Electronic component and manufacturing method thereof
The innovative substrate design with a grooved lower electrode and dual-metal-containing layers addresses miniaturization and reliability issues in MIM capacitors, achieving stable capacitance and improved reliability.
Patent Information
- Application Number
- JP2023072419
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-26
- Publication Date
- 2024-11-08
AI Technical Summary
Existing methods for miniaturizing passive elements and achieving high-density mounting on wiring boards face limitations, and MIM capacitors suffer from reliability issues due to stress-induced variations in capacitance.
A substrate with a lower electrode having a groove extending perpendicularly to its end surface, creating an overhang between the groove and a dielectric layer, and utilizing a dual-metal-containing layer with differing linear expansion coefficients to alleviate stress and maintain shape accuracy.
This design results in MIM capacitors with reduced capacitance variations and enhanced reliability by preventing excessive stress on the dielectric layer, ensuring consistent performance under thermal stress.
Smart Images

Figure 2024157822000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to electronic components. [Background technology]
[0002] As electronic devices become more sophisticated and smaller, there is an increasing demand for higher density wiring boards that constitute semiconductor devices. As circuit wiring is required to be finer, passive elements such as resistors, capacitors, and inductors are also required to be further miniaturized. This further miniaturization is required at a very high level, and there are limitations to the miniaturization of passive elements and their high density mounting in the method of surface mounting passive elements on wiring boards.
[0003] In order to solve such problems, a technique for embedding passive elements in a wiring board has been proposed (for example, Patent Document 1). In the method of Patent Document 1, passive elements are formed by printing or vacuum film formation, and then embedded in a wiring board. Therefore, this method makes it possible to miniaturize passive elements.
[0004] Furthermore, a metal-insulator-metal (MIM) capacitor may be formed on the wiring board. The MIM capacitor has a structure in which an insulating layer is sandwiched between a pair of conductive layers. The MIM capacitor has a problem in that stress caused by the structure reduces reliability. Patent Document 2 proposes adopting a specific structure at the end of the MIM capacitor to address this reliability reduction. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2000-151114 A [Patent Document 2] International Publication No. 2019 / 244382 Summary of the Invention [Problem to be solved by the invention]
[0006] An object of the present invention is to provide a technique that is advantageous in realizing an MIM capacitor with small variations in capacitance. [Means for solving the problem]
[0007] According to one aspect of the present invention, there is provided an electronic component comprising a substrate having an insulating first surface and a second surface which is the back surface of the insulating first surface, a lower electrode provided on the first surface, a dielectric layer provided on the lower electrode, and an upper electrode provided on the dielectric layer, wherein the lower electrode has an end surface on which a groove extending perpendicular to a thickness direction of the lower electrode is provided, the groove surrounding the lower electrode so as to generate an overhang portion between the groove and the dielectric layer, and a first contour on the inside of an orthogonal projection of the groove onto a plane perpendicular to the thickness direction is spaced from and surrounded by a second contour of the orthogonal projection of the dielectric layer onto the plane.
[0008] According to another aspect of the present invention, there is provided an electronic component relating to the above aspect, in which a distance t1 from the deepest part of the groove, which has the greatest depth, to the dielectric layer is shorter than a distance t2 from the deepest part to the substrate.
[0009] According to yet another aspect of the present invention, there is provided an electronic component according to any of the above aspects, wherein an area of a region enclosed by the first contour is within a range of 90% to 99% of an area of a region of the lower electrode that is in contact with the dielectric layer.
[0010] According to yet another aspect of the present invention, there is provided an electronic component relating to any of the above aspects, wherein a distance t1 from an innermost portion of the groove, which is the deepest portion, to the dielectric layer is shorter than a distance t4 from the innermost portion to a plane including an edge of the groove located on the substrate side.
[0011] According to yet another aspect of the present invention, there is provided an electronic component relating to any of the above aspects, wherein the lower electrode includes a first metal-containing layer made of a first material and a second metal-containing layer made of a second material different from the first material, the second metal-containing layer is interposed between the first metal-containing layer and the dielectric layer, and the interface between the first metal-containing layer and the second metal-containing layer is located in an deepest part of the groove that has the greatest depth, or is located between the deepest part and the dielectric layer.
[0012] According to yet another aspect of the present invention, there is provided an electronic component according to the above aspect, wherein the linear expansion coefficient of the second material is greater than the linear expansion coefficient of the material of the dielectric layer and smaller than the linear expansion coefficient of the first material.
[0013] According to yet another aspect of the present invention, there is provided the electronic component according to any of the above aspects, wherein the second material has a greater elastic modulus than the first material.
[0014] According to yet another aspect of the present invention, there is provided an electronic component according to any of the above aspects, wherein a third contour of an orthogonal projection of the upper electrode onto the plane is spaced apart from and surrounded by the second contour.
[0015] According to yet another aspect of the present invention, there is provided an electronic component according to any of the above aspects, wherein a third contour of an orthogonal projection of the upper electrode onto the plane is spaced apart from and surrounded by the first contour.
[0016] According to yet another aspect of the present invention, there is provided an electronic component relating to any of the above aspects, wherein the lower electrode includes a first conductor portion having a surface facing the dielectric layer, and a second conductor portion protruding from the center of the surface of the first conductor portion toward the dielectric layer, and the groove is provided on a side surface of the second conductor portion.
[0017] According to yet another aspect of the present invention, there is provided an electronic component according to any one of the above aspects, which is a wiring board.
[0018] According to yet another aspect of the present invention, there is provided a method for manufacturing an electronic component having a capacitor including a lower electrode, an upper electrode, and a dielectric layer interposed therebetween, the method including the steps of: preparing a substrate having an insulating first surface and a second surface which is an opposite surface of the insulating first surface; forming a first metal-containing layer on the first surface; providing an etching mask on the first metal-containing layer so as to cover a portion of an upper surface of the first metal-containing layer; thereafter, etching the first metal-containing layer to recess an area of the upper surface not covered by the etching mask, thereby generating in the first metal-containing layer a first portion and a second portion protruding from a center of an upper surface of the first portion; removing the etching mask; and forming a resist layer which embeds the first portion and has a through hole at the position of the second portion, the upper surface of which is a front surface of the first metal-containing layer. forming a second metal-containing layer on the second portion and the resist layer, forming a dielectric material layer on the second metal-containing layer, forming an upper electrode on a portion of the dielectric material layer facing the upper surface of the second portion, and removing the resist layer together with the second metal-containing layer and portions of the dielectric material layer covering the upper surface of the resist layer to form a lower electrode including the first metal-containing layer and the portion of the second metal-containing layer that was located in the through hole, and a dielectric layer including the portion of the dielectric material layer that was located in the through hole.
[0019] According to yet another aspect of the present invention, there is provided a method for manufacturing an electronic component having a capacitor including a lower electrode, an upper electrode, and a dielectric layer interposed therebetween, the method comprising the steps of: preparing a substrate having an insulating first surface and a second surface which is an opposite surface of the insulating first surface; forming a first metal-containing layer made of a first material on the first surface; forming a second metal-containing layer made of a second material different from the first material on the first metal-containing layer; forming a dielectric material layer on the second metal-containing layer; forming an upper electrode on the dielectric material layer, the upper electrode covering a portion of an upper surface of the dielectric material layer at the position of the first metal-containing layer; and patterning the dielectric material layer so that at least a portion sandwiched between the first metal-containing layer and the upper electrode remains, to form a dielectric layer. and etching the first metal-containing layer such that a portion of an upper surface of the first metal-containing layer not covered with the patterned second metal-containing layer is recessed and side etching occurs at a portion of the upper surface of the first metal-containing layer covered with the patterned second metal-containing layer, thereby forming a first portion and a second portion in the first metal-containing layer protruding from a center of an upper surface of the first portion, thereby forming a lower electrode including the first metal-containing layer provided with the first portion and the second portion, and the patterned second metal-containing layer. Effect of the Invention
[0020] The present invention provides an advantageous technique for realizing an MIM capacitor with small capacitance variation. [Brief description of the drawings]
[0021] [Figure 1] FIG. 1 is a top view of an electronic component according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II of the electronic component shown in FIG. [Diagram 3]FIG. 3 is a top view of a capacitor included in the electronic component of FIGS. [Figure 4] FIG. 4 is a cross-sectional view of the capacitor taken along line IV-IV shown in FIG. [Diagram 5] FIG. 5 is a cross-sectional view of a capacitor according to a first modification. [Figure 6] FIG. 6 is a cross-sectional view showing a step in the manufacture of the electronic component shown in FIGS. [Figure 7] FIG. 7 is a cross-sectional view showing another process in the manufacture of the electronic component shown in FIGS. [Figure 8] FIG. 8 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 9] FIG. 9 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 10] FIG. 10 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 11] FIG. 11 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 12] FIG. 12 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 13] FIG. 13 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 14] FIG. 14 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 15] FIG. 15 is a cross-sectional view showing still another step in the manufacture of the electronic component shown in FIGS. [Figure 16] FIG. 16 is a cross-sectional view showing a step in the manufacture of the capacitor shown in FIGS. [Figure 17] FIG. 17 is a cross-sectional view showing another step in the manufacture of the capacitor shown in FIGS. [Figure 18]FIG. 18 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Figure 19] FIG. 19 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Figure 20] FIG. 20 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Figure 21] FIG. 21 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Figure 22] FIG. 22 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Diagram 23] FIG. 23 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIGS. [Figure 24] FIG. 24 is a cross-sectional view of a capacitor included in an electronic component according to a second embodiment of the present invention. [Diagram 25] FIG. 2 is a cross-sectional view of a capacitor according to a second modification. [Figure 26] FIG. 26 is a cross-sectional view showing a step in the manufacture of the capacitor shown in FIG. [Figure 27] FIG. 27 is a cross-sectional view showing another step in the manufacture of the capacitor shown in FIG. [Figure 28] FIG. 28 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIG. [Figure 29] FIG. 29 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIG. [Diagram 30] FIG. 30 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIG. [Diagram 31] FIG. 31 is a cross-sectional view showing still another step in the manufacture of the capacitor shown in FIG. [Diagram 32] FIG. 32 is a cross-sectional view of a capacitor included in the electronic component according to Comparative Example 1. As shown in FIG. [Diagram 33]FIG. 33 is a cross-sectional view of a capacitor included in an electronic component according to Comparative Example 2. As shown in FIG. [Diagram 34] FIG. 34 is a cross-sectional view of a capacitor included in an electronic component according to Comparative Example 3. As shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] Hereinafter, embodiments of the present invention will be described with reference to the drawings. The embodiments described below are more specific embodiments of any of the above aspects. The following items can be incorporated into each of the above aspects alone or in combination.
[0023] The embodiments described below are merely examples of configurations for embodying the technical idea of the present invention, and the technical idea of the present invention is not limited by the materials, shapes, structures, etc. of the components described below. Various modifications can be made to the technical idea of the present invention within the technical scope defined by the claims.
[0024] In addition, elements having the same or similar functions are given the same reference numerals in the drawings referred to below, and duplicated explanations are omitted. In addition, the drawings are schematic, and the relationship between dimensions in one direction and dimensions in another direction, the relationship between the dimensions of one member and the dimensions of another member, etc. may differ from the actual ones.
[0025] In the following, the terms "upper" and "lower" are used to indicate positions in the thickness direction of a layer, and correspond to the upper and lower sides, respectively, in a cross-sectional view. In addition, the terms "upper surface" and "lower surface" used in the following mean the upper and lower main surfaces, respectively, of the two main surfaces of a layer whose cross section is drawn so that the thickness direction is the vertical direction.
[0026] <1> First embodiment <1.1> Electronic components Fig. 1 is a top view of an electronic component according to a first embodiment of the present invention. Fig. 2 is a cross-sectional view taken along line II-II of the electronic component shown in Fig. 1. Fig. 3 is a top view of a capacitor included in the electronic component shown in Figs. 1 and 2. Fig. 4 is a cross-sectional view taken along line IV-IV of the capacitor shown in Fig. 3.
[0027] It should be noted that a conductive layer 24a, which will be described later, is omitted in Fig. 1. Moreover, in addition to the conductive layer 24a, an interlayer insulating film 40a, which will be described later, is also omitted in Figs. 3 and 4.
[0028] The electronic component 10 shown in Figures 1 and 2 is a wiring board, specifically a multilayer wiring board. The electronic component 10 can be used as an interposer that relays components with different inter-terminal distances, such as an integrated circuit (IC) chip and a printed wiring board that have different wiring design rules. Note that, although an interposer is shown in Figures 1 and 2 as an example of an electronic component, the technology described here can also be applied to other electronic components, such as a passive element embedded substrate, a semiconductor package substrate, and a substrate for optical elements.
[0029] As shown in FIG. 2, the electronic component 10 includes a substrate 11, a conductive layer 12, a dielectric layer 13, an upper electrode 14, a conductive layer 22, an interlayer insulating film 40a, an interlayer insulating film 40b, a conductive layer 24a and a conductive layer 24b.
[0030] The substrate 11 has a first surface 11a and a second surface 11b, which is the reverse surface of the first surface 11a. The first surface 11a is insulating. In each drawing, the X direction and the Y direction are parallel to the first surface 11a and perpendicular to each other. The Z direction is perpendicular to the X direction and the Y direction, that is, the thickness direction of the substrate 11.
[0031] The substrate 11 is made of glass such as non-alkali glass. The substrate 11 may be made of an inorganic insulating material other than glass, may be made of an organic material, or may be a semiconductor substrate. The substrate 11 has insulating properties at least on its surface, and is desirably made of an insulating material. Here, as an example, the substrate 11 is a glass substrate.
[0032] The thickness of the substrate 11 is preferably in the range of 50 μm to 700 μm. According to one example, the thickness of the substrate 11 is 400 μm.
[0033] The surface roughness (arithmetic mean roughness Ra) of the first surface 11a is preferably small from the viewpoint of preventing transmission loss of high frequency signals in the conductive layers 12 and 22, and is preferably, for example, 50 nm or less, and particularly preferably within the range of 0.1 nm to 30 nm. The arithmetic mean roughness Ra is defined in JIS B0601:2001.
[0034] The substrate 11 is provided with one or more through holes 11H each extending from the first surface 11a to the second surface 11b. Here, the substrate 11 is provided with a plurality of through holes 11H. Here, the through holes 11H are via holes.
[0035] The opening width of the through hole 11H is preferably within a range of 40 μm to 110 μm. Here, as an example, the opening width of the through hole 11H is set to 80 μm.
[0036] Here, the opening width of the through hole 11H is a dimension defined as follows. That is, a reference plane parallel to the first surface 11a is moved from the first surface 11a to the second surface 11b, and the maximum distance between two points on a figure formed by the intersection line between the side wall of the through hole 11H and the reference plane is obtained at each position. The maximum value of the maximum distances thus obtained is set as the opening width of the through hole 11H. Note that, if all of the figures are circles, the opening width of the through hole 11H is the diameter of the largest circle.
[0037] The maximum distance may vary within the section from the first surface 11a to the second surface 11b. In this case, the function of the maximum distance, which uses the distance from the first surface 11a to the reference surface as a variable, may not have either a minimum value or a maximum value. For example, the maximum distance may increase or decrease as the distance from the first surface 11a to the reference surface increases. In addition, the function of the maximum distance, which uses the distance from the first surface 11a to the reference surface as a variable, may have a minimum value, a maximum value, or both a minimum value and a maximum value. Here, the through hole 11H has a truncated cone shape tapered from the second surface 11b to the first surface 11a.
[0038] The maximum distance may be constant within the section from the first surface 11a to the second surface 11b. For example, the through-hole 11H may have a cylindrical shape with its height direction parallel to the Z direction.
[0039] The through-holes 11H can be formed in the substrate 11 by, for example, etching, laser processing, a combination of laser processing and etching, sandblasting, electric discharge processing, or drilling.
[0040] The conductive layer 12 is provided on the first surface 11a. The conductive layer 12 includes a wiring portion, a land portion, and a lower electrode of the capacitor 100A described later. In Fig. 1, the rectangular portion at the left end of the conductive layer 12 corresponds to the lower electrode.
[0041] 4, the conductive layer 12 includes a seed layer 121 and a main conductor layer 122. The seed layer 121 and the main conductor layer 122 are laminated on the substrate 11 in this order.
[0042] The seed layer 121 is provided on the first surface 11a. The seed layer 121 is a part of a power supply layer for forming the main conductor layer 122 by electrolytic plating.
[0043] Here, as an example, the seed layer 121 is a film made of copper (Cu). The seed layer 121 may be a film made of other metals such as chromium (Cr) and titanium (Ti), or may be a laminate made of multiple metal films.
[0044] The thickness of the seed layer 121 is preferably in the range of 20 nm to 800 nm. Here, as an example, the thickness of the seed layer 121 is set to 300 nm.
[0045] The seed layer 121 can be formed by electroless plating, sputtering, etc. The seed layer 121 may be formed by other methods. The seed layer 121 may be omitted.
[0046] The main conductor layer 122 is provided on the seed layer 121. Here, as an example, the main conductor layer 122 is a film made of copper. The main conductor layer 122 may be a film made of another material having electrical conductivity, or may be a laminate made of multiple conductive films.
[0047] The thickness of the main conductor layer 122 is preferably within a range of 0.5 μm to 30 μm. Here, as an example, the thickness of the main conductor layer 122 is assumed to be 8 μm.
[0048] The main conductor layer 122 can be formed by, for example, electrolytic plating. The main conductor layer 122 may be a copper layer formed by sputtering or an electrolytic copper foil that is patterned by etching.
[0049] As described above, the conductive layer 12 includes the seed layer 121 and the main conductor layer 122. The conductive layer 12 may further include one or more other conductive layers. For example, when the through hole 11H is formed in the substrate 11 by etching, the conductive layer 12 may further include an etching stopper film interposed between the seed layer 121 and the substrate 11. The etching stopper film is, for example, a layer made of chromium and formed by a sputtering method.
[0050] Here, the conductive layer 12 is provided on the substrate 11 so as to be in contact with the first surface 11a. One or more insulating layers may be interposed between the conductive layer 12 and the substrate 11.
[0051] For example, when an insulating resin layer is interposed between the conductive layer 12 and the substrate 11, the insulating resin layer can reduce stress caused by the difference in thermal expansion coefficient between the conductive layer 12 and the substrate 11. As the insulating resin constituting the insulating resin layer, for example, epoxy resin, polyimide, polybenzoxazole, or polyamide can be used.
[0052] An adhesion layer for preventing the conductive layer 12 from peeling off from the substrate 11 may be provided between the conductive layer 12 and the substrate 11. The adhesion layer is, for example, a layer containing zinc oxide (ZnO). The adhesion layer containing zinc oxide can be formed by, for example, a sol-gel method.
[0053] As described above, a part of the conductive layer 12 is the lower electrode of the capacitor 100A. As shown in Fig. 4, the lower electrode has a groove G extending perpendicularly to the thickness direction of the lower electrode on its end surface, surrounding the lower electrode, so as to generate an overhang portion OH between the groove G and the dielectric layer 13. The structures of the conductive layer 12 and the capacitor 100A will be described in detail later.
[0054] A dielectric layer 13 is provided over the bottom electrode, which is part of the conductive layer 12. The dielectric layer 13 can be formed, for example, by chemical vapor deposition (CVD).
[0055] Here, the dielectric layer 13 is a film made of silicon nitride (SiN). The dielectric layer 13 may be a film made of an inorganic material such as silicon oxide (SiO), silicon oxynitride (SiON), tantalum oxide (TaO), aluminum oxide (AlO), aluminum nitride (AlN), or hafnium oxide (HfO), or may be a laminate made of a plurality of inorganic material films.
[0056] The dielectric constant of the dielectric layer 13 is desirably higher than that of an interlayer insulating film 40a surrounding the capacitor 100A, which will be described later. The dielectric constant of the dielectric layer 13 is preferably in the range of 2.0 to 9.0, and more preferably in the range of 3.0 to 8.0.
[0057] The thickness of the dielectric layer 13 is preferably in the range of 50 nm to 1500 nm. Here, as an example, the thickness of the dielectric layer 13 is assumed to be 800 nm.
[0058] The upper electrode 14 is provided on the dielectric layer 13. The upper electrode 14, together with the lower electrode and the dielectric layer 13, constitutes the capacitor 100A shown in FIG.
[0059] 4, the upper electrode 14 includes a seed layer 141 and a main conductor layer 142. The seed layer 141 and the main conductor layer 142 are stacked on the dielectric layer 13 in this order.
[0060] The seed layer 141 is provided on the dielectric layer 13. The seed layer 141 is a part of a power supply layer for forming the main conductor layer 142 by electrolytic plating.
[0061] Here, as an example, the seed layer 141 is a film made of copper (Cu). The seed layer 141 may be a film made of other metals such as chromium (Cr) and titanium (Ti), or may be a laminate made of multiple metal films.
[0062] The thickness of the seed layer 141 is preferably in the range of 20 nm to 400 nm. Here, as an example, the thickness of the seed layer 141 is set to 300 nm.
[0063] The seed layer 141 can be formed by electroless plating, sputtering, etc. The seed layer 141 may be formed by other methods. The seed layer 141 may be omitted.
[0064] The main conductor layer 142 is provided on the seed layer 141. Here, as an example, the main conductor layer 142 is a film made of copper. The main conductor layer 142 may be a film made of another material having electrical conductivity, or may be a laminate made of multiple conductive films.
[0065] The thickness of the main conductor layer 142 is preferably in the range of 0.5 μm to 10 μm. Here, as an example, the thickness of the main conductor layer 142 is assumed to be 5 μm.
[0066] The main conductor layer 142 can be formed by, for example, electrolytic plating. The main conductor layer 142 may be a copper layer formed by sputtering or an electrolytic copper foil that is patterned by etching.
[0067] 2, the conductive layer 22 includes a portion provided on the second surface 11b and a portion covering the side wall of the through hole 11H and an area of the lower surface of the conductive layer 12 adjacent to the space within the through hole 11H. The former includes a land portion and a wiring portion, and the latter includes a via portion.
[0068] Here, the conductive layer 22 is a layer formed integrally with a portion provided on the second surface 11b and a portion covering the side wall of the through hole 11H and a region of the lower surface of the conductive layer 12 adjacent to the space in the through hole 11H. The conductive layer 22 may have a multilayer structure including a layer located in the through hole 11H and a layer covering the second surface 11b. In this case, the portion of the conductive layer 22 located in the through hole 11H may be a part of the conductive layer 12.
[0069] Conductive layer 22 is conformal to second surface 11b, the sidewall of through hole 11H, and a region of the lower surface of conductive layer 12 adjacent to the space within through hole 11H. Conductive layer 22 may completely fill through hole 11H.
[0070] The conductive layer 22 may include a seed layer and a main conductor layer, similar to the conductive layer 12. The seed layer may be omitted. Also, the conductive layer 22 may further include an adhesion layer interposed between the seed layer and the substrate 11, similar to the conductive layer 12. These layers may be formed by the same methods as those described above for the conductive layer 12.
[0071] The interlayer insulating film 40a is provided on the first surface 11a. The conductive layer 12, the dielectric layer 13, and the upper electrode 14 are embedded in the interlayer insulating film 40a. The interlayer insulating film 40a has through holes 40Ha at the position of the upper electrode 14 and at the position of a land portion included in the conductive layer 12. The interlayer insulating film 40a is, for example, a layer containing a resin that is an organic material.
[0072] The conductive layer 24a includes a portion covering the upper surface of the interlayer insulating film 40a, and a portion covering the sidewall of the through hole 40Ha and an area adjacent to the space within the through hole 40Ha of the upper surface of the upper electrode 14 and the conductive layer 12. The former portion includes a pad portion for electrically connecting the electronic component 10 to another component such as an IC chip.
[0073] Conductive layer 24a may include a seed layer and a main conductor layer, similar to conductive layer 12. The seed layer may be omitted. These layers may be formed in a manner similar to that described above for conductive layer 12.
[0074] The interlayer insulating film 40b is provided on the second surface 11b. The conductive layer 22 is embedded in the interlayer insulating film 40b. The interlayer insulating film 40b has through holes 40Hb at the positions of the land portions included in the conductive layer 22. The interlayer insulating film 40b is, for example, a layer containing a resin that is an organic material.
[0075] The conductive layer 24b includes a portion covering the lower surface of the interlayer insulating film 40b, and a portion covering the sidewall of the through hole 40Hb and an area adjacent to the space within the through hole 40Hb of the lower surface of the conductive layer 22. The former portion includes a pad portion for electrically connecting the electronic component 10 to another component such as a printed wiring board.
[0076] Conductive layer 24b may include a seed layer and a main conductor layer, similar to conductive layer 12. The seed layer may be omitted. These layers may be formed in a manner similar to that described above for conductive layer 12.
[0077] The electronic component 10 may further include at least one of a bonding conductor provided on the conductive layer 24a and a bonding conductor provided on the conductive layer 24b. The bonding conductor is, for example, a solder ball.
[0078] The electronic component 10 has, on the first surface 11a, two conductive layers 12 and 24a and one interlayer insulating film 40a interposed therebetween. The electronic component 10 may have, on the first surface 11a, three or more conductive layers and two or more interlayer insulating films interposed therebetween. The electronic component 10 also has, on the second surface 11b, two conductive layers 22 and 24b and one interlayer insulating film 40b interposed therebetween. The electronic component 10 may have, on the second surface 11b, three or more conductive layers and two or more interlayer insulating films interposed therebetween.
[0079] <1.2> Capacitor The capacitor 100A is an MIM capacitor. As described above, a part of the conductive layer 12 is the lower electrode of the capacitor 100A. As shown in Fig. 4, the end face of the lower electrode is provided with a groove G extending perpendicularly to the thickness direction of the lower electrode so as to go around the lower electrode. The groove G generates an overhang portion OH, which is a portion of the lower electrode sandwiched between the groove G and the dielectric layer 13.
[0080] The lower electrode here includes a first conductor portion having a surface facing the dielectric layer 13, and a second conductor portion protruding from the center of the above-mentioned surface of the first conductor portion toward the dielectric layer 13. In Fig. 4, the second conductor portion is a portion of the conductive layer 12 that is a distance t1+t4 or less from the dielectric layer 13. The first conductor portion is a portion of the lower electrode other than the first conductor portion. Here, the groove G is provided on the side surface of the second conductor portion.
[0081] As shown in Fig. 3, a first contour OL1 on the inside of the orthogonal projection of the groove G onto a plane perpendicular to the thickness direction of the substrate 11 is spaced from and surrounded by a second contour OL2 on the orthogonal projection of the dielectric layer 13 onto this plane. The outer contour of the orthogonal projection of the overhang portion OH shown in Fig. 4 onto the above plane almost coincides with the second contour OL2 shown in Fig. 3. That is, the end face of the overhang portion OH and the end face of the dielectric layer 13 are almost flush with each other. The outer contour of the orthogonal projection of the overhang portion OH onto the above plane may be located between the first contour OL1 and the second contour OL2.
[0082] 3, the contour of the upper electrode 14 is a third contour OL3 of an orthogonal projection of the upper electrode 14 onto a plane perpendicular to the thickness direction of the substrate 11. Here, the third contour OL3 is spaced apart from and surrounded by the second contour OL2. Here, the third contour is also spaced apart from and surrounded by the first contour OL1.
[0083] This structure is advantageous in realizing a MIM capacitor with excellent reliability and small capacitance variation, as will be explained below.
[0084] The manufacture of electronic components and products containing electronic components involves a process involving heat treatment. Because the lower electrode and the dielectric layer of a capacitor are made of materials with different linear expansion coefficients, the heat treatment generates stress in the dielectric layer. This stress increases with the thickness of the lower electrode. When the stress generated in the dielectric layer increases, the risk of the dielectric layer peeling off from the lower electrode or cracking increases.
[0085] If the lower electrode is formed so that the central portion of its upper surface protrudes relative to the peripheral portion of the upper surface, it is possible to prevent the stress generated in the dielectric layer from becoming excessively large. However, it is difficult for such a lower electrode to achieve high shape accuracy in the portion adjacent to the dielectric layer. This is for the following reasons.
[0086] The above-mentioned shape of the upper surface of the lower electrode can be formed by covering the upper central portion of the lower electrode having a flat upper surface with an etching mask and receding the upper peripheral portion of the lower electrode by etching. However, in order to obtain a sufficient effect of stress relaxation by the above-mentioned shape of the upper surface of the lower electrode, the difference in height between the upper central portion and the upper peripheral portion must be large. If the difference in height is large, a non-negligible amount of side etching occurs directly under the etching mask. And the side etching does not proceed uniformly all around the etching mask. Therefore, it is difficult to achieve high shape accuracy for the upper peripheral portion of a lower electrode formed so that the upper central portion has a shape protruding from the upper peripheral portion.
[0087] When the lower surface of the upper electrode is larger than the peripheral portion of the upper surface of the lower electrode, if the peripheral portion has a low shape accuracy, the effective area of the capacitor will vary, and therefore the capacitance of the capacitor will vary. On the other hand, when the lower surface of the upper electrode is smaller than the peripheral portion of the upper surface of the lower electrode, if the peripheral portion has a low shape accuracy, the parasitic capacitance of the capacitor will vary, and therefore the capacitance of the capacitor will vary.
[0088] In capacitor 100A included in electronic component 10 described above, a groove G is provided on an end face of the lower electrode, extending perpendicularly to the thickness direction of the lower electrode so as to go around the lower electrode. A first contour OL1 on the inside of an orthogonal projection of groove G onto a plane perpendicular to the thickness direction of substrate 11 is separated from and surrounded by a second contour OL2 of an orthogonal projection of dielectric layer 13 onto this plane. Such groove G has the effect of preventing the stress generated in dielectric layer 13 from becoming excessively large.
[0089] Further, the groove G forms an overhang portion OH, which is a portion of the lower electrode that is sandwiched between the groove G and the dielectric layer 13. The overhang portion OH has the effect of enabling the realization of a lower electrode with excellent shape accuracy of the upper surface.
[0090] Thus, by adopting the above-described structure for capacitor 100A, it is possible to prevent the stress generated in dielectric layer 13 from becoming excessively large, and to realize a lower electrode with excellent shape accuracy of the upper surface. Therefore, when this structure is adopted, cracks or peeling of dielectric layer 13 due to heat are unlikely to occur, and the capacitance of capacitor 100A is also unlikely to vary. Therefore, the above-described structure is advantageous in realizing an MIM capacitor with excellent reliability and small capacitance variation.
[0091] The depth of the groove G, i.e., the distance from the second contour OL2 to the first contour OL1, is preferably in the range of 100 nm to 10 μm, more preferably in the range of 300 nm to 5 μm, and even more preferably in the range of 500 nm to 3 μm. Increasing the depth of the groove G enhances the effect of preventing excessive stress generated in the dielectric layer 13. However, increasing the depth of the groove G reduces the mechanical strength of the overhang portion OH.
[0092] The width of the groove G, which is the sum of the distances t3 and t4 in FIG. 4, is preferably in the range of 100 nm to 1500 nm, more preferably in the range of 200 nm to 1000 nm, and even more preferably in the range of 400 nm to 800 nm. Increasing the width of the groove G enhances the effect of preventing the stress generated in the dielectric layer 13 from becoming excessively large. However, increasing the width of the groove G also increases the depth of the groove G. Therefore, increasing the width of the groove G reduces the mechanical strength of the overhang portion OH.
[0093] The area of the region surrounded by the first contour OL1 is preferably in the range of 90% to 99% of the area of the region of the lower electrode that is in contact with the dielectric layer 13, i.e., the area of the region surrounded by the second contour OL2, more preferably in the range of 94% to 99%, and even more preferably in the range of 95% to 98%.
[0094] The distance from the third contour OL3 to the second contour OL2 is preferably in the range of 1 μm to 30 μm, more preferably in the range of 5 μm to 25 μm, and even more preferably in the range of 10 μm to 20 μm. Increasing this distance reduces the effect of position error of the upper electrode 14 on the capacitance of the capacitor 100A. However, increasing this distance reduces the capacitance of the capacitor 100A.
[0095] The distance t1 from the deepest part of the groove G to the dielectric layer 13 is preferably shorter than the distance t2 from the deepest part to the substrate 11. The ratio t1 / t2 of the distance t1 to the distance t2 is preferably in the range of 1 / 1000 to 1 / 2, more preferably in the range of 1 / 500 to 1 / 10, and even more preferably in the range of 1 / 200 to 1 / 20. From the viewpoint of preventing the stress generated in the dielectric layer 13 from becoming excessively large, it is desirable that the ratio t1 / t2 is small. Also, from the viewpoint of the wiring resistance, it is desirable that the ratio t1 / t2 is small. However, if the ratio t1 / t2 is made small, the overhang portion OH becomes thin, and its mechanical strength decreases.
[0096] The distance t1 from the deepest part of the groove G to the dielectric layer 13 is preferably shorter than the distance t4 from the deepest part to a plane including the edge of the groove G located on the substrate 11 side and parallel to the first surface 11a. The ratio t1 / t4 of the distance t1 to the distance t4 is preferably within a range of 1 / 1000 to 1 / 2, more preferably within a range of 1 / 100 to 1 / 3, and even more preferably within a range of 1 / 30 to 1 / 5. From the viewpoint of preventing the stress generated in the dielectric layer 13 from becoming excessively large, it is desirable that the ratio t1 / t4 is small. However, if the ratio t1 / t4 is made small, the overhang portion OH becomes thin and its mechanical strength decreases.
[0097] The distance t1 is preferably in the range of 5 nm to 2000 nm, more preferably in the range of 10 nm to 1000 nm, and further preferably in the range of 30 nm to 300 nm.
[0098] The distance from the edge of the groove G located on the dielectric layer 13 side to the dielectric layer 13, that is, the difference t1-t3 between the distance t1 from the deepest part of the groove G to the dielectric layer 13 and the distance t3 from the deepest part to a plane including the edge of the groove G located on the dielectric layer 13 side and parallel to the first surface 11a, is preferably within a range of 20 nm to 500 nm, more preferably within a range of 30 nm to 200 nm, and further preferably within a range of 40 nm to 100 nm. The distance from the edge of the groove G located on the dielectric layer 13 side to the dielectric layer 13 corresponds to the thickness at the end of the overhang portion OH. From the viewpoint of preventing the stress generated in the dielectric layer 13 from becoming excessively large, it is desirable that the thickness at the end of the overhang portion OH is small. From the viewpoint of the mechanical strength of the overhang portion OH, it is desirable that the thickness at the end of the overhang portion OH is large.
[0099] <1.3> Modified capacitor Fig. 5 is a cross-sectional view of a capacitor according to a first modified example. Capacitor 100B shown in Fig. 5 is similar to capacitor 100A described with reference to Fig. 4 and the like, except that a distance t3 from the deepest part of groove G, which is the deepest part, to a plane including an edge of groove G located on the dielectric layer 13 side and parallel to first surface 11a is zero. Thus, groove G can have various cross-sectional shapes.
[0100] <1.4> Manufacturing methods for electronic components Figures 6 to 15 are cross-sectional views showing a method for manufacturing the electronic component shown in Figures 1 and 2. The electronic component 10 shown in Figures 1 and 2 can be manufactured, for example, by the following method.
[0101] <1.4.1>First step First, a substrate 11 is prepared as shown in Fig. 6. The substrate 11 has a first surface 11a and a second surface 11b which is the reverse surface of the first surface 11a. Here, the substrate 11 is a glass substrate.
[0102] Next, the support 61 is attached to the second surface 11b via the adhesive layer 62. In order to attach the support 61 to the substrate 11, for example, a laminator, a vacuum pressure press, or a reduced pressure attachment machine can be used.
[0103] The adhesive layer 62 is a layer for temporarily fixing the support 61 to the substrate 11. The adhesive layer 62 is made of a resin or a functional group formed on the support 61. Examples of the resin include a resin that becomes peelable by absorbing light such as ultraviolet light and generating heat, sublimating, or changing in quality, or a resin that becomes peelable by foaming due to heat. According to one example, the adhesive layer 62 is a functional group that modifies the second surface 11b. Examples of the functional group include a hydroxyl group.
[0104] In each drawing, the adhesive layer 62 is illustrated as a layer having a thickness for convenience of explanation. However, when a functional group that modifies the second surface 11b is used as the adhesive layer 62, the thickness of the adhesive layer 62 is negligibly small compared to the substrate 11 and the support 61. For this reason, the adhesive layer 62 can also be expressed as an interface between the substrate 11 and the support 61. In this case, the support 61 can also be expressed as being directly bonded to the substrate 11.
[0105] The support 61 is a first support, and is a thin-plate carrier. From the viewpoint of adhesion, it is desirable that the support 61 is made of the same material as the substrate 11. That is, when the substrate 11 is made of alkali-free glass, the support 61 is also preferably made of alkali-free glass. The thickness of the support 61 may be appropriately set according to the thickness of the substrate 11. In consideration of the transportability of the substrate 11, the thickness of the support 61 is preferably within a range of 300 μm to 1500 μm.
[0106] According to one example, Glass On Glass (GOG) manufactured by Nippon Electric Glass Co., Ltd. is used as a laminate including the substrate 11, the adhesive layer 62, and the support 61. In this case, the substrate 11 and the support 61 are made of glass, and the adhesive layer 62 includes a hydroxyl group and a plurality of functional groups.
[0107] Next, the substrate 11 is irradiated with a laser beam LB to form one or more modified regions 11M on the substrate 11. The direction of irradiation of the laser beam LB may be from the first surface 11a to the second surface 11b, or from the second surface 11b to the first surface 11a. The modified region 11M is, for example, a portion that is heated by the laser beam irradiation and has a difference in crystallinity or the like from a portion not irradiated with the laser beam. The modified region 11M is formed at a position corresponding to a through hole to be formed in the substrate 11. The modified region 11M extends, for example, in a direction intersecting the first surface 11a and the second surface 11b. As shown in FIG. 6, when the laser beam LB is irradiated from the first surface 11a to the second surface 11b, the modified region 11M may be formed so as to reach the adhesive layer 62 and the support 61.
[0108] <1.4.2>Second process 7, an etching stopper film and a seed layer 121 (not shown) are formed on the first surface 11a of the substrate 11 by electroless plating or sputtering. As described above, an adhesion layer may be formed before forming the seed layer 121. In this example, the etching stopper film and the seed layer 121 are formed by depositing Cr and Cu in this order by sputtering.
[0109] <1.4.3>Third step 8, a resist layer 35 having openings at least at the positions of the modified portions 11M is formed on the seed layer 121. Next, a first metal-containing layer 122a to be used as part of the main conductor layer 122 is formed by electrolytic plating on the portions of the seed layer 121 exposed at the positions of the openings of the resist layer 35. Thereafter, as shown in FIG. 9, the resist layer 35 is removed.
[0110] <1.4.4> 4th step Next, the top surface of the first metal-containing layer 122a is partially recessed to generate a first portion and a second portion protruding from the center of the top surface of the first portion in the first metal-containing layer 122a. Next, unnecessary portions of the seed layer 121 are removed to form a second metal-containing layer and a dielectric layer 13, which will be described later. As a result, a structure including the conductive layer 12 and the dielectric layer 13 is obtained, as shown in FIG.
[0111] 11, an upper electrode 14 is formed on the dielectric layer 13. In this way, a capacitor 100A is obtained, which includes a lower electrode that is a part of the conductive layer 12, the dielectric layer 13, and the upper electrode 14. The method for forming capacitor 100A will be described in detail later.
[0112] <1.4.5> 5th step 12, an interlayer insulating film 40a is provided on the surface of the substrate 11 on which the capacitors 100A and the like are formed. When a liquid resin is used, the interlayer insulating film 40a is formed by a spin coating method. When a film-like resin is used, the interlayer insulating film 40a is provided on the substrate 11 by applying heat and pressure under vacuum using a vacuum laminator. According to one example, as the interlayer insulating film 40a, ABF-GXT31 (32.5 μm thick), an insulating resin film manufactured by Ajinomoto Fine-Techno Co., Inc., is laminated on the above surface and pre-cured.
[0113] Next, the composite including the substrate 11 and the interlayer insulating film 40a is supported by the support 70. Here, the composite and the support 70 are bonded together via an adhesive layer 71 so that the interlayer insulating film 40a of the composite faces the support 70.
[0114] The adhesive layer 71 is made of a resin or a functional group that modifies the surface of the support 70. Examples of the resin include a resin that becomes peelable by absorbing light such as ultraviolet light and generating heat, sublimating, or changing in quality, and a resin that becomes peelable by foaming due to heat. The adhesive layer 71 is preferably made of a material different from the adhesive layer 62. According to one example, REVALPHA (registered trademark) manufactured by Nitto Denko Corporation is used as the adhesive layer 71.
[0115] The support 70 is a second support, and is a thin-plate carrier. The support 70 is desirably made of the same material as the substrate 11. That is, when the substrate 11 is made of alkali-free glass, the support 70 is desirably made of alkali-free glass. The thickness of the support 70 may be appropriately set according to the thickness of the substrate 11. In consideration of the transportability of the substrate 11, the thickness of the support 70 is desirably within the range of 300 μm to 1500 μm.
[0116] <1.4.6> 6th step 13, the support 61 and the adhesive layer 62 are separated from the substrate 11. When separating the support 61 and the adhesive layer 62 from the substrate 11, an appropriate peeling method is selected from ultraviolet light irradiation, heat treatment, physical peeling, and the like, depending on the material used for the adhesive layer 62. If a residue of the adhesive layer 62 remains on the substrate 11 after the peeling process of the support 61 and the adhesive layer 62, plasma cleaning, ultrasonic cleaning, water cleaning, solvent cleaning using alcohol, and the like may be performed.
[0117] Next, the second surface 11b of the substrate 11 from which the adhesive layer 62 and the support 61 have been peeled off is etched with an etching solution containing hydrogen fluoride. This causes the second surface 11b to recede and also forms through-holes 11H at the positions of the modified portions 11M. The modified portions 11M of the substrate 11 have a higher etching rate than other portions. Therefore, the etching process can simultaneously thin the substrate 11 and form the through-holes 11H.
[0118] The amount of etching in this etching process is appropriately set depending on the thickness of the substrate 11. For example, when the thickness of the substrate 11 before the etching process is 200 μm, the amount of etching of the substrate 11 is preferably within a range of 50 μm to 175 μm. This allows the thickness of the substrate 11 after the etching process to be within a range of 25 μm to 150 μm.
[0119] The etching solution containing hydrogen fluoride is, for example, an aqueous solution of hydrogen fluoride. The etching solution may further contain one or more inorganic acids selected from the group consisting of nitric acid, hydrochloric acid, and sulfuric acid.
[0120] The hydrogen fluoride concentration of the etching solution is, for example, in the range of 1.0 mass% to 6.0 mass%, preferably in the range of 2.0 mass% to 5.0 mass%. The inorganic acid concentration is, for example, in the range of 1.0 mass% to 20.0 mass%, preferably in the range of 3.0 mass% to 16.0 mass%. It is desirable to carry out the etching process at an etching rate of 1.0 μm / min or less using an etching solution in which the concentration of each component is set within the above range. It is desirable to set the temperature of the etching solution during the etching process to be in the range of 10° C. to 40° C.
[0121] <1.4.7> 7th step Thereafter, the second surface 11b of the substrate 11 and the surface adjacent to the internal space of the through hole 11H are sequentially subjected to the following steps: formation of a seed layer by sputtering or electroless plating, formation of a resist layer by pattern exposure and development using a photoresist, formation of a main conductor layer by electrolytic copper plating, removal of the resist layer, and etching of the seed layer using the main conductor layer as an etching mask. This results in the conductive layer 22 shown in FIG. 14. Thereafter, the interlayer insulating film 40b is provided on the second surface 11b by the same method as described above for the interlayer insulating film 40a.
[0122] <1.4.8> 8th step Next, the support 70 and the adhesive layer 71 are separated from the substrate 11. In this separation, an appropriate peeling method is selected from ultraviolet light irradiation, heat treatment, physical peeling, and the like, depending on the material used for the adhesive layer 71. If a residue of the adhesive layer 71 remains on the substrate 11 after the peeling process of the support 70 and the adhesive layer 71, plasma cleaning, ultrasonic cleaning, water cleaning, solvent cleaning using alcohol, and the like may be performed.
[0123] Next, blind vias are formed in the interlayer insulating films 40a and 40b by laser processing, followed by the following steps in sequence: desmearing, formation of a seed layer by sputtering or electroless plating, formation of a resist layer by pattern exposure and development using a photoresist, formation of a main conductor layer by electrolytic copper plating, removal of the resist layer, and etching of the seed layer using the main conductor layer as an etching mask. As a result, conductive layers 24a and 24b are formed as shown in FIG. 15. In this manner, the electronic component 10 is completed.
[0124] <1.5> Capacitor manufacturing method Figures 16 to 23 are cross-sectional views showing a method for manufacturing the capacitor shown in Figures 3 and 4. In manufacturing the above electronic component 10, capacitor 100A can be manufactured, for example, by the following method.
[0125] First, the structure described with reference to Fig. 9 is prepared. Next, the seed layer 121 is etched using the first metal-containing layer 122a as an etching mask, and the exposed portion of the seed layer 121 is removed as shown in Fig. 16.
[0126] 17, a resist layer 31 is provided on the first surface 11a of the substrate 11. The resist layer 31 covers the first surface 11a of the substrate 11 and has an opening at the position of the first metal-containing layer 122a. The resist layer 31 is formed, for example, by using photolithography. For example, a dry film resist is laminated on the first surface 11a of the substrate 11 and then patterned by using photolithography. In this way, the resist layer 31 is obtained.
[0127] Thereafter, an etching mask 32 is provided on the first metal-containing layer 122a, covering a part of its upper surface. The etching mask 32 is formed at a position where the lower electrode of the capacitor 100A is to be formed, and is smaller than the part of the first metal-containing layer 122a to be used for the lower electrode. The etching mask 32 is obtained, for example, by forming a titanium film by sputtering, forming a resist layer on the titanium film using a dry film resist and photolithography, removing the exposed part of the titanium film by etching, and then removing the resist layer. The etching is, for example, wet etching. For this wet etching, for example, a hydrogen peroxide-based alkaline Ti etching solution is used.
[0128] Next, the first metal-containing layer 122a is etched, whereby, as shown in Fig. 18, a region of the upper surface of the first metal-containing layer 122a that is not covered by the etching mask 32 is recessed, and a first portion and a second portion protruding from the center of the upper surface of the first portion are generated in the first metal-containing layer 122a.
[0129] In addition, this etching may cause side etching of the first metal-containing layer 122a below the peripheral portion of the etching mask 32. The grooves caused by this side etching correspond to the grooves G described with reference to FIG. 4 and the like. The width and the like of the grooves G can be adjusted by, for example, the thickness of the resist layer 31.
[0130] The position in the Z direction of the deepest part of the groove G varies depending on the method and conditions employed in this etching.
[0131] As an example, the sulfuric acid concentration of the sulfuric acid-hydrogen peroxide-based etching solution is preferably in the range of 1% by mass to 10% by mass, more preferably in the range of 3% by mass to 5% by mass. The hydrogen peroxide concentration is preferably in the range of 0.1% by mass to 5% by mass, more preferably in the range of 1% by mass to 3% by mass. Copper sulfate is preferably added as a pentahydrate to a concentration in the range of 10 g / L to 50 g / L, more preferably in the range of 20 g / L to 40 g / L. For the purpose of stable operation, additives may be added to the etching solution as appropriate.
[0132] The spray pressure in the wet etching is preferably within the range of 0.05 MPa to 0.15 MPa. After the spray etching, the immersion etching may be performed for a period of preferably 10 to 300 seconds, more preferably 15 to 60 seconds. Note that the etching solution may remain on the substrate surface between the spray etching and the start of the immersion etching.
[0133] By setting the sulfuric acid concentration relatively low within the above range, for example within the range of 1% by mass to 4% by mass, setting the hydrogen peroxide concentration relatively low within the above range, for example within the range of 0.1% by mass to 2% by mass, setting the spray pressure relatively low within the above range, for example within the range of 0.05 MPa to 0.09 MPa, and setting the immersion time long within the above range, for example 30 seconds or more, as in the structure shown in Figure 5, it is possible to make the height in the Z direction of the deepest part of groove G, which has the greatest depth, approximately equal to the height in the Z direction of the edge of groove G located on the dielectric layer 13 side, i.e., to make the distance t3 described with reference to Figure 4 approximately zero.
[0134] Furthermore, by setting the sulfuric acid concentration relatively high within the above range, for example, in the range of 4% by mass to 10% by mass, setting the hydrogen peroxide concentration relatively low within the above range, for example, in the range of 2% by mass to 5% by mass, setting the spray pressure relatively high within the above range, for example, in the range of 0.09 MPa to 0.15 MPa, and setting the immersion time short within the above range, for example, 30 seconds or less, the distance t3 described with reference to Figure 4 can be made closer to the distance t4.
[0135] 19, the etching mask 32 is removed. The etching for removing the etching mask 32 is, for example, wet etching. For this wet etching, for example, a hydrogen peroxide-based alkaline Ti etching solution is used.
[0136] Next, as shown in FIG. 20, a resist layer 33 is formed. The resist layer 33 fills the first portion of the first metal-containing layer 122a and has a through hole at the position of the second portion protruding from the center of the first portion. The upper surface of the resist layer 33 is higher than the upper surface of the second portion. The through hole of the resist layer 33 is provided such that the upper surface of the second portion is exposed in the through hole and is at least partially spaced from the side wall of the through hole.
[0137] Here, the resist layer 33 is composed of a laminate of a first layer 33a and a second layer 33b. The first layer 33a covers the upper surface of the resist layer 31 and the upper surface of the first portion, and fills a groove provided on the side surface of the second portion. The second layer 33b is provided on the first layer 33a. The shape of the opening provided in the second layer 33b corresponds to the outline shape of the overhang portion OH described with reference to FIG. 4 etc.
[0138] Next, as shown in FIG. 21, a second metal-containing layer 122b is formed on the second portion and the resist layer 33. The second metal-containing layer 122b can be formed by depositing a conductive material using a sputtering method. Here, as an example, Cu is used as the material of the second metal-containing layer 122b. The material of the second metal-containing layer 122b may be other conductive materials such as Ti, MoNb, Cr, Au, and Ag. The thickness of the second metal-containing layer 122b is preferably within the range described above with respect to the thickness at the end of the overhang portion OH.
[0139] Subsequently, a dielectric material layer 13 is formed on the second metal-containing layer 122b. The dielectric material layer 13 can be formed by depositing a dielectric material having a desired dielectric constant by a sputtering method, a chemical vapor deposition (CVD) method, or an atomic layer deposition (ALD) method. The dielectric material layer 13 may be a film made of an inorganic material such as silicon nitride (SiN), silicon oxide (SiO), silicon oxynitride (SiON), tantalum oxide (TaO), aluminum oxide (AlO), aluminum nitride (AlN), and hafnium oxide (HfO), or may be a laminate of a plurality of films each made of an inorganic material.
[0140] 22, the upper electrode 14 is formed on a portion of the dielectric material layer 13 facing the upper surface of the second portion. The upper electrode 14 is formed, for example, by the following method.
[0141] First, a seed layer 141 is formed on the dielectric material layer 13 by sputtering. Next, a resist layer having an opening at the position where the upper electrode 14 is to be formed is provided on the seed layer 141. Next, a main conductor layer 142 covering the seed layer at the opening of the resist layer is formed by electrolytic plating. Thereafter, the resist layer is removed, and the exposed portion of the seed layer 141 is removed by etching using the main conductor layer 142 as an etching mask. In this way, the upper electrode 14 consisting of the seed layer 141 and the main conductor layer 142 is obtained.
[0142] 23, the second metal-containing layer 122b and the portions of the dielectric material layer 13 covering the upper surface of the resist layer 33 are removed together with the resist layer 33. When removing the resist layer 33, the resist layer 31 can also be removed. As a result, a lower electrode including the first metal-containing layer 122a and the portions of the second metal-containing layer 122b that were located in the through holes of the resist layer 33, and a dielectric layer including the portions of the dielectric material layer 13 that were located in the through holes of the resist layer 33 are formed.
[0143] In this manner, capacitor 100 A is completed. As described above, capacitor 100 B can be manufactured in the same manner as capacitor 100 A, except that the etching conditions for first metal-containing layer 122 a are changed.
[0144] In this method, the shape of the opening in the second layer 33b determines the shape of the outline of the overhang portion OH. Therefore, it is possible to form a lower electrode with excellent shape and dimensional accuracy of the upper surface. Therefore, this method makes it possible to manufacture a capacitor with small variation in capacitance.
[0145] The bottom electrode formed by the above method includes a first metal-containing layer 122a and a second metal-containing layer 122b. The first metal-containing layer 122a is made of a first material, and the second metal-containing layer 122b is made of a second material. The first material and the second material may be the same or different.
[0146] When the first and second materials are different, the interface between the first and second metal-containing layers 122a and 122b can be confirmed by observing the cross section of the lower electrode. On the other hand, when the first and second materials are the same, the interface between the first and second metal-containing layers 122a and 122b may or may not be confirmed by observing the cross section of the lower electrode.
[0147] The interface between first metal-containing layer 122a and second metal-containing layer 122b may be located in the deepest part of groove G, or between this deepest part and dielectric layer 13. The former is an example of the structure in FIG. 5, and the latter is an example of the structure in FIG. 4.
[0148] When the first material and the second material are different, it is preferable that the linear expansion coefficient of the second material is larger than that of the material of the dielectric layer 13 and smaller than that of the first material. When this configuration is adopted, the second metal-containing layer 122b can relieve stress generated in the dielectric layer 13 due to the difference in linear expansion coefficient between the first metal-containing layer 122a and the dielectric layer 13. Therefore, the risk of peeling of the dielectric layer 13 from the lower electrode and cracking of the dielectric layer 13 can be reduced.
[0149] When the first material and the second material are different, it is preferable that the elastic modulus of the second material is larger than that of the first material. Even when this configuration is adopted, the second metal-containing layer 122b can relieve stress generated in the dielectric layer 13 due to the difference in the linear expansion coefficient between the first metal-containing layer 122a and the dielectric layer 13.
[0150] <2> Second embodiment <2.1> Electronic components and capacitors The electronic component according to the second embodiment of the present invention is similar to electronic component 10 according to the first embodiment, except that the following configuration is adopted for the capacitor.
[0151] FIG. 24 is a cross-sectional view of a capacitor included in an electronic component according to a second embodiment of the present invention.
[0152] Capacitor 100C shown in Fig. 24 is similar to capacitor 100B described with reference to Fig. 5 etc., except for the following points. That is, in capacitor 100C, main conductor layer 122 includes first metal-containing layer 122A made of a first material and second metal-containing layer 122B made of a second material different from the first material. Second metal-containing layer 122B is interposed between first metal-containing layer 122A and dielectric layer 13. First metal-containing layer 122A and second metal-containing layer 122B are similar to first metal-containing layer 122a and second metal-containing layer 122b described above, respectively, except that they are made of different materials.
[0153] <2.2> Modified capacitor Fig. 25 is a cross-sectional view of a capacitor according to a second modification. Capacitor 100D shown in Fig. 2 is similar to capacitor 100C except that groove G has the structure described above for capacitor 100A. In this manner, groove G can have various cross-sectional shapes.
[0154] <2.3> Manufacturing methods for electronic components and capacitors The electronic component according to the second embodiment can be manufactured by the same method as that described with reference to FIGS. 6 to 15 in the first embodiment, except that the capacitor is manufactured by the method described below.
[0155] Fig. 26 to Fig. 31 are cross-sectional views showing a method for manufacturing the capacitor shown in Fig. 24. In the manufacture of the electronic component in accordance with the second embodiment, the capacitor 100C can be manufactured, for example, by the following method.
[0156] First, the structure described with reference to Fig. 9 is prepared. Here, a first metal-containing layer 122A is formed instead of the first metal-containing layer 122a. The first metal-containing layer 122A is made of the first material described above for the first metal-containing layer 122a. Here, as an example, the first material is copper.
[0157] Next, the seed layer 121 is etched using the first metal-containing layer 122A as an etching mask, and the exposed portion of the seed layer 121 is removed as shown in FIG.
[0158] Next, as shown in FIG. 27, a second metal-containing layer 122B is formed on the first metal-containing layer 122a. The second metal-containing layer 122B is made of a second material different from the first material. The second material can achieve a sufficiently low etching rate in etching the first metal-containing layer 122A compared to the first material. Here, as an example, a titanium layer having a thickness of 50 nm is formed by sputtering as the second metal-containing layer 122B, covering the first metal-containing layer 122a and the first surface 11a of the substrate 11.
[0159] The second metal-containing layer 122B may have a single-layer structure or a multi-layer structure. The second metal-containing layer 122B may be formed by a method other than sputtering, such as a CVD method, a vacuum deposition method, or an electroless plating method. The thickness of the second metal-containing layer 122B is preferably within the range described above with respect to the thickness at the end of the overhang portion OH.
[0160] Prior to the formation of the second metal-containing layer 122B, an additional treatment may be performed to control the adhesion. For example, an ion gun treatment using argon gas may be performed to improve the adhesion, or a treatment using oxygen gas may be performed to reduce the adhesion. Here, as an example, the ion gun treatment using argon gas is performed for 30 to 120 seconds under conditions of 2000 V to 3000 V. If the adhesion to the substrate surface is too strong and it is difficult to obtain the groove G with the desired shape, a treatment using oxygen gas may be further performed for 30 to 60 seconds after the above ion gun treatment.
[0161] Next, as shown in Fig. 28, a dielectric material layer 13 is formed on the second metal-containing layer 122B. Here, as an example, a silicon nitride (SiN) layer is formed as the dielectric material layer 13 by a CVD method.
[0162] The dielectric material layer 13 may be a film having a desired dielectric constant. Examples of the film formation method include sputtering, chemical vapor deposition (CVD), and atomic layer deposition (ALD). The dielectric layer 13 may be a film made of an inorganic material such as silicon nitride (SiN), silicon oxide (SiO), silicon oxynitride (SiON), tantalum oxide (TaO), aluminum oxide (AlO), aluminum nitride (AlN), and hafnium oxide (HfO), or may be a laminate of a plurality of films each made of an inorganic material.
[0163] 29, an upper electrode 14 is formed on the dielectric material layer 13, covering a part of the upper surface of the dielectric material layer 13 at the position of the first metal-containing layer 122A. The upper electrode 14 can be formed, for example, by a method similar to that described with reference to FIG.
[0164] 23, the dielectric material layer 13 is patterned to leave at least a portion sandwiched between the first metal-containing layer 122A and the upper electrode 14 to form a dielectric layer. Subsequently, the second metal-containing layer 122B is patterned to leave a portion sandwiched between the dielectric layer 13 and the first metal-containing layer 122A.
[0165] These patterning processes are carried out, for example, by the following method. First, a pattern of photoresist is exposed and developed in sequence to form a resist layer that covers the upper electrode 14 and the portion of the dielectric material layer 13 near the upper electrode 14 and has openings at other positions. Next, dry etching is carried out to remove unnecessary portions of the dielectric material layer 13 and the second metal-containing layer 122B all at once. The resist layer formed by using photolithography has excellent shape and dimensional accuracy of the pattern. Furthermore, dry etching has excellent linearity. Therefore, according to this method, the second metal-containing layer 122B can be patterned with high shape and dimensional accuracy.
[0166] Then, first metal-containing layer 122A is etched so that the portion of the upper surface of first metal-containing layer 122A that is not covered with patterned second metal-containing layer 122B is recessed and side etching occurs in the portion of the upper surface of first metal-containing layer 122A that is covered with patterned second metal-containing layer 122B, thereby generating a first portion and a second portion protruding from the center of the upper surface of the first portion in first metal-containing layer 122A. This forms a lower electrode including first metal-containing layer 122a provided with the first and second portions and patterned second metal-containing layer 122b.
[0167] According to one example, this etching is performed by spray-type wet etching, and a sulfuric acid-hydrogen peroxide-based etching solution is used as the etching solution. With wet etching, etching proceeds isotropically, so that etching can be performed not only in the depth direction but also in the in-plane direction. In addition, by using a sulfuric acid-hydrogen peroxide-based etching solution that can etch copper as the first material with a high selectivity to titanium as the second material, the first and second parts can be generated in the first metal-containing layer 122A without changing the shape of the patterned second metal-containing layer 122B. In addition, by controlling the adhesion control and the etching process described above, excellent shape accuracy and dimensional accuracy can be achieved for the first and second parts as well.
[0168] In this method, as in the method described in the first embodiment, the position in the Z direction of the deepest part of the groove G changes depending on the method and conditions used for etching the first metal-containing layer 122a.
[0169] As an example, the sulfuric acid concentration of the sulfuric acid-hydrogen peroxide-based etching solution is preferably in the range of 1% by mass to 10% by mass, more preferably in the range of 3% by mass to 5% by mass. The hydrogen peroxide concentration is preferably in the range of 0.1% by mass to 5% by mass, more preferably in the range of 1% by mass to 3% by mass. Copper sulfate is preferably added as a pentahydrate to a concentration in the range of 10 g / L to 50 g / L, more preferably in the range of 20 g / L to 40 g / L. For the purpose of stable operation, additives may be added to the etching solution as appropriate.
[0170] The spray pressure in the wet etching is preferably within the range of 0.05 MPa to 0.15 MPa. After the spray etching, the immersion etching may be performed for a period of preferably 10 to 300 seconds, more preferably 15 to 60 seconds. Note that the etching solution may remain on the substrate surface between the spray etching and the start of the immersion etching.
[0171] By setting the sulfuric acid concentration relatively low within the above range, for example in the range of 1% by mass to 4% by mass, setting the hydrogen peroxide concentration relatively low within the above range, for example in the range of 0.1% by mass to 2% by mass, setting the spray pressure relatively low within the above range, for example in the range of 0.05 MPa to 0.09 MPa, and setting the immersion time long within the above range, for example 30 seconds or more, as in the structure shown in Figure 24, it is possible to make the height in the Z direction of the deepest part of groove G approximately equal to the height in the Z direction of the edge of groove G located on the dielectric layer 13 side, that is, to make the distance t3 shown in Figure 25 approximately zero.
[0172] In addition, by setting the sulfuric acid concentration relatively high within the above range, for example, in the range of 4% by mass to 10% by mass, setting the hydrogen peroxide concentration relatively low within the above range, for example, in the range of 2% by mass to 5% by mass, setting the spray pressure relatively high within the above range, for example, in the range of 0.09 MPa to 0.15 MPa, and setting the immersion time short within the above range, for example, 30 seconds or less, the distance t3 shown in Figure 25 can be made closer to the distance t4. EXAMPLES
[0173] Tests carried out in relation to the present invention are described below.
[0174] (Example 1) The electronic component 10 described with reference to Figures 1 and 2 was manufactured. In this example, instead of the capacitor 100A described with reference to Figures 3 and 4, the capacitor 100B described with reference to Figure 5 was formed. That is, the distance t3 was set to zero. The capacitor 100B and the electronic component 10 were manufactured by the method described in the first embodiment.
[0175] The capacitance of the plurality of capacitors 100B of the electronic component 10 was measured using a network analyzer. Next, a high-temperature load was applied to the electronic component 10 at 125°C for 1000 hours, and then the capacitance of the plurality of capacitors 100B was measured using a network analyzer. Then, the variation in capacitance value at 1 GHz was evaluated for both before and after the application of the high-temperature load.
[0176] (Example 2) The electronic component 10 described with reference to Figures 1 and 2 was manufactured. In this example, the ratio t3 / t4 of the distance t3 to the distance t4 was set to 0.9. The capacitor 100A and the electronic component 10 were manufactured by the method described in the first embodiment. The capacitor 100A of this electronic component 10 was also evaluated for variation in capacitance value at 1 GHz before and after application of a high-temperature load by the same method as in Example 1.
[0177] (Example 3) The electronic component 10 described with reference to Figures 1 and 2 was manufactured. In this example, instead of the capacitor 100A described with reference to Figures 3 and 4, the capacitor 100C described with reference to Figure 24 was formed. That is, the distance t3 was set to zero. The capacitor 100C and the electronic component 10 were manufactured by the method described in the second embodiment and the method described in the first embodiment, respectively. The capacitor 100C of this electronic component 10 was also evaluated for variation in capacitance value at 1 GHz before and after application of a high-temperature load by the same method as in Example 1.
[0178] (Example 4) The electronic component 10 described with reference to Figs. 1 and 2 was manufactured. In this example, instead of the capacitor 100A described with reference to Figs. 3 and 4, the capacitor 100D described with reference to Fig. 25 was formed. In this example, the ratio t3 / t4 of the distance t3 to the distance t4 was set to 0.9. The capacitor 100D and the electronic component 10 were manufactured by the method described in the second embodiment and the method described in the first embodiment, respectively. The capacitance value variation at 1 GHz of the capacitor 100D of this electronic component 10 was also evaluated before and after application of a high-temperature load by the same method as in Example 1.
[0179] Comparative Example 1 Fig. 32 is a cross-sectional view of a capacitor included in an electronic component according to Comparative Example 1. In the capacitor 100X shown in Fig. 32, the upper surface of the lower electrode is flat. Furthermore, in the capacitor 100X, no groove G is provided on the side surface of the lower electrode. Apart from this, the capacitor 100X is similar to the capacitor 100A described with reference to Figs. 3 and 4.
[0180] In this example, an electronic component similar to electronic component 10 described with reference to Figures 1 and 2 was manufactured, except that it included capacitor 100X shown in Figure 32 instead of capacitor 100A described with reference to Figures 3 and 4. Capacitor 100X of this electronic component was also evaluated for variation in capacitance value at 1 GHz before and after application of a high-temperature load in the same manner as in Example 1.
[0181] Comparative Example 2 Fig. 33 is a cross-sectional view of a capacitor included in an electronic component according to Comparative Example 2. Similar to the capacitor 100A described with reference to Figs. 3 and 4, the capacitor 100Y shown in Fig. 33 has a lower electrode that has a first conductor portion having a surface facing the dielectric layer 13 and a second conductor portion protruding from the center of the surface toward the dielectric layer 13. However, in the capacitor 100Y, the groove G is not provided on the side surface of the lower electrode. Apart from this, the capacitor 100Y is similar to the capacitor 100A described with reference to Figs. 3 and 4.
[0182] In this example, an electronic component similar to electronic component 10 described with reference to Figures 1 and 2 was manufactured, except that it included capacitor 100Y shown in Figure 33 instead of capacitor 100A described with reference to Figures 3 and 4. Capacitor 100Y of this electronic component was also evaluated for variation in capacitance value at 1 GHz before and after application of a high-temperature load by the same method as in Example 1.
[0183] Comparative Example 3 FIG. 34 is a cross-sectional view of a capacitor included in an electronic component according to Comparative Example 3. In the capacitor 100Z shown in FIG. 34, the lower electrode includes a first metal-containing layer 122A and a second metal-containing layer 122B, similar to the capacitor 100C described with reference to FIG. 24. However, in the capacitor 100Z, the first metal-containing layer 122A does not have a structure including a first portion and a second portion protruding from the center of the upper surface. In addition, in the capacitor 100Z, the groove G is not provided on the side surface of the lower electrode. Except for these points, the capacitor 100Z is similar to the capacitor 100C described with reference to FIG. 24.
[0184] In this example, an electronic component similar to electronic component 10 described with reference to Figures 1 and 2 was manufactured, except that it included capacitor 100Z shown in Figure 34 instead of capacitor 100A described with reference to Figures 3 and 4. Capacitor 100Z of this electronic component was also evaluated for variation in capacitance value at 1 GHz before and after application of a high-temperature load in the same manner as in Example 1.
[0185] (result) The results of the above evaluations are shown in Table 1.
[0186] [Table 1]
[0187] In Table 1, "A" indicates that the variation in capacitance value was sufficiently small, "C" indicates that the variation in capacitance value was large, and "B" indicates that the variation in capacitance value was intermediate between "A" and "C."
[0188] As shown in Table 1, the capacitance values varied widely either before or after the application of the high-temperature load in Comparative Examples 1 to 3. In contrast, the capacitance values varied sufficiently little either before or after the application of the high-temperature load in Examples 1 to 4. [Explanation of symbols]
[0189] 10...electronic component, 11...substrate, 11a...first surface, 11b...second surface, 11H...through hole, 11M...modified portion, 12...conductive layer, 13...dielectric layer (dielectric material layer), 14...upper electrode, 22...conductive layer, 24a...conductive layer, 24b...conductive layer, 31...resist layer, 32...etching mask, 33...resist layer, 33a...first layer, 33b...second layer, 35...resist layer, 40a...interlayer insulating film, 40b...interlayer insulating film, 40Ha...through hole, 40Hb...through hole, 61...support, 62...adhesive layer, 70...support, 71...adhesive layer, 100A...capacitor , 100B...capacitor, 100C...capacitor, 100D...capacitor, 100X...capacitor, 100Y...capacitor, 100Z...capacitor, 121...seed layer, 122...main conductor layer, 122A...first metal-containing layer, 122a...first metal-containing layer, 122B...second metal-containing layer, 122b...second metal-containing layer, 141...seed layer, 142...main conductor layer, G...groove, LB...laser light, OH...overhang portion, OL1...first contour, OL2...second contour, OL3...third contour, t1...distance, t2...distance, t3...distance, t4...distance.
Claims
1. A substrate having an insulating first surface and a second surface which is an opposite surface of the insulating first surface; a capacitor including a lower electrode provided on the first surface, a dielectric layer provided on the lower electrode, and an upper electrode provided on the dielectric layer; Equipped with the lower electrode has an end surface provided with a groove extending perpendicularly to a thickness direction of the lower electrode, surrounding the lower electrode, so as to generate an overhang portion between the groove and the dielectric layer; An electronic component in which a first contour inside an orthogonal projection of the groove onto a plane perpendicular to the thickness direction is spaced from and surrounded by a second contour of an orthogonal projection of the dielectric layer onto the plane.
2. 2. The electronic component according to claim 1, wherein a distance t1 from a deepest portion of the groove that is the deepest to the dielectric layer is shorter than a distance t2 from the deepest portion to the substrate.
3. 2. The electronic component according to claim 1, wherein an area of the region surrounded by the first contour is within a range of 90% to 99% of an area of the region of the lower electrode that is in contact with the dielectric layer.
4. 2. The electronic component according to claim 1, wherein a distance t1 from a deepest portion of the groove, which is the deepest portion, to the dielectric layer is shorter than a distance t4 from the deepest portion to a plane including an edge of the groove located on the substrate side.
5. 2. The electronic component of claim 1, wherein the lower electrode includes a first metal-containing layer made of a first material and a second metal-containing layer made of a second material different from the first material, the second metal-containing layer is interposed between the first metal-containing layer and the dielectric layer, and the interface between the first metal-containing layer and the second metal-containing layer is located in a deepest portion of the groove that has the greatest depth or is located between the deepest portion and the dielectric layer.
6. The electronic component according to claim 5 , wherein the linear expansion coefficient of the second material is larger than the linear expansion coefficient of the material of the dielectric layer and smaller than the linear expansion coefficient of the first material.
7. The electronic component according to claim 5 , wherein the second material has a greater elastic modulus than the first material.
8. 2. The electronic component of claim 1, wherein a third contour of the orthogonal projection of the upper electrode onto the plane is spaced apart from and surrounded by the second contour.
9. 2. The electronic component of claim 1, wherein a third contour of the orthogonal projection of the upper electrode onto the plane is spaced apart from and surrounded by the first contour.
10. 2. The electronic component described in claim 1, wherein the lower electrode includes a first conductor portion having a surface facing the dielectric layer, and a second conductor portion protruding from the center of the surface of the first conductor portion toward the dielectric layer, and the groove is provided on a side surface of the second conductor portion.
11. The electronic component according to claim 1 , which is a wiring board.
12. 1. A method for manufacturing an electronic component including a capacitor including a lower electrode, an upper electrode, and a dielectric layer interposed therebetween, comprising the steps of: Providing a substrate having an insulating first surface and a second surface that is an opposite surface of the insulating first surface; forming a first metal-containing layer over the first surface; providing an etching mask on the first metal-containing layer, the etching mask covering a portion of an upper surface thereof; thereafter, etching the first metal-containing layer to recess an area of the upper surface not covered by the etching mask to produce in the first metal-containing layer a first portion and a second portion protruding from a center of an upper surface of the first portion; removing the etching mask; and forming a resist layer that embeds the first portion and has a through hole at the position of the second portion, the upper surface of the resist layer being higher than the upper surface of the second portion, the upper surface of the second portion being exposed in the through hole and at least partially spaced from a side wall of the through hole; forming a second metal-containing layer over the second portion and the resist layer; forming a layer of dielectric material over the second metal-containing layer; forming a top electrode on a portion of the dielectric material layer opposite the top surface of the second portion; removing the resist layer together with the second metal-containing layer and portions of the dielectric material layer covering an upper surface of the resist layer to form a lower electrode including the first metal-containing layer and the portions of the second metal-containing layer that were located in the through holes, and a dielectric layer including the portions of the dielectric material layer that were located in the through holes; A method for manufacturing electronic components comprising the steps of:
13. 1. A method for manufacturing an electronic component including a capacitor including a lower electrode, an upper electrode, and a dielectric layer interposed therebetween, comprising the steps of: Providing a substrate having an insulating first surface and a second surface that is an opposite surface of the insulating first surface; forming a first metal-containing layer comprising a first material on the first surface; forming a second metal-containing layer on the first metal-containing layer, the second metal-containing layer being made of a second material different from the first material; forming a layer of dielectric material over the second metal-containing layer; forming an upper electrode on the dielectric material layer, the upper electrode covering a portion of an upper surface of the dielectric material layer at the location of the first metal-containing layer; patterning the dielectric material layer such that at least a portion of the dielectric material layer remains sandwiched between the first metal-containing layer and the top electrode to form a dielectric layer; patterning the second metal-containing layer such that a portion of the second metal-containing layer remains sandwiched between the dielectric layer and the first metal-containing layer; etching the first metal-containing layer such that a portion of the upper surface of the first metal-containing layer not covered with the patterned second metal-containing layer is recessed and side etching occurs in a portion of the upper surface of the first metal-containing layer covered with the patterned second metal-containing layer, thereby generating a first portion and a second portion protruding from a center of an upper surface of the first portion in the first metal-containing layer, thereby forming a lower electrode including the first metal-containing layer provided with the first portion and the second portion and the patterned second metal-containing layer; A method for manufacturing electronic components comprising the steps of:
Citation Information
Patent Citations
Multilayer board and manufacture thereof
JP2000151114A
Wiring substrate and semiconductor device
WO2019244382A1
Cited By
Optical element, optical apparatus, imaging apparatus, and method for manufacturing optical element
JP2026103772A