Manufacturing device for resin container, manufacturing method for resin container, and mold

The described resin container and manufacturing method address the limitations of stretch and direct blow molding by using a projecting portion and holding mechanism to achieve high eccentricity and improved aesthetic appearance with reduced resin waste.

JP2024164288AActive Publication Date: 2024-11-26NISSEI ASB MASCH CO LTD

Patent Information

Application Number
JP2024152241
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2018-12-20
Filing Date
2024-09-04
Publication Date
2024-11-26
Estimated Expiration
2039-12-19

AI Technical Summary

Technical Problem

Existing stretch blow molding methods struggle to produce resin containers with a high degree of eccentricity, while direct blow molding methods result in containers with inferior aesthetic appearance and require post-processing, leading to resin waste.

Method used

A resin container design with a projecting portion on the bottom, manufactured using a stretch blow molding method, where a holding mechanism grips and moves the protrusion outside the vertical projection of the neck to achieve a large eccentricity, and a manufacturing apparatus with a clamping and moving mechanism facilitates this process.

Benefits of technology

The method enables the production of resin containers with a high degree of eccentricity and improved aesthetic appearance without the need for post-processing, while minimizing resin waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164288000001_ABST
    Figure 2024164288000001_ABST
Patent Text Reader

Abstract

To provide a resin container which can be manufactured by using the stretch blow molding method and which has large eccentricity, to provide a manufacturing method for a resin container, to provide a manufacturing device for a resin container, and to provide a mold.SOLUTION: A resin container (10) includes: a neck part (12) where an entrance part (11) of a content is formed; a side surface part connected to the neck part; and a bottom part (14) arranged on the opposite side from the neck part, and connected to the side surface part. The resin container is manufactured by the stretch blow molding method. At the bottom part, an overhang part (25) is formed protruding vertically downward. The overhang part 25 is positioned in an eccentric region (S2) out of a region (S1) projected vertically from an opening surface of the entrance part (11) of the neck part, out of the bottom part.SELECTED DRAWING: Figure 1A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a resin container, a method for manufacturing a resin container, an apparatus for manufacturing a resin container, and a mold. [Background technology]

[0002] Patent Documents 1 to 5 disclose a method for manufacturing an eccentric container or a curved-neck container using a stretch blow molding method. For example, Patent Document 4 discloses a synthetic resin bottle-shaped container having at least two axes, in which the center of the opening of the mouth and the center of the bottom surface of the bottom are eccentric, by a biaxial stretch blow molding method. Patent Document 5 discloses a blow-molded container in which the central axis of the body is eccentric to the central axis of the mouth, by a blow molding method using liquid pressure as a pressurizing medium. Patent Document 6 discloses a method for manufacturing a curved container in which the central axes of the neck and the bottom are different from each other, by a direct blow molding method. Patent Document 7 discloses a method for molding a container for holding liquid detergents and the like, in which the neck is curved. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 2006-062110 [Patent Document 2] Japanese Patent Application Publication No. 2009-241429 [Patent Document 3] Japanese Patent Publication No. 2003-181907 [Patent Document 4] Japanese Patent Publication No. 2012-006317 [Patent Document 5] Japanese Patent Publication No. 2003-040233 [Patent Document 6] International Publication No. 2016 / 017059 [Patent Document 7] Japanese Patent Publication No. 08-207128 Summary of the Invention [Problem to be solved by the invention]

[0004] As described above, there are eccentric containers (off-center bottles) whose central axis of the neck is not coaxial with that of the body. Methods for manufacturing such eccentric containers include a manufacturing method using a direct blow molding method and a manufacturing method using a stretch blow molding method. Conventionally, a manufacturing method using a stretch blow molding method has been unable to manufacture a container with a large degree of eccentricity (the degree to which the central axis of the container neck is eccentric with respect to the central axis of the container body or the central axis of the container bottom). On the other hand, a container that can be manufactured using a direct blow molding method can have a larger degree of eccentricity than a container manufactured using a stretch blow molding method, but is inferior in terms of aesthetic appearance and dimensional accuracy. In addition, the direct blow molding method requires post-processing such as cutting off burrs remaining on the container after blow molding and trimming the cut surface. Furthermore, there is also a problem in that a large amount of resin is wasted (discarded). Under such a background, in recent years, there has been an increasing demand to manufacture containers with a large degree of eccentricity using a stretch blow molding method.

[0005] An object of the present disclosure is to provide a resin container with a large degree of eccentricity that can be produced using a stretch blow molding method, a method for producing a resin container, an apparatus for producing a resin container, and a mold. [Means for solving the problem]

[0006] A resin container according to one embodiment of the present disclosure that can solve the above problems is as follows: Manufactured by stretch blow molding, A neck portion having an entrance and exit portion for contents; A side portion connected to the neck portion; a bottom portion disposed opposite the neck portion and connected to the side portion; Equipped with The bottom portion is formed with a protruding portion that protrudes vertically downward, The protruding portion is located in an eccentric region of the bottom that is deviated from a region vertically projected from an opening plane of the entrance / exit portion of the neck portion.

[0007] According to the above configuration, the resin container has a protruding portion that protrudes vertically downward. In this manner, the resin container is largely eccentric to the extent that the protruding portion is formed on the bottom and is located in an eccentric region that is outside the region of the bottom that is vertically projected from the opening surface of the inlet / outlet part of the neck.

[0008] Further, a resin container according to one embodiment of the present disclosure includes: Manufactured by stretch blow molding, A neck portion having an entrance and exit portion for contents; A side portion connected to the neck portion; a bottom portion disposed opposite the neck portion and connected to the side portion; Equipped with A cut-away remnant is formed on the bottom portion by cutting away a protruding portion that protrudes vertically downward, The cut-out remnant is located in an eccentric region of the bottom that is deviated from a region vertically projected from the opening plane of the entrance / exit portion of the neck.

[0009] The resin container according to the above configuration is largely eccentric to such an extent that the cut-out remnant is located in the eccentric region.

[0010] Further, an apparatus for manufacturing a resin container according to an embodiment of the present disclosure includes: a clamping mechanism that is provided independently of a bottom mold of the blow molding die and that is capable of gripping a protrusion that is provided independently of a gate portion on the bottom of a preform accommodated in the blow molding die when the split molds of the blow molding die are open; a moving mechanism that moves the clamping mechanism so that the protrusion is located outside a region of the bottom that is vertically projected from an opening surface of the inlet / outlet portion of the neck while the neck of the preform is held; a stretching mechanism that closes the split mold and stretches the preform using a pressurizing medium; has.

[0011] According to the above-mentioned configuration, after the clamping mechanism grasps the protrusion on the bottom of the preform, the preform is bent so that the protrusion moves to the outside of the area of ​​the bottom that is vertically projected from the opening surface of the inlet / outlet part of the neck. The bent preform is stretch-blowed to produce a resin container with a large degree of eccentricity.

[0012] A method for producing a resin container according to one embodiment of the present disclosure includes the steps of: a clamping step of gripping a protrusion provided independently of a gate portion at a bottom of a preform accommodated in the blow molding die with a clamping mechanism provided independently on a bottom die of the blow molding die while a split die of the blow molding die is open; a bending step of bending the preform by moving the protrusion to the outside of a region of the bottom that is vertically projected from an opening surface of the inlet / outlet portion of the neck while the neck of the preform is held; a blowing step in which the split mold is closed and the preform is stretched by a pressurizing medium; has.

[0013] According to the manufacturing method having the above-mentioned configuration, after the clamping mechanism grasps the protrusion on the bottom of the preform, the preform is bent so that the protrusion moves to the outside of the area of ​​the bottom that is vertically projected from the opening surface of the inlet / outlet part of the neck. The bent preform is stretch-blown to manufacture a resin container with a large degree of eccentricity.

[0014] Moreover, a mold according to one embodiment of the present disclosure includes: A blow molding die including a bottom mold, a holding mechanism, a clamping mechanism, and a moving mechanism, The holding mechanism is configured to be able to hold a neck portion of a preform, the clamping mechanism is provided independently on the bottom mold and is configured to be able to grip a protrusion provided independently of a gate portion on the bottom of the preform, The moving mechanism is configured to move the clamping mechanism and the bottom mold so that, while the neck of the preform is held, the protrusion is positioned outside the area of ​​the bottom projected vertically from the opening surface of the entrance / exit portion of the neck.

[0015] According to the above configuration, after the clamping mechanism grasps the protrusion on the bottom of the preform, the preform is bent so that the protrusion moves to the outside of a projected area of ​​the bottom that extends perpendicularly from the opening surface of the inlet / outlet part of the neck. The bent preform is stretch-blown to produce a resin container with a large degree of eccentricity. Effect of the Invention

[0016] According to the present disclosure, it is possible to provide a resin container with a large degree of eccentricity that can be manufactured using a stretch blow molding method, a method for manufacturing a resin container, an apparatus for manufacturing a resin container, and a mold. [Brief description of the drawings]

[0017] [Figure 1A] FIG. 1A is a front view of a resin container with a large degree of eccentricity. [Figure 1B] FIG. 1B is a right side view of a resin container with a large degree of eccentricity. [Figure 1C] FIG. 1C is a bottom view of a resin container with a large degree of eccentricity. [Diagram 2] FIG. 2 is a functional block diagram of the blow molding device. [Figure 3A] FIG. 3A is a diagram illustrating an example of the appearance of the preform, and is a front view of the preform. [Figure 3B] FIG. 3B is a right side view illustrating the external appearance of the preform. [Figure 3C] FIG. 3C is a diagram illustrating an example of the appearance of the preform, and is a partially enlarged front view of the preform. [Figure 3D] FIG. 3D is a diagram illustrating an example of the appearance of the preform, and is a partially enlarged right side view of the preform. [Figure 4A] FIG. 4A is a front view of a blow molding die. [Figure 4B] FIG. 4B is a right side view of the blow mold. [Diagram 5] FIG. 5 is a diagram illustrating the clamping mechanism. [Figure 6A] FIG. 6A is a diagram illustrating the blow molding process, in which the split molds are closed and a preform is accommodated in the mold. FIG. [Figure 6B] FIG. 6B is a diagram illustrating the blow molding process, showing a state in which the protruding portion of the preform is gripped by a clamping mechanism. [Figure 6C] FIG. 6C is a diagram illustrating the blow molding process, showing a state in which the preform is bent. [Figure 7] FIG. 7 is a diagram showing an example of a conventional blow molding apparatus. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. Note that, for the sake of convenience of explanation, the dimensions of each component shown in the drawings may differ from the actual dimensions of each component.

[0019] In addition, in the description of this embodiment, for convenience of explanation, the "left-right direction", the "front-rear direction", and the "up-down direction" are appropriately mentioned. These directions are directions commonly set in each figure. These directions are directions displayed for convenience of explanation, and are not intended to be limited to the directions shown in the figures. Here, the "up-down direction" is a direction including the "upward direction" and the "downward direction". The "front-rear direction" is a direction including the "forward direction" and the "rearward direction". The "left-right direction" is a direction including the "leftward direction" and the "rightward direction". For example, each direction in FIG. 1A is a direction when the container 10 is observed from the front of the container 10 in an upright state. However, the definition of the direction is not limited to this. In addition, the front-rear direction in FIG. 2 corresponds to the longitudinal direction of the blow molding apparatus 100.

[0020] First, referring to Figs. 1A to 1C, a resin container 10 having a large degree of eccentricity according to this embodiment (hereinafter, simply referred to as "container 10") will be described. Fig. 1A is a front view of the resin container 10 having a large degree of eccentricity. Fig. 1B is a right side view of the resin container 10. Fig. 1C is a bottom view of the resin container 10. As illustrated in Fig. 1A, the container 10 is a resin container comprising a neck portion 12 having an inlet / outlet portion 11 located at the uppermost end, a body portion (side portion) 13 formed so as to be continuous with the neck portion 12 and defining the side wall portion of the container 10, and a bottom portion 14 located at the lowermost end and formed so as to be continuous with the body portion 13. The inlet / outlet portion 11 comprises an opening surface (top surface). The bottom portion 14 is disposed at a position opposite to the neck portion 12 in the vertical direction. The bottom portion 14 comprises a protruding portion 25 described later. The protruding portion 25 comprises a gate portion 26 and a protrusion portion 27. The synthetic resin material is a thermoplastic resin and can be appropriately selected depending on the application. Examples of synthetic resins include PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), PLA (polylactic acid), etc.

[0021] Here, in this embodiment, the area of ​​the bottom 14 formed when projected vertically from the opening surface of the inlet / outlet section 11 is defined as the projection area S1. The projection area S1 is an area of ​​the bottom 14 divided by two parallel lines extending downward from the lower end of the inner peripheral surface of the inlet / outlet section 11 in a vertical cross section. The protruding portion 25 is located in an area S2 outside the projection area S1. This area S2 is referred to as an "eccentric area S2" in this specification. As illustrated in FIG. 1C, the eccentric area S2 is located approximately in the center and on the left side of the bottom 14 of the container 10 (outside the projection area S1 and to the left of the projection area S1). In the container 10 according to this embodiment, the protruding portion 25 is provided in the center of the bottom 14. The center is a portion that spreads within a range of a predetermined distance (approximately several tens of millimeters) from the center point of the bottom 14, and is located approximately in the center of the area of ​​the bottom 14 that is recessed upward.

[0022] As illustrated in FIG. 1A, the center of the opening surface (diameter of the entrance / exit portion 11) of the inlet / outlet portion 11 of the neck portion 12 is defined as a first point CR1, and the intersection point of a vertical line passing through the center of the overhanging portion 25 and the ground surface of the bottom portion 14 (a horizontal line defining the outer diameter of the lowest end of the bottom portion 14) is defined as a second point CR2. In addition, a straight line passing through the first point CR1 and extending vertically perpendicular to the opening surface of the inlet / outlet portion 11 (or the ground surface of the bottom portion 14) is defined as an axis A (first straight line), and a straight line connecting the first point CR1 and the second point CR2 with a line and extending at an angle is defined as an axis B (second straight line). The angle formed by the axis A and the axis B is defined as an eccentricity angle X. The eccentricity angle X can quantitatively indicate the eccentricity of the container 10. The eccentricity angle X of the container 10 according to this embodiment is large, 7° or more, and preferably 10° or more. The eccentric angle X is not limited to 7° or more, and may be greater than this depending on the size of the entrance / exit portion 11.

[0023] When the body 13 is divided into two equal parts in the vertical direction, the upper part has a substantially trapezoidal shape in a front view. When the body 13 is divided into two equal parts in the vertical direction, the lower part has a substantially rectangular shape in a front view. The upper part of the body 13 connected to the end 121 on the major axis of the neck 12 is curved so that the distance between the axis A and the body 13 gradually increases downward. The lower part of the body 13 connected to the end 121 on the major axis of the neck 12 extends parallel to the axis A. As illustrated in FIG. 1A, the body 13 connected to the end 122 on the minor axis of the neck 12 extends parallel to the axis A. As illustrated in FIG. 1A and FIG. 1B, the top surface of the entrance / exit portion 11 and the bottom surface of the bottom portion 14 are parallel to each other.

[0024] Next, a blow molding apparatus 100 for manufacturing a container will be described with reference to Fig. 2. Fig. 2 is a block diagram of the blow molding apparatus 100.

[0025] 2, the blow molding apparatus 100 includes an injection molding section 110 for manufacturing the preform 20, and a temperature adjustment section 120 for adjusting the temperature of the manufactured preform 20. An injection device 112 for supplying a resin material as a raw material is connected to the injection molding section 110. The blow molding apparatus 100 also includes a blow molding section 130 for blowing the preform 20 to manufacture the container 10, and an ejection section 140 for ejecting the manufactured container 10.

[0026] The injection molding section 110, the temperature adjustment section 120, the blow molding section 130, and the removal section 140 are provided at positions rotated by a predetermined angle (90 degrees in this embodiment) around the conveying means 150. The conveying means 150 is composed of a rotating plate and the like, and is configured so that the preforms 20 or the containers 10 with the necks 12, 22 supported by the neck molds 152 attached to the rotating plate are conveyed to each section as the rotating plate rotates, as exemplified in Figs. 4A to 4B and 6A to 6C described later.

[0027] 2 includes an injection cavity mold, an injection core mold, a neck mold, etc. (not shown). These molds are clamped together to form a preform-shaped space, into which a resin material is poured from an injection device 112 to manufacture a bottomed preform 20.

[0028] Here, the preform 20 according to this embodiment will be described with reference to Figs. 3A to 3D. Fig. 3A is a front view of the preform 20, Fig. 3B is a right side view of the preform 20, Fig. 3C is a partially enlarged view of the front view of the preform 20, and Fig. 3D is a partially enlarged view of the right side view of the preform 20. The preform 20 is composed of a neck portion 22 having an opening 21, a body portion 23 formed to be continuous with the neck portion 22 and defining the side wall portion of the preform 20, and a bottom portion 24 formed to be continuous with the body portion 23. A protruding portion 25 is provided at the center portion of the bottom portion 24. The protruding portion 25 is composed of a gate portion 26 close to the injection gate of the resin during preform molding, and a protrusion portion 27 formed vertically above the gate portion 26 and continuous with the lower end of the preform 20. The protrusion 27 is formed in a flat shape, and is formed to have a larger diameter (wider) than the gate portion 26 in a front view (FIGS. 3A and 3C), and is formed to have the same width as the gate portion 26 in a side view (FIGS. 3B and 3D). That is, the length of the protrusion 27 in the left-right direction (the width direction in which the protrusion 27 appears wider than the gate portion 26 when the preform 20 is supported by the neck mold 152) is longer than the length of the gate portion 26 in the left-right direction. The length of the protrusion 27 in the front-rear direction (the direction in which the width of the protrusion 27 and the width of the gate portion 26 appear to be the same when the preform 20 is supported by the neck mold 152) is the same as the length of the gate portion 26 in the front-rear direction.

[0029] Returning to FIG. 2, the blow molding apparatus 100 will be described. The temperature adjustment section 120 is configured to adjust the temperature of the preform 20 manufactured in the injection molding section 110 to a temperature suitable for final blowing. The blow molding section 130 is configured to perform blow molding on the preform 20 whose temperature has been adjusted in the temperature adjustment section 120, to manufacture a resin container 10. The blow molding section 130 includes a blow molding die 200 (see FIG. 4A) and a stretching mechanism (not shown). The stretching mechanism includes a stretching rod 132 (see FIG. 4A) and a blow nozzle (not shown).

[0030] 4A and 4B, the blow molding die 200 provided in the blow molding section 130 will be described in detail. Fig. 4A shows a front view of the die 200, and Fig. 4B shows a right side view of the die 200. The die 200 includes a pair of split dies (blow cavity split dies) 210, a bottom die 220, a pair of neck dies 152, a clamping mechanism 230, and a moving mechanism 240.

[0031] The split mold 210 is configured to be openable and closable in the front-rear direction (opening and closing direction D) with the parting surface C as a reference in a side view (FIG. 4B). As illustrated in FIG. 4A, the pair of split molds 210 form a space S that defines the body 13 of the container 10 in a closed state.

[0032] The bottom mold 220 is composed of a first bottom mold member 221 that defines the bottom 14 of the container 10, and a second bottom mold member (accommodating block) 260 that is disposed below the first bottom mold member 221. The bottom mold 220 is also provided with a clamping mechanism 230 that is accommodated therein (FIGS. 4A and 4B). The first bottom mold member 221 accommodates at least a part of a clamping section 232 (described later) of the clamping mechanism 230, and the second bottom mold member 260 accommodates at least a part of an opening / closing mechanism 234 (described later) of the clamping mechanism 230. The second bottom mold member 260 is provided on the upper surface of a guided portion 244 that will be described later. The bottom mold 220 and the guided portion 244 are configured to be movable together in the left-right direction (the direction in which the second bottom mold member 260 advances or retreats).

[0033] Here, the clamping mechanism 230 will be described with reference to FIG. 5. The clamping mechanism 230 includes a clamping section 232 configured to be able to grip the protrusion 27 of the overhanging section 25 provided on the bottom 24 of the preform 20. The clamping section 232 is provided independently of the bottom mold 220 (separately and not directly provided on the bottom mold 220). The clamping section 232 is configured to be openable and closable by an opening / closing mechanism 234 made of a link mechanism below the bottom mold 220, and clamps the protrusion 27 by going from an open state to a closed state. A claw section 233 protruding inward from the clamping section 232 is provided at the tip of the clamping section 232, and is configured so that the claw section 233 bites into the protrusion 27 when the clamping section 232 is closed.

[0034] The first bottom mold member 221 includes a first storage section 236A. The second bottom mold member 260 includes a second storage section 236B. Here, the portion consisting of the first storage section 236A and the second storage section 236B is defined as a storage section 236 in this specification. The first storage section 236A and the second storage section 236B are connected to each other. The storage block 260 and the bottom mold 220 are each provided with an opening for guiding the protruding section 25 of the preform 20 to the clamping section 232. The clamping section 232 and the opening / closing mechanism 234 are covered by the storage section 236. The clamping mechanism 230 is arranged in the storage section 236.

[0035] Returning to Figures 4A and 4B, the mold 200 will be described. The neck mold 152 is attached to the rotating plate as described above, and is configured to transport the preform 20 or the container 10 to each part as the rotating plate rotates while supporting the neck parts 12, 22. The moving mechanism 240 includes, for example, a flat guide groove 242 disposed below the bottom mold 220, and a guided part 244 connected to a moving block (not shown) fixed directly below the storage part 236 (Figure 4A). The guide groove 242 is configured to draw a straight line extending parallel to the top surface of the entrance / exit part 11 of the preform 20.

[0036] The moving mechanism 240 can move the guided portion 244 along the guide groove 242, thereby moving the bottom mold 220 via the moving block parallel to the top surface of the entrance / exit portion 11 of the stationary preform 20 held by the neck mold 152.

[0037] 2, a description will be given of the removal section 140 of the blow molding apparatus 100. The removal section 140 is configured to release the neck portion 12 of the container 10 manufactured in the blow molding section 130 from the neck mold 152, and remove the container 10.

[0038] 6A to 6C, a method for blow molding the container 10 in the blow molding section 130 of the blow molding apparatus 100 will be described. Fig. 6A is a diagram illustrating a state in which the split mold 210 is open and the preform 20 is accommodated (transported) in the metal mold 200, Fig. 6B is a diagram illustrating a state in which the protrusion 27 of the preform 20 is gripped by the clamping mechanism 230, and Fig. 6C is a diagram illustrating a state in which the preform 20 is bent. The blow molding process of this embodiment includes a clamping process in which, with the split mold 210 of the mold 200 open, the protrusion 27 of the preform 20 contained in the mold 200 is grasped by the clamping mechanism 230 of the mold 200, a bending process in which, with the neck portion 22 of the preform 20 held by the neck mold 152, the protrusion 27 of the preform 20 is moved to a position that becomes the eccentric region S2 to bend the preform 20, and a blowing process in which the split mold 210 is closed and the preform 20 is stretched by a pressurized medium.

[0039] First, the preform 20 supported by the neck mold 152 and adjusted to a temperature suitable for blow molding by the temperature adjustment unit 120 is transported by the transport means 150 to the blow molding unit 130 and accommodated in the mold 200 with the split mold 210 open (FIG. 6A). Next, the stretch rod 132 at the standby position provided in the blow molding unit 130 is lowered to press the bottom 24 of the preform 20 from the inside, stretching the preform 20 toward the bottom mold 220 (pre-stretching step). The preform 20 is stretched to the bottom mold 220, and the protruding part 25 of the bottom 24 is accommodated in the bottom mold 220 and the opening of the accommodation unit 236 (FIG. 6B). The protrusion 27 of the accommodated protruding part 25 is gripped by the clamping mechanism 230, and the bottom mold 220 of the mold 200 and the bottom 24 of the preform 20 are connected (clamping step). After that, the stretch rod 132 is raised to the standby position.

[0040] Next, the guided portion 244 is moved leftward (the direction in which the storage block 260 advances) along the guide groove 242 (FIG. 4A) by the moving mechanism 240 (FIG. 4A). As a result, the bottom mold 220 gripping the protrusion 27 can be moved leftward so as to be parallel to the top surface of the entrance / exit portion 11 of the stationary preform 20 held by the neck mold 152 (FIG. 6C). Therefore, the protrusion 27 moves to the eccentric region S2, which is outside the projection region S1. As a result, the preform 20 is stretched from directly below the neck portion 22 as a starting point so that the protrusion 27 is eccentric with respect to the axis A, and is simultaneously bent (bending process). At this time, the amount of stretching of the body portion of the preform 20 on the left side of the axis A is less than the amount of stretching of the body portion on the right side of the axis A (the body wall of the preform in the opposite direction to the movement direction of the bottom mold 220 or the storage portion 236 is stretched more than the body wall on the same side as the movement direction). Then, the split mold 210 is closed, and the bent preform 20 is accommodated in the space S that defines the outer shape of the container 10 and is formed by the neck mold 152, the split mold 210, and the bottom mold 220. In this state, a pressurized medium such as air is introduced into the preform 20, and the preform 20 is blown and stretched to form the container 10 (blow process). After molding is completed, the split mold 210 is opened to release the container 10, and the container 10 is transported to the removal section 140 by the transport means 150. By the above method, a container 10 with a large degree of eccentricity can be blow-molded from the preform 20.

[0041] Incidentally, there are eccentric containers (off-center bottles) whose necks are not coaxial with each other as containers manufactured by the blow molding method. FIG. 7 is a diagram showing an example of a conventional blow molding apparatus 400. As shown in FIG. 7, the stretch rod 133 is slightly inclined with respect to the axis A1 of the preform 20a and the neck mold 252. Here, the area where the bottom 214 of the inner wall surface 202 of the split mold 211 is divided by two parallel lines extending downward from the lower end of the inner peripheral surface of the inlet / outlet portion 11a of the preform 20a as the base end is defined as an area S3. Thus, in the conventional blow molding apparatus 400, the lower end 133a of the stretch rod 133 is located inside the area S3. The inner wall surface 202 of the split mold 211 that defines the shape of the eccentric container is defined by the split mold 211. When air is blown into the inside of the preform 20a through the blow holes, the preform 20a is molded into a shape corresponding to the inner wall surface 202 of the split mold 211 that defines the shape of the eccentric container.

[0042] Examples of conventional eccentric containers include containers in which the gate is located at the center of the bottom and not directly below the neck (entrance / exit portion) (see Patent Documents 2 and 3), and containers in which the gate is not located at the center of the bottom and is directly below the neck (see Patent Document 4).

[0043] A container in which the gate is at the center of the bottom and not directly below the neck (entrance / exit portion 11a) is manufactured by placing the preform 20a in a blow mold, then lowering the inclined stretch rod 133 obliquely while abutting against the inner wall surface of the bottom of the preform 20a, and inflating it with blow air. For this reason, the preform 20a for such a container is, for example, one in which the thickness distribution of the body of the preform 20a is symmetrical or slightly asymmetrical (i.e., one in which the body of the preform is slightly uneven in thickness). In addition, the preform 20a is usually designed to have an optimal thickness distribution and external shape for each container, taking into consideration the amount of stretching and rigidity of each part corresponding to the container.

[0044] When manufacturing the containers disclosed in Patent Document 2 and Patent Document 3, as shown in FIG. 7, the gate portion of the preform 20a is moved to a designed position on the bottom side of the inner wall surface 202 while the preform is biaxially stretched (blowing and expanding). In Patent Document 3, the stretch rod 133 is slightly tilted (rotated) during the preliminary stretching step to forcibly bend the preform 20a to temporarily form a curved preform, and then the preform is lowered in an oblique direction to perform biaxial stretching, thereby preventing misalignment of the gate portion. In addition, if necessary, the gate portion of the preform is sandwiched between the top surface of the bottom mold and the tip of the stretch rod and crushed. This is because if the stop position of the gate portion relative to the inner wall surface 202 is shifted, misalignment occurs and the preform cannot be stretched as designed. When the core misalignment occurs, undesirable phenomena occur, such as the gate being positioned at an irregular position on the bottom, each part of the preform being stretched in a direction different from that expected, and the preform contacting the blow cavity surface at an unexpected location. As a result, containers with inferior physical properties such as rigidity and containers with inferior aesthetic appearance may be manufactured. Therefore, in order to manufacture such containers with high quality by the stretch blow molding method, it was necessary to position the stretch rod inside the preform during the inclined stretching.

[0045] In a rotary plate type blow molding machine, the stretch rod is housed (placed) in an inclined state so as to be movable up and down inside a blow core mold that moves up and down by circulating air. The tip of the blow core mold is small so as to fit airtightly into the neck of the preform. The diameter of the cylindrical part above the tip of the blow core mold cannot be made large when molding multiple containers at the same time. In addition, the diameter of the cylindrical part above the tip of the blow core mold cannot be made large, taking into account the size of the tapered surface that engages with the neck mold, etc.

[0046] Furthermore, the blow core mold must have sufficient rigidity to withstand the clamping force, so the outer wall cannot be made too thin. The stretch rod also cannot be made too thin, because it must have the strength to withstand the reaction force from the preform during blow molding. Due to the structural reasons of the stretching mechanism, the inclination angle of the stretch rod is limited within the hollow space of the blow core mold with a small inner diameter. As a result, it has been difficult to manufacture containers with a large eccentric angle by the stretch blow method.

[0047] An example of the eccentricity angle is about 5° for a container with an inlet / outlet inner diameter of about 36 mm and an outer diameter of about 40 mm, and about 7° for a container with an inlet / outlet inner diameter of about 46 mm and an outer diameter of about 50 mm. For this reason, the stretch blow molding methods disclosed in Patent Documents 2 and 3 could only manufacture containers with a small eccentricity (eccentric angle X).

[0048] In addition, the manufacturing method disclosed in Patent Document 4 involves straightening a preform with large thickness deviation with a stretching rod, and then blowing air to greatly expand the body side of the thick preform. However, if the thickness deviation ratio (degree of thickness deviation) of the preform is increased, the difference in the flow rate of the resin during injection molding increases, and there is a possibility that a defective appearance such as a weld (a mark where the molten resin adheres) may occur in the body. Therefore, in practice, it is difficult to increase the thickness deviation ratio. In addition, in the manufacturing method disclosed in Patent Document 4, it is also very difficult to adjust the temperature of a preform with large thickness deviation before blow molding to a temperature suitable for blowing. Therefore, when using this method to manufacture a container, especially a container with a large stretch ratio, it is very difficult to stretch the preform as designed. Therefore, even if this method is used, the eccentricity (eccentric angle X) of the manufactured container cannot be made very large.

[0049] Eccentric containers are used, for example, in engine oil containers and trigger-type spray containers. Containers with a relatively small eccentricity angle can also be manufactured by stretch blow molding using the inclined stretching mechanisms of Patent Documents 1 to 3 and the preform with a different wall thickness in the circumferential direction of Patent Document 4. However, even if these means are used, the eccentricity (eccentric angle X) is limited to about 7° in order to prevent quality defects such as misalignment from occurring in the eccentric containers manufactured by the molding method. In this case, the protruding portion is located within a region (projected region) defined by the intersection of the projection line (extension line) of the outer diameter of the neck and the bottom. In other words, the protruding portion exists within the projection region from the inner diameter of the neck to the bottom. Therefore, conventionally, containers with a large eccentricity have been manufactured by direct blow molding.

[0050] However, containers manufactured by the direct blow molding method generally have inferior aesthetic appearances compared to those manufactured by the stretch blow molding method. In addition, there is a concern that containers manufactured by the direct blow molding method may have poor welding (pinholes) at the pinch-off part of the bottom. Containers manufactured by the direct blow molding method do not have high dimensional accuracy of the neck part for shaping the neck part by air blowing. In other words, containers manufactured by the direct blow molding method are not as airtight as containers manufactured by the stretch blow molding method. In addition, containers manufactured by the direct blow molding method require the removal of burrs, resulting in a large amount of wasted resin (loss material). Furthermore, for containers manufactured by the direct blow molding method, a post-process called trimming is required after blow molding. It is difficult to manufacture containers with high surface gloss using the direct blow molding method. Therefore, there is an increasing demand to manufacture containers with a large eccentricity (eccentricity angle X) using the stretch blow molding method.

[0051] In order to solve and improve the above-mentioned problems, the present disclosure does not require a stretching rod that was essential during inclined stretching, and instead employs a method of holding (clamping) and pulling the preform 20 from the outside of the bottom 24 during inclined stretching. This allows the gate portion 26 of the preform 20 to be reliably moved and stopped at a position as designed, even when a container with a large eccentricity angle is manufactured. As a result, each part of the body portion of the preform 20 can be stretched as designed. In other words, by using the manufacturing method and manufacturing device according to the present disclosure, a container 10 can be manufactured in which the eccentricity angle X is large enough that the gate portion 26 is out of the projection area S1, and which also has good physical properties (quality).

[0052] Moreover, the container 10 according to the above embodiment is provided with a protruding portion 25 that protrudes vertically downward on the bottom 14. The container 10 is also largely eccentric to such an extent that the protruding portion 25 is located in an eccentric region S2 that is outside the projection region S1. Therefore, the container 10 has an excellent aesthetic appearance and a large degree of eccentricity.

[0053] Furthermore, in container 10 according to the above embodiment, protrusion 27 is wider than gate 26, so that clamping mechanism 230 can easily clamp protruding portion 25, improving ease of manufacture of the eccentric container.

[0054] Furthermore, according to the manufacturing apparatus, manufacturing method, and blow molding die 200 of the above-described embodiment, a container 10 is manufactured in which the top surface of the inlet / outlet portion 11 of the neck portion 12 is parallel to the bottom surface of the bottom portion 14. Therefore, when the container 10 is placed on a table or the like, liquid in the container 10 is less likely to spill, compared to a container in which the top surface of the inlet / outlet portion 11 is inclined relative to the bottom surface.

[0055] Furthermore, the container 10 according to the above embodiment is provided with an overhanging portion 25 that can be clamped by a clamping mechanism 230 of a mold 200 provided in a blow molding section 130 of a blow molding apparatus 100 that uses a stretch blow molding method. This makes it easier to clamp the overhanging portion 25 by the clamping mechanism 230, improving the ease of manufacturing an eccentric container.

[0056] Furthermore, according to the manufacturing apparatus, manufacturing method, and blow molding die 200 of the above-described embodiment, after the clamping mechanism 230 grips the protrusion 27 on the bottom 14 of the preform 20, the preform 20 is bent so that the protrusion 27 moves to the eccentricity region S2. The bent preform 20 is stretch-blowed to manufacture a container 10 with a large degree of eccentricity.

[0057] Furthermore, according to the manufacturing method of the above embodiment, a container 10 with a large degree of eccentricity and excellent aesthetic appearance can be manufactured using a stretch blow molding method without having to consider the issues associated with the above direct blow molding.

[0058] The present disclosure is not limited to the above-described embodiment, and can be freely modified, improved, etc. as appropriate. In addition, the material, shape, size, numerical value, form, number, arrangement location, etc. of each component in the above-described embodiment are arbitrary and not limited as long as the object of the present disclosure can be achieved.

[0059] In the above embodiment, the container 10 has an eccentric angle X of 7° or more, but according to the mold 200 and blow molding method of this embodiment, it is possible to manufacture a container having an eccentric angle X of 10° or more by stretch blow molding. Furthermore, the operation of the moving mechanism 240 is not limited to horizontal movement, and may be an operation consisting of rotation or linear / multi-stage diagonal upward movement.

[0060] In the above embodiment, air has been given as an example of a pressurizing medium for blowing the preform 20, but a gas medium other than air may be used, and pressure may also be applied using a liquid medium such as water.

[0061] In the above embodiment, the container 10 is described as having the protruding portion 25, but is not limited to this example. For example, the container may have a remnant formed by cutting out the protruding portion 25 instead of the protruding portion 25. The remnant is located in the eccentric region S2.

[0062] In the above embodiment, the blow molding apparatus 100 is a so-called four-station type apparatus in which the temperature adjustment unit 120 is provided between the injection molding unit 110 and the blow molding unit 130, but is not limited to this. The blow molding apparatus 100 may be, for example, a so-called two-station type or three-station type apparatus in which the temperature adjustment unit 120 is not provided.

[0063] This application is based on a Japanese patent application (Patent Application No. 2018-238111) filed on December 20, 2018, the contents of which are incorporated herein by reference.

Claims

1. A neck portion having an entrance and exit portion for contents; A side portion connected to the neck portion; a bottom portion disposed opposite the neck portion and connected to the side portion; Equipped with A protruding portion that protrudes vertically downward is formed on the bottom portion, A resin container manufactured by stretch blow molding, wherein the protruding portion is located in an eccentric area of ​​the bottom that is outside the area projected vertically from the opening surface of the inlet / outlet portion of the neck.

2. The protruding portion is The gate section, a protrusion provided above the gate portion and independent of the gate portion; Including, The protrusion is wider than the gate. The resin container according to claim 1.

3. The top surface of the inlet / outlet portion of the neck portion and the bottom surface of the bottom portion are parallel to each other. The resin container according to claim 1.

4. A neck portion having an entrance and exit portion for contents; A side portion connected to the neck portion; a bottom portion disposed opposite the neck portion and connected to the side portion; Equipped with A cut-away remnant is formed on the bottom portion by cutting away a protruding portion that protrudes vertically downward, A resin container manufactured by stretch blow molding, wherein the cut-out remaining portion is located in an eccentric area of ​​the bottom that is outside the area projected vertically from the opening surface of the inlet / outlet portion of the neck.

5. The protruding portion is formed into a shape that can be clamped by a clamping mechanism provided in the manufacturing apparatus. The resin container according to claim 1.

6. a first straight line that passes through a center of the opening surface and is perpendicular to the ground surface of the bottom portion; A second straight line connecting the intersection point of a vertical line that passes through the center of the overhanging portion and intersects with the ground surface of the bottom portion and the center of the opening surface; The angle between them is 7° or more. The resin container according to claim 1.

7. a clamping mechanism that is provided independently of a bottom mold of the blow molding die and that is capable of gripping a protrusion that is provided independently of a gate portion on the bottom of a preform accommodated in the blow molding die when the split molds of the blow molding die are open; a moving mechanism that moves the clamping mechanism so that the protrusion is located outside a region of the bottom that is vertically projected from an opening surface of the inlet / outlet portion of the neck while the neck of the preform is held; a stretching mechanism that closes the split mold and stretches the preform using a pressurizing medium; The resin container manufacturing apparatus has the following features.

8. The moving mechanism moves the clamping mechanism together with the bottom mold parallel to the top surface of the entrance / exit portion. The manufacturing apparatus according to claim 7.

9. a clamping step of gripping a protrusion provided independently of a gate portion at a bottom of a preform accommodated in the blow molding die with a clamping mechanism provided independently on a bottom die of the blow molding die while a split die of the blow molding die is open; a bending step of bending the preform by moving the protrusion to the outside of a region of the bottom that is vertically projected from an opening surface of the inlet / outlet portion of the neck while the neck of the preform is held; a blowing step in which the split mold is closed and the preform is stretched by a pressurizing medium; The method for producing a resin container comprising the steps of:

10. The manufacturing method according to claim 9 , wherein in the bending step, the clamping mechanism moves together with the bottom mold in a direction parallel to a top surface of the entrance / exit portion.

11. The method further includes a preliminary stretching step of stretching the bottom of the preform toward the bottom mold by a stretching rod before the clamping step. The method for producing a resin container according to claim 9.

12. A blow molding die including a bottom mold, a holding mechanism, a clamping mechanism, and a moving mechanism, The holding mechanism is configured to be able to hold a neck portion of a preform, the clamping mechanism is provided independently on the bottom mold and is configured to be able to grip a protrusion provided independently of a gate portion on the bottom of the preform, The moving mechanism is configured to move the clamping mechanism and the bottom mold so that, in a state in which the neck portion of the preform is held, the protrusion portion is positioned outside an area of ​​the bottom portion projected vertically from an opening surface of the inlet / outlet portion of the neck portion. Mold.

13. The moving mechanism moves the clamping mechanism together with the bottom mold parallel to the top surface of the entrance / exit portion. The mold according to claim 12.

Citation Information

Patent Citations

  • Biaxially oriented blow molded bottle, its manufacture and composite container using the same

    JP1990070420A

  • Plastic bottle which is hard to crush and manufacture thereof

    JP1993305934A

  • Polycarbonate container, as well as method and device for molding the container

    JP1996164557A

  • Method and apparatus for molding bent container

    JP1996207128A

  • PET bottle with eccentric neck and manufacturing method thereof

    JP2003523289A

Cited By

  • Communication device, communication method, and recording medium