Light-emitting element
By using a thermally activated delayed phosphor and a fluorescent material in a light-emitting element, the challenge of low luminous efficiency in organic light-emitting elements is addressed, achieving enhanced light emission through efficient energy transfer between excited states.
Patent Information
- Application Number
- JP2024137765
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2012-08-03
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing light-emitting elements using organic compounds face challenges in achieving high luminous efficiency due to the difficulty in designing materials that can efficiently convert triplet excited states to singlet excited states, which is crucial for enhancing photon quantum efficiency.
Incorporating a thermally activated delayed phosphor (TADF) as an energy donor and a material that emits fluorescence as an energy acceptor, allowing for efficient energy transfer from triplet excited states to singlet excited states, thereby increasing luminous efficiency.
This configuration results in a light-emitting element with higher luminous efficiency by effectively converting triplet excited states to singlet excited states, leading to improved light emission.
Smart Images

Figure 2024161528000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a light-emitting element that uses an organic compound as a light-emitting substance. [Background technology]
[0002] In recent years, electroluminescence (EL) Research and development of light-emitting devices using this material is currently underway. The basic structure of these light-emitting devices is as follows: A layer containing a light-emitting substance (EL layer) is sandwiched between a pair of electrodes. When a voltage is applied to this element, By this, it is possible to obtain light emission from the light emitting substance.
[0003] Since these light-emitting elements are self-luminous, the pixels have higher visibility than LCD displays. This has the advantage that it does not require a backlight, and is therefore favored as a flat panel display element. In addition, displays using such light-emitting elements can be manufactured to be thin and lightweight. Both of these are major advantages. Another feature is the extremely fast response speed.
[0004] These light emitting devices can form the light emitting layer in a film shape, so that light can be emitted in a planar manner. Therefore, a light source with a large area can be easily formed. This is a feature that is difficult to obtain with point light sources such as bulbs and LEDs, or linear light sources such as fluorescent lights. Therefore, it is highly useful as a surface light source for lighting and other applications.
[0005] An organic EL device that uses an organic compound as a light-emitting material and has an EL layer containing the light-emitting material between a pair of electrodes. In the case of an L element, by applying a voltage between a pair of electrodes, electrons flow from the cathode and positive electrons flow from the anode. The holes are then injected into the EL layer, which emits light, causing a current to flow. The recombination of electrons and holes causes the light-emitting organic compound to enter an excited state, Light can be emitted from the light-emitting organic compound.
[0006] There are two types of excited states that organic compounds can form: singlet excited states and triplet excited states. Emission from the singlet excited state (S1) is fluorescence, and emission from the triplet excited state (T1) is phosphorus. The statistical generation ratio of light in a light-emitting element is S1:T1=1: 3. Therefore, it is possible to convert the triplet excited state into luminescence. 2. Description of the Related Art In recent years, light-emitting devices using phosphorescent compounds have been actively developed.
[0007] However, most of the phosphorescent compounds currently in use contain rare elements such as iridium. It is a complex with a metal as the central metal, and there are concerns about its cost and stability of supply.
[0008] This material is capable of converting part of the triplet excited state into light emission without using rare metals. Research is also being conducted on materials that emit delayed fluorescence as a means of emitting delayed fluorescence. A singlet excited state is generated from the doublet excited state by reverse intersystem crossing, and the singlet excited state emits light. will be converted.
[0009] In Patent Document 1 and Patent Document 2, thermally activated delayed fluorescence (TADF) Materials that emit induced delayed fluorescence It has been disclosed. [Prior art documents] [Patent documents]
[0010] [Patent Document 1] JP 2004-241374 A [Patent Document 2] JP 2006-24830 A Summary of the Invention [Problem to be solved by the invention]
[0011] However, in order to increase the luminous efficiency of the light-emitting element, the triplet excited state must be converted to the singlet excited state. Not only can it generate fluorescein, but it can also efficiently emit light from the singlet excited state. It is important that the photon efficiency is high. Therefore, in the configuration of the above-mentioned Patent Document 1, etc. In order to increase the luminescence efficiency, a material that emits TADF and has a high fluorescence quantum yield is required. However, it is extremely difficult to design a material that satisfies both of these requirements at the same time.
[0012] In view of the above, in one embodiment of the present invention, a light-emitting element using a material that emits fluorescence as a light-emitting substance is Another object is to provide a light-emitting element with higher luminous efficiency. [Means for solving the problem]
[0013] In order to achieve the above object, in one aspect of the present invention, a method for generating a singlet excited state from a triplet excited state is provided. The function of forming the singlet excited state and the function of efficiently obtaining light emission from the singlet excited state are assigned to different materials. It was decided.
[0014] More specifically, the light-emitting layer is provided with a compound capable of generating a singlet excited state from a triplet excited state. The material is mixed with a material that can efficiently emit light from a singlet excited state. Ta.
[0015] Materials that can generate a singlet excited state from a triplet excited state include those with thermal activation delay A phosphor is applied.
[0016] In this specification and the like, a thermally activated delayed fluorescent substance is a fluorescent substance that is converted from a triplet excited state to a reverse excited state by thermal activation. Thermally activated delayed fluorescent substances are materials that can generate a singlet excited state by photocrossing. Like materials that emit TADF, materials that independently emit triplet excited states can be converted to singlet excited states by reverse intersystem crossing. The material may include materials that can generate states and form exciplexes. It may also include a combination of the two materials.
[0017] Thermally activated delayed fluorescent materials are materials whose triplet excited state and singlet excited state are close to each other. More specifically, the difference in the energy levels between the triplet excited state and the singlet excited state is within 0.2 eV. In other words, materials that can emit TADF light independently from a triplet excited state to an inverse triplet excited state are preferred. The triplet and singlet excited states in materials that can generate singlet excited states by electron-electron crossing The difference in the levels of the triplet excited state and the singlet excited state in the exciplex is within 0.2 eV. It is preferable that the difference in state levels is within 0.2 eV.
[0018] As a material that can efficiently emit light from a singlet excited state, a known fluorescent material is suitable. Among them, materials with high fluorescence quantum yield, for example, materials with fluorescence quantum yield of 50% or more, are used. It is preferable that
[0019] As described above, one embodiment of the present invention uses a thermally activated delayed fluorescent substance as an energy donor, and The present invention provides a light-emitting device using a material that emits fluorescence as a light acceptor. The thermal activation delay is in the longest wavelength absorption band of the singlet excited state of the fluorescent material. By overlapping the emission spectra of the thermally activated delayed fluorescent substance, the singlet excited state of the thermally activated delayed fluorescent substance can be obtained. The energy of the fluorescing material can be transferred to the singlet excited state of the fluorescing material. From part of the triplet excited state energy of the thermally activated delayed fluorescent substance, A doublet excited state can also be generated and transferred to a singlet excited state of a fluorescent material.
[0020] For example, in the case of using a TADF-emitting material as an energy acceptor, light emission To increase efficiency, a material that emits TADF and has a high fluorescence quantum yield is required. However, as described above, the structure in which a thermally activated delayed fluorescent substance is used as the energy donor By doing so, the energy acceptor has a high fluorescence quantum yield, regardless of whether TADF is present or not. Therefore, it is possible to select the best material.
[0021] Therefore, the singlet excited state of thermally activated delayed fluorescent substances and the triplet excited state of thermally activated delayed fluorescent substances are The singlet excited state of the thermally activated delayed fluorescent substance is generated from a part of the energy of the excited state, and the fluorescent substance emits fluorescence. This allows the light to be more efficiently emitted via the singlet excited state of the emitting material. As a result, a light-emitting element with higher luminous efficiency can be obtained.
[0022] One embodiment of the present invention includes a pair of electrodes and an EL layer sandwiched between the pair of electrodes. The light-emitting layer includes at least a thermally activated delayed phosphor and a material that emits fluorescence. The light emitting element also includes
[0023] In the above, the thermally activated delayed fluorescent substance includes a first organic compound and a second organic compound. The first organic compound and the second organic compound may be combined to form an exciplex. preferable.
[0024] In the above, the lowest energy absorption band of the fluorescent material and the thermal activation delay It is preferred that the emissions of the phosphors overlap.
[0025] In the above, the peak wavelength of the absorption band on the lowest energy side of the fluorescent material, The difference in energy equivalent between the emission peak wavelength of the thermally activated delayed phosphor is 0.2 eV or less. It is preferred.
[0026] In the above, the peak wavelength of the emission of the thermally activated delayed phosphor and the emission of the material emitting fluorescence are It is preferable that the difference from the peak wavelength of the light is within 30 nm.
[0027] In the above, one of the first organic compound and the second organic compound has an electron transporting property. It is preferable that the first material be a material having a hole transporting property and the other be a material having a hole transporting property.
[0028] In the above, one of the first organic compound and the second organic compound is a π-electron deficient complex. It is preferred that one is an aromatic amine and the other is a π-electron rich heteroaromatic or aromatic amine. Effect of the Invention
[0029] According to one embodiment of the present invention, in a light-emitting element using a material that emits fluorescence as a light-emitting substance, A light emitting element with higher light efficiency can be provided. [Brief description of the drawings]
[0030] [Figure 1] 1 is a conceptual diagram of a light-emitting element. [Diagram 2] FIG. 2 is a diagram showing energy transfer in a light-emitting layer. [Diagram 3] A conceptual diagram of a lighting device. [Figure 4] FIG. 1 is a conceptual diagram of a passive matrix light-emitting device. [Diagram 5]FIG. 1 is a conceptual diagram of an active matrix light-emitting device. [Figure 6] FIG. 1 is a conceptual diagram of an active matrix light-emitting device. [Figure 7] A diagram showing an electronic device. [Figure 8] FIG. [Figure 9] 1 is a diagram illustrating an in-vehicle display device and an electronic device. [Figure 10] FIG. 2 is a diagram illustrating the emission wavelength of an exciplex. [Figure 11] FIG. 2 shows the structures of a light-emitting element 1 and a comparative light-emitting element 1 of Example 1. [Figure 12] FIG. 13 shows voltage-luminance characteristics of the light-emitting element 1 of Example 1 and the comparative light-emitting element 1. [Figure 13] FIG. 13 shows luminance-current efficiency characteristics of the light-emitting element 1 of Example 1 and the comparative light-emitting element 1. [Figure 14] FIG. 13 shows luminance-power efficiency characteristics of the light-emitting element 1 of Example 1 and the comparative light-emitting element 1. [Figure 15] FIG. 1 shows luminance vs. external quantum efficiency of the light-emitting element 1 of Example 1 and the comparative light-emitting element 1. [Figure 16] FIG. 13 shows voltage-luminance characteristics of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. [Figure 17] FIG. 13 shows luminance-current efficiency characteristics of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. [Figure 18] FIG. 13 shows voltage-current characteristics of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. [Figure 19] FIG. 13 shows luminance-power efficiency characteristics of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. [Figure 20] FIG. 13 shows luminance-external quantum efficiency characteristics of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. [Figure 21] 13 shows emission spectra of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. FIG. [Figure 22] 13 shows the results of a reliability test of the light-emitting element 2 of Example 2 and the comparative light-emitting element 2. FIG. [Figure 23] FIG. 13 shows voltage-luminance characteristics of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. [Figure 24] FIG. 13 shows luminance-current efficiency characteristics of the light-emitting element 3 and the comparative light-emitting element 3 of Example 3. [Diagram 25] 13 shows voltage-current characteristics of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. [Figure 26] FIG. 13 shows luminance-power efficiency characteristics of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. [Figure 27] FIG. 13 shows luminance vs. external quantum efficiency characteristics of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. [Figure 28] 13 shows emission spectra of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. FIG. [Figure 29] 13 shows the results of a reliability test of the light-emitting element 3 of Example 3 and the comparative light-emitting element 3. FIG. [Diagram 30] FIG. 13 shows voltage-luminance characteristics of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 31] FIG. 13 shows luminance-current efficiency characteristics of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 32] FIG. 13 shows voltage-current characteristics of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 33] FIG. 13 shows luminance-power efficiency characteristics of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 34] FIG. 13 shows luminance-external quantum efficiency characteristics of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 35] FIG. 13 shows emission spectra of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. [Diagram 36] 13 shows the results of a reliability test of the light-emitting element 4 of Example 4 and the comparative light-emitting element 4. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Hereinafter, the embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the above description, and the form and details are not limited thereto without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made. It should not be construed as being limited to the description of the embodiment modes.
[0032] (Embodiment 1) In a light-emitting device using a mixture of a thermally activated delayed phosphor and a material that emits fluorescence, Light emission occurs through such an energy process.
[0033] (1) A material that emits fluorescence when electrons and holes recombine in the material. becomes excited (direct recombination process).
[0034] (1-1) When the excited state of a fluorescent material is a singlet excited state: Fluorescence is emitted. (1-2) When the excited state of the fluorescent material is a triplet excited state: Thermal deactivation occurs.
[0035] In the direct recombination process (1) above, if the fluorescence quantum efficiency is high, high luminescence efficiency can be obtained. The singlet excited state level of the thermally activated delayed fluorescent substance is the same as that of the fluorescent material. It is preferable that the level is higher than the level of the excited state.
[0036] (2) Electrons and holes recombine in the thermally activated delayed phosphor to form a thermally activated delayed phosphor. When the photobody is in an excited state (energy transfer process).
[0037] (2-1) When the excited state of the thermally activated delayed fluorescent substance is a singlet excited state The level of the singlet excited state of the thermally activated delayed fluorescent substance is the same as that of the singlet excited state of the fluorescent material. When the excitation energy is higher than the threshold value, the excitation energy is transferred from the thermally activated delayed fluorescent material to the fluorescent material. The fluorescent material enters a singlet excited state. The material emits fluorescence. The material emits fluorescence from the singlet excited state of the thermally activated delayed fluorescent material. Energy transfer to the triplet excited state level of a fluorescent material is similar to the singlet excited state of a fluorescent material. Since direct transitions from the ground state to the triplet excited state are forbidden, the main energy transfer is This is not a thermal activation process, so we will omit it here. Singlet excited state of delayed fluorescent substance ( 1 H * ) to the singlet excited state ( 1 G * ) is important (wherein 1 G is the singlet ground state of the fluorescent material , 1 H represents the singlet ground state of the thermally activated delayed fluorescent substance).
[0038] 1 H * + 1 G → 1 H+ 1 G * (2-1)
[0039] (2-2) When the excited state of the thermally activated delayed fluorescent substance is a triplet excited state The singlet excited state level of a thermally activated delayed fluorescent substance is the singlet excited state level of a fluorescent material. When the temperature is higher than 1000° C., light emission occurs through the following process. First, the triplet state of the thermally activated delayed fluorescent material The excited state level is converted to the singlet excited state level of the thermally activated delayed fluorescent material by reverse intersystem crossing. The excitation energy is transferred. Then, the thermally activated delayed fluorescent substance emits fluorescence from the singlet excited state. The excitation energy is transferred to the singlet excited state level of the fluorescent material, and the fluorescent material is A fluorescent material that is in a singlet excited state emits fluorescence.
[0040] That is, as shown in the following formula (2-2), the triplet excited state ( 3 H * )from The singlet excited state of thermally activated delayed fluorescent material ( 1 H * ) is generated, and then The singlet excited state of a fluorescent material ( 1 G * ) energy is transferred to
[0041] 3 H * + 1 G →(reverse intersystem crossing) → 1 H * + 1 G → 1 H+ 1 G * (2-2)
[0042] If all the energy transfer processes described above in (2) occur efficiently, a thermally activated delayed fluorescent material will be obtained. A material that efficiently emits fluorescence with both triplet and singlet excitation energies. Singlet excited state ( 1 G * ), which allows for highly efficient light emission. Before the excitation energy is transferred from the thermally activated delayed fluorescent material to the fluorescent material, If the body itself is deactivated by releasing the excitation energy as light or heat, the luminous efficiency will decrease. It will be lowered.
[0043] Next, the intermolecular energy transfer process between the thermally activated delayed fluorescent substance and the fluorescent material described above The mechanism of energy transfer between molecules is the Förster mechanism. Two mechanisms have been proposed: the Dexter mechanism and the axial mechanism.
[0044] First, the first mechanism, the Förster mechanism (dipole-dipole interaction), is The transfer does not require direct contact between the molecules, and the thermally activated delayed fluorescent material and the fluorescent material This is the mechanism by which energy transfer occurs through the resonance phenomenon of dipole vibrations. The thermally activated delayed phosphor transfers energy to the fluorescent material, and the thermally activated delayed phosphor transfers energy to the fluorescent material. The delayed fluorescent material is in the ground state, and the fluorescent material is in the excited state. The rate constant of the mechanism, k h*→g is shown in Equation (1).
[0045]
number
[0046] In formula (1), ν represents the frequency, and f' h (ν) is the standard value of the thermally activated delayed phosphor The emission spectrum (fluorescence spectrum when discussing energy transfer from a singlet excited state) is calculated. When discussing energy transfer from triplet excited states, the spectrum is called phosphorescence spectrum. , ε g (ν) represents the molar extinction coefficient of the fluorescent material, N represents Avogadro's number, n is the refractive index of the medium, and R is the intermolecular distance between the thermally activated delayed fluorescent substance and the fluorescent material. where τ is the measured excited state lifetime (fluorescence lifetime or phosphorescence lifetime), and φ is the emission Quantum yield (fluorescence quantum yield when discussing energy transfer from singlet excited states, triplet excited When discussing energy transfer from an excited state, it stands for phosphorescence quantum yield, and K 2 is heat activated A coefficient (0 to 4) that represents the orientation of the transition dipole moment of a delayed fluorescent material and a fluorescent material. In the case of random orientation, K 2 =2 / 3.
[0047] The second mechanism, the Dexter mechanism (electron exchange interaction), produces thermally activated delayed fluorescence. When the body and the fluorescent material approach a contact distance where orbital overlap occurs, the excited state is thermally activated. Energy transfer occurs through the exchange of electrons between the slow-fluorescing phosphor and the ground-state fluorescent material. The rate constant of the Dexter mechanism is k h*→g is shown in formula (2).
[0048]
number
[0049] In formula (2), h is the Planck constant, and K is a constant with the dimension of energy. where ν is the frequency and f' is the h (ν) is the normalized emission spectrum of the thermally activated delayed phosphor. Spectra (fluorescence spectrum when discussing energy transfer from singlet excited states, triplet When discussing energy transfer from an excited state, it represents the phosphorescence spectrum, and ε' g (ν) represents the normalized absorption spectrum of the fluorescent material, and L represents the effective molecular radius. , R represents the intermolecular distance between the thermally activated delayed fluorescent substance and the fluorescent material.
[0050] Here, the efficiency of energy transfer from the thermally activated delayed fluorescent material to the fluorescent material Φ ET is a number It is considered to be expressed by equation (3). k r The emission process of thermally activated delayed fluorescent materials (singlet excitation) When discussing energy transfer from a state, consider energy transfer from fluorescence and triplet excited states. represents the rate constant of the photoluminescence (phosphorescence in the case of the photoelectron spectrometry), and k n is a non-radiative process of thermally activated delayed phosphors (thermal represents the rate constant of the excited state of the thermally activated delayed fluorescent substance measured. Represents lifespan.
[0051]
number
[0052] From equation (3), the energy transfer efficiency Φ ET To increase the rate of energy transfer, Constant k h*→g By increasing the other competing rate constants k r +k n (=1 / τ) is relatively small It turns out that the smaller it is, the better.
[0053] In both of the above energy transfer processes (2-1) and (2-2), the thermal activation delay The singlet excited state of the fluorescent substance ( 1 H * ) to the fluorescent material. Therefore, the mechanism is based on both the Förster mechanism (equation (1)) and the Dexter mechanism (equation (2)). Energy transfer is possible.
[0054] First, consider the energy transfer by the Förster mechanism. When the ET is the quantum yield φ (energy from the singlet excited state) Since we are talking about the transfer of light, it can be said that a higher fluorescence quantum efficiency is better. An important factor is the emission spectrum of the thermally activated delayed fluorescent substance (from the singlet excited state). Since we are discussing energy transfer, we will look at the fluorescence spectrum and the absorption spectrum of the fluorescent material. (absorption corresponding to the transition from the singlet ground state to the singlet excited state) (Note that it is also preferable that the molar absorption coefficient of the fluorescent material is high.) appears in the emission spectrum of thermally activated delayed fluorescent materials and on the longest wavelength side of fluorescent materials. This means that the absorption bands overlap.
[0055] Next, consider the energy transfer via the Dexter mechanism. According to equation (2), the rate constant k h *→g In order to increase the emission spectrum of the thermally activated delayed fluorescent material (emission from the singlet excited state), Since we are discussing energy transfer, we will use the fluorescence spectrum) and the absorption spectrum ( The larger the overlap with the absorption corresponding to the transition from the singlet ground state to the singlet excited state, the better. It is clear that...
[0056] From the above, the energy transfer efficiency is high in both processes (2-1) and (2-2). The efficiency is optimized by considering the emission spectrum of the thermally activated delayed phosphor and the longest wavelength of the fluorescent material. This is achieved by overlapping the absorption band appearing on the other side of the absorption band.
[0057] However, in order to increase the luminous efficiency of the light-emitting element, the thermally activated delayed phosphor must be in the triplet excited state. Not only can it generate a singlet excited state from the excited state, but it can also produce fluorescent materials with high fluorescence quantum yields. It is important that:
[0058] However, it is possible to generate a singlet excited state from a triplet excited state, and the fluorescence quantum Designing high yield materials is very difficult.
[0059] In addition, the proportion of the energy transfer process (2) is large, and the proportion of the direct recombination process (1) is small. It is preferable to use a lower temperature because this can reduce the thermal deactivation process of (1-2). The concentration of the fluorescent material is preferably 5 wt % or less, and more preferably 1 wt % or less.
[0060] Therefore, one aspect of the present invention is to improve the thermal activation delay when a fluorescent material is used as a light-emitting substance. The efficiency of energy transfer from the triplet excited state of the fluorescent substance to the fluorescent material, and the fluorescence This is a useful method to overcome the problems with the fluorescence quantum efficiency of singlet excited states of light-emitting materials. The specific aspects of the present invention will be described below.
[0061] In one embodiment of the present invention, an energy donor capable of efficiently transferring energy to a fluorescent material is provided. The present invention provides a light-emitting device using a thermally activated delayed phosphor as a light-emitting element. The singlet excited state and the triplet excited state are characterized by being close to each other. In thermally activated delayed fluorescent materials, the transition from the triplet excited state to the singlet excited state is easy to occur. Furthermore, the most important absorption of the singlet excited state of the fluorescent material, which is the energy acceptor, is The absorption band on the long wavelength side (the absorption corresponding to the transition from the singlet ground state to the singlet excited state) By overlapping the emission spectrum of the thermally activated delayed fluorescent substance, the triplet state of the thermally activated delayed fluorescent substance Energy transfer from excited and singlet excited states to the singlet excited state of fluorescent materials Dynamic efficiency can be improved.
[0062] In addition, it has the function of generating a singlet excited state from a triplet excited state and the function of efficiently generating a singlet excited state. By assigning this function to a different material, the effect of delayed thermal activation as a luminescent material can be achieved. Regardless of the presence or absence of fluorescein, select a material with a high fluorescence quantum yield (e.g., a material with a fluorescence quantum yield of 50% or more). You can choose.
[0063] As a result, the energies of the triplet excited state and the singlet excited state of the thermally activated delayed fluorescent substance can be converted more efficiently into emission via the singlet excited state of the fluorescent material, A light-emitting element with high luminous efficiency can be obtained.
[0064] In the light-emitting element having the above-mentioned structure, efficient energy transfer occurs as shown in FIG. In FIG. 2, a light-emitting layer 113 is provided between an electrode 101 and an electrode 102. Optional layers may be present between each electrode and the light-emitting layer 113. Singlet excited state S of the slowly fluorescing phosphor 113D D From the figure, the singlet excited state of the luminescent material 113A is S A In addition, the triplet excited state T of the thermally activated delayed phosphor 113D D is the singlet excited state S of the thermally activated delayed phosphor 113D. D After reverse intersystem crossing, the luminescent material Singlet excited state S of substance 113A A Energy transfer occurs to the luminescent material 113A. Singlet excited state S A Thus, in the light-emitting element according to the present embodiment, The ability to generate a singlet excited state from a triplet excited state and efficiently emit light from the singlet excited state By assigning the function of obtaining the desired energy and the function of emitting the desired light to different materials, the energy transfer and the emission can be achieved, respectively. This is well performed, and a light-emitting element with high luminous efficiency can be provided.
[0065] FIG. 1 shows a conceptual diagram of a light-emitting element in this embodiment. 1(B) and 1(C) are enlarged views of only the light-emitting layer 113. FIG.
[0066] The light-emitting element includes an EL layer 10 sandwiched between a pair of electrodes, a first electrode 101 and a second electrode 102. 3, and the EL layer 103 contains an organic compound as a light-emitting material. The light-emitting layer 113 includes a light-emitting material. The other layers are not limited, and any other layers may be used. A typical laminate structure includes a hole injection layer 111, a hole transport layer 112, and an electron transport layer 114. , electron injection layer 115, etc. In addition, a carrier block layer, etc. may be provided, A plurality of light-emitting layers may be provided.
[0067] The light-emitting layer 113 contains a thermally activated delayed phosphor 113D and a light-emitting material 113A. As shown in FIG. 1(B), the thermally activated delayed fluorescent substance 113D can be inverted from the triplet excited state by itself. The material may be capable of generating a singlet excited state by intersystem crossing. The phosphor 113D may be made of a plurality of materials. As described above, the first organic compound 113D1 and the second organic compound 113D2 are mixed together. It is particularly noted that the combination of these compounds forms an exciplex. An exciplex is the difference between the levels of a singlet excited state and a triplet excited state. Since the triplet excited state tends to become very small, Therefore, the first organic compound that forms an exciplex is easily transferred to the level of the The thermally activated delayed fluorescent substance constituted by combining the compound and the second organic compound is In one embodiment, the thermally activated delayed fluorescent substance is most suitable. If one of the organic compounds is a hole transport material and the other is an electron transport material, the first organic compound By adjusting the mixing ratio of the first organic compound and the second organic compound, the hole and electron Since it is easy to optimize the carrier balance, it is highly reliable in terms of light emission efficiency. In addition, in the light-emitting element of this embodiment, the light-emitting layer 113 contains other substances. Do not exclude the fact that it is included.
[0068] A thermally activated delayed fluorescent substance is in a state in which its singlet excited state and triplet excited state are close to each other. However, in particular, the energy difference between the singlet excited state and the triplet excited state is 0 eV or more and 0.2 eV or less. It is preferable that:
[0069] Furthermore, the thermally activated delayed fluorescent substance and the fluorescent material can be used as the thermally activated delayed fluorescent substance as described above. This is a combination in which the emission of the light source overlaps with the absorption band on the longest wavelength side of the light-emitting material 113A. This makes it possible to emit fluorescence from the singlet excited state of the thermally activated delayed fluorescent substance. Energy is efficiently transferred to the singlet excited state of the material being excited.
[0070] Examples of the fluorescent material that can be used as the luminescent material 113A include the following: Examples include: 5,6-bis[4-(10-phenyl-9-anthryl) phenyl]-2,2'-bipyridine (abbreviation: PAP2BPy), 5,6-bis[4'-( 10-phenyl-9-anthryl)biphenyl-4-yl]-2,2'-bipyridine (abbreviation Name: PAPP2BPy), N,N'-bis[4-(9-phenyl-9H-fluorene-9 -yl)phenyl]-N,N'-diphenyl-pyrene-1,6-diamine (abbreviation: 1,6 FLPAPrn), N,N'-bis[4-(9H-carbazol-9-yl)phenyl] -N,N'-diphenylstilbene-4,4'-diamine (abbreviation: YGA2S), 4-( 9H-Carbazol-9-yl)-4'-(10-phenyl-9-anthryl)triphenyl Nylamine (abbreviation: YGAPA), 4-(9H-carbazol-9-yl)-4'-(9 ,10-diphenyl-2-anthryl)triphenylamine (abbreviation: 2YGAPPA), N,9-diphenyl-N-[4-(10-phenyl-9-anthryl)phenyl]-9H -Carbazole-3-amine (abbreviation: PCAPA), Perylene, 2,5,8,11-tetradecane La-tert-butylperylene (abbreviation: TBP), 4-(10-phenyl-9-anthracene 4'-(9-phenyl-9H-carbazol-3-yl)triphenylamine (abbreviation Name: PCBAPAP), N,N''-(2-tert-butylanthracene-9,10-di N,N',N'-triphenyl-1,4-phenylene)bis[N,N',N'-triphenyl-4,1-phenylene] N,9-diphenyl-N-[4-(9,10-diphenyldiamine] (abbreviation: DPABPA), 2P CAPPA), N-[4-(9,10-diphenyl-2-anthryl)phenyl]-N, N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPPA), N ,N,N',N',N'',N'',N''',N'''-Octaphenyldibenzo[g ,p]chrysene-2,7,10,15-tetraamine (abbreviation: DBC1), coumarin 30 , N-(9,10-diphenyl-2-anthryl)-N,9-diphenyl-9H-carba 2PCAPA, N-[9,10-bis(1,1'-biphenyl) N,9-diphenyl-9H-carbazole-3- Amine (abbreviation: 2PCABPhA), N-(9,10-diphenyl-2-anthryl)- N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPA), N-[9,10-bis(1,1'-biphenyl-2-yl)-2-anthryl]-N,N ',N'-Triphenyl-1,4-phenylenediamine (abbreviation: 2DPABPhA), 9 ,10-Bis(1,1'-biphenyl-2-yl)-N-[4-(9H-carbazole- 9-yl)phenyl]-N-phenylanthracen-2-amine (abbreviation: 2YGABPh A) N,N,9-triphenylanthracene-9-amine (abbreviation: DPhAPhA) Marine 545T, N,N'-diphenylquinacridone, (abbreviation: DPQd), rubrene, 5,12-bis(1,1'-biphenyl-4-yl)-6,11-diphenyltetracene (abbreviation: BPT), 2-(2-{2-[4-(dimethylamino)phenyl]ethenyl}- 6-Methyl-4H-pyran-4-ylidene)propanedinitrile (abbreviation: DCM1), 2 -{2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5H-benzo[i j]Quinolizin-9-yl)ethenyl]-4H-pyran-4-ylidene}propanidine DCM2, N,N,N',N'-tetrakis(4-methylphenyl) ... Helical-5,11-diamine (abbreviation: p-mPhTD), 7,14-diphenyl-N,N ,N',N'-Tetrakis(4-methylphenyl)acenaphtho[1,2-a]fluoran p-mPhAFD, 2-{2-isopropyl-6- [2-(1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H- Benzo[ij]quinolizin-9-yl)ethenyl]-4H-pyran-4-ylidene}pro Pandinitrile (abbreviation: DCJTI), 2-{2-tert-butyl-6-[2-(1, 1,7,7-Tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij ]Quinolizin-9-yl)ethenyl]-4H-pyran-4-ylidene}propanedinitri (abbreviation: DCJTB), 2-(2,6-bis{2-[4-(dimethylamino)phenyl ]ethenyl}-4H-pyran-4-ylidene)propanedinitrile (abbreviation: BisDCM ), 2-{2,6-bis[2-(8-methoxy-1,1,7,7-tetramethyl-2,3 ,6,7-Tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)ethenyl ]-4H-pyran-4-ylidene}propanedinitrile (abbreviation: BisDCJTM), etc. Examples include:
[0071] The concentration of the above-mentioned fluorescent material in the light-emitting layer 113 is preferably 5 wt % or less, and more preferably 1 wt % or less. The following is more preferable. By setting the concentration in this range, the ratio of the energy transfer process of (2) Increasing the ratio of the direct recombination process (1) and decreasing the thermal deactivation process (1-2) It is possible.
[0072] For example, the thermally activated delayed phosphor consists of one material, for example, can be used.
[0073] First, there are fullerene and its derivatives, acridine derivatives such as proflavine, and eosin. In addition, magnesium (Mg), zinc (Zn), cadmium (Cd), tin (Sn), Metal-containing polyimide including platinum (Pt), indium (In), or palladium (Pd) Examples of the metal-containing porphyrin include the following structural formula: Protoporphyrin-tin fluoride complex (SnF2(Proto IX)), mesoporphyrin Hematoporphyrin-Tin Fluoride Complex (SnF2(Meso IX)), Hematoporphyrin-Fluoride Tin complex (SnF2(Hemato IX)), coproporphyrin tetramethyl ester Ter-tin fluoride complex (SnF2(Copro III-4Me)), octaethylpor Ethioporphyrin-tin fluoride complex (SnF2(OEP)), etioporphyrin-tin fluoride complex (SnF2(Etio I)), octaethylporphyrin-platinum chloride complex (PtCl 2OEP) etc.
[0074] [ka]
[0075] In addition, as a thermally activated delayed phosphor composed of one material, 2-(Biphenyl-4-yl)-4,6-bis(12-phenylindolo[2,3-a] Carbazol-11-yl)-1,3,5-triazine (PIC-TRZ) and other π-electron-permeable Heterocyclic compounds having a π-deficient heteroaromatic ring and a π-electron deficient heteroaromatic ring can also be used. Since the heterocyclic compound has a π-electron rich heteroaromatic ring and a π-electron deficient heteroaromatic ring, The π-electron-rich heteroaromatic ring and the π-electron-rich heteroaromatic ring are preferably used because they have high electron transport properties and hole transport properties. In the case of a substance in which a π-deficient heteroaromatic ring is directly bonded, the donor property of the π-electron rich heteroaromatic ring and the π-electron The acceptor properties of the deficient heteroaromatic rings are both strong, and the levels of the singlet excited state and the triplet excited state This is particularly preferable since the difference in the state levels becomes small.
[0076] [ka]
[0077] In addition, as the thermally activated delayed fluorescent substance, two kinds of excitation light of the first organic compound and the second organic compound are used. A combination of organic compounds that form a complex can be used. In this case, a known carrier can be used. Although a suitable transport material can be used, in order to efficiently form an exciplex, a material that accepts electrons must be used. Compounds that easily take up holes (materials with electron transport properties) and compounds that easily accept holes (materials with hole transport properties) It is particularly preferable to combine the material with a material having a high conductivity.
[0078] This is because a material having electron transport properties and a material having hole transport properties are combined and thermally activated. A mixture of a material having electron transport properties and a material having hole transport properties is used as a slow phosphor. By adjusting the combination ratio, the carrier balance between holes and electrons in the light-emitting layer can be optimized. This is because it is easy to optimize the carrier balance between holes and electrons in the light-emitting layer. This makes it possible to suppress the occurrence of a bias in the region where recombination of electrons and holes occurs in the light-emitting layer. By suppressing the bias in the region where the overlapping occurs, the reliability of the light-emitting element can be improved.
[0079] Compounds that readily accept electrons (materials with electron transport properties) include π-electron-deficient heteroaromatic Aromatic groups and metal complexes can be used. Specifically, bis(10-hydroxybenzoxazole) [h]quinolinato) beryllium(II) (abbreviation: BeBq2), bis(2-methyl-8- Quinolinolato)(4-phenylphenolato)aluminum(III)(abbreviation: BAlq) , bis(8-quinolinolato)zinc(II) (abbreviation: Znq), bis[2-(2-benzoyl) bis[2-(2-benzoxazolyl)phenolato]zinc(II) (abbreviation: ZnPBO) Thiazolyl)phenolato]zinc(II) (abbreviation: ZnBTZ) and other metal complexes, 4-biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazide PBD, 3-(4-biphenylyl)-4-phenyl-5-(4-tert-butyl) t-Butylphenyl)-1,2,4-triazole (abbreviation: TAZ), 1,3-bis[5 -(p-tert-butylphenyl)-1,3,4-oxadiazol-2-yl]benzene Zene (abbreviation: OXD-7), 9-[4-(5-phenyl-1,3,4-oxadiazole -2-yl)phenyl]-9H-carbazole (abbreviation: CO11), 2,2',2''- (1,3,5-benzenetriyl)tris(1-phenyl-1H-benzimidazole) (Abbreviation: TPBI), 2-[3-(dibenzothiophen-4-yl)phenyl]-1-phenyl Polyazoles such as phenyl-1H-benzimidazole (abbreviation: mDBTBIm-II) Heterocyclic compounds with a 2-[3-(dibenzothiophen-4-yl)phenyl] skeleton Dibenzo[f,h]quinoxaline (abbreviation: 2mDBTPDBq-II), 2-[3'-( Dibenzothiophene-4-yl)biphenyl-3-yl]dibenzo[f,h]quinoxalate 2-[3'-(9H-carbazole-9-yl) 2mCzBPDB q), 4,6-bis[3-(phenanthren-9-yl)phenyl]pyrimidine (abbreviation: 4,6mPnP2Pm), 4,6-bis[3-(4-dibenzothienyl)phenyl]pyridine Heterocyclic compounds with diazine skeletons such as 4,6mDBTP2Pm-II and 3,5-bis[3-(9H-carbazol-9-yl)phenyl]pyridine (abbreviation :35DCzPPy), 1,3,5-tri[3-(3-pyridyl)phenyl]benzene ( Examples of the heterocyclic compounds having a pyridine skeleton include the above-mentioned heterocyclic compounds. Among them, heterocyclic compounds having a diazine skeleton and heterocyclic compounds having a pyridine skeleton have been shown to be reliable. In particular, heterocyclic compounds having a diazine (pyrimidine or pyrazine) skeleton are preferred. The cyclic compounds have high electron transport properties and contribute to reducing the driving voltage.
[0080] Compounds that easily accept holes (materials with hole transport properties) include π-electron-rich heteroaromatic Aromatic or aromatic amines can be suitably used. Specifically, 2-[N-(9- Phenylcarbazol-3-yl)-N-phenylamino]spiro-9,9'-bifluor PCASF, 4,4'-bis[N-(1-naphthyl)-N-phenylamine] N,N'-bis(3-methylphenyl)-N,N'-biphenyl (abbreviation: NPB) Diphenyl-[1,1'-biphenyl]-4,4'-diamine (abbreviation: TPD), 4,4 '-Bis[N-(spiro-9,9'-bifluoren-2-yl)-N-phenylamino] Biphenyl (abbreviation: BSPB), 4-phenyl-4'-(9-phenylfluorene-9- 4-phenyl-3'-(9-phenylyl)triphenylamine (abbreviation: BPAFLP), mBPAFLP, 4-phenyl -4'-(9-phenyl-9H-carbazol-3-yl)triphenylamine (abbreviation: PCBA1BP), 4,4'-diphenyl-4''-(9-phenyl-9H-carbazol PCBBi1BP), 4-(1-naphthyl)triphenylamine -4'-(9-phenyl-9H-carbazol-3-yl)triphenylamine (abbreviation: PCBANB), 4,4'-di(1-naphthyl)-4''-(9-phenyl-9H-carbazone) PCBNBB, 9,9-dimethyl- N-Phenyl-N-[4-(9-phenyl-9H-carbazol-3-yl)phenyl] -Fluorene-2-amine (abbreviation: PCBAF), N-phenyl-N-[4-(9-phenyl Nyl-9H-carbazol-3-yl)phenyl]-spiro-9,9'-bifluorene Compounds with aromatic amine skeletons such as 2-amine (abbreviation: PCBASF) and 1,3- Bis(N-carbazolyl)benzene (abbreviation: mCP), 4,4'-di(N-carbazolyl) ) Biphenyl (abbreviation: CBP), 3,6-bis(3,5-diphenylphenyl)-9-phenyl CzTP, 9-phenyl-9H-3-(9-phenyl-9 Carbazole skeleton such as H-carbazol-3-yl)carbazole (abbreviation: PCCP) Compounds with 4,4',4''-(benzene-1,3,5-triyl)tri(dibenzyl) 2,8-diphenyl-4-[4-(9- Phenyl-9H-fluoren-9-yl)phenyl]dibenzothiophene (abbreviation: DBT FLP-III), 4-[4-(9-phenyl-9H-fluoren-9-yl)phenyl ]-6-phenyldibenzothiophene (abbreviation: DBTFLP-IV) and other thiophene bone Compounds with the structure 4,4',4''-(benzene-1,3,5-triyl)tri(diphenylphosphine) Benzofuran) (abbreviation: DBF3P-II), 4-{3-[3-(9-phenyl-9H- Fluoren-9-yl)phenyl]phenyl}dibenzofuran (abbreviation: mmDBFFLB i-II) and other compounds having a furan skeleton. Compounds having an isidine skeleton and compounds having a carbazole skeleton have good reliability. This is preferable because it has a high hole transporting property and contributes to reducing the driving voltage.
[0081] The first organic compound and the second organic compound are not limited to these, and may be any compound that transports a carrier. and forming an exciplex, and the emission of the exciplex is a luminescent material. The longest wavelength absorption band in the absorption spectrum of As long as it overlaps with the absorption corresponding to the transition to the excited state, other known materials may be used. stomach.
[0082] Note that the first organic compound and the second organic compound are made of a material having an electron transporting property and a material having a hole transporting property. When constructing organic compounds, the carrier balance can be controlled by the mixture ratio. Specifically, the ratio of the first organic compound to the second organic compound is preferably in the range of 1:9 to 9:1. stomach.
[0083] Here, each compound forming an exciplex (first organic compound 113D1 and second organic compound 113D2) We will now explain in some detail about the compound 113D2) and exciplexes.
[0084] Figure 10(A) and Figure 10(B) show the emission spectra of the four organic compounds alone and the results obtained from them. The emission spectrum of the exciplex formed is shown in Fig. 1. In the figure, compound 1 is 2-[4-(di Benzothiophen-4-yl)phenyl]-1-phenyl-1H-benzimidazole ( Abbreviation: DBTBIm-II), compound 2 is 2-[3-(dibenzothiophen-4-yl) phenyl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTPDBq-II), Product 3 is 4,4',4''-tris[N-(1-naphthyl)-N-phenylamino]triphenylphosphine Compound 4 is 2,7-bis[N-(4-diphenylamine) N-phenylaminophenyl)-spiro-9,9'-bifluorene (abbreviation :DPA2SF). Excitplex 1 is the exciplex of compound 1 and compound 3, and exciplex 2 is the The exciplex of compound 2 and compound 3, and the exciplex of compound 3 and 4,4'-bis[N-(1-naphthalene) The exciplex with N-phenylamino]biphenyl (abbreviation: NPB) is 1 shows the spectrum of an exciplex of compound 2 and compound 4.
[0085] The structural formulas of each compound are shown below.
[0086] [ka]
[0087] FIG. 10(A) shows the emission spectra of exciplex 1, exciplex 2, and compounds 1 to 3. The spectrum represented by exciplex 1 is based on compound 1 and contains a small amount of compound 3. The emission of the added material was measured, and the spectrum represented by exciplex 2 contained compound 2. The results of measuring the luminescence of the material with a small amount of compound 3 added are shown below. In the sample in which the exciplex 1 was measured, either compound 1 or compound 3 was the first The first organic compound corresponds to 113D1, and the other corresponds to the second organic compound 113D2. In addition, in the sample in which the measurement of exciplex 2 was performed, either compound 2 or compound 3 was the first One corresponds to organic compound 113D1, and the other corresponds to second organic compound 113D2.
[0088] As can be seen from FIG. 10(A), even if the minor component, compound 3, is the same, exciplex 1 The difference between the emission from exciplex 1 and that from exciplex 2 is more than 100 nm. This makes it possible to easily adjust the emission wavelength of the exciplex.
[0089] In addition, the peak wavelength of the emission spectrum of exciplex 1 is about 520 nm. The thermally activated delayed fluorescent material containing the compound 3 is mixed with a material that emits blue-green to red fluorescence. It can be suitably used.
[0090] In addition, the peak wavelength of the emission spectrum of exciplex 2 is about 610 nm. The thermally activated delayed fluorescent material containing the compound 3 is preferably used in combination with a material that emits red fluorescence. There can be.
[0091] In FIG. 10(B), the emission spectra of exciplex 3 and exciplex 4 as well as compounds 2 and 4 are shown. The spectrum represented by exciplex 3 is based on compound 2 and contains a small amount of NPB. The emission of the added material was measured, and the spectrum represented by exciplex 4 contained compound 2. The results of measuring the luminescence of a material in which a small amount of compound 4 was added to the base are shown below. In the sample in which exciplex 3 was measured, either compound 2 or NPB was the first The first organic compound corresponds to the organic compound 113D1, and the second organic compound corresponds to the organic compound 113D2. In the sample in which the exciplex 4 was measured, either compound 2 or compound 4 was the first One corresponds to the organic compound 113D1, and the other corresponds to the second organic compound 113D2.
[0092] As can be seen from FIG. 10(B), even though the base material is the same, exciplex 3 and exciplex The difference in the emission of 4 is nearly 100 nm. That is, by changing the substance that is the minor component, It is also possible to easily adjust the emission wavelength of the exciplex by using the above method.
[0093] In addition, the peak wavelength of the emission spectrum of exciplex 3 is about 520 nm. The thermally activated delayed fluorescent material containing NPB is preferably mixed with a material that emits blue-green to red fluorescence. It can be used appropriately.
[0094] In addition, the peak wavelength of the emission spectrum of exciplex 4 is about 580 nm. The thermally activated delayed fluorescent material containing the compound 4 is mixed with a material that emits orange to red fluorescence. It can be suitably used.
[0095] The light-emitting element having the above-mentioned structure has a high efficiency of energy transfer to the fluorescent material. This is a light-emitting element with good luminous efficiency.
[0096] In addition, two organic compounds that form an exciplex as a thermally activated delayed fluorescent substance were used. In this case, it is also preferable that the driving voltage of the light-emitting element can be reduced. By using an exciplex, it is possible to realize a light-emitting element with low power consumption. The reason why the dynamic voltage can be reduced will be explained below.
[0097] When a combination of organic compounds that form an exciplex is used as a thermally activated delayed fluorescent substance, The threshold voltage at which exciplexes are formed by carrier recombination (or singlet excitons) is It is determined by the energy of the peak of the emission spectrum of the exciplex. For example, If the emission spectrum peaks at 620 nm (2.0 eV), the exciplex can be converted into an electric The threshold voltage required to form the energy is also about 2.0V.
[0098] Here, the energy of the peak in the emission spectrum of the exciplex is too high (the wavelength is too short) In this case, the threshold voltage for the formation of the exciplex also increases. To transfer energy to the light-emitting material and make the fluorescent material emit light, a larger This is not desirable because it requires a voltage and consumes extra energy. From the viewpoint, the lower the energy (longer the wavelength) of the peak in the emission spectrum of the exciplex, The threshold voltage becomes smaller, which is preferable.
[0099] Therefore, the peak wavelength of the emission spectrum of the exciplex is calculated by multiplying the absorption spectrum of the fluorescent material by If the wavelength is set to be equal to or longer than the peak wavelength of the absorption band located on the longest wavelength side of the light emitting element, a light emitting device with low driving voltage can be obtained. Even in this case, the emission spectrum of the exciplex and the absorption spectrum of the fluorescent material can be obtained. Energy transfer is possible by utilizing the overlap with the absorption band located at the longest wavelength side of the absorption spectrum. In this way, it is possible to obtain high light emission efficiency while reducing the driving voltage. By achieving high luminous efficiency (external quantum efficiency), high power efficiency can be achieved.
[0100] The light-emitting device has a threshold voltage at which a material that emits fluorescence due to carrier recombination begins to emit light. The threshold voltage at which exciplexes are formed by carrier recombination is smaller than the voltage at which the exciplexes are formed. In other words, the voltage applied to the light-emitting element is lower than the threshold voltage at which the fluorescent material begins to emit light. Even if the charge is not enough, carriers recombine to form exciplexes, and a recombination current flows through the light-emitting element. This allows the realization of a light-emitting device with a lower driving voltage (good voltage-current characteristics). It is possible.
[0101] This also allows the fluorescent material to emit light at a threshold voltage by the time it reaches that voltage. The regeneration of carriers that are present in the layer and can contribute to the emission of the fluorescent material. The binding is smooth and numerous. Therefore, the threshold voltage (luminescence onset) of the fluorescent material is The luminance increases sharply around the voltage at which light is emitted. Since the rise in the peak-to-peak range can be made steeper, the driving voltage required for the desired brightness can be reduced. In order to obtain practical brightness, the threshold voltage of the fluorescent material must be Since the device is driven at a voltage equal to or higher than the light emission start voltage, the light emitted by the fluorescent material is dominant. The light-emitting element can also achieve high current efficiency.
[0102] The effect of the above-mentioned voltage reduction is that the peak of the emission spectrum of the exciplex becomes closer to the emission spectrum of the fluorescent material. Within +30 nm of the peak of the optical spectrum, or the peak wavelength of the emission spectrum of the exciplex The difference in energy conversion value between the peak wavelength of the emission of the fluorescent material and the The emission spectrum of the exciplex is most notable in the region of the luminescence spectrum of the fluorescent material. Within 30 nm of the emission spectrum peak of the exciplex or within 30 nm of the emission spectrum peak of the exciplex The difference in energy between the wavelength of the fluorescent material and the peak wavelength of the fluorescent material is -0.2 eV or less. In the upper region, a relatively high luminous efficiency can be maintained.
[0103] (Embodiment 2) In this embodiment mode, a detailed structure example of the light-emitting element described in Embodiment Mode 1 will be described with reference to FIG. This is explained below.
[0104] The light-emitting element in this embodiment has an EL layer made of a plurality of layers between a pair of electrodes. In the embodiment, the light emitting element includes a first electrode 101, a second electrode 102, and a first electrode 103. The device is composed of a first electrode 101, a second electrode 102 and an EL layer 103 disposed between the first electrode 101 and the second electrode 102. In this embodiment, the first electrode 101 functions as an anode, and the second electrode 102 functions as a cathode. In other words, the first electrode 101 is closer to the second electrode 102 than the first electrode 103. When a voltage is applied between the first electrode 101 and the second electrode 102 so that the potential becomes higher than When the light is incident on the substrate, light emission is obtained.
[0105] Since the first electrode 101 functions as an anode, it is required to use a material having a large work function (specifically, 4.0 eV The above-mentioned metals, alloys, conductive compounds, and mixtures thereof are preferably used. Specifically, for example, indium oxide-tin oxide (ITO) n Oxide), indium oxide-tin oxide containing silicon or silicon oxide, acid Indium oxide containing zinc oxide, tungsten oxide and zinc oxide (I These conductive metal oxide films are usually formed by sputtering. The film is formed, but it may be produced by applying a sol-gel method or the like. Examples of the production method are Indium oxide-zinc oxide is made by adding 1 to 20 wt% zinc oxide to indium oxide. There is also a method of forming the film by sputtering using a target made of titanium oxide. Indium oxide containing zinc oxide and indium oxide (IWZO) has the following properties: A target containing 0.5-5wt% tungsten oxide and 0.1-1wt% zinc oxide. It can also be formed by sputtering using gold (Au), platinum (P t), Nickel (Ni), Tungsten (W), Chromium (Cr), Molybdenum (Mo), Iron (Fe), cobalt (Co), copper (Cu), palladium (Pd), or nitrogen in metallic materials Examples of the material include titanium nitride (e.g., titanium nitride). Graphene can also be used. By using a composite material described later for the layer in contact with the first electrode 101 in the EL layer 103, This allows the electrode material to be selected regardless of its work function.
[0106] Regarding the laminated structure of the EL layer 103, the light-emitting layer 113 has the same structure as that shown in the first embodiment. As long as the layer is a hole injection layer, a hole transport layer, a light emitting layer, an electron transport layer, etc., the other layers are not particularly limited. The layer can be constructed by appropriately combining a transport layer, an electron injection layer, a carrier blocking layer, an intermediate layer, etc. In this embodiment, the EL layer 103 is a hole injection layer laminated in order on the first electrode 101. The electron injection layer 111, the hole transport layer 112, the light emitting layer 113, the electron transport layer 114, and the electron injection layer 115 are The materials constituting each layer will be specifically described below.
[0107] The hole injection layer 111 is a layer containing a material with high hole injection properties. Umium oxide, ruthenium oxide, tungsten oxide, manganese oxide, etc. can be used. Other examples include phthalocyanine (abbreviated as HPc) and copper phthalocyanine (CuPC). Phthalocyanine compounds, 4,4'-bis[N-(4-diphenylaminophenyl) -N-phenylamino]biphenyl (abbreviation: DPAB), N,N'-bis{4-[bis( 3-Methylphenyl)amino]phenyl}-N,N'-diphenyl-(1,1'-biphenyl aromatic amine compounds such as diamine (DNTPD) or polyamines (Ethylenedioxythiophene) / Poly(styrenesulfonic acid) (PEDOT / PSS) The hole injection layer 111 can also be formed from a polymer such as
[0108] In addition, the hole injection layer 111 may be formed by adding an acceptor substance to a material having a hole transporting property. A composite material containing an acceptor substance can be used. By using a material having such a structure, it is possible to select a material for forming the electrode regardless of the work function of the electrode. In other words, not only a material with a large work function but also a material with a low work function can be used for the first electrode 101. This allows the use of materials with small numbers of acceptors. ,8,8-Tetracyano-2,3,5,6-tetrafluoroquinodimethane (abbreviation: F4- Examples of the nitriles include transition metal oxides. In addition, oxides of metals belonging to groups 4 to 8 of the periodic table can be mentioned. Specifically, vanadium oxide, niobium oxide, tantalum oxide, chromium oxide, molybdenum oxide, Libdenum oxide, tungsten oxide, manganese oxide, and rhenium oxide are preferred because of their high electron-accepting properties. Among them, molybdenum oxide is particularly stable in the air, has low hygroscopicity, and is easy to handle. Therefore, it is preferable.
[0109] As hole transporting substances used in the composite material, aromatic amine compounds and carbazole derivatives are , aromatic hydrocarbons, polymer compounds (oligomers, dendrimers, polymers, etc.), etc. The organic compound used in the composite material can be a hole It is preferable that the organic compound has high transportability. -6 cm 2 / Vs or more In the following, the hole transport in the composite material is preferably a material having a hole mobility of 100 nm or less. Specific examples of organic compounds that can be used as the functional substance are listed below.
[0110] For example, the aromatic amine compound is N,N'-di(p-tolyl)-N,N'-diphenyl Nyl-p-phenylenediamine (DTDPPA), 4,4'-bis[N-(4-diphenyl phenylaminophenyl)-N-phenylamino]biphenyl (abbreviation: DPAB), N, N'-Bis{4-[bis(3-methylphenyl)amino]phenyl}-N,N'-diphenyl Nyl-(1,1'-biphenyl)-4,4'-diamine (abbreviation: DNTPD), 1,3, 5-Tris[N-(4-diphenylaminophenyl)-N-phenylamino]benzene( Abbreviated as DPA3B).
[0111] Specific examples of carbazole derivatives that can be used in composite materials include 3-[N-( 9-Phenylcarbazol-3-yl)-N-phenylamino]-9-phenylcarbazo (abbreviation: PCzPCA1), 3,6-bis[N-(9-phenylcarbazole-3- yl)-N-phenylamino]-9-phenylcarbazole (abbreviation: PCzPCA2), 3-[N-(1-naphthyl)-N-(9-phenylcarbazol-3-yl)amino]- 9-phenylcarbazole (abbreviation: PCzPCN1) and the like.
[0112] Another carbazole derivative that can be used in composite materials is 4,4'-dicarbazole. (N-carbazolyl)biphenyl (abbreviation: CBP), 1,3,5-tris[4-(N-carbazolyl) 9-[4-(10-phenyl-9 -anthracenyl)phenyl]-9H-carbazole (abbreviation: CzPA), 1,4-bis [4-(N-carbazolyl)phenyl]-2,3,5,6-tetraphenylbenzene, etc. It can be used.
[0113] In addition, examples of aromatic hydrocarbons that can be used in the composite material include 2-tert- Butyl-9,10-di(2-naphthyl)anthracene (abbreviation: t-BuDNA), 2-t ert-Butyl-9,10-di(1-naphthyl)anthracene, 9,10-bis(3,5 -diphenylphenyl)anthracene (abbreviation: DPPA), 2-tert-butyl-9, 10-Bis(4-phenylphenyl)anthracene (abbreviation: t-BuDBA), 9,10 -Di(2-naphthyl)anthracene (abbreviation: DNA), 9,10-diphenylanthracene DPAnth, 2-tert-butylanthracene (t-BuAnth) h), 9,10-bis(4-methyl-1-naphthyl)anthracene (abbreviation: DMNA), 2-tert-Butyl-9,10-bis[2-(1-naphthyl)phenyl]anthracene , 9,10-bis[2-(1-naphthyl)phenyl]anthracene, 2,3,6,7-tetraphenyl tetramethyl-9,10-di(1-naphthyl)anthracene, 2,3,6,7-tetramethyl 10,10-di(2-naphthyl)anthracene, 9,9'-bianthryl, '-Diphenyl-9,9'-bianthryl, 10,10'-bis(2-phenylphenyl )-9,9'-bianthryl, 10,10'-bis[(2,3,4,5,6-pentaphenyl nyl)phenyl]-9,9'-bianthryl, anthracene, tetracene, rubrene, pentacene perylene, 2,5,8,11-tetra(tert-butyl)perylene, etc. In addition, pentacene, coronene, etc. can also be used. -6 c m 2 The aromatic hydrocarbon having a hole mobility of 14 to 42 carbon atoms is used. is more preferable.
[0114] The aromatic hydrocarbon that can be used in the composite material may have a vinyl skeleton. Examples of aromatic hydrocarbons having a vinyl group include 4,4'-bis(2,2-diphenyl ether). 9,10-bis[4-(2,2-diphenylvinyl)biphenyl (abbreviation: DPVBi) phenylvinyl)phenyl]anthracene (abbreviation: DPVPA), and the like.
[0115] In addition, poly(N-vinylcarbazole) (abbreviation: PVK) and poly(4-vinyltriphenyl PVTPA), poly[N-(4-{N'-[4-(4-diphenylamine N'-phenylamino)phenyl]phenyl-N'-phenylamino}phenyl)methacrylamide Name: PTPDMA), poly[N,N'-bis(4-butylphenyl)-N,N'-bis( It is also possible to use polymer compounds such as poly(phenyl)benzidine (abbreviation: Poly-TPD). Cut.
[0116] By forming the hole injection layer 111, the hole injection property is improved, and the driving voltage is small. It is therefore possible to obtain a light emitting element having a high light emitting property.
[0117] The hole transport layer 112 is a layer containing a material having a hole transport property. For example, 4,4'-bis[N-(1-naphthyl)-N-phenylamino]biphenyl (abbreviation: NPB) and N,N'-bis(3-methylphenyl)-N,N'-diphenyl-[ 1,1'-biphenyl]-4,4'-diamine (abbreviation: TPD), 4,4',4''-triphenyl Tris(N,N-diphenylamino)triphenylamine (abbreviation: TDATA), 4,4' ,4''-Tris[N-(3-methylphenyl)-N-phenylamino]triphenyla MIN (abbreviation: MTDATA), 4,4'-bis[N-(spiro-9,9'-bifluorene -2-yl)-N-phenylamino]biphenyl (abbreviation: BSPB), 4-phenyl-4 '-(9-Phenylfluoren-9-yl)triphenylamine (abbreviation: BPAFLP) The aromatic amine compounds described here have hole transport properties. High, mostly 10 -6 cm 2 The hole mobility is 1 / Vs or more. The organic compounds listed as the hole transporting material in the composite material can also be used for the hole transport layer 112. In addition, poly(N-vinylcarbazole) (abbreviation: PVK) and poly(4-vinyl Polymer compounds such as polyphenyltriphenylamine (PVTPA) can also be used. The layer containing the hole-transporting substance may be a single layer or a two-layer structure containing the above substance. A laminate of more than one may be used.
[0118] The light-emitting layer 113 is a layer that contains at least a light-emitting substance and a thermally activated delayed phosphor. Since the layer 113 has the structure described in the first embodiment, The light emitting element in the light emitting layer 113 can be a light emitting element with very good luminous efficiency. For the main configuration, please refer to the description in embodiment 1.
[0119] The light-emitting layer 113 having the above-mentioned structure can be formed by co-deposition in a vacuum deposition method or by using an indium ion as a mixed solution. It is produced by forming a film using the ink jet method, spin coating method, dip coating method, etc. It is possible.
[0120] The electron transport layer 114 is a layer containing a material having an electron transport property. For example, tris(8-oxo) Aluminum (Alq), tris(4-methyl-8-quinolinolato) Aluminum (abbreviation: Almq3), bis(10-hydroxybenzo[h]quinolinato) Beryllium (abbreviation: BeBq2), bis(2-methyl-8-quinolinolato)(4-phenyl Alphenolato)aluminum (abbreviation: BAlq), etc. The layer is made of a metal complex having a bis[2-(2-hydroxyphenyl)-2-pyridine skeleton. phenyl)benzoxazolato]zinc (abbreviation: Zn(BOX)2), bis[2-(2-phenyl oxazo[1,2-hydroxyphenyl]benzothiazolato[1,2-hydroxyphenyl]zinc (abbreviation: Zn(BTZ)2) Metal complexes having aryl or thiazole ligands can also be used. In addition to the complex, 2-(4-biphenylyl)-5-(4-tert-butylphenyl)-1 ,3,4-Oxadiazole (abbreviation: PBD) and 1,3-bis[5-(p-tert- butylphenyl)-1,3,4-oxadiazol-2-yl]benzene (abbreviation: OXD -7), 3-(4-biphenylyl)-4-phenyl-5-(4-tert-butylphenyl) 1,2,4-triazole (abbreviation: TAZ), bathophenanthroline (abbreviation: BP hen), vasocuproine (abbreviation: BCP), etc. can also be used. The material has high electron transport properties and is mainly -6 cm 2 / Vs or higher. The above-mentioned thermally activated delayed phosphor having electron transport properties may be used in the electron transport layer 114. stomach.
[0121] The electron transport layer 114 may be a single layer or a laminate of two or more layers of the above-mentioned materials. It may also be possible to use the above.
[0122] In addition, a layer for controlling the movement of electrons may be provided between the electron transport layer and the light emitting layer. The layer was made by adding a small amount of a substance with high electron trapping properties to a material with high electron transport properties. By suppressing the movement of electron carriers, it is possible to adjust the carrier balance. This type of structure can prevent problems caused by electrons penetrating the light-emitting layer. This is highly effective in suppressing deterioration (e.g., reduction in element life).
[0123] In addition, an electron injection layer is provided between the electron transport layer 114 and the second electrode 102 in contact with the second electrode 102. The electron injection layer 115 may be formed of lithium fluoride (LiF), Alkali metals such as cesium fluoride (CsF), calcium fluoride (CaF2), etc. Alkaline earth metals or compounds thereof can be used. For example, The layer made of the material contains an alkali metal or an alkaline earth metal or a compound thereof. Note that the electron-injecting layer 115 can be formed from a material having an electron-transporting property. By using a layer containing an alkali metal or an alkaline earth metal, This is more preferable because electron injection from the second electrode 102 can be performed efficiently.
[0124] The material for forming the second electrode 102 is preferably one having a small work function (specifically, 3.8 eV or less). Bottom) Metals, alloys, electrically conductive compounds, and mixtures thereof can be used. Specific examples of such cathode materials include alkali metals such as lithium (Li) and cesium (Cs). Lithium metals, as well as magnesium (Mg), calcium (Ca), strontium (Sr), etc. Elements belonging to Group 1 or 2 of the Periodic Table of the Elements and alloys containing these elements (MgAg, Rare earth metals such as AlLi), europium (Eu), ytterbium (Yb) and the like However, when the second electrode 102 and the electron transport layer are provided with By providing an electron injection layer, the material can be used in a variety of applications, regardless of the magnitude of the work function. Various conductive materials such as indium oxide-tin oxide containing silicon oxide or silicon oxide are used as the second It can be used as the electrode 102. These conductive materials can be formed by sputtering or ink deposition. The film can be formed by using a jet method, a spin coating method, or the like.
[0125] The EL layer 103 can be formed by a variety of methods, including dry and wet methods. For example, a vacuum deposition method, an ink jet method, a spin coating method, or the like can be used. Also, each electrode or each layer may be formed using a different film formation method.
[0126] The electrodes may be formed by a wet method using a sol-gel method, or by using a paste of a metal material. Alternatively, a dry method such as a sputtering method or a vacuum deposition method may be used. It may be formed by using.
[0127] The light-emitting element having the above-mentioned structure has a first electrode 101 and a second electrode 102. The potential difference causes a current to flow, and holes and electrons are generated in the light-emitting layer 113, which is a layer containing a light-emitting substance. In other words, a light emitting region is formed in the light emitting layer 113. It is composed of:
[0128] The light is emitted to the outside through either the first electrode 101 or the second electrode 102, or both. Therefore, either the first electrode 101 or the second electrode 102 Either or both of the first electrode 101 and the second electrode 102 are light-transmitting electrodes. In some cases, light is emitted through the first electrode 101. In other cases, light is emitted through only the second electrode 102. When the first electrode 102 is a light-transmitting electrode, the emitted light is extracted through the second electrode 102. When the first electrode 101 and the second electrode 102 are both light-transmitting electrodes, light is emitted. It passes through the first electrode 101 and the second electrode 102 and is taken out from both.
[0129] The structure of the layers provided between the first electrode 101 and the second electrode 102 is the same as that described above. However, it is not limited to the above. The first electrode 101 and the second electrode 102 are arranged so as to suppress quenching caused by the It is preferable to provide a light-emitting region where holes and electrons recombine at a location away from 02.
[0130] In addition, the hole transport layer and the electron transport layer in contact with the light emitting layer 113, particularly the light emitting region in the light emitting layer 113 The carrier transport layer, which is in contact with the side closer to the light-emitting region, transports energy from the excitons generated in the light-emitting layer. In order to suppress the band gap, the band gap is set to be larger than that of the luminescent material. It is preferable that the material used is one having a gap.
[0131] The light emitting element in this embodiment is provided on a substrate made of glass, plastic, metal, or the like. The substrate through which the light from the light emitting element passes is one that has high translucency in the visible light region. Regarding the order of fabrication on the substrate, the layers may be stacked in order from the first electrode 101 side. The light emitting device may be formed by forming one light emitting element on one substrate. A single light emitting element may be formed on one substrate, or a plurality of light emitting elements may be formed on one substrate. By fabricating multiple elements, it is possible to create lighting devices with separate elements and passive matrix light-emitting devices. Also, a thin film, for example, can be formed on a substrate made of glass, plastic, etc. A thin-film transistor (TFT) is formed, and a light-emitting element is fabricated on the electrode electrically connected to the TFT. This allows an active matrix display device to control the driving of light-emitting elements using TFTs. A light-emitting device of this type can be manufactured. The structure of the TFT is not particularly limited. The TFT may be a TFT of a staggered type or a reverse staggered type. There is no particular limitation on the type of semiconductor, and either an amorphous semiconductor or a crystalline semiconductor may be used. In addition, the driving circuit formed on the TFT substrate is also made up of N-type and P-type TFTs. Alternatively, the TFT may be composed of only one of N-type TFT or P-type TFT. It may be also possible.
[0132] Note that this embodiment mode can be appropriately combined with other embodiment modes.
[0133] (Embodiment 3) In this embodiment, the light-emitting element described in Embodiment 1 or 2 is used as a lighting device. An example of the above-mentioned lighting device will be described with reference to FIG. 3. FIG. 3(B) is a top view of the lighting device, and FIG. FIG. 3B is a cross-sectional view taken along line ef in FIG.
[0134] The lighting device in this embodiment is a first substrate 400 having a light-transmitting property and serving as a support. The first electrode 401 is formed on the substrate 100. The first electrode 401 is the same as the first electrode 10 in the second embodiment. Equivalent to 1.
[0135] An auxiliary electrode 402 is provided on the first electrode 401. In this embodiment, Since an example in which light is emitted from the first electrode 401 side is shown, the first electrode 401 is made of a light-transmitting material. The auxiliary electrode 402 is provided to compensate for the low electrical conductivity of the light-transmitting material. The resistance of the first electrode 401 is high, and the voltage drop in the light-emitting surface is caused by this. The auxiliary electrode 402 has a function of suppressing uneven brightness. The conductive material is preferably aluminum or the like. In addition, the auxiliary electrode 402 is preferably formed of a material having a low resistance. It is preferable that the surface other than the part to be removed is covered with an insulating layer. This is to suppress light emission from the upper part of the auxiliary electrode 402, which is not connected to the electrode, and to reduce reactive current and improve power efficiency. This is to suppress the decrease in the electrical conductivity of the second electrode 404. A pad 412 may be formed for supplying a voltage.
[0136] An EL layer 403 is formed on the first electrode 401 and the auxiliary electrode 402. The EL layer 403 has the structure described in Embodiment 1 or 2. The electrode 401 is formed slightly larger than the electrode 401 in plan view. This is a preferable configuration since it also serves as an insulating layer to prevent short circuits with the electrode 404 .
[0137] A second electrode 404 is formed to cover the EL layer 403. This corresponds to the second electrode 102 in the embodiment and has a similar structure. Since the light is taken out from the first electrode 401 side, the second electrode 404 is made of a material with high reflectivity. In this embodiment, the second electrode 404 is preferably formed by the pad 41. Voltage shall be supplied by connecting to 2.
[0138] The first electrode 401, the EL layer 403, and the second electrode 404 (and the auxiliary electrode 402) The lighting device described in this embodiment has a light-emitting element having a luminous efficiency of Since the light emitting element has a high light emitting property, the lighting device in this embodiment has a low power consumption. It can be said that:
[0139] The light emitting element having the above structure is fixed to a sealing substrate 407 using sealing materials 405 and 406. The lighting device is completed by sealing the light source. Also, a desiccant can be mixed into the inner sealant 406, which This allows the material to absorb moisture, improving reliability.
[0140] In addition, the pad 412, the first electrode 401, and a part of the auxiliary electrode 402 are covered with a sealing material 405, By extending it outside of 06, it can be used as an external input terminal. An IC chip 420 having a converter mounted thereon may be provided.
[0141] As described above, the lighting device according to the present embodiment includes an EL element having the same structure as that described in the first or second embodiment. Since the light emitting element is mounted on the light emitting device, the light emitting device has high light emitting efficiency and consumes low power. can be done.
[0142] (Embodiment 4) In this embodiment mode, the light-emitting element described in Embodiment 1 or 2 is applied with reference to FIG. A passive matrix light-emitting device manufactured using the above method will be described. FIG. 4(B) is a cross-sectional view taken along the line XY in FIG. 4(A). An EL layer 955 is provided between an electrode 952 and an electrode 956 on a substrate 951. The end of the electrode 952 is covered with an insulating layer 953. The sidewall of the partition layer 954 is gradually narrower toward the substrate surface. The partition layer 954 has a slope such that the distance between the side wall and the other side wall becomes narrower. The cross section of the short side direction of the insulating layer 953 is trapezoidal, and the base ( The side in contact with the insulating layer 953) faces in the same direction as the surface direction of the insulating layer 953, and the insulating In this way, the partition layer 954 is provided to prevent static electricity It is possible to prevent defects in the light-emitting element due to the above-mentioned problems. In the device, by including the light-emitting element described in embodiment 1 or embodiment 2, It is possible to provide a lighting device with high luminous efficiency and low power consumption.
[0143] (Embodiment 5) In this embodiment mode, a light-emitting element manufactured using the light-emitting element described in Embodiment 1 or 2 is used. The active matrix light emitting device will be described with reference to FIG.
[0144] 5(A) and 5(B) show a light-emitting device that is full colored by providing a colored layer or the like. FIG. 5A shows a substrate 1001, a base insulating film 1002, a gate insulating film 1003, and a , gate electrodes 1006, 1007, 1008, a first interlayer insulating film 1020, a second interlayer insulating film The insulating film 1021, the peripheral portion 1042, the pixel portion 1040, the driving circuit portion 1041, and the first light-emitting element The first electrode 1024W, the first electrode 1024R, the first electrode 1024G, the first electrode 1024 B, a partition wall 1025, an EL layer 1028, a second electrode 1029 of the light-emitting element, and a sealing substrate 1031 , sealing material 1032a, sealing material 1032b, etc. are shown. You can also mix a desiccant into the colored layer (red colored layer 1034R, green colored layer The blue colored layer 1034G and the blue colored layer 1034B are provided on a transparent substrate 1033. (Black matrix) 1035 may be further provided. The transparent base material 1033 is aligned and fixed to the substrate 1001. The black layer is covered with an overcoat layer 1036. The light-emitting layer emits light to the outside without passing through the colored layers, and the light passes through the colored layers of each color to the outside. The light that does not pass through the colored layer is white, and the light that passes through the colored layer is red, blue, or green. This makes it possible to express images using four color pixels.
[0145] In the light emitting device described above, the light is taken in toward the substrate 1001 on which the TFT is formed. The light emitting device has a bottom emission structure, but the light is taken in from the sealing substrate 1031 side. The light emitting device may have a structure in which the light is emitted from the top (top emission type). A cross-sectional view of a light-emitting device is shown in FIG. 6. In this case, a substrate 1001 that does not transmit light is used. The bottom electrode is not connected to the anode of the TFT and the light-emitting element until the connection electrode is fabricated. The third interlayer insulating film 1037 is then formed in the same manner as in the case of a mission-type light-emitting device. The insulating film may be formed to cover the first interlayer 1022. The insulating film may also serve as a flattening film. The insulating film 1037 is made of the same material as the second interlayer insulating film 1021, or other known materials. It can be formed.
[0146] The first electrodes 1024W, 1024R, 1024G, and 1024B of the light-emitting element are anodes here. However, it may be a cathode. Also, in the case of a top emission type light emitting device as shown in FIG. In the case of the above-mentioned arrangement, it is preferable that the first electrode is a reflective electrode. The configuration described in the first or second embodiment is used to obtain white light emission. The structure for obtaining white light emission is as follows: Blue light is emitted from the emitting layer in one EL layer, and orange light is emitted from the emitting layer in the other EL layer. The blue light is emitted from the light-emitting layer in one EL layer and the blue light is emitted from the light-emitting layer in the other EL layer. A configuration in which red and green light can be obtained from the light-emitting layer in the layer is also conceivable. When three EL layers are used, red, green and blue light is emitted from each emitting layer. By doing so, a light-emitting element that emits white light can be obtained. Alternatively, if the configuration shown in the second embodiment is applied, the configuration for obtaining white light emission is the same as the above. Of course, this is not limited.
[0147] The colored layer is provided on the optical path through which the light from the light emitting element exits to the outside. In the case of an emission type light emitting device, a transparent substrate 1033 is provided with colored layers 1034R and 1034G. , 1034B and fixed to the substrate 1001. As shown in FIG. 5B, a colored layer is formed between the gate insulating film 1003 and the first interlayer insulating film 1020. In the case of a top emission structure as shown in FIG. A sealing material having a colored layer 1034R of a red color, a colored layer 1034G of a green color, and a colored layer 1034B of a blue color) Sealing can also be performed with a substrate 1031. The sealing substrate 1031 has a structure in which a pixel is located between pixels. A black layer (black matrix) 1035 may be provided so as to prevent the color from being colored. The color layer 1034R, the green color layer 1034G, the blue color layer 1034B) and the black layer (black The matrix may be covered with an overcoat layer 1036. The plate 1031 is made of a light-transmitting substrate.
[0148] When a voltage is applied between the pair of electrodes of the light-emitting device thus obtained, a white light-emitting region 1044W is emitted. In addition, by combining with a colored layer, a red light emitting region 1044R and a blue light emitting region 1045R are obtained. A light emitting region 1044B and a green light emitting region 1044G are obtained. Since the light-emitting element described in Embodiment 1 or 2 is used in the device, the driving voltage is It is therefore possible to realize a light emitting device with low light emission and low power consumption.
[0149] In addition, although an example of full-color display using four colors, red, green, blue, and white, is shown here, the present invention is not particularly limited. Alternatively, full color display may be performed using the three colors red, green, and blue.
[0150] This embodiment mode can be freely combined with other embodiment modes.
[0151] (Embodiment 6) In this embodiment, a light-emitting element including the light-emitting element described in Embodiment 1 or 2 is used as a part of the light-emitting element. An example of a child device will be described. The light emitting device described in the first or second embodiment has a light emitting efficiency. As a result, the light-emitting element described in this embodiment has a high efficiency and reduced power consumption. The device may be an electronic device having a light emitting portion with reduced power consumption.
[0152] As an example of an electronic device to which the light-emitting element is applied, a television set (television, (also called revision receivers), computer monitors, digital cameras, digital Video cameras, digital photo frames, mobile phones (also called mobile phones or mobile phone devices) ), portable game machines, personal digital assistants, audio playback devices, pachinko machines and other large game machines, etc. Specific examples of these electronic devices are shown below.
[0153] FIG. 7A shows an example of a television device. The television device includes a housing 710. A display unit 7103 is built into the display unit 1. Also, in this example, the display unit 7103 is attached to the case by a mounting fixture 7105. The display unit 7103 displays images. The display portion 7103 can be formed using the light-emitting element described in Embodiment 1 or 2. The light emitting element is configured by arranging the light emitting elements in a matrix. Therefore, the display portion 7103 including the light-emitting element can be used as a display device. The television set may be a reduced power consumption television set.
[0154] The television device can be operated using an operation switch provided on the housing 7101 or a separate remote control. The remote control device 7110 includes an operation key 7109. This allows you to control the channel and volume, and the image displayed on the display unit 7103 In addition, the remote control operation device 7110 can be operated. A display portion 7107 for displaying information output from the image forming apparatus may be provided.
[0155] FIG. 7(B1) shows a computer, which includes a main body 7201, a housing 7202, a display unit 7203, and a keyboard. keyboard 7204, external connection port 7205, pointing device 7206, etc. This computer is capable of generating the same data as that described in the first or second embodiment. The display unit 7203 is fabricated by arranging optical elements in a matrix. The computer of FIG. 7(B2) may be in the form of the computer of FIG. 7(B2). The computer includes a second keyboard 7204 and a second pointing device 7206. A display unit 7210 is provided. The second display unit 7210 is a touch panel type. By operating the display for input displayed on the second display unit 7210 with a finger or a special pen, In addition, the second display portion 7210 can be used not only for displaying input data but also for It is also possible to display other images. Good. The two screens are connected by a hinge, so you can easily fold the screens apart when storing or transporting. This also prevents damage and other troubles. The data is displayed by arranging the light-emitting elements described in embodiment 1 or embodiment 2 in a matrix. The light-emitting element is manufactured by using the same in the portion 7203. The light-emitting element has good light-emitting efficiency. Therefore, it is possible to display a display portion 7203 including the light-emitting element. The computer may be a reduced power computer.
[0156] FIG. 7C shows a portable game machine that is composed of two housings, a housing 7301 and a housing 7302. The housing 7301 is connected to the connector 7303 so as to be openable and closable. A display unit manufactured by arranging the light-emitting elements described in the first or second embodiment in a matrix. A display unit 7305 is incorporated in the housing 7302. The portable gaming machine shown in FIG. 7(C) also includes a speaker unit 7306 and a recording medium insertion unit 7307. , LED lamp 7308, input means (operation keys 7309, connection terminal 7310, sensor 73 11 (force, displacement, position, velocity, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical Chemical substances, sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration , odor or infrared measuring function), microphone 7312) etc. Of course, the configuration of the portable gaming machine is not limited to the above, and at least the display unit 73 04 and / or the display portion 7305 may be It is sufficient to use a display unit made by arranging light-emitting elements in a matrix, and other accessories The portable game machine shown in FIG. 7(C) is a configuration in which the recording medium The function of reading out the programs or data stored in the device and displaying them on the display unit, It has a function to share information with the mobile game machine by wireless communication. The functions of the strip-type gaming machine are not limited to those described above, and the machine may have various functions. A portable game machine having such a display portion 7304 has a light-emitting element used in the display portion 7304. Since the device has good luminous efficiency, it is a portable gaming machine with reduced power consumption. In addition, the light-emitting element used in the display portion 7304 can be driven at a low driving voltage. Therefore, it is possible to provide a portable gaming machine with a low driving voltage. Since the light emitting element used in the portion 7304 is a light emitting element with a long life, it is highly reliable. It can be a portable gaming machine.
[0157] FIG. 7D shows an example of a mobile phone. The mobile phone is built in a housing 7401. In addition to the display unit 7402, the operation buttons 7403, the external connection port 7404, the speaker 74 05, a microphone 7406, etc. The mobile phone 7400 is the same as that of the first embodiment. The display portion 7402 is manufactured by arranging the light-emitting elements described in Embodiment 2 in a matrix. The light-emitting element can have high light-emitting efficiency. It is possible to provide a light emitting element with a low driving voltage. Therefore, a mobile phone having a display portion 7402 including the light-emitting element can be used. The mobile phone can be a mobile phone with reduced power consumption. It is possible to make a telephone set. It is also possible to make a highly reliable mobile phone. .
[0158] The mobile phone shown in FIG. 7D is a mobile phone that allows users to input information by touching the display portion 7402 with a finger or the like. In this case, the user can make a call or create an email. Such an operation can be performed by touching the display portion 7402 with a finger or the like.
[0159] The screen of the display unit 7402 has three main modes. The first is a display mode that is mainly used for displaying images. The first mode is a display mode, the second is an input mode for inputting information such as characters, and the third mode is a display mode. This is a display + input mode that combines the display mode and the input mode.
[0160] For example, when making a call or composing an e-mail, the display unit 7402 is used to input characters. The main character input mode is to input characters displayed on the screen. It is preferable to display a keyboard or number buttons on most of the screen of the display portion 7402. I wish.
[0161] In addition, the mobile phone may include a sensor that detects the inclination of the mobile phone, such as a gyro or an acceleration sensor. By providing a display device, the orientation of the mobile phone (vertical or horizontal) can be determined and the image of the display portion 7402 can be displayed. The surface display can be switched automatically.
[0162] The screen mode can be changed by touching the display portion 7402 or by operating the housing 7401. This is done by operating the button 7403. Also, depending on the type of image displayed on the display unit 7402, For example, the image signal to be displayed on the display unit is a moving image. If it is data, the mode is switched to display mode, and if it is text data, the mode is switched to input mode.
[0163] In the input mode, the optical sensor of the display unit 7402 detects a signal and displays If there is no input by touch operation of the part 7402 for a certain period of time, the screen mode is changed to the input mode. Alternatively, the display mode may be switched from the normal mode to the display mode.
[0164] The display portion 7402 can also function as an image sensor. By touching the palm or fingers of the user on the sensor 02 and capturing an image of the palm print or fingerprint, the user can be authenticated. In addition, a backlight that emits near-infrared light to the display unit or a sensing light that emits near-infrared light By using a source, it is also possible to image finger veins, palm veins, etc.
[0165] Note that the configuration shown in this embodiment mode is a combination of the configurations shown in Embodiment Modes 1 to 5. They can be used in combination.
[0166] The desk lamp 2003 shown in FIG. 8(A) is a light-emitting device according to the first or second embodiment. This is an example of using the element in a lighting device. A desk lamp 2003 is made up of a housing 2001 and a light source 2002. 002, and as a light source 2002, the light-emitting element described in the first and second embodiments FIG. 8B shows the light-emitting element described in the first and second embodiments. This is an example in which the above-mentioned is used as an indoor lighting device 3001 and a television device 3002. By using the light-emitting element described in embodiment 1 or 2 in these lighting devices, power consumption Use as a reduced power lighting device, a large area lighting device, or a thin lighting device It becomes possible.
[0167] The light-emitting element according to the first or second embodiment is used for a windshield or a dash panel of an automobile. It can also be mounted on a board. The light-emitting element is used in a windshield or dashboard of an automobile.
[0168] The display 5000 and the display 5001 are the display devices according to the first embodiment or the second embodiment, which are provided on the windshield of an automobile. A display device equipped with the light-emitting device according to the second embodiment. The light-emitting element described in the above is manufactured by using a first electrode and a second electrode that are light-transmitting. As a result, a so-called see-through display device can be obtained, in which the opposite side can be seen through. If the display is see-through, even if it is installed on the windshield of a car, the visibility will be reduced. It can be installed without being disturbed. In this case, organic transistors using organic semiconductor materials and transistors using oxide semiconductors are used. For example, a light-transmitting transistor such as a transistor having a light-transmitting property may be used.
[0169] The light-emitting element 5002 is provided in the pillar portion. The display 5002 displays an image captured by an imaging means provided on the vehicle body. By projecting the image, it is possible to complement the view blocked by the pillar. The display 5003 provided on the dashboard is used to display the view of the vehicle that is blocked by the body of the car. By projecting images from an external imaging device, blind spots are compensated for and safety is improved. By projecting an image that complements the invisible parts, it becomes more natural. Safety checks can be performed without any discomfort.
[0170] Display 5004 and Display 5005 display navigation information, speedometer, tachometer, It can provide information such as mileage, fuel level, gear status, air conditioning settings, and much more. The display items and layout can be changed as needed to suit the user's preferences. This information can also be provided in displays 5000 to 5003. In addition, the displays 5000 to 5005 can also be used as lighting devices.
[0171] As shown in FIG. 9B, the display unit of the license plate 5011 may be The light emitting element described in the second embodiment may be applied to the license plate 501. 1 visibility can be improved.
[0172] As shown in FIG. 9C, the hands 5021 and the display unit 5022 of the watch may be The light emitting device according to the second embodiment may be mounted on the wristwatch. Thus, it is possible to improve visibility in dark places without using radioactive materials such as tritium. do.
[0173] As described above, the scope of application of the light emitting device including the light emitting element according to the first embodiment or the second embodiment is as follows: The light emitting device can be used in a wide range of electronic devices. By using the light-emitting element described in embodiment 1 or 2, a light-emitting device with low power consumption can be obtained. You can get a child device. EXAMPLES
[0174] In this example, a thermally activated delayed phosphor and a material that emits fluorescence were mixed and used in the light-emitting layer. A device in which a material that does not emit thermally activated delayed fluorescence and a material that emits fluorescence are mixed and used in the light-emitting layer. The results of actually fabricating and comparing the comparative light-emitting element and the comparative light-emitting element are described with reference to FIGS. 11 to 15. Reveal.
[0175] Hereinafter, the light-emitting device 1 will be described as a device in which a thermally activated delayed phosphor and a material that emits fluorescence are mixed and used in the light-emitting layer. The comparative light-emitting element 1 is a light-emitting element that emits fluorescence using a material that does not have thermally activated delayed fluorescence. The light-emitting element is formed by mixing the above-mentioned material in the light-emitting layer.
[0176] The fluorescent material used in the light-emitting element 1 and the comparative light-emitting element 1 was 5,6,11,12-tetrafluoroethylene. It is tetraphenylnaphthacene (common name: rubrene).
[0177] In the light-emitting element 1, two types of organic compounds that form an exciplex are used as thermally activated delayed fluorescent substances. Specifically, the first organic compound was 2-[3-(dibenzothiophene- 4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 2mDBTPDBq-I I) was used as the second organic compound, and 2-[N-(9-phenylcarbazol-3-yl) )-N-phenylamino]spiro-9,9'-bifluorene (abbreviation: PCASF) was used. Ta.
[0178] In the comparative light-emitting element 1, 2-[3-(dibenzothiophene) 2mDBTPD That is, the light-emitting element 1 was used as a material that does not emit thermally activated delayed fluorescence. Only the first organic compound in was used.
[0179] The chemical formulas of the materials used in this example are shown below.
[0180] [ka]
[0181] A method for fabricating the light-emitting element 1 and the comparative light-emitting element 1 will be described below.
[0182] (Light emitting element 1) First, indium tin oxide containing silicon oxide (ITSO) is deposited on a glass substrate 1100. A film was formed by a tin-sputtering method to form a first electrode 1101 that functions as an anode. The film thickness was 110 nm, and the electrode area was 2 mm × 2 mm (see FIG. 11).
[0183] Next, as a pretreatment for forming a light emitting element on the substrate 1100, the substrate surface is washed with water. After baking at 200°C for 1 hour, UV ozone treatment was performed for 370 seconds.
[0184] Then, 10 -4 The substrate is placed in a vacuum deposition apparatus whose inside has been reduced in pressure to about Pa, and vacuum deposition is performed. After vacuum baking at 170° C. for 30 minutes in the heating chamber of the device, the substrate 1100 is It was left to cool for about 0 minutes.
[0185] Next, the surface on which the first electrode 1101 is formed is placed downward. The substrate 1100 thus formed is fixed to a substrate holder provided in a vacuum deposition apparatus, and then 10 -4 P After reducing the pressure to about a, 1,3,5-tri(dibenzothiophene) was placed on the first electrode 1101. The co-evaporation of DBT3P-II and molybdenum oxide was performed. Thus, a hole injection layer 1111 was formed. The thickness of the layer was set to 40 nm. The mass ratio of molybdenum oxide is 1:0.5 (=DBT3P-II:molybdenum oxide). It was adjusted so that
[0186] Next, BPAFLP (abbreviation) was formed on the hole injection layer 1111 to a thickness of 20 nm. A hole transport layer 1112 was formed.
[0187] In addition, 2mDBTPDBq-II (abbreviation), PCASF (abbreviation), and rubrene were used together. The light-emitting layer 1113 was formed on the hole transport layer 1112 by deposition. The weight ratio of q-II, PCASF, and rubrene was 0.8:0.2:0.01 (=2m The composition of the light-emitting layer 1 was adjusted to be DBTPDBq-II: PCASF: rubrene. The film thickness of 113 was set to 30 nm.
[0188] Next, 2mDBTPDBq-II (abbreviation) was applied to the light-emitting layer 1113 to a thickness of 20 nm. A film was formed to form a first electron transport layer 1114a.
[0189] Next, bathophenanthroline (abbreviation: BPhen) was applied onto the first electron transport layer 1114a. A film was formed to a thickness of 20 nm to form the second electron transport layer 1114b.
[0190] Furthermore, lithium fluoride (LiF) was deposited on the second electron transport layer 1114b to a thickness of 1 nm. An electron injection layer 1115 was formed by evaporation.
[0191] Finally, a 200 nm film of aluminum was deposited on the second electrode 1103, which served as the cathode. The light-emitting element 1 of this example was fabricated by depositing the material so as to have a thickness.
[0192] (Comparative light-emitting element 1) The light-emitting layer 1113 of the comparative light-emitting element 1 was made of 2mDBTPDBq-II (abbreviation) and rubrene. The film was formed by co-evaporation of 2mDBTPDBq-II (abbreviation) and Rubrez. The weight ratio of the benzene was adjusted to 1:0.01 (=2mDBTPDBq-II:rubrene). The thickness of the light-emitting layer 1113 was set to 30 nm. The mice were prepared in the same manner as child 1.
[0193] In the above-mentioned deposition process, the deposition was all performed by a resistance heating method.
[0194] The element structures of the thus obtained light-emitting element 1 and comparative light-emitting element 1 are shown in Table 1.
[0195] [Table 1]
[0196] These light emitting devices were placed in a nitrogen atmosphere glove box so that the light emitting devices were not exposed to the atmosphere. After sealing to prevent leakage, the operating characteristics of the light-emitting element were measured. The measurements were carried out at room temperature (atmosphere maintained at 25°C).
[0197] FIG. 12 shows the voltage-luminance characteristics of the light-emitting element 1 and the comparative light-emitting element 1. The vertical axis represents voltage (V) and the vertical axis represents brightness (cd / m 2 The luminance-current efficiency characteristics are shown in Figure 1. 3. In FIG. 13, the horizontal axis is luminance (cd / m 2 ) and the vertical axis is current efficiency (cd / A) The luminance-power efficiency characteristics are shown in Fig. 14. In Fig. 14, the horizontal axis is the luminance (cd / m 2 The vertical axis indicates the power efficiency (lm / W), and the vertical axis indicates the luminance-external quantum efficiency. In Figure 15, the horizontal axis is luminance (cd / m 2 ) and the vertical axis indicates external quantum efficiency (%).
[0198] The luminance of the light-emitting element 1 and the comparative light-emitting element 1 was 1000 cd / m 2 When the electricity is near Voltage (V), current density (mA / cm 2 ), CIE chromaticity coordinates (x, y), current efficiency (cd / A ), power efficiency (lm / W), and external quantum efficiency (%) are shown in Table 2.
[0199] [Table 2]
[0200] As shown in Table 2, the brightness is 1000cd / m 2The CIE chromaticity coordinates of light-emitting element 1 when ,y)=(0.47,0.52), and the luminance is 1000cd / m 2 Comparison of luminous elements in the vicinity The CIE chromaticity coordinates of child 1 were (x,y)=(0.46,0.50). From this result, It was found that the light-emitting element 1 and the comparative light-emitting element 1 emitted yellow light derived from rubrene. I did.
[0201] As can be seen from Table 2 and FIGS. 12 to 15, the light-emitting element 1 has a higher emission efficiency than the comparative light-emitting element 1. The threshold voltage at which light starts to emit (light emission start voltage) is low, and current efficiency, power efficiency, and external quantum The efficiency was high. Since ASF forms an exciplex, a part of the triplet excited state of the exciplex in the light-emitting layer 1113 The singlet excited state of the exciplex is generated from the However, by transferring the excited state to the singlet state of the fluorescent material, the luminescence efficiency was improved. It is also believed that the emission onset voltage is decreased due to the formation of this exciplex. can be done. EXAMPLES
[0202] In this embodiment, similarly to the first embodiment, a thermally activated delayed phosphor and a material that emits fluorescence were mixed. and a light-emitting device using the same in the light-emitting layer, and a material that does not emit thermally activated delayed fluorescence and a material that emits fluorescence. The results of actually fabricating a comparative light-emitting element using a mixture of the above in the light-emitting layer and a comparison element are shown in Figure 1. 6 to 22.
[0203] Hereinafter, the light-emitting element 2 will be described as a light-emitting layer made of a mixture of a thermally activated delayed phosphor and a material that emits fluorescence. The comparative light-emitting element 2 is a light-emitting element that emits fluorescence using a material that does not have thermally activated delayed fluorescence. The light-emitting element is formed by mixing the above-mentioned material in the light-emitting layer.
[0204] The fluorescent material used in the light-emitting element 2 and the comparative light-emitting element 2 was 5,6,11,12-tetrafluoroethylene. It is tetraphenylnaphthacene (common name: rubrene).
[0205] In the light-emitting element 2, two types of organic compounds that form an exciplex are used as thermally activated delayed fluorescent substances. Specifically, the first organic compound was 4,6-bis[3-(9H-carba 4,6mCzP2Pm was used as the second As an organic compound, N-(1,1'-biphenyl-4-yl)-N-[4-(9-phenyl [(3-(9H-carbazol-3-yl)phenyl]-9,9-dimethyl-9H-fluorene -2-amine (abbreviation: PCBBiF) was used.
[0206] In the comparative light-emitting element 2, 4,6-bis[3-(9H -carbazol-9-yl)phenyl]pyrimidine (abbreviation: 4,6mCzP2Pm) That is, the first active material in the light-emitting element 2 is a material that does not emit thermally activated delayed fluorescence. Only organic compounds were used.
[0207] The chemical formulas of the materials used in this example are shown below.
[0208] [ka]
[0209] A method for fabricating the light-emitting element 2 and the comparative light-emitting element 2 will be described below.
[0210] (Light emitting element 2) First, a first electrode 11 was formed on a glass substrate 1100 using the same material and conditions as those for the light-emitting element 1. 01, a hole injection layer 1111, and a hole transport layer 1112 were formed.
[0211] Next, 4,6mCzP2Pm (abbreviation), PCBBiF (abbreviation) and rubrene were co-evaporated. An emitting layer 1113 was formed on the hole transport layer 1112. The weight ratio of PCBBiF and rubrene was 0.8:0.2:0.0075 (=4.6mC The composition was adjusted so that the composition was zP2Pm:PCBBiF:rubrene. The film thickness was 40 nm.
[0212] Next, 4,6mCzP2Pm (abbreviation) is formed on the light-emitting layer 1113 to a thickness of 10 nm. Thus, a first electron transport layer 1114a was formed.
[0213] Next, bathophenanthroline (abbreviation: BPhen) was applied onto the first electron transport layer 1114a. A film was formed to a thickness of 15 nm to form the second electron transport layer 1114b.
[0214] Furthermore, the electron injection layer 1115 and the second electrode were formed using the same materials and conditions as those for the light-emitting element 1. Thus, the light-emitting element 2 of this example was fabricated.
[0215] (Comparative light-emitting element 2) The light-emitting layer 1113 of the comparative light-emitting element 2 contains 4,6mCzP2Pm (abbreviation) and rubrene. The weight ratio of 4,6mCzP2Pm and rubrene was 1 The ratio was adjusted to 0.005 (=4,6mCzP2Pm:rubrene). The thickness of the layer 1113 was 40 nm. Ta.
[0216] In the above-mentioned deposition process, the deposition was all performed by a resistance heating method.
[0217] Table 3 shows the element structures of the thus obtained light-emitting element 2 and comparative light-emitting element 2.
[0218] [Table 3]
[0219] These light emitting devices were placed in a nitrogen atmosphere glove box so that the light emitting devices were not exposed to the atmosphere. After sealing to prevent leakage, the operating characteristics of the light-emitting element were measured. The measurements were carried out at room temperature (atmosphere maintained at 25°C).
[0220] FIG. 16 shows the voltage-luminance characteristics of the light-emitting element 2 and the comparative light-emitting element 2. The vertical axis represents voltage (V) and the vertical axis represents brightness (cd / m 2 The luminance-current efficiency characteristics are shown in Figure 1. 7. In FIG. 17, the horizontal axis is luminance (cd / m 2 ) and the vertical axis is current efficiency (cd / A) The voltage-current characteristics are shown in FIG. 18. In FIG. 18, the horizontal axis represents voltage (V), The vertical axis indicates the current (mA). The luminance-power efficiency characteristics are shown in FIG. , the horizontal axis is luminance (cd / m 2 ) and the vertical axis indicates power efficiency (lm / W). The photoelectric efficiency is shown in FIG. 20. In FIG. 20, the horizontal axis is the luminance (cd / m 2 ) and the vertical axis is the external quantum Efficiency (%) is shown.
[0221] The luminance of the light-emitting element 2 and the comparative light-emitting element 2 was 1000 cd / m 2 When the electricity is near Voltage (V), current density (mA / cm 2), CIE chromaticity coordinates (x, y), current efficiency (cd / A ), power efficiency (lm / W), and external quantum efficiency (%) are shown in Table 4.
[0222] [Table 4]
[0223] As shown in Table 4, the luminance is 1000cd / m 2 The CIE chromaticity coordinates of the nearby light-emitting element 2 are (x,y )=(0.47,0.52), and the luminance is 1000cd / m 2 Comparative light emission at nearby brightness The CIE chromaticity coordinates of element 2 were (x, y) = (0.47, 0.50).
[0224] Furthermore, the emission spectra when a current of 0.1 mA was applied to the light-emitting element 2 and the comparative light-emitting element 2 were is shown in FIG. 21. In FIG. 21, the vertical axis indicates the emission intensity (arbitrary unit) and the horizontal axis indicates the wavelength (nm). The luminescence intensity is shown as a relative value with the maximum luminescence intensity set to 1. As shown in FIG. The emission spectra of the light-emitting element 2 and the comparative light-emitting element 2 had a maximum emission wavelength around 558 nm. The spectrum is derived from the polystyrene. It was found that the optical element 2 was a light-emitting element that emitted yellow light.
[0225] In addition, the initial brightness is 5000cd / m 2 The current density was kept constant, and the light-emitting element 2 and the comparison FIG. 22 shows the results of a reliability test performed by driving the light-emitting element 2. In FIG. The change in normalized luminance is shown with the value of 100%.
[0226] 16 to 22, the light-emitting element 2 had a higher emission rate than the comparative light-emitting element 2. The threshold voltage (light emission start voltage) is low, and the current efficiency, power efficiency, and external quantum efficiency are excellent. Furthermore, the brightness degradation over time was small, and the device had good reliability. It was found to be a photonic device.
[0227] The 4,6mCzP2Pm and PCBBiF used in the light-emitting layer 1113 form an exciplex. The singlet excited state of the exciplex is converted from a part of the triplet excited state of the exciplex in the light-emitting layer 1113. The energy of the singlet excited state of this exciplex is converted into the singlet state of the material that emits fluorescence. It is believed that the transition to an excited state leads to improved luminescence efficiency. It is believed that the light emission starting voltage was decreased due to the effect of the formation of the solid body. EXAMPLES
[0228] In this embodiment, similarly to the first embodiment, a thermally activated delayed phosphor and a material that emits fluorescence were mixed. and a light-emitting device using the same in the light-emitting layer, and a material that does not emit thermally activated delayed fluorescence and a material that emits fluorescence. The results of actually fabricating a comparative light-emitting element using a mixture of the above in the light-emitting layer and a comparison element are shown in Figure 2. 3 to 29.
[0229] Hereinafter, the light-emitting device 3 will be described as a device in which a thermally activated delayed phosphor and a material that emits fluorescence are mixed and used in the light-emitting layer. The comparative light-emitting element 3 is a light-emitting element that emits fluorescence using a material that does not have thermally activated delayed fluorescence. The light-emitting element is formed by mixing the above-mentioned material in the light-emitting layer.
[0230] The fluorescent material used in the light-emitting element 3 and the comparative light-emitting element 3 is coumarin 6 (common name). be.
[0231] In the light-emitting element 3, the thermally activated delayed fluorescent substance is a combination that forms an exciplex similar to that in Example 2. The first organic compound was 4,6-bis[3- (9H-carbazol-9-yl)phenyl]pyrimidine (abbreviation: 4,6mCzP2Pm ) as the second organic compound, and N-(1,1'-biphenyl-4-yl)-N-[4 -(9-phenyl-9H-carbazol-3-yl)phenyl]-9,9-dimethyl-9 H-fluoren-2-amine (abbreviation: PCBBiF) was used.
[0232] In the comparative light-emitting element 3, the same 4,6-biphenylene as in Example 2 was used as a material that does not emit thermally activated delayed fluorescence. 4,6mCz In other words, a material that does not emit thermally activated delayed fluorescence was used for the light-emitting element 3. Only the first organic compound in the above was used.
[0233] For the chemical formulas of the materials used in this example, see the chemical formulas in Example 2.
[0234] A method for fabricating the light-emitting element 3 and the comparative light-emitting element 3 will be described below.
[0235] (Light emitting element 3) First, a first electrode 11 was formed on a glass substrate 1100 using the same material and conditions as those for the light-emitting element 1. 01, a hole injection layer 1111, and a hole transport layer 1112 were formed.
[0236] Next, 4,6mCzP2Pm (abbreviation), PCBBiF (abbreviation) and Coumarin 6 were co-evaporated. Then, the light-emitting layer 1113 was formed on the hole transport layer 1112. The weight ratio of PCBBiF and coumarin 6 was 0.8:0.2:0.005 (=4,6m The composition was adjusted so that the composition was CzP2Pm:PCBBiF:coumarin6). The film thickness of 3 was set to 40 nm.
[0237] Next, 4,6mCzP2Pm (abbreviation) is formed on the light-emitting layer 1113 to a thickness of 10 nm. Thus, a first electron transport layer 1114a was formed.
[0238] Next, bathophenanthroline (abbreviation: BPhen) was applied onto the first electron transport layer 1114a. A film was formed to a thickness of 15 nm to form the second electron transport layer 1114b.
[0239] Furthermore, the electron injection layer 1115 and the second electrode were formed using the same materials and conditions as those for the light-emitting element 1. Thus, the light-emitting element 3 of this example was fabricated.
[0240] (Comparative light-emitting element 3) The light-emitting layer 1113 of the comparative light-emitting element 3 contains 4,6mCzP2Pm (abbreviation) and coumarin 6. The weight ratio of 4,6mCzP2Pm and coumarin 6 was The ratio was adjusted to 1:0.005 (=4,6mCzP2Pm:coumarin6). The thickness of the light-emitting layer 1113 was 40 nm. It was made.
[0241] In the above-mentioned deposition process, the deposition was all performed by a resistance heating method.
[0242] Table 5 shows the element structures of the thus obtained light-emitting element 3 and the comparative light-emitting element 3.
[0243] [Table 5]
[0244] These light emitting devices were placed in a nitrogen atmosphere glove box so that the light emitting devices were not exposed to the atmosphere. After sealing to prevent leakage, the operating characteristics of the light-emitting element were measured. The measurements were carried out at room temperature (atmosphere maintained at 25°C).
[0245] FIG. 23 shows the voltage-luminance characteristics of the light-emitting element 3 and the comparative light-emitting element 3. The vertical axis represents voltage (V) and the vertical axis represents brightness (cd / m 2 The luminance-current efficiency characteristics are shown in Figure 2. 4. In FIG. 24, the horizontal axis is luminance (cd / m 2 ) and the vertical axis is current efficiency (cd / A) The voltage-current characteristics are shown in FIG. 25. In FIG. 25, the horizontal axis represents voltage (V), The vertical axis indicates the current (mA). The luminance-power efficiency characteristics are shown in FIG. , the horizontal axis is luminance (cd / m 2 ) and the vertical axis indicates power efficiency (lm / W). The photoelectric efficiency is shown in FIG. 27. In FIG. 27, the horizontal axis is the luminance (cd / m 2 ) and the vertical axis is the external quantum Efficiency (%) is shown.
[0246] The luminance of the light-emitting element 3 and the comparative light-emitting element 3 was 1000 cd / m 2 When the electricity is near Voltage (V), current density (mA / cm 2 ), CIE chromaticity coordinates (x, y), current efficiency (cd / A ), power efficiency (lm / W), and external quantum efficiency (%) are shown in Table 6.
[0247] [Table 6]
[0248] As shown in Table 6, the luminance is 1000cd / m 2 The CIE chromaticity coordinates of the nearby light-emitting element 3 are (x,y )=(0.28,0.60), and the luminance is 1000cd / m 2 Comparative light emission at nearby brightness The CIE chromaticity coordinates of element 3 were (x, y) = (0.26, 0.58).
[0249] Furthermore, the emission spectra when a current of 0.1 mA was applied to the light-emitting element 3 and the comparative light-emitting element 3 were is shown in FIG. 28. In FIG. 28, the vertical axis indicates the emission intensity (arbitrary unit) and the horizontal axis indicates the wavelength (nm). The luminescence intensity is shown as a relative value with the maximum luminescence intensity set to 1. As shown in Figure 28, The emission spectra of the light-emitting element 3 and the comparative light-emitting element 3 were similar, with a maximum emission wavelength around 500 nm. The spectrum is derived from Marine 6. The results of Table 6 and the comparative It was found that the light-emitting element 3 was a light-emitting element that emitted green light.
[0250] In addition, the initial brightness is 5000cd / m 2 The current density was kept constant, and the light-emitting element 3 and the comparison The results of a reliability test performed by driving the light-emitting element 3 are shown in FIG. The change in normalized luminance is shown with the value of 100%.
[0251] 23 to 29, the light-emitting element 3 had a higher emission rate than the comparative light-emitting element 3. The threshold voltage (light emission start voltage) is low, and the current efficiency, power efficiency, and external quantum efficiency are excellent. Furthermore, the brightness degradation over time was small, and the device had good reliability. It was found to be a photonic device.
[0252] The 4,6mCzP2Pm and PCBBiF used in the light-emitting layer 1113 form an exciplex. The singlet excited state of the exciplex is converted from a part of the triplet excited state of the exciplex in the light-emitting layer 1113. The energy of the singlet excited state of this exciplex is converted into the singlet state of the material that emits fluorescence. It is believed that the transition to an excited state leads to improved luminescence efficiency. It is believed that the light emission starting voltage was decreased due to the effect of the formation of the solid body. EXAMPLES
[0253] In this embodiment, similarly to the first embodiment, a thermally activated delayed phosphor and a material that emits fluorescence were mixed. and a light-emitting device using the same in the light-emitting layer, and a material that does not emit thermally activated delayed fluorescence and a material that emits fluorescence. The results of actually fabricating a comparative light-emitting element using a mixture of the above in the light-emitting layer and a comparison element are shown in Figure 3. 0 to 35.
[0254] Hereinafter, the light-emitting device 4 will be described using a mixture of a thermally activated delayed phosphor and a material that emits fluorescence in the light-emitting layer. The comparative light-emitting element 4 is a light-emitting element that emits fluorescence using a material that does not have thermally activated delayed fluorescence. The light-emitting element is formed by mixing the above-mentioned material in the light-emitting layer.
[0255] The fluorescent material used in the light-emitting element 3 and the comparative light-emitting element 3 was {2-tert-butyl -6-[2-(1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H, 5H-Benzo[ij]quinolizin-9-yl)ethenyl]-4H-pyran-4-ylidene }propanedinitrile (abbreviation: DCJTB).
[0256] In the light-emitting element 4, the thermally activated delayed fluorescent substance is a combination that forms the same exciplex as in Example 2. The first organic compound was 4,6-bis[3- (9H-carbazol-9-yl)phenyl]pyrimidine (abbreviation: 4,6mCzP2Pm ) as the second organic compound, and N-(1,1'-biphenyl-4-yl)-N-[4 -(9-phenyl-9H-carbazol-3-yl)phenyl]-9,9-dimethyl-9 H-fluoren-2-amine (abbreviation: PCBBiF) was used.
[0257] In the comparative light-emitting element 4, the same 4,6-biphenylene as in Example 2 was used as a material that does not emit thermally activated delayed fluorescence. 4,6mCz In other words, a material that does not emit thermally activated delayed fluorescence was used for the light-emitting element 4. Only the first organic compound in the above was used.
[0258] For the chemical formulas of the materials used in this example, see the chemical formulas in Example 2.
[0259] A method for fabricating the light-emitting element 4 and the comparative light-emitting element 4 will be described below.
[0260] (Light emitting element 4) First, a first electrode 11 was formed on a glass substrate 1100 using the same material and conditions as those for the light-emitting element 1. 01, a hole injection layer 1111, and a hole transport layer 1112 were formed.
[0261] Next, 4,6mCzP2Pm (abbreviation), PCBBiF (abbreviation) and DCJTB (abbreviation) were co-evaporated to form a light-emitting layer 1113 on the hole transport layer 1112. The weight ratio of P2Pm, PCBBiF and DCJTB is 0.8:0.2:0.005 (= 4,6mCzP2Pm:PCBBiF:DCJTB). The thickness of the layer 1113 was set to 40 nm.
[0262] Next, 4,6mCzP2Pm (abbreviation) is formed on the light-emitting layer 1113 to a thickness of 10 nm. Thus, a first electron transport layer 1114a was formed.
[0263] Next, bathophenanthroline (abbreviation: BPhen) was applied onto the first electron transport layer 1114a. A film was formed to a thickness of 15 nm to form the second electron transport layer 1114b.
[0264] Furthermore, the electron injection layer 1115 and the second electrode were formed using the same materials and conditions as those for the light-emitting element 1. Thus, the light-emitting element 4 of this example was fabricated.
[0265] (Comparative light-emitting element 4) The light-emitting layer 1113 of the comparative light-emitting element 3 was made of 4,6mCzP2Pm (abbreviation) and DCJTB( The film was formed by co-evaporation of 4,6mCzP2Pm and DCJTB. The weight ratio was adjusted to 1:0.005 (=4,6mCzP2Pm:DCJTB). The thickness of the light-emitting layer 1113 was 40 nm. was prepared in the same manner as above.
[0266] In the above-mentioned deposition process, the deposition was all performed by a resistance heating method.
[0267] Table 7 shows the element structures of the thus obtained light-emitting element 4 and the comparative light-emitting element 4.
[0268] [Table 7]
[0269] These light emitting devices were placed in a nitrogen atmosphere glove box so that the light emitting devices were not exposed to the atmosphere. After sealing to prevent leakage, the operating characteristics of the light-emitting element were measured. The measurements were carried out at room temperature (atmosphere maintained at 25°C).
[0270] FIG. 30 shows the voltage-luminance characteristics of the light-emitting element 3 and the comparative light-emitting element 3. The vertical axis represents voltage (V) and the vertical axis represents brightness (cd / m 2 The luminance-current efficiency characteristics are shown in Figure 3. 1. In FIG. 31, the horizontal axis is luminance (cd / m 2 ) and the vertical axis is current efficiency (cd / A) The voltage-current characteristics are shown in FIG. 32. In FIG. 32, the horizontal axis represents voltage (V), The vertical axis indicates the current (mA). The luminance-power efficiency characteristics are shown in FIG. , the horizontal axis is luminance (cd / m 2 ) and the vertical axis indicates power efficiency (lm / W). The photoelectric efficiency is shown in FIG. 34. In FIG. 34, the horizontal axis is the luminance (cd / m 2 ) and the vertical axis is the external quantum Efficiency (%) is shown.
[0271] Furthermore, the luminance of the light-emitting element 4 and the comparative light-emitting element 4 was 1000 cd / m 2 When the electricity is near Voltage (V), current density (mA / cm 2 ), CIE chromaticity coordinates (x, y), current efficiency (cd / A ), power efficiency (lm / W), and external quantum efficiency (%) are shown in Table 8.
[0272] [Table 8]
[0273] As shown in Table 8, the luminance is 1000cd / m 2 The CIE chromaticity coordinates of the nearby light-emitting element 4 are (x,y )=(0.57,0.43), and the luminance is 1000cd / m 2 Comparative light emission at nearby brightness The CIE chromaticity coordinates of element 4 were (x, y) = (0.56, 0.41).
[0274] Furthermore, the emission spectra when a current of 0.1 mA was applied to the light-emitting element 4 and the comparative light-emitting element 4 were is shown in FIG. 35. In FIG. 35, the vertical axis indicates the emission intensity (arbitrary unit) and the horizontal axis indicates the wavelength (nm). The luminescence intensity is shown as a relative value with the maximum luminescence intensity set to 1. As shown in Figure 35, The emission spectra of the light-emitting element 4 and the comparative light-emitting element 4 had a maximum emission wavelength of about 595 nm. The spectrum is derived from CJTB, and together with the results in Table 8, the light-emitting element 4 and the comparative It was found that the light-emitting element 4 was a light-emitting element that emitted yellow light.
[0275] In addition, the initial brightness is 5000cd / m 2 The current density was kept constant, and the light-emitting element 4 and the comparison FIG. 36 shows the results of a reliability test performed by driving the light-emitting element 4. In FIG. The change in normalized luminance is shown with the value of 100%.
[0276] 30 to 36, the light-emitting element 4 had a higher emission rate than the comparative light-emitting element 4. The threshold voltage (light emission start voltage) is low, and the current efficiency, power efficiency, and external quantum efficiency are excellent. Furthermore, the brightness degradation over time was small, and the device had good reliability. It was found to be a photonic device.
[0277] The 4,6mCzP2Pm and PCBBiF used in the light-emitting layer 1113 form an exciplex. The singlet excited state of the exciplex is converted from a part of the triplet excited state of the exciplex in the light-emitting layer 1113. The energy of the singlet excited state of this exciplex is converted into the singlet state of the material that emits fluorescence. It is believed that the transition to an excited state leads to improved luminescence efficiency. It is believed that the light emission starting voltage was decreased due to the effect of the formation of the solid body. [Explanation of symbols]
[0278] 101 Electrode 102 electrode 103 EL layer 111 Hole injection layer 112 Hole transport layer 113 Light-emitting layer 113A Luminous materials 113D Thermally activated delayed fluorescent substance 113D1 Organic compounds 113D2 Organic compounds 114 Electron transport layer 115 Electron injection layer 400 Substrates 401 Electrode 402 Auxiliary electrode 403 EL layer 404 Electrode 405 Sealing material 406 Sealing material 407 Sealing substrate 412 Pad 420 IC chip 951 Board 952 Electrode 953 Insulation Layer 954 Partition layer 955 EL layer 956 Electrode 1001 Board 1002 Undercoat insulating film 1003 Gate insulating film 1006 Gate electrode 1007 Gate electrode 1008 Gate electrode 1020 Interlayer insulating film 1021 Interlayer insulating film 1022 Electrode 1024R electrode 1024G electrode 1024B Electrode 1024W electrode 1025 Bulkhead 1028 EL layer 1029 Electrode 1031 Sealing substrate 1032a Sealing material 1032b Sealing material 1033 Base material 1034B Colored layer 1034G colored layer 1034R colored layer 1036 Overcoat layer 1037 Interlayer insulating film 1040 Pixel section 1041 Drive circuit section 1042 Periphery 1044B Light-emitting area 1044G Light-emitting area 1044R Light-emitting area 1044W Light Emitting Area 1100 Substrate 1101 Electrode 1103 Electrode 1111 Hole injection layer 1112 Hole transport layer 1113 Light-emitting layer 1114a Electron transport layer 1114b Electron transport layer 1115 Electron injection layer 2001 Case 2002 light source 2003 Desk lamp 3001 Lighting equipment 5000 display 5001 display 5002 display 5003 display 5004 display 5005 display 5021 needle 5022 Display section 7101 Case 7103 Display section 7105 Mounting fixture 7107 Display section 7109 Operation key 7110 Remote control device 7201 Main unit 7202 Case 7203 Display section 7204 Keyboard 7205 External connection port 7206 Pointing Device 7210 Display section 7301 Case 7302 Case 7303 Connection section 7304 Display section 7305 Display section 7306 Speaker section 7307 Recording medium insertion section 7308 LED Lamp 7309 Operation key 7310 Connection terminal 7311 Sensor 7312 Microphone 7400 Mobile Phone 7401 Case 7402 Display section 7403 Operation button 7404 External connection port 7405 Speaker 7406 Mike
Claims
[Claim 1] A pair of electrodes and a light-emitting layer located between the pair of electrodes, the light-emitting layer includes a first organic compound, a second organic compound, and a third organic compound; the first organic compound and the second organic compound are a combination that forms an exciplex, The third organic compound is a material that emits fluorescence.
Citation Information
Patent Citations
Organic electroluminescent element having exciplex
JP1998106748A
Organic luminescent element material and organic luminescent element using same
JP2001003044A
Organic light emitting element
JP2004047493A
Organic electroluminescence element
JP2007329176A
White light-emitting OLED derived from monomer and aggregate composite emission
JP4509567B2
