Decorative sheet
The decorative sheet with a pattern layer, transparent resin, and surface protective layer addresses design defects by minimizing visible unevenness and enhancing durability and antimicrobial properties.
Patent Information
- Application Number
- JP2024020169
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-27
- Filing Date
- 2024-02-14
- Publication Date
- 2024-10-09
AI Technical Summary
Decorative sheets laminated onto wood base materials with unevenness cause design defects due to differences in gloss and shadow formation, which existing technologies fail to address effectively.
A decorative sheet design with a pattern layer, transparent resin layer, and surface protective layer, featuring an uneven shape and specific gloss and lightness relationships, enhances design quality by minimizing visible unevenness.
The solution effectively reduces the visibility of surface irregularities, improving design aesthetics and providing enhanced durability and antimicrobial properties.
Smart Images

Figure 2024139694000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a decorative sheet. [Background technology]
[0002] 2. Description of the Related Art When it is desired to decorate components used in building materials, furniture, home appliances, and the like, decorative panels having a decorative sheet with a design attached thereto are generally used.
[0003] Since decorative boards are made by directly bonding a thin decorative sheet to a wooden base material (undercoat), if there are irregularities on the surface (coating surface) of the wooden base material, or if dirt, dust, wood powder, etc. get in and cause unevenness, the irregularities will appear on the surface of the decorative material and cause design defects such as reflections.
[0004] Patent Document 1 discloses a decorative sheet having an uneven surface, whereby when light is projected onto the surface from a direction inclined at 82° to the normal direction of the decorative sheet, a shadow is formed that has a length d of 3 mm or more and a width w of 3 mm or more when observed from the normal direction of the decorative sheet.
[0005] Patent Document 1 discloses a technology for making unevenness formed on the coated surface of a base material less noticeable by adjusting (lightening) the shadow that appears when light hits the unevenness on the surface of a decorative sheet. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2018-100502 A Summary of the Invention [Problem to be solved by the invention]
[0007] The technique disclosed in Patent Document 1 is effective when the base material has relatively large (high) irregularities that will cast shadows of the irregularities on the surface of the decorative sheet when the decorative sheet is laminated onto a wood substrate.
[0008] However, humans perceive unevenness not only from the shade of shadow, but also from the difference in the amount of light reflected by flat and uneven areas (difference in gloss). Therefore, even if the wood base material has unevenness that does not cast a shadow on the surface of the decorative sheet when the decorative sheet is laminated to the wood base material, the unevenness may be noticeable due to differences in gloss, and a method for improving design defects caused by such unevenness was required.
[0009] The present invention is devised to solve the above-mentioned problems, and has an object to provide a decorative sheet that can improve design defects caused by unevenness on the surface of a wood substrate. [Means for solving the problem]
[0010] The inventors have discovered that by adjusting the gloss value and brightness of the surface of a decorative sheet within a prescribed range, design defects can be improved even when the wood substrate has unevenness that would not cast a shadow of the unevenness on the surface of the decorative sheet when the decorative sheet is laminated to the wood substrate, and have completed the present invention.
[0011] That is, the present invention provides a decorative sheet comprising, on one side of a base sheet containing a thermoplastic resin, a picture layer, a transparent resin layer containing a thermoplastic resin, and a surface protective layer, at least in this order, wherein the surface on which the surface protective layer is provided has an uneven shape, and the difference in 85 degree specular gloss G between the direction of the uneven shape and a direction perpendicular to the direction of the uneven shape, as measured by a method in accordance with JIS Z 8741:1997, is 15% or more, and the relationship between the maximum 85 degree specular gloss G', as measured by a method in accordance with JIS Z 8741:1997, and the lightness L, as measured by JIS Z 8781-4:2013, satisfies the following formula (1): L>1.5G' 2 -5G'-10 (1) (However, in the above formula (1), G'≧0 and 15≦L≦95 are satisfied.)
[0012] In the decorative sheet of the present invention, the surface protective layer preferably contains an ionizing radiation curable resin. The uneven shape is preferably a ridge-like portion that protrudes in a ridge shape. It is also preferable that the uneven shape is formed by embossing. In addition, it is preferable that a backer layer be provided on the side of the base sheet opposite to the side on which the surface protective layer is laminated. Moreover, the surface protective layer preferably contains at least one agent selected from the group consisting of an antibacterial agent, an antiviral agent, and an antiallergen agent. Effect of the Invention
[0013] The present invention provides a decorative sheet that can improve design defects caused by unevenness on the surface of a wood substrate. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a cross-sectional view for explaining a schematic example of the decorative sheet of the present invention. [Diagram 2] FIG. 2 is an explanatory diagram for explaining the direction of the concave-convex shape and the direction perpendicular to the direction of the concave-convex shape. [Diagram 3] FIG. 3 is an explanatory diagram for explaining the test method for evaluating design defects. [Figure 4] FIG. 4 is a graph of formula (1) and a diagram showing the maximum 85 degree specular gloss G' and lightness L measured for the decorative sheets of the examples and comparative examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The decorative sheet of the present invention will now be described. In the following description, the lower and upper limits of a numerical range expressed with "to" means "greater than or equal to" (for example, if α~β, then it is greater than or equal to α and less than or equal to β).
[0016] The decorative sheet of the present invention comprises, on one side of a base sheet containing a thermoplastic resin, a picture layer, a transparent resin layer containing a thermoplastic resin, and a surface protective layer, at least in this order, and has an uneven shape on the side on which the surface protective layer is provided, and the difference in 85 degree specular gloss G between the direction of the uneven shape and a direction perpendicular to the direction of the uneven shape, as measured by a method in accordance with JIS Z 8741:1997, is 15% or more, and the relationship between the maximum 85 degree specular gloss G', as measured by a method in accordance with JIS Z 8741:1997, and the lightness L, as measured by JIS Z 8781-4:2013, satisfies the following formula (1): L>1.5G' 2 -5G'-10 (1) (However, in the above formula (1), G'≧0 and 15≦L≦95 are satisfied.)
[0017] FIG. 1 is a cross-sectional view for explaining a schematic example of the decorative sheet of the present invention. As shown in FIG. 1, the decorative sheet 10 has a base sheet 1 on one side of which a design layer 2, a transparent resin layer 3, and a surface protective layer 4 are laminated in this order. Each component of the decorative sheet of the present invention will be described in detail below.
[0018] (Optical properties of decorative sheets) The decorative sheet of the present invention has an uneven surface on the side having the surface protective layer, and the difference in 85 degree specular gloss G between the direction of the uneven surface formed on the surface protective layer and a direction perpendicular to the direction of the uneven surface, as measured by a method conforming to JIS Z 8741:1997, is 15% or more. In this specification, the 85 degree specular gloss is an average value of three points measured by Method 1 in accordance with JIS Z 8741:1997. In addition, the "difference in 85-degree specular gloss G" can be calculated by the following formula: The "direction of the uneven shape" will be described later. [(the larger of the two measured values) / {(85-degree specular gloss G in the direction of the uneven surface)-(85-degree specular gloss G in the direction perpendicular to the uneven surface)}] x 100
[0019] The decorative sheet of the present invention has a relationship between the maximum 85 degree specular gloss G' measured according to JIS Z 8741:1997 and the lightness L measured according to JIS Z 8781-4:2013 that satisfies the following formula (1). L>1.5G' 2 -5G'-10 (1) (However, in the above formula (1), G'≧0 and 15≦L≦95 are satisfied.)
[0020] By satisfying the above-mentioned numerical range of the difference in 85-degree specular gloss G and formula (1), it is possible to improve design defects caused by unevenness on the surface of the wood base material.
[0021] The maximum value G' of the 85 degree specular gloss is 0 or more. Furthermore, the maximum value G' of the 85 degree specular gloss is preferably 9.5 or less, more preferably 9 or less, even more preferably 8 or less, and particularly preferably 7 or less. By providing the maximum 85 degree specular gloss value G' within the above range, design defects caused by unevenness on the surface of the wood base material can be more suitably improved. The maximum 85° specular gloss value G' means the maximum value measured at 10 points in total, 5 points in the direction of the uneven shape and 5 points in a direction perpendicular to the direction of the uneven shape.
[0022] The lightness L is 15 or more and 95 or less. The lightness L is preferably 40 or more, and more preferably 70 or more. When the lightness L is within the above range, design defects caused by unevenness on the surface of the wood base material can be more suitably improved.
[0023] (Base sheet) The decorative sheet of the present invention comprises a substrate sheet containing a thermoplastic resin.
[0024] Examples of the thermoplastic resin include olefin-based thermoplastic resins such as low-density polyethylene (including linear low-density polyethylene), medium-density polyethylene, high-density polyethylene, ethylene-α-olefin copolymer, homopolypropylene, polymethylpentene, polybutene, ethylene-propylene copolymer, propylene-butene copolymer, ethylene-vinyl acetate copolymer, saponified ethylene-vinyl acetate copolymer, and mixtures thereof; thermoplastic ester-based resins such as polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polyethylene naphthalate-isophthalate copolymer, polycarbonate, and polyarylate; acrylic thermoplastic resins such as polymethyl methacrylate, polyethyl methacrylate, polyethyl acrylate, and polybutyl acrylate; polyamide-based thermoplastic resins such as nylon-6 and nylon-66; polyimide, polyurethane, polystyrene, acrylonitrile-butadiene-styrene resin, and vinyl chloride. These thermoplastic resins may be used alone or in combination of two or more. Among these, olefin-based thermoplastic resins are preferred because they are excellent in printability for the design layer and inexpensive.
[0025] The base sheet may be colored. In this case, a colorant may be added to the thermoplastic resin, and the pigment or dye used in the design layer described below may be used as the colorant.
[0026] The above-mentioned base sheet may contain various additives, such as a filler, a matting agent, a foaming agent, a flame retardant, a lubricant, an antistatic agent, an antioxidant, an ultraviolet absorbing agent, and a light stabilizer, as required.
[0027] From the viewpoint of excellent scratch resistance and bending processability, the thickness of the above-mentioned base sheet is preferably 30 μm or more and 120 μm or less, more preferably 40 μm or more and 110 μm or less, even more preferably 50 μm or more and 100 μm or less, and particularly preferably 55 μm or more and 95 μm or less.
[0028] (Picture layer) The decorative sheet of the present invention comprises a design layer.
[0029] The design layer is a layer that imparts design to the decorative sheet. The design layer may be, for example, a design pattern layer formed by printing various patterns using ink and a printing machine, or may be a layer combining a concealing layer and a design pattern layer.
[0030] The ink used for the design layer is a suitable mixture of a binder, a colorant such as a pigment or dye, an extender pigment, a solvent, a stabilizer, a plasticizer, a catalyst, a hardener, an ultraviolet absorber, a light stabilizer, etc.
[0031] The binder is not particularly limited, and examples thereof include urethane resin, acrylic polyol resin, acrylic resin, ester resin, amide resin, butyral resin, styrene resin, urethane-acrylic copolymer, polycarbonate-based urethane-acrylic copolymer (urethane-acrylic copolymer derived from a polymer (polycarbonate polyol) having a carbonate bond in the polymer main chain and having two or more hydroxyl groups at the end and side chain), vinyl chloride-vinyl acetate copolymer resin, vinyl chloride-vinyl acetate-acrylic copolymer resin, chlorinated propylene resin, nitrocellulose resin, cellulose acetate resin, etc. These binders can be used alone or in combination of two or more kinds.
[0032] As the colorant, from the viewpoint of coloring and concealing the ground color of the substrate described below and improving the design, for example, inorganic pigments such as white pigments, iron black, yellow lead, titanium yellow, red iron oxide, cadmium red, ultramarine blue, cobalt blue, etc.; organic pigments or dyes such as quinacridone red, isoindolinone yellow, phthalocyanine blue, etc.; metal pigments consisting of scaly foil flakes of aluminum, brass, etc.; and pearlescent (pearl) pigments consisting of scaly foil flakes of titanium dioxide-coated mica, basic lead carbonate, etc. can also be used.
[0033] The pattern formed on the design layer may include a wood grain vascular pattern, a marble pattern (e.g., a travertine marble pattern) or other stone pattern that imitates the surface of rock, a fabric pattern that imitates a cloth grain or fabric-like pattern, a tiled pattern, a brickwork pattern, and the like.
[0034] The thickness of the design layer is preferably 0.5 to 20 μm, and more preferably 1 to 10 μm, from the viewpoints of concealing the background color of the base sheet and improving the design.
[0035] Methods for forming the design layer include, for example, gravure printing, offset printing, screen printing, flexographic printing, electrostatic printing, inkjet printing, etc. In addition, when forming a concealing layer, various coating methods such as roll coating, knife coating, air knife coating, die coating, lip coating, comma coating, kiss coating, flow coating, dip coating, etc. can also be used.
[0036] (Transparent resin layer) The decorative sheet of the present invention comprises a transparent resin layer containing a thermoplastic resin. The transparent resin layer is not particularly limited as long as it allows the design layer to be seen, and includes any of colorless transparent, colored transparent, translucent, and the like.
[0037] Examples of the thermoplastic resin include olefin resins such as polyethylene, polypropylene, polybutene, polymethylpentene, and olefin thermoplastic elastomers; polyester resins such as polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, ethylene glycol-terephthalic acid-isophthalic acid copolymer resin, terephthalic acid-ethylene glycol-1,4 cyclohexanedimethanol copolymer resin, and polyester thermoplastic elastomers; acrylic resins such as polymethyl (meth)acrylate, methyl (meth)acrylate-butyl (meth)acrylate copolymer resin, and methyl (meth)acrylate-styrene copolymer resin; polycarbonate resin, polyvinyl chloride, polystyrene, and ionomers. Among these, polyethylene or polypropylene is more preferred because of its high tensile strength, excellent chemical resistance, and excellent production process. In this specification, (meth)acrylate means acrylate or methacrylate.
[0038] The polyethylene may be a homopolymer of ethylene or a copolymer of ethylene and another comonomer copolymerizable with ethylene (e.g., an α-olefin such as propylene, 1-butene, 1-hexene, or 1-octene, vinyl acetate, or vinyl alcohol). Examples of polyethylene resins include high density polyethylene (HDPE), medium density polyethylene (MDPE), low density polyethylene (LDPE), linear low density polyethylene (LLDPE), very low density polyethylene (VLDPE), ultra high molecular weight polyethylene (UHMWPE), and cross-linked polyethylene (PEX). These polyethylenes may be used alone or in combination of two or more.
[0039] The polypropylene may be a homopolymer of propylene or a copolymer of propylene and another comonomer copolymerizable with propylene (e.g., α-olefins such as ethylene, 1-butene, 1-hexene, and 1-octene; vinyl acetate, vinyl alcohol, etc.). These polypropylenes may be used alone or in combination of two or more. From the viewpoint of bending processability, the polypropylene is preferably a random polypropylene (random PP).
[0040] The transparent resin layer may be composed of one layer, or may be composed of two or more layers. When the transparent resin layer is composed of two or more layers, it is preferable from the viewpoint of adhesion that the side having the design layer is a layer formed from maleic acid modified polyethylene or maleic acid modified polypropylene.
[0041] The transparent resin layer may further contain various additives, if necessary. Examples of the additives include lubricants such as silicone resins, waxes, and fluororesins; colorants such as dyes and pigments; antioxidants, ultraviolet absorbers, light stabilizers, and flame retardants. The content of the additive is, for example, from 0.1% by mass to 10% by mass based on the mass of the transparent resin layer.
[0042] Examples of the ultraviolet absorbing agent include benzotriazole-based ultraviolet absorbing agents, benzophenone-based ultraviolet absorbing agents, and triazine-based ultraviolet absorbing agents, and among these, triazine-based ultraviolet absorbing agents are preferred. The above ultraviolet absorbents can be used alone or in combination of two or more.
[0043] Examples of the light stabilizer include aromatic compounds, amine compounds, organic acid compounds, catechin compounds and hindered amine compounds, and among these, hindered amine compounds are preferred. The hindered amine compound has a structure containing a 2,2,6,6-tetramethylpiperidine skeleton in the molecule. The above light stabilizers can be used alone or in combination of two or more.
[0044] The thickness of the transparent resin layer is preferably 30 μm or more and 150 μm or less, and more preferably 40 μm or more and 120 μm or less, from the viewpoint of obtaining excellent scratch resistance and bending workability. When the transparent resin layer is composed of two or more layers, the total thickness of the transparent resin layer is within the above range.
[0045] When the transparent resin layer is composed of a plurality of layers, the types of resins forming the layers may be the same or different, and the thicknesses may be the same or different. The method for laminating two or more transparent resin layers is not limited as long as it is a common method, and examples thereof include dry lamination and extrusion heat lamination.
[0046] The transparent resin layer may be subjected to surface treatment such as saponification treatment, glow discharge treatment, corona discharge treatment, plasma discharge treatment, ultraviolet (UV) treatment, and flame treatment, without departing from the spirit of the present invention.
[0047] (Surface protective layer) The decorative sheet of the present invention includes a surface protective layer.
[0048] The surface protective layer is a layer that imparts durability (scratch resistance, contamination resistance, weather resistance, etc.) to the decorative sheet, and by having the surface protective layer, it is possible to more effectively protect the pattern layer, and to effectively prevent deterioration of the design due to scratches.
[0049] The surface protective layer may contain, for example, a thermosetting resin or an ionizing radiation curable resin as a main component. The cured product is preferably transparent.
[0050] Examples of the thermosetting resin include ester-based urethane and acrylic-based urethane.
[0051] From the viewpoint of suitably imparting durability to the decorative sheet, the surface protective layer preferably contains an ionizing radiation curable resin.
[0052] Examples of the ionizing radiation curable resin include a cured product of an oligomer and / or a monomer having a radically polymerizable unsaturated group or a cationic polymerizable functional group in the molecule. The ionizing radiation means electromagnetic waves or charged particles having energy capable of polymerizing or crosslinking molecules, and is generally an electron beam (EB) or ultraviolet light (UV). The method for forming the surface protective layer is not particularly limited, and known methods can be used.
[0053] As the oligomer having a radical polymerizable unsaturated group in the molecule, for example, oligomers such as urethane (meth)acrylate, polyester (meth)acrylate, epoxy (meth)acrylate, melamine (meth)acrylate, triazine (meth)acrylate, etc. can be preferably used, and urethane (meth)acrylate oligomer is more preferable. As the molecular weight, those having about 250 or more and 100,000 or less are usually used.
[0054] The monomer having a radically polymerizable unsaturated group in the molecule is preferably, for example, a polyfunctional monomer, and more preferably a polyfunctional (meth)acrylate. Examples of polyfunctional (meth)acrylates include diethylene glycol di(meth)acrylate, propylene glycol di(meth)acrylate, bisphenol A ethylene oxide modified di(meth)acrylate, trimethylolpropane tri(meth)acrylate, trimethylolpropane ethylene oxide tri(meth)acrylate, dipentaerythritol tetra(meth)acrylate, dipentaerythritol penta(meth)acrylate {pentafunctional (meth)acrylate}, dipentaerythritol hexa(meth)acrylate {hexafunctional (meth)acrylate}, etc. Monofunctional monomers may also be used as appropriate.
[0055] The ionizing radiation curable resin preferably contains a urethane acrylate oligomer and a polyfunctional monomer in a mass ratio of urethane acrylate oligomer / polyfunctional monomer in the range of 6 / 4 or more and 9 / 1 or less.
[0056] When the ionizing radiation curable resin is crosslinked by ultraviolet light, it is preferable to use a photopolymerization initiator. The amount of the photopolymerization initiator added is, for example, 0.1 to 10 parts by mass per 100 parts by mass of the ionizing radiation curable resin.
[0057] The surface protective layer may contain a gloss adjuster. By containing the above optical adjusters, the 85 degree specular gloss value G and lightness value L of the decorative sheet can be adjusted. Examples of the gloss regulator include silica, magnesium aluminum silicate, talc, and sericite.
[0058] The content of the gloss regulator in the surface protective layer is preferably 2 parts by mass or more and 45 parts by mass or less with respect to 100 parts by mass of the ionizing radiation curable resin.
[0059] The thickness of the surface protective layer is not particularly limited, but is, for example, 1 μm to 50 μm. If the thickness of the surface protective layer is less than 1 μm, sufficient durability may not be imparted, and if it exceeds 50 μm, the transmittance may decrease, resulting in reduced visibility of the pattern of the pattern layer. The thickness of the surface protective layer may be 3 μm or more and 40 μm or may be 5 μm or more and 35 μm or more.
[0060] The surface protective layer may contain additives other than the inorganic filler as required. Examples of the additives include fillers such as calcium carbonate and clay, flame retardants such as magnesium hydroxide, antioxidants, lubricants, foaming agents, ultraviolet absorbers, light stabilizers, deodorizers, antibacterial agents, antiviral agents, antiallergens, and antifungal agents. The above additives may be used alone or in combination of two or more.
[0061] The surface protective layer preferably contains at least one agent selected from the group consisting of an antibacterial agent, an antiviral agent, and an antiallergen agent.
[0062] The antibacterial agent may be an inorganic antibacterial agent or an organic antibacterial agent. In particular, the inorganic antibacterial agent is preferred because it is generally safer than the organic antibacterial agents and has excellent durability and heat resistance. The inorganic antibacterial agent is an antibacterial metal such as silver, copper, zinc, etc. supported on various inorganic carriers.
[0063] The amount of the antibacterial agent added is preferably 0.1 to 10 parts by mass per 100 parts by mass of the resin component of the surface protective layer, but can be appropriately adjusted depending on the type of the antibacterial agent.
[0064] The above-mentioned antiviral agents can generally be broadly classified into organic and inorganic types. Examples of the organic antiviral agents include quaternary ammonium salt-based, quaternary phosphonium salt-based, pyridine-based, pyrithione-based, benzimidazole-based, organic iodine-based, isothiazolin-based, and anionic antiviral agents. Examples of the inorganic antiviral agent include those in which metal ions such as silver, copper, and zinc are supported on zeolite, apatite, zirconia, glass, molybdenum oxide, and the like. The amount of the antiviral agent added is preferably 0.1 to 10 parts by mass per 100 parts by mass of the resin component of the surface protective layer, but can be appropriately adjusted depending on the type of the antiviral agent.
[0065] Of the above organic antiviral agents, benzimidazole antiviral agents or anionic antiviral agents that maintain a particulate shape are particularly preferably used. The above-mentioned particle shape is maintained means that the particles are present in a particle state without being dissolved in the composition (ink before curing) that becomes the curable resin of the surface protective layer. Therefore, in the process of forming the surface protective layer, the particles of the benzimidazole compound or the particles of the anionic compound are easily floated, and the particles of the benzimidazole compound or the particles of the anionic compound can be easily unevenly distributed on the outermost surface side of the surface protective layer. Furthermore, by distributing the benzimidazole compound particles or the anionic compound particles unevenly on the outermost surface side of the surface protective layer, the amount of antiviral agent required to obtain a predetermined antiviral property can be reduced, making it easier to suppress a decrease in the scratch resistance of the surface protective layer.
[0066] As the anionic antiviral agent, for example, one containing a styrene polymer derivative compound and an unsaturated carboxylic acid derivative compound is preferable. In addition, the above styrene polymer derivative compound and unsaturated carboxylic acid derivative compound preferably contain at least one structure selected from the group consisting of styrene, sodium sulfonate, acrylic acid, maleic acid, and fumaric acid, and more preferably contain all of these structures. This is because there are two types of viruses: enveloped and non-enveloped, and it is believed that the structures of antiviral agents that can effectively inhibit the activity of each type are different.
[0067] As the inorganic antiviral agent, a silver-based antiviral agent is preferable from the viewpoint of lack of biotoxicity and excellent safety, and among them, a phosphate-based glass-supported silver compound, a silver zeolite compound, and a molybdenum oxide-silver double salt compound are more preferable because they exhibit antiviral performance even in small amounts and therefore the amount added can be reduced.
[0068] When the silver-based antiviral agent is added to the surface protective layer, discoloration may occur depending on the surface protective layer (the color may change due to heat or light in the ink after addition, or the color may change due to heat or light after the surface protective layer is formed). In such cases, however, it is possible to improve the situation by appropriately adding an ultraviolet inhibitor, a light stabilizer, or the like. For example, when a benzotriazole compound is used for the molybdenum oxide silver double salt compound, a discoloration preventing effect can be expected.
[0069] The antiallergen agent contains either an inorganic compound or an organic compound, and each of them may be used alone or two or more different types may be mixed. The inorganic compound is preferably a material supporting a metal. The amount of the antiallergen agent added is preferably 0.1 to 40 parts by mass per 100 parts by mass of the resin component of the surface protective layer, but can be appropriately adjusted depending on the type of the antiallergen agent.
[0070] As the inorganic material of the inorganic compound, for example, at least one selected from the group consisting of titanium oxide, calcium phosphate, calcium silicate, zirconium phosphate, zeolite, silica alumina, magnesium silicate, and magnesium phosphate is preferable, and among these, titanium oxide, zirconium phosphate, etc. are more preferable.
[0071] The metal supported on the inorganic material is preferably at least one selected from the group consisting of gold, platinum, zinc and copper other than silver, and among these, zinc is more preferable. As a commercially available product, for example, "Atomy Ball TZ-R: Titanium oxide carrying zinc" manufactured by JGC Catalysts can be suitably used. These anti-allergen agents are effective against various allergens such as mites and pollen.
[0072] The organic compound is preferably a water-insoluble polymer containing a phenolic hydroxyl group, a polyphenol compound supported on an inorganic solid acid, or a polymer containing at least one monomer component selected from the group consisting of styrenesulfonic acid and salts thereof.
[0073] As the water-insoluble polymer containing a phenolic hydroxyl group, commercially available products such as "Allerbuster (trade name)" manufactured by Sekisui Chemical Co., Ltd. and "Marukalinker M (trade name)" manufactured by Maruzen Oil Co., Ltd. can be used. An example of a combination of the polyphenol compound and the zirconium compound is "Allerremove (trade name)" manufactured by Toa Gosei Co., Ltd. These anti-allergen agents are effective against various allergens such as mites and pollen.
[0074] (Backer layer) From the viewpoint of imparting scratch resistance and impact resistance, the decorative sheet of the present invention preferably comprises a backer layer on the side of the base sheet opposite to the side on which the surface protective layer is laminated.
[0075] As the backer layer, a known backer layer disclosed in, for example, JP-A-2014-188941 can be appropriately selected and used.
[0076] The thickness of the backing layer is preferably 50 μm to 500 μm from the viewpoint of providing suitable scratch resistance and impact resistance.
[0077] (Other layers) The decorative sheet of the present invention may, for example, have an adhesive layer between the design layer and the transparent resin layer.
[0078] The adhesive layer is not particularly limited, and any known adhesive may be used. Examples include polyurethanes, acrylics, polyolefins, polyvinyl acetates, polyvinyl chlorides, vinyl chloride-vinyl acetate copolymers, ethylene-acrylic acid copolymers, ionomers, as well as butadiene-acrylonitrile rubber, neoprene rubber, and natural rubber. These adhesives may be used alone or in combination of two or more.
[0079] The adhesive layer preferably has a thickness after drying of about 0.1 to 30 μm, more preferably about 1 to 5 μm.
[0080] The decorative sheet of the present invention may have a primer layer, if necessary.
[0081] The primer layer can be formed by applying a known primer agent. Examples of the primer agent include a urethane resin-based primer agent made of an acrylic-modified urethane resin (acrylic urethane-based resin), a primer agent made of a urethane-cellulose-based resin (for example, a resin obtained by adding hexamethylene diisocyanate to a mixture of urethane and soluble cellulose), and a resin-based primer agent made of a block copolymer of acrylic and urethane.
[0082] The primer agent may contain additives as required. Examples of the additives include fillers such as calcium carbonate and clay, flame retardants such as magnesium hydroxide, antioxidants, lubricants, foaming agents, ultraviolet absorbers, light stabilizers, etc. The amount of additives to be added can be appropriately determined depending on the product characteristics.
[0083] The primer layer may contain an ultraviolet absorbing agent, if necessary. As the ultraviolet absorbing agent, any known ultraviolet absorbing agent can be appropriately selected and used.
[0084] The primer layer can be provided, for example, on one or both sides of the transparent resin layer, on one or both sides of the base sheet, or the like.
[0085] The thickness of the primer layer is not particularly limited, but is, for example, preferably 0.01 to 10 μm, and more preferably 0.1 to 1 μm.
[0086] (Uneven shape) The decorative sheet of the present invention has an uneven shape on the surface on which the above-mentioned surface protective layer is provided, from the viewpoint of providing a suitable design. The uneven shape may reach the transparent resin layer.
[0087] The uneven shape has directionality. Examples of the above-mentioned uneven shapes include wood grain duct shapes, stone grain shapes imitating the surface of rocks such as marble patterns (e.g. travertine marble patterns), fabric shapes imitating cloth grain or fabric-like patterns, tiled shapes, brick masonry shapes, and the like, which have directional characteristics. Specifically, the uneven shape may be one in which the difference in the 85 degree specular gloss G is 15% or more.
[0088] FIG. 2 is an explanatory diagram for explaining the direction of the concave-convex shape and the direction perpendicular to the direction of the concave-convex shape. In FIG. 2, grain vessel-like irregularities are formed. In this specification, the direction in which the wood grain vessels flow as shown in FIG. 2 is defined as the "direction of the uneven shape." In addition, in cases other than wood grain vascular-like unevenness, the direction in which the uneven shape flows is defined as the "direction of the uneven shape," and the direction in which the uneven shape flows is defined as the longitudinal direction of the uneven shape (the longest direction when the end points of the uneven shape are taken).
[0089] The maximum height Rz of the uneven shape is preferably 20 μm or more and 60 μm or less. By having the above-mentioned uneven shape, it is possible to suitably impart an excellent design that gives a three-dimensional feel not only visually but also tactilely (touch-wise). Incidentally, "maximum height Rz" refers to the maximum height Rz specified in JIS B 0601 (2001).
[0090] The uneven shape may be a ridge-like portion that protrudes in a ridge shape.
[0091] The ridge-like protruding portions can be formed, for example, by pre-curing the ionizing radiation curable resin constituting the surface protective layer using a UV irradiation device. Next, the surface of the pre-cured ionizing radiation curable resin is irradiated with excimer light having energy capable of cutting polymer chains to shrink the surface of the ionizing radiation curable resin, thereby forming ridge-like protruding portions on the surface of the surface protective layer. Thereafter, the shrunk ionizing radiation curable resin is irradiated with ionizing radiation (which cures the ionizing radiation curable resin) to cure the ionizing radiation curable resin.
[0092] The UV irradiation device in the above preliminary curing is preferably an LED. The excimer light preferably has a wavelength of about 120 to 230 nm. The ionizing radiation that cures the ionizing radiation curable resin refers to electromagnetic waves or charged particles having energy capable of polymerizing or crosslinking molecules, and generally includes electron beams (EB) or ultraviolet rays (UV).
[0093] The uneven shape may be formed by embossing.
[0094] The uneven shape can be formed, for example, by thermal embossing. The above-mentioned thermal embossing process may be carried out, for example, by a well-known sheet-type or rotary embossing machine. The embossed pattern may be formed according to the pattern of the design layer.
[0095] (Method of manufacturing decorative sheets) In the method for producing a decorative sheet of the present invention, the order in which the above-mentioned layers are formed is not particularly important. For example, a primer layer, a design layer, an adhesive layer, a transparent resin layer, a primer layer, and a surface protective layer may be formed in this order on one surface of a substrate sheet. Furthermore, the steps of forming each layer do not have to proceed consecutively, and other steps or treatments may be carried out between these steps.
[0096] Methods for adjusting the difference in 85 degree specular gloss G between the direction of the uneven shape of the decorative sheet of the present invention and the direction perpendicular to the direction of the uneven shape, as measured by a method conforming to JIS Z 8741:1997, and methods for making the relationship between the maximum 85 degree specular gloss G' measured by a method conforming to JIS Z 8741:1997, and the lightness L as conforming to JIS Z 8781-4:2013 satisfy the above formula (1), include adjusting the L value by adjusting the shade of the color tone of the picture pattern of the picture layer, adjusting the content of the gloss adjuster blended in the ionizing radiation curable resin of the surface protective layer, adjusting the uneven shape caused by irradiation with excimer light, and adjusting the G' value for the uneven shape caused by embossing. In particular, the L value can be increased by making the color tone of the pattern lighter. It is effective to increase the content of gloss regulators, reduce the amount of LED-UV irradiation, increase the ultraviolet output density by excimer irradiation, and deepen the embossing plate to reduce the G' value.
[0097] <Decorative board> The decorative sheet of the present invention can be made into a decorative board by laminating an adherend on the side of the above-mentioned base sheet opposite to the side having the pattern layer.
[0098] Examples of the adherend include a wood board, a gypsum board, a cement board, a ceramic board, a metal board, a resin board, and a fiber-reinforced plastic board. For example, the adherend may be laminated on the side of the substrate sheet of the present disclosure opposite the side having the pattern layer using an adhesive that forms the adhesive layer described above.
[0099] The present specification discloses the following:
[0100] The present disclosure (1) is a decorative sheet comprising, on one side of a base sheet containing a thermoplastic resin, a pattern layer, a transparent resin layer containing a thermoplastic resin, and a surface protective layer, at least in this order, and having an uneven shape on the side on which the surface protective layer is provided, wherein the difference in 85 degree specular gloss G between the direction of the uneven shape and a direction perpendicular to the direction of the uneven shape, as measured by a method in accordance with JIS Z 8741:1997, is 15% or more, and the relationship between the maximum 85 degree specular gloss G', as measured by a method in accordance with JIS Z 8741:1997, and the lightness L, as measured by JIS Z 8781-4:2013, satisfies the following formula (1): L>1.5G' 2 -5G'-10 (1) (However, in the above formula (1), G'≧0 and 15≦L≦95 are satisfied.) The present disclosure (2) is the decorative sheet according to the present disclosure (1), wherein the surface protective layer contains an ionizing radiation curable resin. The present disclosure (3) is the decorative sheet according to the present disclosure (1) or (2), in which the uneven shape is a ridge-like portion protruding in a ridge shape. The present disclosure (4) is the decorative sheet according to any one of the present disclosures (1) to (3), in which the uneven shape is formed by embossing. The present disclosure (5) is the decorative sheet according to any one of the present disclosures (1) to (4), further comprising a backer layer on the side of the base sheet opposite to the side on which the surface protective layer is laminated. The present disclosure (6) is a decorative sheet according to any one of the present disclosures (1) to (5), wherein the surface protective layer contains at least one agent selected from the group consisting of an antibacterial agent, an antiviral agent, and an antiallergen agent. EXAMPLES
[0101] The present invention will now be described in more detail with reference to examples, but is not limited to these examples.
[0102] Example 1 A base sheet made of a 60 μm thick colored polypropylene film was prepared. A 2 μm-thick light-colored wood-grain pattern layer was formed by printing on one side of the above-mentioned base sheet, and then a 3 μm-thick adhesive layer was formed on the pattern layer using a two-component curing urethane-based dry lamination adhesive (mixed with polyester polyol 1,6-hexamethylene diisocyanate (HMDI)). Next, a transparent resin layer (10 μm maleic acid modified PP on the transparent adhesive layer side, 50 μm random PP on the surface protection layer side, total thickness 60 μm) was laminated on the adhesive layer by extrusion lamination. The transparent resin layer was subjected to a corona discharge treatment, and an acrylic urethane resin (a two-component curing polyurethane resin containing an acrylic polyol and a urethane polyol as main agents and containing 1,6-hexamethylene diisocyanate (HMDI) as a curing agent) was applied to the treated surface by a gravure coating method to form a primer layer. A urethane acrylate-based ionizing radiation curable resin (containing 40 parts by weight of a gloss adjuster (product name ACEMATT (registered trademark) 3300, manufactured by EVONIK)) was applied by gravure coating onto the above primer layer as a surface protective layer, and after drying, the uncured surface protective layer was irradiated with an electron beam (accelerating voltage 175 KeV, irradiation dose 5 Mrad) in an environment with an oxygen concentration of 200 ppm or less to harden it, thereby forming a surface protective layer. Next, the surface protective layer side was embossed with an embossing plate to form a grain vessel-like uneven pattern with a maximum height Rz of 50 μm. Thereafter, a 120 μm thick olefin film was attached to the back surface of the substrate sheet (the surface opposite to the surface protective layer) to form a backer layer, thereby producing a decorative sheet. Based on the method described in this specification, the difference in 85-degree specular gloss G between the direction of the uneven shape and the direction perpendicular to the direction of the uneven shape (abbreviated as "difference in 85-degree specular gloss G" in Tables 1 and 2), the maximum value of 85-degree specular gloss G', and the lightness L were measured. These are shown in Table 1. In Tables 1 to 3, those in which a concave-convex shape was formed by embossing were designated "Embossed+", those with ridge-like protruding portions were designated "Excimer+", and those in which a concave-convex shape was formed by embossing and those with ridge-like protruding portions were designated "Embossed+" and "Excimer+". On the other hand, those in which a concave-convex shape was not formed by embossing were designated "Embossed-", and those without ridge-like protruding portions were designated "Excimer-".
[0103] (Examples 2 to 12, Comparative Examples 1 to 5) A decorative sheet was produced in the same manner as in Example 1, except that the color tone of the picture pattern in the picture layer and the content of the gloss regulator in the ionizing radiation curable resin constituting the surface protective layer were changed. Based on the method described in this specification, the difference in 85-degree specular gloss G between the direction of the uneven shape and the direction perpendicular to the direction of the uneven shape, the maximum value G' of the 85-degree specular gloss, and the lightness L were measured. These are shown in Tables 1 and 2.
[0104] Example 13 A base sheet made of a 60 μm thick colored polypropylene film was prepared. A 2 μm-thick pattern layer was formed on one side of the above-mentioned base sheet by printing, and then a 3 μm-thick adhesive layer was formed on the pattern layer using a two-component curing urethane-based dry lamination adhesive (mixed with polyester polyol 1,6-hexamethylene diisocyanate (HMDI)). Next, a transparent resin layer (10 μm maleic acid modified PP on the transparent adhesive layer side, 50 μm random PP on the surface protection layer side, total thickness 60 μm) was laminated on the adhesive layer by extrusion lamination. The transparent resin layer was subjected to a corona discharge treatment, and an acrylic urethane resin (a two-component curing polyurethane resin containing an acrylic polyol and a urethane polyol as main agents and containing 1,6-hexamethylene diisocyanate (HMDI) as a curing agent) was applied to the treated surface by a gravure coating method to form a primer layer. A surface protective layer was formed on the primer layer by applying a urethane acrylate-based ionizing radiation curable resin that did not contain a gloss regulator by gravure coating, and the surface protective layer was irradiated with ultraviolet light using a UV irradiation device consisting of LEDs (LED-UV irradiation, wavelength 395 nm, maximum irradiation 0.6 W / cm). 2 , cumulative light intensity 30mJ / cm 2 ), and preliminary curing was performed. Next, ultraviolet light was irradiated using an excimer light irradiation device (excimer irradiation, wavelength 172 nm (Xe 2 ), UV power density 30mW / cm 2 , cumulative light intensity 30mJ / cm 2 In a nitrogen atmosphere, the film was then irradiated with an electron beam (accelerating voltage 175 KeV, dose 5 Mrad) in an environment with an oxygen concentration of 200 ppm or less to harden the film and form a surface protective layer. Thereafter, the surface protective layer was embossed with an embossing plate to form a grain vessel-like uneven pattern with a maximum height Rz of 50 μm. Finally, a 120 μm thick olefin film was attached to the back surface of the base sheet (the surface opposite to the side having the design layer) to form a backer layer, thereby producing a decorative sheet. Based on the method described in this specification, the difference in 85-degree specular gloss G between the direction of the uneven shape and the direction perpendicular to the direction of the uneven shape, the maximum value G' of the 85-degree specular gloss, and the lightness L were measured. These are shown in Table 3.
[0105] (Examples 14 to 16) A decorative sheet was produced in the same manner as in Example 13, except that the color tone of the picture pattern of the picture layer, the LED-UV irradiation conditions when forming the surface protective layer, and the excimer irradiation conditions were changed. Based on the method described in this specification, the difference in 85-degree specular gloss G between the direction of the uneven shape and the direction perpendicular to the direction of the uneven shape, the maximum value G' of the 85-degree specular gloss, and the lightness L were measured. These are shown in Table 3.
[0106] (Example 17) A decorative sheet was produced in the same manner as in Example 1, except that 3 parts by mass of a phosphate-based glass-silver-supported compound (PG-711, manufactured by Koa Glass Co., Ltd.) was added as an antiviral agent to 100 parts by mass of the urethane acrylate-based ionizing radiation-curable resin used as the surface protective layer.
[0107] (Example 18) A decorative sheet was manufactured in the same manner as in Example 1, except that 16 parts by mass each of an anionic phenol-based material (anti-allergen agent, EXP20530A manufactured by DIC Corporation) and a zinc-based material (anti-allergen agent, EXP20530B manufactured by DIC Corporation) were blended with 100 parts by mass of the urethane acrylate-based ionizing radiation curable resin used as the surface protective layer.
[0108] <Evaluation method> (Preparation of decorative panels for evaluation) A 50 μm thick cellophane adhesive tape measuring 25 mm x 25 mm was applied to the surface of a wooden substrate (MDF) to create an uneven surface. Thereafter, the primer layer formed on the back surface of the base sheet of the decorative sheet produced in the examples and comparative examples was bonded to the above-mentioned wood base material (MDF) using a two-component curing water-based adhesive to produce a decorative panel for evaluation.
[0109] (Design Defect Assessment) The prepared decorative panel for evaluation was placed on a flat surface in a bright room (illuminance of 500 lux according to JIS C 7612). The uneven portion of the cellophane adhesive tape was visually observed at a distance of 50 cm at observation angles of 20 degrees, 60 degrees, and 85 degrees. FIG. 3 is an explanatory diagram for explaining the test method for evaluating design defects. As shown in FIG. 3, the observation angle was the angle between the normal direction to the uneven portion of the cellophane adhesive tape and the direction in which the uneven portion of the cellophane adhesive tape was visually observed. The evaluation criteria are as follows: ++: No unevenness can be recognized even at an observation angle of 85 degrees. +: No unevenness is discernible at an observation angle of 20 degrees or 60 degrees, but unevenness is discernible at an observation angle of 85 degrees. -: Irregularities can be confirmed at an observation angle of 20 degrees or 60 degrees.
[0110] (Anti-virus performance) The decorative sheets produced in Examples 1 and 17 were subjected to an antiviral performance test in accordance with the antiviral test method (ISO21702), and the antiviral activity value against influenza virus was evaluated based on the following evaluation criteria. The results are shown in Table 4. In addition, the antiviral agent (parts by mass) in Table 4 means the amount (parts by mass) of the antiviral agent used per 100 parts by mass of the surface protective layer (urethane acrylate-based ionizing radiation curable resin). +: Antiviral activity value was 2.0 or higher -: Antiviral activity value was less than 2.0 A "+" was considered a pass and a "-" was considered a fail.
[0111] (Anti-allergen performance) The decorative sheets produced in Example 1 and Example 18 were evaluated for anti-allergen performance. Specifically, the decorative sheets (10 cm x 10 cm) produced in Examples 1 and 18 were cut into small pieces and immersed in 60 mL of an aqueous solution of 20 to 30 ng / mL of allergen derived from Dermatophagoides farinae for one day. The amount of allergen was then visually confirmed by horizontal development chromatography (Mighty Checker) and evaluated according to the following evaluation criteria. The results are shown in Table 5. In addition, the anionic phenol-based material (parts by mass) and zinc-based material (parts by mass) listed in Table 5 refer to the amount (parts by mass) of the anionic phenol-based material and zinc-based material used per 100 parts by mass of the coating agent (urethane acrylate-based ionizing radiation curable resin composition). +: A reduction in the amount of allergens was confirmed (the mite allergen level was below + (i.e., about 100 mites / m 2 below) -: No reduction in allergens was confirmed (mite allergen level judged as + or higher) A "+" was considered a pass and a "-" was considered a fail.
[0112] [Table 1]
[0113] [Table 2]
[0114] [Table 3]
[0115] [Table 4]
[0116] [Table 5]
[0117] FIG. 4 is a graph of formula (1) and a diagram showing the maximum 85 degree specular gloss G' and lightness L measured for the decorative sheets of the examples and comparative examples. FIG. 4 shows that all of the decorative sheets of the examples satisfy formula (1), whereas the decorative sheets of the comparative examples do not satisfy formula (1). Tables 1 to 3 and Figure 4 confirm that in a decorative sheet in which the difference in 85-degree specular gloss G between the direction of the unevenness shape and the direction perpendicular to the direction of the unevenness shape is within a specified range, and the relationship between the maximum 85-degree specular gloss G' and the lightness L satisfies the above formula (1), it is possible to improve design defects caused by unevenness on the surface of a wood substrate. In addition, it was confirmed from Table 4 that the surface protective layer can impart antiviral performance by including an antiviral agent, and from Table 5 that the surface protective layer can impart antiallergen performance by including an antiallergen agent. [Explanation of symbols]
[0118] 1 Base sheet 2. Picture layer 3 Transparent resin layer 4 Surface protective layer 10 Decorative Sheet 20 Evaluation board
Claims
1. A substrate sheet including a thermoplastic resin is provided on one side thereof with a design layer, a transparent resin layer including a thermoplastic resin, and a surface protective layer, at least in this order; The surface on the side having the surface protective layer has an uneven shape, a difference in 85-degree specular gloss G between the direction of the unevenness shape and a direction perpendicular to the direction of the unevenness shape, as measured by a method conforming to JIS Z 8741:1997, is 15% or more; A decorative sheet in which the relationship between the maximum 85-degree specular gloss G' measured in accordance with JIS Z 8741:1997 and the lightness L measured in accordance with JIS Z 8781-4:2013 satisfies the following formula (1). L>1.5G' 2 -5G'-10 (1) (However, in the above formula (1), G'≧0 and 15≦L≦95 are satisfied.)
2. The decorative sheet according to claim 1 , wherein the surface protective layer comprises an ionizing radiation curable resin.
3. 3. The decorative sheet according to claim 1, wherein the uneven shape is a ridge-like portion that protrudes in a ridge shape.
4. 3. The decorative sheet according to claim 1, wherein the uneven surface is formed by embossing.
5. 3. The decorative sheet according to claim 1, further comprising a backer layer on the side of the base sheet opposite to the side on which the surface protective layer is laminated.
6. 3. The decorative sheet according to claim 1, wherein the surface protective layer comprises at least one agent selected from the group consisting of an antibacterial agent, an antiviral agent, and an antiallergen agent.
Citation Information
Patent Citations
Decorative sheet and decorative board
JP2018100502A