Solid oxide type battery system

The solid oxide battery system uses a deterioration detection unit to monitor potential differences between electrodes, effectively distinguishing structural from temporal deterioration, ensuring early detection and enhanced safety by identifying step-wise changes in potential difference.

JP2024155233AInactive Publication Date: 2024-10-31SOKEN CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023069788
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-31
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Reversible solid oxide cells face structural deterioration due to volumetric expansion of the fuel electrode, leading to cracks and peeling at the electrolyte layer interface, which is difficult to distinguish from normal deterioration over time, posing safety risks.

Method used

A solid oxide battery system with a deterioration detection unit that monitors the potential difference between electrodes, using second-order differential values to differentiate between structural and temporal deterioration by analyzing the step-wise change in potential difference.

Benefits of technology

Enables early detection of structural deterioration, improving safety by distinguishing it from normal aging, thereby preventing potential damage to the electrolyte layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155233000001_ABST
    Figure 2024155233000001_ABST
Patent Text Reader

Abstract

To provide a solid oxide type battery system capable of detecting a structure deterioration occurring in an electrochemical cell, separated from a time degradation.SOLUTION: A solid oxide type battery system 1 comprises: an electrolyte layer 20 using a solid state oxide ceramic; an electrochemical cell 2 that includes a first electrode 21 provided on its first surface 20a and a second electrode 22 provided on a second surface 20b on the opposite side; and a deterioration detection part 10 that detects a structure deterioration of the electrochemical cell 2. The deterioration detection part 10 includes: a potential difference detection part 11 that detects a potential difference between the first electrode 21 and the second electrode 22; a potential difference monitoring part 12 that monitors an inclination of a time change of the detected potential difference; and a deterioration determination part 13 that determines the presence / absence of the structure deterioration of the electrochemical cell on the basis of an increase and decrease inclination of the time change in the potential difference.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a battery system using a solid oxide electrochemical cell. [Background technology]

[0002] In recent years, battery systems equipped with reversible solid oxide cells have been studied from the viewpoints of reducing carbon dioxide emissions and ensuring a stable supply of energy. A reversible solid oxide cell is an electrochemical cell that uses a solid oxide electrolyte and utilizes an electrochemical process, and functions as a solid oxide fuel cell (SOFC) that generates electricity, or a solid oxide electrolysis cell (SOEC) that performs electrolysis.

[0003] Such a battery system includes a cell stack in which single cells, each having a fuel electrode and an air electrode joined on either side of an electrolyte layer, are stacked with a separator interposed therebetween, and a fuel gas containing hydrogen is supplied to the flow path on the fuel electrode side, and an oxidant gas containing oxygen is supplied to the flow path on the air electrode side to generate electricity. As a reverse reaction, an electrolytic reaction of a raw material gas supplied to the fuel electrode side is induced, and hydrogen, which serves as a fuel gas, can be generated by, for example, electrolysis of water vapor.

[0004] The supply of gas to the flow passages in the cell stack and the recovery of exhaust gas or generated gas are controlled by a control device, and the use of exhaust heat and recovered gas makes it possible to operate a reversible battery system efficiently. Meanwhile, since the battery system is operated at relatively high temperatures (e.g., 600°C or higher), heat-resistant alloys or heat-resistant steels containing Cr are used for conductive members constituting the cell stack, piping, etc. In such cases, it is known that when a portion of Cr evaporates in a high-temperature oxidizing atmosphere, it adheres to the air electrode, causing Cr poisoning, which inhibits the electrode reaction.

[0005] As poisoning substances accumulate over time, the performance of the battery system gradually declines, and the desired output cannot be obtained efficiently. Patent Document 1 discloses a method and device for monitoring the state of a fuel cell used in a fuel cell power generation system in real time to ensure long-term operability in response to such changes in battery characteristics. Specifically, the system receives operation data obtained from the components of the system while controlling each part of the system to operate stably according to the operating characteristics of a fuel cell module including multiple cell stacks and the system configuration including a fuel processing module, etc. Then, the system uses the real-time operating data and the preceding operating data to determine whether or not there is a potential failure state, and depending on the result, measures such as issuing an alert or sending an instruction to resolve the failure state are taken. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] U.S. Pat. No. 1,046,1347 Summary of the Invention [Problem to be solved by the invention]

[0007] In a reversible solid oxide cell, for example, a cermet electrode containing Ni is used for the fuel electrode, and for example, a perovskite-type composite oxide is used for the air electrode. In a power generation environment, the fuel electrode is in a reducing atmosphere and Ni is reduced, but when an oxidizing gas is mixed in during operation shutdown, Ni is easily oxidized to NiO. Therefore, when Ni oxidation progresses, stress due to the volume expansion of the fuel electrode is applied to the electrolyte layer, which may cause microcracks or peeling at the layer interface.

[0008] While deterioration due to the adhesion of poisons etc. is a decrease in performance that progresses over time, structural deterioration such as cracks and peeling is a concern that could lead to gas leakage due to damage to the electrolyte layer, etc. Therefore, from the perspective of improving the safety of cell stacks, it is desirable to quickly and accurately detect structural deterioration of electrochemical cells.

[0009] The present invention has been made in view of the above problems, and has an object to provide a solid oxide battery system that is capable of detecting structural deterioration occurring in an electrochemical cell separately from deterioration over time. [Means for solving the problem]

[0010] One aspect of the present invention is an electrochemical cell (2) including an electrolyte layer (20) using solid oxide ceramics, a first electrode (21) provided on a first surface (20a) of the electrolyte layer, and a second electrode (22) provided on a second surface (20b) of the electrolyte layer opposite to the first surface; A solid oxide battery system (1) comprising: a deterioration detection unit (10) that detects structural deterioration of the electrochemical cell, The deterioration detection unit is a potential difference detection unit (11) that detects a potential difference between the first electrode and the second electrode; a potential difference monitoring unit (12) that monitors the tendency of time-varying change in the detected potential difference; and a deterioration determining section (13) that determines whether or not the structure of the electrochemical cell has deteriorated based on the increase / decrease tendency of the time change of the potential difference. Effect of the Invention

[0011] In the solid oxide battery system having the above configuration, the degradation detection unit detects the potential difference between the first and second electrodes of the electrochemical cell at any time using the potential difference detection unit, and monitors the trend of the potential difference over time using the potential difference monitoring unit. In degradation over time due to poisoning or the like, the output gradually decreases, and the magnitude of the time change also changes continuously, whereas in structural degradation, the output shows intermittent decreases as cracks, peeling, or the like progress. In such a case, since the magnitude of the time change in the potential difference changes stepwise, a threshold value or the like that can be distinguished from normal degradation based on the increase / decrease trend can be set in advance, and the presence or absence of structural degradation can be determined by the degradation determination unit. This allows the occurrence of structural degradation to be detected early, improving safety.

[0012] As described above, according to the above aspect, it is possible to provide a solid oxide battery system that is capable of detecting structural deterioration occurring in an electrochemical cell in a manner that distinguishes it from deterioration over time. In addition, the symbols in parentheses described in the claims and the means for solving the problems indicate a correspondence with the specific means described in the embodiments described below, and do not limit the technical scope of the present invention. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a schematic diagram showing an overall configuration of a solid oxide battery system according to a first embodiment. [Diagram 2] FIG. 2 is a schematic cross-sectional view in the stacking direction showing a schematic configuration of a cell stack in the first embodiment. [Diagram 3] FIG. 2 is a schematic cross-sectional view for explaining a power generating operation of the electrochemical cell in the first embodiment. [Figure 4] FIG. 2 is a schematic cross-sectional view for explaining the electrolysis operation of the electrochemical cell in the first embodiment. [Diagram 5] FIG. 2 is a schematic cross-sectional view for illustrating a deteriorated state of the electrochemical cell in the first embodiment. [Figure 6] FIG. 4 is a graph showing a comparison of the tendency of time-dependent changes in voltage characteristics depending on the degradation mode of the electrochemical cell in the first embodiment. [Figure 7] 4A to 4C are diagrams for explaining the tendency of time-dependent changes in voltage characteristics due to degradation modes of an electrochemical cell and a degradation determination method based on dV / dt and d2V / d2t in the first embodiment. [Figure 8] FIG. 4 is a flowchart showing the procedure of an abnormality detection process performed by an abnormality detection unit in the first embodiment. [Figure 9] FIG. 4 is a block diagram showing the configuration of a deterioration detection unit in the embodiment. [Figure 10] FIG. 11 is a flowchart showing the procedure of an abnormality detection process performed by an abnormality detection unit in the second embodiment. [Figure 11] FIG. 11 is a schematic diagram showing a configuration of a main part of a solid oxide battery system according to a third embodiment. [Figure 12]11A and 11B are a cross-sectional view and an enlarged cross-sectional view of a main part of a poisoning detection sensor according to a third embodiment of the present invention; [Figure 13] FIG. 11 is a graph showing the relationship between the amount of poisoning substance adhered and the current detected by the poisoning detection sensor in the third embodiment. [Figure 14] FIG. 11 is a flowchart showing the procedure of an abnormality detection process performed by an abnormality detection unit in the third embodiment. [Figure 15] FIG. 11 is an exploded perspective view showing the overall configuration of a cell stack in a fourth embodiment. [Figure 16] FIG. 13 is a flowchart showing the procedure of an abnormality detection process performed by an abnormality detection unit in the fourth embodiment. [Figure 17] FIG. 13 is a flowchart showing the procedure of an abnormality detection process performed by an abnormality detection unit in the fifth embodiment. [Figure 18] FIG. 13 is a graph showing the change in voltage over time in a deterioration test according to the fifth embodiment. [Figure 19] FIG. 13 is a graph showing a comparison of changes in voltage over time in a time degradation test and a structural degradation test in the fifth embodiment. [Figure 20] FIG. 13 is a graph showing a comparison of the number of inversions in deterioration determination between time-related deterioration and structural deterioration in the fifth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] (Embodiment 1) An embodiment of a solid oxide battery system (hereinafter, appropriately abbreviated as battery system) will be described with reference to Figs. 1 to 8. As shown in Figs. 1 and 2, the battery system 1 includes a cell stack S including an electrochemical cell 2, and a deterioration detection unit 10 that detects structural deterioration of the electrochemical cell 2. The electrochemical cell 2 has an electrolyte layer 20 using solid oxide ceramics, and a fuel electrode 21 as a first electrode and an air electrode 22 as a second electrode provided on both sides of the electrolyte layer 20. The deterioration detection unit 10 constitutes a part of an abnormality detection unit 100 described later.

[0015] The electrochemical cell 2 of this embodiment includes an electrolyte layer 20 formed of solid oxide ceramics in a flat plate shape, with a fuel electrode 21 provided on a first surface 20a, which is one of the plate surfaces, and an air electrode 22 provided on a second surface 20b opposite the first surface 20a, disposed opposite each other across the electrolyte layer 20. The cell stack S is configured so that a predetermined amount of power can be obtained by electrically connecting a plurality of single cells in series, with the electrochemical cell 2 having such a structure being the minimum structural unit (hereinafter referred to as a single cell).

[0016] The electrochemical cell 2 can perform a power generation operation in which a fuel gas is supplied to the fuel electrode 21 and reacts with an oxidant gas supplied to the air electrode 22 to generate electrical energy. In addition, as a reverse operation to the power generation operation, an electrolysis operation can be performed in which a fuel gas is produced from a raw material gas supplied to the fuel electrode 21 by electrical energy. The electrochemical cell 2 functions as an SOFC during the power generation operation, and functions as an SOEC during the electrolysis operation.

[0017] The fuel gas is hydrogen (H2) or a gas containing hydrogen, and may be, for example, a reformed gas obtained by steam reforming a raw fuel. The raw fuel may be a hydrocarbon fuel such as natural gas containing methane (CH4) as the main component, city gas, liquefied natural gas (LNG), or liquefied petroleum gas (LPG). The oxidant gas is oxygen (O2) or a gas containing oxygen, and may be, for example, air.

[0018] In the electrochemical cell 2, the oxygen partial pressure difference between the fuel electrode 21 and the air electrode 22 is used as a driving force to ionize oxygen in the oxidant gas, which then passes through the electrolyte layer 20 and reacts with hydrogen in the fuel gas, releasing electrons to generate electricity. The overall reaction during power generation is shown in formula (1) below. (Power generation reaction) 2H2+O2→H2+2H2O (1) Moreover, the overall reaction of the electrolysis operation is as shown in the following formula (2), and by applying external energy to decompose water vapor (H2O), hydrogen is produced on the fuel electrode 21 side and oxygen is produced on the air electrode 22 side. (Electrolytic reaction) H2O → H2 + 1 / 2O2 (2)

[0019] The deterioration detection unit 10 has a potential difference detection unit 11, a potential difference monitoring unit 12, and a deterioration determination unit 13. The potential difference detection unit 11 detects the potential difference between the fuel electrode 21 and the air electrode 22, and the potential difference monitoring unit 12 can monitor the trend of time-dependent change in the detected potential difference. Then, the deterioration determination unit 13 determines the presence or absence of structural deterioration of the electrochemical cell 2 based on the trend of increase / decrease in the time-dependent change in the potential difference.

[0020] Specifically, the potential difference monitoring unit 12 calculates a parameter value indicating the tendency of increase or decrease in the time change of the potential difference detected by the potential difference detection unit 11. In this case, the deterioration determination unit 13 can determine that structural deterioration of the electrochemical cell 2 has occurred when the parameter value calculated by the potential difference monitoring unit 12 shows a tendency of inverting positive and negative.

[0021] Preferably, the potential difference monitor 12 measures, as the parameter value, a second derivative (d 2 V / d 2 t) can be calculated. Furthermore, the deterioration determination unit 13 can set threshold values ​​TH1 and TH2 for determining deterioration in advance based on a comparison between the increase / decrease tendency of the time change in the potential difference due to the structural deterioration of the electrochemical cell 2 and the increase / decrease tendency of the time change in the potential difference due to the time-dependent deterioration of the electrochemical cell 2. This makes it possible to determine the presence or absence of an abnormality due to structural deterioration of the electrochemical cell 2, separately from time-dependent deterioration, by comparing the calculated parameter value with the threshold values ​​TH1 and TH2.

[0022] In this way, the state of the electrochemical cells 2 constituting the main part of the battery system 1 can be constantly monitored by the deterioration detection unit 10, and the occurrence of structural deterioration can be detected at an early stage. In addition, based on the difference in the tendency of the change in the potential difference, accurate detection is possible by distinguishing it from deterioration over time, and the safety of the system can be improved by appropriate measures such as stopping the system or issuing an alert.

[0023] The overall configuration of the battery system 1 of this embodiment and the details of each component will be described below. 1, a battery system 1 of this embodiment has a fuel cell module M that can switch between power generation and electrolysis, and a cell control unit C that controls the operation of the fuel cell module M. The fuel cell module M is connected to a fuel gas supply source F via a first pump P1, and is connected to an oxidant gas supply source A via a second pump P2. A fuel recovery unit 3 is connected to the discharge side of the fuel cell module M.

[0024] The cell control unit C has an abnormality detection unit 100 for detecting an abnormality in the fuel cell module M. The cell control unit C is provided with an alarm unit AL, which can notify the outside of the occurrence of an abnormality, for example, by turning on a warning light or sounding an alarm when an abnormality detection signal is output from the abnormality detection unit 100. The battery system 1 can be applied to, for example, a commercial or domestic stationary cogeneration system or the like, and can generate power in the fuel cell module M and produce fuel used for power generation.

[0025] (Fuel cell module M) The fuel cell module M has a cell stack S including an electrochemical cell 2, a first supply flow path 201 that supplies a fuel gas to the fuel electrode 21 of the electrochemical cell 2, and a second supply flow path 202 that supplies an oxidant gas to the air electrode 22. An evaporator 203 that generates water vapor can be disposed in the first supply flow path 201, and the evaporator 203 is connected to a water supply source W via a third pump P3 and a third supply flow path 204. The fuel gas is introduced into the cell stack S from the first supply flow path 201 together with the water vapor generated in the evaporator 203.

[0026] When the fuel gas supplied to the cell stack S is a reformed gas containing hydrogen, a reforming unit (not shown) is provided in the fuel cell module M. The evaporator 203 constitutes a part of the reforming unit, and uses water vapor generated by evaporating water supplied from the third supply flow path 204 to carry out a reforming reaction of hydrocarbons such as methane contained in the raw fuel, thereby generating a hydrogen-rich reformed gas, which can be used as the fuel gas. The reforming reaction between methane and water is generally represented by the following formula (3). (Reforming reaction) CH4 + H2O → 3H2 + CO (3)

[0027] In the cell stack S, power generated by the power generation operation is output to a power conversion circuit (not shown) and can be used to supply power to an external load. In the cell stack S, a first exhaust flow path 211 is provided on the opposite side of the fuel electrode 21 to the first supply flow path 201, and a first off-gas is discharged. On the opposite side of the air electrode 22 to the second supply flow path 202, a second exhaust flow path 212 is provided, and a second off-gas is discharged. In the fuel cell module M, a hydrodesulfurizer for removing sulfur components from the raw fuel can also be provided in the first supply flow path 201 upstream of the evaporator 203.

[0028] The second supply flow path 202 is provided with a poisoning detection sensor S1 as a time deterioration detection device that detects the state of time deterioration of the electrochemical cell 2, and can detect poisoning substances in the fuel gas supplied to the air electrode 22 side of the cell stack S. The cell stack S is also provided with a vibration detection sensor S2 as a vibration detection device that detects the vibration state associated with structural deterioration of the electrochemical cell 2, and can detect vibrations occurring inside the cell stack S. These detection results are used to increase the accuracy of abnormality determination in the abnormality detection unit 100. A configuration without the poisoning detection sensor S1 or the vibration detection sensor S2 may also be used.

[0029] (Fuel recovery section 3) The fuel recovery section 3 includes a recovery flow path 301, a heat exchanger 31, a separator 32, a compressor 33, and a buffer tank 34. A first discharge flow path 211 provided on the anode 21 side of the cell stack S forms part of the recovery flow path 301, and high-temperature first off-gas discharged from the anode 21 is cooled in the heat exchanger 31 and separated into gas and liquid in the separator 32. Hydrogen in the gas phase is compressed in the compressor 33 and recovered in the buffer tank 34.

[0030] The buffer tank 34 is connected to the first supply flow path 201 by a circulation flow path 302, and hydrogen stored in the buffer tank 34 can be circulated through the first supply flow path 201. Liquid water separated by the separator 32 can be drained through a flow path (not shown) or recovered and reused. The exhaust heat from the heat exchanger 31 can also be used to heat or keep warm each part of the fuel cell module M.

[0031] (Poison detection sensor S1, vibration detection sensor S2) The poisoning detection sensor S1 detects poisons such as Cr that may cause deterioration over time of the air electrode 22. The configuration of the poisoning detection sensor S1 is not particularly limited, but for example, a sensor having a detection unit capable of capturing Cr contained in the oxidant gas flowing through the second supply flow path 202 and outputting a sensor signal corresponding to the amount of Cr is used.

[0032] The vibration detection sensor S2 detects vibrations that occur due to structural deterioration of the electrochemical cell 2. The configuration of the vibration detection sensor S2 is not particularly limited, but for example, a sensor equipped with a detection unit that utilizes a known acoustic emission (hereinafter referred to as AE) method is used. AE is a phenomenon in which elastic energy stored inside is released as AE waves due to deformation or destruction of a material, and the detection unit of the vibration detection sensor S2 can be configured to be capable of outputting a sensor signal corresponding to the released energy.

[0033] The sensor signals from the poisoning detection sensor S1 and the vibration detection sensor S2 are input to an abnormality detection unit 100 of the cell control unit C. The procedure for abnormality detection using the poisoning detection sensor S1 or the vibration detection sensor S2 will be described later.

[0034] (Battery control unit C) The cell control unit C is configured with a known microcomputer including a CPU, ROM, RAM, etc. Signals are input to the cell control unit C from various sensors (not shown) provided in each part of the cell system 1, in addition to the poisoning detection sensor S1 and the vibration detection sensor S2. Based on these signals and operation commands from the outside, the cell control unit C drives the first to third pumps P1 to P3, adjusts the flow rate and temperature of the fluid supplied to the fuel cell module M, and controls the power generation operation and electrolysis operation in the cell stack S. In addition, the cell control unit C drives each part of the fuel recovery unit 3 connected to the fuel cell module M and auxiliary equipment (not shown) to control the entire cell system 1.

[0035] The abnormality detection unit 100 of the battery control unit C may be provided with an abnormality determination unit 103 to which a signal from the deterioration detection unit 10 is input. Also, a poisoning determination unit 101 based on a signal from the poisoning detection sensor S1 and a vibration determination unit 102 based on a signal from the vibration detection sensor S2 may be provided. In this case, in addition to the signal from the deterioration detection unit 10, signals from the poisoning determination unit 101 and the vibration determination unit 102 are input to the abnormality determination unit 103, and the abnormality determination unit 103 can determine the presence or absence of a deterioration abnormality based on these signals. Details and operation of the abnormality detection unit 100 including the deterioration detection unit 10 will be described later.

[0036] (Cellstack S) Next, an example of the structure of the cell stack S will be described. As shown in Fig. 2, the cell stack S has a laminate structure in which electrochemical cells 2, which are single cells, and separators 4 are alternately laminated. Hereinafter, the stacking direction of the laminate will be referred to as the X direction, and the direction perpendicular to the X direction will be referred to as the Y direction. In the X direction, a first flow path 221 or a second flow path 222 is formed between the separator 4 and each of the electrochemical cells 2 on both sides. A pair of end plates P is disposed on both ends of the cell stack S, and sandwiches the laminate including a predetermined number of electrochemical cells 2 and separators 4 from the X direction.

[0037] In the X direction, a first flow path 221 to which a fuel gas is supplied is formed on the fuel electrode 21 side of the electrochemical cell 2, and a second flow path 222 to which an oxidant gas is supplied is formed on the air electrode 22 side. In the first flow path 221 and the second flow path 222, the fuel gas or the oxidant gas flows in the Y direction, that is, in a direction parallel to the surface of the fuel electrode 21 or the air electrode 22. Note that the directions of gas introduction into the first flow path 221 and the second flow path 222 shown by arrows in FIG. 2 are for the purpose of explaining the gas flow diagrammatically, and do not need to be the same direction.

[0038] The separator 4 electrically connects adjacent unit cells to each other, and also partitions the first flow path 221 and the second flow path 222 of the adjacent unit cells, forming a partition wall that separates the fuel gas from the oxidizer gas. The separator 4 can be made of a heat-resistant metal plate material such as stainless steel, a heat-resistant Cr alloy, a heat-resistant NiCr alloy, etc. The first flow path 221 of the unit cell communicates with the first supply flow path 201 and the first discharge flow path 211, and the second flow path 222 communicates with the second supply flow path 202 and the second discharge flow path 212.

[0039] (Electrochemical cell 2) In the electrochemical cell 2, a fuel electrode 21 is laminated on a first surface 20a (lower surface in FIG. 2) of an electrolyte layer 20, and an air electrode 22 is laminated on a second surface 20b (upper surface in FIG. 2) located on the opposite side in the X direction. A support layer 5 that supports the electrochemical cell 2 is disposed on the outer side of the fuel electrode 21.

[0040] The material constituting each layer of the electrochemical cell 2 is not necessarily limited, and can be appropriately selected from known materials. For example, the solid oxide ceramics that become the electrolyte layer 20 can be a composite oxide containing at least one of Y, Sc, Sm, Gd, Ce, and Zr. Preferably, a zirconia-based oxide having oxide ion conductivity such as yttria-stabilized zirconia (YSZ), a ceria-based oxide such as samaria-doped ceria (SDC) doped with Sm, or gadolinia-doped ceria (GDC) doped with Gd, or the like can be used. For example, a mixture of a catalyst such as Ni, NiO, or the like and YSZ or SDC can be used as the material of the air electrode 22. For example, a transition metal perovskite-type composite oxide such as La-Sr-Co-based oxide (LSC), La-Sr-Co-Fe-based oxide (LSCF), or the like can be used.

[0041] The fuel electrode 21 and the air electrode 22 are formed to be porous, and the material composition, porosity, etc. are appropriately adjusted so that the supplied fuel gas and oxidant gas can be diffused while the electrode reaction can proceed smoothly with sufficient electronic conductivity and ionic conductivity. In this case, each electrode can have a single-layer or multi-layer structure, and for example, the fuel electrode 21 may have a configuration in which a diffusion layer is disposed outside a reaction layer where the electrode reaction mainly occurs.

[0042] In addition, the air electrode 22 may be configured such that an intermediate layer made of a different material is disposed between the electrolyte layer 20 and the air electrode 22. A bonding layer may be interposed between the intermediate layer and the electrolyte layer 20. The material of each of these layers may be appropriately selected.

[0043] Each layer of the electrochemical cell 2 is formed in the shape of a porous film or plate. The support layer 5 is made of a metal plate having a large number of through holes, and supports the first surface 20a side of the electrolyte layer 20 and supplies the fuel gas through the through holes. Examples of materials for the support layer 5 include stainless steel, heat-resistant Cr alloy, and heat-resistant CrNi alloy.

[0044] Specifically, the electrochemical cell 2 may be configured such that the periphery is supported by a cell frame that includes the support layer 5. In this case, a first flow path 221 or a second flow path 222 is formed between the cell frame and separators 4 arranged on both sides of the cell frame in the X direction. The air electrode 22 may be configured to be electrically connected to the separator 4 via a current collector arranged in the second flow path 222.

[0045] The cell stack S is formed by sequentially repeating a stacking pattern including such unit cells and flow paths between a pair of end plates P. The constituent members of the cell stack S are provided with bolt insertion holes (not shown) and are fastened in place using bolts and nuts.

[0046] (Power generation, electrolysis) In Fig. 1, a fuel cell module M including a cell stack S configured as described above is capable of both SOFC and SOEC operation, and the electrochemical cell 2 functions as a solid oxide reversible cell (hereinafter referred to as SORC) that can switch between power generation operation by SOFC and electrolysis operation by SOEC, as shown in Fig. 3 to Fig. 5. The SORC can supply electricity generated by the SOFC to the outside, and can also produce fuel gas for power generation by the SOEC.

[0047] In the illustrated configuration example, an intermediate layer 23 is interposed between the electrolyte layer 20 and the air electrode 22, and the fuel electrode 21 has a multi-layer structure in which a diffusion layer 21b is disposed on the outer side of a reaction layer 21a.

[0048] 3 and 5, when power generation is performed by the SOFC, a fuel gas containing hydrogen is supplied to the first flow path 221 of the electrochemical cell 2, and air is supplied as an oxidant gas to the second flow path 222. Hydrogen in the fuel gas passes through the through-holes in the support layer 5, diffuses in the diffusion layer 21b of the anode 21, and moves to the reaction layer 21a.

[0049] On the other hand, oxygen in the air is converted into electrons (e- ) and produces oxide ions (O 2- ) and migrate to the fuel electrode 21 through the intermediate layer 23 having oxide ion conductivity and the electrolyte layer 20. The oxide ions react with hydrogen in the reaction layer 21a to generate water and release electrons. The generated water is discharged to the first flow path 221 through the diffusion layer 21b and the support layer 5.

[0050] At this time, the reactions at the fuel electrode 21 and the air electrode 22 are as shown in the following formulas (11) and (12), respectively, and the overall reaction of the power generation operation is expressed by formula (1) as described above. (Fuel electrode 21) 2H2+2O 2- →2H2O+4e - (11) (Air electrode 22) O2+4e - →2O 2- (12) (Power generation reaction) 2H2+O2→H2+2H2O (1) As water is produced, the released electrons are extracted to an external circuit via support layer 5 and flow in a direction from fuel electrode 21 to air electrode 22 (the opposite direction to current I). The potential difference (generated voltage) V generated between fuel electrode 21 and air electrode 22 is measured by voltmeter 7.

[0051] As shown in FIG. 4, when electrolysis is performed by SOEC, a raw gas containing water is supplied to the first flow path 221 of the electrochemical cell 2. The water vapor in the raw gas passes through the through-holes in the support layer 5, diffuses in the diffusion layer 21b of the fuel electrode 21, and moves to the reaction layer 21a. Meanwhile, a power source B is connected between the fuel electrode 21 and the air electrode 22, and hydrogen and oxide ions are generated by electrolysis of water in the reaction layer 21a of the fuel electrode 21, which serves as the negative electrode. The generated hydrogen is discharged to the first flow path 221 via the diffusion layer 21b and the support layer 5. The oxide ions move to the air electrode 22 via the electrolyte layer 20 and the intermediate layer, release electrons, and generate oxygen.

[0052] At this time, the reactions at the fuel electrode 21 and the air electrode 22 are as shown in the following formulas (21) and (22), respectively, and the overall reaction of the electrolysis operation is expressed by formula (2) as described above. (Fuel electrode 21) H2O+2e - →H2+O 2- ···(twenty one) (Air electrode 22) O 2- →1 / 2O2+2e - ···(twenty two) (Electrolytic reaction) H2O→H2+1 / 2O2 (2)

[0053] Here, during operation of the battery system 1, in order to efficiently advance the above reaction, the operating temperature of the cell stack S becomes high, for example, 600°C or higher, preferably about 700°C to 1000°C. Furthermore, when used in a stationary system, the system will be operated continuously for a relatively long period of time. In such a case, it is important to ensure safety during operation, and it is desirable to provide a function for stopping the system when there is a safety concern due to deterioration or the like. For this reason, the battery system 1 is provided with an abnormality detection unit 100 in order to monitor the operating state while appropriately controlling the operation using the battery control unit C, and to be able to detect abnormalities such as deterioration.

[0054] (Abnormality detection unit 100, Deterioration detection unit 10) 5, the degradation modes of the cell stack S in the fuel cell module M include a time-related degradation mode (I), which is degradation due to the adhesion of poisons, and a structural degradation mode (II), which is structural degradation of the electrochemical cell 2. The time-related degradation mode (I) is known as Cr poisoning of the air electrode 22, and occurs when Cr contained in the metal members is oxidized and evaporated during operation at high temperatures. In the power generation environment shown in the figure, if steam containing Cr reaches the air electrode 22 together with the air supplied to the second flow path 222 and Cr oxide (Cr2O3) adheres to the air electrode 22, the function of the air electrode 22 may be impaired.

[0055] The structural deterioration mode (II) is deterioration such as cracks a and peeling b between layers that occur in the constituent layers of the electrochemical cell 2, and is considered to be caused by the volume expansion of the fuel electrode 21 due to the oxidation of Ni contained in the material of the fuel electrode 21. In a power generation environment, fuel gas is supplied to the first flow path 221 on the fuel electrode 21 side to create a reducing atmosphere. However, if the atmosphere becomes an oxidizing atmosphere for some reason, such as when the operation is stopped, the reduced Ni may be oxidized, causing a volume expansion of the fuel electrode 21. If stress due to this volume expansion is applied to the electrolyte layer 20, microcracks a may occur or peeling b may occur between adjacent layers, making the performance more likely to decrease, and there is a concern that the cracks a and peeling b may progress further, leading to damage to the electrolyte layer 20, etc.

[0056] The time-related deterioration mode (I) is deterioration due to aging, and usually no measures such as notification are taken. Alternatively, since the amount of poisoning substances attached increases as the operating time at high temperatures increases, it is possible to predict the progress of deterioration from the operating period and conditions, and adjust the control conditions. In contrast, it is difficult to predict the occurrence and progress of deterioration in the structural deterioration mode (II), and depending on the state of deterioration, there are concerns about a decrease in safety, so that prompt notification or system shutdown may be desirable. For this reason, the battery control unit C is provided with a degradation detection unit 10 for distinguishing and detecting the structural deterioration mode (II) from the time-related deterioration mode (I).

[0057] As shown by the dashed line in FIG. 6, the time transition of the power generation voltage V in the normal time-dependent deterioration mode (I) shows a relatively large voltage drop for a while after the start of operation, and then the voltage drop with time gradually decreases and gradually converges. Therefore, even if a voltage drop occurs due to the structural deterioration mode (II) at the beginning of operation as shown by the solid line in FIG. 6, it is not easy to distinguish it from the time-dependent deterioration mode (I). As a result, it may lead to serious deterioration such as damage to the electrolyte layer 20. In that case, not only will the power generation performance decrease, but the fuel gas side and the oxidant gas side will communicate through the damaged part, which may reduce safety, so it is important to detect an abnormality before serious deterioration occurs.

[0058] Here, as shown in Fig. 7(a) by enlarging a part of the initial operation period in Fig. 6, in the time deterioration mode (I), the generated voltage V drops continuously with time, forming a gently curved characteristic line, whereas in the structural deterioration mode (II), the generated voltage V drops intermittently, forming a stepped characteristic line. The deterioration detection unit 10 distinguishes the deterioration modes from the difference in the tendency of such time-varying voltage characteristics. Specifically, as shown in Fig. 7(b) and (c), the time derivative dV / dt indicating the time-varying change in the generated voltage V and the second-order derivative d 2 V / d 2 By calculating t and monitoring its transition, it is possible to determine whether or not there is an abnormality.

[0059] Fig. 8 is a flowchart showing the procedure of an abnormality detection process by the abnormality detection unit 100. The deterioration detection unit 10 uses the potential difference detection unit 11 in Fig. 1 to take in a voltage signal output from the voltmeter 7 and constantly detects the potential difference V between the fuel electrode 21 and the air electrode 22 of the electrochemical cell 2. Steps S101 and S102 correspond to the potential difference monitoring unit 12 of the deterioration detection unit 10, and steps S103 to S105 correspond to the deterioration determination unit 13. Furthermore, step S106 corresponds to the abnormality determination unit 103.

[0060] When this process is started, first, in step S101, a time differential value dV / dt of the potential difference V in the detected section is calculated based on the detected potential difference V, and then the process proceeds to step S102, where a second-order differential value d 2 V / d 2 t is calculated. The time differential value dV / dt corresponds to the slope of the characteristic line shown in FIG. 7(a), and as shown in FIG. 7(b), in the case of the aging degradation mode (I), the time differential value dV / dt increases continuously. In contrast, in the case of the structural degradation mode (II), the time differential value dV / dt increases intermittently in a stepped manner, exceeding the value in the aging degradation mode (I). However, it is not easy to distinguish between the two degradation modes based on the value of the time differential value dV / dt alone.

[0061] On the one hand, as shown in FIG. 7(c), the second derivative value d 2 V / d 2 t indicates the change in the value of the time derivative dV / dt. In the case of the deterioration mode over time (I), it is almost constant at approximately 0, whereas in the case of the structural deterioration mode (II), it increases or decreases as the generated voltage V drops. Specifically, at the point of a stepwise drop, after the second derivative value d 2 V / d 2 t changes to the negative side, it shows a positive / negative inversion tendency of turning to the positive side. Therefore, a first threshold value TH1 on the negative side and a second threshold value TH2 on the positive side (i.e., TH1 < TH2) of the second derivative value d 2 V / d 2 t are set in advance, and the second derivative value d 2 V / d 2 t is used as a parameter value indicating the increasing or decreasing tendency of the time derivative dV / dt to detect the stepwise drop of the generated voltage V.

[0062] In step S103, the second derivative value d 2 V / d 2 t (Δ 2 (t)) calculated in a predetermined section is compared with the first threshold value TH1 to determine whether it is smaller than the first threshold value TH1. If the determination in step S103 is affirmative, the process proceeds to step S104; if the determination is negative, the process returns to step S101. In step S104, the second derivative value d 2 V / d 2 t (Δ 2 (t + Δt)) in the subsequent section is calculated in the same manner as in steps S101 and S102, and compared with the second threshold value TH2 to determine whether it is larger than the second threshold value TH2. If the determination in step S104 is affirmative, the process proceeds to step S105; if the determination is negative, the process returns to step S101.

[0063] In step S105, the second derivative value d 2 V / d 2After t falls below the first threshold value TH1, it is determined that the vehicle is in the alert mode corresponding to the structural deterioration mode (II), and a deterioration detection signal is output to the abnormality determination unit 103. Based on this, in step S106, an abnormality detection signal can be output from the abnormality determination unit 103, and a warning can be issued to the user using the notification unit AL. Then, this process ends.

[0064] Prior to outputting the abnormality detection signal, the abnormality determination unit 103 may perform abnormality determination by combining the deterioration detection signal with the determination result of the poisoning determination unit 101 or the vibration determination unit 102. For example, when a poisoning detection signal indicating the time-related deterioration mode (I) is input from the poisoning detection sensor S1, the abnormality detection signal may be output only when there is a high possibility of structural deterioration, taking into account the voltage drop due to poisoning deterioration. Alternatively, when a vibration detection signal indicating the structural deterioration mode (II) is input from the vibration detection sensor S2, it may be determined that there is a high possibility of structural deterioration, and the system may be stopped.

[0065] In this way, according to this embodiment, the second-order differential value d 2 V / d 2 By using t as a parameter value indicating the tendency of time-dependent change in the potential difference V and comparing it with the first threshold value TH1 and the second threshold value TH2, a step-like voltage drop can be detected. Then, the presence or absence of the structural deterioration mode (II) can be accurately detected, distinguishing it from the time-dependent deterioration mode (I).

[0066] (Embodiment 2) In this embodiment, as shown in FIG. 9, the configuration of the deterioration detection unit 10 in the battery control unit C is changed, and the deterioration determination unit 13 is provided with a second-order differential value d 2 V / d 2This embodiment is provided with a deterioration mode determination unit 131 that determines the deterioration mode using t, and a count unit 132 that counts the number of times the determination is made. Other configurations of the battery control unit C and the basic configuration of the battery system 1 are similar to those of the first embodiment. Note that, among the symbols used in the second and subsequent embodiments, those that are the same as those used in the previous embodiments represent the same components, etc., as those in the previous embodiments, unless otherwise specified.

[0067] The deterioration mode determination unit 131 detects the second-order differential value d 2 V / d 2 When it is determined that the structural deterioration mode (II) is occurring based on a comparison between t and two thresholds TH1 and TH2, a determination signal is output. The counting unit 132 counts the number of times that the structural deterioration mode (II) is occurring based on the determination signal. The deterioration determination unit 13 repeats this determination and counting, and when the count number N exceeds a preset count threshold THn, it can determine that the structural deterioration mode (II) is occurring and output a deterioration detection signal.

[0068] 10 is a flowchart showing the procedure of the abnormality detection process according to this embodiment, and steps S201 and S202 correspond to steps S101 to S104 in FIG. 8. First, in step S201, the second-order differential value d 2 V / d 2 t is calculated as a parameter value indicating the tendency of time change in the same manner as in steps S101 and S102 described above. Next, in step S202, the calculated second-order differential value d 2 V / d 2 Using t, the deterioration mode is determined in the same manner as in steps S103 and S104 described above.

[0069] Steps S202 to S204 correspond to the degradation determination unit 13, and step S202 corresponds to the degradation mode determination unit 131. In step S202, the second-order differential value d 2 V / d 2By comparing t with the two thresholds TH1 and TH2, it is determined whether or not the structural deterioration mode (II) is in progress. If the determination in step S202 is affirmative, the process proceeds to step S203, and if the determination is negative, the process returns to step S201.

[0070] Step S203 is a process corresponding to the count unit 132, and stores the number of times that the positive determination was made in step S202 as the count number N. Specifically, the previous count number N+1 is updated as the current count number N. Next, the process proceeds to step S204, and it is determined whether the current count number N exceeds the count threshold value THn. If the determination in step S204 is positive, a deterioration detection signal is output to the abnormality determination unit 103, and the process proceeds to step S205, and if the determination is negative, the process returns to step S201.

[0071] The count threshold value THn is not particularly limited, but may be determined by the count number N and the second derivative value d 2 V / d 2 In relation to t, the count threshold value THn can be set to any number equal to or greater than 4. Depending on how the count threshold value THn is set, in addition to issuing a warning mode notification, it is also possible to take measures such as an emergency shutdown of the system.

[0072] 8, in which the abnormality determination unit 103 outputs an abnormality detection signal to the notification unit AL based on the deterioration detection signal from the deterioration determination unit 13, and notifies the user. Furthermore, in the following step S206, a system stop signal is output, and the operation of the fuel cell module M by the cell control unit C is stopped. Thereafter, this process ends.

[0073] According to this embodiment, the second derivative d 2 V / d 2 Since the presence or absence of an abnormality is judged based on the number of judgments of the structural deterioration mode (II) using t, the risk of erroneous detection is reduced, enabling accurate detection. In addition, by appropriately setting the count threshold value THn and promptly stopping the battery system 1 when there is a safety concern, the reliability of the system is improved. In addition, the same effects as those of the first embodiment are achieved.

[0074] (Embodiment 3) This embodiment shows a specific configuration example of a battery system 1 in which a poisoning detection sensor S1 is provided in a fuel cell module M, as shown in Fig. 11. The poisoning detection sensor S1 can be a sensor equipped with a resistance detection type detection unit that detects a change in electrical resistance due to the adhesion of a poisoning substance, as shown in Fig. 12. Other configurations of the battery system 1 are the same as those in the first embodiment.

[0075] 11, the poisoning detection sensor S1 is attached to a piping section close to an inlet to the cell stack S in a second supply flow passage 202 connected to the air electrode 22 side of the electrochemical cell 2. A preheater 205 for preheating the air to be introduced is provided upstream of the attachment position. In addition, in the second supply flow passage 202, a desulfurizer 206 is disposed upstream of the evaporator 203, and an ejector 207 and a reformer 208 are disposed downstream.

[0076] A combustor 35 is provided on the outlet side of the cell stack S, and the first and second exhaust flow paths 211 and 212 are connected to the combustor 35. The combustor 35 constitutes a part of the fuel recovery section 3, and combusts the fuel gas contained in the first off-gas from the first exhaust flow path 211 to introduce high-temperature combustion gas into the reformer 208 and the preheater 205. A part of the first off-gas is introduced from the recovery flow path 301 to the ejector 207, and a part of the fuel gas to the first supply flow path 201 is introduced from the assist flow path 231 to the upstream side of the first pump P1. A flow rate control valve 232 is provided in the assist flow path 231 to assist the driving flow in the ejector 207. The first off-gas is sucked from the recovery flow path 301 by this driving flow, and is mixed with the driving flow injected from a nozzle provided in the ejector 207.

[0077] 12, the poisoning detection sensor S1 has a housing 81 fixed to the pipe wall of the piping portion that becomes the second supply flow path 202, a sensor element 8 held inside the housing 81, and a cover 82 fixed to both axial sides of the housing H. The cover 82 covers the tip side of the sensor element 8 that protrudes into the second supply flow path 202, and air to be supplied to the cell stack S is introduced through a through hole 82a provided on the side surface of the cover and a through hole 82b provided on the tip surface. The output of the sensor element 8 is input to an external abnormality detection unit 100 at any time.

[0078] As shown enlarged in FIG. 12, the tip of the sensor element 8 has a detection section 83 formed on the surface of an insulating substrate 84, in which a pair of electrodes 85 are arranged in parallel. The insulating substrate 84 is made of insulating ceramics such as alumina (Al2O3), and the pair of electrodes 85 is made of a metal such as platinum (Pt). When a conductive poison 80 such as Cr oxide introduced together with air gradually adheres to the detection section 83 and conducts between the pair of electrodes 85, the electrical resistance between the pair of electrodes 85 decreases according to the amount of poison adhered, and the current i flowing between the pair of electrodes 85 changes. By detecting this decrease in electrical resistance or increase in current i, the degree of poisoning deterioration can be known.

[0079] 13 shows the results of investigating the change in current characteristics due to poisoning using the detection unit 83 configured as above, in which a circuit with a resistor R for current detection was connected between a pair of electrodes 85, and the current flowing when a predetermined voltage was applied was measured while the sensor element 8 was exposed to an atmosphere containing Cr oxide at a predetermined element temperature. As shown in the figure, it was confirmed that the current increased almost in proportion to the increase in the amount of adhesion in the range from operation time T1 (e.g., 3000 hours) to T2 (e.g., 9000 hours).

[0080] Therefore, by storing an arithmetic expression or a map based on this relationship in advance, the poisoning determination unit 101 can detect the amount of poisoning substances attached based on the detection signal from the poisoning detection sensor S1, and can determine the degree of poisoning deterioration. Specifically, a poisoning determination threshold value THps (e.g., the amount of poisoning or a current value corresponding to the operation time T1) can be set in advance and compared with the measurement result so that it can be determined that the deterioration over time is due to poisoning. In addition, the result can be output to the abnormality determination unit 103, and in combination with the determination result in the deterioration determination unit 13, it can be determined whether or not to output an abnormality detection signal.

[0081] 14 is a flowchart showing the procedure of the abnormality detection process according to the present embodiment. Steps S301 and S302 correspond to steps S201 and S202 in FIG. 11. Similarly, the second-order differential value d 2 V / d 2 If the result of step S302 is affirmative and the mode is determined to be structural deterioration mode (II), a deterioration detection signal is output and the process proceeds to step S303, whereas if the result of step S302 is negative, the process returns to step S301.

[0082] Steps S303 to S304 are processes corresponding to the poisoning determination unit 101. In step S303, the signal from the poisoning detection sensor S1 is read, and the poisoning detection sensor value PS is calculated based on the above relational expression or the like. Next, in step S304, it is determined whether the poisoning detection sensor value PS is smaller than the poisoning determination threshold value THps. If the determination in step S304 is affirmative, it is determined that the time-related deterioration mode (I) is not in effect, and some kind of measure is required, so the process proceeds to step S305. If the determination in step S304 is negative, the process returns to step S301. In this case, it is determined that the time-related deterioration mode (I) is in effect, but usually no action such as a notification is taken. Alternatively, the poisoning detection sensor value PS may be output to the battery control unit C to be monitored at appropriate times.

[0083] Steps S305 and S306 correspond to steps S205 and S206 in Fig. 11. In step S305, the abnormality determination unit 103 outputs an abnormality detection signal to notify the user. Furthermore, in step S306, a system stop signal is output to stop the system, and this process ends.

[0084] According to this embodiment, the second derivative d 2 V / d 2 Since the determination of the structural deterioration mode (II) using t is combined with the result of the poisoning determination using the poisoning detection sensor S1, the structural deterioration mode (II) can be distinguished from the time-dependent deterioration mode (I) and detected more accurately, thereby improving the safety and reliability of the battery system 1. In addition, the same effects as those of the first embodiment are achieved.

[0085] (Embodiment 4) This embodiment shows a specific configuration example and operation of a cell stack S provided with a vibration detection sensor S2, as shown in Fig. 15. The vibration detection sensor S2 can be a sensor that uses the AE method described above, and has a detection unit that is attached to the outer surface of the cell stack S. Other configurations of the battery system 1 are the same as those in the first embodiment.

[0086] In the X direction, the cell stack S has a structure in which a laminate such as a cell frame 50 supporting an electrochemical cell 2 is sandwiched between a pair of end plates P. Here, an example of a single-layer structure is shown, but as described above, a multi-layer structure may also be used. A vibration detection sensor S2 is fixed to the cell stack S on the side of one end plate P (the upper one in the figure).

[0087] Piping parts and the like (not shown) that become a first supply flow path 201 for fuel gas or a second supply flow path 202 for supplying air, which is an oxidizing gas, are attached to the cell stack S. Here, the first supply flow path 201 is connected to one end face side of the cell stack S in the Y direction, and the second supply flow path 202 is connected to the other end face side, but the connection structure of the piping parts and the like and the internal flow path structure of the cell stack S are not particularly limited.

[0088] The vibration detection sensor S2 has a load rod S21, a wave guide S22 for transmitting vibration, and a detection unit S23. The load rod S21 protrudes in the X direction from the end plate P, and a predetermined load is applied to it by fastening a fastening member (not shown). The tip of the wave guide S22 is fixed to the side of the load rod S21, and vibrations generated in the cell stack S are taken in by the detection unit S23 provided on the base end side.

[0089] The vibration detection sensor S2 detects vibrations from the cell stack S and outputs the vibration to the vibration determination unit 102 of the abnormality detection unit 100. The vibration determination unit 102 compares the vibration detection sensor value NS with a vibration threshold value THns that has been set in advance through testing or the like, and can output a vibration detection signal when vibration exceeding the vibration threshold value THns is detected. The vibration threshold value THns can be appropriately set so as to be able to detect signs of damage that could lead to a decrease in safety, based on the relationship between structural deterioration such as cracks and peeling that occurs in the constituent layers of the electrochemical cell 2 and the AE waves emitted at that time.

[0090] 16 is a flowchart showing the procedure of the abnormality detection process according to the present embodiment. Steps S401 and S402 correspond to steps S301 and S302 in FIG. 14. Similarly, the second-order differential value d 2 V / d 2 If the result of step S402 is affirmative and the mode is determined to be structural deterioration mode (II), a deterioration detection signal is output and the process proceeds to step S403, whereas if the result of step S402 is negative, the process returns to step S401.

[0091] Steps S403 to S404 are processes corresponding to the vibration determination unit 102. In step S403, the vibration detection sensor value NS based on the signal from the vibration detection sensor S2 is read. Next, in step S404, it is determined whether or not the vibration detection sensor value NS exceeds the vibration determination threshold value THns. If the determination in step S404 is affirmative, it is determined that the vehicle is in the structural deterioration mode (II), and the process proceeds to step S305, whereas if the determination is negative, the process returns to step S301.

[0092] Steps S405 and S406 correspond to steps S305 and S306 in Fig. 14. In step S405, the abnormality determination unit 103 outputs an abnormality detection signal to notify the user based on the deterioration detection signal from the deterioration determination unit 13 and the vibration detection signal from the vibration determination unit 102. Furthermore, in step S406, a system stop signal is output to stop the system, and this process ends.

[0093] According to this embodiment, the second derivative d 2 V / d 2 Since the determination of the structural deterioration mode (II) using t is combined with the results of vibration determination using the vibration detection sensor S2, the structural deterioration mode (II) can be distinguished from the time-related deterioration mode (I) and detected more accurately, thereby improving the safety and reliability of the battery system 1. In addition, the same effects as those of the first embodiment are achieved.

[0094] (Embodiment 5) 17, this embodiment is an embodiment in which the procedure for calculating parameter values ​​in the potential difference monitoring unit 12 of the deterioration detection unit 10 is changed in the abnormality detection process in the abnormality detection unit 100. In this embodiment, when performing abnormality detection using the vibration detection sensor S2 similar to that in the fourth embodiment, correction is performed based on a reference profile of the voltage characteristic change due to the time-dependent deterioration mode (I) prior to calculation of parameter values ​​for deterioration detection. Other configurations of the battery system 1 are the same as those in the first embodiment.

[0095] 18, the change in the voltage characteristics of the electrochemical cell 2 with the passage of operating time shows a relatively large voltage drop at the beginning of operation, while the change with time is relatively gradual in the middle of operation. Therefore, by using an arithmetic expression or a map based on this relationship, the potential difference monitoring unit 12 can calculate the reference correction value Vref according to the operating time, thereby making it possible to correct the amount of change with time.

[0096] The reference profile of the degradation mode (I) shown in Fig. 18 was obtained by carrying out a degradation test over time using an evaluation device equipped with the cell stack S of the full-cell structure shown in Fig. 15. The electrochemical cell 2 was configured with an electrolyte layer 20 made of YSZ, a fuel electrode 21 made of Ni / YSZ, and an air electrode 22 made of LSC. In addition, an intermediate layer 23 made of GDC was disposed between the air electrode 22 and the electrolyte layer 20 via a bonding layer (GDC-LSC).

[0097] 17 is a flowchart showing the procedure of the abnormality detection process according to this embodiment, in which step S501 corresponds to the potential difference detection unit 11 of the deterioration detection unit 10, and steps S502 and S503 correspond to the potential difference monitoring unit 12. From step S503 onwards, similar to step S402 onwards in Fig. 16, abnormality detection is performed by combining the deterioration mode determination based on the parameter values ​​and the vibration determination based on the vibration detection sensor S2.

[0098] First, in step S501, the potential difference V between the fuel electrode 21 and the air electrode 22 of the electrochemical cell 2 is detected. In the following step S502, a reference correction value Vref according to the operation time is calculated, and the reference correction value Vref is subtracted from the detected potential difference V to calculate a corrected potential difference V. Then, in step S503, the corrected potential difference V is used to calculate a second-order differential value d 2 V / d 2 Calculate t.

[0099] Steps S504 to S508 correspond to steps S402 to S506 in FIG. 16, and similarly perform the deterioration mode determination, and can also perform the structural deterioration mode (II) determination in combination with the determination using the vibration detection sensor value NS. It should be noted that, instead of the vibration detection sensor value NS, the poisoning detection sensor value PS in the fourth embodiment may be used for the determination.

[0100] In this way, according to this embodiment, the parameter values ​​for determining the deterioration mode can be calculated by subtracting the influence of changes over time due to aging. This makes it possible to eliminate the influence of an initial voltage drop that is likely to occur in the reversible operation type battery system 1, and to more accurately detect the structural deterioration mode (II) by distinguishing it from the time-related deterioration mode (I), thereby improving the safety and reliability of the battery system 1.

[0101] In order to compare the voltage characteristic changes in the time-dependent degradation mode (I) shown in Fig. 18, Fig. 19 shows a comparison of the voltage characteristic changes obtained by performing a degradation test in a structural degradation mode (II) and the voltage gradient range of the voltage characteristic line using the logarithm of the voltage change over time. As shown in Fig. 19, in the time-dependent degradation mode (I), Log(dV / dt) is in the range of -5.3 to 3.7 [V / h], whereas in the structural degradation mode (II), it is in the range of 0.2 to 0.7 [V / h], showing a large difference.

[0102] As shown in Fig. 20, by utilizing such a difference, it is possible to detect the structural deterioration mode (II) by distinguishing it from the aging deterioration mode (I). Fig. 20 shows the results of the procedure shown in the first embodiment, in which the second-order differential value d 2 V / d 2 In the time-deterioration mode (I), no inversion is observed (inversion count 0 times / h). In contrast, in the structural deterioration mode (II), a sufficient number of inversions is confirmed, and more accurate detection is possible, for example, by appropriately setting the count threshold value THn shown in the second embodiment.

[0103] According to each of the above embodiments, it is possible to accurately detect the deterioration mode of the electrochemical cell 2 used in the battery system 1. When a cell stack S is formed by stacking a plurality of electrochemical cells 2, and when a fuel cell module M is formed by combining a plurality of cell stacks S, the deterioration mode may be detected for each unit cell, or the deterioration mode may be determined for a plurality of unit cells to detect a portion where deterioration due to structural deterioration mode (II) has occurred.

[0104] The present invention is not limited to the above-described embodiments, and can be applied to various embodiments without departing from the gist of the present invention. For example, the poisoning detection device has been described as having a configuration in which the poisoning detection sensor S1 is provided in the piping section that serves as the inlet of the cell stack S, but the device may also be configured such that a pair of electrodes are arranged in a detection section provided inside the cell stack S, allowing the poisoning substance to adhere thereto. The configuration of the cell stack S using the electrochemical cell 2 and the configuration of the fuel cell module M are not limited to the above-described configurations, and can be changed according to the application of the battery system 1, etc. In addition, the procedure of the abnormality detection process by the abnormality detection section 100 shown in each of the above-described embodiments may be partially changed or combined. [Explanation of symbols]

[0105] 1. Solid oxide battery system 100 Abnormality detection unit 10 Deterioration detection section 11 Potential difference detection section 12 Potential difference monitor 13 Deterioration determination section 2. Electrochemical Cell 20 Electrolyte layer 21 Fuel electrode (1st electrode) 22 Air electrode (second electrode)

Claims

1. an electrochemical cell (2) including an electrolyte layer (20) using a solid oxide ceramic, a first electrode (21) provided on a first surface (20a) of the electrolyte layer, and a second electrode (22) provided on a second surface (20b) of the electrolyte layer opposite to the first surface; A solid oxide battery system (1) comprising: a deterioration detection unit (10) that detects structural deterioration of the electrochemical cell, The deterioration detection unit is a potential difference detection unit (11) that detects a potential difference between the first electrode and the second electrode; a potential difference monitoring unit (12) for monitoring a trend of time change of the detected potential difference; and a deterioration determination unit (13) that determines whether or not the structure of the electrochemical cell has deteriorated based on the increase / decrease tendency of the time change of the potential difference.

2. the potential difference monitoring unit calculates a parameter value indicating an increase / decrease tendency of a time change of the detected potential difference; 2. The solid oxide battery system according to claim 1, wherein the deterioration determination unit determines that the electrochemical cell is in a structural deterioration mode when the calculated parameter value shows a tendency of positive / negative reversal.

3. The potential difference monitoring unit detects the second derivative of the detected potential difference with respect to time (d 2 V / d 2 t) is calculated, 3. The solid oxide battery system according to claim 2, wherein the deterioration determination unit sets a threshold value for determining deterioration based on a comparison between a trend of increase / decrease in the time change of the potential difference due to structural deterioration of the electrochemical cell and a trend of increase / decrease in the time change of the potential difference due to deterioration over time of the electrochemical cell.

4. 4. The solid oxide battery system according to claim 3, wherein the degradation determination unit determines that the electrochemical cell is in the structural degradation mode when the parameter value becomes smaller than a first threshold value (TH1) on the negative side and then becomes larger than a second threshold value (TH2) on the positive side.

5. 4. The solid oxide battery system according to claim 3, wherein the degradation determination unit includes a counting unit (132) that counts the number of times the electrochemical cell is determined to be in the structural degradation mode, and determines that the electrochemical cell is in the structural degradation mode when the number (n) counted by the counting unit exceeds a count threshold (THn).

6. a degradation detection device for detecting a degradation state of the electrochemical cell over time; An abnormality determination unit (103) that determines whether or not there is a deterioration abnormality based on the determination result of the deterioration determination unit, 5. The solid oxide battery system according to claim 3, wherein the abnormality determination unit determines that the abnormality is due to structural deterioration and outputs an abnormality detection signal when the deterioration determination unit determines that the electrochemical cell is in the structural deterioration mode and the detection result of the time-deterioration detection device determines that the electrochemical cell is not in a state of time-deterioration.

7. 7. The solid oxide battery system according to claim 6, wherein the time-deterioration detection device is a poisoning detection sensor (S1) having a detection unit (83) for detecting a conductive poison, and the detection unit detects a change in electrical resistance between a pair of electrodes (85) provided on an insulating substrate (84).

8. a vibration detection device for detecting a vibration state caused by structural deterioration of the electrochemical cell; An abnormality determination unit (103) that determines whether or not there is a deterioration abnormality based on the determination result of the deterioration determination unit, 5. The solid oxide battery system according to claim 3, wherein when the deterioration determination unit determines that the electrochemical cell is in the structural deterioration mode and the detection result of the vibration detection device determines that the electrochemical cell is in a vibration state associated with structural deterioration, the abnormality determination unit determines that the abnormality is due to structural deterioration and outputs an abnormality detection signal.

9. 9. The solid oxide battery system according to claim 8, wherein the vibration detection device is a vibration detection sensor (S2) having a detection portion using an acoustic emission method.

10. 5. The solid oxide battery system according to claim 3, wherein the potential difference monitoring unit corrects the potential difference detected by the potential difference detection unit (11) using a reference correction value (Vref) based on a reference profile of deterioration over time of the electrochemical cell.

11. 5. The solid oxide battery system according to claim 3, wherein the electrochemical cell is a reversible cell capable of power generation or electrolysis.

Citation Information

Patent Citations

  • Real-time monitoring and automated intervention platform for long term operability of fuel cells

    US10461347B2