Laminar type diffraction grating

The laminar diffraction grating with a specific refractive index relationship and additional film structure enhances diffraction efficiency in the 'water window' region, addressing absorption and efficiency issues, and is cost-effective to produce.

JP2024160842APending Publication Date: 2024-11-15TOHOKU UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023076276
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-02
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing diffraction gratings for soft X-rays in the 'water window' region suffer from low diffraction efficiency and absorption issues, limiting their effectiveness in spectroscopic measurements and two-dimensional imaging.

Method used

A laminar diffraction grating with a complex refractive index structure, using a base film coated with an additional film that has a specific refractive index relationship and thickness to enhance diffraction efficiency, reducing absorption and enhancing the evanescent effect.

Benefits of technology

The laminar diffraction grating achieves high diffraction efficiency in the 200 eV to 543 eV range, reducing specularly reflected light and increasing the intensity of first-order light for measurement, while being cost-effective to manufacture.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024160842000001_ABST
    Figure 2024160842000001_ABST
Patent Text Reader

Abstract

To provide a diffraction pattern which can be easily manufactured and which exhibits high efficiency in a soft x-ray region.SOLUTION: Provided is a laminar type diffraction grating characterized in that, on a substrate 1 having a laminar type groove shape, the real part of complex refractive index of a soft x-ray (target electromagnetic wave) in a 200-543 eV region is coated with a nm basic film 2 in a sufficiently greater thickness than the penetration depth of the target electromagnetic wave, the real part of complex refractive index is further coated with a no additional film 3 on top of the basic film 2, and the relationship no>nm is established in the whole or part of the target electromagnetic wave. This laminar type diffraction grating is used at a larger angle of incidence than the total reflection condition of the additional film 3. The incident electromagnetic wave passes partly through the additional film 3 to reach the basic film 2 surface due to evanescent effects, but due to the face that no>nm, a phenomenon occurs that an electromagnetic wave diffracted on this boundary surface and an electromagnetic wave diffracted on the additional film 3 surface are intensified each other due to the thickness of the additional film 3, causing diffraction efficiency to increase.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a diffraction grating with high diffraction efficiency in the so-called "water window" region, which is a short-wavelength electromagnetic wave known as soft X-rays that cannot propagate through air due to absorption, and which has a particularly high transmittance through water and is therefore of great scientific, technological, and industrial value. [Background technology]

[0002] In the soft X-ray emission spectroscopy of carbon (C), nitrogen (N), and oxygen (O), K emission is generally used, with energies of 277 eV, 392 eV, and 525 eV, respectively, and wavelengths of 4.48 nm, 3.16 nm, and 2.36 nm. Furthermore, the region from around 200 eV to 543 eV, where the oxygen K absorption line (OK) is located, is called the "water window" region, where the transmittance of water is particularly high, and is important for in-situ measurement of biological materials. Soft X-rays have a longer wavelength than X-rays used in X-ray examinations, and are closer to ultraviolet rays. Furthermore, when the wavelength of soft X-rays changes, the ease of transmission changes depending on the element. By utilizing this characteristic, for example, the composition of living cell tissues in a culture solution can be observed with high contrast along with the internal structure. For this reason, "soft X-ray microscopes" that utilize the characteristics of these soft X-rays have attracted attention in the field of life science.

[0003] Furthermore, in spectroscopic analysis such as soft X-ray emission spectroscopy, which uses the interaction between a substance and light or electron beams to analyze the substance, it is extremely important to measure with good sensitivity even with weak light in order to improve the accuracy of the analysis. In particular, in the analysis of biological substances that are easily damaged by excitation X-rays and electron beams, and carbon, nitrogen, and oxygen contained in organic materials, it is not possible to increase the amount of light emission by increasing the amount of excitation energy, so there is a need to develop technology that improves the analytical sensitivity of samples under low doses by improving the performance of spectroscopic elements and detectors.

[0004] For this reason, in the diffraction gratings most widely used in the spectroscopic analysis of soft X-rays in the “water window” region, it is necessary to improve the diffraction efficiency and spectral flux (see, for example, Non-Patent Document 1), which are directly linked to improved spectral sensitivity.

[0005] When using a diffraction grating to disperse soft X-rays (wavelength: 12 nm to 0.6 nm) with energies between about 0.1 keV and 2 keV, the light is made to enter at a grazing angle to the diffraction grating surface in order to obtain practical diffraction efficiency. A material with a refractive index n slightly smaller than 1 is usually laminated on the surface of the diffraction grating as a reflective film, and to obtain high diffraction efficiency, the angle of incidence α measured from the normal direction perpendicular to the diffraction grating surface must satisfy the total reflection condition of the reflective film, sinα≧n.

[0006] However, due to the effect of the diffraction grating grooves, the diffracted light is not only dispersed into zero-order light and many other orders that satisfy the regular reflection condition, but also contains energy components that are absorbed in the surface material, so the intensity of the 1st order light (or -1st order light) used for measurement is much weaker than the intensity in the case of total reflection by a mirror without diffraction grating grooves. For this reason, laminar diffraction gratings with uneven groove shapes are designed to optimize the depth of the rectangular grooves and the area ratio (duty ratio) of the peaks and valleys of the unevenness, so that the light from the peaks and valleys causes positive interference in the diffracted light direction of the desired diffraction order light.

[0007] As a method for obtaining high diffraction efficiency in the soft X-ray region, there is a method of forming a multilayer structure in which low-density material layers and high-density material layers with higher density are alternately laminated on a surface having diffraction grating grooves. In a diffraction grating formed with a multilayer structure, soft X-rays are made to enter the multilayer structure by making the incident angle slightly smaller than the total reflection condition, and the light diffracted by the high-density material layer is intensified by interference, thereby obtaining high diffraction efficiency (for example, see Non-Patent Document 2). However, in this case, the energy absorbed in the multilayer structure is also large, so that soft X-rays in the "water window" region, which have relatively low energy, cannot penetrate deep inside the film, and the interference effect of the multilayer structure cannot be fully utilized due to the occurrence of scattering at the groove end surface, etc. This makes it difficult to obtain high diffraction efficiency with a multilayer diffraction grating in the "water window" region. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2015-94892 A [Patent Document 2] JP 2017-44556 A [Patent Document 3] JP 2018-63307 A [Non-patent literature]

[0009] [Non-Patent Document 1] T. Hatano, M. Koike, et al., 'Design and experimental evaluation of enhanced diffraction efficiency of lanthanum-based material coated laminar-type gratings in the boron K-emission region'Appl. Opt., 60 (16), 4993-4999 (2021) [Non-Patent Document 2] T. Imazono, M. Koike, et al., 'Development of an objective flat-field spectrograph for electron microscopic soft x-ray emission spectrometry in 50-4000 eV'Proc. of SPIE 8848, 884812 (2013) [Non-Patent Document 3] Masato Koike et al., "Application of DLC Optical Elements to Soft X-rays", Laser Society of Japan 471st Workshop Report, RTM-14-71 [Non-Patent Document 4] Yoshihiro Yanagihara, "Optical constants of ultrathin films in the soft x-ray region", Synchrotron Radiation, Vol. 9, No. 1, pp. 1-13 (1996) [Non-Patent Document 5] MG Moharam, 'Diffraction analysis of dielectric surface-relief gratings' JOSA A72, 1386 (1982) [Non-Patent Document 6] MG Moharam,'Rigorous coupled-wave analysis of metallic surface-relief gratings' JOSA A3, 1780 (1986) Summary of the Invention [Problem to be solved by the invention]

[0010] Soft X-rays in the "water window" region have low energy and are therefore largely absorbed by the materials that make up optical elements. This makes it difficult to improve the diffraction efficiency over a wide energy band using a soft X-ray diffraction grating that has a multilayer structure, and the rays are therefore unsuitable for simultaneous spectroscopic measurements with high diffraction efficiency over a wide energy band using two-dimensional imaging elements, which are becoming mainstream in recent years.

[0011] The present inventors have demonstrated through numerical calculations that it is possible to improve the diffraction efficiency of commercially available diffraction gratings for soft X-ray spectroscopic analysis, which have a metal film surface, by adding a diamond-like carbon (DLC), lanthanum-based, oxide-based, or fluoride-based high-density elementary film to the surface of these diffraction gratings, with the aim of achieving high-sensitivity analysis of soft X-rays in the vicinity of the K emission of boron (B) (183 eV, 6.76 nm) (see Patent Documents 1 to 3 and Non-Patent Documents 1 to 3).

[0012] However, when a film containing carbon, nitrogen, or oxygen, which has an emission line energy within the "water window" region, is added to the surface of a diffraction grating and used as a reflective film, the reflectivity and therefore the diffraction efficiency decrease because there are also absorption lines near the emission line. For this reason, it cannot be used as a reflective film, and there was a need to search for a new additional film that does not contain these substances.

[0013] The present invention has been made in consideration of the above problems, and has an object to provide a diffraction grating that can be easily manufactured and exhibits high diffraction efficiency in the energy region from about 200 eV to 543 eV within the "water window" region. [Means for solving the problem]

[0014] The laminar diffraction grating according to the present invention, which has been devised to solve the above problems, is provided on a substrate having laminar grooves, and has a complex refractive index n to m The real part of n m The complex refractive index n~ of electromagnetic waves in the range of 200 to 543 eV is applied to the base film. o The real part of n o The relationship between their real refractive indices is n in all or part of the 200 to 543 eV range. o > n m It is.

[0015] Complex refractive index of the base film n~ m teeth n~ m = (1-δ m ) - iβ m…(1) The complex refractive index is expressed as n~ m The real part of n m is (1 - δ m ). In addition, the complex refractive index of the additional film, n~ o teeth, n~ o = (1 - δ o ) - iβ o …(2) The complex refractive index is expressed as n~ o The real part of n o is (1 - δ o ), where δ m , δ o are the refractive indices of each material, and β m , β o is the extinction coefficient, and the above relationship is true for all or part of the "water window" (200-543 eV) region. m > δ o It states that.

[0016] In the present invention, β m > β o It is preferable that:

[0017] Furthermore, in order to solve the above problem, the thickness of the additional film added on the base film is h o is the condition under which the phases of the light diffracted by the upper and lower surfaces of the additional film match constructively. h o ~ λ / (cosα + cosβ) …(3) It is preferable to satisfy the following. Specifically, h o It is preferable that the wavelength is within a range of 10% of λ / (cosα + cosβ), where λ is the wavelength of the electromagnetic wave, and the wavelength is the wavelength of the electromagnetic wave. λ (nm) = 1239.842 / E (eV) …(4) In addition, α and β are the angle of incidence and the angle of diffraction, respectively, measured from the normal to the diffraction grating surface. Specifically, the thickness of the additional film that satisfies this requirement is 2 nm or more and 30 nm or less, more preferably 5 nm or more and 10 nm or less, and particularly preferably 8 nm.

[0018] In any of the above-described embodiments of the laminar diffraction grating, the base film can be made of gold (Au), platinum (Pt), or tungsten (W).

[0019] The base film may be an alloy of two or more of the above-mentioned metals, gold (Au), platinum (Pt), and tungsten (W), or a compound of the metal and another substance.

[0020] The additional film can be any of the following metals: cobalt (Co), nickel (Ni), or chromium (Cr).

[0021] The additional film may be an alloy of two or more of the above-mentioned metals cobalt (Co), nickel (Ni), and chromium (Cr), or a compound of the metal and a substance other than these.

[0022] The laminar type diffraction grating according to the present invention improves the diffraction efficiency based on a different principle from that of conventional metal film-coated diffraction gratings coated with gold, platinum, etc. That is, in conventional metal film-coated diffraction gratings, the angle of incidence is set to be larger than the total reflection condition to reduce absorption and improve the diffraction efficiency, but absorption cannot be completely eliminated.

[0023] The critical angle α at which total reflection occurs C depends on the complementary refractive index δ, α C = 90 - 180√2δ / π …(5) Generally, the larger the incident angle is, the larger the α / α CThe larger the value of δm, the higher the reflectance. Therefore, in the laminar diffraction grating according to the present invention, the angle of incidence of the target electromagnetic wave (electromagnetic wave to be diffracted) is set to an angle larger than the total reflection condition of the base film and the additional film. Due to the evanescent effect, part of the incident target electromagnetic wave penetrates into the additional film and then into the base film, but when δm > δo, a phenomenon occurs in which the reflectance increases at the interface between the additional film and the base film, similar to total reflection.

[0024] In the past, the surfaces of optical elements such as reflectors have sometimes been coated with chemically inactive substances with low absorption in order to prevent optical deterioration due to oxidation, etc.; however, this was primarily intended to limit chemical and thermodynamic changes between different substances (interfaces), and was not intended as a surface coating for diffraction gratings to increase the efficiency of reflected and diffracted light. Effect of the Invention

[0025] In the present invention, the effect of the additional film coated on the basic film on the diffraction grating surface reduces the specular reflection light (zeroth order light) and increases the ratio of the energy of the +1st order light (or -1st order light) used for measurement in a wide energy band centered on the water window region. In actual production, it is easy to form an additional film of a different metal on the metal film, which is the basic film, and production can be carried out at low cost. [Brief description of the drawings]

[0026] [Figure 1] FIG. 1 is a diagram showing a structure of a conventional diffraction grating. [Diagram 2] 1 is a diagram showing a structure of a diffraction grating having an additional film on its surface according to an embodiment of the present invention. [Diagram 3]This is a table of the electromagnetic wave energy and the complementary refractive indices δm and δC (collectively written as δm,o), real refractive indices nm,no (collectively written as nm,o), extinction coefficients βm and βo (collectively written as βm,o), and critical angles γC for gold (Au), platinum (Pt), tungsten (W), cobalt (Co), nickel (Ni), and chromium (Cr), which are used as reflective films for diffraction gratings. [Figure 4] 4(a) and (b) are diagrams of conventional diffraction gratings in which only Au, which is the material of the base film in the embodiment of the present invention, or Ni, which is the material of the additional film, is formed, respectively.(c) is a diagram showing a diffraction grating in which Au is used as the base film 2 and Ni is used as the additional film 3 in the diffraction grating of the embodiment of the present invention. [Diagram 5] 5(a) and (b) are diagrams showing the diffraction efficiency of a conventional diffraction grating in which only Au, which is the material of the base film according to the embodiment of the present invention, or Ni, which is the material of the additional film, is formed, and (c) is a diagram showing the diffraction efficiency of a diffraction grating in which Au is used as the base film 2 and Ni is used as the additional film 3 in the diffraction grating according to the embodiment of the present invention. [Figure 6] 1 is a graph showing the results of numerical calculations of the diffraction efficiency of a diffraction grating whose base film 2 is gold (Au) and the diffraction efficiency of a diffraction grating on which a film of either cobalt (Co), nickel (Ni), or chromium (Cr) is deposited as an additional film. [Figure 7] 1 is a graph showing the results of numerical calculations of the diffraction efficiency of a diffraction grating having a platinum (Pt) surface and a diffraction grating having an additional film of either cobalt (Co), nickel (Ni), or chromium (Cr). [Figure 8] 1 is a graph showing the results of numerical calculations of the diffraction efficiency of a diffraction grating having a tungsten (W) surface and a diffraction grating having an additional film of either cobalt (Co), nickel (Ni), or chromium (Cr) deposited thereon. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] A laminar diffraction grating for soft X-rays according to one embodiment of the present invention will be described in detail below in comparison with a conventional type.

[0028] The configuration of a conventional laminar diffraction grating will be explained using Figure 1. In a Cartesian coordinate system, the x-axis is the perpendicular (normal) direction of the diffraction grating at the center O of the diffraction grating, the y-axis is the tangent direction perpendicular to the grating grooves of the diffraction grating surface at O, and the z-axis is the axis perpendicular to them at O ​​(axis perpendicular to the paper surface). In this case, the angle from the x-axis direction to the direction of the incident light is defined as the incident angle (α). Additionally, the angle from the x-axis direction to the direction of the 1st-order diffracted light of the diffraction order (m) of the wavelength (λ) used for measurement is defined as the diffraction angle (β). For both angles α and β, the signs are positive counterclockwise from the x-axis.

[0029] The diffraction grating grooves have a rectangular wave shape, generally known as a laminar type, and grating grooves are formed on the surface of a substrate 1 such as SiO2, or on the surface of a resin formed on the substrate 1, with a lattice constant (σ) that is the groove period, a length of the groove peaks (a), and a groove depth (h).

[0030] In the conventional laminar diffraction grating and the diffraction grating according to the embodiment of the present invention described later, the substrate 1 is, for example, a glass (SiO2) substrate having laminar grating grooves with a ruling density (1 / σ): 1200 lines / mm (σ: 833.3 nm), h: 8 nm, and a duty ratio (a / σ): 0.4 (a: 333.3 nm). A base film 2 with a thickness d1 is deposited on the substrate 1. In the conventional type, an Au or Ni film with a thickness (d1): 30 nm is deposited on the substrate 1, and in the embodiment described later, an Au film with a thickness (d1): 30 nm is deposited on the substrate 1.

[0031] The form of a laminar diffraction grating according to one embodiment of the present invention is shown in Fig. 2. The difference from the conventional form in Fig. 1 is that the laminar diffraction grating according to one embodiment of the present invention has an additional film 3 deposited to a thickness d2 on the base film 2 described in Fig. 1. Here, the additional film 3 is a film of cobalt (Co), nickel (Ni), or chromium (Cr) to a thickness d2: 8 nm.

[0032] FIG. 3 shows the complex refractive index δ and the real part n of the complex refractive index of gold (Au), platinum (Pt), and tungsten (W) used as the base film 2 and cobalt (Co), nickel (Ni), and chromium (Cr) used as the additional film 3 in the embodiment of the present invention. m,o (= 1-δ m,o ), extinction coefficient β m,o , the critical angle γ C This is a table of literature values ​​(Non-Patent Document 4).

[0033] In the following, the diffraction efficiency of diffraction gratings having various structures is estimated to show the superiority of the diffraction grating of the embodiment of the present invention shown in Fig. 2 over the conventional diffraction grating shown in Fig. 1. Fig. 4(a) and Fig. 4(b) are diagrams showing the structure of a conventional diffraction grating in which the film thickness of the base film 2 is a base film thickness (d1): 30 nm, which is a thickness at which no light is transmitted to the SiO2 substrate due to absorption, and in which Au and Ni are formed, respectively. Fig. 4(c) is a diagram showing the structure of a diffraction grating of the embodiment of the present invention in which the base film 2 is an Au film with a film thickness d1 of 30 nm, and the additional film 3 is an Ni film with a film thickness d2 of 8 nm.

[0034] The diffraction efficiency of first-order light when light with energy of 62 to 1000 eV (wavelength: 1.2 to 20.0 nm) is incident on the diffraction grating having each of the structures shown in Figures 4(a) to (c) at an incident angle α of 86.0° is shown in Figure 5. The diffraction efficiency was calculated numerically using a method based on MG Moharam et al. (see Non-Patent Documents 5 and 6).

[0035] In the case of a conventional diffraction grating with a Au film on its surface as shown in Figure 4(a), the diffraction efficiency in the "water window" region from around 200 eV (6.2 nm) to 543 eV (2.28 nm) is approximately 10% at maximum, with an average of approximately 8%. In the case of a conventional diffraction grating with a Ni film on its surface as shown in Figure 4(b), the diffraction efficiency in the "water window" region from around 200 eV to 543 eV is approximately 20% at maximum, with an average of approximately 15%. However, in the vicinity of OK emission (525 eV), the real refractive index n m approaches 1, and the critical angle α capproaches approximately 1° smaller than the incident angle α, the diffraction efficiency drops significantly due to the effect of the drop in reflectance.

[0036] In the case of the diffraction grating according to the embodiment of the present invention shown in FIG. 4(c), the diffraction efficiency in the region from about 200 eV to 400 eV is almost the same as that of the conventional diffraction grating having a Ni film on the surface shown in FIG. 4(b). This is because in this region, o < n m < 1, critical angle α C is small and α >> α C This is because strong total reflection occurs on the surface of the additional film.

[0037] On the other hand, above 400 eV, which includes the OK emission, the diffraction efficiency is higher than that of the conventional configuration. This is because m < n o < 1, the incident light enters the additional film 3 as evanescent light, and the electromagnetic wave that reaches the boundary with the base film 2 does not have a geometric optical light direction, but it is believed that an effect of enhanced reflection similar to total reflection occurs. However, for this effect to occur, the electromagnetic wave energy of the incident light needs to reach the boundary surface between the additional film 3 and the base film 2. When an electromagnetic wave of 525 eV is incident at an incident angle of 86°, the film thickness at which the energy becomes 1 / e is about 3 nm, so when the film thickness of the additional film 3 is 8 nm, about 7% of the energy reaches the boundary surface, which is thought to be the reason for this effect.

[0038] 6 to 8 are diagrams showing the diffraction efficiency when Au, Pt, and W are used as the base film 2 and Co, Ni, and Cr are used as the additional film 3 in a diffraction grating according to an embodiment of the present invention. In each diagram, the diffraction efficiency of a diffraction grating having only the base film 2 without the additional film 3 is also shown. When Cr is used as the additional film 3, the diffraction efficiency drops significantly at 400 eV or more compared to the cases of Co and Ni, regardless of the metal of the base film 2. This is because the critical angle α cThis is because the angle of incidence becomes larger than the incident angle α, and the total reflection condition is no longer satisfied. However, since it has almost the same effect as Co and Ni on the lower energy side below 400 eV, it can be effectively used as the diffraction grating according to the present invention depending on the application.

[0039] The practice of the present invention does not depend on the physical properties of the diffraction grating substrate 1, so the same diffraction efficiency as in the above embodiment can be obtained not only with a diffraction grating directly engraved on a substrate such as glass, but also with a replica diffraction grating in which grating grooves are engraved on the surface of a resin layer on a substrate. Replica diffraction gratings can be produced more cheaply than master diffraction gratings in which grating grooves are engraved on the surface of a substrate, and this is also an important characteristic that makes them convenient for industrial mass production.

[0040] The invention according to the embodiment of the present invention can be appropriately modified without departing from the spirit of the present invention. For example, the ruling density is not limited to 1200 lines / mm, but can be changed to 200 lines / mm or more and 5000 lines / mm or less. The groove depth (h) is not limited to 8 nm, but can be 2 nm or more and 20 nm or less. The duty ratio (a / σ) is not limited to 0.4, but can be 0.3 or more and 0.5 or less. The thickness of the base film d1 is not limited to 30 nm, but can be any thickness that does not transmit the target electromagnetic wave. The incidence angle (α) of the soft X-ray is not limited to 86°. However, it is preferable to use it at 84° or more and 88° or less.

[0041] In the present invention, a stable metal film is used as the additional film 3, and since the film thickness is only a few nm, no stress that would cause deformation or roughness of the surface shape is generated between the additional film 3 and the base film 2. This increases the diffraction efficiency, which is the fundamental performance of a diffraction grating, in the wide energy band of the "water window" region, even in replica diffraction gratings that are mechanically fragile, and is therefore highly industrially useful. [Explanation of symbols]

[0042] 1... Diffraction grating substrate 2…Basic membrane 3…Additional film

Claims

1. On a substrate having a laminar groove shape, a layer having a thickness greater than the penetration depth of a target electromagnetic wave having an energy of 200 eV or more and 543 eV or less in the soft X-ray region and a real part of a complex refractive index for the target electromagnetic wave of n m The real part of the complex refractive index for the target electromagnetic wave is n o The target electromagnetic wave is entirely or partially covered with an additional film of n o > n m A laminar diffraction grating characterized in that

2. 2. The laminar diffraction grating according to claim 1, wherein the additional film has a thickness of 2 nm or more and 30 nm or less.

3. 3. The laminar diffraction grating according to claim 1 or 2, characterized in that the base film is made of any one of the metals gold (Au), platinum (Pt) and tungsten (W), or an alloy of two or more of these metals, or a compound formed from the metal or alloy and other substances other than these.

4. 3. The laminar diffraction grating according to claim 1, wherein the additional film is made of any one of the metals cobalt (Co), nickel (Ni), and chromium (Cr), or an alloy of two or more of these metals, or a compound formed from the metal or alloy and a substance other than these metals.

5. The thickness of the additional film is h o Let the wavelength of the target electromagnetic wave be λ, the angle of incidence measured from the perpendicular line to the diffraction grating surface be α, and the angle of diffraction be β. h o = λ / (cosα + cosβ) 3. The laminar diffraction grating according to claim 1, wherein the laminar diffraction grating is within a range of 10% of the above.

6. The extinction coefficient β of the base film m and the extinction coefficient β of the additional film o but, β m > β o 3. The laminar diffraction grating according to claim 1, wherein

Citation Information

Patent Citations

  • Diffraction grating

    JP2015094892A

  • Laminar type diffraction grating

    JP2017044556A

  • Laminar diffraction grating

    JP2018063307A