Microneedle patch for labeling and manufacturing method thereof
The method of manufacturing patterned microneedle patches using a plug and photolithography addresses the inefficiencies of conventional animal identification methods, enabling cost-effective, painless, and precise pattern application for animal identification.
Patent Information
- Application Number
- JP2024077565
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-12
- Filing Date
- 2024-05-10
- Publication Date
- 2024-11-22
AI Technical Summary
Conventional methods for animal identification, such as ear tags and RFID chips, require significant time, effort, and financial costs, and cause physical and mental burden to animals, while existing microneedle patches lack efficient methods for applying various patterns for individual identification.
A method for manufacturing patterned microneedle patches using a plug with specific structures and a photolithography process, allowing for the creation of female molds with diverse patterns without remanufacturing master molds, and incorporating biosoluble materials for application.
Enables efficient production of microneedle patches with various patterns, reducing costs and time, minimizing animal discomfort, and ensuring precise, symmetrical application of patterns for identification.
Smart Images

Figure 2024163899000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a microneedle patch for marking and a method for manufacturing the same. More specifically, the present invention relates to a method for manufacturing a microneedle patch having a pattern, a method for manufacturing a female mold used to manufacture such a microneedle patch, and a microneedle patch having a pattern. [Background technology]
[0002] In recent years, in order to aim for a society where humans and animals can coexist, it has become necessary to know the habits of animals well and to treat them appropriately. In particular, in the management of animals, relevant laws require that industrial animals and household animals (pets) be tagged for identification purposes in order to identify individuals and manage their information accordingly. Labeling is also mandatory for laboratory animals, in order to manage individuals or groups during experiments.
[0003] Conventional methods for identifying individual animals involve attaching external or internal tags to the body, such as by fixing a separate tag to a specific location (e.g., ear tags), by punching a hole in a specific location (e.g., ear punches), by tattooing with a needle punch (e.g., tattoo machines with needles), or by implanting a microchip in the body through minor surgery (e.g., subcutaneous implantation of a Radio Frequency Identification (RFID) chip).
[0004] However, these methods require the preparation and production of tags according to separate standards, the use of external tools that require sterilization and disinfection, and the need for procedures by qualified professionals (veterinarians) and measures to prevent secondary infections related to the tools and post-processing. These preparations require time and effort, and also incur additional financial costs. They may also cause physical and mental stress and pain to the animals.
[0005] In recent years, arrays of needle structures with micro dimensions (lengths of about 1 mm or less), called microneedles, microneedle arrays, or microneedle array patches, have been attracting attention. Microneedles are made of biocompatible materials, and are characterized by being minimally invasive, enabling almost painless transdermal drug delivery, and being easy for anyone to use.
[0006] It has been investigated to label animals by attaching a microneedle patch having a fine needle structure made of such a material that dissolves in the body to the skin of the animal (Patent Document 1). However, in order to efficiently identify many individual animals, it is necessary to mark the animal's skin with various patterns or designs as markers, but an effective method for achieving this has not yet been found. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] WO2019 / 018301A1 [Non-patent literature]
[0008] [Non-Patent Document 1] Bao, L., Park, J., Bonfante, G. et al. Recent advances in porous microneedles: materials, fabrication, and transdermal applications. Drug Deliv. and Transl. Res. 12, 395-414 (2022). [Non-Patent Document 2] Yeu-Chun Kim, Jung-Hwan Park, Mark R. Prausnitz, Microneedles for drug and vaccine delivery, Advanced Drug Delivery Reviews, Volume 64, Issue 14, 2012, Pages 1547-1568, Summary of the Invention Problem to be solved by the invention
[0009] An object of the present invention is to provide a method for efficiently manufacturing a microneedle array or a microneedle patch having a pattern, and a method for manufacturing a female mold used for manufacturing such a microneedle array or a microneedle patch. [Means for solving the problem]
[0010] In the manufacture of microneedle patches, the micromolding method is usually used to mass-produce uniform patch products. In the micromolding method, it is essential to create a female mold, a casting mold, from a master mold that has the same external shape as the final product. In other words, mass production of patch products is only possible using a female mold (see Figure 1). Here, to make one type of female mold, only one female mold can be obtained from one master mold for that purpose. To ensure its strength, the master mold is made from high-strength metal materials and special processing. Therefore, it takes time and high processing costs to make a different female mold each time. Therefore, in order to produce microneedle arrays with different patterns, it is necessary to create a new master mold. Furthermore, when manufacturing microneedle patches that require design changes depending on the application site, it is necessary to create many new molds.
[0011] In order to solve the problems of the present invention, the inventors conducted intensive research into the above problems and discovered that by using a plug having a specific structure, a microneedle patch having a pattern can be efficiently manufactured, thereby completing the present invention. Furthermore, the inventors continued their research and discovered that patterned microneedle patches can also be efficiently manufactured by patterning a photoresist using a photolithography process, thereby completing the present invention.
[0012] That is, the present invention has the following configuration. [1] A method for producing a female mold having a pattern, comprising the steps of: (a) providing a female base mold having a plurality of cavities; (b) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (c) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; and (d) curing the resin A and then removing the plug. Including, the plurality of needle structures are arranged in a pattern on the plug similar to a pattern on the female mold; The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. The manufacturing method. [2] The manufacturing method described in [1], wherein the plug comprises a support layer, a plurality of needle structures provided on the support layer, and supports between the support layer and the needle structures. [3] A female mold having a pattern obtained by the manufacturing method described in [1] or [2]. [4] A method for producing a female mold having a pattern, comprising the steps of: (A) providing a female base mold having a plurality of cavities; and (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. Including, The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. The manufacturing method. [5] A female mold having a pattern obtained by the manufacturing method described in [4]. [6] A method for producing a patterned microneedle array, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution and removing the patterned microneedle array from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method. [7] A method for producing a patterned microneedle patch, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6a) drying the solution and, after drying, attaching and removing the patterned microneedle array to a supporting sheet; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method. [8] A method for producing a patterned microneedle patch, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution and removing the patterned microneedle patch from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method. [9] The method according to any one of [6] to [8], wherein the solution containing a biosoluble material contains a dye and / or a pigment.
[10] The method of any one of [6] to [9], wherein the plug comprises a support layer, a plurality of needle structures provided on the support layer, and a support between the support layer and the needle structures.
[11] A plug used to manufacture a female mold having a pattern, a support layer, a plurality of needle structures provided on the support layer, and a support post between the support layer and the needle structures; the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The plug in question.
[12] The plug according to
[11] , manufactured by a 3D printer.
[13] A method for producing a patterned microneedle array, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle array from the female mold after drying; Including, The manufacturing method.
[14] A method for producing a patterned microneedle patch, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D1) drying the solution or suspension and, after drying, attaching the microneedle array having the pattern to a supporting sheet and removing it; Including, The manufacturing method.
[15] A method for producing a patterned microneedle patch, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle patch from the female mold after drying; Including, The manufacturing method.
[16] The method for producing a composition according to any one of
[13] to
[15] , wherein the solution containing a biosoluble material contains a dye and / or a pigment.
[17] A microneedle structure having a pattern, the microneedle structure comprising a biosoluble polymer and an insoluble material; and A support sheet including a biocompatible or biosoluble polymer; Microneedle patches used to tattoo specific areas of the eyebrows or scalp.
[18] A microneedle structure having a pattern, the microneedle structure comprising a biosoluble polymer and an insoluble material; and A support sheet comprising a biocompatible polymer or a biosoluble polymer; Equipped with two microneedle patches, The pattern of the fine needle structures in each microneedle patch is symmetrical. A microneedle package used to tattoo specific areas of the eyebrows or scalp. Effect of the Invention
[0013] According to the present invention, by additionally producing plugs for one master mold, it is possible to produce a plurality of types of female molds with various patterns. In addition, there is no need to recreate the master mold when changing the design of the microneedle patch, saving costs and time. In addition, since patterns can be freely produced, it is possible to produce microneedle patches with a variety of patterns, and it is also possible to produce microneedle patches of different shapes. Furthermore, the microneedle patch obtained by the present invention can precisely form a patterned fine needle structure, and can provide a fine needle structure having a bilaterally symmetrical pattern, making it suitable for use, for example, when tattooing specific areas of the eyebrows or scalp. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 shows a schematic diagram of the fabrication process of a microneedle patch using a conventional female mold. [Diagram 2] A method for producing a female mold of the present invention and a method for producing a microneedle patch having a pattern using the female mold are described below. [Diagram 3] 1 shows a schematic diagram of a plug of the present invention. [Figure 4] FIG. 1 shows a schematic diagram of a non-limiting example of a plug of the present invention. [Diagram 5] 1 shows a schematic diagram of a non-limiting example of a microneedle patch of the present invention. [Figure 6] 1 shows a microneedle patch for labeling in which the fine needle structure produced in Example 1 is formed. [Figure 7] 4 shows the results of a patch application experiment in Example 2. [Figure 8] 1 shows the results of verifying the injection of a character pattern into the skin of an experimental animal (rat) using the labeling microneedle patch having the character pattern prepared in Example 1. [Figure 9] FIG. 2 shows a non-limiting schematic diagram of manufacturing method B of the microneedle array of the present invention. [Figure 10] 1 shows a photograph of the patterned microneedle patch obtained in Example 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] 1. Method for producing a female mold having a pattern (1-1) Manufacturing method 1 of the female mold of the present invention One embodiment of the invention is a method for making a female mold having a pattern, comprising the steps of: (a) providing a female base mold having a plurality of cavities; (b) inserting a plug having a plurality of needle structures into the female base mold; The plurality of needle structures are inserted into a cavity in a portion of the female base mold, (c) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; and (d) curing the resin and then removing the plug. Including, the plurality of needle structures are arranged in a pattern on the plug similar to a pattern on the female mold; The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. This manufacturing method (hereinafter also referred to as "method 1 for manufacturing the female mold of the present invention").
[0016] As used herein, a microneedle patch refers to a patch in which individual microneedles or a microneedle array are attached (by adhesion, welding, fusion, etc.) to a substrate of a certain size and flexibility. Furthermore, a microneedle array means a state in which a plurality of microneedles are formed in a specific arrangement, and may be simply arranged (without a substrate). Microneedle arrays also include those in which a plurality of microneedles are integrally formed and erected on a base element (microneedle substrate) made of the same or a different material as the microneedles.
[0017] In this specification, the female base mold refers to a female micromold (metal mold) that is commonly used in the micromolding method. The female base mold is prepared from a metal master mold consisting of a large number of microneedles. The material of the female base mold is preferably polydimethylsiloxane (PDMS), SUS, etc. The shape and size of the microneedles of the metal master mold can be appropriately determined according to the shape and size of the desired microneedle.
[0018] The female base mold may have only a plurality of cavities on its surface that correspond to the template shape of the microneedles to be prepared. The female base mold may have a recessed portion of a predetermined depth on its entire surface, and may have multiple cavities at the bottom of the recessed portion. In this case, since the recessed portion corresponds to the shape of the microneedle substrate, a microneedle array in which multiple microneedles are joined to and stand on the microneedle substrate (base element) can be efficiently obtained. The female base mold can have a desired number of cavities. The cavities can be provided vertically and horizontally as appropriate. The interval between the cavities is preferably 500 to 5000 μm.
[0019] A schematic diagram of a female mold manufacturing method 1 of the present invention is shown in FIG.
[0020] The above-mentioned female base mold is prepared (FIG. 2(a)), and a plug having multiple needle structures is inserted into this female base mold (FIG. 2(b)). At this time, the multiple needle structures of the plug are inserted into only some of the cavities of the female base mold.
[0021] This plug is a plug for making a pattern. The plug used in the method for producing a female mold of the present invention is also called the "plug of the present invention." In the plug of the present invention, the needle structures are arranged in a pattern similar to the pattern to be imparted to the female base mold. Figure 3 shows a schematic diagram of the plug of the present invention. In the diagram of Fig. 3(a), the multiple needle structures are arranged so that the character pattern "A1" can be applied to the female base mold. In this case, the needle structures are inserted into the cavities of the female base mold so as to correspond to the character pattern "A1".
[0022] A schematic diagram of a non-limiting example of a plug of the present invention is shown in FIG. The plug of the present invention preferably has a structure including a support layer, a plurality of needle structures disposed on the support layer, and support posts between the support layer and the needle structures.
[0023] That is, one preferred embodiment of the plug of the present invention is a plug used for producing a female mold having a pattern, A support layer, a plurality of needle structures provided on the support layer, and a support post between the support layer and the needle structures, The plurality of needle structures are arranged in the plug in a pattern similar to the pattern in the female mold. Here, the female mold having the above pattern is used to manufacture a microneedle array or a microneedle patch.
[0024] The support layer has a role of fixing the support pillars located below it. In order to prevent distortion of the plug pillars, the thickness of the support layer is preferably 3 mm or more, and more preferably about 3 to 5 mm.
[0025] The needle structure at the tip of the plug has a shape and size similar to the cavity in the female base mold so that it can fit into the cavity. The needle structure of the plug is preferably designed to have the same shape as the master mold, with dimensions approximately 10% smaller than the design values of the master mold, so that the tip of the plug can fit directly into the groove made from the tip shape of the female master mold made from the master mold.
[0026] The support of the plug serves to create a space when filling with a solution containing a resin, which will be described later. In order to ensure a space for injecting a solution from the side when the plug is inserted into the female master mold, the length of the support is preferably about 5 to 10 mm.
[0027] Furthermore, when the plug is large in size, it is preferable that the plug has only a support without a needle structure at the tip.
[0028] The plug of the present invention is preferably manufactured using a 3D printer. By manufacturing using a 3D printer, it is possible to manufacture the plug cheaply and easily. More preferably, the plug of the present invention is produced using a stereolithography 3D printer or a fused deposition model 3D printer using the designed drawing. Here, in consideration of the precision of the tip of the plug, which has a micro-dimension that can be fitted into the cavity of the female base mold, and the roughness of the wall surface of the cavity formed by the plug, it is more preferable to use the stereolithography method. In addition, after production using a stereolithography 3D printer, it is preferable to clean off any surface residues and perform post-processing with UV irradiation to remove any residues caused by incomplete UV curing. This makes it possible to prevent a chemical reaction with the resin to be filled in when the cavity is filled with a solution containing resin A.
[0029] The material used to manufacture the plug of the present invention may be a resin that can be used with a 3D printer, such as an epoxy-based resin that can be cured at a wavelength of 405 nm, or an acrylate-based resin, or a mixture of both.
[0030] Furthermore, in the manufacturing method 1 of the female mold of the present invention, when a highly viscous resin solution is used, it is also effective to coat the surface of the plug with a hydrophobic water-repellent film to prevent the solution from adhering to the plug wall surface.
[0031] After placing the plug on the female base mold and inserting it, it is preferable to fix it with a weight of about 100 g (or using Capton tape, etc.). This improves adhesion and prevents the needle structure from entering the cavity when the solution described below is filled.
[0032] In step (c) of the manufacturing method 1 of the female mold of the present invention, the cavity into which the needle structure is not inserted is filled with a solution containing resin A that is the same as or similar to the resin that constitutes the female base mold (hereinafter also referred to as "solution A"). Polydimethylsiloxane (PDMS) is preferable as such resin A. The type, molecular weight, etc. of the polydimethylsiloxane of resin A may be the same as that of the polydimethylsiloxane constituting the female base mold, and it is better if it is a similar polymer that is crosslinked with polydimethylsiloxane. The solution preferably contains a crosslinking agent (curing agent). An example of a combination of base agent and curing agent that can be used in the present invention is a room temperature curing base agent (PDMS) and curing agent set (which uses platinum as a catalyst to cause a reaction that adds Si-H bonds to the base agent) sold by Dow Corning under the name SILPOT184 (SYLGARD184 overseas). The ratio of resin to hardener in solution A is preferably approximately the same as the ratio of resin to hardener used in producing the female base mold.
[0033] Solution A preferably also contains a solvent to reduce the viscosity. Any solvent that dissolves the above resins can be used, and examples of the solvent include cyclohexane, toluene, tert-butyl alcohol, chloroform, and decamethylcyclopentasiloxane.
[0034] The ratio of the resin (PDMS base material), curing agent, and solvent in solution A is preferably PDMS base material:curing agent:solvent=10:1:10 (mass ratio).
[0035] When filling the cavity with solution A, it is preferable to apply ultrasonic vibration to the female base mold to ensure uniform filling.
[0036] In step (c) of the female mold manufacturing method of the present invention, the resin is cured, and then the plug is removed. The resin is completely cured by heating for a predetermined time (for example, about 1 hour) on a hot plate set at about 50 to 60° C. Thereafter, the plug is removed to obtain a female mold having a pattern.
[0037] (1-2) Manufacturing method 2 of the female mold of the present invention The present inventors conducted further studies and found that a female mold having a pattern can also be manufactured by patterning a photoresist using a photolithography process, similar to the female mold manufacturing method 1 of the present invention. That is, another embodiment of the present invention is a method for manufacturing a female mold having a pattern, comprising: (A) providing a female base mold having a plurality of cavities; and (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) dissolving the photoresist layer using a solvent to obtain a female mold having a pattern; Including, The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. This is the manufacturing method (hereinafter also referred to as "manufacturing method 2 of the female mold of the present invention").
[0038] In manufacturing method 2 for the female mold of the present invention, by using photolithography, a conventional semiconductor manufacturing technology capable of producing fine patterns, it is possible to produce more precise patterns than in manufacturing method 1 for the female mold of the present invention which uses a plug, and this makes it possible to produce a mold with a fine pattern.
[0039] Here, the female mold manufacturing method 2 of the present invention includes an embodiment in which the step (a1) is used in the above step (B) (also referred to as "female mold manufacturing method 2a of the present invention"), and an embodiment in which the step (b1) is used (also referred to as "female mold manufacturing method 2b of the present invention").
[0040] Step (A) of the female mold manufacturing method 2 of the present invention corresponds to step (a) of the female mold manufacturing method 1 of the present invention, and its details are as described in the female mold manufacturing method 1 of the present invention.
[0041] In the female mold manufacturing method 2a of the present invention, step (a1) is used in step (B), which includes forming a photoresist layer on a female base mold (step 1), partially exposing the photoresist layer through a photomask (step 2), and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern (step 3).
[0042] The photoresist used in step 1 can be either a negative type or a positive type. Various types of photoresists can be used, including, but not limited to, AZ series photoresists (MicroChemical), S1800 series (Micro resist technology), OFPR / TSMR series (Tokyo Ohka Kogyo), and SU8 / KMPR series (Kayaku Advanced Materials).
[0043] To form a photoresist layer on the female base mold, a photoresist is applied onto the female base mold, and then baked (usually heated at about 100°C for about 1 to 10 seconds) to evaporate the solvent and harden the resist. The photoresist is usually applied by spin coating (1000 to 4000 rpm / 60 s). The thickness of the photoresist layer is not particularly limited, but is about 1.5 to 50 μm, and preferably about 1.5 to 10 μm.
[0044] The photomask used in step 2 has a pattern, and the pattern is selected according to the pattern of the female mold to be produced, depending on whether the photoresist used is positive type or negative type. For example, when a positive type photoresist is used, the solubility of the resist in the exposed area increases, and it dissolves in the subsequent development process, forming cavities, while the resist in the unexposed area remains, forming a pattern with filled cavities. On the other hand, when a negative-type photoresist is used, the solubility of the resist in the exposed areas decreases, and in the subsequent development process, the exposed areas remain and fill the cavities, while the unexposed areas of the resist dissolve, forming a pattern with cavities.
[0045] Exposure is typically performed at 50-350 mJ / cm after contacting a patterned photomask with the surface of the photoresist layer. 2 This is done by shining ultraviolet light with 1000 times the energy of the light.
[0046] As for the developer, the negative developer is an organic solvent developer, such as a solvent selected from ketones, esters, ethers, hydrocarbons, and mixtures thereof. The positive developer is an aqueous solution of a basic component, such as a solvent selected from potassium hydroxide, tetramethylammonium hydroxide, and mixtures thereof.
[0047] In the female mold manufacturing method 2b of the present invention, the process (b1) is used in the process (B), and the process includes steps (i) to (iii). Step (i) is to form a photoresist layer on the female base mold, partially expose the photoresist layer through a photomask, and immerse the exposed photoresist layer in a developer to obtain a female mold A having a pattern, which is basically the same as step (a1) in the female mold manufacturing method 2a of the present invention (to distinguish the resulting female mold A having a pattern, it is described as "female mold A having a pattern"). Here, the thickness of the photoresist layer formed in the step (b1) is preferably thicker than that of the photoresist layer formed in the step (a1) described above, and is preferably about 5 to 20 μm, for example. In the step (b1), in the step (ii) described below, a solution containing a resin A that is the same as or similar to the resin constituting the female base mold is filled into the hollow portion of the female mold A having the pattern obtained in (i), so it is preferable to make the boundary between the hollow portion and the portion where the photoresist layer is present clearer. By spin-coating the photoresist at a lower rotation speed (for example, 100 to 500 rpm / 60 s), it is possible to make the photoresist layer thicker.
[0048] In step (ii), the hollow portion of the female mold A having the pattern is filled with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold, and the resin A is cured. Here, the solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold (solution A) is the same as that used in step (c) in the female mold manufacturing method 1 of the present invention, and the details are as explained in the female mold manufacturing method 1 of the present invention.
[0049] In step (iii), the photoresist layer is dissolved using a solvent to obtain a female mold having a pattern. The solvent used here may be any solvent commonly used to dissolve photoresist, such as acetone or a photoresist remover (AZ remover 100, manufactured by MicroChemicals). In addition, in step (iii), the photoresist is dissolved using a solvent, so that the solidified material of Solution A (including PDMS, etc.) formed on the photoresist layer can be simultaneously removed (lifted off).
[0050] 2. Method for producing a patterned microneedle array or microneedle patch (2-1) Another embodiment of the present invention is a method for producing a patterned microneedle array, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) hardening the resin and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution and removing the patterned microneedle array from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; This is the manufacturing method (hereinafter also referred to as "manufacturing method A of the microneedle array of the present invention").
[0051] Steps (1) to (4) in the method for producing a microneedle array of the present invention are the same as steps (a) to (d) in the method for producing a female mold of the present invention described above.
[0052] In step (5) of the method for manufacturing a microneedle array of the present invention, a solution or suspension containing a biosoluble material (hereinafter also referred to as "solution B or suspension B") is injected into the female mold having the pattern obtained in step (4).
[0053] In this specification, a biosoluble material means a material that dissolves (dissolves) in the body when it comes into contact with bodily fluids in the body through a chemical reaction (mainly hydrolysis) and is eventually absorbed by the surrounding tissues. The biosoluble material used in the microneedle of the present invention is preferably biocompatible, that is, has a property that does not cause side reactions or the generation or reaction of foreign matter when the material comes into contact with tissues in the body. Such a biosoluble material is at least one selected from the group consisting of hyaluronic acid, polyvinyl alcohol, polyvinylpyrrolidone, and carboxymethylcellulose.
[0054] Solution B or suspension B means a liquid in which a biosoluble material is dissolved or dispersed in water or an organic solvent. Solution B can be obtained by dissolving the biosoluble material in water or an organic solvent. The organic solvent is not particularly limited as long as it dissolves the biodegradable material, and examples of the organic solvent include dichloromethane and acetone. Suspension B can be obtained by dispersing a biosoluble material in water (optionally with the addition of a surfactant).
[0055] Solution B or suspension B preferably contains a dye, a pigment. Preferably, the dye for marking the skin will penetrate pigmented skin, be resistant to photobleaching, be safe to the subject to which the microneedles are applied, have a relatively high quantum yield, high loading capacity, low background noise, and / or be resistant to variations in temperature, pH, or oxidation in an in vivo environment for at least 1 year, 2 years, 3 years, 4 years, 5 years, or longer. The dye is preferably an insoluble material. The dyes are selected from the group consisting of inorganic nanocrystals, lanthanide-based dyes, other fluorophores, and non-fluorescent contrast agents.
[0056] As the pigment, organic or inorganic pigments which are insoluble and have been recognized as safe for use in the body are preferred. When forming a tattoo pattern using the microneedle of the present invention, an insoluble pigment is usually used.
[0057] In one embodiment of the invention, the pigment is carbon or tattoo ink, or cosmetic ink. Carbon (soot or ash) is often used for black. Other elements used as pigments include antimony, arsenic, beryllium, calcium, copper, lithium, selenium, and sulfur. Tattoo ink manufacturers typically blend heavy metal pigments or use lightening agents (such as lead or titanium) to reduce production costs. Some pigments contain inorganic materials, such as ochre, or natural materials such as henna may be used.
[0058] In step (6) of the method for producing a microneedle array of the present invention, solution B is dried, and after drying, the microneedle array having a pattern is removed from the female mold. The drying is carried out, for example, in an environment with a relative humidity of about 5 to 10%, for about 24 to 30 hours.
[0059] Another aspect of the present invention is a method for producing a microneedle array of the present invention using a female mold having a pattern separately produced by the female mold production method 1 of the present invention. That is, another aspect of the present invention is a method for producing a patterned microneedle array, comprising: (0) providing a female mold having a pattern produced by the female mold manufacturing method 1 of the present invention; (5) injecting a solution containing a biodegradable material into the female mold having the pattern; and (6) drying the solution and removing the patterned microneedle array from the female mold after drying; Including, This is the manufacturing method (hereinafter also referred to as "manufacturing method A2 of the microneedle array of the present invention").
[0060] Another aspect of the present invention is a microneedle array obtained by the microneedle array manufacturing method A of the present invention or the microneedle array manufacturing method A2 of the present invention (hereinafter also referred to as "microneedle array A of the present invention").
[0061] The microneedle array of the present invention may be in a state in which a plurality of microneedles are formed in a specific arrangement, that is, in a simple arrangement state (without a substrate attached). Furthermore, the microneedle array A of the present invention may be one in which a plurality of microneedles are integrally formed and erected on a microneedle substrate made of the same or different material as the microneedles. For example, if the female base mold has a recessed portion of a predetermined depth on the entire surface and has a plurality of cavities at the bottom of the recessed portion, the recessed portion corresponds to the shape of the microneedle substrate, so that a microneedle array in which a plurality of microneedles are joined to and erected on the microneedle substrate (base element) can be obtained.
[0062] Another aspect of the present invention is a method for producing a patterned microneedle patch, comprising the steps of: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6a) drying the solution and, after drying, attaching and removing the patterned microneedle array to a supporting sheet; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; This manufacturing method is hereinafter also referred to as "manufacturing method A1 for the microneedle patch of the present invention."
[0063] Another aspect of the present invention is a method for producing a patterned microneedle patch, comprising the steps of: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution and removing the patterned microneedle patch from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; This manufacturing method (hereinafter also referred to as "manufacturing method A2 for the microneedle patch of the present invention").
[0064] Details of steps (1) to (6) in the microneedle patch manufacturing methods A1 and A2 of the present invention are as described in detail in the microneedle array manufacturing method A of the present invention.
[0065] Furthermore, in a different embodiment of the microneedle patch manufacturing methods A1 and A2 of the present invention, similarly to the microneedle array manufacturing method A2 of the present invention, instead of steps (1) to (4), a step of providing a female mold having a pattern produced by the female mold manufacturing method of the present invention can be provided as step (0) before step (5). These embodiments are also referred to as "the microneedle patch manufacturing method A1b of the present invention" and "the microneedle patch manufacturing method A2b of the present invention", respectively.
[0066] Another aspect of the present invention is a microneedle patch obtained by the microneedle patch manufacturing method A1, A1b, A2 or A2b of the present invention (hereinafter also referred to as "microneedle patch A of the present invention").
[0067] The microneedle patch A of the present invention is configured such that individual microneedles or a microneedle array are attached (by adhesion, welding, fusion, etc.) onto a substrate (support sheet) having a certain size and flexibility. The support sheet may be formed from the same biosoluble material as the microneedles, or may be composed of other biocompatible materials. Biocompatible materials include polylactic acid, polyglycolic acid, poly(lactide-co-glycolide) copolymers, PEG copolymers, polyhydroxybutyric acid, ethylcellulose, and the like.
[0068] The support sheet in the microneedle patch A of the present invention may be a sheet-like sheet prepared separately. Such a microneedle patch is manufactured by the manufacturing method A1 or A1b of the microneedle patch of the present invention. In this case, when removing the microneedle array having a pattern from the female mold in step (6a), the microneedle array is attached to a support sheet prepared separately and removed to obtain a microneedle patch having a pattern.
[0069] In the microneedle patch A of the present invention, when the microneedles and the support sheet are made of the same material, they are produced by the microneedle patch production method A2 or A2b of the present invention. Specifically, in step (5), when a solution or suspension containing a biosoluble material is injected into the female mold, an amount of solution or suspension corresponding to the thickness of the support sheet is filled, this is dried, and after drying, it is removed from the female mold to obtain the microneedle patch of the present invention. Furthermore, in step (5), when the solution or suspension containing the biosoluble material is injected into the female mold, the solution or suspension containing the biosoluble material, dye and / or pigment is injected only into the hollow portion of the female mold, and the portion corresponding to the thickness of the support sheet is filled with a solution or suspension containing the biosoluble material but not the dye and / or pigment, which is then dried and removed from the female mold after drying to obtain the microneedle patch of the present invention.
[0070] Furthermore, the microneedle patch A of the present invention, in which the support sheet is made of other biocompatible materials, can also be obtained by injecting a solution or suspension containing a biosoluble material, dye and / or pigment only into the hollow part of the female mold when injecting a solution or suspension containing a biosoluble material into the female mold in step (5) of the manufacturing method A2 or A2b of the microneedle patch of the present invention, filling the part corresponding to the thickness of the support sheet with a solution or suspension containing other biocompatible materials, drying this, and removing it from the female mold after drying. Such a manufacturing method of the microneedle patch is also within the scope of the present invention.
[0071] A schematic diagram of a non-limiting example of microneedle patch A of the present invention is shown in FIG. The microneedle patch of the present invention has a fine needle structure having a pattern composed of a biosoluble polymer and preferably an insoluble material. The microneedle patch of the present invention also has a support sheet made of a biocompatible polymer or a biosoluble polymer.
[0072] (2-2) The present inventors conducted further studies and found that a microneedle array or microneedle patch having a pattern can be manufactured by patterning a photoresist using a photolithography process, similarly to the manufacturing method A of the microneedle array of the present invention and the manufacturing method A of the microneedle patch of the present invention. That is, another embodiment of the present invention is a method for manufacturing a microneedle array having a pattern, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle array from the female mold after drying; Including, This is the manufacturing method (hereinafter also referred to as "manufacturing method B of the microneedle array of the present invention").
[0073] In the microneedle array manufacturing method B of the present invention, steps (A) to (B) are the same as steps (A) to (B) in the female mold manufacturing method 2 of the present invention, and the details are as described in the female mold manufacturing method 2 of the present invention. Furthermore, steps (C) to (D) of manufacturing method B of the microneedle array of the present invention are substantially the same as steps (5) to (6) of manufacturing method A of the microneedle array of the present invention, and the details are as explained in manufacturing method A of the microneedle array of the present invention.
[0074] A non-limiting schematic diagram of manufacturing method B of the microneedle array of the present invention is shown in FIG. In Figure 9, the method consisting of steps (a) to (d) in the upper row shows a non-limiting schematic diagram of manufacturing method B of a microneedle array of the present invention, in which step (a1) is used in step (B) above. In addition, in Figure 9, the method consisting of steps (a), (b), (c') to (e') and (f') represents a non-limiting schematic diagram of manufacturing method B of the microneedle array of the present invention, in which step (b1) is used in step (B) above.
[0075] Another aspect of the present invention is a method for producing a microneedle array of the present invention using a female mold having a pattern separately produced by the female mold production method 2 of the present invention. That is, another aspect of the present invention is a method for producing a patterned microneedle array, comprising: (0') a step of providing a female mold having a pattern produced by the female mold manufacturing method 2 of the present invention; (C) injecting a solution or suspension containing a biodegradable material into the female mold having the pattern; and (D) drying the solution or suspension and removing the patterned microneedle array from the female mold after drying; Including, This is the manufacturing method (hereinafter also referred to as "manufacturing method B2 of the microneedle array of the present invention").
[0076] Another aspect of the present invention is a microneedle array obtained by the microneedle array manufacturing method B of the present invention or the microneedle array manufacturing method B2 of the present invention (hereinafter also referred to as "microneedle array B of the present invention").
[0077] The microneedle array B of the present invention may be in a state where a plurality of microneedles are formed in a specific arrangement, that is, in a simple arrangement state (without a substrate attached). Furthermore, the microneedle array B of the present invention may be one in which a plurality of microneedles are integrally formed and erected on a microneedle substrate made of the same or a different material as the microneedles. For example, if the female base mold has a recessed portion of a predetermined depth on the entire surface and has a plurality of cavities at the bottom of the recessed portion, the recessed portion corresponds to the shape of the microneedle substrate, so that a microneedle array in which a plurality of microneedles are joined to and erected on the microneedle substrate (base element) can be obtained.
[0078] Another aspect of the present invention is a method for producing a patterned microneedle patch, comprising the steps of: 1. A method for manufacturing a patterned microneedle patch, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) a step of applying a photoresist layer to the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) applying a photoresist layer to the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D1) drying the solution or suspension and, after drying, attaching the microneedle array having the pattern to a supporting sheet and removing it; Including, This is the manufacturing method (hereinafter also referred to as "manufacturing method B1 for the microneedle patch of the present invention").
[0079] Another aspect of the present invention is a method for producing a patterned microneedle patch, comprising the steps of: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, the step being the following step (a1) or (b1); (a1) a step of applying a photoresist layer to the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the following steps (i) to (iii): (i) applying a photoresist layer to the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle patch from the female mold after drying; Including, This manufacturing method (hereinafter also referred to as "manufacturing method B2 for the microneedle patch of the present invention").
[0080] Details of steps (A) to (D) or (D1) in the microneedle patch manufacturing methods B1 and B2 of the present invention are as described in detail in the microneedle array manufacturing method B of the present invention and the microneedle patch manufacturing methods A1 and A2 of the present invention.
[0081] Furthermore, in a different embodiment of the microneedle patch manufacturing methods B1 and B2 of the present invention, similarly to the microneedle array manufacturing method B2 of the present invention, instead of steps (A) to (B), a step of providing a female mold having a pattern produced by the female mold manufacturing method 2 of the present invention can be provided as step (0') before step (C). These embodiments are also referred to as "the microneedle patch manufacturing method B1b of the present invention" and "the microneedle patch manufacturing method B2b of the present invention", respectively.
[0082] In the manufacturing method B of the microneedle array of the present invention and the manufacturing methods B1 and B2 of the microneedle patch of the present invention, photolithography, a conventional semiconductor manufacturing technology capable of producing fine patterns, is used, which makes it possible to produce more precise patterns than in the manufacturing method A of the microneedle array of the present invention using the plug described above, thereby making it possible to produce a microneedle array or microneedle patch having a fine pattern.
[0083] Another aspect of the present invention is a microneedle patch obtained by the microneedle patch manufacturing method B1, B1b, B2 or B2b of the present invention (hereinafter also referred to as "microneedle patch B of the present invention").
[0084] The microneedle patch B of the present invention is configured such that individual microneedles or a microneedle array are attached (by adhesion, welding, fusion, etc.) onto a substrate (support sheet) having a certain size and flexibility. Details of the support sheet and biocompatible material are the same as those described in detail for the microneedle patch A of the present invention.
[0085] The support sheet in the microneedle patch B of the present invention may be a sheet-like sheet prepared separately. Such a microneedle patch is manufactured by the manufacturing method B1 or B1b of the microneedle patch of the present invention. In this case, when removing the microneedle array having a pattern from the female mold in step (D1), the microneedle array is attached to a support sheet prepared separately and removed to obtain a microneedle patch having a pattern.
[0086] In the microneedle patch B of the present invention, when the microneedles and the support sheet are made of the same material, they are produced by the microneedle patch production method B2 or B2b of the present invention. Specifically, in step (C), when a solution or suspension containing a biosoluble material is injected into a female mold, an amount of solution or suspension corresponding to the thickness of the support sheet is filled, this is dried, and after drying, it is removed from the female mold to obtain the microneedle patch B of the present invention. Furthermore, in step (C), when the solution or suspension containing the biosoluble material is injected into the female mold, the solution or suspension containing the biosoluble material, dye and / or pigment is injected only into the hollow portion of the female mold, and the portion corresponding to the thickness of the support sheet is filled with a solution or suspension containing the biosoluble material but not the dye and / or pigment, which is then dried and, after drying, removed from the female mold to obtain the microneedle patch B of the present invention.
[0087] In addition, the microneedle patch B of the present invention, in which the support sheet is made of other biocompatible materials, can be obtained by injecting a solution or suspension containing a biosoluble material, dye and / or pigment only into the hollow part of the female mold when injecting a solution or suspension containing a biosoluble material into the female mold in step (C) of the manufacturing method B2 or B2b of the microneedle patch of the present invention, filling the part corresponding to the thickness of the support sheet with a solution or suspension containing other biocompatible materials, drying it, and removing it from the female mold after drying. Such a manufacturing method of the microneedle patch is also within the scope of the present invention.
[0088] The diameter of the fine needles (i.e., microneedles) of the microneedle patch of the present invention (hereinafter, also referred to as "microneedle patches of the present invention", including microneedle patches A and B of the present invention) is usually 10 μm to 60 μm. The diameter or maximum dimension of the base is, for example, about 50 μm to 800 μm. The height of the fine needles (microneedles), which determines the depth of penetration into the skin, is preferably 300 μm or more and 1500 μm or less in the microneedle patch of the present invention, so as to reach the dermis without stimulating pain sensation.
[0089] The interval between the microneedles is preferably 500 μm to 5000 μm.
[0090] Regarding the angle of the tip of the microneedle, the larger the angle, the greater the mechanical strength, but the greater the force required for penetration. A tip angle of 15 to 30° is preferable, since the force required for the microneedle to penetrate is less than 0.2 N.
[0091] The microneedle patch of the present invention has an array of fine needle structures, and can provide a new labeling method using the same. Since the labeling process is completed by attaching the microneedle patch, it is possible to save time and money, or reduce the associated losses, compared to conventional labeling methods.
[0092] In terms of the structure of the needle structure, its length and width are in the micron (1 / 1000 mm) unit, and the length can be adjusted during the manufacturing process. Therefore, a microneedle patch for labeling that takes into account the thickness of the skin of the animal to be labeled can be manufactured without changing the manufacturing method. Therefore, it is considered that the method can be applied to various animals. In addition, the pain caused by the attachment can be minimized because the tag does not reach the skin layer where pain sensory nerves are present. As a result, it is no longer necessary to anesthetize or restrain animals, as is done in conventional tagging. Furthermore, since tagging can be done simply by attaching the tag to the skin, there is no need for anesthesia or post-treatment such as hemostasis, so the presence of medical professionals is not required and tagging can be performed by ordinary people as well. Furthermore, when the preparation process is completed, the finished patch is in a dry state (the patch in the embodiment of the invention), so that it can be stored and managed for a long period of time at room temperature.
[0093] In terms of materials, the needle structure itself is made of a biocompatible soluble material (bioresistance polymers including carboxymethylcellulose and hyaluronic acid) that dissolves in the body, so after application to the skin, all of the needle structure except for the insoluble ink dissolves and is absorbed into the body. As a result, only the support sheet of the patch remains, eliminating the need for marking tools and reducing waste. In addition, there is no leakage of bodily fluids, eliminating the risk of secondary infection that was previously required when marking. During labeling, only the insoluble substances (inks containing organic or inorganic pigments, artificial and natural compounds) contained in the needle structures remain in the skin. In this case, the arrangement of the needle structures is designed into a specific letter or number pattern, so that after application to the skin, the insoluble substances are injected into the skin according to the pattern design. The insoluble substances injected into the skin are repeatedly captured and discharged by macrophage cells in the skin layer, so that they remain permanently unless the insoluble substances are physically removed. As a result, labeling can be easily performed with a single procedure of applying a microneedle patch, and there is no need for re-application due to the fall-off of the conventional labeling tag.
[0094] 3. Application of the microneedle patch of the present invention As described above, the microneedle patch of the present invention can be suitably used for labeling animals (industrial animals and domestic animals (pets)) for identification purposes.
[0095] In addition, the microneedle patch of the present invention is preferably manufactured using a plug manufactured by a 3D printer or by photolithography, so that a fine needle structure having a pattern can be formed densely. Therefore, according to the present invention, for example, a pair of microneedle patches having a microneedle structure with a bilaterally symmetrical pattern and narrow microneedle intervals can be obtained. Currently, tattooing of a black pigment on a specific part of the eyebrow or scalp, which is one type of cosmetic surgery, is performed by dermatologists or cosmetic surgeons using needles one by one. Therefore, tattooing of a specific part of the eyebrow or scalp requires highly skilled techniques, and tattooing of both eyebrows requires even higher skills. The microneedle patch of the present invention can provide a fine needle structure having a symmetrical pattern, and can be suitably used for tattooing of specific parts of the eyebrow or scalp.
[0096] Thus, another embodiment of the present invention comprises a microneedle structure having a pattern comprising a biosoluble polymer and an insoluble material; and A support sheet including a biocompatible or biosoluble polymer; The microneedle patch is used for tattooing specific areas of the eyebrows or scalp (hereinafter also referred to as "microneedle patch X of the present invention"). The biosoluble polymer, biocompatible polymer, shape of the microneedles, etc. are as described above for the microneedle patch of the present invention.
[0097] The insoluble substance is preferably an ink containing organic or inorganic pigments; when making a black tattoo, carbon (soot or ash) is often used. Other elements used as pigments include antimony, arsenic, beryllium, calcium, copper, lithium, selenium, and sulfur. Tattoo ink manufacturers typically blend heavy metal pigments or use lightening agents (such as lead or titanium) to reduce production costs. Some pigments contain inorganic materials, such as ochre, or natural materials such as henna may be used. Furthermore, by using a pigment other than black, the microneedle patch X of the present invention can also be used for dyeing or coloring eyebrows or thinning hair areas.
[0098] Another aspect of the present invention is a microneedle structure having a pattern comprising a biosoluble polymer and an insoluble material; and A support sheet comprising a biocompatible polymer or a biosoluble polymer; Equipped with two microneedle patches, The pattern of the fine needle structures in each microneedle patch is symmetrical. A microneedle package used to tattoo specific areas of the eyebrows or scalp. The insoluble substance is as described for the microneedle patch X of the present invention.
[0099] Furthermore, in the microneedle patch of the present invention, by using a time-aging ink as the insoluble substance, it is possible to provide a tattoo-type patch that is effective only for a specific period of time. That is, another aspect of the present invention is a microneedle structure having a pattern comprising a biosoluble polymer and an aging ink; and A support sheet comprising a biocompatible polymer or a biosoluble polymer; It is a tattoo-type microneedle patch. Long-acting inks include henna or jagua tattoo inks, which are primarily derived from plants. However, in this case, it is necessary to adjust the length of the microneedle to about 300 microns and deliver the ink to the shallow epidermis layer of the skin, because if it enters the deep dermis layer, it may remain there.
[0100] The microneedle patch of the present invention can also be used as a cosmetic patch to hide scars. That is, another aspect of the present invention is a microneedle structure having a pattern comprising a biosoluble polymer and an insoluble material; and A support sheet comprising a biocompatible polymer or a biosoluble polymer; This is a microneedle patch used in cosmetic patches to hide scars. Cosmetic patches for hiding scars can basically be applied to any scar on the skin, but considering the size of the microneedle patch, the face, neck, arms, etc. can be mentioned as suitable areas for application. EXAMPLES
[0101] The present invention will be described below based on examples, but the present invention is not limited to these.
[0102] (1)Equipment Wire EDM: Product name: Robofil 2030si (manufactured by CHARMILLES) Photopolymerization 3D printer: Product name Mars 3 (manufactured by ELEGOO) (2) Material Combination of polydimethylsiloxane (PDMS) base agent and hardener: Product name: SILPOT184 (known overseas as SYLGARD184; manufactured by Dow Corning) The above combination of base agent and curing agent was used to create the female base mold and for the PDMS mixture. Hyaluronic acid (molecular weight 14 kDa; Contipro Inc.) Tattoo ink solution (Carbon black: World Famous Tattoo Ink)
[0103] 1. Plug Preparation (1) Design details Tip: It has the same shape as the master mold, and its dimensions are designed to be 10% less than the design values of the master mold. This is so that the tip of the plug fits directly into the groove made from the tip shape in the female mold made from the master mold. However, the center distance of each microneedle is the same dimension as the master mold or the female mold. Support: To ensure space for injecting the mixed liquid from the side when the plug is inserted into the female mold, the support was made in the range of 5 to 10 mm (final design: 10 mm). Support layer: 3 to 5 mm thick to prevent distortion of the plug support. (2) Using the designed drawings, create the product using a stereolithography 3D printer. The plug used in Example 1 was produced based on the above design.
[0104] [Example 1] The fabrication process of a microneedle patch for labeling with a specific pattern is shown in Figure 2. In this process, a metal male mold with a microneedle structure of a certain length (900 microns in this case) and shape (pyramid) was first fabricated by machining. Then, using the male mold as a mold, a female mold of the same shape was fabricated by filling it with silicone resin (polydimethylsiloxane) and curing it in an oven at 85°C (Figure 2(a)). After that, in order to process the female mold into a mold capable of producing microneedle patches with a specific pattern, a plug for pattern production was inserted into the female mold and fixed by applying pressure (Fig. 2(b)). Here, the plug for pattern production was produced using a stereolithography 3D printer. The plug had a pattern shape designed to fill in the unnecessary parts of the cavity in the female mold when forming the character pattern (Fig. 3). After inserting the plug, a mixture of silicone resin diluted with an organic solvent was poured in and cured, and then the plug was removed to create a female mold that can be used to create a patch with a character pattern with specific areas filled in (Figure 2(c)).The mold was then filled with a mixture of insoluble ink (tattoo ink used here) and a soluble polymer solution, and dried to create a microneedle patch for labeling, with fine needle structures formed only in the areas that correspond to the specific character pattern (Figure 2(df) and Figure 6).
[0105] The details of the fabrication process of the microneedle patch having the pattern of Example 1 are as follows. 1. A master mold of a metal microneedle patch was fabricated using wire EDM (or NC machining). 2. The master mold, silicone rubber (polydimethylsiloxane, PDMS) base agent, and hardener were mixed in a mass ratio of 10:1 and placed in a container, degassed by vacuuming, and placed in an oven at 85°C to harden for 1 hour. After that, the female base mold was obtained by demolding. (a) 3. The plug described below was placed on the base mold and fixed with a 100 g weight (or with Capton tape, etc.) (to improve adhesion and prevent the mixed liquid from entering the grooves). 4. Mix the silicone rubber (polydimethylsiloxane, PDMS) base, curing agent, and hexane (or DOWSIL (registered trademark), 200 Fluid) in a mass ratio of 10:1:10 to create a low-viscosity PDMS mixture. The mixture from step 3 was poured into the mold from step 2. (b) 5. The plug was removed after heating on a hot plate set at 60°C for 30 minutes and allowing it to completely harden. (c) 6. A mixture was prepared by mixing 10% hyaluronic acid (molecular weight 14 kDa) solution and tattoo ink solution (carbon black) in a volume ratio of 7:1. The mixture of 7.6 was poured into the patterned mold made in 5, and then dried for 24 hours in an environment of 5% or less. (e) 8. After drying, the patterned microneedle patch was removed from the mold. (f)
[0106] [Example 2] In animal experiments, rats were used to confirm the injection of insoluble ink into the skin using a labeling microneedle patch made from an insoluble ink mixture and the persistence of the label over a long period of time. Here, a microneedle patch without a letter pattern was applied to the back of a rat, and the persistence of the injected insoluble ink was confirmed on the first day, one week, and one month after application (Figure 7). As a result, it was confirmed that the ink that had entered the skin remained even after one month, and its shape remained the same as when it was first injected.
[0107] [Example 3] Using the labeling microneedle patch having the character pattern prepared in Example 1, the injection of the character pattern into the skin of an experimental animal (rat) was verified (Figure 8). The results confirmed that by attaching the patch, the insoluble ink was injected into the skin through the fine needle structure according to the pre-designed character pattern, and the character pattern was formed.
[0108] [Example 4] Next, instead of using plugs, a patterned microneedle patch was fabricated by patterning a photoresist using a photolithography process. The details of the fabrication process of the microneedle patch having the pattern of Example 4 are as follows.
[0109] a) A fully hollow female mold was prepared using step 2 of Example 1. b) A photoresist was applied to the surface of the female mold by spin coating (at 4000 rpm / 60 s), and then baked at 110° C. for 5 minutes. A positive photoresist (AZ5214E, manufactured by MicroChemicals) was used. In this example, since a positive photoresist is used, the portion to fill the cavity is not exposed to light. A patterned photomask is then contacted with the surface and irradiated with 230 mJ / cm 2 The substrate was irradiated with ultraviolet light (wavelength: 405 nm) with an energy of 100 Hz. After exposure, the substrate was immersed in a developer to form a pattern (developer: AZ400K, manufactured by MicroChemicals). c) A solution containing the active ingredient for the microneedle patch used in Example 1 (a mixture of 10% hyaluronic acid (molecular weight 14 kDa) solution and tattoo ink solution (Carbon black) in a volume ratio of 7:1) was poured into the patterned mold obtained in b), and then the mold was placed in a vacuum chamber and degassed at 20 kPa for 1 hour, and then dried at room temperature for 24 hours. d) After drying, the patterned microneedle patch was removed from the mold.
[0110] A schematic diagram of the above steps and a photograph of the patterned microneedle patch obtained in Example 4 are shown in Figs. 9 and 10.
[0111] [Example 5] Another method using a photolithography process was used to fabricate patterned microneedle patches as follows.
[0112] a) A fully hollow female mold was prepared using step 2 of Example 1. b) A thick photoresist film was formed by spin-coating the photoresist at a lower rotation speed (e.g., 2000 rpm / 60 s) than in Example 4. The photoresist, baking conditions, ultraviolet irradiation conditions, and type of developer used were the same as in Example 4. c') The same diluted PDMS mixture as in Example 1 was poured into the hollow portion of the female mold. Then, the PDMS was cured (heated on a hot plate set at 60°C for 30 minutes as in Example 1). d') The photoresist was dissolved using acetone or a photoresist remover (AZ remover 100, MicroChemicals) to simultaneously remove the PDMS applied on top (lift-off), producing a patterned female mold. e') A patterned microneedle patch was obtained using the same process as in (c) to (d) of Example 4.
[0113] A schematic diagram of the above steps is shown in FIG.
Claims
1. 1. A method for manufacturing a female mold having a pattern, comprising the steps of: (a) providing a female base mold having a plurality of cavities; (b) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (c) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; and (d) curing the resin A and then removing the plug. Including, the plurality of needle structures are arranged in a pattern on the plug similar to a pattern on the female mold; The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. The manufacturing method.
2. The method of claim 1 , wherein the plug comprises a support layer, a plurality of needle structures disposed on the support layer, and posts between the support layer and the needle structures.
3. A female mould having a pattern obtained by the method according to claim 1 or 2.
4. 1. A method for manufacturing a female mold having a pattern, comprising the steps of: (A) providing a female base mold having a plurality of cavities; and (B) a step of obtaining a female mold having a pattern, comprising the following steps (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the steps of: (i) preparing a mixture of a carboxylic acid and a carboxylic acid; (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. Including, The female mold having the pattern is used to manufacture a microneedle array or a microneedle patch. The manufacturing method.
5. A female mould having a pattern obtained by the method according to claim 4.
6. 1. A method for manufacturing a patterned microneedle array, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution or suspension and removing the patterned microneedle array from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method.
7. 1. A method for manufacturing a patterned microneedle patch, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6a) drying the solution or suspension and, after drying, attaching and removing the patterned microneedle array to a supporting sheet; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method.
8. 1. A method for manufacturing a patterned microneedle patch, comprising: (1) providing a female base mold having a plurality of cavities; (2) inserting a plug having a plurality of needle structures into the female base mold, the plurality of needle structures being inserted into a cavity in a portion of the female base mold; (3) filling the cavity into which the needle structure is not inserted with a solution containing a resin A that is the same as or similar to the resin that constitutes the female base mold; (4) curing the resin A and then removing the plug to obtain a female mold having a pattern; (5) injecting a solution or suspension containing a biosoluble material into the female mold obtained in step (4); and (6) drying the solution or suspension and removing the patterned microneedle patch from the female mold after drying; Including, the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The manufacturing method.
9. The method according to claim 6 , wherein the solution containing a biosoluble material contains a dye and / or a pigment.
10. The method of claim 6 , wherein the plug comprises a support layer, a plurality of needle structures provided on the support layer, and a support post between the support layer and the needle structures.
11. A plug used to produce a female mold having a pattern, comprising: a support layer, a plurality of needle structures provided on the support layer, and a support post between the support layer and the needle structures; the plurality of needle structures are arranged in a pattern on the plug similar to the pattern on the female mold; The plug in question.
12. The plug of claim 11 manufactured by a 3D printer.
13. 1. A method for manufacturing a patterned microneedle array, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, comprising the following steps (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the steps of: (i) preparing a mixture of a carboxylic acid and a carboxylic acid; (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle array from the female mold after drying; Including, The manufacturing method.
14. 1. A method for manufacturing a patterned microneedle patch, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, comprising the following steps (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the steps of: (i) preparing a mixture of a carboxylic acid and a carboxylic acid; (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D1) drying the solution or suspension and, after drying, attaching the patterned microneedle array to a supporting sheet and removing it; Including, The manufacturing method.
15. 1. A method for manufacturing a patterned microneedle patch, comprising: (A) providing a female base mold having a plurality of cavities; (B) a step of obtaining a female mold having a pattern, comprising the following steps (a1) or (b1); (a1) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold having a pattern; (b1) A process comprising the steps of: (i) preparing a mixture of a carboxylic acid and a carboxylic acid; (i) forming a photoresist layer on the female base mold, partially exposing the photoresist layer through a photomask, and immersing the exposed photoresist layer in a developer to obtain a female mold A having a pattern; (ii) filling a hollow portion of the female mold A having the pattern with a solution containing a resin A that is the same as or similar to the resin constituting the female base mold, and hardening the resin A; and (iii) Dissolving the photoresist using a solvent to obtain a female mold having a pattern. (C) injecting a solution or suspension containing a biosoluble material into the female mold having the pattern obtained in step (2); and (D) drying the solution or suspension and removing the patterned microneedle patch from the female mold after drying; Including, The manufacturing method.
16. The method according to any one of claims 13 to 15, wherein the solution containing the biosoluble material contains a dye and / or a pigment.
17. a microneedle structure having a pattern comprising a biosoluble polymer and an insoluble material; and A support sheet including a biocompatible or biosoluble polymer; Microneedle patches used to tattoo specific areas of the eyebrows or scalp.
18. a microneedle structure having a pattern comprising a biosoluble polymer and an insoluble material; and A support sheet comprising a biocompatible polymer or a biosoluble polymer; Equipped with two microneedle patches, The pattern of the fine needle structures in each microneedle patch is symmetrical. A microneedle package used to tattoo specific areas of the eyebrows or scalp.
Citation Information