Junction structure between metal wiring and inorganic oxide wiring
By positioning inorganic oxide wiring junctions at minimal thermal stress points and maintaining specific distances, the bonding structure addresses the disconnection issue in scanning antennas, ensuring durability during high-temperature processing.
Patent Information
- Application Number
- JP2023053322
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The disconnection of inorganic oxide wiring at the boundary between metal wiring and an adhesive layer due to thermal stress during high-temperature processing in the manufacturing of scanning antennas, primarily caused by differences in thermal expansion coefficients and Young's modulus, is a significant issue.
A bonding structure is devised where the inorganic oxide wiring is joined to the metal wiring at multiple positions along the longitudinal direction, with these junctions positioned where thermal stress is minimal, typically more than 500 μm away from the metal wiring ends, and the distance between these junctions is maintained at 20 μm or more.
This configuration significantly reduces the likelihood of inorganic oxide wiring disconnection during high-temperature processing, ensuring a stable connection between metal and inorganic oxide wirings.
Smart Images

Figure 2024141588000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a junction structure between a metal wiring and an inorganic oxide wiring, and more particularly to a junction structure between a metal wiring and an inorganic oxide wiring of a scanning antenna. [Background technology]
[0002] Phased array antennas, which are equipped with antenna units, are known as antennas (scanning antennas) that have the function of changing the radiation direction of a beam. Phased array antennas require phase shifters. In order to make phased array antennas cheaper to manufacture, phase shifters using liquid crystal are becoming more and more popular.
[0003] Patent Document 1 describes a scanning antenna that utilizes liquid crystal display technology and includes low-resistance metal wiring and high-resistance inorganic oxide wiring. The low-resistance metal wiring is surrounded by a relatively soft adhesive layer, and high-resistance inorganic oxide wiring is provided across a part of the metal wiring and a part of the adhesive layer. A phase shifter is physically and electrically connected to the high-resistance inorganic oxide wiring arranged on the adhesive layer via an anisotropic conductive film.
[0004] FIG. 3 shows the positional relationship between such metal wiring and inorganic oxide wiring, with FIG. 3(a) being an explanatory plan view and FIG. 3(b) being an explanatory cross-sectional view of the essential parts.
[0005] As can be seen from these figures, an adhesive layer 20 is laminated on one side of a substrate 10, and a metal wiring 30 is disposed on the adhesive layer 20 and fixed to the substrate 10 by the adhesive layer 20. As can be seen from Fig. 3(a), the metal wiring 30 has an elongated planar shape having a longitudinal direction and a lateral direction, and is therefore surrounded by the adhesive layer 20 exposed on the surface. The metal wiring 30 must have low resistance, and for this reason, for example, a metal foil having a thickness of 1 to 10 µm formed by electrolytic plating or sputtering is often used.
[0006] Next, the inorganic oxide wiring 40 is disposed across a part of the metal wiring 30 and a part of the adhesive layer 20 around it, and the metal wiring 30 and the inorganic oxide wiring 40 are physically and electrically connected with each other at the part located on the metal wiring 30 as a joining position. The inorganic oxide wiring 40 needs to have high resistance, and for this reason, a vapor deposition film of an inorganic oxide such as ITO is usually used. In addition, its thickness is thinner than that of the metal wiring 30, about 10 to 1000 nm. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] International Publication No. 2020 / 121876 Summary of the Invention [Problem to be solved by the invention]
[0008] Incidentally, in the manufacturing process of the scanning antenna, a process of heating both the metal wiring 30 and the inorganic oxide wiring 40 after they are formed may be required. For example, in the process of forming a photospacer using a negative photoresist, there is a process of baking the patterned photoresist at a high temperature of about 230°C to completely harden it. Also, even when forming a protective film by forming a film of an inorganic silicone compound such as SiN on the metal wiring 30 and the inorganic oxide wiring 40 to protect them, the film may be heated to a high temperature of 200 to 250°C during the film formation.
[0009] When heated to such a high temperature, as shown in Fig. 4(a) and Fig. 4(b), the inorganic oxide wiring 40 often breaks at the boundary between the metal wiring 30 and the adhesive layer 20. In Fig. 4(a) and Fig. 4(b), 40x indicates the break position of the inorganic oxide wiring 40. It can be assumed that the cause is thermal stress at the boundary between the metal wiring 30 and the adhesive layer 20 due to differences in the thermal expansion coefficient and Young's modulus of the adhesive layer 20, the metal wiring 30, and the inorganic oxide wiring 40. It can also be assumed that the break is related to the fact that the thickness of the inorganic oxide wiring 40 is thinner, about 10 to 1000 nm, while the thickness of the metal wiring 30 is 1 to 10 μm, the material of the inorganic oxide wiring 40 is brittle, and the width of the inorganic oxide wiring 40 is narrow.
[0010] The present invention has been made under the above circumstances, and has an object to provide a junction structure between metal wiring and inorganic oxide wiring in which the inorganic oxide wiring is less likely to break even when heated to high temperatures. [Means for solving the problem]
[0011] With this technical background, the inventors of the present invention performed a simulation of the stress that occurs when heat is applied to a metal wiring having a long and narrow planar shape arranged on an adhesive layer as shown in Fig. 3. As a result, it was found that the stress is large near the end 300 of the side extending along the longitudinal direction of the metal wiring, and therefore, if an inorganic oxide wiring is arranged at this position, it is likely to break.
[0012] On the other hand, the stress decreases with distance from the end 300, and even if an inorganic oxide wiring is disposed at this position, disconnection is unlikely to occur. However, the stress does not decrease with distance from the end 300, but there is a portion at a certain distance where the stress is minimal, but the position varies depending on the shape and dimensions of the metal wiring, the thermal expansion coefficient of the metal wiring, the thermal expansion coefficient of the adhesive layer, the degree of thermal load, etc. Generally, the portion where the stress is minimal is located 500 μm or more away from the end 300.
[0013] The present invention was made based on such research results, and a first aspect of the present invention is a bonding structure between a metal wiring arranged on an adhesive layer and an inorganic oxide wiring arranged across a part of the metal wiring and a part of the adhesive layer surrounding the metal wiring, The metal wiring has an elongated planar shape having a longitudinal direction and a lateral direction, This is a joint structure between a metal wiring and an inorganic oxide wiring, characterized in that the metal wiring and the inorganic oxide wiring are joined at a plurality of joining positions, and that these plurality of joining positions are arranged along the longitudinal direction of the metal wiring.
[0014] The plurality of bonding positions desirably includes a position between the bonding positions at both ends where the stress applied to the metal wiring becomes minimum when the metal wiring is heated. The bonding position may be 500 μm or more away from the longitudinal end of the metal wiring. Also, the distance between the bonding positions at both ends is desirably 20 μm or more.
[0015] It should be noted that instead of a plurality of these joining positions, a wide range of joining positions may be provided so as to encompass all of the plurality of these joining positions.
[0016] The second aspect of the present invention is a bonding structure having such a wide bonding position, which is a bonding structure between a metal wiring arranged on an adhesive layer and an inorganic oxide wiring arranged across a part of the metal wiring and a part of the adhesive layer surrounding the metal wiring, The metal wiring has an elongated planar shape having a longitudinal direction and a lateral direction, The joint between the metal wiring and the inorganic oxide wiring is along the longitudinal direction of the metal wiring. The junction structure between metal wiring and inorganic oxide wiring is characterized by being configured to be wide. Effect of the Invention
[0017] According to the present invention, it is possible to obtain a joint structure between a metal wiring and an inorganic oxide wiring in which the inorganic oxide wiring is less likely to break even when heated to a high temperature. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is an explanatory plan view for explaining the positional relationship between a metal wiring and an inorganic oxide wiring according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is an explanatory plan view for explaining the positional relationship between a metal wiring and an inorganic oxide wiring according to a second embodiment of the present invention. [Diagram 3] FIG. 3 relates to a conventional scanning antenna and shows the positional relationship between metal wiring and inorganic oxide wiring, where FIG. 3(a) is an explanatory plan view and FIG. 3(b) is an explanatory cross-sectional view of a main portion. [Figure 4] FIG. 4 relates to a conventional scanning antenna, and shows the positional relationship between the metal wiring and the inorganic oxide wiring when the inorganic oxide wiring is disconnected, where FIG. 4(a) is an explanatory plan view and FIG. 4(b) is an explanatory cross-sectional view of the main part. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] <First embodiment> In the scanning antenna A according to the first embodiment of the present invention, an adhesive layer 20 is laminated on one side of a substrate 10, and a low-resistance metal wiring 30 is disposed on the adhesive layer 20 and fixed to the substrate 10 by the adhesive layer 20, as in the conventional scanning antenna. The metal wiring 30 has an elongated planar shape having a longitudinal direction and a lateral direction, and is therefore surrounded by the adhesive layer 20 exposed on the surface. Similarly to the conventional scanning antenna, the inorganic oxide wiring 40 is also disposed across a part of the metal wiring 30 and a part of the adhesive layer 20 around it, and the metal wiring 30 and the inorganic oxide wiring 40 are physically and electrically connected with each other at the part located on the metal wiring 30 as the joint position. The difference between the scanning antenna A according to the first embodiment of the present invention and the conventional scanning antenna is in the joint structure between the metal wiring and the inorganic oxide wiring, and in other respects, the two are similar to each other.
[0020] In order to explain the positional relationship between the metal wiring 30 and the inorganic oxide wiring 40 according to the first embodiment of the present invention, an explanatory plan view thereof is shown in FIG.
[0021] 1, the inorganic oxide wiring 40 has its tip branched into branches, and the tips of the branches 41 are connected to the metal wiring 30 as joining positions 400. Therefore, the number of the branches 41 is the same as the number of joining positions 400. The number of the branches 41 and the joining positions 400 may be 2 or more, but may be 10 or more.
[0022] A plurality of these bonding positions 400 are arranged along the longitudinal direction of the metal wiring 30. Therefore, the inorganic oxide wiring 40 extends in a direction perpendicular to the longitudinal direction of the metal wiring 30, in other words, parallel to the lateral direction.
[0023] Incidentally, it is desirable that a position at which the stress applied to the metal wiring 30 is minimal when the metal wiring 30 is heated is included between both ends of the multiple bonding positions 400. When a bonding position 400 exists at a position at which the thermal stress is minimal in this way, the inorganic oxide wiring 40 is least likely to break at the bonding position 400 where the thermal stress is minimal. This is because, when a position at which the thermal stress is minimal is included between both ends of the multiple bonding positions 400, a bonding position 400 that is thus least likely to break exists among these multiple bonding positions 400. Since all of the bonding positions 400 are connected to the inorganic oxide wiring 40, the metal wiring 30 and the inorganic oxide wiring 40 are unlikely to break even when heated to a high temperature.
[0024] The position where the stress applied to the metal wiring 30 becomes minimum when the metal wiring 30 is heated can be determined by an experiment, but may be calculated by a simulation. In general, the position is a position 500 μm or more away from the end 300 in the longitudinal direction of the metal wiring 30. For this reason, it is desirable to arrange the joining position 400, among the plurality of joining positions 400, closest to the end 300 in the longitudinal direction of the metal wiring 30 at a position 500 μm or more away from the end 300 in the longitudinal direction of the metal wiring 30. In the figure, α indicates the distance between the end 300 in the longitudinal direction of the metal wiring 30 and the joining position 400 closest thereto.
[0025] For the same reason, it is desirable that the length β between the bonding position 400 closest to the longitudinal end 300 of the metal wiring 30 and the bonding position 400 furthest from the longitudinal end 300 is 20 μm or more.
[0026] (Base material 10) The substrate 10 is made of an insulating material. A typical material for the substrate 10 is glass, but flexibility can be imparted to the substrate 10 by using various plastic films. In this embodiment, the material for the substrate 10 is glass.
[0027] The adhesive layer 20 is provided on the substrate 10. The adhesive layer 20 is a layer formed from a known adhesive. This adhesive layer 20 is generally relatively soft and has a pencil hardness of HB to 2H. In order to bond the adhesive layer 20 to the metal wiring 30, it is necessary to use an adhesive layer 20 that is relatively soft, and it is difficult to use an adhesive layer 20 with high hardness.
[0028] The metal wiring 30 is provided on a portion of the adhesive layer 20 .
[0029] The metal wiring 30 is formed in an elongated planar shape having a long side direction and a short side direction. In this first embodiment, the metal wiring 30 is in a straight line shape that is folded back halfway.
[0030] The metal wiring 30 is attached to the substrate 10 via an adhesive layer 20. In the scanning antenna A, the metal wiring 30 serves as a low resistance wiring.
[0031] In this first embodiment, the metal wiring 30 is made of copper. The metal wiring 30 may be made of a metal with a low resistivity, such as silver or aluminum.
[0032] From the viewpoint of reducing resistance, it is desirable for the metal wiring 30 to be a thick film, and the thickness of the metal wiring 30 can be set to, for example, 1 to 10 μm.
[0033] The inorganic oxide wiring 40 is provided across a part of the metal wiring 30 and a part of the adhesive layer 20 around it. As a result, the metal wiring 30 and the inorganic oxide wiring 40 are connected with the part located on the metal wiring 30 as a bonding position 400. In the scanning antenna A, the inorganic oxide wiring 40 serves as a high resistance wiring.
[0034] The inorganic oxide wiring 40 is made of an inorganic oxide. For example, it can be made of an inorganic oxide having a high resistivity, such as indium tin oxide (ITO) or indium zinc oxide (IZO). From the viewpoint of increasing the resistance, it is desirable for the inorganic oxide wiring 40 to be a thin film, and the thickness thereof can be, for example, 10 nm to 1000 nm.
[0035] An example of a method for manufacturing the scanning antenna A of this embodiment having the above-mentioned configuration will be described.
[0036] The method for manufacturing the scanning antenna 1 of this embodiment includes a first sub-step, a first step, a second step, a third step, and a fourth step.
[0037] The first sub-step is a step of applying a liquid adhesive to the entire surface of the metal foil facing one side to form an adhesive layer 20. The adhesive layer 20 is formed on the surface of the metal foil facing one side by using a roll coating method.
[0038] The metal foil is a copper foil formed into a sheet shape, and can be formed by sputtering or electrolytic plating.
[0039] The first step is a step of bonding a metal foil onto a substrate 10 via an adhesive layer 20. In the first step, the adhesive layer 20 formed on the entire surface of the metal foil facing one side is first brought into contact with the substrate 10. Next, the adhesive layer 20 is dried while the metal foil and the substrate 10 are pressed together at a predetermined pressure. This allows the metal foil and the substrate 10 to be bonded together via the adhesive layer 20.
[0040] As described above, in the first sub-step, the adhesive layer 20 is formed on the entire surface of the metal foil facing one side, and then in the first step, the metal foil and the substrate 10 are bonded together. However, the procedure for bonding the metal foil and the substrate 10 is not limited to this. For example, in the first sub-step, an adhesive may be applied to the entire surface of the substrate 10 facing the other side to form the adhesive layer 20, and in the first step, the metal foil may be brought into contact with the adhesive layer 20, and then the above-mentioned pressure bonding and drying may be performed to bond the metal foil and the substrate 10. In this case, the adhesive layer 20 is formed on the surface of the substrate 10 facing the other side by a coating method such as a die coating method or a slit & spin coating method.
[0041] The second step is a step of patterning the metal foil to form metal wiring 30 on a part of the adhesive layer 20. The patterning of the metal foil is performed by photolithography.
[0042] In the second step, a photoresist layer is first formed on the metal foil. The photoresist is applied onto the metal foil by a general spin coater to form a photoresist layer.
[0043] Next, the photoresist layer is pre-baked, for example, in a chamber under reduced pressure to dry the photoresist layer, thereby shortening the drying time of the photoresist layer.
[0044] Next, the photoresist layer is exposed to ultraviolet light through a photomask on which a pattern corresponding to the metal wiring 30 is drawn.
[0045] Next, the exposed photoresist layer is developed. A positive developer can be used as the developer. A spray development method can be used as the development method.
[0046] Next, the metal foil is etched to remove the portions of the metal foil from which the photoresist layer has been removed, and the metal foil is patterned into a pattern shape corresponding to the metal wiring 30. As the etching liquid, a mixed aqueous solution of hydrogen peroxide, sulfuric acid, and water can be used.
[0047] Next, the photoresist layer remaining on the metal wiring 30 is stripped. A silicate solution can be used as the stripping liquid. Then, the metal wiring 30 is post-baked. In this embodiment, the post-baking is performed in a chamber with a nitrogen atmosphere. The baking temperature is 250° C. The baking time is 90 minutes. When the post-baking of the metal wiring 30 is completed, the second step is completed, and the metal wiring 30 having the pattern shape is formed on a part of the adhesive layer 20.
[0048] The third step is a step of forming an inorganic oxide layer on the metal wiring 30 and the adhesive layer 20. The inorganic oxide layer is formed by laminating the inorganic oxide on the metal wiring 30 and the adhesive layer 20 by sputtering. When the third step is completed, the inorganic oxide layer is formed on the metal wiring 30 and the adhesive layer 20.
[0049] The fourth step is a step of patterning the inorganic oxide layer to form the inorganic oxide wiring 40. The patterning of the inorganic oxide wiring 40 can be performed by photolithography.
[0050] In the fourth step, a photoresist layer is formed on the inorganic oxide layer. As the photoresist, a novolac resin, which is a positive photoresist, can be used.
[0051] Next, the photoresist layer is pre-baked, and then exposed to ultraviolet light through a photomask on which a pattern corresponding to the inorganic oxide wiring 40 is drawn.
[0052] Next, the exposed photoresist layer is developed. A positive developer can be used as the developer, and a spray development method can be used as the development method.
[0053] Next, the inorganic oxide layer is etched to remove the portion of the inorganic oxide layer from which the photoresist layer has been removed, and the inorganic oxide layer is patterned into a pattern shape corresponding to the inorganic oxide wiring 40. An aqueous solution of oxalic acid can be used as the etching liquid.
[0054] Next, the photoresist layer remaining on the inorganic oxide wiring 40 is stripped off. A silicate solution can be used as the stripping liquid. When the stripping of the photoresist layer is completed, the fourth step is completed, and the scanning antenna A according to the first embodiment is obtained.
[0055] <Second embodiment> In the scanning antenna A according to the first embodiment, an inorganic oxide wiring 40 having a branched tip is used, and the tip is set as a joint position 400, but in the scanning antenna B according to the second embodiment of the present invention, the joint position between the metal wiring 30 and the inorganic oxide wiring 40 is configured to be wide so as to encompass the multiple joint positions 400 of the scanning antenna A, and other points are the same as those of the scanning antenna A. Fig. 2 is an explanatory plan view for explaining the positional relationship between the metal wiring 30 and the inorganic oxide wiring 40.
[0056] As can be seen from Figure 2, in this scanning antenna B, a fan-shaped portion 42 that spreads out like a fan is provided at the tip of the inorganic oxide wiring 40, and the tip portion of the fan-shaped portion 42 is a linear bonding position 400 that is physically and electrically connected to the metal wiring 30.
[0057] The linear bonding positions 400 are aligned along the longitudinal direction of the metal wiring 30, similar to the multiple bonding positions 400 of the scanning antenna A. Therefore, the inorganic oxide wiring 40 extends in a direction perpendicular to the longitudinal direction of the metal wiring 30, in other words, parallel to the lateral direction.
[0058] It is desirable that the linear bonding position 400 includes a position where the stress applied to the metal wiring 30 is minimal when the metal wiring 30 is heated, and the inorganic oxide wiring 40 is least likely to break at the position where the thermal stress is minimal. Therefore, the metal wiring 30 and the inorganic oxide wiring 40 are less likely to break even when heated to high temperatures.
[0059] For this reason, it is desirable to locate the position of the linear joining positions 400 closest to the longitudinal end 300 of the metal wiring 30 at a position 500 μm or more away from the longitudinal end 300 of the metal wiring 30. In the figure, α indicates the distance between the longitudinal end 300 of the metal wiring 30 and the position of the linear joining positions 400 closest to the longitudinal end 300.
[0060] For the same reason, it is desirable that the length β between the position closest to the longitudinal end 300 of the metal wiring 30 and the position farthest from the linear bonding position 400, i.e., the width β of the linear bonding position 400, be 20 μm or more. [Explanation of symbols]
[0061] A, B: Scanning antenna A 10: Base material 20: Adhesive layer 30 Metal wiring 300: End of a side edge extending along the longitudinal direction of the metal wiring 40: Inorganic oxide wiring 400: Joint position 41: Branch 42: Fan-shaped portion 40x: Disconnection position α: Distance between the longitudinal end of the metal wiring and the closest junction position β: Length between the two ends of the joint position
Claims
1. A bonding structure of a metal wiring arranged on an adhesive layer and an inorganic oxide wiring arranged across a part of the metal wiring and a part of the adhesive layer surrounding the metal wiring, The metal wiring has an elongated planar shape having a longitudinal direction and a lateral direction, A joint structure between a metal wiring and an inorganic oxide wiring, characterized in that the metal wiring and the inorganic oxide wiring are joined at a plurality of joining positions, and that these plurality of joining positions are arranged along the longitudinal direction of the metal wiring.
2. A bonding structure of a metal wiring arranged on an adhesive layer and an inorganic oxide wiring arranged across a part of the metal wiring and a part of the adhesive layer surrounding the metal wiring, The metal wiring has an elongated planar shape having a longitudinal direction and a lateral direction, A junction structure between a metal wiring and an inorganic oxide wiring, characterized in that the junction position between the metal wiring and the inorganic oxide wiring is configured to be wide along the longitudinal direction of the metal wiring.
3. 3. The joint structure according to claim 1, wherein a position where a stress acting on the metal wiring when the metal wiring is heated is minimized is included between both ends of the joint position.
4. 3. The junction structure according to claim 1, wherein the junction position is spaced 500 [mu]m or more from an end of the metal wiring in the longitudinal direction.
5. 3. The joint structure according to claim 1, wherein the length between both ends of the joint position is 20 μm or more.
6. 3. The junction structure according to claim 1, wherein the thickness of the metal wiring is 1 to 10 μm, while the thickness of the inorganic oxide wiring is thinner, 10 to 1000 nm.
Citation Information
Patent Citations
Scanning antenna and method for manufacturing scanning antenna
WO2020121876A1