Aluminum profile injection bonding method

The aluminum profile injection joining method addresses deformation and leakage issues in welding by integrating product and mold preparation stages with injection filling, enabling stable and cost-effective assembly of electric vehicle battery housings.

JP2024155719AActive Publication Date: 2024-10-31キムビョンチャン
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2024009038
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-21
Filing Date
2024-01-24
Publication Date
2024-10-31
Estimated Expiration
2044-01-24

AI Technical Summary

Technical Problem

Conventional welding methods for joining aluminum profiles in electric vehicle battery housings result in deformation, require additional deformation prevention members and steps, are difficult to rework, and pose a high risk of leakage.

Method used

An aluminum profile injection joining method involving product preparation, mold preparation, and injection filling stages, including mold gate formation, side through hole creation, pin insertion, and block mounting, to integrate aluminum profiles without deformation and leakage risks.

Benefits of technology

Facilitates easy joining of aluminum profiles with various cross-sectional structures, maintains a stable joint state, reduces the need for additional members, and significantly lowers production and construction costs while shortening construction time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155719000001_ABST
    Figure 2024155719000001_ABST
Patent Text Reader

Abstract

To provide an aluminum profile injection bonding method.SOLUTION: An aluminum profile injection bonding method includes: a product preparation step of manufacturing a plurality of aluminum profiles to be bonded in accordance with a product design; a mold preparation step of manufacturing a mold designed in accordance with the aluminum profiles prepared through the product preparation step; a seating step of seating the plurality of aluminum profiles to be bonded in the mold in a state of being in contact with each other; and an injection filling step of constructing the aluminum profiles to be bonded in an integrated form by filling contact portions of the aluminum profiles with an injection molded material through the mold. The aluminum profile injection bonding method can be provided in which, when manufacturing an electric vehicle battery housing, aluminum profiles with various cross-sectional structures can be easily joined and a stable joint state can be maintained, a large number of bonding or binding members can be omitted, the cost of production and construction can be significantly reduced, and the construction time can be significantly reduced.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an aluminum profile injection joining method, and more particularly to a profile injection joining method for battery housings for electric vehicles. [Background technology]

[0002] The present invention relates to a method for joining multiple aluminum profiles that make up an electric vehicle battery housing, and aims to overcome the problems associated with prior art welding joining methods.

[0003] In the case of the conventional welding joining method, there is a problem that the aluminum profile is deformed after welding. Specifically, the aluminum profile has a characteristic of being deformed by heat of 500 to 600 degrees Celsius, and the heat generated during welding causes thermal deformation of the aluminum profile.

[0004] For this reason, in order to weld a number of aluminum profiles together to create a desired structure, a number of deformation prevention members and a number of additional processes after welding are required to prevent welding deformation. As a result, the conventional welding joining method has a problem in that it is very difficult to accurately adjust tolerances such as flatness and hole position. In addition, the weld bead line interferes with the mounting part, so the weld bead must be removed through a grinding process, which requires an additional process, and it is very fragile to adjust the flatness, resulting in a high risk of leakage.

[0005] Furthermore, in the case of the conventional welding method, it is very difficult to rework the product after a welding defect is found, and the product must be discarded.

[0006] Therefore, there is a need for a technology that can solve the above-mentioned problems of the conventional technology, simplify the steps of the conventional bonding method, prevent deformation of the product, and fundamentally eliminate the risk of leaks. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Korean Patent Publication No. 10-1277453 (Registration Date: June 17, 2013) Summary of the Invention [Problem to be solved by the invention]

[0008] The object of the present invention is to provide an aluminum profile injection joining method that can easily join aluminum profiles having various cross-sectional structures, maintain a stable joining state, and omit a large number of joining and binding members when manufacturing an electric vehicle battery housing, thereby significantly reducing the costs of manufacturing and construction, and also significantly shortening the construction time. [Means for solving the problem]

[0009] To achieve this object, an aluminum profile injection joining method according to one aspect of the present invention may include a product preparation step of preparing a number of aluminum profiles to be joined according to a product design, a mold preparation step of preparing a mold designed to match the aluminum profiles prepared through the product preparation step, a seating step of seating the number of aluminum profiles to be joined in the mold while being in contact with each other, and an injection filling step of filling contact portions of the aluminum profiles through the mold with an injection material to integrally form the aluminum profiles to be joined.

[0010] In one embodiment of the present invention, the mold preparation step may include a mold gate formation step of forming a mold gate having a structure in which an injection material is discharged through the mold and guided into an aluminum profile joint, in accordance with a position in which a filling hole in the aluminum profile is formed.

[0011] In one embodiment of the present invention, the injection filling step may include a side through-hole forming step of forming a through-hole on a side of the aluminum profile to guide the injection material to be integrally bound to the aluminum profile.

[0012] In an embodiment of the present invention, the injection and filling step may include a pin insertion step of integrally binding the injection molded object and the aluminum profile by inserting a pin into the through hole formed in the side through hole forming step.

[0013] In one embodiment of the present invention, the injection filling step may include a block mounting step of mounting a block inside the aluminum profile so as to form a space of a predetermined volume adjacent to the joint inside the aluminum profile. Effect of the Invention

[0014] As described above, according to the aluminum profile injection joining method of the present invention, by including a product preparation step, a mold preparation step, a seating step, and an injection filling step for performing specific processes, it is possible to easily join aluminum profiles having various cross-sectional structures when manufacturing an electric vehicle battery housing, maintain a stable joining state, and omit a large number of joining members and bundling members, thereby significantly reducing the cost of manufacturing and construction, and in addition, significantly shortening the construction time. [Brief description of the drawings]

[0015] [Figure 1] Photographs showing an aluminum profile joining process according to the prior art. [Diagram 2] 1 is a photograph showing the state of an aluminum profile joined by a conventional welding method. [Diagram 3] 2 is a flowchart illustrating an aluminum profile bonding method according to an embodiment of the present invention. [Figure 4] 10 is a flowchart illustrating an aluminum profile bonding method according to yet another embodiment of the present invention. [Diagram 5] This is a perspective view showing how two aluminum profiles to be joined are butted together and a filling hole is formed. [Figure 6] FIG. 5 is a schematic plan view showing a state in which a number of aluminum profiles butted against each other are placed on a die. [Figure 7] FIG. 7 is a schematic plan view showing the state in which the aluminum profile is filled with an injection material from the mold shown in FIG. 6. [Figure 8] 1 is a schematic plan view showing the state in which a block is inserted inside the aluminum profile and the aluminum profile is filled with injection material from a mold. FIG. [Figure 9] 1 is a perspective view showing how a pin is inserted after a through hole is formed in an aluminum profile. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the drawings. Prior to this, the terms and words used in the present specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted as meanings and concepts that correspond to the technical ideas of the present invention.

[0017] Throughout this specification, when a member is said to be "on" another member, this includes not only when the member is in contact with the other member, but also when there is another member between the two members. Throughout this specification, when a part is said to "include" a certain component, this does not mean that the other component is excluded, but that the part may further include the other component, unless otherwise specified.

[0018] FIG. 3 shows a flow chart illustrating an aluminum profile bonding method according to one embodiment of the present invention.

[0019] Referring to FIG. 3, the aluminum profile joining method S100 according to the present embodiment includes a product preparation step S110, a mold preparation step S120, a seating step S130, and an injection filling step S140, which perform specific processes. This allows aluminum profiles having various cross-sectional structures to be easily joined when manufacturing an electric vehicle battery housing, and a stable joining state can be maintained. It is also possible to omit a large number of joining members and bundling members, thereby significantly reducing the cost of manufacturing and construction, and in addition, it is possible to provide an aluminum profile injection joining method that significantly shortens the construction time.

[0020] Hereinafter, each component constituting the aluminum profile injection joining method S100 according to this embodiment will be described in detail with reference to the drawings.

[0021] FIG. 4 shows a flow chart of an aluminum profile joining method according to another embodiment of the present invention, and FIG. 5 shows a perspective view of a state in which two aluminum profiles to be joined are butted against each other and a filling hole is formed. FIG. 6 shows a schematic plan view of a state in which a number of aluminum profiles butted against each other are placed on a mold as shown in FIG. 5, FIG. 7 shows a schematic plan view of a state in which an injection material is filled into the aluminum profile from the mold shown in FIG. 6, and FIG. 8 shows a schematic plan view of a state in which an injection material is filled into the aluminum profile from the mold with a block inserted into the aluminum profile. FIG. 9 shows a perspective view of a state in which a pin is inserted after a through hole is formed in the aluminum profile.

[0022] In the product preparation step S110 according to this embodiment, a number of aluminum profiles to be joined are prepared according to a product design.

[0023] In the mold preparation step S120 according to this embodiment, a mold designed according to the aluminum profile prepared in the product preparation step S110 is manufactured.

[0024] Specifically, the mold preparation step S120 may include a mold gate formation step S121, a side through hole formation step S141, a pin insertion step S142, and a block mounting step S143, which perform specific processes. The mold gate formation step S121 of the mold preparation step S120 performs a process of forming a mold gate, which is structured to guide the injection material discharged through the mold into the aluminum profile joint, in accordance with a filling hole formation position of the aluminum profile. The side through hole formation step S141 performs a process of processing a through hole 12 on the side of the aluminum profile to guide the injection material to be integrally bound with the aluminum profile, as shown in Figs. 6 and 9. The pin insertion step S142 performs a process of inserting a pin 30 into the through hole formed in the side through hole formation step S141 to integrally bind the injection material and the aluminum profile, as shown in Fig. 9. In the block mounting step S143, as shown in FIG. 8, a block 40 is mounted inside the aluminum profile so as to form a space of a predetermined volume adjacent to the joint inside the aluminum profile.

[0025] In the step of mounting (S130) according to the present embodiment, a process of preparing a mold designed according to the aluminum profile prepared in the step of preparing a product (S110) is performed.

[0026] In the injection filling step S140 according to the present embodiment, an injection material is filled into the contact portion of the aluminum profiles through a mold, thereby forming an integrally joined aluminum profile.

[0027] As described above, according to the aluminum profile injection joining method of the present invention, by including a product preparation step S110, a mold preparation step S120, a seating step S130, and an injection filling step S140 for performing specific processes, it is possible to provide an aluminum profile injection joining method S100 that can easily join aluminum profiles having various cross-sectional structures when manufacturing an electric vehicle battery housing, maintain a stable joining state, and omit a large number of joining members and bundling members, thereby significantly reducing the cost of manufacturing and construction, and in addition, significantly shortening the construction time.

[0028] Although the above detailed description of the present invention has described only specific embodiments thereof, it should be understood that the present invention is not limited to the specific forms set forth in the detailed description, but rather includes all modifications, equivalents, and alternatives falling within the spirit and scope of the present invention as defined by the appended claims.

[0029] In other words, the present invention is not limited to the specific embodiments and explanations described above, and various modifications can be made by anyone having ordinary knowledge in the technical field to which the present invention belongs without departing from the gist of the present invention as claimed in the claims, and such modifications are within the scope of protection of the present invention. [Explanation of symbols]

[0030] S100: Aluminum profile injection joining method S110: Product preparation stage S120: Mold preparation stage S121: Mold gate formation stage S130: Safe landing stage S140: Injection filling stage S141: Side through hole formation step S142: Pin insertion stage S143: Block installation stage 10: Aluminum profile 11:Filling hole 12:Through hole 20: Mold 30: Pin 40: Block 50: Projectile

Claims

1. A product preparation step S110 in which a number of aluminum profiles to be joined are prepared according to a product design; A mold preparation step (S120) of preparing a mold designed according to the aluminum profile prepared through the product preparation step (S110); A step S130 of mounting a plurality of aluminum profiles to be joined on a mold while the aluminum profiles are in contact with each other; and The injection filling step S140 includes filling the aluminum profile contact portion through a mold with an injection material to integrally form the aluminum profile. An aluminum profile injection joining method comprising the steps of:

2. The mold preparation step S120 includes: The method includes a mold gate forming step (S121) for forming a mold gate, which is structured so that the injection material is discharged through the mold and guided into the aluminum profile joint, in accordance with a filling hole of the aluminum profile. The aluminum profile injection joining method according to claim 1.

3. The injection and filling step S140 includes: The method includes a side through-hole forming step (S141) of forming a through-hole 12 on a side of the aluminum profile to guide the extrusion to be integrally bound to the aluminum profile. The aluminum profile injection joining method according to claim 1.

4. The injection and filling step S140 includes: The method includes a pin inserting step (S142) of inserting a pin 30 into the through hole formed in the side through hole forming step (S141) to integrally bind the injection molded object and the aluminum profile. The aluminum profile injection joining method according to claim 3.

5. The injection and filling step S140 includes: and a block mounting step (S143) of mounting a block (40) inside the aluminum profile so as to form a space of a predetermined volume adjacent to the joint inside the aluminum profile. The aluminum profile injection joining method according to claim 1.

Citation Information

Patent Citations

  • Structure, method of manufacturing it, housing body device and portable terminal device

    JP2001277292A

  • Case of portable electronic device

    JP2007227423A

  • Bonded composite article of a plurality of metallic shaped bodies, and method for production thereof

    JP2009298144A

  • Clamp device removably connecting two profile parts

    JP2014016028A

  • Resin mold molding method

    JP2018001455A