Lithium secondary battery
The lithium secondary battery design addresses output and productivity issues by using a laminate structure with insulating layers and distinct bonding marks to connect electrodes, improving efficiency and safety.
Patent Information
- Application Number
- JP2024060319
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-04-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing lithium secondary batteries face issues of decreased output characteristics and productivity due to increased resistance and complexity in connecting electrode tabs to current collectors, leading to deteriorated performance and reduced efficiency.
A lithium secondary battery design that includes a first and second laminate with insulating layers between conductive layers, each with electrodes of opposite polarity, connected by a metal sheet with distinct bonding marks to reduce resistance and simplify the connection process, enhancing output characteristics and productivity.
The design improves output characteristics and productivity by reducing resistance at the bonding marks, ensuring stable connections, and maintaining efficient energy transfer, while also enhancing safety through the use of insulating layers to prevent short circuits.
Smart Images

Figure 2024159539000001_ABST
Abstract
Description
[Technical field]
[0001] Exemplary embodiments of the present disclosure relate to lithium secondary batteries. [Background technology]
[0002] Patent Document 1 discloses that the safety of a battery cell is improved by using a current collector in which metal layers are formed on both sides of a resin film. The front and back of the resin film are separated by an insulating resin layer, and electrical conduction is not possible. Therefore, when connecting an electrode tab for drawing wiring to the electrode film, conduction is not possible between the front and back of the electrode, and also between multiple electrodes and the electrode tab. In this regard, Patent Document 2 discloses that the current collector is folded multiple times and laminated on each metal layer in order to connect each metal layer separated by a resin layer to an electrode tab for drawing wiring. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 11-102711 [Patent Document 2] JP 2013-016321 A Summary of the Invention [Problem to be solved by the invention]
[0004] The present disclosure provides a technique for suppressing deterioration in output characteristics and productivity of lithium secondary batteries. [Means for solving the problem]
[0005] In one exemplary embodiment of the present disclosure, there is provided a lithium secondary battery, the battery including: (a) a first laminate including a first current collector having a first insulating layer sandwiched between a pair of first conductive layers, and a first electrode disposed on the first current collector, the first current collector having a first end where the first electrode is not disposed; (b) an intermediate laminate including an electrode having a polarity different from that of the first electrode and a separator; and (c) a second laminate disposed in a stacking direction away from the first laminate via the intermediate laminate, the second current collector having a second insulating layer sandwiched between a pair of second conductive layers, and a first current collector disposed on the second current collector, the first current collector having a first end where the first electrode is not disposed. The present invention provides a lithium secondary battery comprising: (a) a first electrode having the same polarity as the first electrode, and a second electrode having the same polarity as the first electrode, and a second current collector having a second end where the second electrode is not disposed; (d) a metal sheet arranged in parallel with the first end and the second end in the stacking direction, the metal sheet having a first bonding mark due to bonding with either the first end or the second end; and (e) an electrode tab electrically connected to the first stack and the second stack, the electrode tab having a second bonding mark due to bonding with the first end, the metal sheet, and the second end, the second bonding mark being in a position different from the first bonding mark when viewed from the stacking direction. Effect of the Invention
[0006] According to one exemplary embodiment of the present disclosure, a technique for suppressing deterioration in output characteristics and productivity of a lithium secondary battery can be provided. [Brief description of the drawings]
[0007] [Figure 1] FIG. 2 is an exploded perspective view for explaining a configuration example of a secondary battery 1. [Figure 2A] FIG. 2 is a perspective view showing an example of a negative electrode 10. [Figure 2B] FIG. 2 is a perspective view showing another example of the negative electrode 10. [Diagram 3] 2 is a perspective view showing an example of a positive electrode laminate 30 and a metal sheet MS. FIG. [Figure 4A] FIG. 11 is a diagram for explaining an example of a joining mark. [Figure 4B] 13A and 13B are diagrams for explaining other examples of the joining marks. [Figure 4C] 13A and 13B are diagrams for explaining other examples of the joining marks. [Figure 4D] 13A and 13B are diagrams for explaining other examples of the joining marks. [Diagram 5] 13 is a diagram for explaining the bonding state between the positive electrode tab 40, the end P, and the metal sheet MS. FIG. [Figure 6] 13 is a diagram for explaining a second bonding mark WR2. FIG. [Figure 7] 1 is a flowchart showing an example of the present manufacturing method. [Figure 8A] FIG. 8 is a diagram for explaining step ST1 in FIG. 7. [Figure 8B] FIG. 8 is a diagram for explaining step ST1 in FIG. 7. [Figure 9A] 8 is a diagram for explaining step ST2 in FIG. 7. [Figure 9B] 8 is a diagram for explaining step ST2 in FIG. 7. [Figure 9C] 8 is a diagram for explaining step ST2 in FIG. 7. [Figure 9D] FIG. 8 is a diagram for explaining step ST2 in FIG. 7. [Figure 10] 8 is a diagram for explaining step ST3 in FIG. 7. [Figure 11] FIG. 2 is a perspective view showing another example of the negative electrode 10. [Figure 12] FIG. 2 is a perspective view showing another example of the negative electrode 10. [Figure 13] FIG. 4 is a cross-sectional view of a main portion for explaining another example of the configuration of a lithium secondary battery. [Figure 14] FIG. 4 is a cross-sectional view of a main portion for explaining another example of the configuration of a lithium secondary battery. [Figure 15] FIG. 13 is a perspective view illustrating another example of the configuration of the positive electrode laminate. [Figure 16] FIG. 13 is a perspective view illustrating another example of the configuration of the positive electrode laminate. [Figure 17] FIG. 1 is a diagram showing the configurations and results of an example and a comparative example. [Figure 18] FIG. 2 is a diagram showing lamination patterns of metal sheets in examples and comparative examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Each embodiment of the present disclosure will be described below.
[0009] In one exemplary embodiment, a lithium secondary battery includes: (a) a first stack including a first current collector having a first insulating layer sandwiched between a pair of first conductive layers, and a first electrode disposed on the first current collector, the first current collector having a first end where the first electrode is not disposed; (b) an intermediate stack including an electrode having a polarity different from that of the first electrode and a separator; and (c) a second stack disposed in a stacking direction away from the first stack via the intermediate stack, the second current collector having a second insulating layer sandwiched between a pair of second conductive layers, and a first electrode disposed on the second current collector. and a second electrode having the same polarity as the first end and the second end, the second current collector having a second end where the second electrode is not arranged; (d) a metal sheet arranged alongside the first end and the second end in the stacking direction, the metal sheet having a first bonding mark due to bonding to either the first end or the second end; and (e) an electrode tab electrically connected to the first stack and the second stack, the electrode tab having a second bonding mark due to bonding to the first end, the metal sheet, and the second end, the second bonding mark being in a position different from the first bonding mark when viewed from the stacking direction.
[0010] In one exemplary embodiment, the first bond mark is a weld mark.
[0011] In one exemplary embodiment, the first bond mark is in the form of one or more lines.
[0012] In one exemplary embodiment, the first bond mark is in the form of one or more dots.
[0013] In one exemplary embodiment, the second bond mark is a weld mark.
[0014] In one exemplary embodiment, the second bonding mark is in the form of one or more lines.
[0015] In one exemplary embodiment, the second bond mark is in the form of one or more dots.
[0016] In one exemplary embodiment, the second bonding marks include an area where the pair of first conductive layers, the metal sheet, and the pair of second conductive layers are integrated in a cross section in the stacking direction.
[0017] In one exemplary embodiment, the first bonding mark and the second bonding mark do not overlap each other when viewed from the stacking direction.
[0018] In one exemplary embodiment, a plurality of first laminates and second laminates are arranged alternately in the stacking direction with an intermediate laminate sandwiched between them.
[0019] In one exemplary embodiment, the first laminate is formed of a flat sheet, and the second laminate is formed of a flat sheet separate from the first laminate.
[0020] In one exemplary embodiment, the first laminate and the second laminate are constructed from a single folded or rolled sheet.
[0021] In one exemplary embodiment, a total of 10 or more layers of the first laminate and the second laminate are arranged.
[0022] In one exemplary embodiment, the metal sheet is provided on at least one of the plurality of first ends and the plurality of second ends.
[0023] In one exemplary embodiment, the metal sheet is provided on one side of at least one edge.
[0024] In one exemplary embodiment, the metal sheets are provided, one on each side of at least one edge.
[0025] In one exemplary embodiment, the number of metal sheets is less than or equal to three times the total number of first ends and second ends.
[0026] In one exemplary embodiment, the metal sheet is constructed of the same material as the first and second conductive layers.
[0027] In one exemplary embodiment, the first electrode and the second electrode are positive electrodes.
[0028] In one exemplary embodiment, the first electrode and the second electrode are negative electrodes.
[0029] Hereinafter, each embodiment of the present disclosure will be described in detail with reference to the drawings. In each drawing, the same or similar elements are given the same reference numerals, and duplicated explanations will be omitted. Unless otherwise specified, the positional relationship such as up, down, left, right, etc. will be described based on the positional relationship shown in the drawing. The dimensional ratio of the drawings does not indicate the actual ratio, and the actual ratio is not limited to the illustrated ratio.
[0030] As described above, Patent Document 2 proposes folding the current collector multiple times and stacking it on each metal layer in order to connect each metal layer separated by a resin layer to an electrode tab for drawing out wiring. However, this method requires a new device mechanism for stacking the current collector while folding back the end of the current collector for each metal layer. In addition, it is necessary to fold back the end of the current collector while linking with the stacking, which significantly reduces productivity. In addition, in this method, even if the electrode tab can be mechanically joined to the current collector and each metal layer, the resistance of the joint increases and the output characteristics decrease. In a lithium secondary battery 1 (hereinafter also referred to as "secondary battery 1") according to one embodiment, such problems can be solved.
[0031] <Secondary battery configuration example> Fig. 1 is an exploded perspective view for explaining a configuration example of a secondary battery 1. As shown in Fig. 1, the secondary battery 1 includes a negative electrode 10, a separator 20, a first positive electrode laminate 30A, a second positive electrode laminate 30B, a metal sheet MS, a positive electrode tab 40, and a negative electrode tab 42. Each component will be described in detail below.
[0032] (Negative electrode 10) 2A is a perspective view showing an example of a negative electrode 10. In one embodiment, the negative electrode 10 includes a negative electrode current collector 12 and a negative electrode active material 14 disposed on the negative electrode current collector 12.
[0033] 2A, the negative electrode active material 14 is disposed on each of both sides of the negative electrode current collector 12. In one embodiment, the negative electrode active material 14 may be disposed on only one side of the negative electrode current collector 12.
[0034] In one embodiment, the negative electrode current collector 12 is formed from at least one selected from the group consisting of metals that do not react with Cu, Ni, Ti, Fe, and Li, and alloys thereof, and stainless steel.
[0035] The negative electrode active material 14 is a material that causes an electrode reaction, i.e., an oxidation reaction and a reduction reaction, at the negative electrode. The negative electrode active material 14 may be, for example, lithium metal and an alloy containing lithium metal, a carbon-based material, a metal oxide, a metal alloyed with lithium and an alloy containing the metal, etc. The carbon-based material may be, for example, graphene, graphite, hard carbon, carbon nanotubes, etc. The metal oxide may be, for example, a titanium oxide-based compound, a cobalt oxide-based compound, etc. The metal alloyed with lithium may be, for example, silicon, silicon oxide, germanium, tin, lead, aluminum, and gallium, and these may be pre-doped with lithium.
[0036] 2B is a perspective view showing another example of the negative electrode 10. As shown in FIG. 2B, the negative electrode 10 may be configured to include a negative electrode current collector 16 and a negative electrode active material 14 disposed on each of both sides of the negative electrode current collector 16. The material of the negative electrode active material 14 may be the same as that described in FIG. 2A. The negative electrode current collector 16 may be configured to include a negative electrode insulating layer 160 and a pair of negative electrode conductive layers 162 disposed so as to sandwich the negative electrode insulating layer 160 therebetween.
[0037] In one embodiment, the negative electrode insulating layer 160 may be made of a sheet-like (film-like) or fibrous resin. The negative electrode conductive layer 162 is made of at least one selected from the group consisting of metals that do not react with Cu, Ni, Ti, Fe, and Li, alloys thereof, and stainless steel. In one example, the negative electrode conductive layer 162 is made of Cu. By including the negative electrode insulating layer 160, the negative electrode current collector 16 can be made lighter than when the negative electrode current collector 16 is made of only a conductive layer while ensuring a necessary thickness (rigidity) for the negative electrode current collector 16.
[0038] As shown in FIGS. 2A and 2B, the negative electrode current collector (12, 16) has a negative electrode end Q. In one embodiment, the negative electrode end Q is configured as a part of the negative electrode current collector and extends outward (in the x direction) from the side surface of the negative electrode current collector. The negative electrode active material 14 is not formed on the negative electrode end Q. A bonding mark WL2 with the negative electrode tab 42 is formed on the negative electrode end Q.
[0039] (Negative electrode tab 42) 1, the negative electrode tabs 42 are arranged to be aligned in the stacking direction (z direction) with respect to each negative electrode end Q. In one embodiment, the negative electrode tabs 42 may be arranged above or below each negative electrode end Q. In one embodiment, the negative electrode tabs 42 may be arranged between a certain negative electrode end Q and an adjacent negative electrode end Q.
[0040] The negative electrode tab 42 is joined to each negative electrode end Q. The negative electrode end 42 is electrically connected to each negative electrode 10 via each negative electrode end Q. A joining mark WL2 is formed on the negative electrode tab 42 by joining with each negative electrode end Q. The joining mark WL2 may be one or more points (spots), or may be a continuous line or surface. In one embodiment, the negative electrode tab 42 and each negative electrode end Q may be joined by welding. In this case, the joining mark WL2 is a welding mark. The welding may be, for example, ultrasonic welding, laser welding, resistance welding, or spot welding.
[0041] (Separator 20) The separator 20 is disposed on the negative electrode 10. In the example shown in FIG. 1, the separator 20 is disposed on both sides of the negative electrode 10. The separator 20 physically and / or electrically isolates the negative electrode 10 from the positive electrode laminate 30 and ensures ion conductivity of lithium ions. In one embodiment, the separator 20 may be at least one selected from the group consisting of an insulating porous member, a polymer electrolyte, a gel electrolyte, and an inorganic solid electrolyte. The separator 20 may be one type of member used alone or two or more types of members used in combination.
[0042] When the separator 20 includes an insulating porous member, the pores of the porous member are filled with a substance having ion conductivity (such as an electrolytic solution, a polymer electrolyte, and / or a gel electrolyte). This allows the separator 20 to exhibit ion conductivity. The material constituting the insulating porous member is not particularly limited, and examples thereof include insulating polymer materials, specifically, polyethylene (PE) and polypropylene (PP). That is, the separator 20 may be a porous polyethylene (PE) film, a porous polypropylene (PP) film, or a laminated structure thereof.
[0043] In one embodiment, the separator 20 may be coated on one or both sides with a separator coating layer. This may improve the cycle characteristics of the secondary battery 1. In one embodiment, the separator coating layer may be a continuous film with a uniform thickness over 50% or more of the surface area of the separator 20. In one embodiment, the separator coating layer may include a binder such as polyvinylidene fluoride (PVDF), a mixture of styrene butadiene rubber and carboxymethyl cellulose (SBR-CMC), and polyacrylic acid (PAA). In one embodiment, the separator coating layer may be formed by adding inorganic particles such as silica, alumina, titania, zirconia, or magnesium hydroxide to the binder.
[0044] In one embodiment, the thickness of the separator 20 (including the coating layer if the separator 20 includes the coating layer) may be 3.0 μm or more and 40 μm or less. This can reduce the volume occupied by the separator 20 while isolating the negative electrode 10 and the positive electrode laminate 30. In one embodiment, the thickness of the separator 20 may be 5.0 μm or more, 7.0 μm or more, or 10 μm or more. In one embodiment, the thickness of the separator 20 may be 30 μm or less, 20 μm or less, or 10 μm or less.
[0045] (Intermediate laminate LM) As shown in FIG. 1, in one embodiment, the negative electrode 10 and the separator 20 constitute an intermediate laminate LM. The intermediate laminate LM may have a structure in which the separator 20, the negative electrode 10, and the separator 20 are laminated in this order in the stacking direction (z direction). The secondary battery 1 includes a plurality of intermediate laminates LM. In one embodiment, the plurality of intermediate laminates LM may each be configured as a single flat sheet as shown in FIG. 1. In one embodiment, the plurality of intermediate laminates LM may be configured as a single sheet (an example of this embodiment will be described later with reference to FIG. 13 and FIG. 14).
[0046] (Positive electrode laminate 30 and metal sheet MS) As shown in FIG. 1, the first positive electrode laminate 30A includes a current collector 32A and a positive electrode 34A. The first positive electrode laminate 30A is an example of a first laminate. In one embodiment, the first positive electrode laminate may have a structure in which a positive electrode 34A, a current collector 32A, and a positive electrode 34A are laminated in this order in the lamination direction. The current collector 32A has a first end P1 exposed from the positive electrode 34A. In other words, the positive electrode 34A is not formed on the first end P1. The first end P1 extends outward (in the x direction) from a side surface of the current collector 32A as a part of the current collector 32A.
[0047] The second positive electrode laminate 30B includes a current collector 32B and a positive electrode 34B. The second positive electrode laminate 30B is an example of a second laminate. In one embodiment, the second positive electrode laminate 30B may have a structure in which a positive electrode 34B, a current collector 32B, and a positive electrode 34B are laminated in this order in the lamination direction. The current collector 32B has a second end P2 exposed from the positive electrode 34B. In other words, the positive electrode 34B is not formed on the second end P2. The second end P2 extends outward (in the x direction) from the side surface of the current collector 32B as a part of the current collector 32B.
[0048] The first positive electrode laminate 30A and the second positive electrode laminate 30B are alternately laminated in the stacking direction via intermediate laminates LM (hereinafter, when there is no need to distinguish between the first positive electrode laminate 30A and the second positive electrode laminate 30B, they are collectively referred to as the "positive electrode laminate 30"). In one embodiment, the multiple positive electrode laminates 30 may each be configured as a single flat sheet as shown in FIG. 1. In one embodiment, the multiple positive electrode laminates 30 may be configured as a single sheet (an example of this embodiment will be described later with reference to FIG. 15 and FIG. 16).
[0049] In one embodiment, the total number of positive electrode laminates 30 included in the secondary battery 1 may be 5 or more, 10 or more, or 20 or more. In one embodiment, the total number of positive electrode laminates 30 included in the secondary battery 1 may be 50 or less, 40 or less, or 30 or less. In one embodiment, the energy density of the secondary battery 1 may be 300 Wh / kg or more. In one embodiment, the rated capacity of the secondary battery 1 may be 1.5 Ah or more, or may be 5 Ah or more.
[0050] As shown in FIG. 1, the metal sheet MS is placed on a first end P1 and a second end P2 (hereinafter, when there is no need to distinguish between the two, they will be collectively referred to as "ends P"). In one embodiment, the metal sheet MS may be placed on all of the ends P. In one embodiment, the metal sheet MS may be placed on some of the ends P, and no metal sheet MS may be placed on the remaining ends P. For example, the metal sheet MS may be placed every several ends P.
[0051] In one embodiment, the number and thickness of metal sheets arranged on an end P may be set based on the position of the end P in the stacking direction. For example, two or more metal sheets MS may be arranged on the end P in the center of the stacking direction of the secondary battery 1, and one metal sheet MS may be arranged on each of the end Ps at the top and bottom in the stacking direction. Also, for example, the thickness of the metal sheet MS arranged on the end P in the center of the stacking direction of the secondary battery 1 may be made larger than the thickness of the metal sheet arranged on each of the end Ps at the top and bottom in the stacking direction. This can suppress variation in resistance between the end Ps in the center.
[0052] In one embodiment, the number of metal sheets MS may be three times or less than the total number of end parts P. In one embodiment, the number of metal sheets MS may be the same as the total number of end parts P, or may be less than the total number of end parts P, for example, half or less of the total number of end parts P.
[0053] 3 is a perspective view showing an example of a positive electrode laminate 30 and a metal sheet MS. In one embodiment, the positive electrode laminate 30 may have a current collector 32 and positive electrodes 34 disposed on both sides of the current collector 32. The current collector 32 has an insulating layer 320 and conductive layers 322 formed so as to sandwich the insulating layer 320.
[0054] The insulating layer 320 of the current collector 32 may be made of, for example, a sheet-like (film-like) or fibrous resin. The resin may be, for example, at least one of polyolefin resins such as polyethylene terephthalate (PET), polyethylene, and polypropylene, and thermoplastic resins such as polystyrene, polyvinyl chloride, and polyamide. The insulating layer 320 may be made by laminating at least one or more of the resins. In one embodiment, the insulating layer 320 is formed from a material having a melting point of 150° C. or more and 300° C. or less. In one embodiment, the thickness of the insulating layer 320 may be 3 μm or more and 10 μm or less, or 4 μm or more and 8 μm or less.
[0055] The insulating layer 320 can function to melt when abnormal heat is generated due to overcharge or high temperature, to damage the positive electrode laminate 30, and to cut off the short-circuit current inside the battery. This can suppress a sudden increase in temperature inside the secondary battery 1 and suppress the battery from catching fire. In other words, the insulating layer 320 can contribute to improving the safety of the secondary battery 1.
[0056] The conductive layers 322 of the current collector 32 are formed on both sides of the insulating layer 320 so as to sandwich the insulating layer 320. The conductive layers 322 are in physical and / or electrical contact with the positive electrode 34 and function to give and receive electrons to and from the positive electrode 34. The conductive layers 322 are made of a conductor that does not react with lithium ions in a battery. In one embodiment, the conductive layers 322 are made of at least one material selected from the group consisting of aluminum, titanium, stainless steel, nickel, and alloys thereof. In one example, the conductive layers 322 are aluminum or an aluminum alloy. In one embodiment, the conductive layers 322 are formed by vapor deposition, sputtering, electrolytic plating, or lamination of the above-mentioned material on the surfaces of both sides of the insulating layer 320. In one embodiment, the thickness of each of the conductive layers 322 may be 0.5 μm to 5 μm, 0.7 μm to 3 μm, or 0.8 μm to 2.0 μm.
[0057] The positive electrodes 34 are formed on both sides of the current collector 32. A known material may be appropriately selected as the positive electrode 34 depending on the application. The thickness of the positive electrode 34 may be appropriately adjusted depending on the desired capacity and rate characteristics of the battery. In one embodiment, the thickness of each positive electrode 34 is, for example, 20 μm or more and 150 μm or less.
[0058] In one embodiment, the positive electrode 34 has a positive electrode active material. The positive electrode active material is a material for holding a carrier metal in the positive electrode 34, and may also be referred to as a host material for the carrier metal. The positive electrode active material may be a material for holding lithium ions in the positive electrode 34, in which case lithium ions are loaded into and deloaded from the positive electrode active material by charging and discharging the battery. This may improve the stability and output voltage of the battery.
[0059] In one embodiment, the positive electrode active material is a metal oxide or a metal phosphate. The metal oxide may be, for example, a cobalt oxide-based compound, a manganese oxide-based compound, or a nickel oxide-based compound. The metal phosphate may be, for example, an iron phosphate-based compound, or a cobalt phosphate-based compound. In one embodiment, the positive electrode active material is LiCoO2, LiNi x Co y Mn z O(x+y+z=1), LiNi x Co y Al z O(x+y+z=1), LiNi x Mn y The positive electrode active material may be at least one selected from the group consisting of O(x+y=1), LiNiO2, LiMn2O4, LiFePO4, LiCoPO4, LiFeOF, LiNiOF, and LiTiS2. The positive electrode active material may be used alone or in combination of two or more. In one embodiment, the content of the positive electrode active material in the positive electrode 34 may be 50 mass% or more and 100 mass% or less with respect to the entire positive electrode 34.
[0060] In one embodiment, positive electrode 34 may include one or more components other than the positive electrode active material.
[0061] In one embodiment, the positive electrode 34 may include a sacrificial positive electrode material, which is a lithium-containing compound that undergoes an oxidation reaction and does not substantially undergo a reduction reaction in the charge / discharge potential range of the positive electrode active material.
[0062] In one embodiment, the positive electrode 34 may include a gel electrolyte. The gel electrolyte may improve adhesion between the positive electrode 34 and the current collector 32. In one example, the gel electrolyte includes a polymer, an organic solvent, and a lithium salt. The polymer in the gel electrolyte may be, for example, a copolymer of polyethylene and / or polyethylene oxide, polyvinylidene fluoride, and a copolymer of polyvinylidene fluoride and hexafluoropropylene, etc.
[0063] In one embodiment, the positive electrode 34 may include a conductive additive and / or a binder. In one example, the conductive additive is carbon black, single-walled carbon nanotubes (SWCNT), multi-walled carbon nanotubes (MWCNT), carbon nanofibers (CF), or the like. In one example, the binder is polyvinylidene fluoride, polytetrafluoroethylene, styrene butadiene rubber, acrylic resin, polyimide resin, or the like. In one embodiment, the content of the conductive additive is 0.5% by mass to 30% by mass or less with respect to the entire positive electrode 34. In one embodiment, the content of the binder may be 0.5% by mass to 30% by mass or less with respect to the entire positive electrode 34.
[0064] In one embodiment, the positive electrode 34 may include a polymer electrolyte. In one example, the polymer electrolyte is a solid polymer electrolyte that mainly includes a polymer and an electrolyte, and a semi-solid polymer electrolyte that mainly includes a polymer, an electrolyte, and a plasticizer. In one embodiment, the total content of the polymer electrolyte may be 0.5% by mass to 30% by mass or less with respect to the entire positive electrode 34.
[0065] 3, the metal sheet MS may be joined to one surface of the end P of the current collector 32 (one surface of the pair of conductive layers 322). In one embodiment, the metal sheet MS may be joined to the other surface of the end P of the current collector 32 (the other surface of the pair of conductive layers 322). In one embodiment, one or more metal sheets MS may be provided at the end P. For example, one metal sheet MS may be joined to each of the one surface and the other surface of the end P of the current collector 32.
[0066] As shown in FIG. 3, a first bonding mark WR1 is formed between the metal sheet MS and the end P by bonding the metal sheet MS and the end P. In one embodiment, the first bonding mark WR1 may be a bonding mark by welding, i.e., a welding mark. The welding may be, for example, ultrasonic welding, laser welding, resistance welding, or spot welding. In one example, the welding is ultrasonic welding. In one embodiment, the metal sheet MS and the conductive layer 322 of the end P may be integrated by being partially or entirely fused by heat or the like at the first bonding mark WR1. In addition, a second bonding mark WR2 is also formed on the metal sheet MS and the end P. The details will be described later, but the second bonding mark WR2 is a bonding mark between the end P and the metal sheet MS and the positive electrode tab 40.
[0067] In one embodiment, as shown in FIG. 3, the metal sheet MS may be configured to cover only a part of the end P of the current collector 32, not the whole. For example, the metal sheet MS may be disposed at a position spaced a predetermined distance from the positive electrode 34. In this case, an insulating layer may be provided in the area on the conductive layer 322 of the end P where the metal sheet MS is not disposed. In this case, when the separator 20 is damaged, etc., the negative electrode 10 is prevented from shorting with the positive electrode 34 through the conductive layer 322 of the end P and / or the metal sheet MS, and the safety of the secondary battery 1 may be improved. The insulating layer may be, for example, a sheet-shaped (film-shaped) or fibrous resin. The resin may be, for example, at least one of polyolefin resins such as polyethylene terephthalate (PET), polyethylene, and polypropylene, and thermoplastic resins such as polystyrene, polyvinyl chloride, and polyamide. In one embodiment, the metal sheet MS may be configured to cover the entire surface of the end P of the current collector.
[0068] In one embodiment, the metal sheet MS is composed of at least one material selected from the group consisting of aluminum, titanium, stainless steel, nickel, and alloys thereof. The metal sheet MS is, for example, a hard aluminum foil. The metal sheet MS is, for example, a soft aluminum foil. The soft aluminum foil may be formed by subjecting the hard aluminum foil to a heat treatment at a high temperature (around 400°C). In one embodiment, the metal sheet MS may be composed of the same material as the conductive layer 322.
[0069] In one embodiment, the thickness of the metal sheet MS may be set based on the thickness of the insulating layer 320 and the thickness of the conductive layer 322. For example, when the sum of the total thickness (A) of each metal sheet MS and the total thickness (B) of each conductive layer 322 is X (=A + B), and the total thickness of each insulating layer 320 is Y, the thickness of the metal sheet MS may be set so that the relationship 0.85 < X / Y < 2.3 holds. In one embodiment, 1.0 < X / Y < 2.0 may also be satisfied. In one embodiment, the thickness of the metal sheet MS may be greater than the thickness of the insulating layer 320. In one embodiment, all of the metal sheets MS may have the same thickness, or some of them may have different thicknesses. In one embodiment, the thickness of the metal sheet MS may be 3 μm or more, 5 μm or more, or 7 μm or more. In one embodiment, the thickness of the metal sheet MS may be 15 μm or less, 12 μm or less, or 10 μm or less.
[0070] FIG. 4A is a diagram for explaining an example of a joining mark. FIG. 4A is a plan view of the vicinity of the end portion P of the positive electrode laminate 30 shown in FIG. 3. As shown in FIG. 3, the first joining mark WR1 may be formed in a plurality of rows (for example, two rows) in a line along the width direction (y direction) of the end portion P. As shown in FIG. 4A, the first joining mark WR1 is formed at a position different from that of the second joining mark WR2 when viewed from the lamination direction. That is, the first joining mark WR1 and the second joining mark WR2 do not overlap in plan view.
[0071] 4B to 4D are diagrams for explaining other examples of bonding marks. In one embodiment, the first bonding marks WR1 may be formed in a line shape along the width direction (y direction) of the end P as shown in FIG. 4B. In one embodiment, the first bonding marks WR1 may be formed in a line shape along the width direction (y direction) of the end P as shown in FIG. 4C and FIG. 4D, and may be formed in a line (FIG. 4C) or multiple lines (FIG. 4C) along the width direction (y direction) of the end P. In any of FIG. 4B to FIG. 4D, the first bonding marks WR1 and the second bonding marks WR2 are disposed at different positions when viewed from the stacking direction. That is, in any of FIG. 4B to FIG. 4D, the first bonding marks WR1 and the second bonding marks WR2 do not overlap in a plan view.
[0072] (Positive electrode tab 40) 1, the positive electrode tab 40 is arranged to be aligned with each end P (P1, P2) of the current collector 32 (32A, 32B) and each metal sheet MS in the stacking direction (z direction). In one embodiment, the positive electrode tab 40 may be arranged above or below the end P of each current collector 32 and each metal sheet MS. In one embodiment, the positive electrode tab 40 may be arranged between an end P and an end P adjacent thereto.
[0073] The positive electrode tab 40 is made of a conductive material. The positive electrode tab 40 may be made of, for example, aluminum or an aluminum alloy. In one example, the positive electrode tab 40 may be made of hard aluminum. In one embodiment, the thickness of the positive electrode tab 40 may be 0.05 mm or more and 1 mm or less, or 0.1 mm or more and 0.5 mm or less.
[0074] The positive electrode tab 40 is joined to each end P of each current collector 32 and each metal sheet MS. As a result, the positive electrode tab 40 is electrically connected to each positive electrode 34 via each end P. A second joining mark WR2 is formed on the positive electrode tab 40 by joining with each end P. The second joining mark WR2 may be one or a plurality of points (spots) in a plan view, or may be a continuous line or surface.
[0075] In one embodiment, the positive electrode tab 40 and each end P and each metal sheet MS may be joined by welding. The welding may be, for example, ultrasonic welding, laser welding, resistance welding, or spot welding. In one example, the welding is ultrasonic welding.
[0076] Fig. 5 is a diagram for explaining the bonding state of the positive electrode tab 40, the end P, and the metal sheet MS. Fig. 5 shows a schematic cross section of the end P, taken along the xz plane, at a location including the first bonding mark WR1 and the second bonding mark WR2.
[0077] As shown in Fig. 5, the first bonding mark WR1 and the second bonding mark WR2 are provided at different positions from each other when viewed from the stacking direction. The first bonding mark WR1 is formed for each end P. In other words, one first bonding mark WR1 is not formed across multiple ends P. In contrast, the second bonding mark WR2 is formed over the positive electrode tab 40, each end P, and each metal sheet MS. In other words, the second bonding mark WR2 is formed continuously in the stacking direction from the positive electrode tab 40 to the end P of the lowest layer.
[0078] Fig. 6 is a diagram for explaining the second bonding mark WR2. Fig. 6 shows a schematic cross section (AA cross section in Fig. 5) of the second bonding mark WR2 cut along the zy plane. As shown in Fig. 6, the cross section of the second bonding mark WR2 includes a first region R1 and a second region R2. In one embodiment, the cross section of the second bonding mark WR2 may have a recess recessed on one side in the stacking direction.
[0079] In the first region R1, the conductive layer 322 and the metal sheet MS are laminated integrally and joined to the positive electrode tab 40. Here, being laminated integrally includes a state in which the conductive layers 322 and the metal sheet MS are partially or entirely fused together by heat or the like (a state in which the layers cannot be distinguished).
[0080] In one embodiment, the first region R1 may be substantially free of the insulating layer 320 along the stacking direction. The first region R1 provides a physical path for electrical connection between the electrode tab 40 and each of the conductive layers 322 and the metal sheet MS.
[0081] In one embodiment, the first region R1 may be configured between two second regions R2. In one embodiment, the maximum thickness of the first region R1 may be less than or equal to half the maximum thickness of the second region R2.
[0082] In the second region R2, a pair of conductive layers 322 and the metal sheet MS sandwiching the insulating layer 320 are laminated. That is, the second region R2 is a region that includes the insulating layer 320 along the lamination direction.
[0083] In one embodiment, the second joining mark WR2 may be formed by welding. In this case, the second joining mark WR2 is a welding mark. During welding, the positive electrode tab 40, the end P, and the metal sheet MS may be pressed along the stacking direction. As a result, the insulating layer 320 is softened at the welded portion and pushed outward in the width direction (left and right direction in FIG. 6) from the welded portion. Also, at the welded portion, each conductive layer 322 and the metal sheet MS are thermally melted and integrated. As a result, the first region R1 and the second region R2 can be formed.
[0084] As described above, the insulating layer 320 can suppress a rapid temperature rise inside the secondary battery 1 when abnormal heat generation occurs due to overcharge or high temperature, and can suppress the battery from catching fire. In a collector having an insulating layer sandwiched between conductive layers, as the number of collectors increases or the thickness of the insulating layer increases, it becomes difficult to ensure stable bonding quality (variation control) between the end of the collector and the electrode tab and between each layer. For example, if a strong force is applied to weld the electrode tab to all the ends, the conductive layer at the end may be damaged or broken if the conductive layer is thin. On the other hand, if the electrode tab is welded to the electrode tab with a force that does not damage the conductive layer, the bonding may be insufficient and the resistance between the end of the collector and the electrode tab may increase.
[0085] In this regard, in the secondary battery 1 according to one embodiment, a metal sheet MS is disposed between at least one end P. The metal sheet MS functions as an additional conductive layer of the conductive layer 322 in the second bonding trace WR2, and increases the ratio of the conductive layer to the insulating layer 320. Therefore, an increase in resistance in the second bonding trace WR2 can be suppressed. This can improve the output characteristics of the secondary battery 1. The metal sheet MS can also function as a protective layer for the conductive layer 322 of the end P when the positive electrode tab 40 and the end P are bonded to each other. This can suppress damage and breakage of the conductive layer 322 even if the positive electrode tab 40 and each end P are bonded by pressing them with a strong force when the total number (number of layers) of the positive electrode laminate 30 of the secondary battery 1 is large. This can improve the production yield of the secondary battery 1. In one embodiment, the resistance of the second bonding trace WR2 may be 5.0 mΩ or less, 3.0 mΩ or less, 1.0 mΩ or less, or 0.5 mΩ or less.
[0086] (electrolyte) In one embodiment, the secondary battery 1 may contain an electrolytic solution. The electrolytic solution is a liquid containing a solvent and an electrolyte, and has ion conductivity. The electrolytic solution may be referred to as a liquid electrolyte, and acts as a conductive path for lithium ions. Therefore, when the secondary battery 1 contains an electrolytic solution, the internal resistance is reduced, and the energy density, capacity, and cycle characteristics can be improved.
[0087] The electrolytic solution may be, for example, a solution filled in the case (pouch) of the secondary battery 1. Also, for example, the electrolytic solution may be impregnated into the separator 20, or may be held by a polymer to form a polymer electrolyte or a gel electrolyte.
[0088] The electrolyte contained in the electrolytic solution may be, for example, a lithium salt. The lithium salt may be, for example, one or a combination of two or more selected from the group consisting of LiI, LiCl, LiBr, LiF, LiBF4, LiPF6, LiAsF6, LiSO3CF3, LiN(SO2F)2, LiN(SO2CF3)2, LiN(SO2CF3CF3)2, LiB(O2C2H4)2, LiB(C2O4)2, LiB(O2C2H4)F2, LiB(OCOCF3)4, LiNO3, and Li2SO4.
[0089] As the solvent contained in the electrolytic solution, for example, a non-aqueous solvent having fluorine atoms (hereinafter referred to as a "fluorinated solvent") and a non-aqueous solvent not having fluorine atoms (hereinafter referred to as a "non-fluorinated solvent") may be added.
[0090] The fluorinated solvent may be, for example, 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether, 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, 1H,1H,5H-octafluoropentyl-1,1,2,2-tetrafluoroethyl ether, and the like.
[0091] The non-fluorine-containing solvent may be, for example, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, 1,2-dimethoxyethane, dimethoxyethane, dimethoxypropane, dimethoxybutane, diethylene glycol dimethyl ether, acetonitrile, dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, chloroethylene carbonate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, trimethyl phosphate, triethyl phosphate, and 12-crown-4.
[0092] The above fluorinated solvents and / or non-fluorinated solvents may be used alone or in any combination of two or more in any ratio. The contents of the fluorinated solvent and non-fluorinated solvent are not particularly limited, and the ratio of the fluorinated solvent to the entire solvent may be 0 to 100% by volume, and the ratio of the non-fluorinated solvent to the entire solvent may be 0 to 100% by volume.
[0093] <Secondary battery manufacturing method> Next, an example of a method for manufacturing the secondary battery 1 (hereinafter also referred to as "this manufacturing method") will be described with reference to Figs. 7 to 10. Fig. 7 is a flow chart showing an example of this manufacturing method. Figs. 8A and 8B are views for explaining step ST1 in Fig. 7. Figs. 9A to 9D are views for explaining step ST2 in Fig. 7. Fig. 10 is a view for explaining step ST3 in Fig. 7.
[0094] As shown in FIG. 7 , this manufacturing method includes step ST1 of preparing a positive electrode laminate sheet, step ST2 of joining metal sheets of the positive electrode laminate sheet, step ST3 of cutting out the positive electrode laminate sheet or the positive electrode laminate, step ST4 of assembling a molded body, step ST5 of joining electrode tabs and a current collector, and step ST6 of sealing the molded body in an airtight container.
[0095] First, in step ST1, as shown in FIG. 8A and FIG. 8B, a positive electrode laminate sheet S1 is prepared. FIG. 8A is a plan view of the positive electrode laminate sheet S1. FIG. 8B is a cross-sectional view taken along the line BB of FIG. 8A. As shown in FIG. 8A, the positive electrode laminate sheet S1 may be a strip-shaped sheet having a longitudinal direction (y direction) and a lateral direction (x direction). In one embodiment, as shown in FIG. 8A and FIG. 8B, the positive electrode laminate sheet S1 may be composed of a current collector 32 and a positive electrode 34 applied to both sides of the current collector 32. The current collector 32 may have an insulating layer 320 and a conductive layer 322 formed to sandwich the insulating layer 320. At one end of the positive electrode laminate sheet in the lateral direction (x direction), the positive electrode 34 is not formed, and the conductive layer 322 of the current collector 32 is exposed.
[0096] Next, in step ST2, a metal sheet MS is joined to one short-side end of the positive electrode laminate sheet S1 as shown in Fig. 9A to Fig. 9D. Fig. 9A is a plan view of the positive electrode laminate sheet S1 to which the metal sheet MS is joined. Fig. 9B to Fig. 9D are examples of a CC cross section of Fig. 9A.
[0097] As shown in Fig. 9A, the first bonding marks WR1 are formed in the longitudinal direction, for example, in a line shape. The metal sheet MS may be joined to the positive electrode laminate sheet S1 by welding. The welding may be, for example, ultrasonic welding, laser welding, resistance welding, or spot welding. In one example, the welding is ultrasonic welding.
[0098] In one embodiment, the bonding in step ST2 may be performed by pressing the metal sheet MS against the current collector 32. For example, as shown in FIG. 9B and FIG. 9C, the first bonding mark WR1 may be formed so that the metal sheet MS is recessed toward the current collector 32. In one embodiment, the first bonding mark WR1 may be provided between the metal sheet MS and one conductive layer 322 (with which the metal sheet MS is in contact) as shown in FIG. 9B. In this case, the metal sheet MS is not electrically connected to the other conductive layer 322 at the first bonding mark WR1. In one embodiment, the first bonding mark WR1 may be provided between the metal sheet MS and both conductive layers 322 as shown in FIG. 9C. In this case, the metal sheet MS is electrically connected to both conductive layers 322 at the first bonding mark WR1.
[0099] In one embodiment, the bonding in step ST2 may be performed by pressing the current collector 32 against the metal sheet MS. For example, as shown in Fig. 9D, the first bonding mark WR1 may be formed so that the current collector 32 is recessed toward the metal sheet MS. In this case, the metal sheet MS is electrically connected to both conductive layers 322 at the first bonding mark WR1.
[0100] Next, in step ST3, the positive electrode laminate 30 is cut out. Specifically, using a cutting blade, a laser, or the like, a plurality of positive electrode laminates 30 having a given shape are cut out from the positive electrode laminate sheet S1 in a state in which the metal sheet MS is joined to the positive electrode laminate sheet S1 as shown in Fig. 10. In this way, a plurality of positive electrode laminates 30 are obtained.
[0101] Next, in step ST4, a molded body is assembled in which the positive electrode laminates 30 and the intermediate laminates LM are alternately laminated. Specifically, the multiple positive electrode laminates 30 prepared in step ST3 are arranged so as to be spaced apart from each other in the stacking direction via the intermediate laminates LM, as shown in Fig. 1. Note that, when the negative electrode 10 and the separator 20 are configured in a sheet shape as described below, each positive electrode laminate 30 may be arranged between the separators 20 formed by folding the sheet in a zigzag shape (see Fig. 9) or between the separators 20 formed by rolling the sheet (see Fig. 10).
[0102] Next, in step ST5, the electrode tabs and the current collectors are joined. Specifically, the end P of each current collector 32 and the metal sheet MS are joined to the electrode tab 40 so as to form the above-mentioned second joining mark WR2. The second joining mark WR2 is joined so as not to overlap with the first joining mark WR1 in the stacking direction. This makes it possible to... Furthermore, the negative electrode end Q is joined to the negative electrode tab 42 so as to form a joining mark WL2. The joining may be performed by ultrasonic welding, laser welding, resistance welding, or spot welding.
[0103] Next, in step ST6, the molded body prepared in step ST5 is sealed in a sealed container. In one embodiment, an electrolyte may be sealed in the sealed container. The sealed container may be, for example, a laminate film. In this manner, the secondary battery 1 is manufactured.
[0104] In this manufacturing method, in step ST2, the metal sheet MS is bonded to the positive electrode laminate sheet MS in advance. Therefore, in step ST3, the metal sheet MS can be simultaneously cut out to match the shape of the end P of the positive electrode laminate sheet S1. That is, a separate step of cutting the metal sheet MS to match the shape of the end P is not required. In addition, in step ST5, alignment between the metal sheet MS and the end P of the current collector 32 is not required, so that the positive electrode tab 40 and the end P can be easily bonded. Furthermore, in step ST5, it is theoretically possible to provide the second bonding mark WR2 so as not to overlap with the first bonding mark WR1 in the stacking direction. By providing the second bonding mark WR2 so as not to overlap with the first bonding mark WR1 in the stacking direction, the bonding state of the second bonding mark WR2 is improved compared to the case where the two are provided overlapping each other, and an increase in the resistance of the second bonding mark WR2 can be suppressed.
[0105] <How to use secondary batteries> The secondary battery 1 is charged and discharged by connecting the positive electrode tab 40 to one end of an external circuit and the negative electrode tab 42 to the other end of the external circuit. The external circuit may be, for example, a resistor, a power source, an apparatus, a device, another battery, or a potentiostat. The ends P of the multiple positive electrode laminates 30 may be connected to the external circuit at the same potential. The negative electrode ends Q of the multiple negative electrodes 10 may be connected to the external circuit at the same potential.
[0106] When a voltage is applied between the positive electrode tab 40 and the negative electrode tab 42 such that a current flows from the negative electrode tab 42 through an external circuit to the positive electrode tab 40, the secondary battery 1 is charged and lithium metal is deposited on the negative electrode 10. When the positive electrode tab 40 and the negative electrode tab 42 are connected to the charged secondary battery 1 via a desired external circuit, the secondary battery 1 is discharged and the lithium metal in the negative electrode 10 is electrolytically dissolved.
[0107] In one embodiment, the secondary battery 1 may have a solid electrolyte interface layer (SEI layer) formed on the surface of the negative electrode 10 or the surface of the separator 20 (i.e., the interface between the negative electrode 10 and the separator 20) by the first charge (initial charge) after the assembly of the battery. The SEI layer may contain, for example, an inorganic compound containing lithium, or an organic compound containing lithium. In one embodiment, the thickness of the SEI layer is 1.0 nm or more and 10 μm or less. When the secondary battery 1 has an SEI layer formed therein, lithium metal is precipitated or dissolved at the interface between the negative electrode 10 and / or the separator 20 and the SEI layer by charge and discharge.
[0108] According to the secondary battery 1 described above, the output characteristics and productivity of the battery can be improved.
[0109] <Modification> The secondary battery 1 can be modified in various ways without departing from the scope and spirit of the present disclosure.
[0110] (Negative electrode 10) FIG. 11 is a perspective view showing another example of the negative electrode 10. In one embodiment, a metal sheet may be provided at the negative electrode end Q of the negative electrode 10. The example shown in FIG. 11 is an example in which a metal sheet MS2 for the negative electrode is provided on one surface of the negative electrode end Q of the negative electrode 10 shown in FIG. 2B. In one embodiment, the metal sheet MS2 for the negative electrode may be made of the same material as the negative electrode conductive layer 162. In one example, the metal sheet MS2 for the negative electrode is Cu.
[0111] 11, a first bonding mark WL1 may be formed between the negative electrode metal sheet MS2 and the negative electrode end Q by bonding them together. A second bonding mark WL2 may be formed between the negative electrode end Q and the negative electrode metal sheet MS2 and the negative electrode tab 42. The bonding form and positional relationship of the first bonding mark WL1 and the second bonding mark WL2 of the negative electrode end Q may be similar to the first bonding mark WR1 and the second bonding mark WR2 of the end P, and a description thereof will be omitted.
[0112] FIG. 12 is a perspective view showing another example of the negative electrode 10. In one embodiment, the negative electrode 10 may not substantially have a negative electrode active material. In the example shown in FIG. 12, the negative electrode 10 is made of at least one selected from the group consisting of Cu, Ni, Ti, Fe, and other metals that do not react with Li, alloys thereof, and stainless steel (SUS). The "metal that does not react with Li" may be a metal that does not react with lithium ions or lithium metal to form an alloy in the operating state of the secondary battery 1. The negative electrode 10 also functions as a current collector.
[0113] The negative electrode 10 being "substantially free of negative electrode active material" includes, for example, that the layer thickness of the negative electrode active material deposited on the negative electrode 10 at the end of discharge (for example, a state in which the open circuit voltage of the battery is 2.5 V or more and 3.6 V or less) is 25 μm or less. In one embodiment, the layer thickness of the negative electrode active material at the end of discharge may be 20 μm or less, 15 μm or less, 10 μm or less, or 5 μm or less, or may be 0 μm. Since the negative electrode 10 is substantially free of negative electrode active material, the energy density per volume can be improved in addition to the weight energy density. In this case, the secondary battery 1 can also be called an "anode-free lithium battery", a "zero anode lithium battery", or an "anodeless lithium battery".
[0114] In one embodiment, the negative electrode 10 does not have a negative electrode active material before the initial charge of the battery (the state from the assembly of the battery to the first charge). That is, the secondary battery 1 may be charged and discharged by depositing lithium metal on the negative electrode after the initial charge, and then electrolytically dissolving the deposited lithium metal. In this case, the volume and mass occupied by the negative electrode active material are suppressed, the volume and mass of the entire battery are reduced, and the energy density is increased in principle. Note that "lithium metal deposits on the negative electrode" includes not only lithium metal depositing on the surface of the negative electrode, but also lithium metal depositing on the surface of a solid electrolyte interface (SEI) layer or on the surface or inside of a buffer functional layer, which will be described later.
[0115] In one embodiment, the mass of lithium metal deposited on the negative electrode when the voltage is 4.2 V is M 4.2 The same mass at a voltage of 3.0 V is M 3.0 In this case, M 3.0 / M 4.2 may be 40% or less, or 35% or less. In one embodiment, the ratio M 3.0 / M 4.2 may be 1.0% or more, 2.0% or more, 3.0% or more, or 4.0% or more.
[0116] In one embodiment, the thickness of the negative electrode 10 may be 1.0 μm or more and 30 μm or less. This can reduce the volume occupied by the negative electrode 10 in the secondary battery 1, and improve the energy density. The thickness of the negative electrode 10 may be 2.0 μm or more and 20 μm or less, 2.0 μm or more and 18 μm or less, or 3.0 μm or more and 15 μm or less.
[0117] In one embodiment, the negative electrode 10 may be coated on at least a portion of the surface facing the positive electrode laminate 30 with a compound including an aromatic ring to which two or more elements selected from the group consisting of N, S, and O are bonded independently (hereinafter, also referred to as "negative electrode coating agent"). The negative electrode coating agent can be held on the negative electrode 10 by the above-mentioned elements being coordinately bonded to metal atoms constituting the negative electrode 10. According to this embodiment, a non-uniform deposition reaction of lithium metal is suppressed on the surface of the negative electrode 10, and the lithium metal deposited on the negative electrode 10 can be suppressed from growing in a dendritic shape.
[0118] In one embodiment, the negative electrode coating agent is coated on at least a portion of the surface of the negative electrode 10. In one embodiment, 10% or more of the surface area may have the negative electrode coating agent, or 20% or more, 40% or more, 60% or more, or 80% or more of the surface may have the negative electrode coating agent.
[0119] In one embodiment, the aromatic ring included in the negative electrode coating agent may be an aromatic hydrocarbon such as benzene, naphthalene, azulene, anthracene, and pyrene, and a heteroaromatic compound such as furan, thiophene, pyrrole, imidazole, pyrazole, pyridine, pyridazine, pyrimidine, and pyrazine. In one example, the aromatic ring is an aromatic hydrocarbon. In one example, the aromatic ring is benzene or naphthalene. In one example, the aromatic ring is benzene.
[0120] In one embodiment, the negative electrode coating agent may be configured by bonding one or more nitrogen atoms to an aromatic ring. In one embodiment, the negative electrode coating agent may be a compound having a structure in which a nitrogen atom is bonded to an aromatic ring and one or more elements selected from the group consisting of N, S, and O are bonded independently to the nitrogen atom. When a compound in which a nitrogen atom is bonded to an aromatic ring is used as the negative electrode coating agent, the cycle characteristics of the battery may be improved.
[0121] The negative electrode coating agent may be, for example, at least one selected from the group consisting of benzotriazole, benzimidazole, benzimidazole thiol, benzoxazole, benzoxazole thiol, benzothiazole, and mercaptobenzothiazole, and derivatives thereof. In one example, the negative electrode coating agent is at least one selected from the group consisting of benzotriazole, benzimidazole, benzoxazole, and mercaptobenzothiazole, and derivatives thereof.
[0122] (buffer layer) In one embodiment, a porous or fibrous buffer functional layer may be provided between the negative electrode 10 and the separator 20. The buffer functional layer has a solid portion (including a gel portion) having ionic conductivity and electrical conductivity, and a pore portion formed by gaps in the solid portion. In this case, lithium metal may be precipitated on the surface of the negative electrode 10 (the interface between the negative electrode 10 and the buffer functional layer) and / or inside the buffer functional layer (the surface of the solid portion of the buffer functional layer).
[0123] (Intermediate laminate) 13 and 14 are cross-sectional views of a main part for explaining another example of the configuration of a lithium secondary battery. In one embodiment, the negative electrode 10 and the separators 20 arranged on both sides of the negative electrode 10 may be configured as a single sheet SH.
[0124] In one embodiment, as shown in FIG. 13, a sheet SH is folded alternately at acute angles multiple times to form an intermediate laminate, and each positive electrode laminate 30 (30A, 30B) may be disposed between opposing separators 20 of the intermediate laminate.
[0125] In one embodiment, as shown in Fig. 14, a sheet SH is wound multiple times to form an intermediate laminate, and each positive electrode laminate 30 (30A, 30B) may be disposed between the opposing separators 20 of the intermediate laminate. In the example shown in Fig. 14, each positive electrode laminate 30 may also be formed by winding a single sheet as described below (see Fig. 15).
[0126] 13 and 14, even if the negative electrode 10 and the separator 20 are very thin, they can be handled as a single sheet SH, which can improve the productivity of the battery. In addition, in the sheet SH, physical pressure is applied from both sides to the negative electrode 10 sandwiched between the separators 20, so that wrinkles are less likely to occur in the negative electrode 10 when the sheets SH are laminated, which can improve the cycle characteristics of the battery.
[0127] (Positive electrode laminate) 15 and 16 are perspective views for explaining other configuration examples of the positive electrode laminate. In one embodiment, each positive electrode laminate 30 may be configured by winding one sheet SH2 multiple times as shown in FIG. 15. In one embodiment, each positive electrode laminate 30 may be configured by folding one sheet SH2 alternately multiple times at acute angles as shown in FIG. 16. The sheet SH2 may be configured to include, for example, a current collector 32 and a positive electrode 34 disposed on both sides of the current collector 32. In the examples shown in FIG. 15 and FIG. 16, even if the current collector 32 and the positive electrode 34 are very thin, they can be handled as one sheet SH2, so that the productivity of the battery can be improved.
[0128] <Example> Next, examples and comparative examples will be described. The present disclosure is not limited in any way by the following examples and comparative examples.
[0129] Fig. 17 is a diagram showing the configurations and results of the examples and comparative examples. Fig. 18 is a diagram showing the lamination patterns of the metal sheets in the examples and comparative examples. "Pattern 1" to "Pattern 4" in Fig. 18 correspond to "Pattern 1" to "Pattern 4" shown in "Lamination Pattern" in Fig. 17.
[0130] Example 1 As Example 1, a lithium secondary battery having a structure shown in FIG. 1 was prepared. First, a negative electrode 10 having a structure shown in FIG. 2B was prepared. A 6 μm thick polyethylene terephthalate (PET) was used as the negative electrode insulating layer 160 of the negative electrode current collector 16, and 1.0 μm of Cu was evaporated as the negative electrode conductive layer 162. As the negative electrode active material 14, a mixed material was used in which 97 parts by mass of graphite, 0.5 parts by mass of carbon black as a conductive aid, and 1.5 parts by mass of carboxymethyl cellulose (CMC) and 1.0 part by mass of styrene-butadiene rubber (SBR) as binders were mixed with water as a solvent. As described above, 21 negative electrodes 10 were prepared. Then, a metal sheet MS2 (copper foil having a thickness of 4 μm) for the negative electrode was attached to the negative electrode end Q of each negative electrode 10 by ultrasonic welding, resulting in the structure shown in FIG. 11. Next, a sheet (thickness: 15 μm) whose surface was coated with a mixture of polyvinylidene fluoride (PVDF) and Al2O3 was prepared as the separator 20. Then, both sides of the negative electrode 10 were sandwiched and pressed with the separators 20 to obtain an intermediate laminate LM.
[0131] The current collector 32 of the positive electrode laminate 30 was a 6 μm-thick film of polyethylene terephthalate (PET, insulating layer 320) with 1.0 μm of Al (conductive layer 322) vapor-deposited on both sides. The positive electrode 34 was made of N-methyl-pyrrolidone (NMP) as a solvent and LiNi as a positive electrode active material. 0.8 Co 0.15 Al 0.05 A mixture of 96 parts by mass of O2, 2 parts by mass of carbon black as a conductive assistant, and 2 parts by mass of polyvinylidene fluoride (PVDF) as a binder was used. The positive electrode 34 was attached to both sides of the current collector 32 with a basis weight of 23 mg / cm 2 A positive electrode laminate 30 was obtained by applying the coating solution to the positive electrode laminate 30. Twenty positive electrode laminates 30 were prepared. A metal sheet MS (12 μm hard aluminum) having a configuration shown in "Example 1" of FIG. 17 was attached to the end P of the current collector 32 of each of the ten positive electrode laminates 30 by ultrasonic welding. A positive electrode tab 40 (thickness 0.2 mm) made of the material (hard aluminum) shown in "Example 1" of FIG. 17 was also prepared. Nickel-plated copper having a thickness of 0.2 mm was used as the negative electrode tab 42.
[0132] Next, the intermediate laminate LM and the positive electrode laminate 30 were alternately laminated. At this time, the positive electrode laminate 30 with the metal sheet MS attached to the end P and the positive electrode laminate 30 without the metal sheet MS attached were appropriately selected so as to obtain the lamination pattern (pattern 1) shown in FIG. 18. Then, each end P of the current collector 32 and the metal sheet MS were overlapped and joined to the positive electrode tab 40 by ultrasonic welding. In addition, the negative electrode end Q and the metal sheet MS2 for the negative electrode were overlapped and joined to the negative electrode tab 42 by ultrasonic welding. This structure was inserted into a laminate exterior body and sealed together with an electrolyte to obtain a lithium secondary battery. The electrolyte used was an electrolyte solution in which lithium hexafluorophosphate (LiPF6) was dissolved in a solvent mixed with ethylene carbonate (EC), dimethyl carbonate (DMC), and ethyl methyl carbonate (EMC) in a ratio of 30:35:35 parts by mass, to which 2 parts by weight of vinylene carbonate (VC) was added so as to be 1M.
[0133] (Examples 2 to 8) In Examples 2 to 8, lithium secondary batteries were produced in the same manner as in Example 1, except that the material and thickness of the metal sheet MS, the material of the positive electrode tab 40, and the lamination pattern of the metal sheet MS were different, as shown in Figures 17 and 18.
[0134] Comparative Example 1 In Comparative Example 1, a lithium secondary battery was produced in the same manner as in Example 1, except that the metal sheet MS was not used.
[0135] 17, "X / Y" is the value obtained by dividing X by Y when, for Examples 1 to 8, the sum of the total thickness (A) of each metal sheet MS and the total thickness (B) of each conductive layer 322 is X (=A+B) and the total thickness of each insulating layer 320 is Y. In Comparative Example 1, since no metal sheet MS is used, X is the total thickness of each conductive layer.
[0136] In FIG. 17, "resistance [mΩ]" is the resistance at the second bonding mark WR2, and the lithium secondary batteries according to the examples and the comparative examples were disassembled and measured by a four-terminal method. Specifically, the positive electrode of a clip-type lead of a resistance meter BT3561 manufactured by HIOKI was connected to the positive electrode tab 40, and the negative electrode was clipped at a location of one of the 20 positive electrode laminates 30 where the positive electrode active material was not applied, and the impedance at 1 kHz was measured with the four-terminal lead. Next, the negative electrode was connected to another positive electrode laminate and measurement was performed, and the average value of the 20 pieces was obtained. This average value is "resistance (mΩ)" shown in FIG. 17. As shown in FIG. 17, the resistance at the second bonding mark WR2 in Examples 1 to 8 was significantly lower than that in Comparative Example 1.
[0137] In addition, when a nail penetration test was performed on the lithium secondary batteries according to Examples 1 to 8 and Comparative Example 1, no fire or explosion occurred in any of them. The nail penetration test is a test in which a nail is penetrated into each battery to simulate an internal short circuit, and the presence or absence of fire or explosion of the battery is confirmed.
[0138] Comparative Example 2 In Comparative Example 2, a lithium secondary battery was produced in the same manner as in Example 1, except that the metal sheet MS2 for the negative electrode was not used.
[0139] In Example 1 and Comparative Example 2, the resistance in the joint area between the negative electrode tab 42 and the negative electrode end Q was measured in the same manner as described above. In Comparative Example 2, the resistance was 19.4 [mΩ]. In contrast, in Example 1, the resistance was 0.88 mΩ, which was significantly lower than that of Comparative Example 2.
[0140] The embodiments of the present disclosure further include the following aspects.
[0141] (Appendix 1) A lithium secondary battery, (a) a first laminate including a first current collector having a first insulating layer sandwiched between a pair of first conductive layers, and a first electrode disposed on the first current collector, the first current collector having a first end portion where the first electrode is not disposed; (b) an intermediate laminate including an electrode having a polarity different from that of the first electrode and a separator; (c) a second laminate disposed away from the first laminate in a stacking direction via the intermediate laminate, the second laminate including a second current collector having a second insulating layer sandwiched between a pair of second conductive layers, and a second electrode disposed on the second current collector and having the same polarity as the first electrode, the second current collector having a second end portion where the second electrode is not disposed; (d) a metal sheet arranged in the stacking direction with respect to the first end portion and the second end portion, the metal sheet having a first joining mark due to joining with either one of the first end portion and the second end portion; (e) an electrode tab electrically connected to the first laminate and the second laminate, the electrode tab having a second bonding mark by bonding the first end, the metal sheet, and the second end, the second bonding mark being located at a position different from the first bonding mark when viewed from the stacking direction; Lithium secondary battery.
[0142] (Appendix 2) 2. The lithium secondary battery according to claim 1, wherein the first joining mark is a welding mark.
[0143] (Appendix 3) 3. The lithium secondary battery according to claim 1, wherein the first bonding mark is in the form of one or more lines.
[0144] (Appendix 4) 3. The lithium secondary battery according to claim 1, wherein the first bonding mark is in the form of one or more dots.
[0145] (Appendix 5) 5. The lithium secondary battery according to claim 1, wherein the second joining mark is a welding mark.
[0146] (Appendix 6) 6. The lithium secondary battery according to claim 1, wherein the second bonding mark is in the form of one or more lines.
[0147] (Appendix 7) 6. The lithium secondary battery according to claim 1, wherein the second bonding mark is in the form of one or more dots.
[0148] (Appendix 8) 8. The lithium secondary battery according to claim 1, wherein the second bonding marks include, in a cross section in the stacking direction, a region where the pair of first conductive layers, the metal sheet, and the pair of second conductive layers are integrated together.
[0149] (Appendix 9) 9. The lithium secondary battery according to claim 1, wherein the first bonding mark and the second bonding mark do not overlap each other when viewed from the stacking direction.
[0150] (Appendix 10) 10. The lithium secondary battery according to claim 1, wherein the first stack and the second stack are arranged alternately in the stacking direction with the intermediate stack sandwiched between them.
[0151] (Appendix 11) The lithium secondary battery according to claim 10, wherein the first laminate is formed of a flat sheet, and the second laminate is formed of a flat sheet separate from the first laminate.
[0152] (Appendix 12) 11. The lithium secondary battery according to claim 10, wherein the first laminate and the second laminate are formed by folding or rolling a single sheet.
[0153] (Appendix 13) 13. The lithium secondary battery according to claim 10, wherein the first stack and the second stack are arranged in a total of 10 or more layers.
[0154] (Appendix 14) 14. The lithium secondary battery of claim 10, wherein the metal sheet is provided at at least one of the first ends and the second ends.
[0155] (Appendix 15) 15. The lithium secondary battery of claim 14, wherein the metal sheet is provided on one side of the at least one end.
[0156] (Appendix 16) 15. The lithium secondary battery of claim 14, wherein the metal sheets are provided on both sides of the at least one end.
[0157] (Appendix 17) 17. The lithium secondary battery of claim 10, wherein the number of the metal sheets is three times or less than the total number of the first ends and the second ends.
[0158] (Appendix 18) 18. The lithium secondary battery of claim 1, wherein the metal sheet is made of the same material as the first conductive layer and the second conductive layer.
[0159] (Appendix 19) 19. The lithium secondary battery according to claim 1, wherein the first electrode and the second electrode are positive electrodes.
[0160] (Appendix 20) 19. The lithium secondary battery according to claim 1, wherein the first electrode and the second electrode are negative electrodes. [Explanation of symbols]
[0161] 1: Lithium secondary battery, 10: negative electrode, 20: separator, 30: positive electrode laminate, 32: current collector, 320: insulating layer, 322: conductive layer, 34: positive electrode, 40: positive electrode tab, 42: negative electrode tab, MS: metal sheet, LM: intermediate laminate, WR1: first bonding mark, WR2: second bonding mark
Claims
1. A lithium secondary battery, (a) a first laminate including a first current collector having a first insulating layer sandwiched between a pair of first conductive layers, and a first electrode disposed on the first current collector, the first current collector having a first end portion where the first electrode is not disposed; (b) an intermediate laminate including an electrode having a polarity different from that of the first electrode and a separator; (c) a second laminate disposed in a stacking direction away from the first laminate via the intermediate laminate, the second laminate including a second current collector configured by sandwiching a second insulating layer between a pair of second conductive layers, and a second electrode disposed on the second current collector and having the same polarity as the first electrode, the second current collector having a second end portion where the second electrode is not disposed; (d) a metal sheet arranged in the stacking direction with respect to the first end and the second end, the metal sheet having a first joining mark due to joining with either one of the first end and the second end; (e) an electrode tab electrically connected to the first laminate and the second laminate, the electrode tab having a second bonding mark by bonding the first end, the metal sheet, and the second end, the second bonding mark being located at a position different from the first bonding mark when viewed from the stacking direction; Lithium secondary battery.
2. The lithium secondary battery according to claim 1 , wherein the first joining mark is a welding mark.
3. The lithium secondary battery according to claim 2 , wherein the first bonding mark is in the form of one or more lines.
4. The lithium secondary battery according to claim 2 , wherein the first bonding mark is in the form of one or more dots.
5. The lithium secondary battery according to claim 1 , wherein the second joining mark is a welding mark.
6. The lithium secondary battery according to claim 5 , wherein the second bonding mark is in the form of one or more lines.
7. The lithium secondary battery according to claim 5 , wherein the second bonding mark is in the form of one or more dots.
8. The lithium secondary battery according to claim 1 , wherein the second bonding marks include regions where the pair of first conductive layers, the metal sheet, and the pair of second conductive layers are integrated in a cross section in the stacking direction.
9. The lithium secondary battery according to claim 1 , wherein the first bonding mark and the second bonding mark do not overlap each other when viewed from the stacking direction.
10. 10. The lithium secondary battery according to claim 1, wherein a plurality of the first stacks and a plurality of the second stacks are alternately arranged in the stacking direction with the intermediate stack interposed therebetween.
11. 11. The lithium secondary battery according to claim 10, wherein the first laminate is formed of a flat sheet, and the second laminate is formed of a flat sheet separate from the first laminate.
12. The lithium secondary battery according to claim 10 , wherein the first laminate and the second laminate are formed by folding or rolling a single sheet.
13. The lithium secondary battery according to claim 10 , wherein a total of 10 layers of the first stack and the second stack are arranged.
14. The lithium secondary battery according to claim 10 , wherein the metal sheet is provided on at least one of the first ends and the second ends.
15. The lithium secondary battery according to claim 14 , wherein the metal sheet is provided on one side of the at least one end portion.
16. The lithium secondary battery according to claim 14 , wherein the metal sheets are provided on both sides of the at least one end portion, one on each side.
17. The lithium secondary battery according to claim 10 , wherein the number of the metal sheets is equal to or less than three times the total number of the first ends and the second ends.
18. The lithium secondary battery according to claim 1 , wherein the metal sheet is made of the same material as the first conductive layer and the second conductive layer.
19. 10. The lithium secondary battery according to claim 1, wherein the first electrode and the second electrode are positive electrodes.
20. 10. The lithium secondary battery according to claim 1, wherein the first electrode and the second electrode are negative electrodes.
Citation Information
Patent Citations
Lithium ion secondary battery
JP1999102711A
Collector and nonaqueous secondary battery
JP2013016321A