Photocurable foaming adhesive composition

The photocurable foam adhesive composition with acrylic block copolymer and photopolymerization initiator addresses adhesion and removability issues in PVC sheet installations, ensuring strong bonding and residue-free removal.

JP2024138641AInactive Publication Date: 2024-10-09AICA KOGYO CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023049230
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing adhesives for PVC sheets in flooring installations face issues with insufficient adhesion, residue left on the surface, and difficulty in removability, especially during renovations where moisture-absent surfaces complicate the use of water-based adhesives.

Method used

A photocurable foam adhesive composition comprising an acrylic block copolymer, hydroxyl group-containing (meth)acrylate, and a photopolymerization initiator, with specific hardness and composition ratios, ensuring strong adhesion and easy removability without residue.

Benefits of technology

The adhesive composition provides sufficient adhesion to PVC sheets, allows easy removal without residue, and offers cushioning properties, reducing material waste and installation complexity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024138641000001
    Figure 2024138641000001
  • Figure 2024138641000002
    Figure 2024138641000002
  • Figure 2024138641000003
    Figure 2024138641000003
Patent Text Reader

Abstract

To provide a photocurable foaming adhesive composition which has sufficient adhesion to a substrate such as a vinyl chloride sheet and at the same time has excellent removability, i.e., does not leave adhesive residue even when peeled off after being once stuck.SOLUTION: A photocurable foaming adhesive composition comprising an acrylic block copolymer, a hydroxyl group-containing (meth)acrylate, and a photopolymerization initiator, characterized in that the acrylic block copolymer has a hardness of 3 to 68 in Type A durometer according to ISO 7619-1.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a foamable pressure-sensitive adhesive composition which is used by being cured by exposure to ultraviolet light or the like. [Background technology]

[0002] Plastic flooring materials are used in a wide range of buildings, from office buildings and commercial facilities to ordinary homes. Among these plastic flooring materials, vinyl resin flooring materials, including polyvinyl chloride, are relatively inexpensive and easy to install, and have many excellent properties such as chemical resistance, abrasion resistance, scratch resistance, flexibility, and ability to conform to the substrate, so they are used in a wide range of places, including schools, hospitals, factories, and government facilities.

[0003] When installing vinyl flooring, adhesives that have sufficient adhesive strength with the base material are generally used to prevent the flooring from shifting due to foot traffic during use. For example, water-based acrylic resins, solvent-based urethane resins, epoxy resins, etc. are listed, and these are installed on-site, but they require sufficient curing time after bonding, and solvent-based adhesives have the problem of deteriorating the on-site environment due to the evaporation of the solvent.

[0004] More recently, in some cases of renovation, new sheets are installed directly on existing flooring, and in such cases, because the existing flooring does not absorb moisture, it is difficult to use water-based adhesives, and so PVC sheets with pre-applied adhesives have come to be used (e.g., Patent Document 1). However, when such PVC sheets with adhesive are installed on-site, the adhesive may peel off when correcting misalignment, or the adhesive may remain on the floor surface, causing problems with the finished product. For this reason, there has been a demand for an adhesive that has sufficient adhesion to the PVC sheet, leaves no adhesive residue when peeled off, and has excellent removability. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2018-3369 A Summary of the Invention [Problem to be solved by the invention]

[0006] The present invention aims to provide a photocurable foamable pressure-sensitive adhesive composition that has sufficient adhesion to a substrate such as a PVC sheet and at the same time has excellent removability, i.e., is less likely to leave adhesive residue even when peeled off after being once laminated. [Means for solving the problem]

[0007] In order to solve the above problems, the invention described in claim 1 provides a photocurable foamable pressure-sensitive adhesive composition comprising an acrylic block copolymer (A), a hydroxyl group-containing (meth)acrylate (B), and a photopolymerization initiator (C), wherein the hardness of (A) is 3 to 68 in Type A durometer conforming to ISO 7619-1.

[0008] A second aspect of the present invention provides the photocurable foamable pressure-sensitive adhesive composition according to the first aspect, wherein the blending amount of (A) is 8 to 60% by weight based on the total solid content.

[0009] The invention according to claim 3 provides the photocurable foamable pressure-sensitive adhesive composition according to claim 1, further comprising a polyfunctional (meth)acrylate.

[0010] The invention according to claim 4 provides a photocurable foamable pressure-sensitive adhesive composition according to any one of claims 1 to 3, which is a pressure-sensitive adhesive for use with a vinyl chloride substrate.

[0011] The invention described in claim 5 provides a composition comprising an acrylic block copolymer (A), a hydroxyl group-containing (meth)acrylate (B), and a photopolymerization initiator (C), wherein the hardness of (A) is 3 to 68 in Type A durometer conforming to ISO 7619-1, and a method for using a photocurable foamable adhesive, characterized in that the composition is photocured in a foamed state. Effect of the Invention

[0012] The photocurable foamable adhesive composition of the present invention has sufficient adhesion to a substrate and at the same time has excellent removability, i.e., does not leave any adhesive residue even when peeled off after being once laminated, and is therefore useful as an adhesive for use in plastic floor sheets such as those made of PVC resin. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The present invention will be described in detail below.

[0014] The composition of the present invention comprises an acrylic block copolymer (A), a hydroxyl group-containing (meth)acrylate (B), and a photopolymerization initiator (C). In this specification, the term "(meth)acrylate" includes both acrylate and methacrylate.

[0015] The acrylic block copolymer (A) used in the present invention is a plasticizer-like component that is not involved in the curing reaction, and plays a role in alleviating internal stress and enabling a suitable initial peeling force and stable peeling without leaving any adhesive residue. "Acrylic" means that it contains at least one structural unit derived from a monomer selected from the group consisting of (meth)acrylic acid and its esters, and (meth)acrylamide and its derivatives, and among these, copolymers consisting of (meth)acrylic acid and its esters are preferred.

[0016] The structure of (A) may be a linear block copolymer, a branched (star) block copolymer, etc., but a linear block copolymer is preferred in terms of cost and availability. Among linear block copolymers, diblock copolymers (AB) and triblock copolymers (ABA) composed of two types of monomers (A and B) are more preferred in terms of ease of handling during processing, physical properties of the composition, and cost.

[0017] As the monomer constituting the (A), methyl methacrylate (hereinafter referred to as MMA) is preferred because the strength and transparency of the cured resin are good and it is easily and inexpensively available. Furthermore, n-butyl acrylate (hereinafter referred to as BA) is preferred because the cured resin has excellent flexibility and good adhesiveness. Examples of block copolymers composed of MMA and BA include a triblock structure (PMMA-PBA-PMMA) composed of a hard segment made of P(poly)MMA and a soft segment made of P(poly)BA, with both ends of the soft segment sandwiched between hard segments. This structure has the characteristics of combining the transparency and weather resistance of PMMA with the flexibility and adhesiveness of PBA.

[0018] The hardness of (A), in terms of a type A durometer in accordance with ISO 7619-1, is 3 to 68, preferably 5 to 65, more preferably 10 to 55, and particularly preferably 15 to 45. If it is less than 3, the cohesive force of the cured product tends to decrease and adhesive residue tends to be easily left on the substrate, while if it exceeds 68, the peel strength tends to decrease.

[0019] The (A) may be used in combination of two or more copolymers with different hardnesses. In that case, the blending ratio is determined by the hardness as in the case of using each copolymer alone, and the sum of the hardness of each of the different copolymers multiplied by its content ratio is preferably 3 to 68 (for example, if the blending amount of hardness 10 is 40% and the blending amount of hardness 30 is 60%, then 10×0.4+30×0.6=22).

[0020] The blending amount of the (A) is preferably 8 to 60% by weight, more preferably 10 to 55% by weight, and particularly preferably 20 to 45% by weight, based on the total solid content. By making it 8% by weight or more, sufficient adhesiveness can be ensured, and by making it 60% by weight or less, sufficient adhesive strength and expansion ratio can be ensured.

[0021] The hydroxyl-containing (meth)acrylate (B) used in the present invention is blended for the purpose of dissolving the (A) component and improving adhesion to the adherend. There are no particular limitations on the hydroxyl-containing (meth)acrylate, but in terms of cure shrinkage, it is preferably bifunctional or less, and more preferably monofunctional. Examples include 2-hydroxyethyl (meth)acrylate, 3-hydroxypropyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 6-hydroxyhexyl (meth)acrylate, 8-hydroxyoctyl (meth)acrylate, 1,4-cyclohexanedimethanol monoacrylate, and 4-hydroxycyclohexyl (meth)acrylate, and these can be used alone or in combination of two or more.

[0022] The glass transition point (hereinafter referred to as Tg) of the homopolymer of (B) is preferably 0° C. or lower, more preferably -10° C. or lower, and particularly preferably -20° C. or lower. By combining a plurality of (B) having different Tg, it is also possible to control the adhesive strength of the cured product. Examples of (B) having a Tg of 0° C. or lower include 4-hydroxybutyl acrylate (Tg: -32° C.), 2-hydroxyethyl acrylate (Tg: -15° C.), and 2-hydroxypropyl acrylate (Tg: -7° C.).

[0023] The blending amount of the (B) is preferably 30 to 85% by weight, more preferably 35 to 80% by weight, and particularly preferably 45 to 70% by weight, based on the total solid content. By making it 30% by weight or more, sufficient solubility and adhesion of (A) can be ensured, and by making it 85% by weight or less, sufficient adhesion can be ensured. The blending ratio of (B) having a Tg of 0°C or less to the total amount of (B) is preferably 50% by weight or more, more preferably 60% by weight or more, and particularly preferably 70% by weight or more.

[0024] The photopolymerization initiator (C) used in the present invention generates radicals when irradiated with ultraviolet light or an electron beam, and the radicals trigger the polymerization reaction, and general-purpose photopolymerization initiators such as benzyl ketal, acetophenone, and phosphine oxide photopolymerization initiators can be used. By arbitrarily selecting the light absorption wavelength of the polymerization initiator, it is possible to impart curability over a wide wavelength range from the ultraviolet region to the visible light region. Specifically, 2.2-dimethoxy-1.2-diphenylethan-1-one is a benzyl ketal type, 1-hydroxy-cyclohexyl-phenyl-ketone and 1-[4-(2-hydroxyethoxy)-phenyl]-2-hydroxy-2-methyl-1-propan-1-one are α-hydroxyacetophenone types, 2-methyl-1-(4-methylthiophenyl)-2-morpholinopropan-1-one are α-aminoacetophenone types, and 2.4.6-trimethylbenzoyl-diphenyl-phosphine oxide and bis(2.4.6-trimethylbenzoyl)-phenylphosphine oxide are acylphosphine oxide types, which can be used alone or in combination of two or more. Among these, it is preferable to include α-hydroxyacetophenone types that are resistant to yellowing, and acylphosphine oxide types that have excellent internal curing properties.

[0025] The amount of (C) is preferably 5 to 15 parts by weight, more preferably 8 to 12 parts by weight, per 100 parts by weight of the photopolymerizable component. By using 5 parts by weight or more, sufficient curability can be ensured, and by using 15 parts by weight or less, an excessive amount is not added, and sufficient molecular weight can be ensured even after curing. When an α-hydroxyacetophenone type and an acylphosphine oxide type are used in combination, the latter is preferably 0.1 to 2.0 parts per 10 parts of the former. Examples of commercially available products include Omnirad 184 and 2959 for α-hydroxyacetophenone types, and Omnirad TPO H and 819 for phosphine oxide types (trade names: both manufactured by IGM Resins).

[0026] In addition, additives such as reactive diluents, foam stabilizers, surfactants, tackifiers, antioxidants, UV absorbers, flame retardants, defoamers, wettability adjusters, organic fine particles, and inorganic filler antistatic agents can be used in combination with the photocurable pressure-sensitive adhesive composition of the present invention within the scope of not impairing the performance.

[0027] As the reactive diluent, it is preferable to use a polyfunctional (meth)acrylate, because it has a low viscosity and is excellent in compatibility with (A) and (B). For example, bifunctional diluents include (poly)ethylene glycol di(meth)acrylate, hexanediol di(meth)acrylate, and dicyclopentanyl diacrylate, trifunctional dimethylolpropane tri(meth)acrylate and pentaerythritol tri(meth)acrylate, tetrafunctional diglycerol tetra(meth)acrylate, diglycerin tetra(meth)acrylate, pentafunctional dipentaerythritol penta(meth)acrylate, and hexafunctional dipentaerythritol hexa(meth)acrylate, and these can be used alone or in combination of two or more kinds.

[0028] The amount of the reactive diluent blended is preferably 10% by weight or less, more preferably 1 to 8% by weight, and particularly preferably 3 to 6% by weight, based on the total solid content. By adjusting the amount of the reactive diluent blended to this range, it is possible to adjust the viscosity to a level suitable for coating and improve the curability while maintaining the dissolution stability of (A).

[0029] The foam stabilizer is not particularly limited as long as it is a compound that can suppress localized aggregation of foam and disperse foam uniformly and stably in the pressure-sensitive adhesive layer. For example, it can be a sulfate type, a sulfonate type, or a silicone type surfactant. Among these, a silicone type surfactant that exhibits an excellent foam stabilizing effect is preferred.

[0030] The amount of the foam stabilizer is preferably 0.1 to 10% by weight or less, more preferably 0.5 to 8% by weight, and particularly preferably 1 to 5% by weight, based on the total solid content. By making it 0.1% by weight or more, it is expected that the foam can be uniformly and stably dispersed in the adhesive layer, and by making it 10% by weight or less, the foam stabilizer does not act as a softener, and sufficient adhesion and heat resistance to the adherend can be ensured.

[0031] The photocurable adhesive composition of the present invention (hereinafter referred to as the present adhesive composition) may be diluted with a solvent. However, in the case of a substrate that is highly soluble in polar solvents such as vinyl chloride, it is preferable to use a solvent with low polarity. The blending amount is preferably 10% or less, and more preferably solvent-free. In the present invention, "solvent-free" means excluding intentional blending of a solvent for the purpose of dilution, and does not mean excluding even trace amounts of volatile components contained in each component of the composition, and refers to a solvent content of 5% by weight or less, typically 1% by weight or less.

[0032] The viscosity of the pressure-sensitive adhesive composition before foaming at 25° C. is preferably 100 to 300,000 mPa·s, more preferably 1,000 to 100,000 mPa·s, and particularly preferably 5,000 to 50,000 mPa·s. By setting the viscosity within this range, it becomes easier to ensure an expansion ratio suitable for application, and it is possible to stably apply a film thickness of about 0.1 to 1 mm in one coat.

[0033] The adhesive composition can be used, for example, by foaming, applying it to an adherend, and then photocuring it. The foaming makes the adhesive layer softer, providing cushioning properties. In addition, the foamed bubbles break to form a suction cup shape, which allows the adhesive to adhere to the adherend and cure, and is expected to improve peel strength. Furthermore, the increased volume allows the amount of adhesive used to be reduced, making it possible to reduce costs.

[0034] The foaming method of the present pressure-sensitive adhesive composition is not particularly limited, and may be a known method. For example, a chemical foaming method in which a foaming agent is added to the pressure-sensitive adhesive composition and the composition is heated to foam the composition, or a mechanical foaming method in which air bubbles are added to the pressure-sensitive adhesive composition by mechanical stirring means, etc., are included. Among these, the mechanical foaming method is preferred because it is easy to control the foaming state.

[0035] Specific examples of the mechanical foaming method include mixing the pressure-sensitive adhesive composition at high speed with a mixer or the like to mix air into the composition, or mixing an inert gas into the pressure-sensitive adhesive composition under negative pressure, compressing the mixture, and then discharging the mixture to incorporate fine bubbles. The foaming ratio of the pressure-sensitive adhesive composition is preferably 1.5 to 5.0, and more preferably 2.0 to 4.0.

[0036] The method of applying the pressure-sensitive adhesive composition is not particularly limited, and may be a known method. When applying to the entire surface of the adherend, for example, a roll coater, a reverse roll coater, a knife coater, an air knife coater, a bar coater, a slot die coater, a lip coater, a gravure coater, a reverse gravure coater, etc. may be used. When applying to a specific part of the adherend, a dispenser, a comb trowel, a hand gun, etc. may be used.

[0037] The pressure-sensitive adhesive composition applied to the substrate after foaming is cured using light such as ultraviolet light. Examples of light sources include low-pressure mercury lamps, high-pressure mercury lamps, ultra-high-pressure mercury lamps, carbon arc lamps, xenon lamps, metal halide lamps, LED lamps, and electrodeless ultraviolet lamps. The curing conditions are 50 mW / cm. 2 ~3000mW / cm 2 The irradiation intensity is 100 to 2,000 mJ / cm2 as the cumulative light quantity. 2 The irradiation atmosphere may be air or an inert gas such as nitrogen or argon.

[0038] The adhesive composition is solvent-free and can be used as an adhesive to be applied to long PVC sheets. The adhesive composition has sufficient adhesion and excellent removability, which means that it is unlikely to leave adhesive residue on the substrate when peeled off after application, making it possible to greatly improve the efficiency of work on site.

[0039] The present invention will be described in detail below based on examples and comparative examples, but these are specific examples and are not intended to be limiting. Unless otherwise specified, measurements were performed under conditions of room temperature of 25°C and relative humidity of 65%. The blend amounts are in parts by weight.

[0040] Example 1 A photocurable adhesive composition of Example 1 was prepared by mixing KURARITY LA3710 (product name: manufactured by Kuraray Co., Ltd., MMA / BA / MMA block polymer, hardness of 9 on a type A durometer) as (A), HOP(N) (product name: manufactured by Kyoeisha Chemical Co., Ltd., hydroxypropyl methacrylate) and 4-HBA (product name: manufactured by Osaka Organic Chemical Industry Co., Ltd., 4-hydroxybutyl acrylate) as (B), Omnirad184 (product name: manufactured by IGM Resins Co., Ltd.) and OmniradTPO H (product name: manufactured by IGM Resins Co., Ltd.) as (C) and MIRAMER M200 (product name: manufactured by MIWON Co., Ltd., 1,6-hexanediol diacrylate) as a reactive diluent in the formulation shown in Table 1 until uniformly dissolved.

[0041] Examples 2 to 8 In addition to the materials used in Example 1, LA2140 (product name: manufactured by Kuraray Co., Ltd., MMA / BA / MMA block polymer, hardness 32) and LA2250 (product name: manufactured by Kuraray Co., Ltd., MMA / BA / MMA block polymer, hardness 65) were used as (A), and L-895 (product name: manufactured by MOMENTIVE Co., Ltd., siloxane-polyalkylene oxide copolymer) and BYK-UV3570 (product name: manufactured by BYK-Chemie Co., Ltd., polyester-modified polydimethylsiloxane) were used as foaming agents. The mixture was stirred until uniformly dissolved in the formulation shown in Table 1 to prepare the photocurable pressure-sensitive adhesive compositions of Examples 2 to 8.

[0042] Comparative Examples 1 to 3 In addition to the materials used in the examples, LA2270 (product name: manufactured by Kuraray Co., Ltd., MMA / BA / MMA block polymer, hardness 71) and LA2114 (product name: manufactured by Kuraray Co., Ltd., MMA / BA / MMA block polymer, fluid form with hardness less than 3) were used as acrylic copolymers and stirred until uniformly dissolved in the formulation shown in Table 2, to prepare photocurable pressure-sensitive adhesive compositions of Comparative Examples 1 to 3.

[0043] Table 1 JPEG2024138641000001.jpg129150

[0044] Table 2 JPEG2024138641000002.jpg226153

[0045] The evaluation method was as follows.

[0046] Curability: 100 g of the adhesive composition was placed in a 1000 mL cylindrical disposable beaker, and the composition was foamed by stirring with a hand mixer at 950 rpm for 5 minutes. The composition was then applied to a PVC sheet (thickness 2 mm) using a comb trowel (comb height 2 mm), and passed through a conveyor-type UV irradiator (manufactured by Fusion Co., Ltd.) to measure how many times it took to completely cure. The UV irradiation conditions were a Fusion D bulb as the light source, and 200 mW / cm per irradiation. 2 , 500mJ / cm 2 The working temperature when stirring the pressure sensitive adhesive composition and applying it to the substrate was 80°C only for Example 7, which had a high viscosity, and 23°C for the others. The evaluation method was ◯ for 3 passes or less, and × for 4 passes or more.

[0047] Viscosity: A Toki Sangyo RE-215R cone-plate viscometer was used, and measurements were taken at 25±1°C and 2 rpm, with a cone angle of 3°×R17.65 for viscosities between 100 and 50,000 mPa·s, and a cone angle of 3°×R7.7 for viscosities of 50,000 mPa·s or more. The evaluation method was as follows: ◯ if the value was 100 to 300,000 mPa·s, and × if it was outside this range.

[0048] Adhesion: The PVC sheet coated with the adhesive composition cured in the above curing evaluation was cut to a width of 100 mm x 50 mm, attached to a glass plate (thickness 2 mm), pressed with a hand roller at a load of 5 kgf, and left to stand for 1 hour. After that, the 90° peel strength was measured at a pulling speed of 300 mm / min using a digital force gauge ZP-500N manufactured by Imada. The evaluation method was as follows: over 1.0N was rated as ◎, 0.5-1.0N was rated as 〇, and less than 0.5N was rated as ×.

[0049] Adhesive residue: After the adhesiveness evaluation, the glass surface was visually inspected. If no adhesive residue was present, it was rated as ◯, and if adhesive residue was present, it was rated as ×.

[0050] Expansion ratio: 100 g of the adhesive composition was placed in a cylindrical disposable beaker of 1000 mL, and the composition was foamed by stirring with a hand mixer at 950 rpm for 5 minutes. After foaming, the height of the liquid surface was measured from the bottom of the beaker, and the ratio of the height before and after foaming was taken as the expansion ratio. The working temperature when stirring the adhesive composition was 80°C only for Example 7, which had a high viscosity, and 23°C for the others. The evaluation method was as follows: over 2 times was marked with ◎, 1.5 to 2 times was marked with 〇, and less than 1.5 times was marked with ×.

[0051] Example evaluation results Table 3 JPEG2024138641000003.jpg81135

[0052] Comparative Example Evaluation Results Table 4 JPEG2024138641000004.jpg152140

[0053] Each of the resin compositions of the Examples obtained good results in the evaluations of viscosity, curability, adhesion, adhesive residue, and expansion ratio.

[0054] On the other hand, Comparative Example 1, which did not contain (B), and Comparative Example 2, which used (A) with a high Type A hardness, had low adhesion, and Comparative Example 3, which used (A) with a low Type A hardness, left adhesive residue, and neither of these were suitable for the present invention.

Claims

1. A photocurable foamable pressure-sensitive adhesive composition comprising an acrylic block copolymer (A), a hydroxyl group-containing (meth)acrylate (B), and a photopolymerization initiator (C), the hardness of (A) being 3 to 68 in Type A durometer according to ISO 7619-1.

2. 2. The photocurable foamable pressure-sensitive adhesive composition according to claim 1, wherein the blending amount of said (A) is 8 to 60% by weight based on the total solid content.

3. 2. The photocurable foamable pressure-sensitive adhesive composition according to claim 1, further comprising a polyfunctional (meth)acrylate.

4. 4. The photocurable foamable pressure-sensitive adhesive composition according to claim 1, which is an adhesive for use with a vinyl chloride substrate.

5. A method for using a photocurable foaming adhesive comprising: (A) an acrylic block copolymer; (B) a hydroxyl group-containing (meth)acrylate; and (C) a photopolymerization initiator, the composition having a hardness of 3 to 68 in terms of a Type A durometer in accordance with ISO 7619-1; and (C) a composition comprising the composition in a foamed state and photocuring the composition.

Citation Information

Patent Citations

  • Floor construction method and floor structure

    JP2018003369A