Photocurable composition, cured matter thereof, article manufacturing method, and article
The photocurable composition with refractive index-matched particles and phosphorus compounds addresses flame retardancy and optical properties in stereolithography, ensuring high dimensional accuracy and transparency.
Patent Information
- Application Number
- JP2023053343
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Acrylic and epoxy resins used in stereolithography lack flame retardancy, dimensional accuracy, and optical properties, necessitating improvements to meet industry standards and enhance performance.
A photocurable composition comprising a photocurable liquid and particles with a translucent inorganic substance and a phosphorus compound attached to its surface, ensuring a refractive index difference of 0.20 or less between the particles and the liquid, which suppresses light scattering and enhances flame retardancy through thermal decomposition of the phosphorus compound.
The composition achieves high flame retardancy, optical properties, and dimensional accuracy by minimizing light scattering and forming a char barrier during combustion, while maintaining high transparency and structural integrity.
Smart Images

Figure 2024141603000003 
Figure 2024141603000001 
Figure 2024141603000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a photocurable composition used in producing a three-dimensional article by stereolithography, a cured product thereof, and a stereolithography method using the photocurable composition. [Background technology]
[0002] In recent years, in fields such as medicine, architecture, and manufacturing, three-dimensional modeling processes have been attracting attention for the purpose of obtaining products or parts of desired shapes by layering resin materials, and various methods such as photolithography, powder sintering, and fused deposition modeling have been proposed and put to practical use. Among these, photolithography is a method in which a liquid photocurable resin is cured with a laser beam or lamp to form a three-dimensional shape, and is characterized by its ability to produce highly precise and accurate models. Patent Document 1 discloses a liquid photocurable resin composition for photolithography containing a filler as a material used in photolithography. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Special Publication No. 2019-505628 Summary of the Invention [Problem to be solved by the invention]
[0004] Acrylic resins, epoxy resins, etc. used in stereolithography have poor flame retardancy, so there is a demand for improving the flame retardancy. There is also a demand for ensuring the dimensional accuracy and optical properties of the cured product. An object of the present invention is to provide a photocurable composition for stereolithography that can provide a cured product with excellent flame retardancy, optical properties, and dimensional accuracy. [Means for solving the problem]
[0005] A first aspect of the present invention is a photocurable composition comprising a photocurable liquid and particles dispersed in the photocurable liquid, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, The difference in refractive index between the photocurable liquid and the particles is 0.20 or less. A second aspect of the present invention is a cured product obtained by curing the photocurable composition of the first aspect of the present invention. A third aspect of the present invention is a method for producing an article using a stereolithography method, comprising the steps of: A step of disposing the first photocurable composition of the present invention in a layer form; and a step of irradiating the layered photocurable composition with light energy to cure the composition based on slice data of the model. A fourth aspect of the present invention is an article comprising a solid resin material and particles dispersed in the resin material, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, The difference in refractive index between the resin material and the particles is 0.20 or less. Effect of the Invention
[0006] According to the present disclosure, it is possible to provide a photocurable composition for stereolithography that is advantageous in terms of achieving both flame retardancy, optical properties, and dimensional accuracy. [Brief description of the drawings]
[0007] [Figure 1] FIG. 1 is a diagram illustrating an example of the configuration of a photo-fabrication apparatus. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] In recent years, as the use of resin materials for 3D printers has been expanding, improvements in various physical properties such as mechanical strength, environmental resistance, heat resistance, and flame retardancy are required. In addition, when used in products such as electrical and electronic equipment, office automation equipment, cameras, and computers, high flame retardancy in accordance with IEC standards, ISO standards, and national standards is required. Recently, in flame retardancy of resins, it is expected that the flame retardancy will be improved by adding halogen-free flame retardants or inorganic fillers in order to reduce environmental impact. The photocurable composition of this embodiment is used when manufacturing a three-dimensional article by a photo-molding method, and is characterized in that it contains a photocurable liquid and particles having a second part made of a phosphorus compound attached to the surface of a first part made of a translucent inorganic material, and the difference in refractive index between the particles and the photocurable liquid is 0.20 or less. In the photocurable composition of this embodiment, since the difference in refractive index between the particles and the photocurable liquid is small, light scattering occurring at the interface between the particles and the photocurable liquid during photo-molding is suppressed, and high dimensional accuracy is obtained in the obtained article. In addition, when the article is burned, the phosphorus compound contained in the second part on the particle surface is thermally decomposed to form char, which forms a strong oxygen barrier film together with the first part that does not contribute to the combustion, resulting in high flame retardancy. Furthermore, in the article, light scattering occurring at the interface between the particle and the resin material is suppressed, and the resulting article has excellent optical properties. The photocurable composition of this embodiment will be described in detail below.
[0009] (light curing liquid) The photocurable liquid used in this embodiment is a liquid that is cured by irradiation with light energy. The photocurable liquid preferably contains at least a photocurable resin and a photopolymerization initiator. The photocurable resin is a material that is cured by crosslinking or polymerization by irradiation with light energy, and does not necessarily have to be a polymeric material. Various photocurable materials such as polymerizable vinyl compounds and epoxy compounds can be selected. Specifically, monomers and oligomers of monofunctional compounds and polyfunctional compounds are used. These monofunctional compounds and polyfunctional compounds are not particularly limited. Representative ones are listed below.
[0010] Examples of the monofunctional polymerizable vinyl compounds include isobornyl acrylate, isobornyl methacrylate, dicyclopentenyl acrylate, bornyl acrylate, bornyl methacrylate, 2-hydroxyethyl acrylate, 2-hydroxypropyl acrylate, propylene glycol acrylate, vinylpyrrolidone, acrylamide, vinyl acetate, and styrene. Examples of the polyfunctional compounds include trimethylolpropane triacrylate, EO-modified trimethylolpropane triacrylate, ethylene glycol diacrylate, tetraethylene glycol diacrylate, polyethylene glycol diacrylate, 1,4-butanediol diacrylate, 1,6-hexanediol diacrylate, neopentyl glycol diacrylate, dicyclopentenyl diacrylate, polyester diacrylate, and diallyl phthalate. One or more of these monofunctional compounds and polyfunctional compounds can be used alone or in the form of a mixture.
[0011] Examples of polymerizable epoxy compounds include hydrogenated bisphenol A diglycidyl ether, 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexane carboxylate, 2-(3,4-epoxycyclohexyl-5,5-spiro-3,4-epoxy)cyclohexane-m-dioxane, and bis(3,4-epoxycyclohexylmethyl)adipate.
[0012] (particle) The particles according to this embodiment have a first portion made of a light-transmitting inorganic substance and a second portion made of a phosphorus compound attached to the surface thereof. The difference between the refractive index of the particles and the refractive index of the photocurable liquid is 0.20 or less, preferably 0.10 or less, and more preferably 0.05 or less. Here, the refractive index is the refractive index in visible light. Specifically, the refractive index can be compared at a general d-line (wavelength: 589 nm), but in this embodiment, any of the c-line (wavelength: 656 nm), f-line (wavelength: 486 nm), g-line (wavelength: 436 nm), e-line (wavelength: 405 nm), and i-line (wavelength: 365 nm) may be used.
[0013] The difference between the refractive index of the particles and the refractive index of the photocurable liquid at the exposure wavelength (e.g., ultraviolet light) of the photocurable liquid is also preferably 0.20 or less. Typically, when the difference in Abbe number Vd between the particles and the photocurable liquid in visible light is small, it can be considered that the difference in refractive index between the particles and the photocurable liquid in ultraviolet light is also small. In this embodiment, it is preferable that the difference in Abbe number Vd between the particles and the photocurable liquid is ±10 or less. The Abbe number Vd is expressed by the following formula [1]. Vd = (n d -1) / (n f -n c ) [1] n d : Refractive index at d line n f : Refractive index at f-line n c : Refractive index at c line The particles are preferably contained in the photocurable composition in an amount ranging from 15% by mass to 35% by mass. The particles can function as a filler in the photocurable composition.
[0014] [Part 1] Examples of the first part include translucent inorganic particles such as glass beads, glass powder, glass fiber, ceramic powder, and ceramic fiber, which can be used alone or in combination, and glass beads are preferred. The shape is also not particularly limited, and may be a rod such as a cylindrical or prismatic shape, but a spherical shape is preferred because of its excellent fluidity.
[0015] The first part has a refractive index at the d line (n d ) is preferably 1.40 to 1.90, 1.40 to 1.65, 1.45 to 1.6, particularly preferably 1.5 to 1.55. If the refractive index is within the above range, the difference between the refractive index in the state where the particles have the second portion provided on the surface and the refractive index of many resins such as vinyl resins, epoxy resins, and ABS resins before curing is as small as 0.20 or less, and the particles can be used in stereolithography with high dimensional accuracy.
[0016] The volume average particle size of the first part (D 50 The smaller the particle size of the first portion, the more the scattering components of ultraviolet light due to the refractive index difference can be suppressed. From the viewpoints of keeping the viscosity of the photocurable composition within an appropriate range and preventing air bubbles from being mixed into the obtained cured product, the volume average particle size of the first portion is preferably 0.1 μm or more.
[0017] [Phosphorus Compounds] To attach a phosphorus compound to the surface of the first part as the second part, for example, there is a method of surface treating the first part with a silane coupling agent containing a phosphorus atom, or a method of contacting the first part with a phosphate ester compound to support it. Among them, surface treatment with a silane coupling agent that forms a strong covalent bond with the inorganic surface is preferred.
[0018] The silane coupling treatment includes a wet treatment in which the first part is mixed with a silane coupling agent in a solvent to perform surface treatment, and a dry treatment in which the silane coupling agent diluted with an organic solvent is sprayed onto the first part using a spray or the like to perform surface treatment. The present invention is not limited to either method, but a wet treatment that can adhere more uniformly to the surface of the first part is preferred. The wet treatment is usually performed by mixing the first part with a silane coupling agent in a solvent in which the silane coupling agent can be dissolved, such as water, ethanol, or a mixed solution of water and ethanol. After the surface treatment, solid-liquid separation can be performed using a centrifuge or the like to obtain particles with a phosphorus compound attached to the surface of the first part as a solid content. The obtained particles are preferably washed with an alcohol solvent such as ethanol to remove unreacted materials.
[0019] Regarding the amount of the second portion, in order to obtain sufficient flame retardancy, the amount of phosphorus atoms contained in the second portion is preferably 3.0 mg or more per gram of the inorganic material that becomes the first portion, and in order to reduce the scattered components of ultraviolet light and improve dimensional accuracy, the amount of phosphorus atoms contained in the second portion is preferably 10.0 mg or less per gram of the inorganic material that becomes the first portion. In addition, the second portion is preferably attached to 50% or more of the surface area of the first portion, more preferably 90% or more. In this way, the second portion is easily exposed to the surface of the article, and the effect of improving flame retardancy is enhanced. In addition, the thickness of the second portion is preferably 1 nm or more and 20 nm or less, and may be 10 nm or less. If the thickness of the second portion is this small, the influence of the refractive index of the second portion in the particle is minor, and the refractive index of the particle can be approximated by the refractive index of the first portion. In the silane coupling treatment by wet treatment as described above, the second portion is applied to the surface of the first portion in a liquid containing a component for forming the second portion, so that it is easy to attach the second portion to the entire surface of the first portion. In the silane coupling treatment by wet treatment, even if there is a region on the surface of the first portion where the second portion does not locally adhere, it is considered that the second portion adheres to 90% or more of the surface area of the first portion. In the silane coupling treatment, the second portion having a molecular level size adheres to the first portion via hydroxyl groups or the like on the surface of the first portion. Therefore, the thickness of the second portion formed by the silane coupling treatment can be 20 nm or less.
[0020] Examples of the phosphorus compound include, but are not limited to, diethylphosphate ethyltriethoxysilane (manufactured by Gelest, product name: "SID3412.0"), 2-diphenylphosphinoethyltriethoxysilane (manufactured by Gelest, product name: "SID4558.0"), diphenylphosphinoethyldimethylethoxysilane (manufactured by Gelest, product name: "SID4557.5"), and bis-2-diphenylphosphinoethoxyethyl-methoxysilylethoxyltriethoxysilane (manufactured by Gelest, product name: "SIB1091.0")
[0021] (Photopolymerization initiator) As the photopolymerization initiator, a radical polymerization initiator is preferably used, and can be appropriately selected according to the curing conditions (irradiation wavelength, irradiation amount) of the photocurable resin. As the polymerization initiator that generates radical species by light irradiation, 2,4,6-trimethylbenzoyl-diphenylphosphine oxide, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-1-butanone, 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-2-methyl-1-phenyl-propan-1-one, bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide, 4-phenylbenzophenone, 4-phenoxybenzophenone, 4,4'-diphenylbenzophenone, 4,4'-diphenoxybenzophenone, etc. can be mentioned, but are not limited thereto.
[0022] It is also possible to use in combination a polymerization initiator that generates radical species by heat. Examples of such polymerization initiators include azo compounds such as azobisisobutylnitrile (AIBN), and peroxides such as benzoyl peroxide, tert-butyl peroxypivalate, tert-butyl peroxyneohexanoate, tert-hexyl peroxyneohexanoate, tert-butyl peroxyneodecanoate, tert-hexyl peroxyneodecanoate, cumyl peroxyneohexanoate, and cumyl peroxyneodecanoate, but are not limited to these.
[0023] The photopolymerization initiator may be used alone or in combination of two or more. The amount of the radical polymerization initiator added is preferably in the range of 0.01 to 10.00 parts by mass relative to 100 parts by mass of the photocurable resin. The ratio of the photopolymerization initiator added may be appropriately selected depending on the amount of light irradiation and further the additional heating temperature. It may also be adjusted depending on the target average molecular weight of the resulting polymer (cured product of the photocurable resin).
[0024] (Other additives) To the photocurable composition of this embodiment, a polymerization inhibitor, a photosensitizer, a light resistance stabilizer, a heat resistance stabilizer, an antioxidant, a chain transfer agent, a curing aid, and the like can be added within a range that does not significantly deteriorate the performance of the cured product.
[0025] Examples of the polymerization inhibitor include hydroquinone-based polymerization inhibitors such as hydroquinone, hydroquinone monomethyl ether, hydroquinone monoethyl ether, hydroquinone monopropyl ether, hydroquinone monobutyl ether, hydroquinone monopentyl ether, hydroquinone monohexyl ether, hydroquinone monooctyl ether, and hydroquinone monoheptyl ether, and phenol-based polymerization inhibitors having a substituent such as 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate. However, hydroquinone-based polymerization inhibitors such as hydroquinone and benzoquinone-based polymerization inhibitors such as benzoquinone may turn yellow when exposed to ultraviolet light, and are therefore suitable for obtaining thin-film cured products such as coatings. Examples of the polymerization inhibitor include, but are not limited to, those mentioned above as polymerization inhibitors during reaction and storage. The amount of addition is preferably in the range of 0.01 parts by mass or more and 1.00 parts by mass or less relative to 100 parts by mass of the photocurable composition. In addition, only one polymerization inhibitor may be used, or two or more polymerization inhibitors may be used in combination. In consideration of the reduction in coloration, it is preferable to use a hydroquinone-based polymerization inhibitor in combination.
[0026] Examples of the photosensitizer include benzophenone, 4,4-diethylaminobenzophenone, 1-hydroxycyclohexyl phenyl ketone, isoamyl p-dimethylaminobenzoate, methyl 4-dimethylaminobenzoate, benzoin, benzoin ethyl ether, benzoin isobutyl ether, benzoin isopropyl ether, 2,2-diethoxyacetophenone, methyl o-benzoylbenzoate, 2-hydroxy-2-methyl-1-phenylpropan-1-one, acylphosphine oxide, etc. The amount of addition is preferably in the range of 0.01 parts by mass to 10.00 parts by mass relative to 100 parts by mass of the photocurable composition.
[0027] There are no particular limitations on the light resistance stabilizer as long as it does not significantly affect the properties of the cured product, and examples thereof include 2-(2H-benzotriazol-2-yl)-p-cresol, 2-(2H-benzotriazol-2-yl)-4,6-bis(1-methyl-1-phenylethyl)phenol, 2-[5-chloro(2H)-benzotriazol-2-yl]-4-methyl-6-(tert-butyl)phenol, 2-(2H-benzotriazol-2-yl)-4,6-di-tert-pentylphenol, 2-(2H-benzotriazol-2-yl)-4-(1,1,3,3-tetramethylbutyric acid), and the like. Examples of the photosensitizer include benzotriazole-based compounds such as 2,2'-methylenebis[6-(2H-benzotriazol-2-yl)]-4-(1,1,3,3-tetramethylbutyl)phenol, 2-(2H-benzotriazol-2-yl)-6-dodecyl-4-methylphenol, cyanoacrylate-based compounds such as ethyl 2-cyano-3,3-diphenylacrylate and 2-ethylhexyl 2-cyano-3,3-diphenylacrylate, triazine-based compounds, and benzophenone-based compounds such as octabenzone and 2,2'-4,4'-tetrahydrobenzophenone. The light resistance stabilizer may also function as a photosensitizer, in which case the photosensitizer need not be added. The amount of the photosensitizer added is preferably in the range of 0.01 parts by mass to 10.00 parts by mass relative to 100 parts by mass of the photocurable composition.
[0028] There are no particular limitations on the heat stabilizer as long as it does not significantly affect the properties of the cured product, and examples thereof include pentaerythritol tetrakis[3-(3,5-di-tert-butyl-4-hydroxyphenyl)]propionate, octadecyl-3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, alkyl esters of 3,5-bis(1,1-dimethylethyl)-4-hydroxybenzenepropanoic acid having a side chain and a carbon number of 7 to 9, and 4,6-bis(octylthiomethyl)-o-cresol. Examples of the compound include hindered phenol compounds such as 4,6-bis(dodecylthiomethyl)-o-cresol, ethylene bis(oxyethylene) bis[3-(5-tert-butyl-4-hydroxy-m-tolyl)]propionate and hexamethylene bis[3-(3,5-di-tert-butyl-4-hydroxyphenyl)]propionate, phosphorus compounds such as tris(2,4-di-tert-butylphenyl)phosphite, and sulfur compounds such as dioctadecyl-3,3'-thiodipropionate. The amount of the compound added is preferably in the range of 0.01 parts by mass to 10.00 parts by mass relative to 100 parts by mass of the photocurable composition.
[0029] The antioxidant is not particularly limited as long as it does not significantly affect the properties of the cured product, and examples thereof include hindered amine compounds such as bis(2,2,6,6-tetramethyl-4-piperidyl)sebacate and bis(1,2,2,6,6-pentamethyl-4-piperidyl)[[3,5-bis(1,1-dimethylethyl)-4-hydroxyphenyl]methyl]butylmalonate. The amount added is preferably in the range of 0.01 parts by mass to 10.00 parts by mass relative to 100 parts by mass of the photocurable composition.
[0030] Examples of chain transfer agents and curing assistants include β-mercaptopropionic acid, 2-ethylhexyl-3-mercaptopropionate, n-octyl-3-mercaptopropionate, methoxybutyl-3-mercaptopropionate, stearyl-3-mercaptopropionate, 1-butanethiol, cyclohexanethiol, cyclohexyl 3-mercaptopropionate, 1-decanethiol, 2,4-diphenyl-4 methyl-1-pentene, 1-dodecanethiol, 3-mercaptopropionate, dodecyl mercaptoacetate, 2-ethylhexyl mercaptoacetate, 2-ethylhexyl 3-mercaptopropionate, ethyl mercaptoacetate, 1-hexadecanethiol, hexyl 3-mercaptopropionate, 2-mercaptoethanol, 3-mercapto-1,2-propanediol, mercaptoacetic acid, sodium 2-mercaptoethanesulfonate, 3-mercaptopropionic acid, methyl mercaptoate, mercaptosuccinic acid, methyl 3-mercaptopropionate, octyl 3-mercaptopropionate Tadecyl, octyl 3-mercaptopropionate, 1-octanethiol, 1-octadecanethiol, tridecyl 3-mercaptopropionate, thiophenol, polyfunctional thiols such as bis(2-mercaptoethyl)sulfide, 3,6-dioxa-1,8-octanedithiol, trimethylolpropane tris(3-mercaptopropionate), 1,4-butanediol bis(thioglycolate), pentaerythritol tetra(3-mercaptopropionate), 1,4-benzene Thiol, 3,7-dithia-1,9-nonanol, DL-1,4-dimercapto-2,3-butanediol, 1,5-dimercaptonaphthalene, dithioerythritol, ethylene bisthioglycolate, pentaerythritol tetrakismercaptoacetate, tris-[(3-mercaptopropionyloxyethyl)-isocyanurate, tetraethylene glycol bis(3-mercaptopropionate), dipentaerythritol hexakis(3-mercaptopropionate), 3,Examples of commercially available products include 3'-thiodipropionic acid, dithiodipropionic acid, laurylthiopropionic acid (dodecylthiopropionic acid), and TS-G, C3TS-G, TA-G, and LDAIC (manufactured by Shikoku Chemical Industry Co., Ltd.), Karenz MTPE1, BD1, NR1, and TPMB (manufactured by Showa Denko K.K.).
[0031] (Method for producing photocurable composition) The method for producing the photocurable composition of this embodiment is not particularly limited, but examples thereof include a method for mixing the components to be used with a three-roll mill, a kneader, a planetary mixer, a ball mill, etc. Among these, a planetary mixer is preferred because it causes relatively little contamination during preparation.
[0032] (Production method of the article) In the method for manufacturing a three-dimensional object by a stereolithography method using the photocurable composition of the present embodiment, a conventionally known stereolithography method and device can be used. Specifically, the method is a method of laminating a plurality of cured layers obtained by photocuring the photocurable composition of the present embodiment to a predetermined thickness. That is, the method is a method of repeating a step of arranging the photocurable composition in layers and a step of irradiating the layered photocurable composition with light energy to cure it based on slice data generated based on three-dimensional shape data of the target object. If necessary, a step of subjecting the obtained object to heat treatment may be performed.
[0033] There are two main types of stereolithography: the free surface method and the controlled surface method. Fig. 1 shows an example of the configuration of a modeling apparatus 100 using the free liquid surface method. The modeling apparatus 100 has a tank 11 that contains a liquid photocurable composition 10. Inside the tank 11, a modeling stage 12 is provided so as to be drivable in the vertical direction by a drive shaft 13. An active energy beam 15 emitted from a light source 14 to cure the photocurable composition 10 has its irradiation position changed by a galvanometer mirror 16 controlled by a control unit 18 according to slice data, and scans the surface of the tank 11. In Fig. 1, the scanning range is indicated by a thick dashed line.
[0034] The thickness d of the photocurable composition 10 cured by the active energy beam 15 is a value determined based on the settings at the time of generating the slice data, and affects the accuracy of the obtained article (reproducibility of the three-dimensional shape data of the article to be molded). The thickness d is achieved by the control unit 18 controlling the drive amount of the drive shaft 13.
[0035] First, the control unit 18 controls the drive shaft 13 based on the settings, and the photocurable composition is supplied to the stage 12 at a thickness d. The photocurable composition on the stage 12 is selectively irradiated with active energy rays 15 based on slice data so as to obtain a cured layer having a desired pattern, and a cured layer is formed. Next, the stage 12 is moved in the direction of the white arrow, and uncured photocurable composition is supplied to the surface of the cured layer at a thickness d. Then, active energy rays 15 are irradiated based on the slice data, and a cured product integrated with the previously formed cured layer is formed. By repeating this layer-by-layer curing process, the desired three-dimensional object (article) 17 can be obtained.
[0036] When the surface of the photocurable composition is irradiated with active energy rays 15 to form a cured layer having a predetermined pattern, the resin can be cured by a pointillist method or a line drawing method using light energy focused in a dotted or line shape. Alternatively, the resin may be cured by irradiating the active energy rays in a planar manner through a planar drawing mask formed by arranging a plurality of microscopic light shutters such as liquid crystal shutters or digital micromirror shutters.
[0037] Examples of the active energy ray 15 include ultraviolet rays, electron beams, X-rays, radiation, and high frequency waves. Among them, ultraviolet rays having a wavelength of 300 nm to 430 nm are preferably used from an economical viewpoint, and as a light source in this case, an ultraviolet laser (e.g., a semiconductor pumped solid-state laser, an Ar laser, a He-Cd laser, etc.), a high-pressure mercury lamp, an ultra-high-pressure mercury lamp, a mercury lamp, a xenon lamp, a halogen lamp, a metal halide lamp, an ultraviolet LED (light-emitting diode), a fluorescent lamp, etc. Among them, an ultraviolet laser is preferably used because it has excellent light-collecting properties, can increase the energy level to shorten the modeling time, and can obtain high modeling accuracy.
[0038] Like the free liquid level method, modeling by the regulated liquid level method is also preferred. A modeling apparatus using the regulated liquid level method is configured such that the stage 12 of the modeling apparatus 100 in FIG. 1 is provided so as to raise the model 17 above the liquid level, and the light irradiation means is provided below the tank 11. A typical modeling example by the regulated liquid level method is as follows. First, the support surface of the stage, which is provided so as to be freely raised and lowered, and the bottom surface of the tank containing the photocurable composition are set at a predetermined distance, and the photocurable composition is supplied between the support surface of the stage and the bottom surface of the tank. Next, light is selectively irradiated from the bottom surface side of the tank containing the photocurable composition by a laser light source or a projector according to slice data to the photocurable composition between the stage support surface and the bottom surface of the tank. The photocurable composition between the stage support surface and the bottom surface of the tank is cured by the irradiation of light, and a solid cured layer is formed. After that, the stage is raised, and the cured layer is peeled off from the bottom surface of the tank.
[0039] Next, the height of the stage is adjusted so that the distance between the hardened layer formed under the support surface of the stage and the bottom surface of the tank is a predetermined distance. Then, as before, a photocurable composition is supplied between the bottom surface of the tank and the hardened layer, and a new hardened layer is formed between the hardened layer and the bottom surface of the tank by irradiating light according to the slice data. By repeating this process multiple times, a model 17 consisting of multiple hardened layers stacked together can be obtained. The shaped object 17 thus obtained is removed from the tank 11, and any unreacted photocurable composition remaining on its surface is removed. After that, the desired article can be obtained by carrying out post-processing as necessary.
[0040] (How to clean the model) As a cleaning agent used for cleaning the shaped object, an alcohol-based organic solvent such as isopropyl alcohol, ethyl alcohol, etc. may be used. In addition, a ketone-based organic solvent such as acetone, ethyl acetate, methyl ethyl ketone, etc., or an aliphatic organic solvent such as terpenes may be used.
[0041] (Post-processing of the model) After cleaning the molded object, a post-cure may be performed by light irradiation, heat irradiation, or both, as necessary. The post-cure can cure any unreacted photocurable composition that may remain on the surface and inside of the molded object, and can suppress stickiness of the surface of the molded object and can improve the initial strength of the molded object. In addition, post-processing such as cutting and polishing may be carried out as appropriate.
[0042] The article obtained by using the photocurable composition of this embodiment has a solid resin material and particles dispersed in the resin material, and the particles have a first part made of a light-transmitting inorganic material and a second part made of a phosphorus compound attached to the first part. The difference in refractive index between the resin material and the particles is preferably 0.20 or less, and the article is highly transparent. The refractive index is the refractive index in visible light, as in the refractive index described in the above description of the particles, and may be any of d-line, c-line, f-line, g-line, e-line, and i-line.
[0043] [Included configuration] The disclosure of this embodiment includes the following configuration. (Configuration 1) A photocurable composition comprising a photocurable liquid and particles dispersed in the photocurable liquid, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, A photocurable composition, wherein the difference in refractive index between the photocurable liquid and the particles is 0.20 or less. (Configuration 2) 2. The photocurable composition according to claim 1, wherein the amount of phosphorus atoms contained in the second portion is 3.0 mg or more and 10.0 mg or less per gram of the inorganic material constituting the first portion. (Configuration 3) 3. The photocurable composition according to claim 1 or 2, wherein the content of the particles is from 15% by mass to 35% by mass. (Configuration 4) 4. The photocurable composition according to any one of claims 1 to 3, wherein the first portion has a volume average particle size of 0.1 μm or more and 20 μm or less. (Configuration 5) 5. The photocurable composition according to any one of claims 1 to 4, wherein the second portion has a thickness of 1 nm or more and 20 nm or less.
[0044] (Configuration 6) A photocurable composition according to any one of claims 1 to 5, wherein in one of the particles, the second portion is attached to 50% or more of the surface area of the first portion. (Configuration 7) 7. The photocurable composition according to any one of claims 1 to 6, wherein the first portion is a glass particle. (Configuration 8) 8. The photocurable composition according to any one of claims 1 to 7, wherein the phosphorus compound is a silane coupling agent containing a phosphorus atom. (Configuration 9) The photocurable composition according to configuration 8, wherein the phosphorus compound is a silane coupling agent having a phosphate ester structure. (Configuration 10) 10. The photocurable composition according to any one of configurations 1 to 9, wherein the photocurable liquid contains a photocurable resin and a photopolymerization initiator.
[0045] (Configuration 11) 11. The photocurable composition according to claim 10, wherein the photocurable resin is a polymerizable vinyl compound or an epoxy compound. (Configuration 12) 12. The photocurable composition according to claim 10 or 11, wherein the photopolymerization initiator is a radical polymerization initiator. (Configuration 13) 13. The photocurable composition according to any one of configurations 1 to 12, wherein the difference in refractive index between the photocurable liquid and the particles is 0.10 or less. (Configuration 14) 13. The photocurable composition according to any one of configurations 1 to 12, wherein the difference in refractive index between the photocurable liquid and the particles is 0.05 or less. (Configuration 15) 15. The photocurable composition according to claim 1, wherein the refractive index is a refractive index for visible light. (Configuration 16) 16. A cured product obtained by curing the photocurable composition according to claim 1.
[0046] (Configuration 17) A method for manufacturing an article using a stereolithography method, comprising the steps of: A step of disposing the photocurable composition according to any one of configurations 1 to 15 in a layer form; and curing the layered photocurable composition by irradiating the layered photocurable composition with light energy based on slice data of a model. (Configuration 18) 18. The method for producing an article according to claim 17, further comprising a step of subjecting the photocurable composition to a heat treatment after the step of irradiating the composition with light energy. (Configuration 19) 18. The method for manufacturing an article according to claim 17, wherein the light energy is light emitted from a laser light source or a projector. (Configuration 20) An article comprising a solid resin material and particles dispersed in the resin material, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, An article, characterized in that the difference in refractive index between the resin material and the particles is 0.20 or less. EXAMPLES
[0047] The present embodiment will be described in detail below with reference to examples, but the present embodiment is not limited to these examples. (material) The materials used in the examples and comparative examples are listed below. A-1: Methyl 2-(allyloxymethyl)acrylate; trade name "FX-AO-MA" (manufactured by Nippon Shokubai Co., Ltd.) A-2: Urethane acrylate; product name "KAYARAD UX-6101" (manufactured by Nippon Kayaku Co., Ltd.) A-3: Tris-(2-acryloxyethyl)isocyanurate; product name "A-9300S" (manufactured by Shin-Nakamura Chemical Co., Ltd.) B-1: Glass filler; product name "CF0018" (d n =1.52,D 50 = 2.0μm, Takara Standard Co., Ltd.) B-2: Glass filler; product name "CF0018" (D 50 = 20.0μm, Takara Standard Co., Ltd.) B-3: Alumina filler; product name "AA-2" (D 50 =2.0μm, manufactured by Sumitomo Chemical Co., Ltd.) C-1: Diethyl phosphate ethyl triethoxysilane; Trade name: "SID3412.0" (manufactured by Gelest) E-1: Bis(2,4,6-trimethylbenzoyl)phenyl phosphate oxide; Trade name: Omnirad 819 (manufactured by IGM Resins)
[0048] (Surface treatment of the first part) 2.5 parts by mass of diethyl phosphate ethyl triethoxysilane (C-1) was dissolved in pure water and stirred at room temperature for 10 minutes. 50 parts by mass of glass filler (B-1) was added thereto and further stirred at room temperature for 30 minutes. The dispersion liquid was transferred to a centrifuge tube and centrifuged at 3000 rpm for 5 minutes using a centrifuge (manufactured by Kubota Manufacturing Co., Ltd., product name "7780"), and the supernatant liquid was removed. Pure water was added to the centrifuge tube containing the precipitate, and the precipitate was washed by shaking well by hand. Centrifugation was again performed at 3000 rpm for 5 minutes using a centrifuge, and the supernatant liquid was removed to obtain a precipitate. The precipitate was dried at 110 ° C for 3 hours to obtain particles (D-1). Using the same method as above, particles (D-2) to (D-7) were prepared according to the conditions in Table 1.
[0049] (Evaluation of surface treatment) The particles prepared by the above method were subjected to thermogravimetric analysis, and the mass loss at the end of heating was taken as the amount of phosphorus compound constituting the second portion, and the amount of phosphorus atoms was calculated from the amount of phosphorus compound to evaluate. Specifically, the mass loss was determined by using a thermogravimetric analyzer (manufactured by METTLER TOLEDO, product name "TGA / DSC3+") to heat the particles in an air atmosphere at a heating rate of 10°C / min up to 600°C, and heating at 600°C for 30 minutes, from the masses before and after heating.
[0050] (Refractive index evaluation) The particles prepared by the above method were dispersed in Cargill standard refractive index liquid (manufactured by Takara Standard Co., Ltd., Standard Series, product name "Series E"), and the dispersion was dropped onto a smooth film-forming plate to produce a cast film. The refractive index (n d ) was measured.
[0051] [Table 1]
[0052] (Photocurable liquid preparation) 30 parts by mass of methyl 2-(allyloxymethyl)acrylate (A-1), 30 parts by mass of urethane acrylate (A-2), and 40 parts by mass of tris-(2-acryloxyethyl)isocyanurate (A-3) were weighed out and mixed at 60 rpm and 50°C for 12 hours in a mix rotor (manufactured by AS ONE Corporation, product name "VMRC-5") to obtain a photocurable liquid (A-4). The photocurable liquid (A-4) was dropped onto a prism, and the refractive index (n d ) was measured and found to be 1.55. It was also confirmed that the change in refractive index due to photocuring of the photocurable liquid (A-4) was sufficiently small.
[0053] Example 1 72 parts by mass of the photocurable liquid (A-4), 26 parts by mass of the particles (D-1), and 2 parts by mass of bis(2,4,6-trimethylbenzoyl)phenyl phosphate oxide (E-1) were weighed out and mixed at 2000 rpm for 5 minutes in a centrifugal vacuum mixer (manufactured by Thinky Corporation, product name "Awatori Rentaro ARV-310") to obtain a photocurable composition.
[0054] The obtained photocurable composition was used to produce a three-dimensional object by the following method. A 3D printer (manufactured by FlashForge, product name "Foto8.9") was used, and the exposure wavelength was set to 305 nm, the layer thickness per layer was set to 100 μm, and the irradiation time per layer was set to 10 seconds, and multiple layers were formed to produce cured products with thicknesses of 4 mm and 5 mm. The cured product was washed with ethanol and thoroughly dried at room temperature, and then a secondary ultraviolet curing process was performed for 1 hour using a secondary curing device (manufactured by Formlabs, product name "Formcure"). Furthermore, the product was placed in a heating oven at 100 ° C. and heat-treated for 1 hour to obtain an article for a test piece.
[0055] [Evaluation of flame retardancy] The test specimens (length 125 mm, width 13 mm, thickness 4 mm or 5 mm) were used to conduct the UL94-20mm vertical flammability test, and the test specimens were rated as V-0, V-1, or V-2 based on the after-flame or after-glow time of the specimens after exposure to flame, and the presence or absence of burning or falling objects. A: Test piece thickness 4mm, V-1 or V-0 B: Test piece thickness 4mm, V-2 C: Test piece thickness 5mm, V-2 D: Combustion
[0056] [Evaluation of dimensional accuracy] The dimensions of a 4 mm thick test piece prepared based on the 3D data (length 80 mm, width 10 mm, thickness 4 mm) were measured with a vernier caliper, and the difference between the test piece dimensions and the 3D data was evaluated. A: The difference between the measured dimensions of the cured product and the 3D data is less than ±1.0% B: The difference between the measured dimensions of the cured product and the 3D data is less than ±2.0% C: The difference between the measured dimensions of the cured product and the 3D data is less than ±3.0% D: The difference between the measured dimensions of the cured product and the 3D data is ±3.0% or more.
[0057] (comprehensive evaluation) A comprehensive evaluation was carried out based on the results of the flame retardancy evaluation and the dimensional accuracy evaluation. A (Pass): Both flame retardancy and dimensional accuracy are A B (Pass): The lower of the flame retardancy rating and dimensional accuracy rating is B. C (Pass): The lower of the flame retardancy rating and the dimensional accuracy rating is C. D (Fail): The lower of the flame retardancy rating and the dimensional accuracy rating is D.
[0058] (Examples 2 to 12, Comparative Examples 1 and 2) Using the particles shown in Table 1 and the material composition ratio shown in Table 2, test pieces were prepared and evaluated in the same manner as in Example 1. In Comparative Example 2, a glass filler (B-1) that does not adhere to the second portion was used instead of the particles.
[0059] [Table 2]
[0060] From Table 2, for Examples 1 to 12 containing particles (D-1) to (D-6), articles with high flame retardancy, excellent impact resistance, and heat resistance were obtained, and the appearance was also good. On the other hand, for Comparative Example 1 containing particles (D-7) whose first portion is an alumina filler, the refractive index of the particles was 1.77, and the refractive index difference with the photocurable liquid (A-4) was large at 0.22, so that the scattering component of ultraviolet light during molding was large, and the dimensional accuracy was low. In addition, for Comparative Example 2 which does not have a second portion and contains glass filler (B-1) in the first portion, since no phosphorus compound is present on the surface of the first portion, char and oxygen barrier film cannot be formed during combustion, and the flame retardancy was low.
Claims
1. A photocurable composition comprising a photocurable liquid and particles dispersed in the photocurable liquid, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, A photocurable composition, wherein the difference in refractive index between the photocurable liquid and the particles is 0.20 or less.
2. 2. The photocurable composition according to claim 1, wherein the amount of phosphorus atoms contained in the second portion is 3.0 mg or more and 10.0 mg or less per gram of the inorganic substance constituting the first portion.
3. 2. The photocurable composition according to claim 1, wherein the content of the particles is from 15% by mass to 35% by mass.
4. 2. The photocurable composition according to claim 1, wherein the first portion has a volume average particle size of 0.1 μm or more and 20 μm or less.
5. 2. The photocurable composition according to claim 1, wherein the second portion has a thickness of 1 nm or more and 20 nm or less.
6. 2. The photocurable composition of claim 1, wherein in one of said particles, said second portion is attached to at least 50% of the surface area of said first portion.
7. 2. The photocurable composition of claim 1, wherein the first portion is a glass particle.
8. 2. The photocurable composition according to claim 1, wherein the phosphorus compound is a silane coupling agent containing a phosphorus atom.
9. 9. The photocurable composition according to claim 8, wherein the phosphorus compound is a silane coupling agent having a phosphate structure.
10. 2. The photocurable composition according to claim 1, wherein the photocurable liquid contains a photocurable resin and a photopolymerization initiator.
11. 11. The photocurable composition according to claim 10, wherein the photocurable resin is a polymerizable vinyl compound or an epoxy compound.
12. The photocurable composition according to claim 10, wherein the photopolymerization initiator is a radical polymerization initiator.
13. 2. The photocurable composition according to claim 1, wherein the difference in refractive index between the photocurable liquid and the particles is 0.10 or less.
14. 2. The photocurable composition according to claim 1, wherein the difference in refractive index between the photocurable liquid and the particles is 0.05 or less.
15. 2. The photocurable composition according to claim 1, wherein the refractive index is a refractive index for visible light.
16. A cured product obtained by curing the photocurable composition according to claim 1 .
17. A method for manufacturing an article using a stereolithography method, comprising the steps of: disposing the photocurable composition according to any one of claims 1 to 15 in a layer; and curing the layered photocurable composition by irradiating the layered photocurable composition with light energy based on slice data of a model.
18. The method for producing an article according to claim 17, further comprising the step of subjecting the photocurable composition to a heat treatment after the step of irradiating the composition with light energy.
19. The method for manufacturing an article according to claim 17, wherein the light energy is light emitted from a laser light source or a projector.
20. An article comprising a solid resin material and particles dispersed in the resin material, the particle has a first portion made of a light-transmitting inorganic material and a second portion made of a phosphorus compound attached to the first portion, An article, characterized in that the difference in refractive index between the resin material and the particles is 0.20 or less.
Citation Information
Patent Citations
Photocurable resin composition for stereolithography, three-dimensional article produced using said composition, and related manufacturing method
JP2019505628A