Laminate type battery

The laminated battery design with a cover member addressing battery expansion-induced wrinkles enhances flexibility and energy density by contacting critical surfaces and maintaining design freedom.

JP2024158033AInactive Publication Date: 2024-11-08TOYOTA JIDOSHA KK
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023072837
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Batteries expand and contract during charging and discharging, leading to wrinkles in the laminate exterior body, which can cause it to break.

Method used

A laminated battery design with a cover member that contacts the sealing surface, wide surface, and corner of the battery cell, featuring an opening with an outer edge inside the electrode coated portion, suppressing wrinkles and allowing expansion without reducing design freedom.

Benefits of technology

The design effectively suppresses wrinkles in the laminate exterior body while maintaining battery flexibility and improving energy density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158033000001_ABST
    Figure 2024158033000001_ABST
Patent Text Reader

Abstract

To provide a laminate type battery in which the occurrence of wrinkles in a laminate outer casing body is suppressed.SOLUTION: A laminate type battery 100 comprises a battery cell 10 and a cover member 20 covering the battery cell 10. The battery cell 10 includes: an electrode lamination body 11 having a plurality of electrodes laminated in a thickness direction; and a laminate outer casing body 12 housing the electrode lamination body 11. The battery cell 10 includes: a sealing surface Ma1; a wide surface Mb1; and a corner part C. The cover member 20 includes an open part 21 that is in contact with the sealing surface Ma1, the wide surface Mb1, and the corner part C, and haing the laminate outer casing body 12 exposed in the wide surface Mb1. In the plan view of the laminate type battery 100 from a thickness direction, the electrode lamination body 11 includes: an electrode coating part 11a in which an electrode layer is formed; and an electrode uncoating part 11b in which the electrode layer is not formed. In the laminate type battery 100, an outer edge of the open part 21 is positioned to an inner side of the outer edge of the electrode coating part 11a.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a laminate-type battery. [Background technology]

[0002] Batteries such as lithium ion secondary batteries usually include an electrode assembly having a positive electrode current collector, a positive electrode active material layer, an electrolyte layer, a negative electrode active material layer, and a negative electrode current collector. The electrode assembly is sealed in an internal space surrounded by, for example, an exterior material.

[0003] For example, Patent Document 1 discloses a flat-plate electrochemical cell that includes an exterior body that contains and hermetically seals electrodes and an electrolyte. Patent Document 2 discloses a secondary battery that includes an electrode unit that includes a positive electrode, a negative electrode, and a separator, and an exterior body that covers the electrode unit. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2005-183556 A [Patent Document 2] JP 2016-134199 A Summary of the Invention [Problem to be solved by the invention]

[0005] Batteries may expand and contract during charging and discharging, and the laminated exterior body may be stretched when the battery expands, which may cause wrinkles. Furthermore, if wrinkles occur, the laminated exterior body may break at the wrinkled parts.

[0006] The present disclosure has been made in consideration of the above-mentioned circumstances, and has as its main object to provide a laminate-type battery in which the occurrence of wrinkles in the laminate exterior body is suppressed. [Means for solving the problem]

[0007] [1] a laminated battery including a battery cell and a cover member covering the battery cell, wherein the battery cell has an electrode laminate having a plurality of electrodes laminated in a thickness direction, and a laminated exterior body that houses the electrode laminate, the battery cell has a sealed surface having a sealing portion where ends of the laminated exterior body are welded to each other, a wide surface located in the thickness direction, and a corner portion connecting the sealed surface and the wide surface, the cover member contacts the sealed surface, the wide surface, and the corner portion, and has an opening at the wide surface through which the laminated exterior body is exposed, when the laminated battery is viewed in a plane from the thickness direction, the electrode laminate has an electrode coated portion on which an electrode layer is formed, and an electrode uncoated portion on which the electrode layer is not formed, and an outer edge of the opening is located inside the outer edge of the electrode coated portion. Effect of the Invention

[0008] The present disclosure has an effect of providing a laminated battery in which the occurrence of wrinkles is suppressed. [Brief description of the drawings]

[0009] [Figure 1] 1A to 1C are a schematic perspective view, a schematic plan view, and a schematic cross-sectional view illustrating a laminate-type battery according to the present disclosure. [Diagram 2] 1A and 1B are a schematic perspective view and a schematic cross-sectional view illustrating a battery cell in the present disclosure. [Diagram 3] 1A and 1B are a schematic cross-sectional view and a schematic plan view illustrating an electrode stack according to the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The laminated battery of the present disclosure will be described in detail below with reference to the drawings. Each of the drawings shown below is a schematic illustration, and the size and shape of each part are appropriately exaggerated to facilitate understanding. In addition, hatching of each part may be omitted as appropriate. A detailed description will be given.

[0011] Fig. 1(a) is a schematic perspective view illustrating a laminated battery in the present disclosure, Fig. 1(b) is a schematic plan view of the laminated battery shown in Fig. 1(a) seen from the thickness direction, and Fig. 1(c) is an AA cross-sectional view of the laminated battery shown in Fig. 1(a). Fig. 2(a) is a schematic perspective view illustrating a battery cell in the present disclosure, and Fig. 2(b) is an AA cross-sectional view of Fig. 2(a). Fig. 3(a) is a schematic cross-sectional view illustrating a battery cell in the present disclosure, and Fig. 3(b) is a schematic plan view of the battery cell shown in Fig. 3(a) seen from the thickness direction.

[0012] As shown in Figs. 1(a) to (c), the laminated battery 100 includes a battery cell 10 and a cover member 20 that covers the battery cell 10. As shown in Figs. 1(c) and 3(a), the battery cell 10 includes an electrode laminate 11 having a plurality of electrodes E laminated in the thickness direction Z, and a laminated exterior body 12 that houses the electrode laminate 11. As shown in Figs. 2(a) and (b), the battery cell 10 includes a sealing surface (Ma1 and Ma2) having a sealing portion S formed by welding the ends of the laminated exterior body 12, wide surfaces (Mb1 and Mb2) located in the thickness direction Z, and a corner portion C that connects the sealing surface and the wide surface. As shown in Figs. 2(a) and (b), the corner portion is a portion that connects the two sealing surfaces (Ma1 and Ma2) to the two wide surfaces (Mb1 and Mb2), respectively.

[0013] As shown in Figs. 1(a) to (c), the cover member 20 contacts the sealing surface (Ma1 and Ma2), the wide surface (Mb1 and Mb2), and the corner C, and has an opening 21 through which the laminated exterior body 12 is exposed at the wide surface (Mb1 and Mb2). When the laminated battery is viewed in plan from the thickness direction, as shown in Figs. 3(a) and 3(b), the electrode laminate 11 has an electrode coated portion 11a where the electrode layers (positive electrode active material layer 2 and negative electrode active material layer 3) are formed, and an electrode uncoated portion 11b where the electrode layers (positive electrode active material layer 2 and negative electrode active material layer 3) are not formed, and as shown in Fig. 1(b), the outer edge E1 of the opening 21 is located inside the outer edge E2 of the electrode coated portion 11a. The outer edge of the electrode coated portion will be described later.

[0014] Stress is likely to concentrate at the corners connecting the sealing surface and the wide surface, and wrinkles are likely to occur due to the expansion and contraction of the battery cell, and the occurrence of wrinkles is also likely to cause the exterior body to break. In contrast, in the laminated battery of the present disclosure, the cover member contacts the sealing surface, wide surface, and corners of the battery cell, and has an opening with a specified outer edge, so that the shape of the laminated exterior body can be well maintained, resulting in a laminated battery in which the occurrence of wrinkles is suppressed.

[0015] Furthermore, in the laminated battery of the present disclosure, wrinkles can be suppressed by adjusting the size of the cover member according to the battery size, so that wrinkles can be suppressed without reducing the freedom of design of the battery.

[0016] 1. Battery cell A battery cell in the present disclosure has an electrode stack and a laminate exterior body that houses the electrode stack.

[0017] (1) Electrode laminate 3A and 3B are a schematic cross-sectional view and a schematic plan view illustrating an electrode laminate 11 according to the present disclosure. As shown in Fig. 3A, the electrode laminate 11 according to the present disclosure has a plurality of electrodes E laminated in the thickness direction Z.

[0018] The electrode laminate 11 shown in FIG. 3(a) has a bipolar electrode BP, a positive electrode end electrode CA, and a negative electrode end electrode AN as electrodes E. The bipolar electrode BP has a current collector 1, a positive electrode active material layer 2 arranged on one surface of the current collector 1, and a negative electrode active material layer 3 arranged on the other surface of the current collector 1. The positive electrode end electrode CA has a current collector 1 and a positive electrode active material layer 2 arranged on one surface of the current collector 1. The negative electrode end electrode AN has a current collector 1 and a negative electrode active material layer 3 arranged on one surface of the current collector 1. Each electrode E is laminated with a separator 4 interposed therebetween.

[0019] Moreover, as shown in FIG. 3(a), the electrode laminate 11 typically has a power generation unit U (U1-U2) having a positive electrode active material layer 1, a separator 4, and a negative electrode active material layer 3 in this order, and the electrode laminate 11 typically has a seal portion 5 on the outer edge of the electrode E (the outer edge of the power generation unit U).

[0020] Each member of the electrode laminate may be a member that is normally used in batteries. An electrolyte solution is normally injected into the electrode laminate.

[0021] As shown in Fig. 3(b), when viewed in plan from the thickness direction Z, the electrode laminate 11 has an electrode-coated portion 11a, which is a region where the electrode layers (positive electrode active material layer 2 and negative electrode active material layer 3) are formed, and an uncoated portion 11b where the electrode layers are not formed. As shown in Fig. 3(b), the electrode-coated portion 11a has an outer edge E2, and the outer side of the outer edge E2 is the electrode-uncoated portion 11b. As shown in Fig. 3(a), the electrode-uncoated portion includes the current collector 1, a part of the separator 4, and a seal portion 5.

[0022] Here, as shown in Fig. 3(a), in a battery cell, the electrode layers (positive electrode active material layer 2 and negative electrode active material layer 3) may have different sizes. In such a case, the outer edge of the electrode layer with the largest size can be regarded as the outer edge of the electrode coated portion. For example, in Fig. 3(a), the negative electrode active material layer 3 is larger in size than the positive electrode active material layer 2, so that the outer edge of the negative electrode active material layer 3 becomes the outer edge E2 of the electrode coated portion 11a.

[0023] (2) Laminate exterior body The laminate exterior body is not particularly limited, and conventionally known materials can be used. For example, the laminate exterior body can be a laminate film having a heat-sealing layer, a metal layer, and a resin layer in this order along the thickness direction. For the heat-sealing layer, the metal layer, and the resin layer, conventionally known materials can be used.

[0024] (3) Battery cell As shown in FIG. 2(a), a battery cell has sealing surfaces (Ma1 and Ma2) and wide surfaces (Mb1 and Mb2), and typically also has side surfaces (Mc1 and Mc2). The wide surfaces are the top and bottom surfaces of the battery in the thickness direction, and can be considered as the main surfaces of the battery cell. The sealing surfaces are connected to the wide surfaces and extend in direction X perpendicular to the thickness direction Z. The side surfaces are connected to the wide surfaces and extend in direction Y perpendicular to direction X.

[0025] 2(a) and 2(b), the corner C of the battery cell extends in the extension direction (X direction) of the sealing surfaces (Ma1 and Ma2) and includes parts of the sealing surfaces and the wide surfaces. Part of the side surfaces is also included in the corner.

[0026] 2.Cover material The cover member is a member that covers the above-mentioned battery cell. The cover member contacts the sealing surface, the wide surface, and the corners of the above-mentioned battery cell.

[0027] The cover member has an opening at the wide surface through which the laminated exterior body is exposed. As shown in FIG. 1(b), the outer edge E1 of the opening 21 is located inside the outer edge E2 of the electrode coated portion. It is preferable to provide the opening so that the center of the electrode coated portion is located inside the opening. Since no restraining pressure is applied to the battery cell at the opening, the opening can be regarded as an unrestrained portion of the laminated battery. As shown in FIG. 1(a), the cover member 30 may have a side opening at one side Mc1 through which the laminated exterior body and a current terminal 30 described later are exposed.

[0028] The material of the cover member is not particularly limited, but examples thereof include resins such as polybutylene terephthalate (PBT), polyphthalamide (PPA), and polyphenylene sulfide (PPS). Cover members using such resins are flexible, so that they can leave room for the battery cell to expand. As a result, the absolute value of the internal pressure can be reduced, the need to enlarge the sealing portion can be reduced, and the energy density of the battery can be improved.

[0029] The cover member may be in direct contact with the laminated exterior body, or may be in contact with the laminated exterior body via an adhesive (adhesive layer). As for the adhesive, any adhesive conventionally known in the field of batteries can be used.

[0030] 3. Laminated battery As shown in FIG. 1(a), a laminated battery 100 may have a current terminal 30 that protrudes from the inside of the laminated exterior body to the outside of the laminated exterior body on a side surface (Mc1) of the battery cell 10.

[0031] The laminated battery in the present disclosure is typically a lithium ion secondary battery. In addition, the laminated battery can be used as a power source for vehicles such as hybrid electric vehicles (HEV), plug-in hybrid electric vehicles (PHEV), electric vehicles (BEV), gasoline automobiles, and diesel automobiles. In particular, it is preferable to use the laminated battery as a driving power source for hybrid electric vehicles (HEV), plug-in hybrid electric vehicles (PHEV), or electric vehicles (BEV). In addition, the all-solid-state battery can be used as a power source for moving objects other than vehicles (for example, railways, ships, and aircraft), and can be used as a power source for electrical products such as information processing devices.

[0032] The present disclosure is not limited to the above-described embodiment. The above-described embodiment is merely an example, and any configuration that is substantially the same as the technical idea described in the claims of the present disclosure and that exhibits similar effects is included in the technical scope of the present disclosure. [Explanation of symbols]

[0033] 10... Battery cell 11 ... Electrode laminate 12 ... Laminate exterior body 20 ... Cover member 100 ... Laminated battery

Claims

[Claim 1] A laminated battery comprising a battery cell and a cover member that covers the battery cell, The battery cell includes an electrode stack having a plurality of electrodes stacked in a thickness direction, and a laminate exterior body that houses the electrode stack, the battery cell has a sealing surface having a sealing portion formed by welding ends of the laminate exterior body, a wide surface located in the thickness direction, and a corner portion connecting the sealing surface and the wide surface, the cover member is in contact with the sealing surface, the wide surface, and the corner portion, and has an opening at the wide surface through which the laminate exterior body is exposed, When the laminated battery is viewed in a plan view from the thickness direction, The electrode laminate has an electrode-coated portion on which an electrode layer is formed and an electrode-uncoated portion on which the electrode layer is not formed, an outer edge of the opening is located inside an outer edge of the electrode coating portion.

Citation Information

Patent Citations

  • JP134199A

  • JP183556A