is low.

[0043] Therefore, if a large cross flow is generated in the first section, the electrolyte membrane may dry out, which may result in a decrease in fuel cell performance. On the other hand, even if a cross flow is generated in the section where x / L is 0.15 or more, the electrolyte membrane is less likely to dry out. Rather, it is expected that performance will improve as liquid water is discharged from the cathode-side gas diffusion layer.

[0044] The position of x / L=0.7 corresponds to the upper limit of the range where performance can be improved by increasing the crossflow amount. The amount of water generated increases as you approach the outlet of the cathode gas flow channel, making it difficult to completely drain the liquid water that has accumulated in the cathode-side gas diffusion layer due to the crossflow. Therefore, even if the crossflow rate is further increased in the section where x / L is 0.7 or more, little improvement in performance can be expected. On the contrary, a further increase in the crossflow rate in the outlet section may lead to an increase in pressure loss.

[0045] [B. Average Cross Flow] The "average crossflow amount (of the i-th section)" refers to the average value of the crossflow amount occurring within the section. Equations (1) to (3) mean that when the cathode gas flow path is divided into three sections, a first section, a second section, and a third section, the average crossflow volume Q1 of the first section is smaller than the average crossflow volume Q2 of the second section and the average crossflow volume Q3 of the third section.

[0046] When Q1 is larger than Q2 and Q3, the electrolyte membrane dries out due to cross-flow in the first section, and the proton conductivity of the electrolyte membrane decreases. On the other hand, in the second and / or third sections, a large amount of liquid water may remain in the cathode-side gas diffusion layer immediately below the rib, which may hinder the supply of oxygen to the cathode-side catalyst layer. On the other hand, if Q1 is made smaller than Q2 and Q3, it is possible to suppress drying of the electrolyte membrane in the first section. Also, in the second and third sections, the excess liquid water remaining in the cathode-side gas diffusion layer can be discharged to the cathode gas flow channel by the cross flow.

[0047] [1.7.2. Equations (4) and (5)] The cross-flow structure may further satisfy the following formula (4) and / or formula (5) in addition to the above formulas (1) to (3). A cross-flow structure that further satisfies formula (4) and / or formula (5) may exhibit higher performance than a cross-flow structure that only satisfies formulas (1) to (3). 0≦Q1≦Q2 / 10 …(4) Q2≧Q3…(5)

[0048] Equation (4) means that the average crossflow amount Q1 in the first section should be as close to zero as possible. As described above, the humidity of the cathode gas is low in the first section, so if excessive crossflow occurs in the first section, the electrolyte membrane is likely to dry out. In contrast, optimizing Q1 to satisfy equation (4) can prevent the electrolyte membrane from drying out.

[0049] Equation (5) means that the crossflow volume Q3 in the third section is equal to or less than the crossflow volume Q2 in the second section. As mentioned above, even if Q3 is made larger than Q2, the performance improvement due to the crossflow is small and may even result in an increase in pressure loss. In contrast, optimizing Q3 to satisfy equation (5) can suppress the increase in pressure loss.

[0050] [1.7.3. Total length of cathode gas passage] In the present invention, the total length L of the cathode gas flow channel is not particularly limited as long as it is possible to generate the above-mentioned cross flow, and an optimal length can be selected depending on the purpose.

[0051] When unhumidified cathode gas is passed through the cathode gas flow channel, if L is too short, the cathode gas is discharged from the cathode gas flow channel before being sufficiently humidified. As a result, the proportion of the region that is easily dried out increases in the entire flow channel, and performance may decrease. Therefore, L is preferably 190 mm or more. L is preferably 200 mm or more. On the other hand, if L is too long, the ratio of the area in the cathode gas diffusion layer where liquid water is likely to accumulate increases, and performance may decrease. Therefore, L is preferably 300 mm or less.

[0052] [2. Specific examples of cathode side separators] In the present invention, the structure of the cathode side separator is not particularly limited as long as it is capable of generating a cross flow. The structure of the cathode separator is, for example, (a) A flow channel structure with a constriction. (b) Alternating blockage type flow channel structure; (c) End-narrowed flow channel structure The cathode-side separator may include any one of these structures, or may include two or more of them.

[0053] [2.1. Cathode-side separator with a flow channel structure with a narrowed section] [2.1.1. Definition] "Flow path structure with a narrowed section" means (a) A plurality of cathode gas flow paths, each open at both ends, are arranged in one direction; (b) At least one cathode gas flow channel has a non-uniform cross-sectional area and has a narrowed portion (a region where the cross-sectional area of ​​the flow channel is locally reduced) in the middle of the flow channel. This refers to the structure.

[0054] Note that "multiple cathode gas flow channels are arranged in one direction" does not necessarily mean that the multiple cathode gas flow channels are arranged perfectly parallel (the angle between the center lines of two cathode gas flow channels is zero), but means that the arrangement of the multiple cathode gas flow channels may deviate slightly from perfectly parallel as long as the cathode gas can flow in approximately the same direction. The angle between the center lines of the two cathode gas flow channels is preferably 10° or less, or 5° or less.

[0055] In a cathode-side separator having a flow path structure with narrowed portions, the cathode gas is introduced from one end of each cathode gas flow path and flows in the same direction within each cathode gas flow path. When the cathode gas introduced into the cathode gas flow path reaches the narrowed portion, the pressure of the cathode gas increases. As a result, a part of the cathode gas flows into the adjacent cathode gas flow path through the cathode-side gas diffusion layer located immediately below the rib (i.e., a cross flow occurs). In this case, the amount of cross flow in the inlet section, middle section, and outlet section can be controlled by optimizing the number, position, cross-sectional area, etc. of the narrowed portions.

[0056] [2.1.2. Cross flow volume] When the cathode-side separator has a flow channel structure with a narrowed portion, i.e., a first cathode gas flow channel and a second cathode gas flow channel arranged in parallel with each other across a rib; A narrowed portion provided in the first cathode gas flow channel and / or the second cathode gas flow channel; In the case where the cross-flow structure is provided with the above formulae (1) to (3), it is preferable that the cross-flow structure further satisfies the above formulae (4) and / or (5).

[0057] When the cathode-side separator has a flow path structure with a narrowed portion, by optimizing the shape, position, number, etc. of the narrowed portion, a cross-flow structure that satisfies formulas (1) to (3), or a cross-flow structure that further satisfies formulas (4) to (5) in addition to formulas (1) to (3), can be obtained. A cross-flow structure that further satisfies formula (4) and / or formula (5) exhibits higher performance than a cross-flow structure that only satisfies formulas (1) to (3).

[0058] 2.1.3. Number of stenoses When the cathode gas flow path has a narrowed portion, the number n of narrowed portions is not particularly limited as long as it is possible to generate the above-mentioned crossflow, and an optimal number can be selected depending on the purpose.

[0059] If n is too small, it becomes difficult to generate an appropriate average crossflow amount in each section. As a result, the performance improvement due to the crossflow becomes small, and the required output may not be achieved. Therefore, n is preferably 5 or more. On the other hand, if n is too large, the pressure loss increases. In addition, the pump pressure for supplying air also increases, which may reduce the energy efficiency of the fuel cell system. Therefore, n is preferably 9 or less.

[0060] [2.2. Cathode-side separator with alternating blocked flow channel structure] The "alternate blocked flow channel structure" is (a) A plurality of cathode gas flow paths are arranged in one direction; (b) A first cathode gas flow channel with a blocked outlet side and a second cathode gas flow channel with a blocked inlet side are disposed adjacent to each other. This refers to the structure.

[0061] In a cathode-side separator having an alternating blocked flow channel structure, cathode gas is introduced into the inlet of a first cathode gas flow channel. Since the outlet of the first cathode gas flow channel is blocked, when cathode gas is introduced into the first cathode gas flow channel, the pressure in the first cathode gas flow channel increases. As a result, the cathode gas in the first cathode gas flow channel flows into the adjacent second cathode gas flow channel by cross flow. The cathode gas that has flowed into the second cathode gas flow channel is discharged from the outlet of the second cathode gas flow channel.

[0062] In this case, the crossflow amounts in the inlet section, middle section, and outlet section can be controlled by optimizing the in-plane permeability coefficient of the cathode gas diffusion layer, the thickness of the cathode gas diffusion layer, etc. In other words, by optimizing the material and structure of the cathode gas diffusion layer, a crossflow structure that satisfies formulas (1) to (3), or a crossflow structure that further satisfies formulas (4) to (5) in addition to formulas (1) to (3), can be obtained. The in-plane permeability coefficient of the cathode side gas diffusion layer can be controlled, for example, by the penetration depth of the water-repellent layer (microporous layer) into the substrate. The amount of cross flow can also be controlled by, for example, the height and width of the ribs and the thickness of the cathode side gas diffusion layer immediately below the ribs.

[0063] [2.3. Cathode-side separator with closed-end flow channel structure] "End narrowing type flow channel structure" means (a) A plurality of cathode gas flow paths are arranged in one direction; (b) A first cathode gas flow passage having a narrowed outlet side and a second cathode gas flow passage having a narrowed inlet side are disposed adjacent to each other. This refers to the structure.

[0064] In a cathode-side separator having an end-narrowed flow channel structure, cathode gas is introduced from one end of the first and second cathode gas channels and flows in the same direction in the first and second cathode gas channels. Because the outlet of the first cathode gas channel is narrowed, when cathode gas is introduced into the first cathode gas channel, the pressure in the first cathode gas channel increases. As a result, part of the cathode gas in the first cathode gas channel flows into the adjacent second cathode gas channel due to cross flow.

[0065] In this case, the crossflow amounts in the inlet section, middle section, and outlet section can be controlled by optimizing the in-plane permeability coefficient of the cathode gas diffusion layer, the thickness of the cathode gas diffusion layer, etc. In other words, by optimizing the material and structure of the cathode gas diffusion layer, a crossflow structure that satisfies formulas (1) to (3), or a crossflow structure that further satisfies formulas (4) to (5) in addition to formulas (1) to (3), can be obtained.

[0066] [3. Effect] In a polymer electrolyte fuel cell having a laminated structure of MEA / gas diffusion layer / separator, water is likely to accumulate in the cathode-side gas diffusion layer (particularly in the cathode-side gas diffusion layer directly below the rib of the cathode-side separator). In contrast, when the cathode-side separator and the cathode-side gas diffusion layer have a cross-flow structure, the water that has accumulated in the cathode-side gas diffusion layer is likely to be discharged to the gas flow path by the cross-flow.

[0067] However, even when the cathode separator and the cathode gas diffusion layer have a cross-flow structure, if the flow path structure or the gas diffusion layer structure is inappropriate, the pressure loss may increase. Furthermore, in the case of fuel cells sized for vehicle use, the vapor pressure in the gas flow channel increases from the inlet to the outlet due to water produced during power generation. Under high humidification conditions, the cross-flow expels liquid water from the gas diffusion layer, improving performance. On the other hand, under low humidification conditions, the cross-flow dries out the electrolyte membrane, which can reduce performance. This effect is particularly noticeable when generating power without a humidifier.

[0068] Therefore, when the cathode-side separator and the cathode-side gas diffusion layer have a crossflow structure, if the average crossflow amount Q1 in the inlet section of the cathode gas flow channel is greater than the average crossflow amount Q2 in the middle section and the average crossflow amount Q2 in the outlet section, the electrolyte membrane is likely to dry out on the upstream side of the cathode gas flow channel, and flooding is likely to occur on the downstream side of the cathode gas flow channel.

[0069] On the other hand, when the cathode separator and the cathode gas diffusion layer have a cross-flow structure, if Q1 is smaller than Q2 and Q3, drying of the electrolyte membrane in the inlet section and flooding in the middle section and the outlet section can be suppressed, and as a result, a local decrease in current density in the plane of the electrolyte membrane can be suppressed. Furthermore, by optimizing the cross-flow rate from the inlet to the outlet of the cathode gas flow path, it is possible to improve the performance of a fuel cell without increasing pressure loss, even when operating a vehicle-sized fuel cell without humidification. EXAMPLES

[0070] [1. Preparation of fuel cell] Figure 1 shows the cross-sectional area ratio (S 2in / S 1in ) is the cross-sectional area ratio of the outlet (S 2out / S 1out 1 shows a schematic diagram of a separator having a structure different from that of the separator 10 shown in FIG. 1. In FIG. 1, a separator 10 has a rib 12, and a first cathode gas flow channel 14 and a second cathode gas flow channel 16 arranged in parallel with the rib 12 in between.

[0071] A first gas inlet pipe 14a is connected to the inlet of the first cathode gas flow passage 14, and a first gas exhaust pipe 14b is connected to the outlet of the first cathode gas flow passage 14. The cross-sectional area (S 1in ) is the cross-sectional area (S 1out ) is larger. On the other hand, a second gas introduction pipe 16a is connected to the inlet of the second cathode gas flow passage 16, and a second gas exhaust pipe 16b is connected to the outlet of the second cathode gas flow passage 16. The cross-sectional area (S 2in ) is the cross-sectional area (S 2out ) is smaller than the separator 10. 2in / S 1in 2out / S 1out It satisfies the relationship.

[0072] ​ When gas is supplied to each of the first cathode gas flow channel 14 and the second cathode gas flow channel 16 of the separator 10 having such a structure, the pressure in the first cathode gas flow channel 14 becomes higher than the pressure in the second cathode gas flow channel 16. As a result, a part of the gas supplied to the first cathode gas flow channel 14 is pushed out through the gas diffusion layer 18 to the second cathode gas flow channel 16.

[0073] As shown in FIG. 1, the cathode separator used was a separator 10 in which the diameter of the pipes connected to the gas flow path was alternately narrowed. The anode separator used was a separator in which the diameter of the pipes connected to the gas flow path was the same. A cathode gas diffusion layer, a Nafion (registered trademark) membrane coated with a catalyst layer on both sides, and an anode gas diffusion layer were sandwiched between these separators to produce a fuel cell. The length of the gas flow path was 6 mm.

[0074] 2. Test Method Using this fuel cell, the current density and the amount of liquid water in the gas diffusion layer were measured while maintaining a voltage of 0.2 V. Table 1 shows the cell temperature during power generation and the relative humidity (RH) of the gas supplied to the cathode. Under each of the conditions shown in Table 1, power generation was performed while changing the amount of crossflow, and the current density and amount of liquid water were measured. The amount of crossflow was adjusted by installing a needle valve just before the gas inlet in Figure 1.

[0075] The liquid water distribution during power generation was quantified using X-ray radiography as described in Reference 1. [Reference 1] D. Hayashi et al., Synchrotoron X-Ray Visualization and Simulation for Operating Fuel Cell Diffusion Layers, SAE, 2017-01-1188

[0076] [Table 1]

[0077] [3. Results] [3.1. Changes in current density and liquid volume due to crossflow] Figure 2 shows the relationship between the crossflow amount, current density, and liquid water amount when the cell temperature is 40° C. Figure 3 shows the relationship between the crossflow amount, current density, and liquid water amount when the cell temperature is 60° C. Figure 4 shows the relationship between the crossflow amount and current density when the cell temperature is 80° C.

[0078] 2 to 4 show that the extent of the decrease in the amount of liquid water with an increase in cross flow and the extent of the improvement in performance with an increase in cross flow vary depending on the temperature and the relative humidity of the cathode supply gas. When the temperature was 80°C, no liquid water was observed. There was also a tendency for the decrease in the amount of liquid water and the improvement in performance with an increase in cross flow to increase as the temperature decreased.

[0079] [3.2. Relationship between distance x from flow path inlet and relative humidity RH] The relative humidity distribution in the flow channels of a polymer electrolyte fuel cell was calculated using computational fluid dynamics calculations as shown in Reference 2. Figure 5 shows the relationship between the distance x from the flow channel inlet and the relative humidity when the cell temperature is 80°C. Figure 6 shows the relationship between the distance x from the flow channel inlet and the relative humidity when the cell temperature is 60°C. [Reference 2] Chao-Yang Wang, Chem. Rev, 2004, 104, 4727-4766, Fundamental Models for Fuel Cell Engineering

[0080] From the graphs in Figures 5 and 6, the relative humidity RH at the position where crossflow occurs (distance x from the flow path inlet) can be calculated as a parameter at that position and temperature. The amount of liquid water at that position and temperature can be calculated from that RH and temperature and the experimental data in Figures 2 to 4. Furthermore, once the amount of liquid water at that position is known, the reduction in the amount of crossflow due to liquid water and the improvement in performance due to the crossflow, including the reduction in the amount of crossflow (increase in current density), can be calculated from Reference 3. By repeating such calculations for each distance x from the flow path inlet, the crossflow position at which performance can be improved and the amount of crossflow at that position can be calculated.

[0081] The effect of liquid water on the cross-flow rate was calculated using the results from Reference 3. [Reference 3] IS Hussaini, CY Wang, Measurement of relative permeabolity of fuel cell diffusion media, J. Power Sources, Vol. 195(2010), 3830-3840

[0082] Table 2 shows the sum of the current values ​​when the average cross flow rates Q1 to Q3 in the first to third sections are changed when the total length L of the gas flow path is 280 mm. The electrode area is 11.2 cm 2 It was assumed that: Table 3 shows the sum of the current values ​​when the average cross flow rates Q1 to Q3 in the first to third sections are changed when the total length L of the gas flow path is 200 mm. The electrode area is 8.1 cm 2 It was assumed that: It should be noted that "the sum of the current values" refers to the sum of the current values ​​at 40°C, 60°C, and 80°C.

[0083] The following can be seen from Tables 2 and 3. (1) The fuel cells satisfying formulas (1) and (2) (Examples 1 to 6) had a larger sum of current values ​​than the fuel cells not satisfying formula (1) (Comparative Examples 1 and 2). (2) The fuel cell units (Examples 4 and 5) which further satisfied formula (4) had a larger sum of current values ​​than the fuel cell unit (Example 6) which did not satisfy formula (4). (3) The fuel cells (Examples 1 and 4) which further satisfied formula (5) had a larger sum of current values ​​than the fuel cells (Examples 2 and 5) which did not satisfy formula (5).

[0084] [Table 2]

[0085] [Table 3]

[0086] [3.3. Total length of gas flow path L] A simulation was used to investigate the effect of the total length L of the gas flow channel on the total current value when unhumidified cathode gas was passed through a cathode gas flow channel with a narrowed section. The flow channel structure of the cathode side separator was a structure in which n cathode gas flow channels with a total length L were arranged in parallel. Furthermore, each flow channel structure had the same L×n, but L and n were different. There were five narrowed sections, arranged so that Q1=0 and Q2>Q3>0. Figure 7 shows the relationship between the total length L of the cathode gas flow channel and the total current value.

[0087] As shown in FIG. 7, when L was made excessively short and the number of flow paths was increased, the total current value ultimately decreased. This is because the proportion of the area that is easily dried out increases among all the flow paths. Conversely, when L was made excessively long and the number of flow paths was reduced, the total current value ultimately decreased. This is because the number of narrowed parts is finite, and therefore the range of all the flow paths where the performance improvement due to the narrowed parts can be obtained is limited. From FIG. 7, it can be seen that L is preferably 190 mm to 300 mm.

[0088] 3.4. Number of stenoses A simulation was used to investigate the effect of the number of constrictions on pressure loss and performance when unhumidified cathode gas was passed through a cathode gas flow channel equipped with constrictions. The flow channel structure of the cathode side separator was a structure in which eight cathode gas flow channels with a total length of 280 mm were arranged in parallel. The constrictions were arranged so that Q1=0 and Q2>Q3>0. Figure 8 shows the relationship between the number of constrictions and pressure loss. Figure 9 shows the relationship between the number of constrictions and performance.

[0089] As shown in FIG. 8, the more the number of narrowed portions, the greater the pressure loss. When the pressure loss increases, the pump pressure for air supply also increases, and the energy efficiency of the fuel cell system decreases. On the other hand, as shown in FIG. 9, if there are fewer narrowed portions, the performance improvement due to cross flow becomes small, and the required output cannot be achieved. From FIG. 8 and FIG. 9, it can be seen that the number of narrowed portions provided in one cathode gas flow channel is preferably 5 to 9.

[0090] Although the embodiment of the present invention has been described in detail above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the gist of the present invention. [Industrial Applicability]

[0091] The polymer electrolyte fuel cell according to the present invention can be used as an on-board power source, a small stationary generator, and the like.

Claims

1. A polymer electrolyte fuel cell having the following configuration. (1) The solid polymer electrolyte fuel cell is a membrane electrode assembly in which an anode side catalyst layer and a cathode side catalyst layer are bonded to both sides of an electrolyte membrane; an anode-side gas diffusion layer disposed on the outer side of the anode-side catalyst layer; a cathode-side gas diffusion layer disposed on the outer side of the cathode-side catalyst layer; an anode-side separator disposed on the outer side of the anode-side gas diffusion layer; a cathode-side separator disposed on the outer side of the cathode-side gas diffusion layer; It is equipped with: (2) The solid polymer fuel cell is used to generate power by supplying unhumidified cathode gas to the cathode. (3) The cathode-side separator and the cathode-side gas diffusion layer have a structure (cross-flow structure) that generates a gas flow (cross flow) between the cathode gas flow paths through the cathode-side gas diffusion layer, The cross-flow structure satisfies the following formulas (1) to (3). Q 1 <Q 2 …(1) Q 1 <Q 3 …(2) Q i (i=1、2、3)=ktΔP i / μw(cm 3 / min / cm) …(3) however, Q 1 is the average cross flow volume in the first section (inlet section) where 0≦x / L<0.15, Q 2 is the average cross flow volume in the second section (middle section) where 0.15≦x / L<0.7; Q 3 is the average crossflow volume in the third section (outlet section) where 0.7≦x / L≦1.0; L is the total length of the cathode gas flow channel, x is the distance from the inlet of the cathode gas channel, k is the in-plane permeability coefficient of the cathode gas diffusion layer, t is the thickness of the cathode side gas diffusion layer, ΔP i is the pressure P in the first cathode gas flow channel in the i-th section i1 and a pressure P in a second cathode gas flow passage adjacent to the first cathode gas flow passage. i2 The absolute value of the difference between μ is the viscosity of the cathode gas, w is the width of a rib that separates the first cathode gas flow passage and the second cathode gas flow passage.

2. The cathode side separator is (a) A flow channel structure having a narrowed portion; (b) an alternating blocked flow channel structure; and (c) End-narrowed flow channel structure 2. The polymer electrolyte fuel cell according to claim 1, comprising at least one structure selected from the group consisting of:

3. The cathode side separator is The first cathode gas flow channel and the second cathode gas flow channel are arranged in parallel with each other across the rib; a narrowed portion provided in the first cathode gas flow channel and / or the second cathode gas flow channel; Equipped with The cross-flow structure further satisfies the following formula (4) and / or formula (5): The polymer electrolyte fuel cell according to claim 1 . 0≦Q 1 ≦Q 2 / 10 …(4) Q 2 ≧Q 3 …(5)

4. 2. The polymer electrolyte fuel cell according to claim 1, wherein the total length L of the cathode gas flow channel is 190 mm or more and 300 mm or less.

5. the cathode gas flow passage includes a narrowed portion, 2. The polymer electrolyte fuel cell according to claim 1, wherein the number n of the narrowed portions provided in one cathode gas flow channel is 5 or more and 9 or less.

Citation Information

Patent Citations

  • Fuel cell

    JP2005056671A

  • Fuel cell stack and separator

    JP2011086519A

  • Fuel battery

    JP2011150801A

  • Fuel cell porous separator

    JP2013125744A

  • Separator for fuel cell

    JP2022169222A