Display panel and manufacturing method of display panel
The display panel design addresses transmittance unevenness by promoting uniform polymerization across the frame region using a substrate without light-shielding and additional features, achieving consistent transmittance and reducing display unevenness.
Patent Information
- Application Number
- JP2023075664
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-01
- Publication Date
- 2024-11-14
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Display panels with PDLC layers exhibit transmittance unevenness near the frame region due to differences in anchoring transition temperatures, leading to display unevenness.
The display panel design includes a first substrate with a photocurable monomer layer and a second substrate without a light-shielding portion in the frame area, promoting uniform polymerization and reducing residual monomer, along with additional features like colored portions and ink layers to enhance uniformity.
This configuration suppresses display unevenness by ensuring consistent polymerization across the panel, maintaining uniform transmittance and reducing irreversible transparent areas near the frame region.
Smart Images

Figure 2024160543000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a display panel and a method for manufacturing the display panel, and more particularly to a display panel and a method for manufacturing the display panel. [Background technology]
[0002] In recent years, display panels such as see-through panels that can display images through the back of the display panel have been attracting attention. For example, display panels using a polymer dispersed liquid crystal (PDLC) layer have been developed. The PDLC layer has a structure in which liquid crystal components are dispersed in a polymer network obtained by photopolymerizing a photocurable monomer, and the orientation state of the liquid crystal components is changed by applying a voltage, and the difference in refractive index between the liquid crystal components and the polymer network can be used to switch between a transparent state and a scattering state.
[0003] As an example of technology relating to a display panel using a PDLC layer, Patent Document 1 discloses a liquid crystal display device comprising a first substrate and a second substrate arranged opposite each other, a polymer dispersed liquid crystal layer provided between the first substrate and the second substrate, and a black matrix provided on the first substrate, the liquid crystal display device defining a display area for displaying images and a frame area around the display area, in which the black matrix is constituted by a plurality of light-shielding portions spaced apart from each other. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2010 / 103589 Summary of the Invention [Problem to be solved by the invention]
[0005] Fig. 28 is a schematic diagram showing the appearance of a display panel according to a comparative embodiment. As shown in Fig. 28, in the comparative display panel 1R, an area with a different transmittance from other areas appears near the frame region 1NA (specifically, the frame region 1NA on the opposite side to the terminal side) at a certain temperature (e.g., 45°C). Thus, in the comparative display panel 1R having a PDLC layer, the transmittance increases at a certain temperature (e.g., 30 to 40°C, depending on the panel manufacturing conditions and materials) in the vicinity of the frame region 1NA on the opposite side to the terminal side where the terminals are provided, compared to other areas, causing unevenness (display unevenness).
[0006] As with the comparative display panel, the liquid crystal display device of Patent Document 1 also has a problem in that the transmittance in the vicinity of the frame region is higher than in other areas, causing display unevenness.
[0007] The present invention has been made in consideration of the above-mentioned current situation, and aims to provide a display panel that can suppress display unevenness in the vicinity of the frame region, and a manufacturing method for the display panel. [Means for solving the problem]
[0008] (1) One embodiment of the present invention is a display panel comprising a display area for displaying an image and a frame area provided around the display area, the display panel comprising, in this order, a first substrate having a switching element, a polymer-containing layer containing a polymer of a photocurable monomer, and a second substrate having a light-shielding portion that blocks light of a wavelength used for polymerization of the photocurable monomer and that is not disposed in the frame area.
[0009] (2) Moreover, in addition to the configuration of (1), an embodiment of the present invention is a display panel, wherein the polymer-containing layer contains a polymer network constituted by a polymer of the photocurable monomer, and a liquid crystal component.
[0010] (3) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1) above, the polymer-containing layer is composed of a polymer of the photocurable monomer, and contains a pair of polymer layers located on the surface facing the first substrate and the surface facing the second substrate, and a liquid crystal component located between the pair of polymer layers.
[0011] (4) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), or (3), the first substrate is provided with a plurality of gate lines extending parallel to each other and a plurality of source lines extending parallel to each other in a direction intersecting the plurality of gate lines via an insulating layer, and a black matrix layer is provided in the display region at a position overlapping the plurality of gate lines and the plurality of source lines.
[0012] (5) Furthermore, in one embodiment of the present invention, in addition to the configuration of (1), (2), (3) or (4), the second substrate further includes a colored portion in the frame region that transmits light of a wavelength used for polymerization of the photocurable monomer.
[0013] (6) Furthermore, in an embodiment of the present invention, in addition to the configuration of (1), (2), (3), (4) or (5), the display panel further comprises an ink portion in at least one of a frame region of the first substrate opposite the polymer-containing layer and a frame region of the second substrate opposite the polymer-containing layer.
[0014] (7) Furthermore, in one embodiment of the present invention, in addition to the configuration of (6) above, the display panel further comprises a second substrate side film located on the opposite side of the second substrate to the polymer-containing layer, and the ink portion comprises a second substrate side ink portion located at least either between the second substrate side film and the second substrate, or on the opposite side of the second substrate of the second substrate side film to the second substrate.
[0015] (8) Furthermore, in one embodiment of the present invention, in addition to the configuration of (7) above, the second substrate side ink portion is located between the second substrate side film and the second substrate.
[0016] (9) Moreover, in one embodiment of the present invention, in addition to the configuration of (7) or (8), the second substrate side film is a UV cut film.
[0017] (10) Moreover, in accordance with another embodiment of the present invention, in addition to the configuration of (7) or (8), the second substrate side film is a polarizer.
[0018] (11) Furthermore, in one embodiment of the present invention, in addition to the configuration of (6), (7), (8), (9) or (10), the display panel further comprises a first substrate side film located on the opposite side of the first substrate to the polymer-containing layer, and the ink portion comprises a first substrate side ink portion located at least either between the first substrate side film and the first substrate, or on the opposite side of the first substrate side film to the first substrate.
[0019] (12) Moreover, in one embodiment of the present invention, in addition to the configuration of (11) above, the first substrate side ink portion is located between the first substrate side film and the first substrate.
[0020] (13) Moreover, in one embodiment of the present invention, in addition to the configuration of (11) or (12), the first substrate side film is a UV cut film.
[0021] (14) Moreover, in accordance with another embodiment of the present invention, in addition to the configuration of (11) or (12), the first substrate side film is a polarizer.
[0022] (15) Furthermore, in one embodiment of the present invention, in addition to the configuration of (6), (7), (8), (9), (10), (11), (12), (13) or (14), the display panel further includes a housing, and the ink portion is the same color as the housing.
[0023] (16) Furthermore, another embodiment of the present invention is a method for manufacturing a display panel, comprising an exposure step of irradiating light from the second substrate side to a panel precursor having a composition containing a photocurable monomer filled between a first substrate having switching elements and a second substrate having no light-shielding portion in a frame region provided around a display region for displaying an image.
[0024] (17) Furthermore, in one embodiment of the present invention, in addition to the configuration of (16), a method for manufacturing a display panel further includes, after the exposure step, a bonding step of bonding a first substrate side film, having a first substrate side ink portion arranged in the frame region, to the side of the first substrate opposite the second substrate.
[0025] (18) Furthermore, in one embodiment of the present invention, in addition to the configuration of (16) or (17), a method for manufacturing a display panel further includes, after the exposure step, a bonding step of bonding a second substrate side film, having a second substrate side ink portion arranged in the frame region, to the side of the second substrate opposite the first substrate. Effect of the Invention
[0026] According to the present invention, it is possible to provide a display panel capable of suppressing display unevenness in the vicinity of the frame region, and a method for manufacturing the display panel. [Brief description of the drawings]
[0027] [Figure 1A] 1 is a schematic plan view of a display panel according to Embodiment 1. FIG. [Figure 1B] 2 is a plan view illustrating a first substrate included in the display panel according to the first embodiment. FIG. [Figure 1C]3 is a plan view illustrating a second substrate included in the display panel according to the first embodiment. FIG. [Figure 1D] 1B is a cross-sectional view of the display panel according to the first embodiment taken along the line A1-A2 in FIG. 1A. [Diagram 2] FIG. 11 is a schematic plan view of a TFT substrate of a display panel according to a comparative embodiment. [Diagram 3] 3 is a scanning electron microscope photograph of the TFT substrate in the region enclosed by the dashed line in FIG. 2. [Figure 4] 1 is a cross-sectional view illustrating an example of a display panel according to a first embodiment. [Diagram 5] 10 is a cross-sectional view illustrating a case where a second substrate ink portion is located on the opposite side of the second substrate of the second substrate side film in the display panel according to the first embodiment. FIG. [Figure 6] 4 is a cross-sectional view illustrating a case where a second substrate side ink section is provided between a second substrate side film and a second substrate in the display panel according to the first embodiment. FIG. [Figure 7] 3A to 3C are schematic diagrams illustrating a method for manufacturing the display panel according to the first embodiment. [Figure 8] 1 is a cross-sectional view illustrating a display panel according to a first modified example of the first embodiment. [Figure 9] 4 is a cross-sectional view illustrating frame reflection of the display panel according to the first embodiment. FIG. [Figure 10] 10 is a cross-sectional view illustrating frame reflection of a display panel according to Modification 1 of Embodiment 1. FIG. [Figure 11] 11 is a table comparing frame reflections of a display panel according to the first embodiment and a display panel according to a first modified example of the first embodiment. [Figure 12] 1 is a plan view illustrating a first substrate side film included in a display panel according to a first modified example of the first embodiment. FIG. [Figure 13] 11 is a plan view illustrating a first substrate side film included in a display panel according to Modification 2 of Embodiment 1. FIG. [Figure 14] 11 is a cross-sectional view illustrating a liquid crystal display device including a display panel and a backlight according to a third modification of the first embodiment. FIG. [Figure 15] 11A to 11C are schematic diagrams illustrating a method for manufacturing a display panel with a housing according to a fourth modified example of the first embodiment. [Figure 16] 11 is a cross-sectional view illustrating a display panel according to a fifth modified example of the first embodiment. FIG. [Figure 17] 4 is a schematic cross-sectional view illustrating the function of a vertical alignment film. FIG. [Figure 18] FIG. 2 is a schematic cross-sectional view illustrating entanglement between a vertical alignment film and a polymer. [Figure 19] 4 is a schematic cross-sectional view illustrating the function of a horizontal alignment film. FIG. [Figure 20] FIG. 2 is a schematic cross-sectional view illustrating entanglement between a horizontal alignment film and a polymer. [Figure 21] 3A to 3C are schematic diagrams illustrating a method for manufacturing the display panel according to the first embodiment. [Figure 22] 1 is a schematic plan view of a panel precursor used in a manufacturing process of a display panel according to Comparative Example 1. FIG. [Diagram 23] 23 is an enlarged schematic plan view of the area surrounded by the dashed line in FIG. 22. [Figure 24] 5A to 5C are schematic diagrams illustrating a method for manufacturing a display panel according to Comparative Example 1. [Diagram 25] 13 is a schematic plan view showing display unevenness on a display panel of Comparative Example 3 exposed at 40J. FIG. [Figure 26] 13 is a schematic plan view showing display unevenness of a display panel of Comparative Example 3 exposed at 100 J. FIG. [Figure 27] 13 is a graph showing the relationship between the amount of exposure light used in manufacturing a display panel according to Comparative Example 3 and the retention rate of the display panel. [Figure 28] FIG. 13 is a schematic diagram showing the appearance of a display panel according to a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] Hereinafter, an embodiment of the present invention will be described. The present invention is not limited to the contents described in the following embodiment, and appropriate design changes can be made within the scope of the configuration of the present invention. In the following description, the same reference numerals are appropriately used in common between different drawings for the same parts or parts having similar functions, and repeated explanations thereof will be omitted as appropriate. Each aspect of the present invention may be appropriately combined within the scope of the gist of the present invention.
[0029] (Embodiment 1) FIG. 1A is a plan view schematic diagram of a display panel according to embodiment 1. FIG. 1B is a plan view schematic diagram of a first substrate included in the display panel according to embodiment 1. FIG. 1C is a plan view schematic diagram of a second substrate included in the display panel according to embodiment 1. FIG. 1D is a cross-sectional schematic diagram of the display panel according to embodiment 1 taken along line A1-A2 in FIG. 1A. As shown in FIGS. 1A to 1D, the display panel 1 of this embodiment includes a display area 1AA for displaying an image and a frame area 1NA provided around the display area 1AA, and includes a first substrate 100 having a thin film transistor (TFT) 120 as a switching element, a polymer-containing layer 200 containing a polymer of a photocurable monomer, and a second substrate 300 in which a light-shielding portion 320 for blocking light of a wavelength used for polymerization of the photocurable monomer is not disposed in the frame area 1NA, in this order. By adopting such an embodiment, the polymerization of the photocurable monomer is promoted in the frame region 1NA, and it is possible to suppress the amount of remaining monomer (unreacted monomer) in the polymer-containing layer 200. As a result, it is possible to suppress display unevenness in the vicinity of the frame region 1NA.
[0030] As described above, in the comparative display panel 1R having a PDLC layer, the transmittance increases at a certain temperature compared to other areas, resulting in reversible display unevenness. This phenomenon occurs at the transition point of the "anchoring transition" where the liquid crystal components vertically aligned on the polymer network surface in the PDLC layer change to horizontal alignment at a certain temperature. Since the anchoring is weak at the temperature of the transition point, the area becomes transparent even at a voltage below the threshold (for example, a voltage of 0.5 V), which is thought to cause display unevenness. Although the anchoring transition also occurs in other areas, the temperature at which the anchoring transition occurs is higher, so it is thought that only the frame area 1NA on the opposite side to the terminal side is recognized as uneven.
[0031] That is, the reason why the display unevenness is observed only in the vicinity of the frame region 1NA on the opposite side of the terminal side is thought to be because the temperature at which the anchoring transition occurs (anchoring transition point) is lower in the frame region 1NA on the opposite side of the terminal side than in other regions. The reason for this is thought to be as follows.
[0032] Fig. 2 is a schematic plan view of a TFT substrate of a display panel according to a comparative embodiment. Fig. 3 is a scanning electron microscope photograph of the TFT substrate in the region surrounded by the dashed line in Fig. 2. The display panel 1R of the comparative embodiment includes a TFT substrate 100R provided with TFTs as switching elements, as shown in Fig. 2. On the side opposite to the terminal side of the TFT substrate 100R, a wiring pattern 101X outside the display area is arranged between the display region 1AA and the seal 500R.
[0033] 2 and 3, the area not overlapping the wiring pattern 101X is sufficiently exposed to form a polymer, but the back of the wiring pattern 101X (the area overlapping the lower layer of the wiring pattern 101X) is not sufficiently exposed to form a polymer. As a result, the unexposed photocurable monomer contained in the PDLC layer seeps into the display area 1AA, lowering the anchoring transition point, and the anchoring transition occurs at a low temperature.
[0034] In addition, in the comparative display panel 1R, an irreversible transparent area occurs in the vicinity of the frame area 1NA on the opposite side to the terminal edge during high-temperature reliability testing. The reason for this is believed to be as follows: As described above, the unexposed photocurable monomer contained in the PDLC layer seeps into the display area 1AA, and aging at high temperatures changes the surface state of the polymer, resulting in irreversible transparent area unevenness (irreversible display unevenness).
[0035] In the liquid crystal display device of Patent Document 1, the black matrix in the frame region is arranged in a striped pattern at intervals. This reduces the area of the light-shielding area in the frame region caused by the black matrix, and the amount of residual monomer can be reduced. However, in the liquid crystal display device of Patent Document 1, since the light-shielding area still exists in the frame region, when the PDLC layer is formed by exposure, part of the frame region is in the shadow of the light-shielding area. As a result, residual monomer exists in the light-shielding area. Therefore, in the liquid crystal display device of Patent Document 1, the influence of the seepage of the residual monomer cannot be sufficiently reduced.
[0036] On the other hand, in this embodiment, the second substrate 300 that does not have a light-shielding portion 320 such as a black matrix is used in the frame region 1NA, so there is no portion that is shaded by the light-shielding portion when the PDLC layer is formed by exposure, as in Patent Document 1. Therefore, polymerization of the photocurable monomer is promoted in the frame region 1NA, and the amount of remaining monomer becomes equal to or less than that in the display region 1AA, so that display unevenness in the vicinity of the frame region 1NA can be suppressed. The display panel 1 of this embodiment will be described in detail below.
[0037] Fig. 4 is a cross-sectional schematic diagram showing an example of a display panel according to embodiment 1. As shown in Fig. 4, the display panel 1 of this embodiment has a first substrate 100, a polymer-containing layer 200, and a second substrate 300 in this order.
[0038] The first substrate 100 includes, in order toward the polymer-containing layer 200, a first support substrate 110, a source line 101S, an insulating layer 130, and a pixel electrode 140. The second substrate 300 includes, in order toward the polymer-containing layer 200, a second support substrate 310, a light-shielding portion 320, an overcoat layer 321, and a counter electrode 322. The first substrate 100 is also called a TFT substrate. The second substrate 300 is also called a counter substrate.
[0039] In the display region 1AA, the first substrate 100 includes a plurality of gate lines 101G extending parallel to each other and a plurality of source lines 101S extending parallel to each other in a direction intersecting the gate lines with an insulating layer interposed therebetween on a first support substrate 110. The plurality of gate lines 101G and the plurality of source lines 101S are formed in a lattice pattern as a whole so as to partition each pixel.
[0040] At the intersections of each source line 101S and each gate line 101G, TFTs 120 are disposed as switching elements. In each region surrounded by two adjacent source lines 101S and two adjacent gate lines 101G, a pixel electrode 140 is disposed. The pixel electrode 140 is electrically connected to the corresponding source line 101S via a semiconductor layer provided in the TFT 120.
[0041] The display panel 1 further includes a source driver electrically connected to the source lines 101S, a gate driver electrically connected to the gate lines 101G, and a controller. The gate driver sequentially supplies scanning signals to the gate lines under the control of the controller. The source driver supplies data signals to the source lines 101S under the control of the controller at the timing when the TFTs 120 are in a voltage applied state by the scanning signal. A terminal pattern (frame pattern) 120A of the TFTs 120 is provided in a frame region 1NA where the driver is arranged.
[0042] Each pixel electrode 140 is set to a potential according to a data signal supplied through the corresponding TFT 120, and a vertical electric field is generated between the pixel electrode 140 and the counter electrode 322. The liquid crystal component 220 having positive dielectric anisotropy contained in the polymer-containing layer 200 tends to align parallel to the electric field direction, that is, the liquid crystal component 220 having positive dielectric anisotropy is oriented perpendicular to the electrode. In a state where no voltage is applied, in which the liquid crystal component 220 exists in a random direction relative to the polymer network 210, light can be scattered. In addition, when the magnitude of the voltage applied between the pixel electrode 140 and the counter electrode 322 is controlled and the liquid crystal component 220 is aligned parallel to the electric field direction, a transmissive state can be achieved when viewed from the front.
[0043] If the average refractive index of the polymer is np, the refractive index of the liquid crystal in the long axis direction is ne, and the refractive index in the short axis direction is no, then ne >> no ≒ np. When no voltage is applied, there is a refractive index difference between np and the average value of ne and no ((ne + no) / 2), so the light appears "scattered." On the other hand, when a voltage is applied, np ≒ no holds when the panel is viewed from the front (parallel to the electric field direction), so the refractive index difference is small and the light appears "transparent."
[0044] Examples of the first support substrate 110 and the second support substrate 310 include insulating substrates such as glass substrates and plastic substrates. Examples of materials for the glass substrate include glass such as float glass and soda glass. Examples of materials for the plastic substrate include plastics such as polyethylene terephthalate, polybutylene terephthalate, polyethersulfone, polycarbonate, and alicyclic polyolefin.
[0045] Each TFT 120 is a three-terminal switch connected to a corresponding source line 101S and gate line 101G among a plurality of source lines and a plurality of gate lines, and has a gate electrode protruding from the corresponding gate line 101G (part of the gate line), a source electrode protruding from the corresponding source line 101S (part of the source line 101S), a drain electrode connected to a corresponding pixel electrode 140 among a plurality of pixel electrodes 140, and a thin-film semiconductor layer. The source electrode and drain electrode are electrodes provided in the same layer as the source line 101S, and the gate electrode is an electrode provided in the same layer as the gate line 101G.
[0046] The thin-film semiconductor layer of each TFT 120 is composed of, for example, a high-resistance semiconductor layer made of amorphous silicon, polysilicon, or the like, and a low-resistance semiconductor layer made of n+ amorphous silicon, which is amorphous silicon doped with impurities such as phosphorus, or the like. Alternatively, an oxide semiconductor layer such as zinc oxide may be used as the thin-film semiconductor layer.
[0047] The insulating layer 130 is, for example, an inorganic insulating film, an organic insulating film, or a laminate of the organic insulating film and the inorganic insulating film. As the inorganic insulating film, for example, an inorganic film such as silicon nitride (SiNx) or silicon oxide (SiO2), or a laminate of these films can be used. As the organic insulating film, for example, an organic film such as an acrylic resin, a polyimide resin, or a novolac resin, or a laminate of these films can be used. The insulating layer 130 is not colored and is colorless and transparent.
[0048] The overcoat layer 321 has a function of planarizing the surface of the second substrate 300 on the side of the polymer-containing layer 200. The overcoat layer 321 is, for example, an organic insulating film. As the organic insulating film, for example, an organic film such as an acrylic resin, a polyimide resin, or a novolac resin, or a laminate thereof can be used. In this embodiment, an aspect in which the display panel 1 includes the overcoat layer 321 will be described, but the display panel 1 does not necessarily need to include the overcoat layer 321.
[0049] The pixel electrodes 140 are electrodes disposed in each region surrounded by two adjacent source lines 101S and two adjacent gate lines 101G. The pixel electrodes 140 are set to a potential corresponding to a data signal supplied via the corresponding TFT 120. A common signal maintained at a constant value is supplied to the counter electrode 322, and the counter electrode 322 is maintained at a constant potential.
[0050] The polymer-containing layer 200 contains a polymer of a photocurable monomer. The polymer of a photocurable monomer is a polymer obtained by irradiating the photocurable monomer with light to polymerize it. The polymer-containing layer 200 is, for example, a layer obtained by irradiating a composition containing a photocurable monomer with light to polymerize it. The composition may contain a liquid crystal component 220 in addition to the photocurable monomer. In this case, the polymer-containing layer 200 also contains the liquid crystal component 220.
[0051] The polymer-containing layer 200 contains a polymer network 210 constituted by a polymer of the photocurable monomer, and a liquid crystal component 220. The polymer-containing layer 200 of this embodiment is also called a polymer-dispersed liquid crystal layer. In the polymer-containing layer 200, a fibrous matrix of a polymer of the photocurable monomer (a cured product of the photocurable monomer) is aggregated to form a three-dimensionally continuous polymer network 210, and the liquid crystal component 220 exists in the polymer network 210.
[0052] The polymer-containing layer 200, which is a polymer-dispersed liquid crystal layer, is in a scattering state when no voltage is applied, and is in a transparent state when a voltage is applied. By adopting such an embodiment, a display panel 1 that does not require a polarizing plate can be realized. More specifically, it is in a scattering state when no voltage is applied, and when a voltage is applied, the orientation of the liquid crystal component 220 changes to a transparent state. The display panel 1 functions as a see-through panel. In this specification, a voltage-applied state in which a voltage equal to or greater than a threshold is applied between the pixel electrode 140 and the counter electrode 322 is simply referred to as a "voltage-applied state" or "when a voltage is applied," and a voltage-free state in which a voltage less than a threshold is applied between the pixel electrode 140 and the counter electrode 322 (including when no voltage is applied) is simply referred to as a "voltage-free state" or "when no voltage is applied." More specifically, the voltage-free state refers to a 0-level state (V0) in a 256-level display.
[0053] For example, when liquid crystal component 220 is present in polymer network 210, in the absence of applied voltage, liquid crystal component 220 is oriented along polymer network 210. Due to the difference in refractive index between polymer network 210 and liquid crystal component 220, incident light cannot travel in a straight line and is scattered, resulting in a cloudy glass state (scattered state).
[0054] On the other hand, in the voltage applied state, the liquid crystal component 220 having positive dielectric anisotropy aligns its long axis parallel to the electric field direction, so that the liquid crystal component 220 is oriented perpendicular to the electrodes (pixel electrode 140 and counter electrode 322). If the ordinary light refractive index of the liquid crystal component is equal to the refractive index of the polymer, the refractive index difference between the liquid crystal component 220 and the polymer network 210 disappears, resulting in an optically non-interface state. As a result, the incident light travels straight without being scattered, realizing a transparent state.
[0055] The scattering state is a state in which light is scattered. For example, the transmittance of the polymer-dispersed liquid crystal layer in the scattering state may be, for example, 20% or less. The lower limit of the transmittance of the polymer-dispersed liquid crystal layer in the scattering state is, for example, 0 to 1%. In this specification, the transmittance of the polymer-dispersed liquid crystal layer in the scattering state refers to the parallel light transmittance of the polymer-dispersed liquid crystal layer in the scattering state.
[0056] The transmittance of the polymer-dispersed liquid crystal layer in the scattering state can be obtained, for example, as follows. The luminance when a display panel having a polymer-dispersed liquid crystal layer in a no-voltage-applied state is placed on a normal backlight (light source for liquid crystal display devices) having an LED as a light source, and the luminance when nothing is placed on the backlight are measured at a light receiving angle of 2° using a Topcon luminance meter (SR-UL1). The measurement wavelength is the luminosity Y value, and is set to a wavelength of about 550 nm. The transmittance of the polymer-dispersed liquid crystal layer in the scattering state can be obtained by dividing the luminance when a display panel in a no-voltage-applied state is placed on the backlight by the luminance when nothing is placed on the backlight.
[0057] The haze, which indicates the light scattering rate of the polymer-dispersed liquid crystal layer in the scattering state, may be, for example, 80% or more, or 90% or more. The upper limit of the haze, which indicates the light scattering rate of the polymer-dispersed liquid crystal layer in the scattering state, is, for example, 90 to 100%. In this embodiment, the polymer-dispersed liquid crystal layer in the scattering state scatters visible light. Therefore, the polymer-dispersed liquid crystal layer in the scattering state is in the same state as frosted glass. In this specification, the haze is measured by a method conforming to JIS K 7136. The haze can be measured, for example, by a turbidity meter "HazeMeter NDH2000" manufactured by Nippon Denshoku Industries Co., Ltd., using a halogen lamp as a light source.
[0058] The transparent state is a state having transparency to light. For example, the transmittance of the polymer-dispersed liquid crystal layer in the transparent state may be 25% or more, or may be 30% or more. If there is no influence of wiring, the transmittance is, for example, 60% or more. The upper limit of the transmittance of the polymer-dispersed liquid crystal layer in the transparent state is, for example, 100%. In this embodiment, the polymer-dispersed liquid crystal layer in the transparent state is transparent to visible light. In this specification, the transmittance of the polymer-dispersed liquid crystal layer in the transparent state refers to the parallel light transmittance of the polymer-dispersed liquid crystal layer in the transparent state.
[0059] The transmittance of the polymer-dispersed liquid crystal layer in a transparent state can be obtained, for example, as follows. The luminance when a display panel having a polymer-dispersed liquid crystal layer in a voltage-applied state is placed on a normal backlight (light source for liquid crystal display devices) having an LED as a light source, and the luminance when nothing is placed on the backlight are measured at a light receiving angle of 2° using a Topcon luminance meter (SR-UL1). The measurement wavelength is the visual sensitivity Y value, and the wavelength is about 550 nm. The transmittance of the polymer-dispersed liquid crystal layer in a transparent state can be obtained by dividing the luminance when a display panel in a voltage-applied state is placed on the backlight by the luminance when nothing is placed on the backlight.
[0060] In this way, the display panel 1 adjusts the amount of light passing through the display panel 1 by changing the refractive index difference ne and the refractive index difference no between the polymer network 210 and the liquid crystal component 220 in the polymer dispersed liquid crystal layer, and therefore does not require a polarizing plate which is required in general liquid crystal display panels.
[0061] The photocurable monomer is compatible with the liquid crystal component 220 at room temperature, and when it is cured by ultraviolet irradiation to form a polymer, it phase-separates from the liquid crystal component 220. The wavelength of the light used for polymerization of the photocurable monomer is preferably 315 nm or more and 400 nm or less, more preferably 340 nm or more and 380 nm or less, and even more preferably 350 nm or more and 380 nm or less.
[0062] The photocurable monomer preferably has a reactive group represented by, for example, any of the following formulas (M1) to (M21).
[0063] [ka]
[0064] [ka]
[0065] [ka]
[0066] [ka]
[0067] [ka]
[0068] Specific examples of photocurable monomers having reactive groups represented by the above formulas (M1) to (M21) include acrylic monomers having reactive groups represented by (M1) to (M3), allyl ether monomers having a reactive group represented by (M4), such as diallyl ether, bisphenol A diallyl ether, bisphenol A diallyl ether, and polyallyl ether of novolac resin, epoxy compounds having reactive groups represented by (M7) to (M10), such as bisphenol A type epoxy resin, bisphenol F type epoxy resin, and novolac type epoxy resin, and (M11). Preferred are 3,4-epoxycyclohexylmethyl methacrylate having a reactive group represented by (M12) or (M13), oxetane compounds having a reactive group represented by (M14), such as ethyl-3-hydroxymethyloxetane (OXA) or 3-ethyl-3-chloromethyloxetane (OXC), and maleimide compounds having a reactive group represented by (M14), such as maleimide ethyl acetate or polyalkylene ether bismaleimide. In this embodiment, however, acrylic monomers having a reactive group represented by (M1) or (M2) are particularly preferred in terms of the effect of improving adhesion.
[0069] Specific examples of the acrylic monomer include trimethylolpropane tri(meth)acrylate, EO-modified trimethylolpropane tri(meth)acrylate, isocyanuric acid EO-modified tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, ditrimethylolpropane tetra(meth)acrylate, dipentaerythritol penta(meth)acrylate, dipentaerythritol hexa(meth)acrylate, and other examples include polyfunctional urethane oligomers, polyester acrylates, and epoxy acrylates.
[0070] Furthermore, among the photocurable monomers having the above-mentioned reactive groups, it is more preferable to contain a compound having three or more reactive groups, and even more preferable to contain a compound having four or more reactive groups, in terms of the effect of improving adhesion and excellent heat cycle resistance.
[0071] The photocurable monomer may be used alone or in combination of two or more. Furthermore, the photocurable monomer is preferably one having a hydrophilic group such as a hydroxyl group in the molecular structure, since this has a significant effect of improving adhesion and heat cycle resistance, and is particularly preferably used as a mixture containing four or more reactive compounds, the mixture containing 40 to 80 mass % of compounds having a hydrophilic group.
[0072] A polymerization initiator may be added as necessary. As the thermal polymerization initiator, a known and commonly used one can be used, for example, methyl acetoacetate peroxide, cumene hydroperoxide, benzoyl peroxide, bis(4-t-butylcyclohexyl)peroxydicarbonate, t-butyl peroxybenzoate, methyl ethyl ketone peroxide, 1,1-bis(t-hexylperoxy)3,3,5-trimethylcyclohexane, p-pentahydroperoxide, t-butyl hydroperoxide, dicumyl peroxide, isobutyl peroxide, di(3-methyl-3-methoxybutyl)peroxydicarbonate, Organic peroxides such as 1,1-bis(t-butylperoxy)cyclohexane, azonitrile compounds such as 2,2'-azobisisobutyronitrile and 2,2'-azobis(2,4-dimethylvaleronitrile), azoamide compounds such as 2,2'-azobis(2-methyl-N-phenylpropion-amidine) dihydrochloride, azoamide compounds such as 2,2'azobis{2-methyl-N-[1,1-bis(hydroxymethyl)-2-hydroxyethyl]propionamide}, and alkylazo compounds such as 2,2'azobis(2,4,4-trimethylpentane) can be used.Specific examples include "V-40" and "VF-096" manufactured by Wako Pure Chemical Industries, Ltd., and "Perhexyl D" and "Perhexyl I" manufactured by Nippon Oil & Fats Corporation (now NOF Corporation). Examples of photopolymerization initiators include "Irgacure 651", "Irgacure 184", "Darocure 1173", "Irgacure 907", "Irgacure 127", "Irgacure 369", "Irgacure 379", "Irgacure 819", "Irgacure 2959", "Irgacure 1800", "Irgacure 250", "Irgacure 754", "Irgacure 784", "Irgacure OXE01", "Irgacure OXE02", "Irgacure OXE04", "Lucirin TPO", "Darocure 1173", and "Darocure MBF" manufactured by BASF, and "Esacure 1001M", "Esacure KIP150", "Speedcure BEM", "Speedcure BMS", "Speedcure MBP", "Speedcure PBZ", "Speedcure ITX", and "Speedcure 2959", "Irgacure 1800", "Irgacure 250", "Irgacure 754", "Irgacure 784", "Irgacure OXE01", "Irgacure OXE02", "Irgacure OXE04", "Lucirin TPO", "Darocure 1173", and "Darocure MBF" manufactured by LAMBSON. DETX, Speedcure EBD, Speedcure MBB, Speedcure BP, Nippon Kayaku's Kayacure DMBI, Nippon SiberHegner (now DKSH)'s TAZ-A, ADEKA's ADEKA Optomer SP-152, ADEKA Optomer SP-170, ADEKA Optomer N-1414, ADEKA Optomer N-1606, ADEKA Optomer N-171 7," "ADEKA OPTOMER N-1919," UCC's "CYRACURE UVI-6990," "CYRACURE UVI-6974," and "CYRACURE UVI-6992," Asahi Denka Kogyo's "ADEKA OPTOMER SP-150, SP-152, SP-170, and SP-172," Rhodia's "PHOTOINITIATOR2074," BASF's "IRGACURE 250," GE Silicones' "UV-9380C," and Midori Kagaku's "DTS-102." In addition, when cationic polymerization is performed, examples of the usable compounds include sulfonium salts such as UVACURE1590 (manufactured by Daicel-Cytec) and CPI-110P (manufactured by San-Apro), and iodonium salts such as IRGACURE250 (manufactured by Chiba Specialty Chemicals), WPI-113 (manufactured by Wako Pure Chemical Industries, Ltd.), and Rp-2074 (manufactured by Rhodia Japan).
[0073] In the case of electron beam curing, a polymerization initiator may be used or not.
[0074] The amount of these polymerization initiators to be used is preferably 0.1 to 10 parts by mass, particularly preferably 0.5 to 5 parts by mass, based on the photocurable monomer. These can be used alone or in combination of two or more. If necessary, a sensitizer or the like can also be used.
[0075] The liquid crystal component 220 may not have a polymerizable group such as an acrylate, a methacrylate, a maleimide, an N-phenylmaleimide, or a siloxane.
[0076] In this embodiment, the liquid crystal component 220 may have a dielectric anisotropy (Δε) defined by the following formula (L) having either a positive value or a negative value. Δε = (dielectric constant of the liquid crystal component in the long axis direction) - (dielectric constant of the liquid crystal component in the short axis direction) (L)
[0077] Liquid crystal components (liquid crystal molecules) with positive dielectric anisotropy are oriented parallel to the electric field, while liquid crystal components with negative dielectric anisotropy are oriented perpendicular to the electric field. Liquid crystal components with positive dielectric anisotropy are also called positive type liquid crystals, and liquid crystal components with negative dielectric anisotropy are also called negative type liquid crystals. The long axis direction of the liquid crystal component is the direction of the slow axis. The direction of the long axis of the liquid crystal component when no voltage is applied is also called the initial orientation direction of the liquid crystal component.
[0078] As the liquid crystal component 220, for example, a tolan-based liquid crystal material (a liquid crystal material having -C≡C- (carbon-carbon triple bond) as a linking group) can be used.
[0079] It is preferable that the refractive index anisotropy Δn of the liquid crystal component 220 is 0.18 or more and 0.24 or less, the dielectric anisotropy Δε of the liquid crystal component 220 is 15 or more and 25 or less, and the rotational viscosity γ1 of the liquid crystal component 220 is 100 mPa·s or more and 300 mPa·s or less. By adopting such an embodiment, it is possible to achieve both strong scattering and low voltage driving, and to realize a response speed equivalent to that of a normal liquid crystal display device that does not contain a polymer network. Such an effect can be realized by having the refractive index anisotropy Δn, the dielectric anisotropy Δε, and the rotational viscosity γ1 of the liquid crystal component 220 all within the above ranges.
[0080] A specific example of the tolan-based liquid crystal material is a liquid crystal material having a structure represented by the following general formula (L1).
[0081] [ka] (In the above formula, Q1 and Q2 each independently represent an aromatic ring group, X represents a fluorine group or a cyano group, and n1 and n2 each independently represent 0 or 1.)
[0082] In the above general formula (L1), n1 and n2 cannot simultaneously be 0. That is, the sum of n1 and n2 is 1 or 2.
[0083] The aromatic ring group in the above general formula (L1) may have a substituent.
[0084] In the above general formula (L1), Q1 and Q2 each preferably independently represent any one of the structures of the following general formulae (L2-1) to (L2-7).
[0085] [ka]
[0086] Specific examples of the liquid crystal material having the structure represented by the above general formula (L1) include the following structures.
[0087] [ka]
[0088] The weight ratio of the liquid crystal component 220 to the polymer network 210 is preferably 7:3 to 9:1. That is, it is preferable that the weight ratio of the liquid crystal component 220 is 7 or more and 9 or less, and when the weight ratio of the liquid crystal component 220 is 7 or more, the weight ratio of the polymer network 210 is 3 or less, and when the weight ratio of the liquid crystal component 220 is 9 or less, the weight ratio of the polymer network 210 is 1 or more. By adopting such an embodiment, it is possible to effectively achieve both strong scattering and low voltage driving. When the weight ratio of the polymer network 210 exceeds 10, strong scattering is obtained but the driving voltage becomes high, and when the weight ratio of the polymer network 210 is less than 3, the driving voltage is suppressed but strong scattering may not be obtained. The degree of scattering and the driving voltage can be effectively controlled by adjusting the weight ratio of the liquid crystal component 220 to the polymer network 210, as well as the network size and the components forming the network.
[0089] In the second substrate 300, the light shielding portion 320 that blocks the light of the wavelength used for polymerization of the photocurable monomer is not disposed in the frame region 1NA. By adopting such an embodiment, the light of the wavelength used for polymerization of the photocurable monomer can be transmitted through the entire frame region 1NA of the second substrate 300, the polymerization of the photocurable monomer is promoted in the frame region 1NA, and the amount of remaining monomer (unreacted monomer) in the polymer-containing layer 200 can be suppressed. As a result, display unevenness in the vicinity of the frame region 1NA can be suppressed.
[0090] The fact that the light shielding portion 320 that blocks the light of the wavelength used for polymerization of the photocurable monomer is not disposed in the frame region 1NA means that the light shielding portion 320 is not disposed substantially in the entire frame region 1NA.
[0091] The second substrate 300 includes a light-shielding portion 320 that overlaps the display region 1AA but does not overlap the frame region 1NA. The light-shielding portion 320 has a function of blocking light of a wavelength used for polymerization of the photocurable monomer. The light-shielding portion 320 may have optical characteristics, for example, an OD value of 3 or more, which is an index of light absorbance. The OD value of the light-shielding portion 320 is preferably 3.5 or more, and more preferably 4 or more. The upper limit of the OD value of the light-shielding portion 320 is not particularly limited, but is, for example, 6 or less.
[0092] The OD value (OD(λ)) at a measurement wavelength λ can be calculated by the following formula. The measurement wavelength λ is, for example, the wavelength used for polymerization of a photocurable monomer. The OD value can be measured by the Macbeth densitometry using a TD-904 manufactured by Kollmorgen. OD(λ)=Log10[T(λ) / I(λ)]=Log10T(λ)-Log10I(λ) where λ is the measurement wavelength, T(λ) is the amount of transmitted light at the measurement wavelength, and I(λ) is the amount of incident light at the measurement wavelength.
[0093] The light shielding portion 320 is disposed between the second support substrate 310 and the polymer-containing layer 200. The light shielding portion 320 is preferably, for example, a black matrix layer. The black matrix layer is preferably made of a resin material containing a black pigment or a metal material having light shielding properties. The black matrix layer is formed, for example, by a photolithography method in which a photosensitive resin containing a black pigment is applied to form a film, and then exposed to light and developed.
[0094] The first substrate 100 includes a plurality of gate lines extending parallel to each other, and a plurality of source lines 101S extending parallel to each other in a direction intersecting the plurality of gate lines via an insulating layer, and a black matrix layer is provided in the display region 1AA at a position overlapping the plurality of gate lines and the plurality of source lines 101S, and it is preferable that the black matrix layer as the light shielding portion 320 is not disposed in the frame region 1NA. By adopting such an embodiment, it is possible to suppress reflection in the display region 1AA while suppressing display unevenness in the vicinity of the frame region 1NA.
[0095] The second substrate 300 may include, in the frame region 1NA, a colored portion 321a that transmits light of a wavelength used for polymerization of the photocurable monomer. By adopting such an embodiment, the colored portion 321a can function as a frame of the display panel 1. The colored portion 321a is obtained, for example, by coloring the frame region 1NA of the overcoat layer 321.
[0096] The colored portion 321a is disposed between the second support substrate 310 and the polymer-containing layer 200. The colored portion 321a may transmit light having a wavelength other than the wavelength used for polymerization of the photocurable monomer. For example, when the photocurable monomer is polymerized with light having a wavelength of 400 nm, the colored portion 321a may transmit light having a wavelength other than 400 nm in addition to light having a wavelength of 400 nm.
[0097] It is also preferable that the overcoat layer 321 does not have the colored portion 321a. By adopting such an embodiment, the region can be made to have the same state as the transmissive portion of the display region 1AA, and problems such as display defects can be suppressed and productivity can be improved.
[0098] The display panel 1 preferably further includes an ink portion 500 in at least one of the frame region 1NA on the opposite side of the polymer-containing layer 200 of the first substrate 100 and the frame region 1NA on the opposite side of the polymer-containing layer 200 of the second substrate 300. This embodiment can prevent the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA from being affected by exposure to light. Also, frame reflection of the display panel 1 can be suppressed. The ink portion 500 functions as a frame of the display panel 1.
[0099] In this embodiment, as shown in FIG. 4, a mode in which a second substrate side ink portion 520 is disposed in a frame region 1NA on the opposite side of the second substrate 300 from the polymer-containing layer 200 will be described.
[0100] The ink section 500 may or may not transmit light of a wavelength used for polymerization of the photocurable monomer, but it is preferable that the ink section 500 does not transmit light of a wavelength used for polymerization of the photocurable monomer. By adopting such an embodiment, decomposition of the photocurable monomer can be suppressed. The ink section 500 is, for example, a member colored with at least one of a pigment and a dye. The second substrate side ink section 520 is obtained, for example, by applying additive color printing to a frame region 1NA of the second substrate side film 620 described later.
[0101] The display panel 1 may include a second substrate-side film 620 on the side of the second substrate 300 opposite to the polymer-containing layer 200. The second substrate-side film 620 is, for example, a protective film such as a triacetylcellulose (TAC) film. Also, by using a UV-absorbing adhesive as the adhesive, a PET (Polyethylene terephthalate) film can be used as the second substrate-side film 620. The thickness of the second substrate-side film 620 is not particularly limited, but is, for example, 50 μm or more and 300 μm or less.
[0102] The display panel 1 includes a second substrate side film 620 located on the opposite side of the second substrate 300 to the polymer-containing layer 200, and the ink section 500 preferably includes a second substrate side ink section 520 located at least one of between the second substrate side film 620 and the second substrate 300 and on the opposite side of the second substrate 300 of the second substrate side film 620. By adopting such an embodiment, it is possible to suppress the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA from being affected by exposure to light from the second substrate 300 side. In addition, it is possible to suppress frame reflection on the second substrate 300 side of the display panel 1.
[0103] Fig. 5 is a schematic cross-sectional view illustrating a case where the second substrate ink section is located on the opposite side of the second substrate film from the second substrate in the display panel according to embodiment 1. Fig. 6 is a schematic cross-sectional view illustrating a case where the second substrate ink section is provided between the second substrate film and the second substrate in the display panel according to embodiment 1.
[0104] The second substrate side ink section 520 is preferably located between the second substrate side film 620 and the second substrate 300. By adopting such an embodiment, the range of the terminal pattern 120A visible to the observer can be narrowed, and the display characteristics can be improved, compared to the case where the second substrate side ink section 520 is located on the opposite side of the second substrate side film 620 to the second substrate 300, as shown in Fig. 5 .
[0105] 4, 5, and 6, the greater the distance 500D between the ink portion 500 and the pixel electrode 140, the larger the area outside the pixel (frame region 1NA) that is visible when observed from an oblique angle. Therefore, it is preferable to provide the second substrate-side ink portion 520 by additive color printing on the second adhesive layer 720 side of the second substrate-side film 620.
[0106] The second substrate side film 620 is preferably a UV cut film 621. By adopting such an embodiment, it is possible to prevent a small amount of remaining monomer present under the pixel wiring in the display area 1AA from being exposed to ultraviolet light contained in sunlight or fluorescent lamps, which can cause unevenness, and thus to prevent a decrease in display quality. Examples of UV cut films include protective films such as TAC films, the base material of which absorbs ultraviolet rays.
[0107] The display panel 1 may include a first substrate-side film 610 on the side of the first substrate 100 opposite to the polymer-containing layer 200. The first substrate-side film 610 is, for example, a protective film such as a triacetylcellulose (TAC) film. Also, by using a UV-absorbing adhesive as the adhesive, a PET (Polyethylene terephthalate) film can be used as the first substrate-side film 610. The thickness of the first substrate-side film 610 is not particularly limited, but is, for example, 50 μm or more and 300 μm or less.
[0108] The first substrate side film 610 is preferably a UV cut film 611. By adopting such an embodiment, it is possible to prevent a small amount of remaining monomer present under the pixel wiring in the display area 1AA from being exposed to ultraviolet light contained in sunlight or fluorescent lamps, which can cause unevenness, and thus to prevent a decrease in display quality. Examples of UV cut films include protective films such as TAC films, the base material of which absorbs ultraviolet rays.
[0109] The display panel 1 includes a first adhesive layer 710 between the first substrate 100 and the first substrate side film 610. The thickness of the first adhesive layer 710 is not particularly limited, but is, for example, 15 μm or more and 50 μm or less, and preferably 15 μm or more and 25 μm or less.
[0110] Similarly, the display panel 1 includes a second adhesive layer 720 between the second substrate 300 and the second substrate side film 620. The thickness of the second adhesive layer 720 is not particularly limited, but is, for example, 15 μm or more and 50 μm or less, and preferably 15 μm or more and 25 μm or less.
[0111] The adhesive layer is a layer that bonds the surfaces of adjacent members and integrates them with sufficient adhesive strength and adhesion time for practical use. Examples of materials that form the adhesive layer include acrylic, silicone, and urethane resin materials.
[0112] The first adhesive layer 710 preferably contains a UV absorber. This embodiment can prevent a small amount of remaining monomer present under the pixel wiring in the display area 1AA from being exposed to ultraviolet light contained in sunlight or fluorescent lamps, which can cause unevenness.
[0113] Similarly, the second adhesive layer 720 preferably contains a UV absorber.
[0114] The UV absorber contains, for example, at least one of a benzotriazole-based UV absorber, a triazine-based UV absorber, and a benzophenone-based UV absorber.
[0115] As the benzotriazole-based UV absorber, known compounds can be used. Specifically, octyl 3-[3-tert-butyl-4-hydroxy-5-(5-chloro-2H-benzotriazol-2-yl)phenyl]propionate, 2-ethylhexyl 3-(3-tert-butyl-4-hydroxy-5-(5-chloro-2H-benzotriazol-2-yl)phenyl)propionate, [3-[3-(2H-benzotriazol-2-yl)-5-(1,1-methylethyl)-4-hydroxyphenyl]-1-oxopropyl]-w-[3-[3-(2H-benzotriazol-2-yl)-5-(1,1-dimethylethyl)-4-hydroxyphenyl]-1-oxopropoxy]poly(oxy-1,2-ethanediyl), (3-(3-(2H-benzotriazol-2-yl)-5-(1,1-dimethylethyl)-4-hydroxyphenyl]-1-oxopropoxy)poly(oxy-1,2-ethanediyl), Ethyl)-4-hydroxyphenyl)-1-oxopropyl)-hydroxypoly(oxo-1,2-ethanediyl), 2-(3-tert-butyl-2-hydroxy-5-methylphenyl)-5-chloro-2H-benzotriazole, 2-(2H-benzotriazol-2-yl)-4,6-ditert-pentylphenol, 3-(2H-benzotriazolyl)-5-(1,1-dimethylethyl)-4-hydroxy-benzylpropionic acid octyl ester, 2-(2H-benzotriazol-2-yl)-4,6-bis(1-methyl-1-phenylethyl)phenol, 2-(2H-benzotriazol-2-yl)-6-(1-methyl-1-phenylethyl)-4-(1,1,3,3-tetramethylbutyl)phenol and the like are preferred.
[0116] As the triazine-based UV absorber, known compounds can be used. Specifically, 2-(4,6-dimethyl-1,3,5-triazin-2-yl)-5-((hexyl)oxy)-phenol, 2-(4-(2-hydroxy-3-tridecyloxypropyl)oxy)-2-hydroxyphenyl)-4,6-bis(2,4-dimethylphenyl)-1,3,5-triazine, 2-(4-(2-hydroxy-3-didecyloxypropyl)oxy)-2-hydroxyphenyl)-4,6-bis(2,4-dimethylphenyl)-1,3,5-triazine, 2-(2- Hydroxy-4-(3-(2-ethylhexyl-1-oxy)-2-hydroxypropyloxy)phenyl)-4,6-bis(2,4-dimethylphenyl)-1,3,5-triazine, 2,2'-[6-(2,4-dibutoxyphenyl)-1,3,5-triazine-2,4-diyl]bis(5-butoxyphenol), 6-methylheptyl 2-{4-[4,6-di(4-biphenylyl)-1,3,5-triazine-2-yl]-3-hydroxyphenoxy}propanoate, and the like.
[0117] As the benzophenone-based UV absorber, known compounds can be used, specifically, 2-hydroxy-4-n-octyloxybenzophenone, 2-hydroxy-4-methoxybenzophenone, etc.
[0118] FIG. 7 is a schematic diagram showing a manufacturing method of a display panel according to the first embodiment. The manufacturing method of the display panel 1 of this embodiment includes an exposure step of irradiating light L from the second substrate 300 side to a panel precursor 10 filled with a composition containing a photocurable monomer between a first substrate 100 having a TFT 120 as a switching element and a second substrate 300 having no light shielding portion 320 in a frame region 1NA provided around a display region 1AA for displaying an image. By adopting such an embodiment, polymerization of the photocurable monomer is promoted in the frame region 1NA of the panel precursor 10, and the amount of remaining monomer (unreacted monomer) in the polymer-containing layer 200 formed by polymerization of the photocurable monomer can be suppressed. As a result, display unevenness in the vicinity of the frame region 1NA can be suppressed. In this way, since the remaining monomer can be suppressed in this embodiment, it is not necessary to increase the exposure amount too much to suppress the remaining monomer, and a good display panel 1 can be obtained. This also suppresses burn-in.
[0119] 7, the first substrate 100 includes a plurality of gate lines 101G extending parallel to each other, a plurality of source lines 101S extending parallel to each other in a direction intersecting the plurality of gate lines 101G via an insulating layer, and a TFT 120, and includes a terminal pattern 120A of the TFT 120 in a frame region 1NA. On the other hand, the second substrate 300 does not include a light-shielding portion 320 in the frame region 1NA. The second substrate 300 includes a light-shielding portion 320 in a display region 1AA.
[0120] The panel precursor 10 can be manufactured, for example, by applying a sealant to the first substrate 100 or the second substrate 300, forming the composition in the area surrounded by the sealant, and then bonding the first substrate 100 and the second substrate 300 together with the sealant. Note that the composition can be filled into the area surrounded by the sealant after the first substrate 100 and the second substrate 300 are bonded together. Specifically, a vacuum injection method can be used in which an injection port is provided in the seal drawing pattern and liquid crystal is injected in a vacuum chamber.
[0121] The panel precursor 10 is exposed to light to polymerize the photocurable monomer to form a polymer-containing layer 200, thereby realizing a display panel 1 which sequentially comprises a first substrate 100 having a TFT 120, a polymer-containing layer 200, and a second substrate 300.
[0122] 7, the manufacturing method of the display panel 1 of this embodiment may include a bonding step of bonding the second substrate film 620, in which the second substrate ink part 520 is arranged in the frame region 1NA, to the side of the second substrate 300 opposite to the first substrate 100, after the exposure step. By adopting such an embodiment, it is possible to suppress the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA from being affected by exposure to light from the second substrate 300 side. In addition, it is possible to suppress frame reflection on the second substrate 300 side of the display panel 1.
[0123] When performing panel exposure using the conventional manufacturing method, exposure is performed from the TFT substrate side, which has a smaller light-shielding area than the substrate with the black matrix, in order to suppress residual monomers. However, the shadow of the light-shielding member of the TFT substrate is not sufficiently exposed, which results in residual monomers and causes display unevenness.
[0124] On the other hand, in this embodiment, the second substrate 300 that does not have a light shielding portion 320 such as a black matrix in the frame region 1NA is used, and exposure is performed from the second substrate 300 side, thereby suppressing the unreacted monomer from remaining in the frame region 1NA. In the display panel produced by this method, if left as is, the terminal pattern 120A of the TFT 120 in the frame region 1NA may be exposed to light, and the electrical characteristics may be affected. Therefore, by additively printing the frame region of a film (e.g., a UV-cut film) that is attached to the panel during mounting, the electrical characteristics can be suppressed from being affected. Thus, in this embodiment, after producing a panel composed of the first substrate 100, the polymer-containing layer 200, and the second substrate 300, a frame can be provided on the display panel 1 by attaching a UV-cut film with additive printing on the frame region 1NA.
[0125] (Modification 1 of the first embodiment) In the above embodiment 1, an aspect has been described in which the ink section 500 is arranged in the frame region 1NA on the opposite side of the second substrate 300 from the polymer-containing layer 200, but the ink section 500 may be arranged on the first substrate 100 side in addition to the second substrate 300 side.
[0126] 8 is a cross-sectional schematic diagram of a display panel according to Modification 1 of the embodiment 1. As shown in FIG. 8, the display panel 1 of this modification includes a first substrate side film 610 located on the side opposite to the polymer-containing layer 200 of the first substrate 100, and the ink part 500 includes a first substrate side ink part 510 located at least one of between the first substrate side film 610 and the first substrate 100 and on the side opposite to the first substrate 100 of the first substrate side film 610. By adopting such an embodiment, it is possible to suppress the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA from being affected by exposure to light from the first substrate 100 side. In addition, it is possible to suppress frame reflection on the first substrate 100 side of the display panel 1.
[0127] The first substrate side ink portion 510 is obtained by, for example, applying additive color printing to the frame region 1NA of the first substrate side film 610.
[0128] The first substrate side ink section 510 is preferably located between the first substrate side film 610 and the first substrate 100. By adopting such an embodiment, as in the case of the second substrate side ink section 520, the range of the terminal pattern 120A visible to the observer can be narrowed compared to the case where the first substrate side ink section 510 is located on the opposite side of the first substrate side film 610 to the first substrate 100, and the display characteristics can be improved.
[0129] Fig. 9 is a cross-sectional view illustrating frame reflection of the display panel according to embodiment 1. Fig. 10 is a cross-sectional view illustrating frame reflection of the display panel according to modification 1 of embodiment 1. Fig. 11 is a table comparing frame reflection of the display panel according to embodiment 1 and the display panel according to modification 1 of embodiment 1.
[0130] When the polymer-containing layer 200 is a polymer-dispersed liquid crystal layer, the display panel 1 functions as a see-through panel that can be viewed from both sides. A display panel with a backlight cannot be viewed from the TFT substrate side, but a see-through display that does not have a backlight and can be viewed from both sides can be viewed from the TFT substrate side.
[0131] As shown in Fig. 9, the first substrate side film 610 in the above-mentioned embodiment 1 is a UV cut film 611 having no ink portion, and the second substrate side film 620 is a UV cut film 621 having the second substrate side ink portion 520 in the frame region 1NA. As shown in Fig. 9 and Fig. 11, in the display panel 1 of embodiment 1, a UV cut film with frame additive color printing is attached to the second substrate 300 side, thereby suppressing frame reflection on the second substrate 300 side, which is the opposing substrate. However, since frame additive color printing is not applied to the first substrate 100 side, which is the TFT substrate, metal reflection of the frame may be noticeable.
[0132] On the other hand, as shown in Fig. 10, the first substrate side film 610 in this modification is a UV cut film 611 having the first substrate side ink portion 510 in the frame region 1NA, and the second substrate side film 620 is a UV cut film 621 having the second substrate side ink portion 520 in the frame region 1NA. As shown in Fig. 10 and Fig. 11, in the display panel 1 of this modification, by bonding the UV cut film 611 with frame-added color printing to the first substrate 100 side as well as the second substrate 300, frame reflection on the first substrate 100 side and the second substrate 300 side can be suppressed, and a display panel with the same appearance from both the first substrate 100 side and the second substrate 300 side can be realized.
[0133] In this way, in the display panel 1 of the first embodiment, when viewed from the first substrate 100 side, the display quality is likely to deteriorate due to metal reflection, and the reflection is particularly noticeable in the frame region 1NA, which has a large wiring area. However, as in this modification, by arranging the ink portion 500 in the frame region 1NA on the first substrate 100 side as well as on the second substrate 300 side, it is possible to reduce the metal reflection in the frame region 1NA and improve the display quality.
[0134] The manufacturing method of the display panel 1 of this modified example may further include, after the exposure step, a bonding step of bonding the first substrate film 610, in which the first substrate ink part 510 is arranged in the frame region 1NA, to the side of the first substrate 100 opposite to the second substrate 300. By adopting such an embodiment, it is possible to suppress the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA from being affected by exposure to light from the first substrate 100 side. Also, it is possible to suppress frame reflection on the first substrate 100 side of the display panel 1.
[0135] (Modification 2 of the first embodiment) Fig. 12 is a plan view schematic of a first substrate side film included in a display panel according to Modification 1 of Embodiment 1. Fig. 13 is a plan view schematic of a first substrate side film included in a display panel according to Modification 2 of Embodiment 1.
[0136] As shown in FIG. 12, in the above-mentioned modified example 1, additive color printing is applied only to the frame region 1NA of the first substrate side film 610. That is, the first substrate side ink section 510 is provided only in the frame region 1NA. On the other hand, in this modified example, as shown in FIG. 13, additive color printing is applied not only to the frame region 1NA of the first substrate side film 610 but also to the wiring positions in the display region 1AA. That is, the first substrate side ink section 510 is provided in the display region 1AA in addition to the frame region 1NA. Specifically, the first substrate side ink section 510 overlaps with the source line 101S and the gate line in the display region 1AA.
[0137] Here, the first substrate 100, which is a TFT substrate, has metal wiring, and therefore has a higher reflectance than the second substrate 300, which is an opposing substrate, and visibility may be reduced due to the influence of external light. In the above-mentioned modification 1, as shown in Fig. 12, the first substrate side film 610, which has additive color printing applied only to the frame region 1NA, is bonded, so that reflection in the frame region 1NA is suppressed, but it is difficult to reduce reflection in the display region 1AA.
[0138] On the other hand, in this modified example, as shown in FIG. 13, a first substrate side film 610 is bonded which is additively printed to match the pixel wiring not only in the frame region 1NA but also in the display region 1AA, so that it is possible to suppress reflection in not only the frame region 1NA but also the display region 1AA, thereby improving visibility.
[0139] (Modification 3 of embodiment 1) In the above embodiment 1 and variants 1 and 2, the polymer-containing layer 200 contains a polymer network 210 composed of a polymer of a photocurable monomer and a liquid crystal component 220. In the present variant, however, the polymer-containing layer 200 contains a pair of polymer layers located on the surfaces of the first substrate 100 and the second substrate 300, and a liquid crystal component located between the pair of polymer layers.
[0140] Fig. 14 is a cross-sectional schematic diagram of a liquid crystal display device including a display panel and a backlight according to Modification 3 of Embodiment 1. The polymer-containing layer 200 in the above-mentioned Embodiment 1 and Modifications 1 and 2 is a polymer-dispersed liquid crystal layer in which a liquid crystal component 220 is phase-separated in a polymer network 210, but the polymer-containing layer 200 in this modification, as shown in Fig. 14, is made of a polymer of the above-mentioned photocurable monomer, and contains a pair of polymer layers 230 located on the surface on the first substrate 100 side and the surface on the second substrate 300 side, and a liquid crystal component 220 located between the pair of polymer layers 230.
[0141] The polymer layer 230 is a layer that controls the alignment of the liquid crystal component 220, and is also called an alignment sustaining layer (PSA: Polymer Sustained Alignment). The polymer layer 230 can be formed, for example, by sealing a liquid crystal composition, which is a mixture of a liquid crystal material and a polymerizable component such as a monomer or an oligomer, between the array substrate and the opposing substrate, and polymerizing the monomer or the like by irradiating heat or light (for example, ultraviolet light). In this modification, the weight ratio of the liquid crystal component 220 to the polymer network 210 is preferably liquid crystal component:polymer network=99.0:1.0 to 99.9:0.1. By adopting such an embodiment, the polymer layer 230 effectively functions as an alignment sustaining layer.
[0142] As shown in FIG. 14, the second substrate 300 of this modification includes a color filter layer 330. The second substrate 300 including the color filter layer 330 is also called a color filter substrate. The color filter layer 330 includes a red color filter 330R, a green color filter 330G, and a blue color filter 330B, and each pixel includes three pixels in a stripe pattern: a pixel including the red color filter 330R, a pixel including the green color filter 330G, and a pixel including the blue color filter 330B. The red color filter, the green color filter, and the blue color filter are made of, for example, a transparent resin containing a pigment. Usually, a combination of a red color filter, a green color filter, and a blue color filter is arranged in every pixel, and a desired color is obtained in each pixel by mixing the colors while controlling the amount of color light transmitted through the red color filter, the green color filter, and the blue color filter.
[0143] The first substrate side film 610 of this modification is a first polarizer 612. The second substrate side film 620 is a second polarizer 622. The first polarizer 612 and the second polarizer 622 (hereinafter simply referred to as polarizers) are both absorptive polarizers, and are arranged in a crossed Nicol configuration with their absorption axes perpendicular to each other. As the polarizer, for example, a polarizer (absorptive polarizer) obtained by dyeing and adsorbing an anisotropic material such as an iodine complex (or dye) on a polyvinyl alcohol (PVA) film and then stretching and aligning the same can be used. In general, in order to ensure mechanical strength and resistance to moist heat, a polyvinyl alcohol film is used in practical use with protective films such as triacetyl cellulose films laminated on both sides of the film. In this specification, the term "polarizer" refers to a linear polarizer (absorptive polarizer) and is distinguished from a circular polarizing plate.
[0144] The liquid crystal display device 2 shown in FIG. 14 includes a display panel 1 and a backlight 800 arranged on the rear side of the display panel 1. As the backlight 800, a backlight that is usually used in the field of liquid crystal display devices can be used. The backlight 800 is not particularly limited as long as it emits light including visible light, and may be a backlight that emits light including only visible light, or a backlight that emits light including both visible light and ultraviolet light. To enable color display by the liquid crystal display device 2, a backlight that emits white light is preferably used.
[0145] The backlight 800 is disposed on the rear side of the display panel 1, and may be of a direct type or an edge light type, as long as the light generated by the backlight 800 is transmitted through the polymer-containing layer 200 of the display panel 1 and emitted to the observation surface side. The type of light source of the backlight 800 is not particularly limited, and examples thereof include light-emitting diodes (LEDs) and cold cathode fluorescent lamps (CCFLs). The amount of light emitted by the backlight 800 that is transmitted through the display panel 1 is controlled by the voltage applied to the polymer-containing layer 200. In this specification, the term "visible light" refers to light (electromagnetic waves) having a wavelength of 380 nm or more and less than 800 nm.
[0146] 14, the greater the distance 500D between the ink part 500 and the pixel electrode 140, the larger the area outside the pixel (frame region 1NA) that is visible when observed obliquely. For this reason, it is preferable that additive color printing is performed on the adhesive layer side of the second polarizer 622 as the second substrate side film 620. In other words, it is preferable to provide the ink part 500 between the second polarizer 622 as the second substrate side film 620 and the second adhesive layer 720.
[0147] (Fourth Modification of the First Embodiment) Fig. 15 is a schematic diagram showing a manufacturing method of a display panel according to Modification 4 of Embodiment 1. As shown in Fig. 15, the display panel 1 of this modification further includes a housing 900, and the ink section 500 has the same color as the housing 900. By adopting such an embodiment, it is possible to match the frame color with the housing color, so that the boundary between the frame region 1NA and the housing 900 is not emphasized, and the appearance can be improved.
[0148] The term "same color" does not necessarily mean that the colors are the same in the strict sense, but means, for example, that the color difference in the L*a*b* color system defined in JIS Z 8730 is within 20. The color difference is preferably greater than 0 and equal to or less than 0.5.
[0149] The display panel of this modified example can be fabricated as follows: As shown in Fig. 15, a panel precursor 10 in which a composition containing a photocurable monomer is filled between a first substrate 100 having a TFT 120 as a switching element and a second substrate 300 having no light-shielding portion 320 in a frame region 1NA is irradiated with light L from the second substrate 300 side.
[0150] Furthermore, a UV cut film 611 as a first substrate side film 610 is bonded to the side of the first substrate 100 opposite to the second substrate 300 via a first adhesive layer 710. Similarly, a UV cut film 621 as a second substrate side film 620 is bonded to the side of the second substrate 300 opposite to the first substrate 100 via a second adhesive layer 720. At least one of a frame region 1NA on the first adhesive layer 710 side of the first substrate side film 610 and a frame region 1NA on the second adhesive layer 720 side of the second substrate side film 620 is printed with additive colors in the same color as the housing 900 described in a process described later. The additive color printed portion corresponds to the ink section 500 (first substrate side ink section 510, second substrate side ink section 520). As an example, FIG. 15 shows an embodiment in which the second substrate side ink portion 520 is provided in the frame region 1NA on the second adhesive layer 720 side of the second substrate side film 620.
[0151] The laminate with the UV-cut film obtained as described above is fitted into a housing 900 of the same color as the ink portion 500, thereby obtaining the display panel 1 of this modified example.
[0152] (Fifth Modification of the First Embodiment) FIG. 16 is a cross-sectional schematic diagram showing a display panel according to Modification 5 of Embodiment 1. As shown in FIG. 16, the display panel 1 of this modification may have an alignment film between the first substrate 100 and the polymer-containing layer 200 and / or between the second substrate 300 and the polymer-containing layer 200. This aspect also provides the same effect as in Embodiment 1. The alignment film disposed between the first substrate 100 and the polymer-containing layer 200 is also called the first alignment film 410, and the alignment film disposed between the second substrate 300 and the polymer-containing layer 200 is also called the second alignment film 420. Note that the display panel 1 of this modification shown in FIG. 16 does not have an overcoat layer 321, but the display panel 1 of this modification may have an overcoat layer 321 between the light-shielding portion 320 and the counter electrode 322, as in Embodiment 1.
[0153] As the material of the alignment film, a material generally used in the field of liquid crystal display panels can be used, such as a polymer having polyimide in the main chain, a polymer having polyamic acid in the main chain, a polymer having polysiloxane in the main chain, etc. The polymer contained in the alignment film may be one type or two or more types.
[0154] The alignment film can be formed by applying an alignment film material, and the application method is not particularly limited, and for example, flexographic printing, inkjet application, etc. can be used. The alignment film may be a horizontal alignment film that aligns liquid crystal molecules approximately horizontally to the film surface, or a vertical alignment film that aligns liquid crystal molecules approximately perpendicularly to the film surface. The alignment film may be a photo-alignment film that has a photofunctional group and has been subjected to a photo-alignment treatment as an alignment treatment, a rubbing alignment film that has been subjected to a rubbing treatment as an alignment treatment, or an alignment film that has not been subjected to an alignment treatment.
[0155] In addition, as a method of alignment treatment applied to an alignment film, a rubbing method in which the surface of the alignment film is rubbed with a roller or the like has been widely used in the past. In contrast to this, in recent years, a photo-alignment method in which the surface of the alignment film is irradiated with light has been widely deployed as an alternative alignment treatment method to the rubbing method. According to the photo-alignment method, the alignment treatment can be performed without contacting the surface of the alignment film, and therefore, unlike the rubbing treatment, there is an advantage that the generation of dirt, dust, etc. during the alignment treatment can be suppressed.
[0156] The first alignment film 410 and the second alignment film 420 may be either a horizontal alignment film or a vertical alignment film, but are preferably vertical alignment films. By adopting such an embodiment, peeling between the polymer-containing layer 200 and the alignment film in the display panel 1 can be suppressed.
[0157] The reason why the vertical alignment film can suppress peeling between the polymer-containing layer 200 and the alignment film compared to the horizontal alignment film is believed to be due to the difference in the amount of side chains of the alignment film polymer present at the interface between the alignment film and the polymer-containing layer 200. That is, the more the amount of side chains of the alignment film polymer present at the interface, the more the side chains of the alignment film polymer can be entangled with the polymer contained in the polymer-containing layer 200, and it is believed that peeling between the polymer-containing layer 200 and the alignment film can be suppressed.
[0158] Fig. 17 is a cross-sectional view illustrating the function of the vertical alignment film. Fig. 18 is a cross-sectional view illustrating the intertwining of the vertical alignment film and the polymer. Fig. 19 is a cross-sectional view illustrating the function of the horizontal alignment film. Fig. 20 is a cross-sectional view illustrating the intertwining of the horizontal alignment film and the polymer.
[0159] As shown in FIG. 17, the vertical alignment film 430 generally has a function of vertically aligning liquid crystal molecules 931 contained in a liquid crystal layer 930 sandwiched between a substrate 910 having a support substrate 911 and an electrode 912 (e.g., a reflective electrode (Al, Ag, etc.)) and a substrate 920 having a support substrate 921 and an electrode 922 (e.g., a transparent electrode (ITO (Indium Tin Oxide))) to the alignment film. Therefore, the vertical alignment film polymer 431 contained in the vertical alignment film 430 has many side chains 433 in addition to the main chain 432 to vertically align the liquid crystal molecules 931 to the alignment film. Therefore, in this modification, as shown in FIG. 18, entanglement 434 is effectively generated between the side chain 433 of the vertical alignment film polymer 431 and the polymer 240 (e.g., the polymer network 210, the polymer layer 230) contained in the polymer-containing layer 200, and it is considered that the polymer-containing layer 200 and the vertical alignment film 430 are unlikely to peel off from each other.
[0160] On the other hand, as shown in FIG. 19, the horizontal alignment film 440 generally has a function of aligning the liquid crystal molecules 931 horizontally with respect to the alignment film. Therefore, the horizontal alignment film polymer 441 contained in the horizontal alignment film 440 has a main chain 442 but no side chain (or has fewer side chains than the vertical alignment film polymer 431 of the vertical alignment film 430). Therefore, as shown in FIG. 20, in this modification, entanglement between the horizontal alignment film polymer 441 and the polymer 240 contained in the horizontal alignment film 440 does not occur (is unlikely to occur). Therefore, the vertical alignment film 430 can suppress peeling between the polymer-containing layer 200 and the alignment film more effectively than the horizontal alignment film 440.
[0161] The vertical alignment film polymer 431 is, for example, a polymer having a polyamic acid in the main chain. The vertical alignment film polymer 431 preferably has a structure represented by the following formula (PA-1). By adopting such an embodiment, peeling between the polymer-containing layer 200 and the alignment film can be effectively suppressed.
[0162] [ka]
[0163] In the above formula (PA-1), X1 represents a tetravalent group, Y1 represents a trivalent group, Z represents a monovalent group, and s represents an integer of 1 or greater.
[0164] X1 in the above formula (PA-1) is preferably the following formula (X1-1) or (X1-2).
[0165] [ka]
[0166] [ka]
[0167] In the above formula (PA-1), Y1 is preferably represented by the following formula (Y1-1) or (Y1-2).
[0168] [ka]
[0169] [ka]
[0170] In the above formulae (Y1-1) and (Y1-2), * indicates the bonding position with Z.
[0171] Z in the above formula (PA-1) is preferably the following formula (Z-1) or (Z-2).
[0172] [ka]
[0173] [ka]
[0174] In the above formulae (Z-1) and (Z-2), * indicates the bonding position with Y.
[0175] The side chain represented by the formula (Z-2) is a fluorine-based side chain. Z in the formula (PA-1) is preferably the formula (Z-2). By adopting such an embodiment, it is possible to perform a photoalignment treatment.
[0176] It is also preferable that the vertical alignment film polymer 431 is a polymer having polysiloxane in the main chain. By adopting such an embodiment, peeling between the polymer-containing layer 200 and the alignment film can be effectively suppressed. In addition, since the vertical alignment film polymer 431 contains a polymer having polysiloxane in the main chain, it becomes possible to perform a photoalignment treatment.
[0177] The polymer having polysiloxane in the main chain preferably has a radical reactive functional group. By adopting such an embodiment, the vertical alignment film polymer having polysiloxane in the main chain can be cured by radical polymerization, and curing shrinkage can be minimized. Examples of the radical reactive functional group include unsaturated organic groups such as vinyl group, α-methylvinyl group, acryloyl group, methacryloyl group, and styryl group. Among these, those having an acryloyl group or methacryloyl group are preferred because the curing reaction proceeds smoothly.
[0178] The polymer having polysiloxane in the main chain is preferably a hydrolysis condensation product of a hydrolyzable silane compound.
[0179] The hydrolyzable silane compound is preferably a hydrolyzable silane compound containing (s1) a hydrolyzable silane compound represented by the following formula (MS-1) (hereinafter also referred to as (s1) compound) and (s2) a hydrolyzable silane compound represented by the following formula (MS-2) (hereinafter also referred to as (s2) compound).
[0180] [ka]
[0181] [ka]
[0182] In the above formula (MS-1), R 11 R is an alkyl group having 1 to 6 carbon atoms. 12 is an organic group containing a radical reactive functional group. p is an integer of 1 to 3. 11 and R 12 If there are multiple R 11 and R 12 are independent of each other.
[0183] In the above formula (MS-2), R 13 R is an alkyl group having 1 to 6 carbon atoms.14 is a hydrogen atom, an alkyl group having 1 to 20 carbon atoms, a fluorinated alkyl group having 1 to 20 carbon atoms, a phenyl group, a tolyl group, a naphthyl group, an epoxy group, an amino group, or an isocyanate group. n is an integer of 0 to 20. q is an integer of 0 to 3. 13 and R 14 If there are multiple R 13 and R 14 are independent of each other.
[0184] ((s1) compound) In the above formula (MS-1), R 11 R is an alkyl group having 1 to 6 carbon atoms. 12 is an organic group containing a radical reactive functional group. p is an integer of 1 to 3. 11 and R 12 If there are multiple R 11 and R 12 are independent of each other. 11 Examples of the alkyl group having 1 to 6 carbon atoms include a methyl group, an ethyl group, an n-propyl group, an i-propyl group, and a butyl group. Among these, from the viewpoint of ease of hydrolysis, a methyl group and an ethyl group are preferred. From the viewpoint of the progress of the hydrolysis condensation reaction, the above p is preferably 1 or 2, and more preferably 1.
[0185] Examples of the organic group having a radical reactive functional group include a linear, branched or cyclic alkyl group having 1 to 12 carbon atoms, an aryl group having 6 to 12 carbon atoms, and an aralkyl group having 7 to 12 carbon atoms, in which one or more hydrogen atoms are substituted with the above-mentioned radical reactive functional group. 12 These are independent when R exists. 12 The organic group represented by may have a heteroatom. Examples of such an organic group include an ether group, an ester group, and a sulfide group.
[0186] Examples of the (s1) compound include vinyltrimethoxysilane, vinyltriethoxysilane, vinyltrippropoxysilane, o-styryltrimethoxysilane, o-styryltriethoxysilane, m-styryltrimethoxysilane, m-styryltriethoxysilane, p-styryltrimethoxysilane, p-styryltriethoxysilane, allyltrimethoxysilane, allyltriethoxysilane, methacryloxytrimethoxysilane, methacryloxytriethoxysilane, methacryloxytrippropoxysilane, acryloxytrimethoxysilane, acryloxytriethoxysilane, acryloxytrippropoxysilane, 2-methacryloxyethyltrimethoxysilane, 2-methacryloxyethyltriethoxysilane, 2-methacryloxyethyltrippropoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropyltriethoxy ... Trimethoxysilane, 3-methacryloxypropyltriethoxysilane, 3-methacryloxypropyltripropoxysilane, 2-acryloxyethyltrimethoxysilane, 2-acryloxyethyltriethoxysilane, 2-acryloxyethyltripropoxysilane, 3-acryloxypropyltrimethoxysilane, 3-acryloxypropyltriethoxysilane, 3-acryloxypropyltripropoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropyltriethoxysilane, 3-methacryloxypropyltripropoxysilane, trifluoropropyltrimethoxysilane, trifluoropropyltriethoxysilane, trifluorobutyltrimethoxysilane, and 3-(trimethoxysilyl)propyl succinic anhydride are examples of trialkoxysilane compounds.
[0187] ((s2) compound) In the above formula (MS-2), R 13 R is an alkyl group having 1 to 6 carbon atoms. 14 is a hydrogen atom, an alkyl group having 1 to 20 carbon atoms, a fluorinated alkyl group having 1 to 20 carbon atoms, a phenyl group, a tolyl group, a naphthyl group, an epoxy group, an amino group, or an isocyanate group. n is an integer of 0 to 20. q is an integer of 0 to 3. 13 and R 14 If there are multiple R13 and R 14 are independent of each other.
[0188] The above mentioned R 13 Examples of the alkyl group having 1 to 6 carbon atoms include a methyl group, an ethyl group, an n-propyl group, an i-propyl group, and a butyl group. Among these, from the viewpoint of ease of hydrolysis, a methyl group and an ethyl group are preferred. From the viewpoint of the progress of the hydrolysis condensation reaction, the above q is preferably 1 or 2, and more preferably 1.
[0189] The above mentioned R 14When is an alkyl group having 1 to 20 carbon atoms, examples of the alkyl group include a methyl group, an ethyl group, an n-propyl group, an i-propyl group, an n-butyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, a 3-methylbutyl group, a 2-methylbutyl group, a 1-methylbutyl group, a 2,2-dimethylpropyl group, an n-hexyl group, a 4-methylpentyl group, a 3-methylpentyl group, a 2-methylpentyl group, a 1-methylpentyl group, a 3,3-dimethylbutyl group, a 2,3-dimethylbutyl group, a 1,3-dimethylbutyl group, a 2,2-dimethylbutyl group, a 1,2-dimethylbutyl group, a 1,1-dimethylbutyl group, an n-heptyl group, a 5-methylhexyl group, a 4-methylhexyl group, a 3-methylhexyl group, a 2-methylhexyl group, a 1-methylhexyl group, a 4,4-dimethylpentyl group, a 3,4-dimethyl Pentyl group, 2,4-dimethylpentyl group, 1,4-dimethylpentyl group, 3,3-dimethylpentyl group, 2,3-dimethylpentyl group, 1,3-dimethylpentyl group, 2,2-dimethylpentyl group, 1,2-dimethylpentyl group, 1,1-dimethylpentyl group, 2,3,3-trimethylbutyl group, 1,3,3-trimethylbutyl group, 1,2,3-trimethylbutyl group, n-octyl group, 6-methyl Examples of the alkyl group include heptyl group, 5-methylheptyl group, 4-methylheptyl group, 3-methylheptyl group, 2-methylheptyl group, 1-methylheptyl group, 2-ethylhexyl group, n-nonanyl group, n-decyl group, n-undecyl group, n-dodecyl group, n-tridecyl group, n-tetradecyl group, n-heptadecyl group, n-hexadecyl group, n-heptadecyl group, n-octadecyl group, and n-nonadecyl group. Preferred are alkyl groups having 1 to 10 carbon atoms, and more preferred are alkyl groups having 1 to 3 carbon atoms.
[0190] Among these (s2) compounds, particularly preferred hydrolyzable silane compounds include, for example, tetraethoxysilane, methyltrimethoxysilane, methyltriethoxysilane, methyltri-i-propoxysilane, methyltributoxysilane, phenyltrimethoxysilane, tolyltrimethoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, ethyltriisopropoxysilane, ethyltributoxysilane, butyltrimethoxysilane, γ-glycidoxypropyltrimethoxysilane, naphthyltrimethoxysilane, γ-aminopropyltrimethoxysilane and γ-isocyanatepropyltrimethoxysilane.Such hydrolyzable silane compounds may be used alone or in combination of two or more.
[0191] (Hydrolysis and condensation of compound (s1) and compound (s2)) The conditions for hydrolyzing and condensing the above-mentioned (s1) compound and (s2) compound are not particularly limited as long as they are capable of hydrolyzing at least a portion of the (s1) compound and the (s2) compound, converting the hydrolyzable groups into silanol groups, and inducing a condensation reaction.
[0192] The horizontal alignment film preferably contains a polymer having a structure represented by the following formula (PA-2).
[0193] [ka]
[0194] In the above formula (PA-2), X2 represents a tetravalent group, Y2 represents a trivalent group, and t represents an integer of 1 or greater.
[0195] In the above formula (PA-2), X2 is preferably the following formula (X2-1) or (X2-2).
[0196] [ka]
[0197] [ka]
[0198] In the above formula (PA-2), Y2 is preferably represented by the following formula (Y2-1), (Y2-2) or (Y2-3).
[0199] [ka]
[0200] [ka]
[0201] [ka] In the above formula (PA-2), Y2 is preferably the above formula (Y2-2) or (Y2-3). By adopting such an embodiment, it becomes possible to carry out a photo-alignment treatment. EXAMPLES
[0202] The effects of the present invention will be described below with reference to examples and comparative examples, but the present invention is not limited to these examples.
[0203] Example 1 FIG. 21 is a schematic diagram showing a manufacturing method of a display panel according to Example 1. A display panel of Example 1 corresponding to the display panel 1 of Embodiment 1 was manufactured by the method shown in FIG. 21. Specifically, a panel precursor 10 was prepared in which a composition containing a photocurable monomer was filled between a first substrate 100 having a TFT 120 as a switching element and a second substrate 300 not having a light-shielding portion 320 in a frame region 1NA. An exposure process was performed on the panel precursor 10, in which light L was irradiated from the second substrate 300 side, to manufacture the display panel 1 of Example 1. The display panel 1 had a polymer-containing layer 200 formed by polymerization of a photocurable monomer between the first substrate 100 and the second substrate 300. In the exposure process, the wavelength of light used for polymerization of the photocurable monomer was 360 nm, and the exposure dose was 20 J.
[0204] Furthermore, a UV cut film 611 as a first substrate side film 610 was attached to the side of the first substrate 100 opposite to the second substrate 300 via a first adhesive layer 710. Similarly, a UV cut film 621 as a second substrate side film 620 was attached to the side of the second substrate 300 opposite to the first substrate 100 via a second adhesive layer 720. Note that additive color printing was applied to the frame region 1NA on the second adhesive layer 720 side of the second substrate side film 620. The additive color printed portion corresponds to the second substrate side ink section 520.
[0205] The display panel 1 of this embodiment obtained in the above manner was a high-quality display panel with reduced display unevenness in the vicinity of the frame region 1NA. The reason for this is believed to be as follows: Since the frame region 1NA is transparent during exposure, the photocurable monomer is sufficiently irradiated with light, and there is no or only a very small amount of remaining monomer in the frame region 1NA, so that the seepage of the remaining monomer into the display region 1AA is suppressed, and display unevenness in the vicinity of the frame region 1NA is suppressed.
[0206] Moreover, the display panel 1 of this embodiment had a good retention rate. The reason for this is believed to be as follows. As described above, in this embodiment, the frame region 1NA was made transparent, thereby making it possible to suppress the generation of residual monomers in the frame region 1NA. Therefore, it is believed that excessive exposure was not necessary in order to expose as much of the residual monomers in the frame region 1NA as possible, and the retention rate of the liquid crystal component 220 was maintained high.
[0207] Furthermore, in the display panel 1 of the present embodiment, the range of the terminal pattern 120A visible to the viewer can be narrowed, and the display characteristics can be improved.
[0208] Furthermore, by providing the second substrate side ink portion 520, it is possible to suppress the influence of light from the second substrate 300 side on the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA. Also, it is possible to suppress frame reflection on the second substrate 300 side of the display panel 1.
[0209] Example 2 A display panel 1 of Example 2 corresponding to Modification 1 of the above-mentioned Embodiment 1 was produced. Specifically, the display panel 1 was produced in the same manner as in Example 1, except that in addition to the frame region 1NA on the second adhesive layer 720 side of the second substrate side film 620, the frame region 1NA on the first adhesive layer 710 side of the first substrate side film 610 was also subjected to additive color printing to provide an ink portion 500 (first substrate side ink portion 510).
[0210] As in Example 1, the display panel 1 of Example 2 was a display panel with high display quality in which display unevenness in the vicinity of the frame region 1NA was suppressed. The display panel of Example 2 also had a good retention rate. The display panel of Example 2 was also able to narrow the range of the terminal pattern 120A visible to the observer, thereby improving the display characteristics.
[0211] Also, similarly to Example 1, the display panel 1 of Example 2 is provided with the second substrate side ink part 520, which can suppress the influence of the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA on exposure to light from the second substrate 300 side. Also, frame reflection on the second substrate 300 side of the display panel 1 can be suppressed.
[0212] Furthermore, by providing the first substrate side ink part 510, the display panel 1 of Example 2 was able to suppress the influence of light from the first substrate 100 side on the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA. Also, the frame reflection on the first substrate 100 side of the display panel 1 was able to be suppressed.
[0213] Example 3 A display panel 1 of Example 3 corresponding to Modification 2 of the above-mentioned Embodiment 1 was produced. Specifically, the display panel 1 was produced in the same manner as in Example 2, except that additive color printing was performed not only on the frame region 1NA of the first substrate side film 610 but also on the region overlapping with the pixel wirings (the multiple gate lines 101G and the source lines 101S) of the display region 1AA to provide the first substrate side ink portion 510.
[0214] As in Example 2, the display panel 1 of Example 3 was a display panel with high display quality in which display unevenness in the vicinity of the frame region 1NA was suppressed. The display panel of Example 3 also had a good retention rate. The display panel of Example 3 was also able to narrow the range of the terminal pattern 120A visible to the observer, thereby improving the display characteristics.
[0215] Also, in the same manner as in Example 2, the display panel 1 in Example 3 is provided with the second substrate side ink part 520, and thus it is possible to suppress the influence on the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA due to exposure to light from the second substrate 300 side. Also, it is possible to suppress frame reflection on the second substrate 300 side of the display panel 1.
[0216] Also, in the same manner as in Example 2, the display panel 1 in Example 3 was provided with the first substrate side ink part 510, which could suppress the influence on the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA due to exposure to light from the first substrate 100 side. Also, the frame reflection on the first substrate 100 side of the display panel 1 could be suppressed.
[0217] Furthermore, in the display panel 1 of Example 3, by arranging the first substrate side ink part 510 in the display area 1AA of the first substrate side film 610, metal reflection is reduced not only in the frame area 1NA but also in the display area 1AA, thereby realizing a see-through panel with improved visibility.
[0218] Example 4 A display panel 1 of Example 4 corresponding to Modification 3 of the above-mentioned Embodiment 1 was produced. Specifically, the polymer-containing layer 200 in the display panel 1 of Example 1 was replaced with a layer containing a polymer layer 230 and a liquid crystal component 220, a color filter layer 330 was provided on the second substrate 300, the first substrate side film 610 was replaced with a first polarizer 612, the second substrate side film 620 was replaced with a second polarizer 622, and further, a backlight 800 was disposed on the rear side of the display panel 1 to produce the display panel 1 of Example 4 and a liquid crystal display device 2 including the display panel 1 and the backlight 800.
[0219] As in Example 1, the display panel 1 of Example 4 was a display panel with high display quality in which display unevenness in the vicinity of the frame region 1NA was suppressed. The display panel of Example 4 also had a good retention rate. The display panel of Example 4 was also able to narrow the range of the terminal pattern 120A visible to the observer, thereby improving the display characteristics.
[0220] Also, similarly to Example 1, the display panel 1 of Example 4 was provided with the second substrate side ink part 520, which could suppress the influence of the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA on exposure to light from the second substrate 300 side. Also, frame reflection on the second substrate 300 side of the display panel 1 could be suppressed.
[0221] Example 5 A display panel 1 of Example 5 corresponding to Modification 4 of the above-mentioned Embodiment 1 was produced. Specifically, the display panel 1 of Example 1 was fitted into a housing 900. The ink portion 500 was the same color as the housing 900.
[0222] As in Example 1, the display panel 1 of Example 5 was a display panel with high display quality in which display unevenness in the vicinity of the frame region 1NA was suppressed. The display panel 1 of Example 5 also had a good retention rate. The display panel 1 of Example 5 was also able to narrow the range of the terminal pattern 120A visible to the observer, thereby improving the display characteristics.
[0223] Also, similarly to Example 1, the display panel 1 of Example 5 was provided with the second substrate side ink part 520, which could suppress the influence of the electrical characteristics of the terminal pattern 120A of the TFT 120 in the frame region 1NA on exposure to light from the second substrate 300 side. Also, frame reflection on the second substrate 300 side of the display panel 1 could be suppressed.
[0224] Furthermore, in the display panel with housing 20 of Example 5, the boundary between the display panel 1 and the housing 900 was difficult to distinguish, and the appearance was good.
[0225] Example 6 A display panel corresponding to the above-mentioned modified example 5 of the embodiment 1 was produced. Specifically, the display panel of the example 6 was produced in the same manner as in the example 1, except that a vertical alignment film was provided as the first alignment film 410 between the first substrate 100 and the polymer-containing layer 200, and a vertical alignment film was provided as the second alignment film 420 between the second substrate 300 and the polymer-containing layer 200.
[0226] When a horizontal alignment film is used, peeling may occur between the polymer-containing layer 200 and the alignment film when the display panel is lifted, but peeling did not occur in the display panel of Example 6 using a vertical alignment film. This is thought to be due to the difference in the "amount of side chains" present at the interface between the alignment film and the polymer-containing layer 200, and it is thought that the vertical alignment film, which has more side chains than the horizontal alignment film, more effectively entangles the side chains of the alignment film polymer with the polymer, making peeling less likely to occur.
[0227] Comparative Example 1 Fig. 22 is a plan view schematic diagram of a panel precursor used in the manufacturing process of a display panel according to Comparative Example 1. Fig. 23 is an enlarged plan view schematic diagram of a region surrounded by a dashed line in Fig. 22. Fig. 24 is a schematic diagram showing a manufacturing method of a display panel according to Comparative Example 1.
[0228] As shown in Figs. 22 to 24, a panel precursor 10R was prepared in which a composition containing a photocurable monomer was filled between a first substrate 100 having a TFT as a switching element and a second substrate 300R having a black matrix layer in a frame region 1NA. An exposure process was performed in which light L was irradiated from the first substrate 100 side (TFT substrate side) to the panel precursor 10R, thereby producing a display panel 1R of Comparative Example 1 having a polymer-containing layer 200R formed by polymerization of the photocurable monomer between the first substrate 100 and the second substrate 300R. In the exposure process, the wavelength of light used for polymerization of the photocurable monomer was 360 nm, and the exposure dose was 20 J.
[0229] The panel precursor 10R had a gate electrode 11a, a capacitance line 11b, and a source electrode 14a in the display region 1AA, and had protection circuits 4a, 4b, test TFTs 5b, 5ca, 5cb, and a light-shielding portion 21b in the frame region 1NA.
[0230] In the display panel 1 of Comparative Example 1, reversible display unevenness was observed in the vicinity of the frame region 1NA, where the transmittance was higher than in other areas at a certain temperature. Furthermore, in the display panel 1 of Comparative Example 1, irreversible transparent area unevenness (irreversible display unevenness) was observed in the vicinity of the frame region 1NA in a high-temperature reliability test.
[0231] In Comparative Example 1, the panel precursor 10R filled with a liquid crystal material containing a photocurable monomer was exposed from the TFT substrate side to form a polymer network. At this time, the liquid crystal material containing a photocurable monomer filled in the shadow of the pattern (such as the terminal pattern (light-shielding portion 21b) of the TFT) formed in the frame region 1NA of the TFT substrate was not irradiated with light, so it is considered that the photocurable monomer was not polymerized in that region of the polymer-containing layer 200R and remained as a residual monomer. In other words, it is considered that the residual monomer remained behind the TFT pattern. It is considered that the residual monomer seeped into the display region 1AA, causing a display non-uniform area in the display panel 1R of Comparative Example 1.
[0232] TFT substrates often have patterns such as slits, and the polymerization reaction of the photocurable monomer proceeds in areas exposed to light, but since there are also areas not exposed to light, it is difficult to completely remove the remaining monomer. Therefore, in the display panel 1R of Comparative Example 1, display unevenness may occur during normal use, aging, use within a certain temperature range, etc., and it is considered that the display unevenness may be either reversible or irreversible.
[0233] Comparative Example 2 A display panel 1R of Comparative Example 2 was produced in the same manner as in Comparative Example 1, except that light L was irradiated from the second substrate 300R side (opposing substrate side).
[0234] In Comparative Example 2, the panel precursor 10R filled with the liquid crystal material containing the photocurable monomer was exposed from the opposing substrate side to form a polymer network. At this time, the liquid crystal material containing the photocurable monomer filled in the shadow of the black matrix layer formed in the frame region 1NA of the opposing substrate was not irradiated with light, so it is considered that the photocurable monomer was not polymerized in that region and remained as a residual monomer. In other words, it is considered that the residual monomer remained behind the black matrix layer. Since the black matrix layer in the frame region 1NA is a light-shielding portion that is solid all over, it is considered that the amount of the residual monomer in Comparative Example 2 is greater than that in Comparative Example 1. It is considered that the residual monomer seeped into the display region 1AA, which caused the display non-uniform area to occur in the display panel 1R of Comparative Example 1.
[0235] In the display panel 1R of Comparative Example 2, display unevenness may occur during normal use, aging, use within a certain temperature range, etc., and it is considered that the display unevenness may be either reversible or irreversible. The display unevenness occurring during use within a certain temperature range refers to, for example, a case where the display is uniform across the entire surface at room temperature and there is no problem, but at a certain temperature, display unevenness occurs only in an area where the influence of the residual monomer is large.
[0236] Comparative Example 3 The display panels of Comparative Example 3 were produced by changing the amount of exposure in the exposure process of Comparative Example 1. Specifically, a display panel exposed at 40 J, a display panel exposed at 60 J, a display panel exposed at 100 J, and a display panel exposed at 200 J were produced.
[0237] Fig. 25 is a plan view schematic diagram showing display unevenness of a display panel of Comparative Example 3 exposed at 40 J. Fig. 26 is a plan view schematic diagram showing display unevenness of a display panel of Comparative Example 3 exposed at 100 J. Fig. 27 is a graph showing the relationship between the exposure dose in manufacturing the display panel of Comparative Example 3 and the retention rate of the display panel.
[0238] As shown in Figures 25 and 26, it was found that the display unevenness was suppressed in the display panel exposed at 100 J compared to the display panel exposed at 40 J. It is considered that by increasing the exposure amount, the exposure of the remaining monomer behind the light-shielding part was promoted slightly, and the bleeding of the remaining monomer was suppressed slightly. However, the degree of suppression of the display unevenness was not sufficient.
[0239] In addition, it was found that increasing the amount of exposure reduces the retention rate of the liquid crystal material, as shown in Figure 27. The reduction in retention rate causes defects such as edge burn-in. [Explanation of symbols]
[0240] 1, 1R: Display panel 1AA:Display area 1NA: Frame area 2:LCD display device 4a, 4b: Protection circuit 5b, 5ca, 5cb: Inspection TFT 10, 10R: Panel precursor 11a: Gate electrode 11b: Capacitance line 14a: Source electrode 21b, 320: Light shielding part 100, 300: Substrate 100R:TFT board 101G: Gate line (gate metal) 101S: Source line (source metal) 101X: Wiring pattern 110, 310: supporting substrate 120: Thin Film Transistor (TFT) 120A: Terminal pattern (frame pattern) 130: Insulating layer 140: pixel electrode 200, 200R: Polymer-containing layer 210: Polymer network 220: Liquid crystal component 230: Polymer layer 240: Polymer 321: Overcoat layer 321a: Colored part 322: Counter electrode 330: Color filter layer 330B: Blue color filter 330G: Green color filter 330R: Red color filter 410, 420: Alignment film 430: Vertical alignment film 431: Vertically aligned polymer film 432, 442: Main chain 433: Side chain 434: Entanglement 440: Horizontal alignment film 441: Horizontal alignment polymer 500D: distance 500R: Seal 500, 510, 520: Ink section 610, 620: Film 611, 621: UV cut film 612, 622: Polarizer 710, 720: Adhesive layer 800: Backlight 900: Cabinet 910, 920: Substrate 911, 921: Support substrate 912, 922: Electrode 930: Liquid crystal layer 931: Liquid crystal molecules
Claims
1. A display area for displaying an image and a frame area provided around the display area, A display panel comprising, in this order, a first substrate having a switching element, a polymer-containing layer containing a polymer of a photocurable monomer, and a second substrate having a light-shielding portion that blocks light of a wavelength used for polymerization of the photocurable monomer and is not disposed in the frame region.
2. 2. The display panel according to claim 1, wherein the polymer-containing layer contains a polymer network formed of a polymer of the photocurable monomer and a liquid crystal component.
3. 2. The display panel according to claim 1, wherein the polymer-containing layer is composed of a polymer of the photocurable monomer, and contains a pair of polymer layers located on the surface on the first substrate side and the surface on the second substrate side, and a liquid crystal component located between the pair of polymer layers.
4. the first substrate includes a plurality of gate lines extending parallel to one another, and a plurality of source lines extending parallel to one another in a direction intersecting the plurality of gate lines via an insulating layer; 2. The display panel according to claim 1, further comprising a black matrix layer provided in the display region at a position overlapping the gate lines and the source lines.
5. 2. The display panel according to claim 1, wherein the second substrate further comprises, in the frame region, a colored portion that transmits light having a wavelength used for polymerization of the photocurable monomer.
6. The display panel according to claim 1, further comprising an ink portion in at least one of a frame region of the first substrate opposite the polymer-containing layer and a frame region of the second substrate opposite the polymer-containing layer.
7. Further, a second substrate side film is provided on the second substrate opposite to the polymer-containing layer, The display panel according to claim 6, characterized in that the ink portion comprises a second substrate side ink portion located at least in one of the areas between the second substrate side film and the second substrate and on the side of the second substrate side film opposite the second substrate.
8. The display panel according to claim 7 , wherein the second substrate side ink portion is located between the second substrate side film and the second substrate.
9. 8. The display panel according to claim 7, wherein the second substrate side film is a UV cut film.
10. 8. The display panel according to claim 7, wherein the second substrate side film is a polarizer.
11. Further, a first substrate side film is provided on the side of the first substrate opposite to the polymer-containing layer, The display panel according to claim 6, characterized in that the ink portion comprises a first substrate side ink portion located at least in one of the areas between the first substrate side film and the first substrate and on the side of the first substrate side film opposite the first substrate.
12. The display panel according to claim 11 , wherein the first substrate side ink portion is located between the first substrate side film and the first substrate.
13. The display panel according to claim 11 , wherein the first substrate side film is a UV cut film.
14. The display panel according to claim 11 , wherein the first substrate side film is a polarizer.
15. Further comprising a housing, The display panel according to claim 6 , wherein the ink portion has the same color as the housing.
16. A method for manufacturing a display panel, comprising an exposure step of irradiating light from the second substrate side to a panel precursor filled with a composition containing a photocurable monomer, the panel precursor being between a first substrate having switching elements and a second substrate having no light-shielding portion in a frame region provided around a display region for displaying an image.
17. 17. The method for manufacturing a display panel according to claim 16, further comprising, after the exposure step, a bonding step of bonding a first substrate side film, in which a first substrate side ink portion is arranged in the frame region, to the side of the first substrate opposite the second substrate.
18. 17. The method for manufacturing a display panel according to claim 16, further comprising, after the exposure step, a bonding step of bonding a second substrate side film, in which a second substrate side ink portion is arranged in the frame region, to the side of the second substrate opposite the first substrate.
Citation Information
Patent Citations
Liquid crystal display device and method for manufacturing same
WO2010103589A1