Battery including fixing member

JP2024144595AActive Publication Date: 2024-10-11PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024119297
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-10-11
Estimated Expiration
2041-06-09

AI Technical Summary

Technical Problem

Batteries are susceptible to damage from external forces, particularly affecting the electrode tab groups due to their soft nature and susceptibility to vibrations and shocks, leading to unstable electrical connections and potential connection failures.

Method used

A battery design that includes a fixing member to secure the electrode tab groups to rigid electrode current collectors, preventing movement and reducing load on the tab groups, thereby minimizing damage.

Benefits of technology

The design effectively prevents damage to the electrode tab groups by stabilizing their position within the battery case, ensuring reliable electrical connections and enhancing the battery's durability against external forces.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144595000001_ABST
    Figure 2024144595000001_ABST
Patent Text Reader

Abstract

To provide a battery that suitably prevents damage to a group of electrode tabs.SOLUTION: A battery 100 includes electrode bodies 20a (first electrode body), 20b, 20c (second electrode body) of flat hexahedron shape and a battery case 10 for accommodating them, the electrode bodies 20a, 20b, 20c, including a positive electrode 22 and a negative electrode 24 and having a pair of rectangular flat outer surfaces 27. Here, from at least one of the pairs of flat outer surfaces 27 of the electrode bodies 20a, 20c to a positive electrode collector part 50 or a negative electrode collector part 60, a fixing member 1 is arranged.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a battery provided with a fixing member. [Background technology]

[0002] A battery such as a lithium ion secondary battery generally includes a flat hexahedral electrode body having a positive electrode and a negative electrode (hereinafter, simply referred to as "electrodes"); an exterior body having an opening and housing the electrode body; a sealing plate sealing the opening of the exterior body; and a terminal electrically connected to the electrode inside the exterior body and extending from the sealing plate to the outside of the exterior body. This type of battery typically includes an electrode tab group including a plurality of tabs for collecting current on the electrode, and the electrode tab group is connected to the terminal via an electrode current collector. For example, the following Patent Document 1 discloses a battery in which a positive electrode tab group is provided at one end of the electrode body in the longitudinal direction and a negative electrode tab group is provided at the other end. A technology is also disclosed in which the electrode tab group is connected to the electrode current collector in a folded state. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-50069 A Summary of the Invention [Problem to be solved by the invention]

[0004] Incidentally, when the battery is in use, vibrations, impacts, and the like may be applied to the battery from the outside. The tabs are, for example, made of a part of the current collector, and are soft and easily affected by external forces. For this reason, if the electrode body is displaced from a predetermined arrangement position by an external force (specifically, an external force applied in the longitudinal direction of the electrode body) and a load is applied to the electrode tab group, the electrode tab group may be damaged. As a result, the electrical connection between the electrode and the terminal may become unstable or may become defective, which is undesirable. In addition, according to the study by the present inventors, it was found that, particularly when the electrode tab group is connected to the electrode current collector in a folded state, the electrode tab group is easily damaged due to the concentration of external forces at the folded portion.

[0005] The present invention has been made in view of the above circumstances, and a main object of the present invention is to provide a battery in which damage to the electrode tab group is suitably prevented. [Means for solving the problem]

[0006] The present invention provides a battery including a first electrode body having a flat hexahedral shape including a positive electrode and a negative electrode and a pair of rectangular flat outer surfaces, and a battery case that houses the first electrode body. The battery case includes an exterior body having a bottom wall, a pair of first side walls extending from the bottom wall and facing each other, a pair of second side walls extending from the bottom wall and facing each other, and an opening facing the bottom wall, and a sealing plate that seals the opening. A positive electrode terminal and a negative electrode terminal are attached to the sealing plate, a positive electrode tab group including a plurality of positive electrode tabs is arranged on one of the pair of second side walls, and a negative electrode tab group including a plurality of negative electrode tabs is arranged on the other of the pair of second side walls. The positive electrode tab group and the positive electrode terminal are electrically connected via a positive electrode current collector, the positive electrode tab group is joined to the positive electrode current collector in a state where it is curved so as to extend along the second side wall, and the negative electrode tab group and the negative electrode terminal are electrically connected via a negative electrode current collector, and the negative electrode tab group is joined to the negative electrode current collector in a state where it is curved so as to extend along the second side wall. Here, a fixing member is arranged from at least one of the pair of flat outer surfaces to the positive electrode current collector or the negative electrode current collector.

[0007] By disposing the fixing member as described above, the electrode body is fixed to the rigid electrode current collecting portion fixed to the sealing plate, and thus movement of the electrode body in the longitudinal direction inside the battery case can be suitably suppressed, thereby suppressing the load on the electrode tab group and suitably preventing damage to the electrode tab group.

[0008] In one aspect of the battery disclosed herein, the positive electrode tab group is joined to a surface of the positive electrode current collector facing the first electrode body, and the negative electrode tab group is joined to a surface of the negative electrode current collector facing the first electrode body.

[0009] In one aspect of the battery disclosed herein, the positive electrode tab group is joined to the positive electrode current collector while being collected on one of the pair of flat outer surfaces, and the negative electrode tab group is joined to the negative electrode current collector while being collected on one of the pair of flat outer surfaces.

[0010] In a preferred embodiment of the battery disclosed herein, the fixing member does not cover either the joint between the positive electrode tab group and the positive electrode current collector or the joint between the negative electrode tab group and the negative electrode current collector. This configuration is preferable because it can reliably prevent the electrode tab group from being damaged by a load applied thereto due to interference between the fixing member and the electrode tab group.

[0011] In one embodiment of the battery disclosed herein, the positive electrode tab is made of aluminum or aluminum alloy foil, and the negative electrode tab is made of copper or copper alloy foil, and the fixing member is disposed from at least one of the pair of flat outer surfaces to the negative electrode current collector, but is not disposed from either of the pair of flat outer surfaces to the positive electrode current collector.

[0012] In a preferred embodiment of the battery disclosed herein, the positive electrode current collector includes a positive electrode first current collector arranged between the sealing plate and the first electrode body, and a positive electrode second current collector to which the positive electrode tab group is joined, and the negative electrode current collector includes a negative electrode first current collector arranged between the sealing plate and the first electrode body, and a negative electrode second current collector to which the negative electrode tab group is joined. Here, the fixing member covers at least the joint between the positive electrode first current collector and the positive electrode second current collector, or the joint between the negative electrode first current collector and the negative electrode second current collector. In this way, the electrode body is fixed to a position close to the sealing plate in the electrode current collector, so that the movement of the electrode body in the longitudinal direction within the battery case can be more suitably suppressed.

[0013] In one embodiment of the battery disclosed herein, the pair of flat outer surfaces are made of separators, and a layer containing polyvinylidene fluoride is formed on the outermost surface of the separator.

[0014] In one embodiment of the battery disclosed herein, a second electrode body having the same configuration as the first electrode body is further disposed within the battery case.

[0015] In one aspect of the battery of this aspect, one or more electrode bodies having the same configuration as the first electrode body are further disposed between the first electrode body and the second electrode body.

[0016] In a preferred embodiment of the battery of this aspect, the first electrode body, an electrode body disposed between the first electrode body and the second electrode body, and the second electrode body are fixed together. With this configuration, movement of the electrode body disposed between the first electrode body and the second electrode body in the longitudinal direction can be suitably suppressed.

[0017] In a preferred embodiment of the battery of this aspect, the fixing member of the first electrode body and the fixing member of the second electrode body are not disposed between the first electrode body, the electrode body disposed between the first electrode body and the second electrode body, and the second electrode body. With this configuration, the integrated thickness of the electrode body group can be reduced, so that the pressure distribution of each electrode body can be mitigated. This makes it possible to suitably suppress uneven reactions in each electrode body.

[0018] In a preferred embodiment of the battery of this aspect, an auxiliary fixing member is further arranged from one of the pair of flat outer surfaces of the first electrode body that faces the first side wall to one of the pair of flat outer surfaces of the second electrode body that faces the first side wall. Here, the auxiliary fixing member is arranged on the first electrode body, an electrode body arranged between the first electrode body and the second electrode body, and a portion other than the positive electrode current collector and the negative electrode current collector of the second electrode body. With this configuration, it is possible to suitably suppress movement of the electrode body arranged between the first electrode body and the second electrode body in the longitudinal direction.

[0019] In a preferred embodiment of the battery of this aspect, an insulating member is disposed in the battery case between a first side wall of the pair of first side walls that faces the flat outer surface of the first electrode body and the flat outer surface of the first electrode body, and between the other first side wall of the pair of first side walls and the flat outer surface of the second electrode body. Here, the coefficient of friction between the first electrode body, the electrode body disposed between the first electrode body and the second electrode body, and the second electrode body is greater than the coefficient of friction between the insulating member and the flat outer surface of the first electrode body and the coefficient of friction between the insulating member and the flat outer surface of the second electrode body. With this configuration, the movement of each electrode body in the longitudinal direction can be suitably suppressed.

[0020] In a preferred embodiment of the battery of this aspect, the insulating member is made of a resin film, and the coefficient of friction between the first electrode body, the electrode body disposed between the first electrode body and the second electrode body, and the second electrode body is greater than the coefficient of friction between the insulating member and the first side wall. With this configuration, longitudinal movement of each electrode body can be suitably suppressed. [Brief description of the drawings]

[0021] [Figure 1] FIG. 1 is a perspective view showing a battery according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic vertical cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 2 is a schematic vertical cross-sectional view taken along line III-III in FIG. [Figure 4] FIG. 2 is a schematic cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. 2 is a schematic diagram showing an electrode assembly attached to a sealing plate according to one embodiment. [Figure 6] FIG. 2 is a perspective view that shows a schematic diagram of an electrode assembly to which a positive electrode second current collecting portion and a negative electrode second current collecting portion are attached according to one embodiment. [Figure 7] FIG. 2 is a schematic diagram showing the configuration of a wound electrode body according to one embodiment. [Figure 8] 3 is a partially enlarged cross-sectional view that illustrates a schematic view of the vicinity of the positive electrode terminal in FIG. 2. [Figure 9] 1 is a perspective view showing a schematic diagram of a sealing plate to which a positive electrode terminal, a negative electrode terminal, a positive electrode first connection part, a negative electrode first connection part, a positive electrode insulating member, and a negative electrode insulating member are attached according to one embodiment. FIG. [Figure 10] FIG. 10 is a perspective view of the sealing plate of FIG. 9 turned over. [Figure 11] 5A to 5C are schematic cross-sectional views illustrating a battery insertion process according to one embodiment. [Figure 12] FIG. 13 is a schematic diagram showing an electrode assembly attached to a sealing plate according to another embodiment. [Figure 13] FIG. 13 is a schematic diagram showing an electrode assembly attached to a sealing plate according to another embodiment. [Figure 14] 13 is a schematic diagram showing an electrode assembly group attached to a sealing plate according to another embodiment. FIG. [Figure 15] 13 is a schematic diagram showing an electrode assembly group attached to a sealing plate according to another embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0022] Hereinafter, some preferred embodiments of the technology disclosed herein will be described with reference to the drawings. It should be noted that matters other than those specifically mentioned in this specification and necessary for carrying out the present invention (for example, the general configuration and manufacturing process of a battery that does not characterize the present invention) can be understood as design matters of a person skilled in the art based on the prior art in the field. The present invention can be carried out based on the contents disclosed in this specification and the technical common sense in the field. In addition, the expression "A to B" indicating a numerical range in this specification includes the meaning of A or more and B or less, as well as "preferably greater than A" and "preferably smaller than B".

[0023] In this specification, the term "battery" refers to any power storage device capable of extracting electrical energy, and is a concept that includes primary batteries and secondary batteries. In addition, in this specification, the term "secondary battery" refers to any power storage device capable of repeated charging and discharging, and is a concept that includes so-called storage batteries (chemical batteries) such as lithium ion secondary batteries and nickel metal hydride batteries, and capacitors (physical batteries) such as electric double layer capacitors.

[0024] <Battery 100> FIG. 1 is a perspective view of the battery 100. FIG. 2 is a schematic longitudinal sectional view taken along line II-II in FIG. 1. FIG. 3 is a schematic longitudinal sectional view taken along line III-III in FIG. 1. FIG. 4 is a schematic transverse sectional view taken along line IV-IV in FIG. 1. In the following description, the symbols L, R, F, Rr, U, and D in the drawings represent left, right, front, rear, top, and bottom, and the symbols X, Y, and Z in the drawings represent the short side direction, the long side direction perpendicular to the short side direction (which can also be referred to as the longitudinal direction of the electrode body), and the up-down direction, respectively, of the battery 100. However, these directions are merely for the convenience of description, and do not limit the installation form of the battery 100 in any way.

[0025] As shown in FIG. 2, the battery 100 includes a battery case 10, an electrode assembly 20, a positive terminal 30, a negative terminal 40, a positive current collector 50, a negative current collector 60, a positive insulating member 70, and a negative insulating member 80. Although not shown, the battery 100 further includes an electrolyte. The battery 100 is a lithium ion secondary battery. The battery 100 is characterized by including a fixing member 1 described later, and other configurations may be similar to those of a conventional battery. The fixing member 1 is an example of a fixing member disclosed herein.

[0026] The battery case 10 is a housing that houses the electrode assembly 20. Here, the battery case 10 has a flat, bottomed rectangular parallelepiped (rectangular) outer shape. The material of the battery case 10 may be the same as that conventionally used, and is not particularly limited. The battery case 10 is preferably made of a metal, and more preferably made of, for example, aluminum, an aluminum alloy, iron, an iron alloy, or the like. As shown in FIG. 2, the battery case 10 includes an exterior body 12 having an opening 12h, and a sealing plate (lid body) 14 that closes the opening 12h.

[0027] As shown in FIG. 1, the exterior body 12 includes a bottom wall 12a, a pair of long side walls 12b extending from the bottom wall 12a and facing each other, and a pair of short side walls 12c extending from the bottom wall 12a and facing each other. The bottom wall 12a is substantially rectangular. The bottom wall 12a faces the opening 12h. The area of ​​the short side wall 12c is smaller than the area of ​​the long side wall 12b. The long side wall 12b and the short side wall 12c are examples of the first side wall and the second side wall disclosed herein. The sealing plate 14 is attached to the exterior body 12 so as to close the opening 12h of the exterior body 12. The sealing plate 14 faces the bottom wall 12a of the exterior body 12. The sealing plate 14 is substantially rectangular in plan view. The battery case 10 is integrated by joining (for example, welding) a sealing plate 14 to the periphery of the opening 12h of the exterior body 12. The battery case 10 is hermetically sealed (sealed).

[0028] As shown in FIG. 2, the sealing plate 14 is provided with a liquid inlet 15, a gas exhaust valve 17, and two terminal outlet holes 18 and 19. The liquid inlet 15 is for injecting an electrolyte after the sealing plate 14 is assembled to the exterior body 12. The liquid inlet 15 is sealed by a sealing member 16. The gas exhaust valve 17 is configured to break when the pressure inside the battery case 10 reaches a predetermined value or more, thereby discharging the gas inside the battery case 10 to the outside. The terminal outlet holes 18 and 19 are formed at both ends of the sealing plate 14 in the long side direction Y. The terminal outlet holes 18 and 19 penetrate the sealing plate 14 in the up-down direction Z. The terminal outlet holes 18 and 19 each have an inner diameter large enough to insert the positive electrode terminal 30 and the negative electrode terminal 40 before being attached to the sealing plate 14 (before being crimped).

[0029] The positive electrode terminal 30 and the negative electrode terminal 40 are each fixed to the sealing plate 14. The positive electrode terminal 30 is disposed on one side of the sealing plate 14 in the long side direction Y (the left side in Figs. 1 and 2). The negative electrode terminal 40 is disposed on the other side of the sealing plate 14 in the long side direction Y (the right side in Figs. 1 and 2). As shown in Fig. 1, the positive electrode terminal 30 and the negative electrode terminal 40 are exposed on the outer surface of the sealing plate 14. As shown in Fig. 2, the positive electrode terminal 30 and the negative electrode terminal 40 extend from the inside to the outside of the sealing plate 14 through the terminal pull-out holes 18 and 19. Here, the positive electrode terminal 30 and the negative electrode terminal 40 are crimped to the peripheral portion surrounding the terminal pull-out holes 18 and 19 of the sealing plate 14 by crimping. The positive electrode terminal 30 and the negative electrode terminal 40 have crimping portions 30c, 40c formed at their ends on the exterior body 12 side (the lower ends in FIG. 2).

[0030] As shown in Fig. 2, the positive electrode terminal 30 is electrically connected to the positive electrode 22 of the electrode assembly 20 via a positive electrode current collector 50 inside the exterior body 12. The negative electrode terminal 40 is electrically connected to the negative electrode 24 of the electrode assembly 20 via a negative electrode current collector 60 inside the exterior body 12. The positive electrode terminal 30 is insulated from the sealing plate 14 by a positive electrode insulating member 70 and a gasket 90. The negative electrode terminal 40 is insulated from the sealing plate 14 by a negative electrode insulating member 80 and a gasket 90. The positive electrode terminal 30 and the negative electrode terminal 40 are examples of terminals disclosed herein.

[0031] The positive electrode terminal 30 is preferably made of a metal, and more preferably made of, for example, aluminum or an aluminum alloy. The negative electrode terminal 40 is preferably made of a metal, and more preferably made of, for example, copper or a copper alloy. The negative electrode terminal 40 may be configured by joining two conductive members together. For example, the portion connected to the negative electrode current collecting portion 60 may be made of copper or a copper alloy, and the portion exposed on the outer surface of the sealing plate 14 may be made of aluminum or an aluminum alloy.

[0032] As shown in FIG. 1, a plate-shaped positive electrode external conductive member 32 and a plate-shaped negative electrode external conductive member 42 are attached to the outer surface of the sealing plate 14. The positive electrode external conductive member 32 is electrically connected to the positive electrode terminal 30. The negative electrode external conductive member 42 is electrically connected to the negative electrode terminal 40. The positive electrode external conductive member 32 and the negative electrode external conductive member 42 are members to which bus bars are attached when electrically connecting a plurality of batteries 100 to each other. The positive electrode external conductive member 32 and the negative electrode external conductive member 42 are preferably made of metal, and more preferably made of aluminum or an aluminum alloy, for example. The positive electrode external conductive member 32 and the negative electrode external conductive member 42 are insulated from the sealing plate 14 by an external insulating member 92. However, the positive electrode external conductive member 32 and the negative electrode external conductive member 42 are not essential and may be omitted in other embodiments.

[0033] FIG. 5 is a perspective view that shows a schematic view of the electrode assembly 20 attached to the sealing plate 14. The electrode assembly 20 has three electrode bodies 20a, 20b, and 20c. The electrode bodies 20a, 20b, and 20c have a pair of rectangular flat outer surfaces 27 and are formed in a flat hexahedral shape. The electrode bodies 20a and 20c are examples of the first electrode body and the second electrode body disclosed herein. However, the number of electrode bodies arranged inside one exterior body 12 is not particularly limited, and may be two or more (plural), or may be one. The electrode assembly group 20 is arranged inside the exterior body 12 in a state where it is covered with an insulating member 29 (see FIG. 3) made of a resin film.

[0034] FIG. 6 is a perspective view showing the electrode body 20a. FIG. 7 is a schematic diagram showing the configuration of the electrode body 20a. In the following, the electrode body 20a will be described in detail as an example, but the electrode bodies 20b and 20c can also be configured in a similar manner. As shown in FIG. 7, the electrode body 20a has a positive electrode 22 and a negative electrode 24. The electrode body 20a is a flat-shaped wound electrode body in which a strip-shaped positive electrode 22 and a strip-shaped negative electrode 24 are stacked with a strip-shaped separator 26 interposed therebetween and wound around a winding axis WL.

[0035] The electrode body 20a is disposed inside the exterior body 12 with the winding axis WL oriented parallel to the long side direction Y. In other words, the electrode body 20a is disposed inside the exterior body 12 with the winding axis WL oriented parallel to the bottom wall 12a and perpendicular to the short side wall 12c. An end face of the electrode body 20a (in other words, the layered surface where the positive electrode 22 and the negative electrode 24 are layered, the end face in the long side direction Y in FIG. 7) faces the short side wall 12c.

[0036] 3, the electrode body 20a has a pair of curved portions 20r that face the bottom wall 12a and the sealing plate 14 of the exterior body 12, and a flat portion 20f that connects the pair of curved portions 20r and faces the long side wall 12b of the exterior body 12. However, the electrode body 20a may be a laminated electrode body in which a plurality of square-shaped (typically rectangular) positive electrodes and a plurality of square-shaped (typically rectangular) negative electrodes are stacked in an insulated state.

[0037] As shown in FIG. 7, the positive electrode 22 has a positive electrode collector 22c, and a positive electrode active material layer 22a and a positive electrode protective layer 22p fixed on at least one surface of the positive electrode collector 22c. However, the positive electrode protective layer 22p is not essential and can be omitted in other embodiments. The positive electrode collector 22c is strip-shaped. The positive electrode collector 22c is made of a conductive metal such as aluminum, an aluminum alloy, nickel, or stainless steel. The positive electrode collector 22c is a metal foil, specifically an aluminum foil, here. The width (see FIG. 7) of the positive electrode collector 22c perpendicular to the long side direction Y is not particularly limited as long as the effect of the technology disclosed herein is exerted, but is preferably 0.5 mm or more, for example.

[0038] A plurality of positive electrode tabs 22t are provided at one end of the positive electrode current collector 22c in the long side direction Y (the left end in FIG. 7). The plurality of positive electrode tabs 22t each protrude toward one side of the long side direction Y (the left side in FIG. 7). The plurality of positive electrode tabs 22t protrude in the long side direction Y beyond the separator 26. The plurality of positive electrode tabs 22t are provided at intervals (intermittently) along the longitudinal direction of the positive electrode 22. Each of the plurality of positive electrode tabs 22t has a trapezoidal shape. The positive electrode tab 22t is a part of the positive electrode current collector 22c here, and is made of a metal foil (aluminum foil, aluminum alloy foil, etc.). The positive electrode tab 22t is a portion (current collector exposed portion) of the positive electrode current collector 22c where the positive electrode active material layer 22a and the positive electrode protective layer 22p are not formed. However, the positive electrode tab 22t may be a member separate from the positive electrode current collector 22c. The positive electrode tab 22t may be provided at the other end in the long side direction Y (the right end in FIG. 7), or at both ends in the long side direction Y.

[0039] As shown in FIG. 4, the positive electrode tabs 22t are stacked at one end in the long side direction Y (the left end in FIG. 4, i.e., one of the pair of short side walls 12c (second side walls)) to form a positive electrode tab group 23. The positive electrode tabs 22t are bent and curved so that the outer end extends along the short side wall 12c. The positive electrode tab group 23 is electrically connected to the positive electrode terminal 30 via the positive electrode current collector 50. It is preferable that the positive electrode tabs 22t are bent and joined to a surface of the electrode body side of the positive electrode second current collector 52 described later, and electrically connected to the positive electrode terminal 30. In addition, as shown in FIG. 4, the positive electrode tab group 23 is preferably joined in a state where they are gathered to one flat outer surface side of the pair of flat outer surfaces 27. The size of the positive electrode tabs 22t (the length in the long side direction Y and the width perpendicular to the long side direction Y, see FIG. 7) can be appropriately adjusted, for example, by the position of the positive electrode tabs 22t, taking into consideration the state of connection to the positive electrode current collecting part 50. The width perpendicular to the long side direction Y of the positive electrode tabs 22t is not particularly limited as long as the effects of the technology disclosed herein are exhibited, but is preferably 3 μm to 50 μm, more preferably 5 μm to 30 μm, and particularly preferably 10 μm to 20 μm. The positive electrode tabs 22t here are different in size from each other so that the outer ends are aligned when curved. The positive electrode tab group 23 is an example of an electrode tab group disclosed herein.

[0040] As shown in FIG. 7, the positive electrode active material layer 22a is provided in a strip shape along the longitudinal direction of the strip-shaped positive electrode current collector 22c. The positive electrode active material layer 22a contains a positive electrode active material (for example, a lithium transition metal composite oxide such as a lithium nickel cobalt manganese composite oxide) capable of reversibly absorbing and releasing charge carriers. When the entire solid content of the positive electrode active material layer 22a is taken as 100 mass%, the positive electrode active material may occupy approximately 80 mass% or more, typically 90 mass% or more, for example 95 mass% or more. The positive electrode active material layer 22a may contain any component other than the positive electrode active material, such as a conductive material, a binder, various additive components, etc. As the conductive material, for example, a carbon material such as acetylene black (AB) can be used. As the binder, for example, polyvinylidene fluoride (PVdF) can be used.

[0041] As shown in FIG. 7, the positive electrode protective layer 22p is provided at the boundary between the positive electrode collector 22c and the positive electrode active material layer 22a in the long side direction Y. Here, the positive electrode protective layer 22p is provided at one end (the left end in FIG. 7) of the positive electrode collector 22c in the long side direction Y. However, the positive electrode protective layer 22p may be provided at both ends in the long side direction Y. The positive electrode protective layer 22p is provided in a strip shape along the positive electrode active material layer 22a. The positive electrode protective layer 22p contains an inorganic filler (e.g., alumina). When the entire solid content of the positive electrode protective layer 22p is taken as 100 mass%, the inorganic filler may occupy approximately 50 mass% or more, typically 70 mass% or more, for example 80 mass% or more. The positive electrode protective layer 22p may contain any component other than the inorganic filler, such as a conductive material, a binder, or various additive components. The conductive material and binder may be the same as those exemplified as those that may be contained in the positive electrode active material layer 22a.

[0042] As shown in Fig. 7, the negative electrode 24 has a negative electrode current collector 24c and a negative electrode active material layer 24a fixed on at least one surface of the negative electrode current collector 24c. The negative electrode current collector 24c is strip-shaped. The negative electrode current collector 24c is made of a conductive metal such as copper, a copper alloy, nickel, or stainless steel. The negative electrode current collector 24c is a metal foil, specifically a copper foil, here. The width (see Fig. 7) of the negative electrode current collector 24c perpendicular to the long side direction Y is not particularly limited as long as the effect of the technology disclosed herein is exhibited, but is preferably 0.5 mm or more, for example.

[0043] A plurality of negative electrode tabs 24t are provided at one end of the negative electrode current collector 24c in the long side direction Y (the right end in FIG. 7). The plurality of negative electrode tabs 24t protrude toward one side of the long side direction Y (the right side in FIG. 7). The plurality of negative electrode tabs 24t protrude in the long side direction Y beyond the separator 26. The plurality of negative electrode tabs 24t are provided at intervals (intermittently) along the longitudinal direction of the negative electrode 24. Each of the plurality of negative electrode tabs 24t has a trapezoidal shape. The negative electrode tab 24t is a part of the negative electrode current collector 24c here, and is made of a metal foil (copper foil, copper alloy, etc.). The negative electrode tab 24t is a portion of the negative electrode current collector 24c where the negative electrode active material layer 24a is not formed (current collector exposed portion). However, the negative electrode tab 24t may be a member separate from the negative electrode current collector 24c. The negative electrode tab 24t may be provided at the other end in the long side direction Y (the left end in FIG. 7), or at both ends in the long side direction Y.

[0044] As shown in FIG. 4, the negative electrode tabs 24t are stacked at one end in the long side direction Y (the right end in FIG. 4, i.e., the other short side wall side of the pair of short side walls 12c (second side walls)) to form a negative electrode tab group 25. The negative electrode tabs 24t are bent and curved so that the outer end extends along the short side wall 12c. The negative electrode tab group 25 is electrically connected to the negative electrode terminal 40 via the negative electrode current collector 60. It is preferable that the negative electrode tabs 24t are bent and joined to a surface of the electrode body side of the negative electrode second current collector 62 described later, and electrically connected to the negative electrode terminal 40. In addition, as shown in FIG. 4, the negative electrode tab group 25 is preferably joined in a state where they are gathered to one flat outer surface side of the pair of flat outer surfaces 27. The size of the negative electrode tabs 24t (the length in the long side direction Y and the width perpendicular to the long side direction Y, see FIG. 7) can be appropriately adjusted, for example, by the position of the negative electrode tabs 24t, in consideration of the state of connection to the negative electrode current collecting part 60. The width perpendicular to the long side direction Y of the negative electrode tabs 24t is not particularly limited as long as the effects of the technology disclosed herein are exhibited, but is preferably 3 μm to 50 μm, more preferably 5 μm to 30 μm, and particularly preferably 5 μm to 20 μm. The negative electrode tabs 24t here are different in size from each other so that the outer ends are aligned when curved. The negative electrode tab group 25 is an example of an electrode tab group disclosed herein.

[0045] The negative electrode active material layer 24a is provided in a strip shape along the longitudinal direction of the strip-shaped negative electrode current collector 24c. The negative electrode active material layer 24a contains a negative electrode active material (e.g., a carbon material such as graphite) that can reversibly store and release charge carriers. When the entire solid content of the negative electrode active material layer 24a is taken as 100 mass%, the negative electrode active material may occupy approximately 80 mass% or more, typically 90 mass% or more, for example 95 mass% or more. The negative electrode active material layer 24a may contain any component other than the negative electrode active material, such as a binder, a dispersant, various additive components, etc. As the binder, for example, rubbers such as styrene butadiene rubber (SBR) can be used. As the dispersant, for example, celluloses such as carboxymethyl cellulose (CMC) can be used.

[0046] The separator 26 is a member that insulates the positive electrode active material layer 22a of the positive electrode 22 from the negative electrode active material layer 24a of the negative electrode 24. As the separator 26, for example, a porous resin sheet made of a polyolefin resin such as polyethylene (PE) or polypropylene (PP) is suitable. A heat resistance layer (HRL) containing an inorganic filler may be provided on the surface of the separator 26. As the inorganic filler, for example, alumina, boehmite, aluminum hydroxide, titania, etc. may be used.

[0047] The electrolyte may be the same as that used in the past and is not particularly limited. The electrolyte is, for example, a non-aqueous electrolyte containing a non-aqueous solvent and a supporting salt. The non-aqueous solvent contains, for example, carbonates such as ethylene carbonate, dimethyl carbonate, and ethyl methyl carbonate. The supporting salt is, for example, a fluorine-containing lithium salt such as LiPF6. However, the electrolyte may be in a solid state (solid electrolyte) and integrated with the electrode body group 20.

[0048] The positive electrode current collecting part 50 constitutes a conductive path that electrically connects the positive electrode tab group 23 consisting of the multiple positive electrode tabs 22t to the positive electrode terminal 30. As shown in FIG. 2, the positive electrode current collecting part 50 includes a positive electrode first current collecting part 51 disposed between the sealing plate 14 and the electrode body 20a, and a positive electrode second current collecting part 52 to which the positive electrode tab group 23 is joined. The positive electrode first current collecting part 51 and the positive electrode second current collecting part 52 may be made of the same metal type as the positive electrode current collecting body 22c, for example, a conductive metal such as aluminum, an aluminum alloy, nickel, or stainless steel.

[0049] FIG. 8 is a partially enlarged cross-sectional view that typically shows the vicinity of the positive electrode terminal 30 in FIG. 2. FIG. 9 is a perspective view that typically shows the sealing plate 14. FIG. 10 is a perspective view of the sealing plate in FIG. 9 turned over. FIG. 10 shows the surface of the sealing plate 14 on the side of the exterior body 12 (inner side). As shown in FIGS. 8 to 10, the positive electrode first current collecting part 51 is attached to the inner surface of the sealing plate 14. The positive electrode first current collecting part 51 is an example of a current collecting part disclosed herein. The positive electrode first current collecting part 51 has a first region 51a and a second region 51b. The positive electrode first current collecting part 51 may be formed by bending one member, for example, by pressing or the like, or may be formed by integrating a plurality of members by welding or the like. Here, the positive electrode first current collecting part 51 is fixed to the sealing plate 14 by crimping.

[0050] The first region 51a is a region disposed between the sealing plate 14 and the electrode assembly 20. The first region 51a extends along the long side direction Y. The first region 51a spreads horizontally along the inner surface of the sealing plate 14. A positive electrode insulating member 70 is disposed between the sealing plate 14 and the first region 51a. The first region 51a is insulated from the sealing plate 14 by the positive electrode insulating member 70. The first region 51a is electrically connected to the positive electrode terminal 30 by crimping. In the first region 51a, a through hole 51h penetrating in the up-down direction Z is formed at a position corresponding to the terminal lead-out hole 18 of the sealing plate 14. The second region 51b is a region disposed between the short side wall 12c of the exterior body 12 and the electrode assembly 20. The second region 51b extends from one end of the first region 51a in the long side direction Y (the left end in FIG. 8) toward the short side wall 12c of the exterior body 12. The second region 51b extends in the up-down direction Z.

[0051] The positive electrode second current collecting portion 52 extends along the short side wall 12c of the exterior body 12. As shown in FIG. 6, the positive electrode second current collecting portion 52 has a current collecting plate connection portion 52a, an inclined portion 52b, and a tab joint portion 52c. The current collecting plate connection portion 52a is a portion electrically connected to the positive electrode first current collecting portion 51. The current collecting plate connection portion 52a extends along the up-down direction Z. The current collecting plate connection portion 52a is disposed substantially perpendicular to the winding axis WL of the electrode bodies 20a, 20b, and 20c. The current collecting plate connection portion 52a is provided with a recess 52d that is thinner than its surroundings. The recess 52d is provided with a through hole 52e that penetrates in the short side direction X. The through hole 52e is provided with a joint with the positive electrode first current collecting portion 51. The joint is a welded joint formed by welding such as ultrasonic welding, resistance welding, and laser welding. The positive electrode second current collecting portion 52 may be provided with a fuse.

[0052] The tab joint 52c is a portion that is attached to the positive electrode tab group 23 and electrically connected to the multiple positive electrode tabs 22t. As shown in FIG. 5, the tab joint 52c extends along the up-down direction Z. The tab joint 52c is disposed substantially perpendicular to the winding axis WL of the electrode bodies 20a, 20b, and 20c. The surface of the tab joint 52c that is connected to the multiple positive electrode tabs 22t is disposed substantially parallel to the short side wall 12c of the exterior body 12. As shown in FIG. 4, the tab joint 52c has a joint J with the positive electrode tab group 23. The joint J is a welded joint formed by welding such as ultrasonic welding, resistance welding, and laser welding in a state where the multiple positive electrode tabs 22t are overlapped. The welded joint is disposed by moving the multiple positive electrode tabs 22t toward one side of the short side direction X of the electrode bodies 20a, 20b, and 20c. This makes it possible to more suitably bend the multiple positive electrode tabs 22t, and stably form the curved positive electrode tab group 23 as shown in FIG.

[0053] The inclined portion 52b is a portion that connects the lower end of the current collector connection portion 52a and the upper end of the tab joint portion 52c. The inclined portion 52b is inclined with respect to the current collector connection portion 52a and the tab joint portion 52c. The inclined portion 52b connects the current collector connection portion 52a and the tab joint portion 52c so that the current collector connection portion 52a is located closer to the center than the tab joint portion 52c in the long side direction Y. This makes it possible to expand the storage space of the electrode body group 20 and to increase the energy density of the battery 100. It is preferable that the lower end of the inclined portion 52b (in other words, the end portion on the side of the bottom wall 12a of the exterior body 12) is located lower than the lower end of the positive electrode tab group 23. This makes it possible to more suitably bend the multiple positive electrode tabs 22t and stably form the curved positive electrode tab group 23 as shown in FIG. 4.

[0054] The negative electrode current collecting part 60 constitutes a conductive path that electrically connects the negative electrode tab group 25 consisting of a plurality of negative electrode tabs 24t and the negative electrode terminal 40. As shown in FIG. 2, the negative electrode current collecting part 60 includes a negative electrode first current collecting part 61 arranged between the sealing plate 14 and the electrode body 20a, and a negative electrode second current collecting part 62 to which the negative electrode tab group 25 is joined. The negative electrode first current collecting part 61 is an example of a current collecting part disclosed herein. The negative electrode first current collecting part 61 and the negative electrode second current collecting part 62 may be made of the same metal type as the negative electrode current collecting body 24c, for example, a conductive metal such as copper, a copper alloy, nickel, or stainless steel. The configurations of the negative electrode first current collecting part 61 and the negative electrode second current collecting part 62 may be the same as those of the positive electrode first current collecting part 51 and the positive electrode second current collecting part 52 of the positive electrode current collecting part 50.

[0055] As shown in FIG. 10, the negative electrode first current collecting portion 61 has a first region 61a and a second region 61b. A negative electrode insulating member 80 is disposed between the sealing plate 14 and the first region 61a. The first region 61a is insulated from the sealing plate 14 by the negative electrode insulating member 80. In the first region 51a, a through hole 61h penetrating in the up-down direction Z is formed at a position corresponding to the terminal pull-out hole 19 of the sealing plate 14. As shown in FIG. 6, the negative electrode second current collecting portion 62 has a current collecting plate connection portion 62a electrically connected to the negative electrode first current collecting portion 61, an inclined portion 62b, and a tab joint portion 62c attached to the negative electrode tab group 25 and electrically connected to the multiple negative electrode tabs 24t. The current collecting plate connection portion 62a has a recess 62d connected to the tab joint portion 62c. The recess 62d is provided with a through hole 62e penetrating in the short side direction X.

[0056] The positive electrode insulating member 70 is a member that insulates the sealing plate 14 and the positive electrode first current collecting portion 51 inside the battery case 10. The positive electrode insulating member 70 is made of, for example, a resin material that has resistance to the electrolyte used, electrical insulation properties, and is elastically deformable. The positive electrode insulating member 70 is preferably made of, for example, a polyolefin resin such as polypropylene (PP), a fluorinated resin such as tetrafluoroethylene-perfluoroalkoxyethylene copolymer (PFA), polyphenylene sulfide (PPS), or the like. As shown in FIG. 2, the positive electrode insulating member 70 has a base portion 70a and a protruding portion 70b. Here, the base portion 70a and the protruding portion 70b are integrally molded.

[0057] The base portion 70a is a portion that is disposed between the sealing plate 14 and the first region 51a of the positive electrode first current collecting portion 51 in the vertical direction Z. The base portion 70a spreads horizontally along the first region 51a of the positive electrode first current collecting portion 51. The base portion 70a has a through hole (not shown) that penetrates in the vertical direction Z. The through hole is formed at a position corresponding to the terminal lead-out hole 18 of the sealing plate 14.

[0058] The protrusions 70b protrude toward the electrode body group 20 relative to the base portion 70a. As shown in Fig. 10, the protrusions 70b are provided closer to the center of the sealing plate 14 (to the right in Fig. 10) than the base portion 70a in the long side direction Y. As shown in Fig. 3, the protrusions 70b face the curved portions 20r of the electrode bodies 20a, 20b, and 20c that constitute the electrode body group 20 here.

[0059] 2, the negative electrode insulating member 80 is disposed symmetrically to the positive electrode insulating member 70 with respect to the long side direction Y of the electrode body group 20. The specific configuration of the negative electrode insulating member 80 may be similar to that of the positive electrode insulating member 70. Here, like the positive electrode insulating member 70, the negative electrode insulating member 80 has a base portion 80a disposed between the sealing plate 14 and the negative electrode first current collecting portion 61, and a protruding portion 80b.

[0060] As shown in FIG. 5, in the battery 100 according to this embodiment, the fixing member 1 is arranged in a U-shape from the flat outer surface 27a to the flat outer surface 27f so as to cover the positive electrode second current collecting portion 52 of the three electrode bodies 20a, 20b, and 20c. In this way, by fixing the electrode bodies 20a, 20b, and 20c using the fixing member 1, the movement of the electrode body 20b in the longitudinal direction can be more suitably suppressed. In addition, the fixing member 1 according to this embodiment is arranged so as to cover three joints between the positive electrode first current collecting portion 51 and the positive electrode second current collecting portion 52. In this way, by fixing the electrode body group 20 to a position close to the sealing plate 14 in the positive electrode current collecting portion 50, the movement of the electrode body group 20 in the longitudinal direction can be more suitably suppressed.

[0061] As the fixing member 1, for example, one having a base material and an adhesive layer formed on the base material can be preferably used. Examples of the base material include polyethylene (PE), polypropylene (PP), polyester, nylon, vinyl chloride, Teflon (registered trademark), polyimide, Kapton (registered trademark), polyphenylene sulfide, and polyethylene naphthalate. The thickness of the base material is not particularly limited as long as the effect of the technology disclosed herein is exerted, but it can be about 5 μm to 100 μm, and preferably 10 μm to 50 μm. Examples of materials constituting the adhesive layer include acrylic adhesives, silicon adhesives, and rubber adhesives. The adhesive layer preferably has adhesiveness at room temperature (typically, about 20° C.). The thickness of the adhesive layer is not particularly limited as long as the effect of the technology disclosed herein is exerted, but it can be about 5 μm to 100 μm, and preferably 5 μm to 20 μm.

[0062] As shown in FIG. 3, in the battery 100 according to this embodiment, an insulating member 29 is disposed between the long side wall of the pair of long side walls 12b (first side walls) facing the flat outer surface 27a and the flat outer surface 27a, and between the other long side wall of the pair of long side walls 12b and the flat outer surface 27f in the battery case 10. The friction coefficients of the electrode bodies 20a, 20b, and 20c (i.e., the friction coefficients of the flat outer surfaces 27b and 27c, and the flat outer surfaces 27d and 27e; hereinafter also referred to as friction coefficient A) are greater than the friction coefficients of the insulating member 29a and the flat outer surface 27a, and the friction coefficients of the insulating member 29b and the flat outer surface 27f (hereinafter also referred to as friction coefficient B). This configuration is preferable because it suppresses the movement of the electrode body group 20 in the longitudinal direction. Here, as the friction coefficients A and B, for example, friction coefficients measured based on the provisions of JIS K7125 can be adopted. The difference between the friction coefficients A and B can be about 0.1 to 0.9, preferably about 0.5 to 0.8, but is not limited thereto. A method for providing the above-mentioned difference between the friction coefficients A and B includes a method of appropriately selecting materials constituting the insulating member 29 and the flat outer surface 27. Those skilled in the art can easily select such materials by conducting a preliminary test or the like.

[0063] In the battery 100 according to this embodiment, the coefficient of friction between the electrode body 20a and the electrode body 20b (i.e., the coefficient of friction between the flat outer surface 27b and the flat outer surface 27c) and the coefficient of friction between the electrode body 20b and the electrode body 20c (i.e., the coefficient of friction between the flat outer surface 27d and the flat outer surface 27e) (hereinafter also referred to as the friction coefficient C) are greater than the coefficient of friction between the insulating member 29 and the long side wall 12b (i.e., the coefficient of friction between the insulating member 29a and the long side wall 12b, and the coefficient of friction between the insulating member 29b and the long side wall 12b; hereinafter also referred to as the friction coefficient D). This configuration is preferable because it suppresses the movement of the electrode body group 20 in the longitudinal direction. Here, as the friction coefficients C and D, for example, the friction coefficients measured based on the provisions of JIS K7125 can be adopted. The difference between the coefficients of friction C and D can be about 0.1 to 0.9, preferably about 0.5 to 0.8, but is not limited thereto. A method for providing the coefficients of friction C and D with the difference as described above can be achieved by appropriately selecting materials for forming the insulating member 29, the long side wall 12b, and the flat outer surface 27. Those skilled in the art can easily select such materials by conducting a preliminary test or the like.

[0064] 5, in the battery 100 according to this embodiment, the fixing member 1 is not disposed between the electrode body 20a and the electrode body 20b, and between the electrode body 20b and the electrode body 20c. With this configuration, the integrated thickness of the electrode body group 20 can be reduced, and therefore the pressure distribution of each electrode body constituting the electrode body group 20 can be alleviated. This is preferable because it can suitably suppress uneven reactions in each electrode body constituting the electrode body group 20.

[0065] <Manufacturing method of battery 100> The manufacturing method of the battery 100 is characterized by including the fixing member 1 as described above. The rest of the manufacturing process may be the same as in the past. In addition to the fixing member 1, the battery 100 can be manufactured by preparing the battery case 10 (exterior body 12 and sealing plate 14), the electrode body group 20 (electrode bodies 20a, 20b, 20c), the electrolyte, the positive electrode terminal 30, the negative electrode terminal 40, the positive electrode current collector 50 (positive electrode first current collector 51 and positive electrode second current collector 52), the negative electrode current collector 60 (negative electrode first current collector 61 and negative electrode second current collector 62), the positive electrode insulating member 70, and the negative electrode insulating member 80, for example, by a manufacturing method including a first mounting step, a second mounting step, an insertion step, and a sealing step. In addition, the manufacturing method disclosed herein may further include other steps at any stage.

[0066] In the first attachment step, a first combination is prepared as shown in Fig. 9 and Fig. 10. Specifically, first, the positive terminal 30, the positive electrode first current collecting part 51, the positive electrode insulating member 70, the negative electrode terminal 40, the negative electrode first current collecting part 61, and the negative electrode insulating member 80 are attached to the sealing plate 14.

[0067] The positive electrode terminal 30, the positive electrode first current collecting portion 51, and the positive electrode insulating member 70 are fixed to the sealing plate 14 by, for example, crimping (riveting). As shown in FIG. 8, the crimping is performed by sandwiching a gasket 90 between the outer surface of the sealing plate 14 and the positive electrode terminal 30, and further sandwiching the positive electrode insulating member 70 between the inner surface of the sealing plate 14 and the positive electrode first current collecting portion 51. The material of the gasket 90 may be the same as that of the positive electrode insulating member 70. In detail, the positive electrode terminal 30 before the crimping is inserted from above the sealing plate 14 into the through hole 90h of the gasket 90, the terminal lead-out hole 18 of the sealing plate 14, the through hole 70h of the positive electrode insulating member 70, and the through hole 51h of the positive electrode first current collecting portion 51, in that order, so as to protrude downward from the sealing plate 14. Then, the portion of the positive electrode terminal 30 that protrudes downward from the sealing plate 14 is crimped so that a compressive force is applied in the vertical direction Z. As a result, a crimped portion 30c is formed at the tip end portion of the positive electrode terminal 30 (the lower end portion in FIG. 2).

[0068] By such crimping, the gasket 90, the sealing plate 14, the positive electrode insulating member 70, and the positive electrode first current collecting portion 51 are integrally fixed to the sealing plate 14, and the terminal pull-out hole 18 is sealed. The crimped portion 30c may be welded to the positive electrode first current collecting portion 51. This can further improve the reliability of conduction.

[0069] The negative electrode terminal 40, the negative electrode first current collecting part 61, and the negative electrode insulating member 80 can be fixed in the same manner as the positive electrode side described above. That is, the negative electrode terminal 40 before crimping is inserted from above the sealing plate 14 into the through hole of the gasket, the terminal lead-out hole 19 of the sealing plate 14, the through hole of the negative electrode insulating member 80, and the through hole of the negative electrode first current collecting part 61 in that order, so as to protrude below the sealing plate 14. Then, the portion of the negative electrode terminal 40 protruding below the sealing plate 14 is crimped so that a compressive force is applied in the vertical direction Z. As a result, a crimped portion 40c is formed at the tip portion (the lower end portion in FIG. 2) of the negative electrode terminal 40.

[0070] Next, the positive electrode external conductive member 32 and the negative electrode external conductive member 42 are attached to the outer surface of the sealing plate 14 via the external insulating member 92. The material of the external insulating member 92 may be the same as that of the positive electrode insulating member 70. The timing of attaching the positive electrode external conductive member 32 and the negative electrode external conductive member 42 may be after the insertion step (for example, after the liquid injection hole 15 is sealed).

[0071] In the second mounting step, the first combined body produced in the first mounting step is used to produce a second combined body as shown in FIG. 5. That is, an electrode body group 20 integrated with a sealing plate 14 is produced. Specifically, as shown in FIG. 6, three electrode bodies 20a to which a positive electrode second current collecting portion 52 and a negative electrode second current collecting portion 62 are attached are prepared, and the electrode bodies 20a, 20b, and 20c are arranged in parallel in the short side direction X. At this time, the electrode bodies 20a, 20b, and 20c may be arranged in parallel such that the positive electrode second current collecting portion 52 is arranged on one side of the long side direction Y (the left side in FIG. 5) and the negative electrode second current collecting portion 62 is arranged on the other side of the long side direction Y (the right side in FIG. 5).

[0072] Next, as shown in FIG. 4, in a state where the multiple positive electrode tabs 22t are bent, the positive electrode first current collecting portion 51 (specifically, the second region 51b) fixed to the sealing plate 14 is joined to the positive electrode second current collecting portion 52 (specifically, the current collecting plate connection portion 52a) of the electrode body 20a, 20b, 20c. In addition, in a state where the multiple negative electrode tabs 24t are bent, the negative electrode first current collecting portion 61 fixed to the sealing plate 14 is joined to the negative electrode second current collecting portion 62 of the electrode body 20a, 20b, 20c. As a joining method, for example, welding such as ultrasonic welding, resistance welding, and laser welding can be used. In particular, it is preferable to use welding by irradiation of high energy rays such as laser. By such welding processing, joints are formed in the recess 52d of the positive electrode second current collecting portion 52 and the recess 62d of the negative electrode second current collecting portion 62.

[0073] 5, the fixing member 1 is arranged in a U-shape so as to cover the positive electrode second current collecting portion 52 of the three electrode bodies 20a, 20b, and 20c from the flat outer surface 27a to the flat outer surface 27f. The timing of arranging the fixing member 1 may be before joining the positive electrode first current collecting portion 51 (specifically, the second region 51b) fixed to the sealing plate 14 and the positive electrode second current collecting portion 52 (specifically, the current collecting plate connection portion 52a) of the electrode bodies 20a, 20b, and 20c. That is, in the embodiment shown in FIG. 6, the fixing member 1 may be arranged after bending the positive electrode tab group 23. From the viewpoint of improving the work efficiency, it is more preferable to arrange the fixing member 1 at the above-mentioned timing.

[0074] In the insertion step, the second combined product prepared in the second attachment step is accommodated in the internal space of the exterior body 12. FIG. 11 is a schematic cross-sectional view for explaining the insertion step. Specifically, first, an insulating resin sheet (resin film) made of a resin material such as polyethylene (PE) is folded into a bag-like or box-like shape to prepare an insulating member 29. Next, the electrode body group 20 is accommodated in the insulating member 29. Then, the electrode body group 20 covered with the insulating member 29 is inserted into the exterior body 12. When the weight of the electrode body group 20 is heavy, approximately 1 kg or more, for example 1.5 kg or more, or even 2 to 3 kg, it is preferable to insert the electrode body group 20 into the exterior body 12 by arranging the long side wall 12b of the exterior body 12 so as to intersect with the direction of gravity (the exterior body 12 is oriented horizontally).

[0075] In the sealing step, the sealing plate 14 is joined to the edge of the opening 12h of the exterior body 12 to seal the opening 12h. The sealing step can be performed simultaneously with or after the insertion step. In the sealing step, the exterior body 12 and the sealing plate 14 are preferably welded together. The welded joint between the exterior body 12 and the sealing plate 14 can be performed by, for example, laser welding. Thereafter, the electrolyte is injected through the liquid injection hole 15, and the liquid injection hole 15 is blocked with a sealing member 16 to hermetically seal the battery 100. In this manner, the battery 100 can be manufactured.

[0076] Although the battery 100 can be used for various purposes, it is preferably used in applications where external forces such as vibrations and impacts may be applied during use, for example, as a power source (driving power source) for a motor mounted on a moving body (typically a vehicle such as a passenger car or truck). The type of vehicle is not particularly limited, but examples include a plug-in hybrid vehicle (PHV), a hybrid vehicle (HV), and an electric vehicle (EV). The battery 100 can also be preferably used as a battery pack in which a plurality of batteries 100 are arranged in a predetermined arrangement direction and a load is applied from the arrangement direction by a restraining mechanism.

[0077] Although several embodiments of the present invention have been described above, the above embodiments are merely examples. The present invention can be implemented in various other forms. The present invention can be implemented based on the contents disclosed in this specification and the technical common sense in the field. The technology described in the claims includes various modifications and changes to the above-exemplified embodiments. For example, it is possible to replace a part of the above-mentioned embodiment with another modified form, and it is also possible to add another modified form to the above-mentioned embodiment. Furthermore, if a technical feature is not described as essential, it is also possible to delete it as appropriate.

[0078] In the above embodiment, in the electrode body 20a, the positive electrode tab group 23 and the negative electrode tab group 25 are joined in a state where they are gathered on the flat outer surface 27a side (see FIG. 4), but this is not limited thereto. For example, in the electrode body 20a, the positive electrode tab group 23 may be joined in a state where they are gathered on the flat outer surface 27a side, and the negative electrode tab group 25 may be joined in a state where they are gathered on the flat outer surface 27b side. Alternatively, the positive electrode tab group 23 (negative electrode tab group 25) may be joined in a state where they are separately gathered on the flat outer surface 27a side and the flat outer surface 27b side. The same applies to the electrode bodies 20b and 20c.

[0079] In the above embodiment, the number of times that the positive electrode tab group 23 and the negative electrode tab group 25 in the electrode body 20a are folded is one (see FIG. 4), but this is not limited to this. For example, the number of times that such folding may be multiple. The same applies to the electrode bodies 20b and 20c.

[0080] In the above embodiment, the length of the fixing member 1 in the Y direction is arranged on the flat outer surface 27a of the electrode body 20a so as to be about 1 / 20 of the length La of the flat outer surface 27a in the Y direction (see FIG. 5), but is not limited thereto. For example, the length of the fixing member in the Y direction can be approximately (1 / 30)La or more, and from the viewpoint of improving the fixing strength, it can be preferably (1 / 20)La or more, more preferably (1 / 10)La or more, and even more preferably (1 / 5)La or more. The length of the fixing member in the Y direction may be La, or it can be (3 / 4)La or less, (1 / 2)La or less, or (1 / 3)La or less. The same applies to the length in the Y direction of the fixing member 1 arranged on the flat outer surface 27f.

[0081] In the above embodiment, the fixing member 1 is arranged in a U-shape so as to cover the positive electrode second current collecting portion 52 of the three electrode bodies 20a, 20b, and 20c from the flat outer surface 27a to the flat outer surface 27f, but the present invention is not limited thereto. For example, the fixing member may be arranged in a U-shape so as to cover the negative electrode second current collecting portion 62 of the three electrode bodies 20a, 20b, and 20c from the flat outer surface 27a to the flat outer surface 27f. Note that, compared with the case where the fixing member is arranged in a U-shape on the positive electrode side (i.e., the arrangement described above), the case where the fixing member is arranged in a U-shape on the negative electrode side (i.e., the arrangement described below) is preferable because fixing the electrode body to the negative electrode side can suitably prevent buckling of the positive electrode tab group, which is considered to be prone to buckling and stretching. Also, for example, the fixing member may be arranged from the flat outer surface 27a of the electrode body 20a to the positive electrode second current collecting portion 52 of the electrode body 20b, and from the flat outer surface 27f of the electrode body 20c to the negative electrode second current collecting portion 62 of the electrode body 20b. Note that these are merely examples, and various other forms are possible.

[0082] In the above embodiment, the fixing member 1 is arranged so as to cover three joints between the positive electrode 1 current collecting portion 51 and the positive electrode 2 current collecting portion 52, but the present invention is not limited thereto. For example, as shown in FIG. 12, the fixing member 1a may be arranged in a U-shape so as to cover the vicinity of the center of the positive electrode 2 current collecting portion 52 included in the three electrode bodies 20a, 20b, and 20c. Also, as shown in FIG. 13, the fixing member 1b may be arranged in a U-shape so as to cover the lower part of the positive electrode 2 current collecting portion 52 included in the three electrode bodies 20a, 20b, and 20c. Furthermore, the embodiments of FIG. 5, FIG. 12, and FIG. 13 can be appropriately combined and implemented. Note that, when the fixing member is arranged as shown in FIG. 12 and FIG. 13, it is preferable not to cover the tab joint portion 52c. Also, the above description focuses on the positive electrode 2 current collecting portion 52, but the same naturally applies to the negative electrode 2 current collecting portion 62. Note that these are only examples, and various other forms are possible.

[0083] In the above embodiment, the fixing member 1 is also disposed on the positive electrode second current collecting portion 52 of the electrode body 20b, but the present invention is not limited thereto. For example, as shown in Fig. 14, the fixing member 1c may be disposed from the flat outer surface 27a of the electrode body 20a to the positive electrode second current collecting portion 52, and from the flat outer surface 27f of the electrode body 20c to the positive electrode second current collecting portion 52. In this case, it is preferable that the movement of the electrode body 20b in the longitudinal direction is suppressed by friction generated between the flat outer surface 27b and the flat outer surface 27c, and between the flat outer surface 27d and the flat outer surface 27e.

[0084] Alternatively, in the case where the flat outer surface is composed of the separator 26 as in the electrode assemblies 20a, 20b, and 20c according to the present embodiment (see FIG. 7), an adhesive layer may be provided on the flat outer surface (i.e., the outermost surface of the separator) of the electrode assemblies 20a, 20b, and 20c in order to suppress the movement of the electrode assemblies 20b in the longitudinal direction. An example of the adhesive layer is a layer containing PVdF. The adhesive layer may also contain other components such as an inorganic filler. Examples of the inorganic filler include alumina, boehmite, aluminum hydroxide, and titania. Here, when the total components constituting the adhesive layer are taken as 100% by mass, the content of PVdF can be approximately 5% by mass or more, preferably 10% by mass or more, more preferably 15% by mass or more, and even more preferably 20% by mass or more. The content of PVdF may be 100% by mass, or, for example, 90% by mass or less, and preferably 80% by mass or less.

[0085] As a preferred embodiment, the fixing member may be arranged as shown in FIG. 15. In FIG. 15, the fixing members 1d and 1e are arranged from the flat outer surface 27a to the flat outer surface 27f so as to cover the lower part and the vicinity of the center of the positive electrode second current collecting portion 52 of the three electrode bodies 20a, 20b, and 20c. The fixing members 1f and 1g are arranged from the flat outer surface 27a to the flat outer surface 27f so as to cover the lower part and the vicinity of the center of the negative electrode second current collecting portion 62 of the three electrode bodies 20a, 20b, and 20c. Furthermore, the auxiliary fixing members 1h, 1i, and 1j are arranged in a U-shape in the part other than the positive electrode second current collecting portion 52 and the negative electrode second current collecting portion 62 from the flat outer surface 27a to the flat outer surface 27f. This can suitably suppress the movement of the electrode body 20b in the longitudinal direction. In FIG. 15, the fixing members 1d, 1e, 1h and the fixing members 1f, 1g, 1i are arranged symmetrically with respect to the center line CL passing through the center of the battery case 10 in the Y direction, but this is not limited thereto and they may be arranged asymmetrically with respect to CL. In FIG. 15, the auxiliary fixing member 1j is arranged at the center of La, but this is not limited thereto and they may be arranged shifted appropriately in the left-right direction (left-right direction in FIG. 15). As shown in FIG. 15, from the viewpoint of effectively suppressing the movement of the electrode body 20b in the longitudinal direction, it is preferable that all the auxiliary fixing members 1h, 1i, 1j are arranged, but they may be reduced appropriately. Although not shown in FIG. 15, the fixing members may be arranged in a U-shape so as to cover the sealing plate 14 from the flat outer surface 27a to the flat outer surface 27f.

[0086] In the above embodiment, the battery 100 including three electrode bodies has been described, but is not limited thereto. For example, a plurality of (i.e., two or more) electrode bodies may be disposed between the electrode body 20a and the electrode body 20c. In this case, it is preferable that the electrode body 20a, the plurality of electrode bodies disposed between the electrode body 20a and the electrode body 20c, and the electrode body 20c are fixed. As an example of a method for fixing the electrode bodies to each other, a method of disposing a fixing member in a U-shape so as to cover the positive electrode second current collecting portion and / or the negative electrode second current collecting portion of each electrode body from the flat outer surface 27a to the flat outer surface 27f can be mentioned. In addition, the flat outer surface of each electrode body may be provided with an adhesive layer as described above. This can suitably suppress the movement of each electrode body in the longitudinal direction.

[0087] In the above embodiment, the battery 100 having three electrode bodies is described, but is not limited thereto. For example, the battery may have only one electrode body. For example, when the battery has the electrode body 20a, the fixing member can be arranged in an L-shape from the flat outer surface 27a to the positive electrode second current collecting portion 52. Alternatively, the fixing member can be arranged in a U-shape from the flat outer surface 27a to the flat outer surface 27b. Here, when the fixing member is arranged in a U-shape or other tensioned state, the electrode body 20a is firmly fixed to the positive electrode second current collecting portion 52, which is preferable. In addition, the positive electrode second current collecting portion 52 is described above, but the same is naturally true for the negative electrode second current collecting portion 62. Note that these are only examples, and various other forms are possible. [Explanation of symbols]

[0088] 1, 1a to 1g Fixing members 1h~1j Auxiliary fixing members 10 Battery case 12 Exterior body 14 Sealing plate 20 Electrode group 20a (first electrode body), 20b, 20c (second electrode body) Electrode body 27 Flat outer surface 23 Positive electrode tab group (electrode tab group) 25 Negative electrode tab group (electrode tab group) 30 Positive terminal (terminal) 40 Negative terminal (terminal) 50 Positive electrode current collector 51 Positive electrode first current collecting part (current collecting part) 52 Positive electrode second current collector 60 Negative electrode current collector 61 Negative electrode first current collector 62 Negative electrode second current collector 70 Positive electrode insulating material (insulating material) 70a Base 70b Protrusion 80 Negative electrode insulating material (insulating material) 80a Base 80b Protrusion 100 batteries

Claims

1. A battery comprising: a first electrode body having a flat hexahedral shape including a positive electrode and a negative electrode and having a pair of rectangular flat outer surfaces; and a battery case housing the first electrode body, the battery case includes an exterior body having a bottom wall, a pair of first side walls extending from the bottom wall and facing each other, a pair of second side walls extending from the bottom wall and facing each other, and an opening facing the bottom wall, and a sealing plate that seals the opening, A positive electrode terminal and a negative electrode terminal are attached to the sealing plate, a positive electrode tab group including a plurality of positive electrode tabs is disposed on one of the pair of second side walls, a negative electrode tab group including a plurality of negative electrode tabs is disposed on the other second side wall side of the pair of second side walls, the positive electrode tab group and the positive electrode terminal are electrically connected via a positive electrode current collecting portion, and the positive electrode tab group is joined to the positive electrode current collecting portion in a curved state so as to extend along one of the pair of second side walls, In the positive electrode current collecting portion, a region facing one of the pair of second side walls includes a first region and a second region, the first region is disposed at a position farther from the one second side wall of the pair of second side walls than the second region is disposed in a direction perpendicular to the one second side wall of the pair of second side walls, the negative electrode tab group and the negative electrode terminal are electrically connected via a negative electrode current collecting portion, and the negative electrode tab group is joined to the negative electrode current collecting portion in a curved state so as to extend along the other of the pair of second side walls, In the negative electrode current collecting portion, a region facing the other of the pair of second side walls includes a third region and a fourth region, the third region is disposed at a position farther from the other second side wall of the pair of second side walls than the fourth region is in a direction perpendicular to the other second side wall of the pair of second side walls, Here, a fixing member is arranged from at least one of the pair of flat outer surfaces to the first region of the positive electrode current collector or the third region of the negative electrode current collector.

2. The battery according to claim 1 , wherein the fixing member includes a substrate and an adhesive layer formed on the substrate.

3. the positive electrode tab group is joined to the positive electrode current collecting portion in a state where the positive electrode tab group is collected on one of the pair of flat outer surfaces, The battery according to claim 1 , wherein the negative electrode tab group is joined to the negative electrode current collector in a state where the negative electrode tab group is gathered on one of the pair of flat outer surfaces.

Citation Information

Patent Citations

  • Nonaqueous electrolyte secondary battery, and separator

    JP2011138762A

  • Battery including fixing member

    JP2022188665A

  • Secondary battery and method of manufacturing same

    WO2021060010A1

  • Power storage device

    JP2017050069A