Display device

By employing oxide semiconductors in a specific thin film transistor configuration, the aperture ratio and display quality of liquid crystal displays are enhanced, addressing mobility and manufacturing complexity issues in existing technologies.

JP2024161149AActive Publication Date: 2024-11-15SEMICON ENERGY LAB CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2024146337
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2009-10-09
Filing Date
2024-08-28
Publication Date
2024-11-15
Estimated Expiration
2030-10-05

AI Technical Summary

Technical Problem

Existing thin film transistors used in liquid crystal display devices face challenges with low field-effect mobility and require complex crystallization processes, limiting their suitability for high-resolution displays with improved aperture ratios.

Method used

The use of oxide semiconductors, such as In-Ga-Zn-O, in thin film transistors with a specific configuration where the oxide semiconductor layer protrudes from the wiring area, allowing for overlapping with the pixel electrode, enhances the aperture ratio and improves display quality.

Benefits of technology

This configuration results in a liquid crystal display device with higher definition and improved aperture ratio, enabling better light transmission and reduced manufacturing defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024161149000001_ABST
    Figure 2024161149000001_ABST
Patent Text Reader

Abstract

To provide a liquid crystal display device in which a pixel, including a thin film transistor using an oxide semiconductor, has an improved aperture ratio.SOLUTION: The liquid crystal display device includes a plurality of pixels each including the thin film transistor and a pixel electrode. The pixel is electrically connected to first wiring functioning as a scan line. The thin film transistor includes an oxide semiconductor layer over the first wiring via a gate insulating film. The oxide semiconductor layer is extended beyond the edge of a region where the first wiring is provided. The pixel electrode and the oxide semiconductor layer overlap with each other.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a liquid crystal display device and also to an electronic device equipped with the liquid crystal display device. [Background technology]

[0002] As typified by liquid crystal display devices, thin film transistors formed on flat plates such as glass substrates They are made of amorphous silicon and polycrystalline silicon. Thin-film transistors using GaN have low field-effect mobility, but they are suitable for enlarging the area of ​​glass substrates. On the other hand, thin-film transistors using crystalline silicon have high field-effect mobility. However, a crystallization process such as laser annealing is required, and it is essential to enlarge the area of ​​the glass substrate. It has the characteristic that it is not adapted to

[0003] In response to this, thin-film transistors are being fabricated using oxide semiconductors, and they are being used in electronic devices and optical devices. For example, zinc oxide and In-GaAs films are used as oxide semiconductors. Thin-film transistors were fabricated using a-Zn-O oxide semiconductors, and used as switches for liquid crystal display devices. Patent Document 1 discloses a technique for use in a switching element and the like. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2009-99887 A Summary of the Invention [Problem to be solved by the invention]

[0005] Thin-film transistors that use oxide semiconductors for the channel region are similar to those that use amorphous silicon for the channel region. The field effect mobility is higher than that of a thin film transistor using a GaN-based GaN thin film transistor in the panel region. A pixel including a thin film transistor formed using an oxide semiconductor is used in a liquid crystal display device or the like. It is expected to be applied to display devices. It is also expected to be used in 3D displays, 4k2k displays, and other displays. In LCD devices with added value, the area per pixel is expected to become smaller. On the other hand, there is a demand for a liquid crystal display device having pixels with an improved aperture ratio.

[0006] Therefore, the present invention provides a pixel having a thin film transistor using an oxide semiconductor. An object of the present invention is to provide a liquid crystal display device capable of improving the display efficiency. [Means for solving the problem]

[0007] One embodiment of the present invention includes a plurality of pixels each having a thin film transistor and a pixel electrode. The thin film transistor is electrically connected to a first wiring functioning as a scan line. The oxide semiconductor layer is provided on the wiring of the first embodiment via a gate insulating film. The first wiring is provided outside the region where the pixel electrode and the oxide semiconductor layer and are provided so as to overlap each other.

[0008] One embodiment of the present invention includes a plurality of pixels each having a thin film transistor and a pixel electrode. , electrically connected to a first wiring functioning as a scanning line and a second wiring functioning as a signal line The thin film transistor is formed on an oxide film provided on the first wiring via a gate insulating film. The oxide semiconductor layer is provided so as to extend beyond a region in which the first wiring is provided. The second wiring extends on the gate insulating film on the first wiring and is connected to the oxide semiconductor layer. The liquid crystal display device has a pixel electrode and an oxide semiconductor layer that overlap each other.

[0009] One embodiment of the present invention includes a plurality of pixels each having a thin film transistor and a pixel electrode. , electrically connected to a first wiring functioning as a scanning line and a second wiring functioning as a signal line The thin film transistor is formed on an oxide film provided on the first wiring via a gate insulating film. The oxide semiconductor layer is provided so as to extend beyond a region in which the first wiring is provided. The second wiring is formed on the gate insulating film on the first wiring and on the interlayer insulating film on the gate insulating film. The pixel electrode is extended to contact the oxide semiconductor layer, and the pixel electrode and the oxide semiconductor layer are overlapped with each other. It is a liquid crystal display device. Effect of the Invention

[0010] When manufacturing a pixel having a thin film transistor using an oxide semiconductor, it is necessary to improve the aperture ratio. Therefore, a liquid crystal display device having a high-definition display portion can be obtained. [Brief description of the drawings]

[0011] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating a liquid crystal display device. [Diagram 2] FIG. 1 is a cross-sectional view illustrating a liquid crystal display device. [Diagram 3] FIG. 1 is a top view illustrating a liquid crystal display device. [Figure 4] 1A and 1B are a top view and a cross-sectional view illustrating a liquid crystal display device. [Diagram 5] FIG. 1 is a top view illustrating a liquid crystal display device. [Figure 6] 1A and 1B are a top view and a cross-sectional view illustrating a liquid crystal display device. [Figure 7] FIG. 1 is a circuit diagram illustrating a liquid crystal display device. [Figure 8]FIG. 1 is a circuit diagram illustrating a liquid crystal display device. [Figure 9] 1A and 1B are a circuit diagram and a timing chart illustrating a liquid crystal display device. [Figure 10] FIG. 1 is a circuit diagram illustrating a liquid crystal display device. [Figure 11] FIG. 1 is a circuit diagram illustrating a liquid crystal display device. [Figure 12] 1A to 1C are diagrams illustrating electronic devices. [Figure 13] 1A to 1C are diagrams illustrating electronic devices. [Figure 14] 1A and 1B are a top view and a cross-sectional view illustrating a liquid crystal display device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The present invention will be described in detail with reference to the accompanying drawings. The present invention is not limited to the above, and various modifications and variations in form and detail are possible without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that the present invention can be modified in the following manner. The present invention is not limited to the above-described embodiment. In the structure, the same parts or parts having similar functions are designated by the same reference numerals in different drawings. and the repeated explanation will be omitted.

[0013] In each figure described in this specification, the size, layer thickness, or area of ​​each component is not clearly indicated. The figures may be exaggerated for illustrative purposes and are not necessarily limited to scale.

[0014] In this specification, the terms "first", "second", "third", etc. are used in order to avoid confusion of components. The number is not limited to the number of the first one. For example, "first one" can be changed to " The terms "second" or "third" can be used interchangeably to explain the present invention.

[0015] (Embodiment 1) In this embodiment, as an example, a thin film transistor (hereinafter, also referred to as a TFT) and the T The electrodes that function as pixel electrodes connected to the FT (also simply called pixel electrodes) are shown. A liquid crystal display device will now be described. Note that a pixel is an element provided in each pixel of a display device, e.g. For example, thin film transistors, electrodes that function as pixel electrodes, and wiring are used to display the image. A pixel is a group of elements that control the display of a color filter. Each pixel is equivalent to one color element whose brightness can be controlled. Thus, as an example, in the case of a color display device consisting of RGB color elements, The smallest unit of an image is composed of three pixels: an R pixel, a G pixel, and a B pixel. , an image can be obtained by a plurality of pixels.

[0016] In addition, when it is stated that A and B are connected, it means that A and B are electrically connected. This includes the cases where A and B are directly connected, and the cases where A and B are directly connected. Specifically, the object is a transistor or other switch. A and B are connected via a switching element, and when the switching element is turned on, A and When A and B are approximately at the same potential, or when A and B are connected via a resistor element, When the potential difference between the terminals A and B is small enough not to affect the operation of the circuit including A and B, When considering the circuit operation, it is acceptable to consider the part between A and B as the same node. This represents the case where the

[0017] First, a top view of a pixel is shown in FIG. 1(A). The structure of the TFT shown in FIG. 1(A) is as follows: It has a bottom-gate structure, and the oxide semiconductor that forms the channel region from the gate wiring On the other side of the layer, there is a wiring layer that becomes the source electrode and drain electrode of the TFT. A staggered configuration is shown.

[0018] A pixel 100 shown in FIG. 1A includes a first wiring 101 functioning as a scan line, The second wiring 102A, the oxide semiconductor layer 103, the capacitance line 104, and the pixel electrode 105 function as the second wiring 102A. The pixel 100 shown in FIG. 1A includes an oxide semiconductor layer 103 and a pixel electrode 105. A third wiring 102B for electrically connecting the first and second wirings is provided, and a thin film transistor 106 is formed. can be.

[0019] The first wiring 101 also functions as a gate of the thin film transistor 106. The wiring 102A is connected to one of the source electrode or the drain electrode of the thin film transistor 106 and The third wiring 102B also functions as one electrode of the storage capacitor. It also serves as the other of the source electrode and drain electrode of the transistor 106. The line 104 is a wiring that functions as the other electrode of the storage capacitor. The capacitor line 104 is provided in the same layer, and the second wiring 102A and the third wiring 102B are provided in the same layer. The third wiring 102B and the capacitance line 104 are provided in a partially overlapping manner. This forms a storage capacitor for the liquid crystal element.

[0020] Note that the oxide semiconductor layer 103 included in the thin film transistor 106 is The oxide semiconductor layer 103 is provided on the first wiring 101 through a gate insulating film (not shown). It is provided outside the area in which 101 is provided.

[0021] In addition, when A protrudes from B, it is seen from the top view of the stacked elements A and B. In this case, the ends of the elements do not coincide, with A extending outward beyond the end of B.

[0022] FIG. 1B shows a cross-sectional structure between dashed lines A1 and A2 in FIG. In the cross-sectional structure shown in FIG. 1(B), a gate electrode is formed on a substrate 111 via an undercoat film 112. The first wiring 101 and the capacitance line 104 are provided. A gate insulating film 113 is provided so as to cover the line 104. The oxide semiconductor layer 103 is provided on the second wiring 102. The oxide semiconductor layer 103, the second wiring 102A, and the third wiring 102B are provided. An oxide film functioning as a passivation film is provided on the wiring 102A and the third wiring 102B. The oxide insulating layer 114 is provided with an opening. In the opening, the pixel electrode 105 and the third wiring 102B are connected. The wiring 102B and the capacitance line 104 form a capacitance element with the gate insulating film 113 as a dielectric. is.

[0023] The pixels shown in FIGS. 1A and 1B are formed by disposing a plurality of pixels on a substrate 700 as shown in FIG. In FIG. 7, the pixels 701 are arranged in a matrix on the substrate 700. 7 shows a configuration including a display section 702, a scanning line driver circuit 703, and a signal line driver circuit 704. The pixel 701 is supplied with a first wiring 101 connected to a scanning line driving circuit 703. The scanning signal applied determines whether each row is selected or not. The pixel 701 selected by the signal is connected to the second wiring line driving circuit 704. Line 102A provides a video voltage (also called an image signal, a video signal, or video data). will be provided.

[0024] In FIG. 7, a scanning line driver circuit 703 and a signal line driver circuit 704 are provided on a substrate 700. However, either the scanning line driver circuit 703 or the signal line driver circuit 704 is The pixel portion 702 may be provided on the substrate 700. Alternatively, only the pixel portion 702 may be provided on the substrate 700. It may also be configured so that

[0025] In FIG. 7, a pixel section 702 has a plurality of pixels 701 arranged in a matrix (striped arrangement). It should be noted that the pixels 701 do not necessarily need to be arranged in a matrix. For example, the pixels 701 may be arranged in a delta arrangement or a Bayer arrangement. The display method in the element 702 is either the progressive method or the interlace method. In addition, the color elements controlled by pixels when displaying colors are RGB ( R is red, G is green, B is blue) and may be more than three colors, for example, RGBW ( W is white), or RGB plus one or more colors such as yellow, cyan, or magenta The size of the display area may be different for each dot of the color element.

[0026] In FIG. 7, the first wiring 101 and the second wiring 102A are arranged in a number equal to the number of pixels in the row and column directions. The first wiring 101 and the second wiring 102A are wirings that constitute a pixel. The number of subpixels (also called sub-pixels) or the number of transistors in a pixel In accordance with the above, the number of wirings may be increased. A configuration in which 102A is shared to drive pixel 701 may also be used.

[0027] In FIG. 1A, the shape of the TFT is shown as being rectangular in the second wiring 102A. However, the shape of the third wiring 102B is such that it surrounds the third wiring 102B (specifically, U-shaped or C-shaped), A configuration may be adopted in which the area of ​​the region through which carriers move is increased to increase the amount of current that flows.

[0028] The width of the first wiring 101 other than the region that will become the thin film transistor 106 is partially narrowed. By reducing the width of the first wiring, the aperture ratio of the pixel can be reduced. Improvements can be achieved.

[0029] The aperture ratio indicates the area through which light passes per unit area. When the area occupied by the non-transmitting material becomes larger, the aperture ratio decreases and the area occupied by the transmitting material becomes larger. The larger the area occupied, the higher the aperture ratio. The area of ​​the wiring to be folded, the area occupied by the capacitance line, and the size of the thin film transistor are reduced. This will result in improved oral intake.

[0030] A thin film transistor is a transistor that has at least three elements including a gate, a drain, and a source. An element having terminals, and a channel region between a drain region and a source region, A current can be passed through the drain region, the channel region, and the source region. The source and drain are different depending on the transistor structure and operating conditions, so which one is It is difficult to determine whether the source or drain is the source or drain. The region that functions as a gate may not be called a source or drain. For example, they may be written as the first terminal and the second terminal, respectively. These may be referred to as the first electrode and the second electrode, or as the first region and the second region. There are cases.

[0031] Next, the method for fabricating a pixel will be described based on the top view and cross-sectional view shown in Figure 1(A) and (B). 2 will be used to explain.

[0032] First, a glass substrate can be used as the light-transmitting substrate 111. Preventing diffusion of impurities from the substrate 111 or providing close contact with each element provided on the substrate 111 In order to improve the performance, a base film 112 is provided. There is no need to provide a

[0033] Next, a conductive layer is formed on the entire surface of the substrate 111, and then a first photolithography process is performed. A resist mask is formed, and unnecessary portions are removed by etching to form the first wiring 101, The capacitor line 104 is formed. At this time, at least the first wiring 101 and the end of the capacitor line 104 are The cross section at this stage is shown in Figure 2(A).

[0034] The first wiring 101 and the capacitance line 104 are made of low resistance metal such as aluminum (Al) or copper (Cu). It is preferable to use a conductive material, but aluminum alone has poor heat resistance and is prone to corrosion. Since there are problems such as the above, it is formed in combination with a heat-resistant conductive material. The following are titanium (Ti), tantalum (Ta), tungsten (W), molybdenum (Mo), An element selected from chromium (Cr), neodymium (Nd), scandium (Sc), or Alloys containing the above elements, or combinations of the above elements, or It is formed of a nitride containing the components.

[0035] In addition, the wiring that constitutes the TFT can be formed using an inkjet or printing method. These allow fabrication at room temperature, in low vacuum, or on large substrates. Since it can be manufactured without using a photomask, the transistor layout can be It is easy to change. Furthermore, since there is no need to use resist, the material cost is low. This reduces the number of processes. In addition, the resist mask can be formed using inkjet or printing methods. It is also possible to form the resist only in the required areas using inkjet or printing methods. By forming a resist mask by exposure and development, it is possible to reduce the size of the resist mask compared to forming a resist on the entire surface. This allows for cost reduction.

[0036] In addition, a multi-tone mask is used to create a resist mask having multiple (typically two types) of thickness regions. A wiring or the like may be formed by forming a wiring.

[0037] Next, an insulating film (hereinafter, referred to as a gate insulating film 113) is formed on the first wiring 101 and the capacitance line 104. The gate insulating film 113 is formed by sputtering or the like.

[0038] For example, the gate insulating film 113 is formed using a silicon oxide film by a sputtering method. Of course, the gate insulating film 113 is not limited to such a silicon oxide film. Other insulating films such as silicon oxide film, silicon nitride film, aluminum oxide film, and tantalum oxide film may be used and may be formed as a single layer or a laminate structure made of these materials.

[0039] Before forming an oxide semiconductor film, a reverse scanning laser was used to generate plasma by introducing argon gas. It is preferable to remove dust adhering to the surface of the gate insulating film 113 by puttering. Instead of the argon atmosphere, nitrogen, helium, or the like may be used. It may be performed in an atmosphere containing oxygen, N2O, etc. Also, the atmosphere may be mixed with Cl2 Alternatively, the reaction may be carried out in an atmosphere containing CF4 or the like.

[0040] Next, an oxide semiconductor is deposited on the gate insulating film 113 by plasma treatment of the surface of the gate insulating film 113. After the treatment, the oxide semiconductor is deposited without being exposed to the air. This results in a higher field effect transport rate compared to silicon-based semiconductor materials such as amorphous silicon. The oxide semiconductor can be, for example, zinc oxide (ZnO), oxide Tin oxide (SnO2) can also be used. In addition, by adding In or Ga to ZnO, It is also possible.

[0041] InMO3(ZnO) as an oxide semiconductor x It is possible to use a thin film represented by (x>0) M can be any of gallium (Ga), iron (Fe), nickel (Ni), manganese (M n) and cobalt (Co). For example, M may be Ga, or may be any of the above except Ga, such as Ga and Ni or Ga and Fe. In some cases, a metal element is contained. In addition, in the above oxide semiconductor, the metal contained as M is In addition to the group elements, impurity elements include Fe, Ni, and other transition metal elements, or oxides of the transition metals. For example, the In-Ga-Zn-O system is used as an oxide semiconductor layer. A membrane may be used.

[0042] Oxide semiconductor (InMO3(ZnO) x (x>0) film) as In-Ga-Zn-O system film Instead of InMO3(ZnO), M is another metal element. x (x>0) membrane may be used In addition to the above, other oxide semiconductors include In-Sn-Zn-O and In-Al-Z nO system, Sn-Ga-Zn-O system, Al-Ga-Zn-O system, Sn-Al-Zn-O system , In-Zn-O system, Sn-Zn-O system, Al-Zn-O system, In-O system, Sn-O system, A Zn-O based oxide semiconductor can be used.

[0043] Note that in this embodiment, an In-Ga-Zn-O-based oxide semiconductor is used. The target used is In2O3:Ga2O3:ZnO=1:1:1. The distance between the target and the target was 100 mm, the pressure was 0.6 Pa, the DC power supply was 0.5 kW, and the acid The film is formed in a nitrogen atmosphere (oxygen flow rate 100%) using a pulsed direct current (DC) power supply. This reduces the amount of powdery material (also called particles or dust) that is generated during film formation, and improves the film thickness distribution. This is preferable because the thickness becomes uniform.

[0044] The oxide semiconductor film was formed in the same chamber as the previous reverse sputtering. Alternatively, the film may be formed in a chamber different from the chamber in which the previous reverse sputtering was performed.

[0045] The sputtering method uses a high-frequency power supply as the sputtering power source, while the RF sputtering method uses a DC power supply. There are two types of sputtering: DC sputtering and pulsed DC sputtering, which uses a pulsed bias. The sputtering method is mainly used to deposit insulating films, while the DC sputtering method is mainly used to deposit metal films. It is used when:

[0046] There are also multi-target sputtering devices that can accommodate multiple targets of different materials. The equipment can deposit layers of different materials in the same chamber, or multiple types of films in the same chamber. It is also possible to form a film by discharging two or more materials at the same time.

[0047] Also, a sputtering apparatus using a magnetron sputtering method equipped with a magnet mechanism inside the chamber and ECR sputtering using plasma generated by microwaves without glow discharge. There is a sputtering apparatus that uses this method.

[0048] In addition, in a film formation method using a sputtering method, a target material and a sputtering gas component are mixed during film formation. Reactive sputtering is a method of forming thin films of compounds by chemically reacting them with each other, and There is also a bias sputtering method in which a voltage is also applied to the substrate.

[0049] Next, the oxide semiconductor layer is dehydrated or dehydrogenated. The temperature of the heat treatment in step 1 is 400° C. or higher and lower than 750° C., preferably 425° C. or higher. If the temperature is 425°C or higher, the heat treatment time may be 1 hour or less. In this case, the heat treatment time is set to be longer than one hour. The substrate is placed in an electric furnace, and the oxide semiconductor layer is subjected to heat treatment in a nitrogen atmosphere. After this, the oxide semiconductor layer is prevented from being exposed to the air, and water and hydrogen are prevented from re-mixing into the oxide semiconductor layer. In this embodiment, a process for dehydrating or dehydrogenating an oxide semiconductor layer is performed. From the heating temperature T, use the same furnace until it reaches a temperature that is high enough to prevent water from entering again. The temperature is gradually cooled in a nitrogen atmosphere until it drops by 100°C below the temperature T. Dehydration or dehydrogenation under a rare gas (helium, neon, argon, etc.) atmosphere Do the following.

[0050] The heat treatment device is not limited to an electric furnace, and may be a heat treatment device using heat conduction or heat from a heating element such as a resistance heating element. The apparatus may be equipped with a device for heating the object to be treated by radiation. For example, a GRTA (Gas Rapid Thermal Anneal) equipment, LRTA (Lamp Rapid Thermal Annealing equipment such as RTA (Rapid Thermal Annealing) The LRTA device can be used with halogen lamps, metal halide lamps, etc. lamp, xenon arc lamp, carbon arc lamp, high pressure sodium lamp, high pressure A device that heats the workpiece by radiating light (electromagnetic waves) emitted from a lamp such as a mercury lamp. The GRTA device is a device that uses high-temperature gas for heat treatment. A rare gas such as argon or nitrogen that hardly reacts with the material to be treated by heat treatment. An inert gas is used.

[0051] The oxide semiconductor layer is heat-treated at a temperature of 400° C. or higher and lower than 750° C. This will dehydrate and dehydrogenate the carbon black, preventing it from being re-impregnated with water (H2O) thereafter.

[0052] In the first heat treatment, nitrogen or a rare gas such as helium, neon, or argon is used. It is preferable that the nitrogen introduced into the heat treatment device does not contain water, hydrogen, etc. Or the purity of rare gases such as helium, neon, and argon must be 6N (99.9999%) or higher. Preferably, the concentration of impurities is 7N (99.99999%) or more (i.e., the impurity concentration is 1 ppm or less, It is preferable to keep the concentration of the ion exchange resin at 0.1 ppm or less.

[0053] Note that depending on the conditions of the first heat treatment or the material of the oxide semiconductor layer, In some cases, the film crystallizes to become a microcrystalline or polycrystalline film. For example, the crystallization rate is 90% or more. In some cases, the oxide semiconductor film is microcrystalline, or 80% or more of the oxide semiconductor film is microcrystalline. Depending on the conditions or the material of the oxide semiconductor layer, an amorphous oxide semiconductor layer containing no crystalline components may be obtained. It may also be a conductive film.

[0054] The oxide semiconductor layer becomes oxygen-deficient after the first heat treatment for dehydration or dehydrogenation. The oxide semiconductor layer after the first heat treatment has a lower resistance than the oxide semiconductor film just after the deposition. The carrier concentration is increased to 1×10 18 / cm 3 having a carrier concentration of This becomes an oxide semiconductor layer.

[0055] Next, a second photolithography step is performed to form a resist mask and etch. The unnecessary portions are removed by this process to form the oxide semiconductor layer 103 made of an oxide semiconductor. The first heat treatment on the oxide semiconductor layer is performed on the oxide semiconductor layer before it is processed into an island-shaped oxide semiconductor layer. The etching method used in this case is wet etching or dry etching. The cross-sectional view at this stage is shown in Figure 2(B).

[0056] Next, a conductive film made of a metal material is formed on the oxide semiconductor layer by a sputtering method or a vacuum deposition method. The conductive film is made of an element selected from Al, Cr, Ta, Ti, Mo, and W, or Examples of the alloy include alloys containing the above elements or alloys of combinations of the above elements. In addition, when performing heat treatment at 200°C to 600°C, the conductive film must be heat-resistant to withstand this heat treatment. Aluminum alone has problems such as poor heat resistance and susceptibility to corrosion. Therefore, it is formed by combining it with a heat-resistant conductive material. Heat-resistant conductive material combined with Al Titanium (Ti), tantalum (Ta), tungsten (W), molybdenum (Mo ), chromium (Cr), neodymium (Nd), and Sc (scandium), is an alloy containing the above elements, an alloy of a combination of the above elements, or It is formed from nitrides containing elements.

[0057] Here, the conductive film has a single-layer structure of titanium film. The conductive film may also have a two-layer structure. Alternatively, a titanium film may be laminated on an aluminum film. A layer of aluminum containing neodymium (Al-Nd) is layered on top of the Ti film, and then a layer of aluminum containing neodymium (Al-Nd) is layered on top of that. The conductive film may be a single layer of aluminum film containing silicon. It may also have a layered structure.

[0058] Next, a third photolithography process is performed to form a resist mask and perform etching. The unnecessary portions are removed to form the second wiring 102A and the third wiring 102B made of a conductive film. The etching method used in this process is either wet etching or dry etching. For example, ammonia hydrogen peroxide solution (31% by weight hydrogen peroxide solution: 28% by weight ammonia solution: water The conductive film of the Ti film was etched by wet etching using a SiO2 / SiO2 (SiO2=5:2:2) The second wiring 102A and the third wiring 102B are selectively etched to remove the oxide semiconductor layer 10 The cross-sectional view at this stage is shown in FIG.

[0059] In addition, depending on the etching conditions, the oxide semiconductor The exposed areas of the layer may be etched. In that case, the second wiring 102A and the third wiring 102B are The oxide semiconductor layer 103 in the region sandwiched between the wirings 102B is formed on the first wiring 101 by the second wiring 102B. The thickness of the oxide semiconductor layer is thinner than that of the oxide semiconductor layer in the region where the line 102A and the third wiring 102B overlap. do.

[0060] Next, the gate insulating film 113, the oxide semiconductor layer 103, the second wiring 102A, the third wiring An oxide insulating layer 114 is formed on the oxide semiconductor layer 102B. The first wiring 101 is in contact with the oxide insulating layer 114 with the gate insulating film 113 interposed therebetween. A region of the oxide semiconductor layer 103 overlapping with the first insulating film 104 serves as a channel formation region.

[0061] The oxide insulating layer 114 has a thickness of at least 1 nm and is formed by an oxide method such as a sputtering method. The insulating layer can be formed by any suitable method that does not allow impurities such as water and hydrogen to be mixed into the insulating layer. In this embodiment mode, a silicon oxide film is formed as the oxide insulating layer by a sputtering method. The substrate temperature during film formation may be set to room temperature or higher and 300° C. or lower. In this embodiment, the substrate temperature is set to 100° C. The silicon oxide film is formed by sputtering in a rare gas (typically argon) atmosphere. In air, oxygen, or a mixture of rare gas (typically argon) and oxygen, The target may be a silicon oxide target or a silicon target. For example, a silicon target can be used under an oxygen and rare gas atmosphere. A silicon oxide film can be formed by sputtering. The oxide insulating layer formed in contact with the dielectric layer is resistant to moisture, hydrogen ions, and OH - Contains impurities such as First, an inorganic insulating film is used to block these substances from entering from the outside, typically an oxide film. A silicon film, a silicon nitride oxide film, an aluminum oxide film, an aluminum oxide nitride film, or the like is used. Note that the oxide insulating layer formed by sputtering is particularly dense, and impurities may enter the adjacent layer. It can be used as a single layer as a protective film to suppress the phenomenon of phosphorus diffusion. Using a target doped with phosphorus (P) or boron (B), phosphorus (P) or boron (B) is added to the oxide insulating layer. B) can also be added.

[0062] In this embodiment, a columnar polycrystalline B-doped silicon target (resistance value 0 The distance between the substrate and the target (TS distance) was 89 mm, and the pressure was Pulse was measured under an oxygen atmosphere (oxygen flow rate 100%) with a pressure of 0.4 Pa and a direct current (DC) power of 6 kW. The film is formed by DC sputtering. The film thickness is 300 nm.

[0063] Note that the oxide insulating layer 114 is provided over and in contact with a region that serves as a channel formation region of the oxide semiconductor layer. It also functions as a channel protection layer.

[0064] Next, a second heat treatment (preferably at 200° C. or higher and 400° C. or lower, for example at 250° C. or higher and 3 50°C or less) may be carried out under an inert gas atmosphere or a nitrogen gas atmosphere. For example, A second heat treatment is performed at 250° C. for 1 hour in a nitrogen atmosphere. The oxide semiconductor layer 103 is heated in a state where a part of the oxide semiconductor layer 103 is in contact with the oxide insulating layer 114 .

[0065] The oxide semiconductor layer 103 whose resistance has been reduced by the first heat treatment is in contact with the oxide insulating layer 114. When the second heat treatment is performed in this state, the region in contact with the oxide insulating layer 114 becomes an oxygen-excess state. As a result, the oxide semiconductor layer 103 is oxidized from a region in contact with the oxide insulating layer 114. The semiconductor layer 103 is made I-type (high resistance) in the depth direction.

[0066] Next, an opening 121 is formed in the oxide insulating layer 114 by a fourth photolithography process. The conductive film having light-transmitting properties is formed by forming a conductive film having light-transmitting properties. Indium (In2O3) and indium oxide tin oxide alloy (In2O3-SnO2, IT The conductive film is formed by sputtering or vacuum deposition. Another material for the conductive film is the Al-Zn-O film containing nitrogen, i.e. the Al-Zn-ON film. Alternatively, a Zn-O-based film containing nitrogen or a Sn-Zn-O-based film containing nitrogen may be used. The composition ratio (atomic %) of zinc in the Al-Zn-ON film is 47 atomic % or less. The composition ratio of aluminum in the film (atomic percent) is larger than the composition ratio of aluminum in the film (atomic percent). %) is larger than the composition ratio of nitrogen (atomic %) in the film. It is done with a hydrochloric acid-based solution. However, ITO etching is particularly prone to leaving residues, so Indium oxide-zinc oxide alloy (In2O3-ZnO) to improve etching processability may also be used.

[0067] The composition ratio of the light-transmitting conductive film is expressed in atomic percent. (EPMA:Electron Probe X-ray MicroAnalyzer ) will be used for the evaluation.

[0068] Next, a fifth photolithography step is performed to form a resist mask and perform etching. The unnecessary portions are removed to form the pixel electrode 105. The cross-sectional view at this stage is shown in FIG. As shown in.

[0069] In this way, a pixel having a thin film transistor 106 can be fabricated. These are arranged in a matrix to correspond to each pixel, forming a pixel section, which allows active The present invention can be used as one of the substrates for manufacturing a liquid crystal display device of a sub-matrix type. For the sake of convenience, this document refers to such a substrate as an active matrix substrate.

[0070] In an active matrix type liquid crystal display device, pixels arranged in a matrix are By driving the element electrodes, a display pattern is formed on the screen. A voltage is applied between the pixel electrode and the counter electrode corresponding to the pixel electrode, The liquid crystal layer disposed between the pixel electrode and the counter electrode is optically modulated, and this optical modulation is reflected by the display panel. A display element such as a liquid crystal element is provided on the pixel electrode 105. do.

[0071] The advantages of the configuration of this embodiment described with reference to FIGS. 1 and 2 will now be described with reference to FIGS. 3(A) and 3(B). A detailed explanation will be given below.

[0072] 3A and 3B are enlarged views of the oxide semiconductor layer and its vicinity in the top view of FIG. In addition, the width of the oxide semiconductor layer 103 in FIG. 3A (W1 in FIG. 3A) is increased. The diagram shows the width of the oxide semiconductor layer 103 (W2 in FIG. 3B) in FIG. handle.

[0073] In the top view of the pixel in FIG. 1A in this embodiment mode, as shown in FIGS. In addition, an oxide semiconductor is formed on the first wiring 101 without branching the wiring from the first wiring 101. The second wiring 102A and the third wiring 102B are formed in the oxide semiconductor layer. A channel region formed between the first wiring 101 and the second wiring 102 is formed in an overlapping region on the first wiring 101. The oxide semiconductor layer 103 has a channel region that is irradiated with light, and the TFT characteristics are varied. In order to prevent this, the wiring branched from the first wiring 101 is used to ensure light shielding. This is a factor that reduces the aperture ratio of the pixel. An oxide semiconductor layer is provided so as to overlap with the first wiring 101, and a By not forming wiring, the aperture ratio can be improved. By using a light-transmitting oxide semiconductor layer as the semiconductor layer, is formed in a region shifted from the region overlapping with the first wiring 101 to a position different from the designed position, Even if it overlaps with the electrode 105, display can be performed without reducing the aperture ratio. Cut.

[0074] By forming an oxide semiconductor layer with a pattern larger than a predetermined size, Even if the oxide semiconductor layer is formed at a position that is out of alignment with the substrate, there is no problem in terms of malfunction and a decrease in aperture ratio. Therefore, the active matrix of the liquid crystal display device can provide a good display without any distortion. This makes it easier to manufacture risk boards and improves yields.

[0075] As described above, by using the structure described in this embodiment, a thin film using an oxide semiconductor When manufacturing a pixel having a film transistor, the aperture ratio can be improved. As a result, a liquid crystal display device having a high-definition display portion can be obtained.

[0076] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is.

[0077] (Embodiment 2) An example of configuring pixels of a display device having a TFT configuration different from that of the above embodiment will be described below.

[0078] A top view of a pixel having a structure different from that of the embodiment mode 1 is shown in FIG. The TFT structure shown in Fig. 1 is a bottom gate structure, and the channel is The source and drain electrodes of the TFT are formed on the opposite side of the oxide semiconductor layer that will become the gate region. A so-called inverted staggered configuration having line layers is shown.

[0079] A pixel 400 shown in FIG. 4A includes a first wiring 401 functioning as a scan line, The second wiring 402A, the oxide semiconductor layer 403, the capacitance line 404, and the pixel electrode 405 are In addition, a third insulating film for electrically connecting the oxide semiconductor layer 403 and the pixel electrode 405 is provided. The first wiring 401 has a thin film transistor 406. The second wiring 402A also functions as the gate of the transistor 406. The third wiring 402B also functions as one of a source electrode and a drain electrode. The wiring that functions as the other of the source electrode or drain electrode and one electrode of the storage capacitor. The capacitor line 404 is a wiring that functions as the other electrode of the storage capacitor.

[0080] The first wiring 401 and the capacitance line 404 are provided in the same layer, and the second wiring 402A and the The third wiring 402B is provided in the same layer. The third wiring 402B and the capacitance line 404 are They are partially overlapped to form a storage capacitor for the liquid crystal element. The oxide semiconductor layer 403 of the gate electrode 406 is formed on the first wiring 401 by a gate insulating film (not shown). The oxide semiconductor layer 403 is provided with the first wiring 401 interposed therebetween. It is provided outside the area.

[0081] FIG. 4B shows a cross-sectional structure between dashed lines A1 and A2 in FIG. In the cross-sectional structure shown in FIG. 4(B), a gate electrode is formed on a substrate 411 via an undercoat film 412. The first wiring 401 and the capacitance line 404 are provided. A gate insulating film 413 is provided so as to cover the line 404. An oxide semiconductor layer 403 is provided on the second wiring 402. In addition, an oxide semiconductor layer 403, a second wiring 402A, and a third wiring 402B are provided. An oxide film functioning as a passivation film is provided on the wiring 402A and the third wiring 402B. An oxide insulating layer 414 is provided. An opening is formed in the oxide insulating layer 414. In the opening, the pixel electrode 405 and the third wiring 402B are connected. The wiring 402B and the capacitance line 404 form a capacitance element with the gate insulating film 413 as a dielectric. is.

[0082] The pixels shown in FIGS. 4A and 4B are the same as those described in FIGS. 1A and 1B of the first embodiment. Similarly, a plurality of pixels 701 arranged in a matrix on a substrate 700 in FIG. The explanation regarding FIG. 7 is the same as that in the first embodiment.

[0083] The cross-sectional view shown in FIG. 4B is the same as the cross-sectional view shown in FIG. 1B. The method is the same as that explained in FIG. 2 in the first embodiment.

[0084] The advantages of the configuration of this embodiment described with reference to FIGS. 4(A) and 4(B) are shown in FIGS. ) will be used for a detailed explanation.

[0085] 5A and 5B are enlarged views of the oxide semiconductor layer and its vicinity in the top view of FIG. 4A. In addition, the width of the oxide semiconductor layer 403 in FIG. 5A (W1 in FIG. 5A) is increased. The photograph corresponds to the width (W2 in FIG. 5B) of the oxide semiconductor layer 403 in FIG. handle.

[0086] In the top view of the pixel in FIG. 4(A) in this embodiment, as shown in FIGS. In addition, an oxide semiconductor is formed on the first wiring 401 without branching the wiring from the first wiring 401. The second wiring 402A and the third wiring 402B are formed in the oxide semiconductor layer. A channel region formed between the first wiring 401 and the second wiring 402 is formed in an overlapping region on the first wiring 401. In addition, in this embodiment, the oxide semiconductor layer 403 serves as a gate insulator over the first wiring 401. The insulating film extends to contact the second wiring 402A and the third wiring 402B. The semiconductor layer 403 has a channel region that is irradiated with light, causing variations in the TFT characteristics. Therefore, it is necessary to reliably block light by using wiring branched from the first wiring 401. This has also been a factor in reducing the aperture ratio of the pixel. An oxide semiconductor layer is provided so as to overlap with the first wiring 401, and a wiring branched from the first wiring 401 is formed. The first wiring 401 is not connected to the gate insulating film, and the second wiring 402A is connected to the gate insulating film. The third wiring 402B is in contact with the oxide semiconductor layer 403, thereby improving the aperture ratio. In addition, a light-transmitting oxide semiconductor layer can be used as a semiconductor layer of a thin film transistor. By using the second wiring 402, the oxide semiconductor layer 402 can be moved from a region overlapping with the first wiring 401 to a region at a design position. Even if the pixel electrode 405 overlaps the pixel electrode 405, the aperture ratio is not reduced. The display can be performed without any need for a display.

[0087] In addition, the second wiring 402A and the third wiring 402B extending over the first wiring 401 shown in FIG. The second wiring 402B may be provided so as to overlap the first wiring 401. The third wiring 402A and the third wiring 402B may be routed in a meandering manner. The wiring may be arranged in a straight line.

[0088] By forming an oxide semiconductor layer with a pattern larger than a predetermined size, Even if the oxide semiconductor layer is formed at a position that is out of alignment with the substrate, there is no problem in terms of malfunction and a decrease in aperture ratio. Therefore, the active matrix of the liquid crystal display device can provide a good display without any distortion. This makes it easier to manufacture risk boards and improves yields.

[0089] As described above, by using the structure described in this embodiment, a thin film using an oxide semiconductor When manufacturing a pixel having a film transistor, the aperture ratio can be improved. As a result, a liquid crystal display device having a high-definition display portion can be obtained.

[0090] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is.

[0091] (Embodiment 3) An example of configuring pixels of a display device having a TFT configuration different from that of the above embodiment will be described below.

[0092] A top view and a cross-sectional view of a pixel having a structure different from that of the second embodiment are shown in FIG. The structure shown in the top view of FIG. 6(A) is the same as that shown in FIG. 4(A). The structure shown in the cross-sectional view of FIG. 6B is the same as that shown in the cross-sectional view of FIG. The difference from the previous structure is that an insulating layer 601A is provided between the first wiring 401 and the second wiring 402A. and an insulating layer 601 is provided between the first wiring 401 and the third wiring 402B. In FIG. 6C, the dashed line B1-B2 in FIG. 4, an insulating layer 601 is provided between the capacitance line 404 and the second wiring 402A. A configuration having A is shown.

[0093] A second wiring 402A and a third wiring 402B are extended on the first wiring 401 and the capacitance line 404. In the case where the first wiring 401 and the second wiring 402 are provided in a separated state, depending on the thickness of the gate insulating film 413, Between the wiring 402A, the first wiring 401 and the third wiring 402B, and between the capacitance line 404 and the second Therefore, a parasitic capacitance is generated between the wiring 402A and the wiring 402B. As shown in FIG. 1, the insulating layers 601A and 601B are provided to reduce parasitic capacitance and prevent errors. It is possible to reduce malfunctions, etc.

[0094] As described above, by using the structure described in this embodiment, a thin film using an oxide semiconductor When manufacturing a pixel having a film transistor, the aperture ratio can be improved. In this embodiment, in addition to the configuration of the second embodiment, it is possible to reduce parasitic capacitance. Therefore, the liquid crystal display device has a high-definition display portion and is capable of reducing malfunctions. It is possible.

[0095] (Embodiment 4) In this embodiment, a pixel configuration and pixel operation that can be applied to a liquid crystal display device will be described. explain.

[0096] FIG. 8A is a diagram showing an example of a pixel configuration that can be applied to a liquid crystal display device. The pixel includes a transistor 881, a liquid crystal element 882, and a capacitor element 883. A gate of the transistor 881 is electrically connected to a wiring 885. A first terminal of the transistor 881 is The second terminal of the transistor 881 is electrically connected to the first terminal of the liquid crystal element 882. The second terminal of the liquid crystal element 882 is electrically connected to the wiring 887. A first terminal of the capacitor 883 is electrically connected to a first terminal of the liquid crystal element 882. The second terminal of the element 883 is electrically connected to the wiring 886 .

[0097] The wiring 884 can function as a signal line. The signal line is a line that receives an input from outside the pixel. The wiring 885 functions as a scanning line. The scan line is a wiring for controlling the on / off of the transistor 881. The wiring 886 can function as a capacitor line. This is the wiring for applying a certain voltage to the two terminals. The transistor 881 acts as a switch. The capacitor 883 can function as a storage capacitor. The storage capacitor keeps applying the signal voltage to the liquid crystal element 882 even when the switch is off. The wiring 887 can function as a counter electrode. The counter electrode is a wiring for applying a predetermined voltage to the second terminal of the liquid crystal element 882. The functions that each wiring can have are not limited to these, and each wiring can have various functions. For example, by changing the voltage applied to the capacitance line, the The voltage can also be adjusted.

[0098] FIG. 8B is a diagram showing an example of a pixel configuration that can be applied to a liquid crystal display device. 8A, the pixel configuration example shown in FIG. 8B is different from the pixel configuration example shown in FIG. In addition, the second terminal of the liquid crystal element 882 and the second terminal of the capacitance element 883 are electrically connected. Except for this difference, the pixel configuration example shown in FIG. 8(A) is the same as that shown in FIG. The pixel configuration example shown in FIG. 8B is particularly suitable for liquid crystal elements in a lateral electric field mode (IPS mode, FFS This is applicable when the liquid crystal element is in the lateral electric field mode. In this case, the second terminal of the liquid crystal element 882 and the second terminal of the capacitance element 883 are formed on the same substrate. Therefore, the second terminal of the liquid crystal element 882 and the second terminal of the capacitor element 883 can be electrically connected to each other. This is because it is easy to efficiently connect the pixels as shown in FIG. Since the wiring 887 can be omitted, the manufacturing process can be simplified and the manufacturing cost can be reduced. This can reduce the

[0099] The pixel configuration shown in FIG. 8(A) or FIG. 8(B) can be arranged in a matrix. In this way, a display section of a liquid crystal display device is formed, and various images can be displayed. FIG. 9A shows a pixel configuration in which a plurality of pixels shown in FIG. 8A are arranged in a matrix. The circuit configuration shown in FIG. 9A is a circuit diagram showing a case where a display unit includes a plurality of pixels. The figure shows four pixels extracted from the i-th column and j-th row (i and j are natural numbers). The pixel located at is represented as pixel 880_i,j, and the pixel 880_i,j is connected to a wiring 884 _i, wiring 885_j, and wiring 886_j are electrically connected to each other. For 880_i+1,j, wiring 884_i+1, wiring 885_j, wiring 886_j Similarly, for the pixel 880_i,j+1, The pixel 880_j+1 is electrically connected to the wiring 885_j+1 and the wiring 886_j+1. For i+1, j+1, wiring 884_i+1, wiring 885_j+1, wiring 886_j Each wiring is electrically connected to +1 by multiple pixels belonging to the same column or row. In the pixel configuration shown in FIG. Since the counter electrode is common to all pixels, the wiring 887 is The notation using natural numbers i or j will not be used. Therefore, even in the configuration in which the wiring 887 is shown, the wiring 887 is not essential and can be omitted by being shared with other wiring, etc.

[0100] The pixel configuration shown in FIG. 9(A) can be driven in various ways. The LCD is driven by a method called "burn-in" which prevents deterioration of the LCD element. FIG. 9B shows a case where dot inversion driving, which is one of the AC driving methods, is performed. The timing chart of the voltage applied to each wiring in the pixel configuration shown in FIG. This is a diagram showing a gate in which AC driving is performed by performing dot inversion driving. In this case, the flickering that is visible can be suppressed. , a signal 985_j input to a wiring 885_j, a signal 985_j input to a wiring 885_j+1 85_j+1, a signal 984_i input to the wiring 884_i, and a signal 984_i input to the wiring 884_i+1 9 shows the signal 984_i+1 being supplied to the line 886, and the voltage 986 being supplied to the line 886.

[0101] In the pixel configuration shown in FIG. 9A, in a pixel electrically connected to the wiring 885_j, The switch in the jth gate selection period in one frame period is in the selected state (on state). During the other periods, the gate is in a non-selected state (off state). After the jth gate selection period, the j+1th gate selection period is provided. In this manner, sequential scanning is performed. In this way, all pixels are selected in sequence within one frame period. In the timing chart, when the voltage is high (high level), the switch in the pixel When the voltage is low (low level), the switch is in a non-selected state.

[0102] In the timing chart shown in FIG. 9B, the jth gate in the kth frame (k is a natural number) During the port selection period, a positive signal voltage is applied to the wiring 884_i used as a signal line, A negative signal voltage is applied to the wiring 884_i+1. In one gate selection period, a negative signal voltage is applied to the wiring 884_i. A positive signal voltage is applied to +1. After that, each signal line is As a result, in the kth frame, a signal with the polarity inverted is applied to pixel 8. A positive signal voltage is applied to pixel 880_i,j, a negative signal voltage is applied to pixel 880_i+1,j, and a pixel 880 _i,j+1 has a negative signal voltage, and pixel 880_i+1,j+1 has a positive signal voltage. In the k+1th frame, In the kth frame, a signal voltage having a polarity opposite to that of the signal voltage written in the kth frame is written. As a result, in the k+1-th frame, the pixel 880_i,j has a negative signal voltage, A positive signal voltage is applied to pixel 880_i+1,j, a positive signal voltage is applied to pixel 880_i,j+1, A negative signal voltage is added to each of the elements 880_i+1, j+1. In the same frame, signal voltages of different polarities are applied to adjacent pixels. Furthermore, the polarity of the signal voltage in each pixel is inverted every frame. The dot inversion drive suppresses the deterioration of the liquid crystal element while displaying This can reduce flicker that is visible when the entire image or part of the image displayed is uniform. In addition, the following is added to all the wirings 886 including the wiring 886_j and the wiring 886_j+1: The voltage can be a constant voltage. The signal voltage is indicated only by polarity, but in reality, the polarity indicated varies The signal voltage value can be taken as the value. In this example, the polarity is inverted for each dot (pixel). However, the present invention is not limited to this, and the polarity can also be inverted for every several pixels. For example, by inverting the polarity of the signal voltage written every two gate selection periods, This reduces the power consumption required for writing. In addition, the polarity is inverted for each column. It is also possible to invert the polarity of each row (source line inversion) or to invert the polarity of each row (gate line inversion). It is also possible to invert the

[0103] Next, the liquid crystal element is a vertical alignment (VA) type, typically represented by MVA mode or PVA mode. A pixel configuration and a driving method thereof that are particularly preferable in the VA mode will be described. This LCD has many advantages, such as no rubbing process required during manufacturing, little light leakage during black display, and low driving voltage. However, the image quality deteriorates when the screen is viewed at an angle (the viewing angle is narrow). In order to widen the viewing angle in the VA mode, the following problems are solved: As shown in (B), a pixel configuration having multiple sub-pixels in one pixel is used. In the pixel configuration shown in FIG. 10(A) and FIG. 10(B), the pixel 1080 has two 10. An example of a case where the pixel includes two sub-pixels (a first sub-pixel 1080-1 and a second sub-pixel 1080-2). The number of sub-pixels in one pixel is not limited to two, and various numbers are possible. The larger the number of sub-pixels, the wider the viewing angle can be. The sub-pixels can have the same circuit configuration. The circuit configuration of the first subpixel 108 is the same as that shown in FIG. 0-1 includes a transistor 1081-1, a liquid crystal element 1082-1, and a capacitance element 1083-1. The connections of the respective components are in accordance with the circuit configuration shown in FIG. Similarly, the second subpixel 1080-2 includes a transistor 1081-2 and a liquid crystal element 1082- 2, and a capacitance element 1083-2, and the respective connections are as shown in FIG. This shall conform to the road configuration.

[0104] The pixel configuration shown in FIG. 10(A) is used as a scanning line for two sub-pixels that make up one pixel. There are two wires 1085 (wire 1085-1 and wire 1085-2) that are used as signal lines. The wiring 1084 is used as a capacitor line, and the wiring 1086 is used as a capacitor line. In this way, the signal line and the capacitance line are shared by two sub-pixels, The throughput can be improved and the signal line driver circuit can be simplified. This reduces manufacturing costs and the number of connections between the liquid crystal panel and the driver IC. The pixel configuration shown in FIG. 10B is a pixel configuration in which two sub-pixels make up one pixel. For each pixel, there is one wiring 1085 used as a scanning line, and one wiring 10 The wiring 1084 is used as a capacitance line. In this way, the scanning lines and the capacitance lines are divided into two sub-pixels. By sharing the same pixel, the aperture ratio can be improved and the total number of scanning lines can be reduced. This allows the gate line selection period per pixel to be sufficiently reduced even in high-resolution LCD panels. Therefore, the signal voltage can be appropriately written to each pixel.

[0105] 11(A) and 11(B) show the pixel configuration shown in FIG. 10(B) in which the liquid crystal element is This is an example that shows a schematic diagram of the electrical connection state of each element after replacing it with the shape of a pixel electrode. In FIG. 11(A) and FIG. 11(B), electrode 1088-1 represents the first pixel electrode. The electrode 1088-2 represents the second pixel electrode. The electrode 1088-1 corresponds to the first terminal of the liquid crystal element 1082-1 ​​in FIG. The pixel electrode 1088-2 corresponds to the first terminal of the liquid crystal element 1082-2 in FIG. That is, the first pixel electrode 1088-1 corresponds to the source of the transistor 1081-1. The second pixel electrode 1088-2 is electrically connected to one of the drain and the drain of the transistor 1. 11B, the source or drain of the transistor 081-2 is electrically connected to the transistor 081-3. In this embodiment, the connection relationship between the pixel electrode and the transistor is reversed. 88-1 is electrically connected to one of the source and drain of the transistor 1081-2. The second pixel electrode 1088-2 is connected to the source or drain of the transistor 1081-1. It is assumed that one of them is electrically connected.

[0106] In the pixel of this embodiment, by combining with the configuration of the above embodiment, In order to improve the aperture ratio, a pixel having a thin film transistor using a nitride semiconductor is manufactured. It is possible.

[0107] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is.

[0108] (Embodiment 5) In this embodiment, an electronic device including the liquid crystal display device described in the above embodiment is An example will be described.

[0109] FIG. 12A shows a portable game machine, which includes a housing 9630, a display unit 9631, and a speaker 9633. , operation keys 9635, a connection terminal 9636, a recording medium reading unit 9672, etc. The portable game machine shown in FIG. 12(A) can be used to play a program or data recorded on a recording medium. The function of reading the data and displaying it on the display unit, and the function of sharing information with other portable gaming machines through wireless communication The portable gaming machine shown in FIG. 12(A) has the following functions. The functions are not limited to these, and various functions can be provided.

[0110] FIG. 12B shows a digital camera, which includes a housing 9630, a display portion 9631, and a speaker 963 3, operation keys 9635, connection terminal 9636, shutter button 9676, image receiving unit 9677 , etc. The digital camera with a television receiving function shown in FIG. 12(B) can have the following: Functions for taking still images, shooting videos, and automatically or manually correcting captured images Functions, such as acquiring various information from the antenna, capturing images, or acquiring information from the antenna The function to save the captured information, the function to display the captured image or the information obtained from the antenna on the display. In addition, the digital camera with a television receiving function shown in FIG. The functions of the mobile camera are not limited to those described above, and the mobile camera may have a variety of functions.

[0111] FIG. 12C shows a television receiver, which includes a housing 9630, a display portion 9631, and a speaker 9633. , operation keys 9635, connection terminals 9636, etc. A television receiver has two functions: to process television radio waves and convert them into image signals, and to process image signals and It has functions such as converting signals suitable for display and converting the frame frequency of image signals. Note that the functions of the television receiver shown in FIG. 12(C) are not limited to these. It can have a variety of functions.

[0112] FIG. 13A shows a computer, which includes a housing 9630, a display portion 9631, and a speaker 9633. , operation keys 9635, connection terminals 9636, pointing devices 9681, external connection points The computer shown in FIG. 13A can store various information. The function to display images (still images, videos, text images, etc.) on the display, A function to control processing by a program, a communication function such as wireless communication or wired communication, The ability to connect to various computer networks using the communication function, The function of transmitting or receiving data can be provided. The functions possessed by the computer are not limited to those described above, and the computer may have a variety of functions.

[0113] Next, FIG. 13B shows a mobile phone, which includes a housing 9630, a display portion 9631, and a speaker 963. 3, operation keys 9635, microphone 9638, etc. The mobile phone shown in Figure 1 has the function of displaying various information (still images, videos, text images, etc.). A function to display the calendar, date, or time on the display, and to operate the information displayed on the display Or editing functions, functions to control processing by various software (programs), etc. Note that the functions of the mobile phone shown in FIG. 13B are not limited to these. It can have a variety of functions.

[0114] Next, FIG. 13C shows an electronic paper (also called an E-book). The electronic pen 9631 and the operation keys 9635 may be included. The user interface has the functions to display various information (still images, videos, text images, etc.), a calendar, , a function to display the date or time on the display unit, and a function to operate or edit the information displayed on the display unit Functions such as the ability to control processing using various software (programs) Note that the functions of the electronic paper shown in FIG. 13C are not limited to these. It can have a variety of functions.

[0115] The electronic device described in the present embodiment has a plurality of pixels constituting a display unit, each of which has an aperture ratio It is possible to improve the

[0116] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is. EXAMPLES

[0117] In this embodiment, to what extent a liquid crystal display device can be improved by using a thin film transistor including an oxide semiconductor layer We estimate how the aperture ratio of each pixel will be improved, and show the results.

[0118] In a thin film transistor having an oxide semiconductor, a gate is connected to the transistor to make the transistor non-conductive. The current that flows through the transistor when a voltage is applied (hereafter referred to as leakage current) is 0.1 pA. or less, whereas thin-film transistors using amorphous silicon have a current of several hundreds of nA. Therefore, in a thin film transistor having an oxide semiconductor, it is necessary to reduce the storage capacitance. That is, in a pixel provided with a thin film transistor having an oxide semiconductor, The aperture ratio is improved compared to pixels in which thin film transistors having amorphous silicon are provided. Here, we will roughly estimate how much the aperture ratio can be improved. The leakage current of a thin film transistor using an oxide semiconductor layer was set to 1×10 -13 (A) , the leakage current of a thin-film transistor using amorphous silicon is 1×10 -11 (A) The following explanation will be given assuming that this is the case.

[0119] Other parameters for estimating the pixel aperture ratio are the panel size of 3.4 inches and the The display has 256 gradations, the input voltage is 10V, and one frame is 1.66 x 10 - 2 The dielectric constant of the gate insulating film is set to 3.7 (F / m), and the Thickness 1×10 -7 This is explained as (m).

[0120] First, apply the above parameters to a panel with a pixel count of 540 x RGB x 960 (called the first panel). The area of ​​the storage capacitor and the aperture ratio when the method is applied are roughly estimated. The pixel size is 26 (μm) × 78 (μm), or 2.03 × 10 -9 (m 2 ) Of this, the area excluding the wiring and TFTs is 1.43 × 10 -9 (m 2 )and The area occupied by the wiring and TFT is 6.00×10 -10 (m 2 )

[0121] In order to provide a storage capacitor having a minimum required capacitance value in the first panel, The pixel has a thin-film transistor that can detect 4.25 x 10 -14 (F). In this case, The required capacitance area is 1.30×10 -10 (m 2 ) and the ratio of the area of ​​the storage capacitor to the pixel is The ratio of aperture is 64.0%. To make a storage capacitor with a capacitance, a thin film transistor having amorphous silicon is used. With 4.25 x 10 pixels -12 (F). In this case, the required capacity area is 1.3 0×10 -8 (m 2 ), the ratio of the area of ​​the storage capacitor to the pixel is 639.9(%), That is, a storage capacitance larger than the size of the pixel is required.

[0122] In addition, the above parameters are set on a panel with a pixel count of 480 x RGB x 640 (called the second panel). The area of ​​the storage capacitor and the aperture ratio when the above are applied are roughly estimated. In this case, the pixel size is 36 (μm) × 108 (μm), or 3.89 × 10 -9 (m 2 )and Of this, the area excluding the area occupied by wiring and TFT is 3.29 × 10 -9 (m 2 ), and the area occupied by the wiring and TFT is 6.00×10 -10 (m 2 )

[0123] In order to provide a storage capacitor having a minimum required capacitance value in the second panel, The pixel has a thin-film transistor that can detect 4.25 x 10 -14 (F). In this case, The required capacitance area is 1.30×10 -10 (m 2 ) and the ratio of the area of ​​the storage capacitor to the pixel is The ratio of aperture is 3.3% and the aperture ratio is 81.2%. To make a storage capacitor with a capacitance, a thin film transistor having amorphous silicon is used. With 4.25 x 10 pixels -12(F). In this case, the required capacity area is 1.3 0×10 -8 (m 2 ), the ratio of the area of ​​the storage capacitor to the pixel is 333.8(%), That is, a storage capacitance larger than the size of the pixel is required.

[0124] In the first and second panels described above, a thin-film transistor having an oxide semiconductor layer is Since the leakage current of the capacitor is very small, the capacitance line for forming the storage capacitance can be omitted. Specifically, the top view and the cross-sectional view of the case where the capacitance line is omitted are shown in FIG. 14A and 14B are diagrams showing the pixel configuration of the pixel shown in FIG. 14A. The pixel shown in FIG. 14A is the pixel shown in FIG. This corresponds to a top view of FIG. 1(A) with the capacitance lines omitted. As can be seen from the top view and the cross-sectional view in FIG. 14B, a thin film having an oxide semiconductor layer is formed. By using a transistor, the area occupied by the pixel electrode 105 can be expanded. In other words, the aperture ratio can be improved. Also, as can be seen from the cross-sectional view shown in FIG. By using a thin film transistor having an oxide semiconductor layer, a capacitance line can be reduced and Since the area occupied by the electrode 105 can be expanded, the aperture ratio can be improved. In addition, under the conditions of the first panel in FIG. 14(A) and (B), the aperture ratio is 70 0.4(%). Also, the second panel in Fig. 14(A) and (B) Under the conditions described above, the aperture ratio can be improved to 84.5%.

[0125] As explained above, the higher the resolution of the panel, the more the oxide semiconductor becomes necessary to improve the aperture ratio. It can be seen that there are great advantages to using a conductor layer in a thin film transistor. [Explanation of symbols]

[0126] 100 pixels 101 Wiring 102 Wiring 103 Oxide semiconductor layer 104 Capacitive Line 105 Pixel electrode 106 Thin Film Transistor 111 Substrate 112 Base film 113 Gate insulating film 114 Oxide insulating layer 121 Opening 400 pixels 401 Wiring 402 Wiring 403 Oxide semiconductor layer 404 Capacitive Line 405 Pixel electrode 406 Thin Film Transistor 411 Substrate 412 Base film 413 Gate insulating film 414 Oxide insulating layer 700 Substrates 701 pixels 702 Pixel section 703 Scanning line driver circuit 704 Signal line driver circuit 880 pixels 881 Transistor 882 Liquid crystal element 883 Capacitive element 884 Wiring 885 Wiring 886 Wiring 887 Wiring 984 signal 985 signal 986 Voltage 102A Wiring 102B Wiring 1080 pixels 1081 Transistor 1082 Liquid crystal element 1083 Capacitive element 1084 Wiring 1085 Wiring 1086 Wiring 1088 pixel electrode 402A Wiring 402B Wiring 601A Insulation layer 601B Insulating layer 9630 Case 9631 Display section 9633 Speaker 9635 Operation Key 9636 Connection terminal 9638 Microphone 9672 Recording medium reading unit 9676 Shutter button 9677 Image receiving unit 9680 External connection port 9681 Pointing Device

Claims

1. A pixel portion including at least a first transistor and a second transistor, a first conductive layer electrically connected to one of a source and a drain of the first transistor and one of a source and a drain of the second transistor, the first conductive layer having a region extending in a first direction; a first oxide semiconductor layer including a channel formation region of the first transistor; a second oxide semiconductor layer including a channel formation region of the second transistor; a second conductive layer having a region located under the first oxide semiconductor layer and functioning as a gate of the first transistor; a third conductive layer having a region in contact with the first oxide semiconductor layer and functioning as the other of the source and the drain of the first transistor; a first insulating layer having a region overlying the third conductive layer; a fourth conductive layer having a region in contact with an upper surface of the third conductive layer in the opening of the first insulating layer and functioning as a first pixel electrode; a fourth conductive layer that does not overlap with the first oxide semiconductor layer and that overlaps with the second oxide semiconductor layer in a plan view;

2. A pixel portion including at least a first transistor and a second transistor, a first conductive layer electrically connected to one of a source and a drain of the first transistor and one of a source and a drain of the second transistor, the first conductive layer having a region extending in a first direction; a first oxide semiconductor layer including a channel formation region of the first transistor; a second oxide semiconductor layer including a channel formation region of the second transistor; a second conductive layer having a region located under the first oxide semiconductor layer and functioning as a gate of the first transistor; a third conductive layer having a region in contact with the first oxide semiconductor layer and functioning as the other of the source and the drain of the first transistor; a first insulating layer having a region overlying the third conductive layer; a fourth conductive layer having a region in contact with an upper surface of the third conductive layer in the opening of the first insulating layer and functioning as a first pixel electrode; In a plan view, the fourth conductive layer does not overlap with the first oxide semiconductor layer and overlaps with the second oxide semiconductor layer; A display device, wherein a channel length direction of the first transistor intersects with the first direction.

Citation Information

Patent Citations

  • Image display device

    JP1984005229A

  • Thin film transistor display board and liquid crystal display device including the same

    JP2005018079A

  • Manufacturing method of transistor array substrate, and transistor array substrate

    JP2005077822A

  • Multiple domain thin film transistor display board and liquid crystal display device including same

    JP2006085133A

  • Electro-optical device, electronic equipment, and method for manufacturing electro-optical device