Pressing and cutting device, manufacturing method of lamination type electrode and manufacturing method of lamination type battery

The push-splitting device with controlled blade angles and clearance lengths addresses the issue of interlayer short circuits and cracks in electrode cutting, enabling precise and reliable separation of laminated electrode sheets.

JP2024154792AActive Publication Date: 2024-10-31TOYOTA JIDOSHA KK
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023068857
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-19
Publication Date
2024-10-31
Estimated Expiration
2043-04-19

AI Technical Summary

Technical Problem

Existing electrode cutting devices risk interlayer short circuits and cracks during the separation of laminated electrode sheets due to rubbing surfaces and shearing actions, which are not effectively addressed by conventional cutting methods.

Method used

A push-splitting device with specific blade angles and clearance lengths is employed to minimize interlayer short circuits and cracks by using a cutting edge tool with a rake angle of 15° to 30° and a clearance length of 10% to 35% of the electrode sheet length, along with a pressing mechanism to separate the laminated electrode sheets.

Benefits of technology

The device effectively separates laminated electrode sheets into desired dimensions while suppressing interlayer short circuits and cracks, ensuring the integrity of the electrode structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154792000001_ABST
    Figure 2024154792000001_ABST
Patent Text Reader

Abstract

To provide a pressing and cutting device which can separate lamination type electrode sheets into the desired dimensions by suppressing the occurrence of interlayer short circuits and cracks.SOLUTION: A pressing and cutting device according to the present disclosure includes a placement table on which lamination type electrode sheets are placed, a pressing mechanism which presses the lamination type electrode sheets, and at least one cutting blade tool. The pressing and cutting device according to the present disclosure presses, bends and breaks a portion of protruding portions protruding from the placement table and the pressing mechanism of the lamination type electrode sheets pressed by the pressing mechanism in the second direction orthogonal to the first direction with the cutting blade tool that moves along the first direction relative to the placement table. The angle of a blade part of the cutting blade tool relative to the second direction is between 15° and 30°. The angle of the blade part relative to the first direction is an acute angle. The length in the second direction of a clearance between the blade part and the end on the cutting blade tool side of the placement table is 10% to 35% of the length in the first direction of the lamination type electrode sheets.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a press-breaking device, a method for manufacturing a stacked electrode, and a method for manufacturing a stacked battery. [Background technology]

[0002] In recent years, there has been an increasing demand for high-output lithium secondary batteries as large-scale energy sources for electric vehicles, etc. In general, in the manufacture of lithium secondary batteries, in order to improve the energy density, parts that do not function as power generating elements of the lithium secondary battery (for example, parts with poor coating, parts with lamination misalignment, etc.) are cut off.

[0003] Patent Document 1 discloses an electrode cutting device. The cutting device disclosed in Patent Document 1 cuts a sheet-like electrode having an active material layer on a foil-like current collector by a shearing action based on the meshing of a lower blade and an upper blade of a straight blade type arranged opposite to each other, by the approaching and separating action of the two. The upper blade has a cutting edge at the outer corner formed by the blade side surface of the upper blade and the work contact surface. The cutting edge angle of this cutting edge is set to 90°. The upper blade has a specific flank surface. Specifically, there is no clearance between the lower blade and the upper blade.

[0004] 11A to 11C show the operation process of the cutting device disclosed in Patent Document 1. In Fig. 11A to 11C, reference numeral 901 denotes a current collector, reference numeral 902 denotes an active material layer, and reference numeral 903 denotes an active material layer.

[0005] In Patent Document 1, an electrode base material 900 is disposed between an upper blade 910 and a lower blade 920 that are spaced apart in the vertical direction, and the electrode base material 900 is separated into a first electrode 900A and a second electrode 900B by lowering the upper blade 910. In detail, when the upper blade 910 is lowered, the upper blade 910 comes into contact with the electrode base material 900 as shown in FIG. 11A. Then, as shown in FIG. 11B, the upper blade 910 presses down the electrode base material 900. Then, as shown in FIG. 11C, the cutting edge 911 of the upper blade 910 comes into mesh with the cutting edge 921 of the lower blade 920. At this time, the electrode 930 is cut from the electrode base material 900 by a shearing action based on the meshing between the cutting edge 911 of the upper blade 910 and the cutting edge 921 of the lower blade 920. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2015-153538 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, when cutting the electrode base material 900 using the cutting device disclosed in Patent Document 1, as shown in Figures 11B and 11C, the sheared surface S900A of the first electrode 900A and the blade side surface S910 of the upper blade 910 may rub against each other. Furthermore, the sheared surface S900A of the first electrode 900A and the sheared surface S900B of the second electrode 900B may rub against each other. This may cause the constituent layers of the first electrode 900A to mix with each other on the surface of the sheared surface S900A of the first electrode 900A, resulting in a short circuit between the constituent layers of the first electrode 900A (hereinafter, also referred to as an "interlayer short circuit").

[0008] The present disclosure has been made in consideration of the above circumstances. An object of the present disclosure is to provide a press-and-break device capable of separating a laminated electrode sheet into pieces of desired dimensions while suppressing the occurrence of interlayer short circuits and cracks, a method for manufacturing a laminated electrode, and a method for manufacturing a laminated battery. [Means for solving the problem]

[0009] Means for solving the above problems include the following embodiments.

[0010] <1> The press-breaking device according to the first aspect of the present disclosure is a mounting table for mounting the laminated electrode sheet; a pressing mechanism that presses the laminated electrode sheet placed on the mounting table; At least one cutting tool; Equipped with A press-and-break device that presses and bends and breaks a part of a protruding portion of the laminated electrode sheet that protrudes from the mounting table and the pressing mechanism in a second direction perpendicular to the first direction, the protruding portion being pressed by the pressing mechanism in a second direction perpendicular to the first direction, by the at least one cutting blade tool that moves relative to the mounting table along a first direction, The angle of the cutting edge of the cutting edge tool with respect to the second direction is 15° to 30°, The angle of the blade portion with respect to the first direction is an acute angle, In the press-cutting device, the length in the second direction of the clearance between the blade portion and the end of the placement table on the cutting blade tool side is 10% to 35% of the length in the first direction of the laminated electrode sheet.

[0011] A "laminated electrode sheet" has at least a first active material sheet, a second active material sheet, and an insulating sheet that electrically insulates the first active material sheet and the second active material sheet. The insulating sheet is interposed between the first active material sheet and the second active material sheet in a first direction. The "edge portion" refers to the rake face of the cutting edge tool and the flank face of the cutting edge tool.

[0012] In the first embodiment, when the laminated electrode sheet is separated into at least two pieces, a cutting blade tool moving along a first direction relative to the mounting table comes into contact with the protruding portion of the laminated electrode sheet pressed by the pressing mechanism, and bends the protruding portion. The blade of the cutting blade tool bites into the surface of the protruding portion while the protruding portion is in a bent state. When the cutting blade tool further moves along the first direction, a crack is generated starting from the portion of the protruding portion into which the blade of the cutting blade tool has bitten (hereinafter also referred to as the "bite line"), and a part of the protruding portion is separated. This results in a laminated electrode in which the end of the laminated electrode sheet on the cutting blade tool side (hereinafter "fracture") is separated. In the first embodiment, the angle of the blade of the cutting blade tool with respect to the second direction (hereinafter also referred to as the "rake angle") is 15° or less. This makes it easier for the blade of the cutting blade tool to bite into the protruding portion than when the rake angle is less than 15°. Therefore, cracks are more likely to occur in the protruding portion starting from the bite line. In other words, the shape of the end of the obtained laminated electrode on the cutting blade tool side when viewed from the first direction is less likely to be saw-toothed. As a result, the press-cutting device of the first embodiment can separate the laminated electrode sheet into desired dimensions. In the first embodiment, the rake angle is 30° or less. This makes it harder for the blade of the cutting blade tool to bite into the protruding portion than when the rake angle is more than 30°. Therefore, the sharp blade itself is less likely to cut off the protruding portion. In other words, when a part of the protruding portion is separated, the blade of the cutting blade tool and the separated surface of the protruding portion are less likely to rub against each other. As a result, the press-cutting device of the first embodiment can suppress the occurrence of interlayer short circuits. In the first embodiment, the angle of the blade of the cutting tool with respect to the first direction (hereinafter also referred to as the "clearance angle") is an acute angle. This makes it less likely that the separation surface of the resulting laminated electrode will rub against the cutting tool than when the clearance angle is not acute. As a result, the press-cutting device of the first embodiment can suppress the occurrence of interlayer short circuits. In the first embodiment, the length in the second direction of the clearance between the blade portion and the end of the mounting table on the cutting blade tool side (hereinafter also referred to as the "clearance length") is 10% or more of the length in the first direction of the laminated electrode sheet. This makes it easier for the protruding portion to be pushed and bent by the moving cutting blade tool than when the clearance length is less than 10% of the length in the first direction of the laminated electrode sheet. Therefore, in the process of separating the broken material from the laminated electrode sheet, the separation surface of the laminated electrode is less likely to rub against each of the cutting blade tool and the broken material. As a result, the press-cutting device of the first embodiment can suppress the occurrence of interlayer short circuits. In the first embodiment, the length of the clearance is 35% or less of the length in the first direction of the laminated electrode sheet. This makes the bending moment centered on the part of the protruding part near the end of the mounting table on the cutting blade tool side smaller than when the length of the clearance is more than 35% of the length in the first direction of the laminated electrode sheet. In other words, when the moving cutting blade tool is bending the protruding part, stress is less likely to concentrate on the part of the laminated electrode sheet near the end of the pressing mechanism on the cutting blade tool side. Therefore, cracks are less likely to occur on the surface of the part of the laminated electrode sheet near the end of the pressing mechanism on the cutting blade tool side. If a crack occurs in the laminated electrode, the laminated electrode may break during charging and discharging of the laminated electrode. As described above, the press-cutting device of the first aspect can separate the laminated electrode sheet into pieces of desired dimensions while suppressing the occurrence of interlayer short circuits and cracks.

[0013] <2> The press-breaking device according to the second aspect of the present disclosure is the pressing mechanism has a contact member that comes into contact with the laminated electrode sheet when pressing the laminated electrode sheet, In the second direction, a position of an end of the contact member on the cutting edge tool side is the same position as a position of an end of the table on the cutting edge tool side, or is a position closer to the cutting edge tool than a position of an end of the table on the cutting edge tool side. <1> 2 is a press-breaking device according to the first embodiment.

[0014] In the second embodiment, when the moving cutting blade tool presses and bends the protruding portion, stress is less likely to concentrate in a portion of the laminated electrode sheet near the cutting blade tool side end of the pressing mechanism than when the cutting blade tool side end of the contact member is located on the opposite side of the cutting blade tool side from the cutting blade tool side end of the mounting table in the second direction. As a result, the pressing and splitting device of the second embodiment can separate the laminated electrode sheet while further suppressing the occurrence of cracks.

[0015] <3> The press-breaking device according to the third aspect of the present disclosure is The angle of the blade with respect to the first direction is 5° to 15°. <1> or <2> 2 is a press-breaking device according to the first embodiment.

[0016] In the third embodiment, the laminated electrode obtained by separating the broken material is less likely to rub against the cutting tool than when the clearance angle is outside the range of 5° to 15°. As a result, the press-cutting device of the third embodiment can separate the laminated electrode sheet while further suppressing the occurrence of interlayer short circuits.

[0017] <4> The fourth aspect of the present disclosure relates to a press-breaking device. The length of the clearance in the second direction is 20 μm to 50 μm. <1> ~ <3> 1. The pressing and cracking device according to claim 1 ,

[0018] The press-breaking device of the fourth embodiment can separate the specific laminated electrode sheet into desired dimensions while suppressing the occurrence of interlayer short circuits and cracks, compared to when the clearance length is outside the range of 20 μm to 50 μm. The specific laminated electrode sheet is formed by laminating a first active material layer, a solid electrolyte layer, and a second active material layer in this order along a first direction on both sides of a first current collector. The length (thickness) of the specific laminated electrode sheet in the first direction is, for example, 0.2 mm.

[0019] <5> The press-breaking device according to the fifth aspect of the present disclosure is a lower holder; and an upper holder disposed opposite the lower holder and movable relative to the lower holder along the first direction, the first direction is parallel to the direction of gravity; The cutting edge tool and the pressing mechanism are attached to the upper holder, The mounting table is attached to the lower die holder. <1> ~ <4> 1. The pressing and cracking device according to claim 1 ,

[0020] In the fifth aspect, the laminated electrode sheet is disposed between the cutting blade tool and the mounting table that are spaced apart in the first direction, and the upper holder is lowered to press and restrain the laminated electrode sheet with the pressing mechanism, so that a part of the protruding part of the laminated electrode sheet can be separated. As a result, the pressing and splitting device of the fifth aspect can efficiently separate the laminated electrode sheet with a simple configuration.

[0021] <6> The press-breaking device according to the sixth aspect of the present disclosure is The cutting edge tool is an upper blade, The mounting table is a lower blade. <5> 2 is a press-cutting device according to the first embodiment.

[0022] The press-cutting device of the sixth embodiment can efficiently separate the laminated electrode sheet.

[0023] <7> A method for producing a laminated electrode according to a seventh aspect of the present disclosure includes the steps of: The above <1> ~ <6> A method for producing a laminated electrode by using the press-cutting device according to any one of the above items, Preparing the laminated electrode sheet; placing the laminated electrode sheet on the mounting table so that the protruding portion is formed; and moving the at least one cutting edge tool in the first direction to bend and split the protruding portion of the laminated electrode sheet.

[0024] The term "laminated electrode" refers to an electrode in which a first active material layer in a sheet shape, an insulating layer in a sheet shape, a second active material layer in a sheet shape, and a second current collector are laminated in this order along the first direction on both sides of a first current collector in a sheet shape. The first current collector sheet, the first active material sheet, the insulating sheet, and the second active material sheet included in the laminated electrode sheet are split to become the first current collector, the first active material layer, the insulating layer, and the second active material layer included in the laminated electrode. The "insulating layer" includes a solid electrolyte layer of a lithium secondary battery using a solid electrolyte, and a separator of a lithium secondary battery using a nonaqueous electrolyte.

[0025] The electrode manufacturing method of the seventh aspect can manufacture a laminated electrode sheet having desired dimensions while further suppressing the occurrence of interlayer short circuits and cracks.

[0026] <8> In an eighth aspect of the present disclosure, a method for producing a laminated electrode includes the steps of: the laminated electrode sheet is formed by laminating a first active material sheet, a solid electrolyte sheet, and a second active material sheet in this order on both sides of a first current collector sheet along the first direction; and laminating a second current collector on a second active material layer obtained from the second active material sheet by performing the pressing and breaking. <7> 2 is a method for producing the electrode according to the present invention.

[0027] The method for producing a laminated electrode according to the eighth embodiment can produce a laminated electrode having desired dimensions while suppressing the occurrence of interlayer short circuits and cracks.

[0028] <9> A method for producing a stacked battery according to a ninth aspect of the present disclosure includes the steps of: The above <7> or <8> A method for producing a stacked battery, comprising producing a stacked electrode by the method for producing a stacked electrode according to the above-mentioned item 1.

[0029] "Stacked battery" refers to a battery that includes at least one stacked electrode.

[0030] The manufacturing method of the stacked battery of the ninth aspect makes it possible to manufacture a stacked battery that is equipped with stacked electrodes having desired dimensions and that is free from interlayer short circuits and cracks. Effect of the Invention

[0031] According to the present disclosure, there are provided a press-and-break device capable of separating a laminated electrode sheet into pieces of desired dimensions while suppressing the occurrence of interlayer short circuits and cracks, a method for manufacturing a laminated electrode, and a method for manufacturing a laminated battery. [Brief description of the drawings]

[0032] [Figure 1] FIG. 1 is a cross-sectional view of a push-cutting device according to an embodiment of the present disclosure. [Diagram 2] FIG. 2 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure. [Diagram 3] FIG. 3 is a cross-sectional view of a push-cutting device according to an embodiment of the present disclosure. [Figure 4] FIG. 4 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure. [Diagram 5] FIG. 5 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure. [Figure 6] FIG. 6 is a cross-sectional view of a push-cutting device according to an embodiment of the present disclosure. [Figure 7] FIG. 7 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure. [Figure 8] FIG. 8 is a cross-sectional view of a laminated electrode sheet in an embodiment of the present disclosure. [Figure 9] FIG. 9 is a top view of a laminated electrode of a comparative example. [Figure 10] FIG. 10 is a top view of a laminated electrode of a comparative example. [Figure 11A] FIG. 11A is a diagram for explaining the operation process of a conventional cutting device. [Figure 11B] FIG. 11B is a diagram for explaining the operation process of the conventional cutting device. [Figure 11C]FIG. 11C is a diagram for explaining the operation process of the conventional cutting device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0033] In the present disclosure, a numerical range indicated using "~" means a range including the numerical values ​​described before and after "~" as the minimum and maximum values, respectively. In the numerical ranges described in stages in the present disclosure, the upper limit or lower limit described in a certain numerical range may be replaced with the upper limit or lower limit of another numerical range described in stages. In the present disclosure, a combination of two or more preferred embodiments is a more preferred embodiment. In the present disclosure, the term "process" includes not only an independent process, but also a process that cannot be clearly distinguished from other processes, as long as the intended purpose of the process is achieved.

[0034] Hereinafter, embodiments of the press-breaking device, the manufacturing method of the stacked electrode, and the manufacturing method of the stacked battery of the present disclosure will be described with reference to the drawings. In the drawings, the same or corresponding parts are designated by the same reference characters, and the description will not be repeated.

[0035] (1) Press-breaking device The press-breaking device 1 according to the embodiment of the present disclosure presses and bends the laminated electrode sheet 4 to break the laminated electrode sheet 4. This results in a laminated electrode precursor 40. The laminated electrode precursor 40 is obtained by removing a portion 41 (hereinafter, also referred to as "broken material 41") that does not function as a power generating element from the laminated electrode sheet 4. Details of the laminated electrode sheet 4 will be described later.

[0036] As shown in Fig. 1, the press-breaking device 1 includes an upper die 2 and a lower die 3. The upper die 2 is disposed opposite the lower die 3. The upper die 2 is movable relative to the lower die 3 along the direction of gravity. The upper die 2 has two linear upper blades 21, which are an example of at least one cutting blade tool.

[0037] In this embodiment, the direction of gravity is defined as the lower side, and the opposite side is defined as the upper side. One side of the two upper blades 21 is defined as the right side, and the opposite side is defined as the left side. One side in the longitudinal direction of the upper blade 21 is defined as the front side, and the opposite side is defined as the rear side. The up-down direction, which is an example of the first direction, the left-right direction, which is an example of the second direction, and the front-rear direction are mutually perpendicular. Note that these directions do not limit the orientation of the pressing and splitting device of the present disclosure when it is used.

[0038] (1.1) Upper mold The upper die 2 has two upper blades 21, a pressing mechanism 22, multiple guide pins 23, and an upper die holder 24. The two upper blades 21, the pressing mechanism 22, and the multiple guide pins 23 are attached to the upper die holder 24. The pressing mechanism 22 is located in the center of the upper die holder 24 in the left-right direction. The two upper blades 21 are located on both sides of the pressing mechanism 22 in the left-right direction. The multiple guide pins 23 are located outside the pressing mechanism 22 in the left-right direction.

[0039] (1.1.1) Upper blade The upper blade 21 is wedge-shaped as shown in Fig. 2. The upper blade 21 has a blade portion 210 extending in the front-rear direction. The upper blade 21 is formed with a rake face S210A and a clearance face S210B. The blade portion 210 is made up of the rake face S210A and the clearance face S210B.

[0040] The angle θA of the blade portion 210 of the upper blade 21 relative to the left-right direction (hereinafter also referred to as "rake angle θA") is 15° to 30°.

[0041] The angle θB of the blade portion 210 of the upper blade 21 with respect to the vertical direction (hereinafter also referred to as "clearance angle θB") is an acute angle. In the press-breaking device 1, the clearance angle θB is 5° to 15°.

[0042] The length of the upper blade 21 in the front-rear direction is appropriately selected depending on the size of the laminated electrode sheet 4, and may be longer than the length of the laminated electrode sheet 4 in the front-rear direction. The material of the upper blade 21 is not particularly limited and may be appropriately selected depending on the type of the laminated electrode sheet 4, and examples of the material include steel and superhard metal.

[0043] (1.1.2) Pressing mechanism The pressing mechanism 22 presses the laminated electrode sheet 4 placed on the lower blade 31 included in the lower die 3. The pressing mechanism 22 has a contact member 221 and an elastic member 222. An upper end of the elastic member 222 is fixed to the upper die holder 24. A lower end of the elastic member 222 is fixed to the contact member 221.

[0044] The contact member 221 comes into contact with the laminated electrode sheet 4 when the pressing mechanism 22 presses the laminated electrode sheet 4. The contact member 221 is a flat plate. The left-right length L1 (see FIG. 1) of the contact member 221 is shorter than the left-right length L2 (see FIG. 1) of the laminated electrode sheet 4, and is appropriately selected according to the length L2 of the laminated electrode sheet 4. The material of the contact member 221 is not particularly limited, and examples thereof include resin and metal.

[0045] The elastic member 222 applies a biasing force to the contact member 221 when the pressing mechanism 22 presses the laminated electrode sheet 4. The vertical length of the elastic member 222 may be such that the position of the lower part BS221 of the contact member 221 is located lower than the position of the lower part BS21 of the upper blade 21 when the contact member 221 is not in contact with the laminated electrode sheet 4. The elastic member 222 may be any member that is expandable and contractable in the vertical direction, and examples of the elastic member 222 include a coil spring. The material of the elastic member 222 is not particularly limited, and examples of the material include resin and metal.

[0046] (1.1.3) Guide pin The guide pins 23 are used to vertically control the direction in which the upper die 2 moves relative to the lower die 3. Each of the multiple guide pins 23 extends downward from the lower surface S24 of the upper die holder 24. The number of guide pins 23 should be at least two and is appropriately selected according to the size of the laminated electrode sheet 4. The material of the guide pins 23 is not particularly limited, and examples include resin and metal.

[0047] (1.1.4) Upper holder The upper die holder 24 holds the two upper blades 21, the pressing mechanism 22, and a plurality of guide pins 23. The upper die holder 24 is a plate-like object. The material of the upper die holder 24 is appropriately selected depending on the size of the laminated electrode sheet 4, etc. The material of the upper die holder 24 is not particularly limited, and examples thereof include resin and metal.

[0048] (1.2) Lower mold The lower die 3 has a lower blade 31, which is an example of a mounting base, and a lower die holder 32. The lower blade 31 is attached to the lower die holder 32. The lower blade 31 is located in the center of the lower die holder 32 in the left-right direction.

[0049] (1.2.1) Lower blade The lower blade 31 places the laminated electrode sheet 4 on it. The lower blade 31 is a plate-like object. The lower blade 31 has a linear blade portion 310 extending in the front-rear direction. The lower blade 31 has an end surface S310A and a contact surface S310B that contacts the laminated electrode sheet 4. The blade portion 310 is composed of the end surface S310A and the contact surface S310B. The angle θC between the end surface S310A and the contact surface S310B is 90°. The length of the lower blade 31 in the front-rear direction is appropriately selected according to the size of the laminated electrode sheet 4, and may be longer than the length of the laminated electrode sheet 4 in the front-rear direction. The material of the lower blade 31 is not particularly limited and is appropriately selected according to the type of the laminated electrode sheet 4, and examples of the material include steel and superhard metal.

[0050] (1.2.2) Lower holder The lower die holder 32 holds the lower blade 31. The lower die holder 32 is a plate-like object. A plurality of guide holes H32 are formed in the lower die holder 32. The guide pins 23 of the upper die 2 are inserted into the guide holes H32. The guide holes H32 are formed along the up-down direction and pass through the lower die holder 32. The positions of the plurality of guide holes H32 correspond to the positions of the plurality of guide pins 23. The material of the lower die holder 32 is not particularly limited, and examples thereof include resin and metal.

[0051] (1.3) Layout The left-right length L3 (see FIG. 2) of the clearance between the blade portion 210 of the upper blade 21 and the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310) is 10% to 35% of the left-right length L4 (see FIG. 2) of the laminated electrode sheet 4. In other words, in the press-cutting device 1, the clearance length L3 is 20 μm to 50 μm.

[0052] In the left-right direction, the position of the end 2210 of the contact member 221 on the upper blade 21 side is the same as the position of the end of the lower blade 31 on the upper blade 21 side (ie, the blade portion 310).

[0053] (1.4) Driving means The press-breaking device 1 may or may not be equipped with a known driving means (e.g., a hydraulic cylinder, a driving motor, etc.). When the press-breaking device 1 is equipped with a driving means, the upper mold 2 may be moved relatively to the lower mold 3 by the driving means. When the press-breaking device 1 is not equipped with a driving means, the upper mold 2 may be moved relatively to the lower mold 3 manually.

[0054] (1.5) Operation The operation of the press-breaker 1 will be described with reference to FIGS.

[0055] First, as shown in FIG. 1, the upper die 2 and the lower die 3 are vertically separated from each other, and the laminated electrode sheet 4 is placed on the lower blade 31 of the lower die 3 . Next, when the upper die 2 is moved downward, each of the multiple guide pins 23 of the upper die 2 is inserted into each of the multiple guide holes H32 of the lower die 3. When the upper die 2 is further moved downward, the contact member 221 of the pressing mechanism 22 comes into contact with the laminated electrode sheet 4, as shown in Fig. 2 and Fig. 3. As a result, the contact member 221 of the pressing mechanism 22 presses and restrains the laminated electrode sheet 4 by the biasing force of the elastic member 222. At this time, as shown in Fig. 2, both end portions R4 in the left-right direction of the laminated electrode sheet 4 (hereinafter, also referred to as "protruding portions R4") protrude from the contact member 221 and the lower blade 31 of the pressing mechanism 22. At this point, the upper blade 21 is not in contact with the laminated electrode sheet 4. Next, when the upper die 2 is further moved downward, the blade portion 210 of the upper blade 21 comes into contact with the protruding portion R4 of the laminated electrode sheet 4 restrained by the pressing mechanism 22. Next, when the upper die 2 is moved further downward, as shown in Fig. 4, the protruding portion R4 is pressed downward by the upper blade 21, following the movement of the upper blade 21. At this time, the blade portion 210 of the upper blade 21 bites into the upper surface TS4 of the protruding portion R4 while the protruding portion R4 is being pressed and bent. As a result, a bite line X1 is formed on the upper surface TS4 of the protruding portion R4. The bite line X1 extends linearly in the front-rear direction from the front end to the rear end of the protruding portion R4. Next, when the upper mold 2 is moved further downward, the crack X2 originating from the bite line X1 of the protruding portion R4 reaches the lower surface BS4 of the protruding portion R4 as shown in Fig. 5. In other words, a crack occurs in the laminated electrode sheet 4 originating from the bite line X1. Next, when the upper die 2 is moved further downward, the broken material 41 is separated from the laminated electrode sheet 4 as shown in Fig. 6. This results in a laminated electrode precursor 40. When the broken material 41 is separated from the laminated electrode sheet 4, a portion R40 protruding from the contact member 221 and the lower blade 31 of the laminated electrode precursor 40 (hereinafter also referred to as "protruding portion R40") is released from the pressure of the upper blade 21 and deforms so as to return to the state before the laminated electrode sheet 4 was pressed by the upper blade 21 as shown in Fig. 7.

[0056] (1.6) Multilayer electrode sheet 8, the laminated electrode sheet 4 is formed by stacking a negative electrode active material sheet 43, which is an example of a first active material sheet, a solid electrolyte sheet 44, and a positive electrode active material sheet 45, which is an example of a second active material sheet, in this order along the top-bottom direction on both sides of a negative electrode current collector sheet 42, which is an example of a first current collector sheet. The laminated electrode sheet 4 does not include a negative electrode current collector sheet on the positive electrode active material sheet 45.

[0057] The laminated electrode sheet 4 has non-functioning regions NR4 (hereinafter also referred to as "non-power generation regions NR4") that do not function as power generation elements at both left and right ends. In the non-power generation regions NR4, the negative electrode active material sheet 43 and the positive electrode active material sheet 45 do not face each other with the solid electrolyte sheet 44 interposed therebetween in the vertical direction.

[0058] The length L4 of the laminated electrode sheet 4 in the up-down direction is, for example, 0.2 mm. The length of the laminated electrode sheet 4 in the front-rear direction is, for example, 70 mm.

[0059] (1.6.1) Negative electrode current collector sheet Examples of the material of the negative electrode current collector sheet 42 include stainless steel, aluminum, copper, nickel, iron, titanium, and carbon, and copper is preferable. The shape of the negative electrode current collector sheet 42 is, for example, a foil shape or a mesh shape. The negative electrode current collector sheet 42 may have a configuration in which a buffer layer, an elastic layer, or a PTC (Positive Temperature Coefficient) thermistor layer is disposed on the surface.

[0060] (1.6.2) Negative electrode active material sheet The negative electrode active material sheet 43 contains a negative electrode active material. Examples of the negative electrode active material include Li-based active materials such as metallic lithium, carbon-based active materials such as graphite, oxide-based active materials such as lithium titanate, and Si-based active materials such as simple silicon.

[0061] The negative electrode active material sheet 43 may contain at least one of a negative electrode solid electrolyte, a conductive assistant, and a binder, as necessary. Examples of the negative electrode solid electrolyte and binder include the same solid electrolyte and binder as those exemplified in the solid electrolyte layer contained in the solid electrolyte sheet 44 described later.

[0062] Examples of the conductive assistant include carbon materials, metal materials, and conductive polymer materials. Examples of the carbon materials include carbon black (e.g., acetylene black, furnace black, ketjen black, etc.), fibrous carbon (e.g., vapor-phase carbon fiber, carbon nanotube, carbon nanofiber, etc.), graphite, and carbon fluoride. Examples of the metal materials include metal powder (e.g., aluminum powder, etc.), conductive whiskers (e.g., zinc oxide, potassium titanate, etc.), conductive metal oxides (e.g., titanium oxide, etc.). Examples of the conductive polymer materials include polyaniline, polypyrrole, and polythiophene. Only one type of conductive assistant may be used alone, or two or more types may be mixed and used.

[0063] (1.6.3) Solid electrolyte sheet The solid electrolyte sheet 44 preferably includes one selected from the group consisting of a sulfide solid electrolyte, an oxide solid electrolyte, and a halide solid electrolyte.

[0064] The sulfide solid electrolyte preferably contains sulfur (S) as a main component of an anion element, and further preferably contains, for example, Li element and A element. The A element is at least one selected from the group consisting of P, As, Sb, Si, Ge, Sn, B, Al, Ga, and In. The sulfide solid electrolyte may further contain at least one of O and a halogen element. Examples of the halogen element (X) include F, Cl, Br, and I. The composition of the sulfide solid electrolyte is not particularly limited, and may be, for example, xLi 2 S·(100-x)P 2 S 5 (70≦x≦80), yLiI・zLiBr・(100-yz)(xLi 2 S (1-x)P 2 S 5 ) (0.7≦x≦0.8, 0≦y≦30, 0≦z≦30). The sulfide solid electrolyte may have a composition represented by the following general formula (1). Formula (1): Li 4-x Ge 1-x P x S 4(0 <x<1) In formula (1), at least a portion of Ge may be substituted with at least one selected from the group consisting of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. At least a portion of P may be substituted with at least one selected from the group consisting of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. At least a portion of Li may be substituted with at least one selected from the group consisting of Na, K, Mg, Ca, and Zn. At least a portion of S may be substituted with a halogen. The halogen is at least one of F, Cl, Br, and I.

[0065] The oxide solid electrolyte preferably contains oxygen (O) as a main component of the anion element, and may contain, for example, Li, Q element (Q represents at least one of Nb, B, Al, Si, P, Ti, Zr, Mo, W, and S), and O. Examples of the oxide solid electrolyte include garnet-type solid electrolytes, perovskite-type solid electrolytes, Nasicon-type solid electrolytes, Li-PO-based solid electrolytes, and Li-BO-based solid electrolytes. Examples of the garnet-type solid electrolyte include Li 7 La 3 Zr 2 O 12 , Li 7-x La 3 (Zr 2-x Nb x )O 12 (0≦x≦2), Li 5 La 3 Nb 2 O 12 Examples of perovskite-type solid electrolytes include (Li, La)TiO 3 , (Li, La)NbO 3 , (Li,Sr)(Ta,Zr)O 3 Examples of Nasicon-type solid electrolytes include Li(Al,Ti)(PO 4 ) 3 , Li(Al,Ga)(PO 4 ) 3 Li-PO solid electrolytes include Li 3 PO 4, LIPON (a compound in which part of the O of Li 3 PO 4 is replaced by N), as the Li-B-O solid electrolyte, Li 3 BO 3 , Li 3 BO 3 and compounds in which part of the O is replaced by C, etc. can be mentioned.

[0066] As the halide solid electrolyte, a solid electrolyte containing Li, M, and X (M represents at least one of Ti, Al, and Y, and X represents F, Cl, or Br) is suitable. Specifically, Li 6-3z Y z X 6 (X represents Cl or Br, and z satisfies 0 < z < 2), Li 6-(4-x)b (Ti 1-x Al x ) b F 6 (0 < x < 1, 0 < b ≤ 1.5) is preferable. Among Li 6-3z Y z X 6 , Li 3 YX 6 (X represents Cl or Br) is more preferable in terms of excellent lithium ion conductivity, and further, Li 3 YCl 6 is preferable. Also, Li 6-(4-x)b (Ti 1-x Al x ) b F 6 (0 < x < 1, 0 < b ≤ 1.5) is preferably included together with a solid electrolyte such as a sulfide solid electrolyte from the viewpoint of suppressing oxidative decomposition of the sulfide solid electrolyte, etc.

[0067] The solid electrolyte sheet 44 may have a single-layer structure or a multilayer structure of two or more layers.

[0068] The solid electrolyte sheet 44 may or may not include a binder. Examples of binders that may be included in the solid electrolyte sheet 44 include halogenated vinyl resins, rubbers, polyolefin resins, and the like. Examples of halogenated vinyl resins include polyvinylidene fluoride (PVdF), copolymers of polyvinylidene fluoride and hexafluoropropylene (PVdF-HFP), and the like. Examples of polyolefin resins include butadiene rubber (BR), acrylate butadiene rubber (ABR), styrene-butadiene rubber (SBR), acrylonitrile-butadiene rubber (NBR), butyl rubber (isobutylene-isoprene rubber), and the like. Examples of polyolefin resins include polyethylene, polypropylene, and the like. The binder may be a diene-based rubber containing a double bond in the main chain, for example, a butadiene-based rubber in which butadiene accounts for 30 mol % or more of the total.

[0069] (1.6.4) Positive electrode active material sheet The positive electrode active material sheet 45 contains a positive electrode active material. The positive electrode layer may contain at least one of a positive electrode solid electrolyte, a conductive assistant, and a binder, as necessary.

[0070] The positive electrode active material preferably contains a lithium composite oxide. The lithium composite oxide may contain at least one selected from the group consisting of F, Cl, N, S, Br, and I. The lithium composite oxide may have a crystal structure belonging to at least one space group selected from the space groups R-3m, Immm, and P63-mmc (also called P63mc or P6 / mmc). The lithium composite oxide may have an O2 type structure in which the transition metal, oxygen, and lithium are mainly arranged.

[0071] Examples of lithium composite oxides having a crystal structure belonging to R-3m include Li x Me y O α X β(Me represents at least one selected from the group consisting of Mn, Co, Ni, Fe, Al, Cu, V, Nb, Mo, Ti, Cr, Zr, Zn, Na, K, Ca, Mg, Pt, Au, Ag, Ru, W, B, Si, and P, and X represents at least one selected from the group consisting of F, Cl, N, S, Br, and I, and satisfies 0.5≦x≦1.5, 0.5≦y≦1.0, 1≦α<2, and 0<β≦1.)

[0072] Examples of lithium composite oxides having a crystal structure belonging to Immm include Li x1 M 1 A 1 2 (1.5≦x1≦2.3 is satisfied, M 1 contains at least one selected from the group consisting of Ni, Co, Mn, Cu and Fe, and A 1 contains at least oxygen, and A 1 The ratio of oxygen in the oxide is 85 atomic % or more. 2 NiO 2 ), Li x1 M 1A 1-x2 M 1B x2 O 2-y A 2 y (0≦x2≦0.5, 0≦y≦0.3, and at least one of x2 and y is not 0; M 1A represents at least one selected from the group consisting of Ni, Co, Mn, Cu, and Fe, and M 1B represents at least one selected from the group consisting of Al, Mg, Sc, Ti, Cr, V, Zn, Ga, Zr, Mo, Nb, Ta and W, and A2 represents at least one selected from the group consisting of F, Cl, Br, S and P.

[0073] Examples of lithium composite oxides having a crystal structure belonging to P63-mmc include M1 x M2 y O 2(M1 represents an alkali metal (preferably at least one of Na and K), M2 represents a transition metal (preferably at least one selected from the group consisting of Mn, Ni, Co, and Fe), and 0 < x + y ≦ 2. The composite oxide represented thereby is exemplified.)

[0074] As the lithium composite oxide having an O2-type structure, for example, Li x [Li α (Mn a Co b M c ) 1-α O 2 (0.5 < x < 1.1, 0.1 < α < 0.33, 0.17 < a < 0.93, 0.03 < b < 0.50, 0.04 < c < 0.33, and M represents at least one selected from the group consisting of Ni, Mg, Ti, Fe, Sn, Zr, Nb, Mo, W, and Bi). The composite oxide represented thereby is exemplified, and specific examples include Li 0.744 [Li 0.145 Mn 0.625 Co 0.115 Ni 0.115 O 2 and the like.

[0075] The solid electrolyte for the positive electrode preferably contains one selected from the group consisting of a sulfide solid electrolyte, an oxide solid electrolyte, and a halide solid electrolyte. As the sulfide solid electrolyte, those similar to those exemplified as the sulfide solid electrolyte contained in the solid electrolyte are included. As the oxide solid electrolyte, those similar to those exemplified as the oxide solid electrolyte contained in the solid electrolyte are included. As the halide solid electrolyte, those similar to those exemplified as the halide solid electrolyte contained in the solid electrolyte are included.

[0076] As the binder, those similar to those exemplified as the binder contained in the solid electrolyte layer are included.

[0077] (1.7) Effects As described with reference to Figs. 1 to 7, the press-breaking device 1 includes a lower blade 31, a pressing mechanism 22, and two upper blades 21. The press-breaking device 1 presses and bends a part of the protruding portion R4 of the laminated electrode sheet 4 pressed by the pressing mechanism 22 with the two upper blades 21 that move relative to the lower blade 31 in the vertical direction to break it. The rake angle θA is 15° to 30°. The relief angle θB is an acute angle. The clearance length L3 is 10% to 35% of the length L4 of the laminated electrode sheet 4. As a result, the press-cutting device 1 can separate the laminated electrode sheet 4 into pieces of desired dimensions while suppressing the occurrence of interlayer short circuits and cracks.

[0078] The inventors cut the laminated electrode sheet 4 using a device similar to the press-cutting device 1, except that the rake angle θA was changed to less than 15° (specifically, 0°, 5°, and 10°). A top view of the cut part of the cut laminated electrode sheet 4 is shown in FIG. 9. As shown in FIG. 9, it was found that the shape D1 of the end of the cut part of the laminated electrode was sawtooth-shaped. In the left-right direction, the distance L5 between the top of the convex part and the bottom of the concave part of the shape D1 of the end of the cut part of the laminated electrode was not less than 100 μm. This is presumed to be due to the following reason. That is, if the rake angle θA is less than 15°, the blade part 210 of the upper blade 21 is unlikely to bite into the protruding part R4, and the linear bite line X1 is unlikely to be stably formed. As a result, no cracks originating from the bite line X1 occurred. Therefore, it is presumed that the shape D1 of the end of the cut part of the laminated electrode was sawtooth-shaped. As a result, it was experimentally found that if the rake angle θA was less than 15°, the laminated electrode sheet 4 was difficult to separate into desired dimensions.

[0079] The inventors cut the laminated electrode sheet 4 using a device similar to the press-cutting device 1, except that the rake angle θA was changed to more than 30° (specifically, 45°, 60°). When the cut surface of the cut laminated electrode sheet 4 was visually observed, the boundaries of the layers constituting the laminated electrode sheet 4 could not be clearly distinguished. This is presumed to be due to the following reasons. That is, it is presumed that the blade portion 210 of the upper blade 21 cuts the protruding portion R4 by press-cutting, and at that time, the blade portion 210 of the upper blade 21 rubs against the separation surface S40 of the laminated electrode precursor 40. As a result, it was experimentally found that when the rake angle θA is more than 30°, the laminated electrode sheet 4 is difficult to separate while suppressing the occurrence of interlayer short circuits.

[0080] The inventors cut the laminated electrode sheet 4 using a device similar to the pressing and breaking device 1 except that the clearance angle was changed to 0°. When the cut surface of the cut laminated electrode sheet 4 was visually observed, the boundaries of each layer constituting the laminated electrode sheet 4 could not be distinguished. Furthermore, powder derived from the material of the laminated electrode sheet 4 was scattered on the floor near the device. This is presumably because the blade portion 210 of the upper blade 21 and the separation surface S40 of the laminated electrode precursor 40 rubbed against each other after the broken material 41 was separated from the laminated electrode sheet 4. As a result, it was experimentally found that when the clearance angle is not acute, the laminated electrode sheet 4 is difficult to separate while suppressing the occurrence of interlayer short circuits.

[0081] The inventors cut the laminated electrode sheet 4 using a device similar to the pressing and breaking device 1, except that the clearance length L3 was set to less than 10% of the length L4 of the laminated electrode sheet 4. When the cut surface of the cut laminated electrode sheet 4 was visually observed, the boundaries of the layers constituting the laminated electrode sheet 4 could not be clearly distinguished. This is presumably because the protruding portion R4 was cut without being pressed and bent by the upper blade 21, and the separation surface S40 of the laminated electrode precursor 40 rubbed against the upper blade 21 and the broken material 41. As a result, it was experimentally found that when the clearance length L3 is less than 10% of the length L4 of the laminated electrode sheet 4, the laminated electrode sheet 4 is difficult to separate while suppressing the occurrence of interlayer short circuits.

[0082] The inventors cut the laminated electrode sheet 4 using a device similar to the pressing and breaking device 1, except that the clearance length L3 was set to more than 35% of the length L4 of the laminated electrode sheet 4. A top view of the cut part of the cut laminated electrode sheet 4 is shown in FIG. 10. As shown in FIG. 10, a crack D2 was confirmed at a position a distance L6 (about 70 μm) away from the edge of the cut part on the surface of the laminated electrode sheet 4 toward the center in the left-right direction. The crack D2 extended linearly along the front-rear direction. This is presumably because stress was concentrated in the part CR4 near the end 2210 of the pressing mechanism 22 on the upper blade 21 side of the laminated electrode sheet 4 when the moving upper blade 21 was pressing and bending the protruding part R4. As a result, it was experimentally found that when the clearance length L3 was more than 35% of the length L4 of the laminated electrode sheet 4, the laminated electrode sheet 4 was less likely to be separated by suppressing the occurrence of cracks.

[0083] 1 to 7, in the press-and-break device 1, the pressing mechanism 22 has a contact member 221. In the left-right direction, the position of the end 2210 of the contact member 221 on the upper blade 21 side is the same as the position of the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310). As a result, when the moving upper blade 21 presses and bends the protruding portion R4, stress is less likely to concentrate on the portion CR4 near the end 2210 of the pressing mechanism 22 on the upper blade 21 side of the laminated electrode sheet 4. As a result, the press-and-break device 1 can separate the laminated electrode sheet 4 while further suppressing the occurrence of cracks.

[0084] As described with reference to Figs. 1 to 7, in the press-breaking device 1, the clearance angle is 5° to 15°. This makes it possible for the laminated electrode precursor 40 obtained by separating the broken material 41 to be less likely to rub against the upper blade 21. As a result, the press-cutting device 1 can separate the laminated electrode sheet 4 while further suppressing the occurrence of interlayer short circuits.

[0085] As described with reference to Figs. 1 to 7, in the press-breaking device 1, the clearance length L3 is 20 µm to 50 µm. This allows the press-cutting device 1 to prevent interlayer short circuits and cracks from occurring and separate the laminated electrode sheet 4 into pieces of desired dimensions. The length L4 of the laminated electrode sheet 4 in the up-down direction is, for example, 0.2 mm.

[0086] As described with reference to Figs. 1 to 7, the press-breaking device 1 further includes a lower die holder 32 and an upper die holder 24. The upper blade 21 and the pressing mechanism 22 are attached to the upper die holder 24. The lower blade 31 is attached to the lower die holder 32. As a result, the press-cutting device 1 can efficiently separate the laminated electrode sheet 4 with a simple configuration.

[0087] As described with reference to FIGS. 1 to 7, the press-and-break device 1 includes an upper blade 21 and a lower blade 31. As shown in FIG. This allows the press-cutting device 1 to separate the laminated electrode sheet 4 efficiently.

[0088] (2) Manufacturing method of laminated electrodes The method for producing a laminated electrode according to this embodiment produces a laminated battery using a press-breaking device 1. The method for producing a laminated electrode according to this embodiment includes a preparation step, a placement step, a press-breaking step, and a stacking step. The preparation step, placement step, press-breaking step, and stacking step are performed in this order.

[0089] (2.1) Stacked battery The laminated battery is formed by stacking a negative electrode active material layer, a solid electrolyte layer, a positive electrode active material layer, and a positive electrode current collector in this order on both sides of a negative electrode current collector along the up-down direction. In other words, the laminated battery includes a laminated electrode precursor 40 and two positive electrode current collectors stacked on the two positive electrode active material layers of the laminated electrode precursor 40. The first current collector sheet, the first active material sheet, the insulating sheet, and the second active material sheet included in the laminated electrode sheet are split to function as the first current collector, the first active material layer, the insulating layer, and the second active material layer. The negative electrode current collector sheet 42, the negative electrode active material sheet 43, the solid electrolyte sheet 44, and the positive electrode active material sheet 45 included in the laminated electrode sheet are split to become the negative electrode current collector, the negative electrode active material layer, the solid electrolyte layer, and the negative electrode active material layer included in the laminated electrode.

[0090] The positive electrode current collector may be, for example, stainless steel, aluminum, copper, nickel, iron, titanium, carbon, etc., and is preferably an aluminum alloy foil or aluminum foil. The aluminum alloy foil and aluminum foil may be manufactured using powder. The shape of the positive electrode current collector is, for example, a foil shape or a mesh shape. The positive electrode current collector may have a positive electrode current collector tab. The positive electrode current collector tab is electrically connected to a positive electrode terminal of a laminated electrode described later. The positive electrode current collector tab may extend in one of the left and right directions from a portion of the positive electrode current collector corresponding to one of the left and right ends of the positive electrode active material layer in the left and right direction. The positive electrode current collector may have a buffer layer, an elastic layer, or a PTC (Positive Temperature Coefficient) thermistor layer disposed on the surface.

[0091] (2.2) Preparation process In the preparation step, there is prepared a laminated electrode sheet 4. The method for preparing the laminated electrode sheet 4 is not particularly limited, and may be any known method.

[0092] (2.3) Placement process In the placing step, the laminated electrode sheet 4 is placed on the lower blade 31 so as to form the protruding portion R4 of the laminated electrode sheet 4. The method for placing the laminated electrode sheet 4 on the lower blade 31 is not particularly limited and may be any known method.

[0093] (2.4) Press-bending process In the pressing and bending process, the upper die 2 including the two upper blades 21 is moved downward to press and bend and break a part of the protruding portion R4 of the laminated electrode sheet 4. In this embodiment, the upper die 2 is simply moved downward to press and bend and break a part of the protruding portion R4. This results in a laminated electrode precursor 40 in which the broken material 41 is separated from the laminated electrode sheet 4. The method of moving the upper die 2 is not particularly limited, and may be any known method. When the pressing and breaking device 1 is equipped with the above-mentioned driving means, the upper die 2 may be moved by the driving means. When the pressing and breaking device 1 is not equipped with the above-mentioned driving means, the upper die 2 may be moved manually. The moving speed of the upper die 2 is not particularly limited, and is, for example, 30 mm / sec.

[0094] (2.5) Lamination process In the lamination step, a positive electrode current collector is laminated on the positive electrode active material layer (i.e., the two positive electrode active material layers of the laminated electrode precursor 40) obtained from the positive electrode active material sheet 45 by carrying out the pressing and bending step. This results in a laminated battery. The method for laminating the positive electrode current collector on the positive electrode active material layer is not particularly limited and may be any known method.

[0095] (2.6) Effects In the method for producing a laminated electrode according to this embodiment, a laminated electrode is produced using a press-breaking device 1. The method for producing a laminated electrode according to this embodiment includes a preparation step, a placement step, and a press-bending step. The electrode manufacturing method of the seventh aspect can manufacture a laminated electrode sheet having desired dimensions while suppressing the occurrence of interlayer short circuits and cracks.

[0096] In the method for manufacturing a laminated electrode according to this embodiment, the laminated electrode sheet 4 is formed by laminating a negative electrode active material sheet 43, a solid electrolyte sheet 44, and a positive electrode active material sheet 45 in this order along the first direction on both sides of a negative electrode current collector sheet 42. The method for manufacturing a laminated electrode according to this embodiment further includes a lamination step. This makes it possible to manufacture a laminated electrode having desired dimensions while further suppressing the occurrence of interlayer short circuits and cracks.

[0097] (3) Manufacturing method of stacked battery The method for producing a stacked battery according to this embodiment includes producing a stacked electrode by the method for producing a stacked battery according to this embodiment (hereinafter, also referred to as an "electrode production step").

[0098] (3.1) Multilayer electrode The laminated electrode includes at least one laminated electrode, a positive electrode terminal, a negative electrode terminal, and an exterior body. The positive electrode terminal is electrically connected to a positive electrode current collector included in the laminated electrode. The negative electrode terminal is electrically connected to a negative electrode current collector included in the laminated electrode. The exterior body houses at least one laminated electrode, the positive electrode terminal, and the negative electrode terminal such that the positive electrode terminal and the negative electrode terminal are electrically connected to the outside.

[0099] The number of the laminated electrodes is appropriately selected depending on the application of the laminated electrodes, etc. When the number of the laminated electrodes is plural, the plural laminated electrodes may be laminated, for example, along the vertical direction.

[0100] The shape and size of the positive electrode terminal and the negative electrode terminal are appropriately selected depending on the application of the laminated electrode. Examples of the material of the positive electrode terminal and the negative electrode terminal include metal (e.g., stainless steel (SUS)).

[0101] The exterior body is not particularly limited, and examples thereof include a laminate exterior body, a metal can (e.g., a rectangular or cylindrical type), etc. The shape and size of the exterior body are appropriately selected depending on the application of the laminated electrode, etc.

[0102] (3.2) Electrode manufacturing process The method for manufacturing a stacked battery according to this embodiment includes an electrode manufacturing step.

[0103] In the electrode manufacturing step, a stacked electrode is manufactured by the manufacturing method for a stacked battery according to this embodiment.

[0104] (3.3) Other processes The manufacturing method of the stacked battery according to the present embodiment may include other steps. The other steps include general steps for manufacturing a battery. The other steps include a step of stacking a plurality of stacked electrodes to prepare an electrode stack, a step of housing the electrode stack in an exterior body (e.g., a laminate film, a can, etc.), a step of electrically connecting a plurality of negative electrode current collectors included in the electrode stack to at least one negative electrode terminal, a step of electrically connecting a plurality of positive electrode current collectors included in the electrode stack to at least one positive electrode terminal, etc.

[0105] (3.4) Effects The method for manufacturing a stacked battery according to this embodiment includes an electrode manufacturing step. As a result, the method for manufacturing a stacked battery according to this embodiment can manufacture a stacked battery that is equipped with stacked electrodes having desired dimensions while suppressing the occurrence of interlayer short circuits and cracks.

[0106] (4) Variations In this embodiment, in the left-right direction, the position of the end 2210 of the contact member 221 on the upper blade 21 side is the same as the position of the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310), but it may be a position closer to the upper blade 21 than the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310).

[0107] In this embodiment, the clearance angle θB is between 5° and 15°, but may be outside the range of 5° to 15° as long as it is an acute angle.

[0108] In this embodiment, the clearance length L3 is 20 μm to 50 μm, but may be outside the range of 20 μm to 50 μm as long as it is 10% to 35% of the left-right length L4 of the laminated electrode sheet 4.

[0109] In this embodiment, the press-breaking device 1 includes the upper die holder 24 and the lower die holder 32, but at least one of the upper die holder 24 and the lower die holder 32 may not be included.

[0110] In this embodiment, the press-cutting device 1 includes a lower blade 31, but the press-cutting device 1 does not necessarily need to include the lower blade 31 if a mounting table on which the laminated electrode sheet 4 is placed is provided.

[0111] The method for producing the laminated electrode of the present embodiment includes a lamination step, but does not necessarily have to include the lamination step.

[0112] In this embodiment, the laminated electrode sheet 4 is formed by stacking a negative electrode active material sheet 43, a solid electrolyte sheet 44, and a positive electrode active material sheet 45 in this order on both sides of a negative electrode current collector sheet 42 along the vertical direction, but the present disclosure is not limited thereto. The laminated electrode sheet may be formed by stacking a positive electrode active material sheet 45, a solid electrolyte sheet 44, and a negative electrode active material sheet 43 in this order on both sides of a positive electrode current collector sheet along the vertical direction. In the present disclosure, a separator of a lithium secondary battery using a nonaqueous electrolyte may be used instead of the solid electrolyte sheet 44.

[0113] In this embodiment, the laminated battery sheet is a battery sheet used in a lithium secondary battery using a solid electrolyte, but it may be a battery sheet used in a secondary battery (such as a nickel-metal hydride battery).

[0114] In this embodiment, the angle θC between the end surface S310A and the contact surface S310B of the lower blade 31 is 90°, but may be less than 90°. [Explanation of symbols]

[0115] 1: pressing and breaking device, 2: upper die, 21: upper blade, 210: blade portion, 22: pressing mechanism, 23: guide pin, 24: upper die holder, 3: lower die, 31: lower blade, 32: lower die holder, 4: laminated electrode sheet, 40: laminated electrode precursor, 41: broken material, 42: negative electrode current collector sheet, 43: negative electrode active material sheet, 44: solid electrolyte sheet, 45: positive electrode active material sheet

Claims

1. a mounting table for mounting the laminated electrode sheet; a pressing mechanism that presses the laminated electrode sheet placed on the mounting table; At least one cutting tool; Equipped with a pressing and breaking device for pressing and breaking a part of a protruding portion of the laminated electrode sheet, the protruding portion protruding from the mounting table and the pressing mechanism, of the laminated electrode sheet pressed by the pressing mechanism in a second direction perpendicular to the first direction, by the at least one cutting blade tool that moves relative to the mounting table along a first direction, The angle of the cutting edge of the cutting tool with respect to the second direction is 15° to 30°, An angle of the blade portion with respect to the first direction is an acute angle, A press-cutting device, wherein the length in the second direction of a clearance between the blade portion and the end of the mounting table on the cutting blade tool side is 10% to 35% of the length in the first direction of the laminated electrode sheet.

2. the pressing mechanism has a contact member that comes into contact with the laminated electrode sheet when pressing the laminated electrode sheet, The pressing and breaking device according to claim 1, wherein in the second direction, the position of the end of the contact member on the cutting blade tool side is the same as the position of the end of the mounting table on the cutting blade tool side, or is a position closer to the cutting blade tool than the position of the end of the mounting table on the cutting blade tool side.

3. The press-cutting device according to claim 1, wherein the angle of the blade portion with respect to the first direction is 5° to 15°.

4. The press-cutting device according to claim 1, wherein the length of the clearance in the second direction is 20 μm to 50 μm.

5. a lower holder; and an upper holder disposed opposite the lower holder and movable relative to the lower holder along the first direction, the first direction is parallel to the direction of gravity; the blade and the pressing mechanism are attached to the upper holder, The press-cutting device according to claim 1 , wherein the mounting table is attached to the lower die holder.

6. The cutting edge tool is an upper blade, The press-cutting device according to claim 5, wherein the support is a lower blade.

7. A method for producing a laminated electrode, comprising the steps of: producing a laminated electrode using the press-cutting device according to any one of claims 1 to 6; Preparing the laminated electrode sheet; placing the laminated electrode sheet on the mounting table so that the protruding portion is formed; and moving the at least one cutting edge tool in the first direction to bend and split a portion of the protruding portion to thereby split the laminated electrode sheet.

8. the laminated electrode sheet is formed by laminating a first active material sheet, a solid electrolyte sheet, and a second active material sheet in this order on both sides of a first current collector sheet along the first direction; The method for producing a laminated electrode according to claim 7 , further comprising laminating a second current collector on a second active material layer obtained from the second active material sheet by performing the pressing and breaking.

9. A method for producing a stacked battery, comprising producing a stacked electrode by the method for producing a stacked electrode according to claim 7.

Citation Information

Patent Citations

  • Electrode cutting blade and electrode cutting device using the same

    JP2010253615A

  • Breaking device for electrode

    JP2015153538A

  • Slitter

    JP2022517975A

  • Solid battery, solid battery manufacturing method, and solid battery manufacturing apparatus

    JP2023047936A