Solar cell module for laminated glass and method for producing the same, and laminated glass and method for producing the same
The encapsulation of solar cells in a rigid resin film with a minimal refractive index difference and adhesive layer addresses the load and disconnection issues in laminated glass, ensuring secure positioning and efficient power generation.
Patent Information
- Application Number
- JP2023046522
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Encapsulating solar cells within laminated glass poses a risk of load application to the peripheral portions and wiring due to their high rigidity, especially in curved configurations, which can lead to scratches and disconnection.
A solar cell module for laminated glass comprising a plurality of solar cells encapsulated in a rigid resin film with an adhesive layer, where the refractive index difference between the resin film and adhesive layer is minimal, and the resin film has a Young's modulus of 500 MPa or more, ensuring the solar cells and wiring are protected and securely positioned.
The solution effectively alleviates load on the peripheral portions and wiring of solar cells, enhancing handling properties and preventing scratches and disconnection, while maintaining high power generation efficiency.
Smart Images

Figure 2024135705000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a solar cell module for laminated glass and a manufacturing method thereof, and to laminated glass and a manufacturing method thereof. [Background technology]
[0002] Vehicle window glass is glass that can be installed in the opening of a vehicle, and is subject to a wide range of regulations. For example, there are UN Regulation No. 43 "Uniform Provisions for Approval of Safety Glazing Materials and Their Installation in Vehicles" and domestic standards such as JIS R3211 (2015) "Automotive Safety Glass" and JIS R3212 (2015) "Test Methods for Automotive Safety Glass". These regulations refer to safety glass that aims to reduce personal injury in the event of breakage, and laminated glass is included in the category of safety glass. Laminated glass is made by bonding multiple glass sheets together with a resin adhesive layer, also commonly referred to as an interlayer film.
[0003] In recent years, the inclusion of various functional films inside laminated glass has been considered. For example, Patent Document 1 discloses a specific laminated glass comprising a pair of glass plates facing each other and specific interlayers in contact with the facing surfaces of the pair of glass plates. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2017 / 099167 Summary of the Invention [Problem to be solved by the invention]
[0005] In recent years, the inclusion of solar cells inside laminated glass has also been considered. From the viewpoint of power generation efficiency, it is desirable to enclose a plurality of solar cells in an array inside the laminated glass. A plurality of solar cells usually each have high rigidity, and in the case of curved laminated glass, for example, there is a risk that loads will be generated on the periphery of the solar cells and on the wiring between the solar cells.
[0006] In view of the above problems, the present disclosure provides a solar cell module suitable for laminated glass and a manufacturing method thereof, as well as laminated glass using the solar cell and a manufacturing method thereof. [Means for solving the problem]
[0007] The present disclosure provides a solar cell module, laminated glass, and methods for manufacturing the same, having the following configurations. [1] A resin film; A solar cell module for laminated glass comprising: a resin film; and a plurality of solar cells disposed inside the resin film. [2] The solar cell module for laminated glass according to [1], further comprising an adhesive layer between the solar cell and the resin film. [3] The solar cell module for laminated glass according to [2], wherein the absolute value of the difference between the refractive index n1 of the resin film and the refractive index n2 of the adhesive layer, |n1-n2|, is 0.5 or less. [4] The solar cell module for laminated glass according to any one of [1] to [3], wherein the resin film has a Young's modulus at 23° C. of 500 MPa or more. [5] The plurality of solar cells are arranged in a first direction and a second direction intersecting the first direction, The solar cell module for laminated glass according to any one of [1] to [4], wherein adjacent solar cells are electrically connected to each other by wiring to form a solar cell group. [6] The solar cell module for laminated glass according to any one of [1] to [5], wherein the resin film has a curved shape. [7] The solar cell module for laminated glass according to any one of [1] to [6], wherein the solar cell is a silicon solar cell. [8] A solar cell module comprising: a first glass plate; a second glass plate; an intermediate layer provided between the first and second glass plates; and a solar cell module provided within the intermediate layer; The solar cell module is a solar cell module for laminated glass according to any one of [1] to [7]. [9] The laminated glass according to [8], wherein the Young's modulus of the intermediate layer is lower than the Young's modulus of the resin film.
[10] The laminated glass according to [8] or [9], wherein the Young's modulus of the intermediate layer at 23° C. is 100 MPa or less.
[11] The laminated glass according to any one of [8] to
[10] , wherein the absolute value of the refractive index difference between the refractive index n1 of the resin film included in the solar cell module and the refractive index n3 of the intermediate layer, |n1-n3|, is 0.5 or less.
[12] The laminated glass according to any one of [8] to
[11] , wherein the solar cell module is a solar cell module having an adhesive layer, and the intermediate layer and the adhesive layer contain the same resin.
[13] A method for producing a solar cell module for laminated glass according to any one of [1] and [3] to [7], comprising the steps of: A method for producing a solar cell module for laminated glass, comprising laminating a solar cell and a first resin film in this order on a second resin film, and applying pressure while heating.
[14] A method for producing a solar cell module for laminated glass according to any one of [1] and [3] to [7], comprising the steps of: A manufacturing method for a solar cell module for laminated glass, in which a solar cell is placed inside a bag-shaped first resin film and heated while degassing.
[15] A method for producing a solar cell module for laminated glass according to any one of [2] to [7], comprising the steps of: A method for producing a solar cell module for laminated glass, comprising laminating and adhering a second adhesive layer, a solar cell, a first adhesive layer, and a first resin film in this order onto a second resin film.
[16] A method for producing a solar cell module for laminated glass according to any one of [2] to [7], comprising the steps of: A frame-shaped pattern adhesive layer is disposed on the second resin film; A solar cell covered with an adhesive composition is placed within the frame pattern; A method for producing a solar cell module for laminated glass, comprising laminating a first resin film onto the adhesive composition.
[17] A solar cell module for laminated glass according to any one of [1] to [7] is prepared, A method for producing laminated glass, comprising laminating a second glass plate, a second intermediate layer, the solar cell module, a first intermediate layer and a first glass plate in this order, and bonding them under pressure. Effect of the Invention
[0008] The present invention provides a solar cell module suitable for laminated glass and a method for producing the same, as well as laminated glass using the solar cell and a method for producing the same. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is an exploded perspective view of a laminated glass according to an embodiment. [Diagram 2] 1 is a cross-sectional view of a solar cell module according to a first embodiment. [Diagram 3] FIG. 2 is a schematic diagram for explaining the arrangement of solar cells. [Figure 4] FIG. 11 is a cross-sectional view of a solar cell module according to a second embodiment. [Diagram 5] 1A to 1C are schematic diagrams illustrating a method for manufacturing a solar cell module according to a first embodiment. [Figure 6] 1A to 1C are schematic diagrams illustrating a method for manufacturing a solar cell module according to a first embodiment. [Figure 7] 5A to 5C are schematic diagrams showing a method for manufacturing a solar cell module according to a second embodiment. [Figure 8] 5A to 5C are schematic diagrams showing a method for manufacturing a solar cell module according to a second embodiment. [Figure 9] FIG. 1 is a cross-sectional view of a laminated glass according to an embodiment. [Figure 10]FIG. 2 is a schematic diagram showing a method for producing laminated glass according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The present invention will be described below through embodiments of the invention, but the invention according to the claims is not limited to the following embodiments. Furthermore, not all of the configurations described in the embodiments are necessarily essential as means for solving the problems. In each embodiment, the same configurations are denoted by the same reference numerals, and the description thereof will be omitted or simplified. For clarity of explanation, the following description and drawings may be simplified as appropriate, and the scale of each component may differ significantly. For clarity of explanation, one direction of the main surface of the object may be the X-axis, one direction of the main surface of the object perpendicular to the X-axis may be the Y-axis, and the normal direction of the main surface of the object may be the Z-axis. Note that the XY plane may be a curved surface. Unless otherwise specified, "~" indicating a numerical range includes the numerical values before and after it as the lower and upper limits. The outer edge of an object is referred to as the "periphery," and the area of the object that is adjacent to the "periphery" and has a certain width is referred to as the "periphery portion." Furthermore, the "solar cell module for laminated glass" may be simply referred to as the "solar cell module."
[0011] [Laminated glass solar cell module] 1 is an exploded perspective view of a laminated glass described below. A solar cell module 100 according to this embodiment can be suitably used as a solar cell module provided inside a laminated glass 200 including a first glass plate 11, a second glass plate 12, and an intermediate layer 20 provided between the first and second glass plates. In this specification, the first glass plate 11 refers to a glass plate that is disposed on a surface on which sunlight is incident when the laminated glass 200 is installed. That is, for example, when the laminated glass 200 is attached to a vehicle, the first glass plate 11 is a glass plate that is disposed on the exterior side of the vehicle. The second glass plate 12 refers to an interior glass plate that faces the interior side of the vehicle when the laminated glass 200 is attached to the vehicle. The first glass plate 11 and the second glass plate 12 are joined together with an intermediate layer 20 sandwiched therebetween.
[0012] First Embodiment The solar cell module according to the first embodiment will be described with reference to Fig. 2. Fig. 2 is a ZX cross-sectional view of the solar cell module. The solar cell module 100 according to the first embodiment includes a plurality of solar cells 41 arranged inside a resin film 30. The solar cells 41 are usually electrically connected to each other by wiring 42, forming a solar cell group 40.
[0013] In the solar cell module according to the first embodiment, the solar cell group 40 is encapsulated in the resin film 30 with high rigidity, so that even when applied to, for example, curved laminated glass, the load acting on the peripheral parts of the solar cells 41 and the wiring 42 between the solar cells is mitigated. Furthermore, this solar cell module has excellent handleability during the manufacture of laminated glass, and scratches on the solar cells and breaks in the wiring can be suppressed.
[0014] (Resin film) From the viewpoint of protecting the solar cell and wiring, the resin film 30 preferably has a higher rigidity than the intermediate layer of the laminated glass described later. Specifically, the Young's modulus of the resin film 30 at 23° C. is preferably 500 MPa or more, more preferably 750 MPa or more, and even more preferably 1,000 MPa or more. On the other hand, the upper limit of the Young's modulus is not particularly limited, but is usually 5 GPa or less. Here, the Young's modulus is determined as the slope of the linear portion of a strain-stress curve obtained at 23° C. by a tensile test in accordance with Japanese Industrial Standard JIS K7127:1999.
[0015] From the viewpoint of power generation efficiency of the solar cell module, the resin film 30 preferably has excellent light transmittance. For example, the total light transmittance of the resin film 30 is preferably 60% or more, more preferably 70% or more, and even more preferably 80% or more. The total light transmittance of the resin film is usually less than 100%. The total light transmittance is a value measured in accordance with JIS K7375:2008.
[0016] The refractive index n1 of the resin film 30 is preferably 1.1 to 1.8, more preferably 1.2 to 1.7, and even more preferably 1.25 to 1.65, in order to easily reduce the difference in refractive index between the resin film 30 and an adhesive layer or intermediate layer described below.
[0017] The material of the resin film 30 may be appropriately selected from those satisfying the above physical properties, and may be a thermosetting resin or a thermoplastic resin. When a thermoplastic resin is used as the resin for the resin film, the glass transition temperature of the thermoplastic resin is preferably lower than the glass transition temperature of the intermediate layer described below, in order to suppress the flow of the resin during the production of the laminated glass.
[0018] Specific examples of resins used for the resin film 30 include, for example, polyethylene terephthalate, polyethylene naphthalate, polyamide, polyether, polysulfone, polyethersulfone, polycarbonate, polystyrene, cyclic polyolefin, polyarylate, polyetherimide, polyetheretherketone, polyimide, aramid, polybutylene terephthalate, triacetyl cellulose, polyurethane, and cycloolefin polymer.
[0019] The resin film 30 may further contain other components within the scope of the effects of the present invention, such as various additives such as an infrared absorbing agent, an ultraviolet absorbing agent, a fluorescent agent, an adhesion regulator, a coupling agent, a surfactant, an antioxidant, a heat stabilizer, a light stabilizer, a dehydrating agent, an antifoaming agent, an antistatic agent, and a flame retardant.
[0020] The shape of the resin film 30 may be such that the main surface is flat, or may be curved as shown in Fig. 2. When the solar cell module 100 is used for manufacturing laminated glass having a curved main surface, the resin film 30 preferably has a shape that follows the curved shape of the glass plate used in the laminated glass. However, since the resin film 30 has flexibility, it can be used suitably even if it does not completely match the curvature of the glass plate.
[0021] (Solar cell) Next, the arrangement of the solar cell enclosed in the solar cell module will be described with reference to FIG. 3. The solar cell group 40 shown in the example of FIG. 3 is arranged in a two-dimensional array of A1 to D4, with A1, A2, A3, and A4 arranged in a first direction (e.g., X-axis direction) and A1, B1, C1, and D1 arranged in a second direction (e.g., Y-axis direction) intersecting the first direction. That is, the first direction and the second direction are included in a plane perpendicular to the thickness direction of the solar cell module and are non-parallel to each other. Adjacent solar cells are electrically connected to each other by wiring 42 (not shown in FIG. 3) to form the solar cell group 40. The shape, size, and number of the main surface of the solar cell 41 are not particularly limited, and may be appropriately designed according to the shape, size, and the like of the laminated glass.
[0022] The type of solar cell 41 is not particularly limited, and may be appropriately selected and used. Specific examples of solar cells include gallium arsenide solar cells; silicon solar cells such as single crystal silicon, polycrystalline silicon, and amorphous silicon; perovskite solar cells; CIS solar cells, and CIGS solar cells, and these may be used in combination. Since the solar cell module of this embodiment is suitable for laminated glass applications even if the solar cell has high rigidity, silicon solar cells are preferred, and single crystal silicon solar cells are more preferred. The wiring may be any of a metal foil film, a transparent conductive film, a conductor on a wire, and the like.
[0023] The thickness of the solar cell is preferably 0.1 μm or more, more preferably 10 μm or more, and even more preferably 150 μm or more, from the viewpoint of the performance of the solar cell, etc. On the other hand, the thickness of the solar cell is preferably 500 μm or less, more preferably 450 μm or less, and even more preferably 150 μm or less, from the viewpoint of ease of manufacturing a solar cell module with a curved main surface, etc. A suitable thickness of the solar cell is, for example, 0.1 μm to 500 μm, preferably 10 μm to 450 μm, and more preferably 150 μm to 400 μm. The thickness of the resin film 30 is preferably 50 μm to 500 μm. The thickness of the resin film 30 may be measured at a position that does not overlap with the solar cell group 40 in a plan view. For example, it may be measured at a position (e.g., position P in FIG. 3) in the gap between the solar cells in the center of the solar cell module 100 and that does not overlap with the wiring 42. Note that when the resin film 30 is separated in the thickness direction (for example, when it includes a first resin film and a second resin film described later), the thickness may be the total thickness of those films.
[0024] The thickness of the entire solar cell module of the first embodiment is preferably 200 μm or more, more preferably 250 μm or more, and more preferably 300 nm or more. On the other hand, the thickness of the entire solar cell module is preferably 1,200 μm or less, more preferably 900 μm or less, and even more preferably 800 μm or less. The thickness of the entire solar cell module is preferably 200 μm to 1,200 μm, more preferably 250 μm to 900 μm, and even more preferably 300 μm to 800 μm.
[0025] (Manufacturing method) The method for producing the solar cell module according to the first embodiment is not particularly limited as long as it is a method capable of forming the above-mentioned layer structure. Meanwhile, according to the following two examples of the production method, it is possible to obtain a solar cell module with excellent adhesion between the resin film and the solar cell by suppressing residual gas.
[0026] With reference to FIG. 5, a first manufacturing method of the solar cell module according to the first embodiment will be described. In the first manufacturing method, as shown in FIG. 5(a), first, a solar cell group 40 including a solar cell 41 and a first resin film 31 are laminated in this order on a second resin film 32. Next, while applying pressure 71 in the lamination direction, the resin films 31, 32 are heated to a glass transition temperature or higher if they are thermoplastic resins, or to a crosslinking temperature or higher if they are thermosetting resins, so that the solar cell 41 is encapsulated in the first resin film 31 and the second resin film 32, and the contact portion between the first resin film 31 and the second resin film 32 is integrated to become the resin film 30 (FIG. 5(b)). Pressurization in the lamination direction may be performed from the second resin film 32 side instead of the first resin film 31 side, or may be performed from both sides. The pressurization and heating method are not particularly limited, but a known method such as a thermal lamination method can be appropriately used. In addition, a solar cell module with a curved main surface can be manufactured, for example, by a method of hot pressing using a mold of a desired shape.
[0027] Next, a second manufacturing method of the solar cell module according to the first embodiment will be described with reference to Fig. 6. In the second manufacturing method, as shown in Fig. 6(a), solar cells are arranged in a first resin film 31 formed into a bag shape. Next, while degassing 72 the bag, the resin film 31 is heated to a temperature above its glass transition temperature if it is a thermoplastic resin, or to a temperature above its crosslinking temperature if it is a thermosetting resin, thereby sealing the solar cells in the first resin film and integrating the openings of the first resin film to form the resin film 30 (Fig. 6(b)).
[0028] <Second embodiment> Next, a solar cell module according to a second embodiment will be described with reference to Fig. 4. Fig. 4 is a ZX cross-sectional view of the solar cell module. The solar cell module 100 according to the second embodiment includes a plurality of solar cells 41 arranged inside a resin film 30, and further includes an adhesive layer 50 between the solar cells 41 and the resin film 30.
[0029] In the solar cell module according to the second embodiment, the solar cell group 40 is encapsulated together with the adhesive layer 50 in the highly rigid resin film 30, so that even when applied to, for example, curved laminated glass, the load acting on the peripheral parts of the solar cells 41 and the wiring 42 between the solar cells is mitigated. Furthermore, this solar cell module has excellent handleability during the manufacture of laminated glass, and scratches on the solar cells and breaks in the wiring can be suppressed. The resin film 30 and the solar cell group 40 may have the same configuration as the solar cell module of the first embodiment, and therefore a description thereof will be omitted here.
[0030] (Adhesive layer) The adhesive layer 50 is a layer that contacts the solar cell 41 and bonds the first resin film 31 and the second resin film 32. The type of adhesive layer 50 is not limited as long as it can bond them, but it is preferable that the adhesive layer 50 is a resin that can follow the shape and gaps of the solar cell during the manufacturing process of the solar cell module. The adhesive layer 50 may be a thermoplastic resin or a thermosetting resin. It may also be a curable resin other than thermosetting, such as photocuring (particularly ultraviolet curing) or two-part mixing curing. The adhesive layer 50 may be the same type of thermoplastic resin as the intermediate layer 20 described later, or may be an acrylic resin such as PMMA, a silicone resin, an epoxy resin, or the like.
[0031] When the adhesive layer 50 is made of a thermoplastic resin, the Young's modulus of the adhesive layer 50 at 23° C. is preferably 100 MPa or less, more preferably 90 MPa or less, and even more preferably 70 MPa or less. When the adhesive layer 50 is made of a thermosetting resin, the Young's modulus of the adhesive layer 50 at 23° C. is preferably 2,000 MPa to 5,000 MPa, and more preferably 2,200 to 3,000 MPa.
[0032] The refractive index n2 of the adhesive layer 50 is preferably 1.1 to 1.8, more preferably 1.2 to 1.7, and even more preferably 1.25 to 1.65, in order to easily reduce the difference in refractive index with the resin film. In addition, from the viewpoint of suppressing interfacial reflection between the resin film and the adhesive layer, the absolute value of the difference in refractive index between the refractive index n1 of the resin film and the refractive index n2 of the adhesive layer, |n1-n2|, is preferably 0.5 or less, more preferably 0.4 or less, and even more preferably 0.35 or less.
[0033] The thickness of the adhesive layer 50 is preferably equal to or greater than the thickness of the solar cell 41. Specifically, the thickness of the adhesive layer 50 is preferably equal to or greater than 100 μm, more preferably equal to or greater than 120 μm, even more preferably equal to or greater than 150 μm, and particularly preferably equal to or greater than 180 μm. On the other hand, the thickness of the solar cell 41 is preferably equal to or less than 800 μm, more preferably equal to or less than 600 μm, even more preferably equal to or less than 550 μm, and particularly preferably equal to or less than 500 μm. The thickness of the adhesive layer 50 is preferably 100 μm to 800 μm, more preferably equal to or less than 120 μm to 600 μm, even more preferably equal to or less than 150 μm to 550 μm, and particularly preferably equal to or less than 180 μm to 500 μm.
[0034] The thickness of the entire solar cell module of the second embodiment is preferably 200 μm or more, more preferably 250 μm or more, and more preferably 300 nm or more. On the other hand, the thickness of the entire solar cell module is preferably 1,200 μm or less, more preferably 900 μm or less, and even more preferably 800 μm or less. The thickness of the entire solar cell module is preferably 200 μm to 1,200 μm, more preferably 250 μm to 900 μm, and even more preferably 300 μm to 800 μm.
[0035] (Manufacturing method) The method for producing the solar cell module according to the second embodiment is not particularly limited as long as it is a method capable of forming the above-mentioned layer structure. Meanwhile, according to the following two examples of the production method, it is possible to obtain a solar cell module with excellent adhesion between the resin film and the solar cell by suppressing residual gas.
[0036] A first manufacturing method of the solar cell module according to the second embodiment will be described with reference to FIG. 7. In the seventh manufacturing method, as shown in FIG. 7(a), first, a second adhesive layer 52, a solar cell group 40 including a solar cell 41, a first adhesive layer 51, and a first resin film 31 are laminated in this order on a second resin film 32. A frame-shaped third adhesive layer 53 may be disposed on the periphery of the solar cell group 40. Next, by applying pressure 71 in the lamination direction, the solar cell 41 is sealed in the first resin film 31 and the second resin film 32, and the contact portion between the first adhesive layer 51 and the second adhesive layer 52 is integrated to form an adhesive layer 50 (FIG. 7(b)). Although not shown, the resin films 31 and 32 may be selected to be longer in the X-axis direction than the adhesive layers 51 and 52 to provide a contact portion between the first resin film 31 and the second resin film 32, and the first resin film and the second resin film may be integrated when pressurized.
[0037] A second manufacturing method of the solar cell module according to the second embodiment will be described. In the second manufacturing method, a frame-shaped patterned adhesive layer is disposed on a second resin film, a solar cell coated with an adhesive composition is disposed in the frame-shaped pattern, and a first resin film is laminated on the adhesive composition. The second manufacturing method can be suitably used when the adhesive composition is liquid (including paste-like). A specific example of this manufacturing method will be described with reference to FIG. 8. In the example of FIG. 8, as shown in FIG. 8(a), a frame-shaped patterned adhesive layer 53 is disposed on a second resin film 32, and a solar cell group 40 including a solar cell 41 is disposed in the frame-shaped pattern. Next, a liquid adhesive composition 54 is dripped 73 into the frame-shaped pattern, and the solar cell group 40 is immersed therein (FIG. 8(b)). Note that the dripping 73 in FIG. 8 may be any method as long as it is a method of coating an adhesive on a solar cell, and other means such as coating may be used. Next, a first resin film 31 is laminated on the adhesive composition 54 to obtain a solar cell module (FIG. 8(c)). Alternatively, for example, a frame-shaped pattern of adhesive layer 53 may be disposed on second resin film 32, a certain amount of liquid adhesive composition 54 may be dripped (applied) into the frame-shaped pattern, and then solar cell group 40 may be disposed, followed by further dripping (applying) of liquid adhesive composition 54, as shown in Fig. 8(b). When bonding, heating or pressure may be applied as necessary. The liquid adhesive composition 54 is a liquid composition having a resin that can be contained in the adhesive layer. The adhesive composition 54 may be, for example, a paste-like composition in which the resin is dissolved or dispersed in a solvent or the like.
[0038] [Laminated glass] As shown in Figures 1 and 9, the laminated glass 200 of this embodiment includes a first glass plate 11, a second glass plate 12, an intermediate layer 20 provided between the first and second glass plates, and a solar cell module 100 provided inside the intermediate layer 20, and the solar cell module is the solar cell module of the first or second embodiment.
[0039] The laminated glass 200 may have a flat plate shape, but when used in a moving body such as a vehicle, a curved shape is preferable from the viewpoint of safety. The curved shape may be a single curved shape curved in a first direction (e.g., the X-axis direction) or a compound curved shape curved in both the first direction (e.g., the X-axis direction) and the second direction (e.g., the Y-axis direction). The angle between the first direction and the second direction here is arbitrary, and may or may not be perpendicular to each other.
[0040] When the laminated glass 200 has a curved shape, it is preferable that the laminated glass 200 is curved so as to be convex toward the exterior side of the vehicle. That is, it is preferable that the first glass sheet 11 is curved so as to be convex toward the side opposite to the intermediate layer 20, and it is preferable that the second glass sheet 12 is curved so as to be convex toward the intermediate layer 20 side. The shape of the main surface of the laminated glass 200 in a plan view may be any shape depending on the installation location.
[0041] <Glass plate> The first glass plate 11 and the second glass plate 12 may be inorganic glass or organic glass. The inorganic glass and the organic glass may be colored as long as they are transparent, but colorless glass is preferable from the viewpoint of power generation efficiency of the solar cell. Examples of inorganic glass include soda-lime glass, aluminosilicate glass, borosilicate glass, alkali-free glass, and quartz glass, and soda-lime glass is preferable. Examples of organic glass include transparent resins such as polycarbonate, acrylic resins such as polymethyl methacrylate, polyvinyl chloride, and polystyrene. The materials of the first glass plate 11 and the second glass plate 12 may be the same or different.
[0042] The inorganic glass may be either unstrengthened glass or strengthened glass. The strengthened glass may be either physically strengthened glass such as air-cooled strengthened glass or chemically strengthened glass.
[0043] The method for forming the first glass sheet 11 and the second glass sheet 12 is not particularly limited, and for example, in the case of inorganic glass, glass sheets formed by a float method or the like are preferable. The first glass sheet 11 and the second glass sheet 12 may be bent using a gravity forming method, a press forming method, a roller forming method, or the like.
[0044] From the viewpoint of strength such as stone chip resistance, the thickness of the first glass plate 11 is preferably 1.1 mm or more, and more preferably 1.8 mm or more. On the other hand, from the viewpoint of suppressing the mass of the laminated glass 200 from being too large and suppressing the fuel consumption of the vehicle, the thickness of the first glass plate 11 is preferably 3 mm or less, more preferably 2.8 mm or less, even more preferably 2.6 mm or less, even more preferably 2.2 mm or less, and particularly preferably 2.0 mm or less. The thickness of the first glass plate 11 is preferably 1.1 mm to 3 mm, more preferably 1.8 mm to 2.8 mm, even more preferably 1.8 mm to 2.6 mm, even more preferably 1.8 mm to 2.2 mm, and particularly preferably 1.8 mm to 2.0 mm. From the viewpoint of ease of handling, the thickness of the second glass plate 12 is preferably 0.3 mm or more, more preferably 0.5 mm or more, and even more preferably 0.7 mm or more. On the other hand, from the viewpoint of preventing the mass of the laminated glass 200 from becoming too large and suppressing the fuel consumption of the vehicle, the thickness is preferably 2.3 mm or less, more preferably 2.1 mm or less, and even more preferably 1.9 mm or less. The thickness of the second glass plate 12 is preferably 0.3 mm to 2.3 mm, more preferably 0.5 mm to 2.1 mm, and even more preferably 0.7 mm to 1.9 mm.
[0045] <Middle Class> The intermediate layer 20 is disposed so as to sandwich the solar cell module 100. Thermoplastic resins are preferably used as the intermediate layer 20, and examples of such thermoplastic resins include polyvinyl acetal resins such as polyvinyl butyral resin (PVB), polyvinyl chloride resins, saturated polyester resins, polyurethane resins (PU), ethylene-vinyl acetate copolymer resins (EVA), ethylene-ethyl acrylate copolymer resins (EEA), cycloolefin polymers (COP), ionomer resins, and other thermoplastic resins that have been used conventionally for this type of application. In addition, a resin composition containing a modified block copolymer hydrogenated product described in Japanese Patent No. 6065221 can also be suitably used.
[0046] Among these, PVB, EVA, PU, ionomer resin, and COP are preferred, and PVB and EVA are more preferred. These thermoplastic resins may be used alone or in combination of two or more. The intermediate layer 20 may also contain functional particles such as an infrared absorbing agent, an ultraviolet absorbing agent, and a luminescent agent.
[0047] The intermediate layer 20 may have three or more layers. For example, when the intermediate layer is formed of three or more layers and the shear modulus of any layer other than the layers on both sides is made smaller than the shear modulus of the layers on both sides by adjusting the plasticizer or the like, the sound insulation of the laminated glass 200 can be improved. In this case, the shear modulus of the layers on both sides may be the same or different.
[0048] The thickness of the intermediate layer 20 is preferably 0.5 mm or more. When the intermediate layer 20 has a plurality of layers, the thickness of the intermediate layer 20 is the total thickness obtained by adding up the thicknesses of the respective layers. When the thickness of the intermediate layer 20 is 0.5 mm or more, the impact resistance required for the laminated glass 200 is sufficient. Furthermore, the thickness of the intermediate layer 20 is preferably 3 mm or less. When the maximum thickness of the intermediate layer 20 is 3 mm or less, the mass of the laminated glass 200 is suppressed. The maximum thickness of the intermediate layer 20 is more preferably 2.8 mm or less, and further preferably 2.6 mm or less.
[0049] Furthermore, when the intermediate layer 20 has a plurality of layers, each layer included in the intermediate layer 20 (for example, the first intermediate layer 21 and the second intermediate layer 22) is desirably formed of the same material, but may be formed of different materials.
[0050] Furthermore, the intermediate layer 20 and the adhesive layer 50 may contain the same resin. In this case, as shown in the example of Fig. 9, the intermediate layer 20 and the adhesive layer 50 are integrated together. This makes the periphery of the solar cell module 100 less noticeable, and also makes it difficult for air bubbles to remain between the side surface of the solar cell module 100 and the adhesive layer 50.
[0051] The Young's modulus of the intermediate layer 20 is preferably lower than that of the resin film 30. The Young's modulus of the intermediate layer at 23° C. is preferably 100 MPa or less, more preferably 90 MPa or less, and even more preferably 70 MPa or less. The absolute value of the refractive index difference |n1-n3| between the refractive index n1 of the resin film 30 and the refractive index n3 of the intermediate layer 20 is preferably 0.5 or less, more preferably 0.4 or less, and even more preferably 0.35 or less, in order to suppress interface reflection.
[0052] To prepare the intermediate layer 20, for example, the above-mentioned resin material to be the intermediate layer is appropriately selected and extruded in a heated and molten state using an extruder. The extrusion conditions such as the extrusion speed of the extruder are set to be uniform. Thereafter, the extruded resin film is stretched as necessary to complete the intermediate layer 20.
[0053] As shown in Figure 10, the laminated glass 200 is obtained by first preparing the solar cell module 100 for laminated glass of the present embodiment, and then stacking a second glass plate 12, a second intermediate layer 22, the solar cell module 100, a first intermediate layer 21, and a first glass plate 11 in this order, and pressing them together. The solar cell module 100 may be prepared, for example, by manufacturing the solar cell module using the method described above. The pressure bonding is performed by placing the laminate in a rubber bag, a rubber chamber, a resin bag, or the like, and bonding the laminate in a vacuum controlled at a gauge pressure of -100 kPa to -65 kPa and at a temperature controlled in the range of about 70°C to 110°C for a predetermined period of time. Heating conditions, temperature conditions, and lamination methods are appropriately selected.
[0054] Furthermore, by carrying out a pressure bonding treatment in which heating and pressing are carried out for a predetermined time under controlled conditions, for example, a temperature of 100° C. to 150° C. and an absolute pressure of 0.6 MPa to 1.3 MPa, it is possible to obtain a laminated glass 200 with even greater durability. However, in some cases, this heating and pressing step may not be used in consideration of simplification of the process and the properties of the material to be filled in the laminated glass 200.
[0055] A method called "cold bending" may be used in which either or both of the first glass plate 11 and the second glass plate 12 are joined in an elastically deformed state. Cold bending can be achieved by using a laminate including the intermediate layer 20 and the solar cell module 100 between the first glass plate 11 and the second glass plate 12 fixed by a temporary fixing means such as tape, a conventionally known preliminary pressure bonding device such as a nip roller, a rubber bag, or a rubber chamber, and an autoclave.
[0056] The total thickness of the laminated glass 200 is preferably 1.9 mm or more, and more preferably 2.8 mm or more, from the viewpoint of rigidity. On the other hand, the total thickness is preferably 10 mm or less, from the viewpoint of obtaining sufficient transmittance and providing lightweight properties to the laminated glass 200. The total thickness of the laminated glass 200 is, for example, 1.9 mm or more and 10 mm or less, and preferably 2.8 mm or more and 10 mm or less.
[0057] The laminated glass 200 may include various members as necessary. For example, the laminated glass 200 may be provided with a shielding layer 61 on the periphery. The shielding layer 61 may be provided at a position that does not overlap with the solar cell module 100 in a plan view, or may be provided at a position that overlaps with the periphery of the solar cell module 100. The shielding layer 61 may be provided at any position between the main surface of the first glass plate 11 opposite to the intermediate layer 20 and the main surface of the second glass plate 12 opposite to the intermediate layer 20.
[0058] Furthermore, films or devices having various functions may be provided between the first glass sheet 11 and the second glass sheet 12, provided that the effects of the present application are not impaired. Furthermore, a film having functions such as anti-fogging, water repellency, heat shielding, and low reflection may be provided on the surface of the laminated glass 200. Furthermore, a film having functions such as heat shielding and heat generation may be provided on the main surfaces of the glass sheets.
[0059] The use of the laminated glass of the present embodiment is not particularly limited, but it can be suitably used as a laminated glass mounted on a moving body such as a vehicle, a train, a ship, or an aircraft, for example, as a roof glass for a vehicle. Examples of the vehicle include a passenger car.
[0060] Although the preferred embodiments have been described in detail above, the present invention is not limited to the above-described embodiments, and various modifications and substitutions can be made to the above-described embodiments without departing from the scope of the claims. [Explanation of symbols]
[0061] 100 Solar Modules 200 Laminated Glass 11 First glass plate 12 Second Glass Pane 20 Middle Class 21 First Middle Class 22 The second middle class 30 Resin Film 31 First resin film 32 Second resin film 40 Solar cell group 41, A1~D4 solar cell 42 Wiring 50 Adhesive layer 51 1st adhesive layer 52 Second adhesive layer 53 Third adhesive layer 54 Adhesive composition 61 Shielding layer 71 Pressurization 72 Degassing 73 Dripping
Claims
1. A resin film; A solar cell module for laminated glass comprising: a resin film; and a plurality of solar cells disposed inside the resin film.
2. The solar cell module for laminated glass according to claim 1 , further comprising an adhesive layer between the solar cell and the resin film.
3. 3. The solar cell module for laminated glass according to claim 2, wherein the absolute value of the difference between the refractive index n1 of the resin film and the refractive index n2 of the adhesive layer, |n1-n2|, is 0.5 or less.
4. The solar cell module for laminated glass according to any one of claims 1 to 3, wherein the resin film has a Young's modulus at 23°C of 500 MPa or more.
5. The plurality of solar cells are arranged in a first direction and a second direction intersecting the first direction, The solar cell module for laminated glass according to any one of claims 1 to 4, comprising a solar cell group in which adjacent solar cells are electrically connected to each other by wiring.
6. The solar cell module for laminated glass according to any one of claims 1 to 5, wherein the resin film has a curved shape.
7. The solar cell module for laminated glass according to any one of claims 1 to 6, wherein the solar cell is a silicon solar cell.
8. A solar cell module comprising: a first glass plate; a second glass plate; an intermediate layer provided between the first and second glass plates; and a solar cell module provided within the intermediate layer; The solar cell module is the solar cell module for laminated glass according to any one of claims 1 to 7.
9. The laminated glass according to claim 8 , wherein the intermediate layer has a Young's modulus lower than a Young's modulus of the resin film.
10. 10. The laminated glass according to claim 8, wherein the intermediate layer has a Young's modulus at 23°C of 100 MPa or less.
11. The laminated glass according to any one of claims 8 to 10, wherein an absolute value of a refractive index difference |n1-n3| between a refractive index n1 of the resin film and a refractive index n3 of the intermediate layer is 0.5 or less.
12. The laminated glass according to any one of claims 8 to 11, wherein the solar cell module is a solar cell module including an adhesive layer, and the intermediate layer and the adhesive layer contain the same resin.
13. A method for producing a solar cell module for laminated glass according to any one of claims 1 and 3 to 7, comprising the steps of: A method for producing a solar cell module for laminated glass, comprising laminating a solar cell and a first resin film in this order on a second resin film, and applying pressure while heating.
14. A method for producing a solar cell module for laminated glass according to any one of claims 1 and 3 to 7, comprising the steps of: A method for manufacturing a solar cell module for laminated glass, comprising disposing a solar cell in a bag-shaped first resin film and heating the film while degassing the film.
15. A method for producing a solar cell module for laminated glass according to any one of claims 2 to 7, comprising the steps of: A method for producing a solar cell module for laminated glass, comprising laminating and adhering a second adhesive layer, a solar cell, a first adhesive layer, and a first resin film in this order onto a second resin film.
16. A method for producing a solar cell module for laminated glass according to any one of claims 2 to 7, comprising the steps of: An adhesive layer having a frame-shaped pattern is disposed on the second resin film; A solar cell covered with an adhesive composition is placed within the frame pattern; A method for producing a solar cell module for laminated glass, comprising laminating a first resin film onto the adhesive composition.
17. A solar cell module for laminated glass according to any one of claims 1 to 7 is prepared, A method for producing laminated glass, comprising laminating a second glass plate, a second intermediate layer, the solar cell module, a first intermediate layer, and a first glass plate in this order, and bonding them under pressure.
Citation Information
Patent Citations
Laminated glass
WO2017099167A1
Cited By
Vehicle laminated glass
WO2026075155A1
Laminated glass, vehicle, and method for producing laminated glass