Method and apparatus for digital manufacturing of object using actuated micro-pixelation and dynamic density control
By employing particulate materials and advanced image generation techniques, the SFF process achieves high-precision, high-density parts with improved surface finish and speed, addressing the limitations of traditional SFF methods.
Patent Information
- Application Number
- JP2024124493
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-03-12
- Filing Date
- 2024-07-31
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-03-06
AI Technical Summary
Existing solid free-form manufacturing (SFF) techniques face limitations in producing high-precision parts with poor surface finish, inaccurate layer formation, and slow processing times, particularly in methods like powder injection molding (PIM) and stereolithography (SLA), which hinder their application in high-precision manufacturing.
The use of particulate materials, photocurable resin, and dynamic density control through methods such as diffusion, electrostatic deposition, and in-situ material mixing, combined with advanced image generation systems like refractive pixel shift and micropixelation, to enhance layer deposition and bonding, allowing for improved resolution and speed in SFF processes.
This approach enables the production of high-density, high-precision parts with improved surface finish and increased production speed, overcoming the limitations of traditional SFF methods by enhancing material bonding and layer accuracy.
Smart Images

Figure 2024167199000001_ABST
Abstract
Description
CROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims priority from U.S. Provisional Patent Application No. 62 / 817,431, filed March 12, 2019. No. 6,399,433, the disclosure of which is incorporated herein by reference in its entirety. [Technical field]
[0002] The subject matter disclosed herein generally relates to solid freeform fabrication of objects. More specifically, In particular, the subject matter disclosed herein is directed to a combination of one or more types of materials, such as metals, plates, A system for solid freeform fabrication of objects from plastics, ceramics, and composites. The present invention relates to systems, devices, and methods. [Background technology]
[0003] The embodiments described herein generally include metals, plastics, ceramics, and Solid freeform fabrication of objects from composite materials, including combinations of one or more types of materials The present invention relates to a device and method for
[0004] Solid Freeform Manufacturing (SFF), 3D Printing (3DP), Direct Digital Manufacturing (DDM), and Solid Additive Manufacturing (AM), also known as shape imaging, creates both visually demonstrative and functional parts. In some cases, this has become a widely adopted method to reduce the cost of production. It is also an effective way to produce a wide variety of ingredients based on digital models. There are tools available that reduce the time and cost required for a complete design cycle. This has accelerated the pace of innovation in many industries.
[0005] Typically, SFF is accomplished using a layered surface approach, where the digital model is sliced horizontally into The slices are then divided into slices, each of which is generated as a 2D image on the build surface. Secondary manufacturing involves the aggregation of thin layers that collectively make up the three-dimensional object represented by the digital model. Generate aggregates. CNC (Computer Numerically Controlled) machining, injection molding, etc. In contrast to traditional manufacturing techniques such as ,It has been widely adopted for research and development purposes where small-scale production by traditional means becomes prohibitively expensive. In addition, SFF equipment generally requires less expertise to operate when compared to CNC machines. The cost of individual parts produced from CNC machines is generally high, which is why This is due to the longer manufacturing time and higher cost of machine operations. They often have stronger and more detailed features than SFF manufactured parts, which means some SFF techniques will be desirable for applications where parts have the resolution and functionality of CNC-produced parts. Until that happens, the use of SFF in part production will remain limited.
[0006] Powder injection molding (PIM) is a process that allows the production of high-precision parts from materials that were previously not possible with other molding methods. It is a mass production technique that has been widely adopted as a means of The raw material is formed and then injected into a mold in the same way as plastic injection molding. The manufactured parts are , a powder composite part called a "green" part, and the green part is called a debonder The process removes most of the binder and the resulting part is called a "brown" part. The brown area is then subjected to a heat treatment to sinter the powder particles together. The part shrinks and the voids between the powder particles are eliminated. The end result is a nearly fully dense part. Depending on the powder feedstock composition utilized, densities of over 99.5% can be achieved. Further post-processing may be employed to
[0007] Some of the most common techniques for SFF are stereolithography (SLA), selective deposition Modeling (SDM), Fused Deposition Modeling (FDM), and Selective Laser Sintering (SLS). These approaches vary in the types of materials they can use, the manner in which the layers are produced, and subsequently vary in resolution and quality of the produced parts. are fabricated by bulk material deposition or selective material deposition techniques. In techniques using this method, layer imaging is typically performed using thermal, chemical, or optical processes. One technology, binder jet, is an inkjet process. A hot-press print head is used to deposit the binder onto the powder bed to form a pre-formed powder in the PIM process. This green part is then used to produce the final part. Unfortunately, the process for manufacturing green components is Due to imperfections in the process, the final parts manufactured through this process may have poor finish, especially in terms of surface finish. When the temperature drops, they often do not meet the tolerances required for high precision applications. The accuracy and speed of the mixture injection process is limited. Summary of the Invention [Problem to be solved by the invention]
[0008] Manufacture components (e.g., plastic, metal, and ceramic parts) for a variety of applications Embodiments of a device and associated method for solid freeform fabrication for performing a method for producing a solid freeform pattern are disclosed herein. This will be disclosed in the details. [Means for solving the problem]
[0009] In some embodiments, the SFF methods and apparatus disclosed herein include The surface that will receive layers of material to produce a three-dimensional solid representation of the model and the required build material. and means for depositing a layer or layers of said build material based on data contained in a digital model. In one embodiment, the build material comprises a particle The build surface is made up of a photo-curable material and a photo-curable resin material. The rheological limitations of the above-mentioned devices used to manufacture powder composite parts are overcome. In one embodiment, the build material is a photocurable resin material that produces a polymeric component. In another embodiment, the materials are mixed prior to the build process and the density of the mixture is may be varied during the build process to optimize properties of the printed part.
[0010] Additionally, in some embodiments, the methods and apparatus described below comprise: One may utilize particulate materials (eg, ceramic, plastic, or metal). Parts produced from this device have been engineered to be made using a build process that promotes bonding between adjacent particles. The treatment may include heat treatment, chemical treatment, and pressure treatment, and the like. The results of this manufacturing and treatment process include, but are not limited to, a combination of Dense metal parts, dense ceramic parts, dense plastic parts, porous metal parts , porous ceramic parts, porous plastic parts, dense composite plastic parts, and Includes, but is not limited to, composite parts that contain more than one type of material.
[0011] Material deposition of particulate materials can be achieved by several means - spreading by blade mechanism, powder metering system and blade Combination of powder measuring system and roller mechanism for dispersion deposition on the build surface, including, but not limited to, electrostatic deposition on a transport surface followed by deposition on the build surface. The injection of the light-curable material (e.g., resin) can be realized by a specialized This is achieved by injection through the body of the part being built using a built-in injection build platform. Other methods of material deposition and in-situ material mixing are described below.
[0012] In addition, the method of producing the layer of the powder and binder slurry mixture can be spray deposition, pump system, etc. The formation of the layer may include dispensing the material by a dispenser or other method of dispensing a viscous fluid. In addition, the conditions can be adjusted by a blade, a membrane imaging window, a membrane reinforced by a solid surface, or Other methods of controlling layer thickness and uniformity may be included.
[0013] The imaging of the layers can be achieved by multiple means, e.g. a reflective pixel shifting system, to achieve the effective resolution of the projection system. This includes programmable area light sources (e.g. DLP projectors) that are used to increase the However, the present invention is not limited to the above. By being modified, the resolution of the imaging process can be further improved.
[0014] In yet another embodiment, the object is photocurable in accordance with digital data representing a given three-dimensional object. A solid freeform fabrication device is provided that is manufacturable using a resin material.
[0015] In another embodiment, a SF 3000 can be used to generate a composite object composed of a particulate material and a photocurable resin material. F device is provided.
[0016] In another embodiment, an SFF apparatus is provided that utilizes bulk deposition techniques to produce layers of material.
[0017] In another embodiment, a particulate material is combined with a photocurable resin material to produce a composite layer of material. FF equipment is provided.
[0018] In another aspect, the interchangeability of material components allows for the use of a wide range of material combinations. An SFF device is provided that makes this possible.
[0019] In another aspect, an SFF apparatus is provided that provides for the creation of composite layers by in-situ injection of a powder layer. do.
[0020] In another embodiment, an SFF apparatus is provided that uses an injection platform to perform in situ bonding of materials. will be done.
[0021] In another embodiment, an SFF device utilizes micropixelation to achieve improved resolution. Placement is provided.
[0022] In another embodiment, an SFF device utilizes pixel shifting means to achieve improved resolution. Placement is provided.
[0023] In other embodiments, the objects produced by the SFF apparatus can be thermally, chemically, or mechanically treated. This may result in improved internal bonding of the material components.
[0024] In another embodiment, a feedback system is used to optimize the rate of material deposition. obtain.
[0025] In another aspect, the build process is adapted to increase particle loading density within the printed part. A mixed feedstock may be used that is altered during processing.
[0026] In another aspect, the printed parts are subjected to surface quality testing prior to heat treatment to achieve high final density. It may be chemically treated to improve
[0027] Further features of the present invention will become more readily apparent from the following detailed description of the invention taken in conjunction with the accompanying drawings. It will become clear in [Brief description of the drawings]
[0028] Hereinafter, preferred embodiments of the present invention will be described with reference to the drawings. [Figure 1] FIG. 1 is an elevated perspective view of a machine for solid freeform fabrication according to one embodiment of the subject matter of the present disclosure; [Diagram 2] FIG. 2 is a perspective view from below of the machine of FIG. 1; [Diagram 3] FIG. 2 is a perspective view of the machine of FIG. 1 in a second configuration. [Figure 4] FIG. 4 is a cross-sectional view of the machine of FIG. [Diagram 5] FIG. 4 is a cross-sectional view of the machine of FIG. 3 in a third configuration. [Figure 6] FIG. 2 is an elevated perspective view of another embodiment of the machine of FIG. 1. [Figure 7] FIG. 7 is a cross-sectional view of the machine of FIG. [Figure 8] 7 is an enlarged cross-sectional view of the machine of FIG. 6 during the manufacturing process. [Figure 9] FIG. 7 is a schematic diagram of a part being built by the machine of FIG. [Figure 10] 2 is an elevated perspective view of a first configuration of a micromirror array utilized in a potential embodiment of the machine in FIG. 1; FIG. [Figure 11] 11 is an elevated perspective view of the micromirror array of FIG. 10 in a second configuration. [Figure 12] FIG. 2 is a schematic diagram of a micro-pixelation and pixel shifting system as may be used in a potential embodiment of the machine in FIG. 1. [Figure 13] FIG. 1 is a schematic diagram of a reflective beam steering system. [Figure 14] FIG. 1 is a schematic diagram of a refractive beam steering system. [Figure 15] FIG. 15 is a schematic diagram of an alternative embodiment of the system of FIG. [Figure 16] FIG. 9 is an elevated perspective view of one embodiment of the system of FIG. 8. [Figure 17] FIG. 17 is a front perspective view of the system of FIG. [Figure 18] FIG. 17 is an elevated perspective view of the system of FIG. 16 in a second configuration. [Figure 19] FIG. 17 is an elevated perspective view of the system of FIG. 16 in a third configuration. [Figure 20] FIG. 17 is an elevated perspective view of a first configuration of a micro LED array for use in a potential embodiment of the image generation system in FIG. [Figure 21] FIG. 21 is an elevated perspective view of a second configuration of the micro LED array in FIG. [Figure 22] FIG. 17 is an elevated perspective view of an LCD mask imaging system for use in a potential embodiment of the imaging system in FIG. 16. [Diagram 23] FIG. 1 is a top view of a pixel projected using a pixel shifting imaging system. [Figure 24] FIG. 24 is a top view of the pixel in FIG. 23 in the second configuration. [Diagram 25] FIG. 24 is a top view of a pixel in FIG. 23 in a third configuration. [Figure 26] FIG. 24 is a top view of a pixel in FIG. 23 in a fourth configuration. [Figure 27] FIG. 17 is a top view of pixels projected by the system of FIG. 16. [Figure 28] FIG. 17 is another top view of a pixel projected by the system of FIG. 16. [Figure 29]13 is an elevated perspective view of another embodiment of the micromixing system of FIG. 12. [Diagram 30] FIG. 30 is a bottom perspective view of the system of FIG. 29. [Diagram 31] FIG. 1 is a top view of the micropixel rastering path. [Diagram 32] FIG. 13 is a top view of the second micropixel rastering path. [Diagram 33] FIG. 11 is a top view of the third micropixel rastering path. [Diagram 34] FIG. 13 is an elevated perspective view of a second embodiment of a machine for solid freeform fabrication in accordance with an embodiment of the disclosed subject matter. [Diagram 35] FIG. 35 is a cross-sectional view of the machine of FIG. 34. [Diagram 36] FIG. 35 is a schematic diagram of a first step of a conveying process that may be used by the machine of FIG. 34. [Figure 37] FIG. 35 is a schematic diagram of a second step of a conveying process that can be used by the machine of FIG. 34. [Figure 38] FIG. 35 is a schematic diagram of a third step of a conveying process that can be used by the machine of FIG. [Figure 39] FIG. 35 is a schematic diagram of a fourth step of a conveying process that may be used by the machine of FIG. 34. [Diagram 40] FIG. 13 is an elevated perspective view of a third embodiment of a machine for solid freeform fabrication in accordance with an embodiment of the disclosed subject matter. [Diagram 41] FIG. 41 is an enlarged view of the machine of FIG. [Diagram 42] FIG. 41 is an elevated perspective view of a material deposition system that may be used in the machine of FIG. [Diagram 43] FIG. 43 is a perspective view from below of the material deposition system in FIG. [Diagram 44] FIG. 41 is a schematic diagram of a first step of a conveying process that may be used by the machine in FIG. 40. [Diagram 45] FIG. 41 is a schematic diagram of a second step of a conveying process that can be used by the machine of FIG. [Diagram 46]FIG. 41 is a schematic diagram of a third step of a conveying process that may be used by the machine of FIG. [Figure 47] FIG. 41 is a schematic diagram of a first step of an alternative material handling process that may be used by the machine of FIG. [Figure 48] FIG. 41 is a schematic diagram of a second step of an alternative material handling process that may be used by the machine of FIG. [Figure 49] FIG. 13 is an elevated perspective view of a fourth embodiment of a machine for solid freeform fabrication in accordance with an embodiment of the disclosed subject matter. [Figure 50] FIG. 50 is a front view of a material deposition system that may be used with the machine of FIG. 49. [Figure 51] FIG. 51 is an elevated perspective view of the material deposition system of FIG. 50. [Figure 52] 1 is a schematic flow chart illustrating a material handling process that may be used in one or more of the previous embodiments of the presently disclosed subject matter. [Diagram 53] FIG. 35 is an elevated perspective view of an object that can be manufactured with the machine of FIG. [Figure 54] FIG. 54 is a top view of an image that can be used to manufacture a first layer of the object of FIG. 53. [Figure 55] FIG. 54 is a top view of an image that can be used to manufacture a second layer of the object of FIG. 53. [Figure 56] 35 is a top view of a first step in a method of modulating resin flow within an object manufactured by the machine of FIG. 34. [Figure 57] FIG. 35 is a top view of a second step in a method of modulating resin flow within an object manufactured by the machine of FIG. 34. [Figure 58] FIG. 35 is a top view of a third step in the method of modulating resin flow within an object manufactured by the machine of FIG. 34. [Figure 59] FIG. 35 is a top view of a method of modulating resin flow around an object produced by the machine of FIG. [Figure 60] FIG. 35 is an elevated perspective view of a first embodiment of a material deposition system for use in the machine of FIG. [Figure 61]FIG. 61 is an enlarged cross-sectional view of a second embodiment of the material deposition system in FIG. [Figure 62] FIG. 35 is an elevated perspective view of an alternative embodiment of a build surface for use in the machine of FIG. [Figure 63] FIG. 35 is an elevated perspective view of a second embodiment of a material deposition system for use in the machine of FIG. [Figure 64] FIG. 35 is an elevated perspective view of a third embodiment of a material deposition system for use in the machine of FIG. [Figure 65] FIG. 65 is an elevated perspective view of the imaging array depicted in the system of FIG. [Figure 66] FIG. 66 is a perspective view from below of the imaging array of FIG. [Figure 67] FIG. 66 is a perspective view of the imaging array of FIG. 65 in a second configuration. [Figure 68] FIG. 66 is a top view of pixels projected by the imaging array in FIG. 65. [Figure 69] FIG. 66 is a top view of pixels projected by the second configuration of the imaging array in FIG. 65. [Figure 70] FIG. 65 is a cross-sectional view of the gas phase module depicted in the system of FIG. [Figure 71] FIG. 35 is an elevated perspective view of a fourth embodiment of a material deposition system for use in the machine of FIG. [Figure 72] FIG. 72 is a schematic diagram of a first step of a conveying process that may be used by the machine of FIG. 71. [Figure 73] FIG. 72 is a schematic diagram of a second step of a conveying process that can be used by the machine of FIG. 71. [Figure 74] FIG. 72 is a schematic diagram of a third step of a conveying process that can be used by the machine of FIG. 71. [Figure 75] FIG. 72 is a schematic diagram of a fourth step of a conveying process that may be used by the machine of FIG. 71. [Figure 76] FIG. 35 is an elevated perspective view of a fifth embodiment of a material deposition system for use in the machine of FIG. [Figure 77]FIG. 77 is a perspective view from below of a microdroplet deposition system such as that depicted in FIG. 76. [Figure 78] FIG. 77 is a cross-sectional view of material deposited by the system in FIG. 76. [Figure 79] FIG. 1 is an elevated perspective view of a part that can be manufactured by any of the aforementioned systems. [Figure 80] 79A-79C are cross-sectional schematic diagrams of powder particle distribution and possible hardening patterns in a first step of the manufacture of the part in FIG. [Figure 81] FIG. 80 is a cross-sectional schematic diagram of powder particle distribution in a second step of manufacturing the part in FIG. 79. [Figure 82] FIG. 1 is an elevated perspective view of a component and support structure that may be constructed by one or more of the systems described above. [Figure 83] FIG. 1 is an elevated perspective view of an array of components and support structures that may be constructed by one or more of the systems described above. [Figure 84] FIG. 84 is an elevated perspective view of an array of components and support structures of FIG. 83 in a second configuration. [Figure 85] 1 is a schematic flow chart depicting a process for integrating a support structure into a printing and sintering process. [Figure 86] 13 is a schematic flow chart illustrating a process for debinding a printed part. [Figure 87] 1 is a schematic flow chart illustrating a method for post-processing a printed part. Detailed Description of the Drawings
[0029] Stereolithography (SLA) manufacturing uses photopolymer resins and 1-5 show a system (100) that embodies this concept. In this embodiment, the build platform (102) includes a vat (104) containing resin (110). The image (105) is formed by solidifying a part of the resin (110) to form a layer of solid components (112). To achieve this, the projection unit 106 projects the image through a window 108 onto the resin 110. After a given layer is at least partially cured, the platform (102) moves upward to deposit the resin. The grease (110) is allowed to flow under the part (112) to provide material for the next layer.
[0030] The system is generally compatible with any photopolymer resin material or photopolymer resin. It can be used to process mixtures with powders. In some cases, this method A powder composite can be produced by the above-mentioned method, which can then be post-processed to produce a powder composite. The binder can then be removed and the powdered raw materials sintered into a solid component. The substrate is generally made of metal or ceramic, or any combination of sinterable materials. This is also fine.
[0031] In many cases where powder composite parts are being manufactured and the resin material has a high viscosity, There is a speed limit for this process presented by the fluidity of the material. The build tank (104) is moved to apply shear forces to the product (112) and the resin (110) in the tank (104). This shear action helps to detach the most recently cured layer from the window (108) and also To create the next layer, additional material is forced under the part (112).
[0032] 6-8 show an alternative embodiment of this system, which includes a build platform (102 ) is pumped onto the porous build surface and onto the parts (114) being built or sucked therefrom. and a fluid path contained therein for the fluid to be introduced therein. is constructed in a manner similar to that previously described, with a part (114) having a porous internal structure. Resin (110) is pumped through the build platform (102) and the part (114). The excess resin is then released into the build tank (114) and collected in the build tank (114). The pressure from this excess resin supply increases as the layers harden. This can aid in separating the part (114) from the build window (108) after the part is molded. To produce the part (114), the part (114) is post-cured to form a Any remaining resin (110) is allowed to solidify. To maintain the support structure (116), the support structure (116) is constructed of a plurality of sections such that the support structure (116) has a hollow overall structure. Any overhanging features of the part (114) may be built up and the tension of the part (114) being printed may be increased. It may have a porous surface that allows fluid communication to the protruding features.
[0033] FIG. 9 illustrates a method in which the system of FIGS. 6-8 may be utilized to manufacture a high density powder composite part. Typically, in slurry-based systems, density is limited. The load increases density, which improves the quality of the final part sintered from the printed powder composite part. However, increasing the powder loading also increases the slurry viscosity, reducing the manufacturing process. The process shown in FIG. 9 uses a low viscosity slurry to produce a dense sinterable mixture. Degree parts may be manufactured.
[0034] The powder (118) is suspended in the resin (110) to form a slurry. As a new layer is formed, The resin (110) is sucked through the part (117) to be built. This allows the resin to be removed. The powder loading rate is increased by adding powder (118) to the part, which is suspended in the original slurry. The powder (118) in the part (117) is packed more densely than the resin (110). A stiffening lattice structure that holds the powder (118) in place while allowing it to flow through the article (117). (119) are used to hold the powder together and ultimately sinter it into a solid final part. Additional for building porous parts that allow liquid resin to flow while bonding to The method will now be further described.
[0035] One of the most common imaging systems for curing resin materials is shown in Figures 10 and 11. The actuators in the DMD array are shown in Fig. By applying a charge to the individual mirrors (122), the light reflected from these mirrors (122) The light that falls off the filter may be rotated so that it is included in the final image or is discarded by an absorber. These systems are capable of curing all layers of material at the same time, significantly increasing production speeds. While this offers significant advantages over laser-based systems, the build area and Generally, images from DMD systems are limited in their resolution and accuracy by dividing each pixel into arbitrary widths, even numbers. The system can be focused to within a micron of a second. Most high resolution chips have an array of about 1000x2000 pixels. If a pixel size of 10 microns is desired, this corresponds to an imaging area of 1 cm x 2 cm. The 10 micron resolution produces surface finishes and textures not currently available from 3D printers. This translates to a level of precision and functionality that is highly desirable for printed parts, but the 1cm x 2cm The area of the field is insufficient for many applications. There are several ways to get around this limitation: Use multiple projectors and / or space the projectors around the build area. Multiple exposures are made by moving the lens, the sum of which makes up the completed image in the build area. Moving the projector to produce the image requires a very precise mechanical actuation system. This slows down the production process.
[0036] Using multiple projectors allows the image produced by each projector to be A usable build area is only possible if both the horizontal and vertical dimensions of the projection unit are as large as the projection unit itself. Otherwise there will be significant gaps between the images produced by the projector. In the case of a small number of projectors, multiple mirrors are required to produce images that are aligned with each other. There are more sophisticated options for using lasers and other optical elements, but in general this is Not scalable for larger production areas. Arrays of projectors are used. where each projector produces a small image, but the array fills the entire build area. The method is performed in a precise manner to generate a plurality of images for a complete image. The problem of slower production speeds remains, as the more extreme problems of slower operation systems are more common. and will have it.
[0037] The ideal configuration would be an array of projection units, each of which would have a different resolution than the one it occupies. Each projection unit must produce an image that is at least as large as the physical footprint it will The accuracy achieved by the component is consistent with the target component accuracy. Even a single projection unit can provide significant improvements in accuracy and speed for optical 3D printing systems. This would constitute a significant improvement.
[0038] Figure 12 shows the elements of a system that achieves this goal. FIG. 1 is a schematic diagram of the optical behavior of a light source (124) in either the "on" or "off" position. The pixel (122) that can rotate is illuminated, and the excitation light from the pixel (122) is When in the "on" position, the image of the pixel is focused on the microlens (126). is focused to a size smaller than its nominal size as seen on the imaging plane (130). The amount by which the focused image is smaller than the nominal size is determined by the resolution limits of the light source. Depending on the requirements of the application, such as situations where the resolution is not sufficient to achieve the desired resolution of the object shape to be In some embodiments, for example, the illumination generated by each illumination source may be selected. The illumination area covered by the captured image is less than the total size of each pixel area. Although both are 20% smaller, those skilled in the art will appreciate that a larger or smaller reduction in image size may affect image generation. It will be appreciated that this may be selected to adjust the final resolution of the system.
[0039] However, in this configuration, the size of the pixel image is too small to produce a complete image. Such pixels would be too small and too accurate to completely cover the imaging surface (130). To this end, refractive pixel shifting elements When the refractive pixel shift element (128) is rotated, the image of the pixel shifts laterally. A clockwise rotation of the refractive pixel shift element (128) shifts the pixel image to the left. A counterclockwise rotation of the refractive pixel shift element (128) produces a shift in the direction of the Causes a horizontal shift of the pixel image to the right.
[0040] In most imaging systems, the size of a pixel roughly matches the pixel pitch in the image. That is, the center-to-center distance between adjacent pixels. Neglecting losses from the gap, the projection from such a device with a pixel spacing of 50 microns is The pixel array depicted will have pixels 50 microns wide. For purposes of clarity, This type of pixel image would be called a "saturated" pixel image. Also called pixelization, this technique is used to improve the effective resolution of pixel-based image generation systems. Typically, this is done by projecting multiple images at different positions. where the position shift between subsequent images in the series is greater than the width of one pixel. In the case of projection systems for viewing images, these overlap to create a smoother A projection system for curing reactive materials. In the case of a pixel array, these overlapping images produce smoother features than are possible with a static pixel array. can be generated.
[0041] Conventional pixel shifting systems usually use mirrors, or Using microactuators on the DMD itself, these systems subdivide the pixels. It has a limited degree of flexibility and does not fundamentally change the size of the pixels. This requires that the edges of the images are defined by overlapping pixel images of When photocuring of the photosensitive material is required, the image may become blurred, which is undesirable for high precision imaging applications. This behavior is more clearly seen in the context of Figs. Will be discussed in detail.
[0042] The system described herein has several advantages over conventional pixel shifting systems. First, the pixel size is significantly smaller than the pixel pitch. Saturation of smaller pixels despite the pixel pitch being large relative to the cell size This means that the curing response of the irradiated material behaves as if an array was used. This allows for a larger total imaging area. Second, the pixel shift system , a refractive element is used to shift the pixel image. This configuration can be used in reflective systems or microphone It has a much higher inherent accuracy than those requiring a single actuator. The deflection of the excitonic beam from the stem is twice the rotation of the reflective element in the system. Therefore, if an angular accuracy of 1 degree is required for beam positioning, it is necessary to control this appropriately. A rotation system with an angular accuracy of 0.5 degrees is required to achieve this. Typically, the beam on the image plane To control placement to submicron accuracy, angular precision of microns is required. This can be difficult to achieve.
[0043] Figures 13 and 14 show this difference in accuracy. In this system, an incident beam (142) strikes a reflective object at a particular angular position (148, 150). At position 48, a first excitation beam (146) is generated, and at position 150, a second excitation beam (144) is generated. These excitonic beams (144, 146) then strike the image plane (130) In this system, the angular deflection of the excitatory beam (144, 146) is achieved by the reflecting element (148, 1 50) is twice the angular deflection of the actuator. As mentioned before, this places a premium on the accuracy of the actuation system. By comparison, FIG. 14 shows a refractive beam guidance system, in which the beam Instead of deflecting the beam by an angle, it is offset laterally by a specific distance. The beam (152) strikes the refractive elements (158, 160) and is irradiated by the entrance and coolant surfaces of the coolant elements (158, 160). The refracted beam of coolant (154, 156) strikes the image plane (130). The stem allows for much better alignment of actuator travel relative to beam travel for precise control. The refractive system provides a ratio of 0.1 degrees or more of rotation of the refractive element to lateral deviations on the order of 1 micron or less. This relationship may be configured to cause a directional translation at a specified thickness and refraction. The refractive index can be adjusted by using refractive elements, but generally, The level of angular accuracy required for the accelerator shift is comparable to that of a standard galvanometer or other rotary actuator. This can be easily achieved by using a
[0044] Finally, the cure response of many reactive materials is nonlinear, and doubling the radiation intensity increases the cure rate by as much as necessary. It can be seen that the required exposure time is reduced by more than a factor of two. The use of high intensities effectively reduces the dose required to achieve a significant cure response. This reduces energy consumption and increases the overall speed of the manufacturing process. Any pixel shifting system requires mechanical actuation of the shifting system itself and This system significantly reduces the amount of incident radiation, although some time will be lost to control. Some configurations allow the resin to be properly concentrated and the cure time reduced enough to compensate for this loss. In this case, the velocity obtained by concentrating the incident radiation is limited by the constraints on the motion of the refractive shift element. This more than compensates for the loss of control and the previously mentioned gains in accuracy and scalability. Together, this can produce a net gain in overall speed.
[0045] The refractive pixel shifting system from FIG. 14 above uses a single plate (158, 160). This is appropriate for monochromatic light sources, but generally Additionally, optical materials have refractive indices that vary at different wavelengths, which allows this device to be more accurate than other For all factors to be held constant, the incident beam (152 ) to fully characterize the photorefractive response of a material. The index-wavelength curve must be determined. The fact that this curve is not a flat line is This causes chromatic aberration in conventional optical systems. Typically, this occurs when two reference wavelengths are have different refractive index-wavelength curves that can be calibrated to have the same refractive effect for This is overcome by using an achromatic doublet, which is a system of lenses that A triad is a similar system that instead uses three lenses and is calibrated at three reference wavelengths. Yes; higher complexity systems may be used, but are rarely necessary.
[0046] Even when using a monochromatic light source, the use of a refractive panel as a shift mechanism makes it possible to It should also be noted that there are certain constraints on the rotation angle and beam The relationship with displacement is substantially linear; this relationship becomes non-linear for non-paraxial rays. Considering this, an ideal implementation of an image generation system using this shifting mechanism would be The system is constrained to collect only paraxial rays of the image source. This can reduce the light efficiency and overall light output. To mitigate these drawbacks, Other modifications to specific embodiments may be made.
[0047] A similar approach may be taken here and is shown in Figure 15. This example shows an achromatic birefringence. A birefringent pixel shift system is shown in FIG. 1. In this system, a primary shift window (160) is The beam (152) is shifted by an amount D1. Next, a second shift window (170) is opened to focus the beam exiting the first window (160). Shift the beam (164) back by an amount D2. The total displacement D is therefore the difference between D1 and D2: The system may be calibrated so that D is the same at the two reference wavelengths. In general, for any target displacement D, both windows (16 0,170) there will be an appropriate angle rotation. Therefore, Chromatic aberration is minimized over the spectrum. This approach is similar to the achromatic triad. Alternatively, it may be generalizable to the design of more complex systems, but this is not necessary depending on the application.
[0048] Generally, previous systems for reducing chromatic aberration have involved applying a chromatic aberration correction technique to a target build surface in both the X and Y directions. This can be applied to both shifting pixels, whether the light source is dichroic or polychromatic. This is useful when the light output of the image generating system is to be maximized. do.
[0049] 16-19 show two refractive shifters driven by two rotary actuators (202, 206). The element (204, 208) is focused both vertically and horizontally on the image plane (130). An implementation of this system is shown that displaces a pixel image (212). For simplicity, In these figures, a path of only five pixels is shown. This imaging surface (130) is generally It may be a window (108) in a build chamber (104) in a telelithography system (100), or or any other surface that includes a material that substantially changes state in response to irradiation. or simply any surface useful for producing high resolution images. Although other optical elements may be used to improve the system, the optical elements shown herein may include substantially the minimum set of elements to produce a desired effect.
[0050] In this system, a projection unit (106) projects pixels onto a microlens array (210). The image projected onto the microlens array (210) is generally a closely-saturated The microlens array (210) converts this saturated image into an unsaturated image. where the pixel image (212) is converted to a pixel pitch of For example, in many SFF systems, the thickness is 50 microns or more. The pixel size used is approximately the size of the projection unit that produces the image. This is to generate an image that fits the image. Multiple images of this size are arranged in a large size with no gaps between adjacent images. This can be produced by an array of projection units that completely images a large build area. However, if 10 micron accuracy is required for a particular build process, this conventional The image generation system is not sufficient. The microlens array (210) has a resolution of 1000 sq.m. relative to the pixel pitch. A filter that produces a 5:1 drop in pixel size can be used. The 10 micron pixels are generated with 50 micron spacing between adjacent pixel centers. Good too.
[0051] The rotational actuation of the horizontal shift actuator (206) rotates the horizontal refractive pixel shift element (208). A vertical shift actuator generates a shift in the pixel image (212) that will result in a horizontal shift of the pixel image (212). The rotational actuation of the actuator (202) produces a rotation of the vertical refractive pixel shift element (204), which This results in a vertical shift of the pixel image (212). The image generated by the laser beam behaves similarly to a laser imaging system. The spot can be moved around the imaging surface to trace out the image. , the spot size is focused to be very small to produce a high resolution image. The key difference is that this system can image large areas very quickly. , effectively having millions of focused beams moving in tandem. Using the specification in the example, the luminous intensity at the imaging plane is For a given system, the number of separate scans may be increased by a factor of 25 or more. Although more exposure is required, this increase in light intensity results in a net increase in imaging speed. The fact that the peak luminous intensity is achieved at the imaging plane makes this system a holographic It may also be advantageous for the application.
[0052] Generally, in any of the above systems, the pitch of the array is greater than the size of each light source. An array of illumination sources may be utilized. Alternative embodiments of potential sources are shown in Figures 20-22. FIG. 20 shows an array of micro LEDs (214), while FIG. 21 shows the array of micro LEDs (214) optimized for optical efficiency of the device. To illustrate this, such an array is shown with a corresponding array of microlenses (215). FIG. 22 depicts a light source (216) shining through an LCD mask (217), with individual apertures arranged in a grid. The images of these apertures are transferred by a projection optical system (218), A pixel image (219) can be generated on the display surface. Similar to the previously described system, In addition, refractive pixel shifting is utilized to generate a high-resolution complete image of the display area. This may also be the case.
[0053] A more detailed analysis of the shortcomings of conventional pixel shifting is demonstrated by Figures 23-26. For these images, the saturated array of pixels is The figure depicts a system in which the pixel is shifted by half the pixel width. FIG. 23 shows four pixels (232, 234, 236) projected onto the image plane (230). 36, 238). Line (240) indicates the ideal boundary of the hardened area, and the hardened part is This analysis was done primarily to determine the effect of the imaging technique used to cure the reactive material. Other pixels are used in this array that are relevant to the synthesis application and are not shown to simplify the analysis. In these figures, four different projection images are shown. Each image represents the pixel location where the energy required to cure the target material is - A material that delivered 25% of the dose and was fully cured only in the exposed areas in all four images There are other pixels above and below the four pixels shown (232, 234, 236, 238). Knowing that all material to the right of the ball flight line (240) will actually receive the proper dose However, some pixels (232, 236) are in the same pixel as in Figs. They are therefore divided into regions within the target region (244, 248) and the target region (242 , 246). The effect of this is to illuminate an area half a pixel wide, covering the entire border (240) The irradiation of the area to the left of the target boundary (240), extending along the 50% of the curing dosage, but this may still partially cure the material, depending on the properties of the material in question. In this case, the pixel shift distance was 1 / 2 the pixel width. , which we refer to as having a 2:1 subpixelation ratio. At higher subpixelation ratios, Energy dose gradients provide more steps from 100% energy dose to 0% energy dose. In general, any subpixel array that uses saturated pixels will In pixelated systems there is always an energy dose gradient.
[0054] In contrast, Figures 27 and 28 show the use of microlenses in an imaging system that uses pixel shifting. This shows the effect of introducing a lenses array. As mentioned before, this takes the saturated pixel array (252) and Convert it to an unsaturated pixel array (252). These figures show a 5:1 reduction in pixel size. The system is pixel shifted so that these micropixels are all you need. 4. The imaging system of claim 2, wherein the imaging device is a stent or a stent-type imaging system. The system behaves like a projection unit with 25 times the nominal number of available pixels. In the future, this amplification of precision can be much higher, potentially improving precision by several orders of magnitude. We will call the technique micropixelation.
[0055] As shown in FIG. 28, multiple exposures at different shift positions result in a saturated array of pixels. This can be achieved by using a shift system before exposing each image. It may be necessary to activate the system and lower it to a new position, which may affect the imaging Alternative techniques for imaging with this system may be considered. Further explanation will be given.
[0056] The essential elements of the projection unit (106) in the previous embodiment are the light source (124) and the micromirror (126). The first was an array of lasers (122), which is generally shown diagrammatically in Figures 29 and 30 and in Figures 20-23. As mentioned in 1, it can be replaced by an array of micro LEDs. When a pixel pattern is used during the image generation process, pixels that do not have equal heights and widths It may be useful to have an image where the primary motion during rastering is horizontal, to reduce the blur introduced into the image by turning it on and off while moving Sometimes it is useful to have pixels whose width is reduced relative to their height. To achieve this, a microlens (221) with astigmatic properties can be used. In the example, the display LED (220) illuminates the primary surface (222) of the display lens (221). Next, the micro LED (22 Illumination from point 0) exits the secondary surface (223) of the microlens (221) and reaches the image surface (224). In this case, the curvature of the secondary lens surface (223) is greater than the curvature of the primary lens surface (222) and is other than 1. The array of astigmatic micro-pixels produces a pixel image with an aspect ratio of 1:1. may be used in conjunction with a pixel shift mechanism or other pixel actuation mechanisms to image arbitrarily large surfaces. Good too.
[0057] Using a system such as any of the above also provides a method for detecting the presence of a sigma-based image on the imaging surface (130). This provides an opportunity to determine the optimal path for shifting the pixel image (212). In the previous example, 10 micron pixels can be used to image an area 50 microns wide. Figures 31-33 show some options for doing this. A pixel (262) intersects the pixel area (260). The pixel area (260) is a region in which micropixelization is performed. This is understood to mean the area that pixel (262) would occupy if the pixel (262) were not selected. will make the micropixel (262) start in the upper left corner of its pixel domain (260) and Move it across, move it down 10 microns, and then move it back to the left side of that domain (260). Shift the raster pattern before and after processing as shown in FIG. Another possibility, shown in Figs. 32 and 33, is to raster diagonally, a spiral pattern. or to provide substantially adequate illumination as is useful for a particular application. The micropixels may be turned on or off during operation. may be used to increase the speed of the image production process.
[0058] In general, you can also use a combination of standard pixel shifting and micropixeling. By subdividing the image into regions smaller than the nominal pixel size projected by each illumination source, Each illumination source (as defined above) also utilizes a pixel shifting system that Illumination sources in a grid pattern with a pitch dimension larger than the size of the source capable of generating It would be advantageous to have a system with an array of such sources. The smaller each illumination source is, the better the results and Although the resulting image resolution is higher, it is not possible to achieve high resolution directly from the imaging source. This requires a driver system that can render a very large number of pixels simultaneously. By using a micropixelation device, fewer pixels can be created. The images must be rendered simultaneously, and the higher resolution is achieved by sequential images. The degree to which pixel shifting is used to add a pixel to the image is generally determined by the micropixel shift, depending on the application. The resolution may be finer than that inherently achieved by the pixelization itself. For example, D chips are fabricated with 10um pixels spaced at a 30um pitch, and the projection optics are If this results in a 4:1 increase in linear image size from the projection surface to the projection surface, this is equivalent to a 1:1 increase in linear image size at the image generation surface. This results in 40um pixels on a 20um pitch. If a resolution of 10um is desired, then Multiple exposures shifted by um are used, which, as mentioned above, reduces the However, the energy gradient becomes less severe and The image will be sharper overall than if the 120um pixels were shifted in 10um increments. Furthermore, this resolution would be achievable if the pixels in the microLED array were 2.5um wide. However, since the power output from an LED is roughly proportional to the chip area, This results in a net output of approximately 1 / 16 the optical power of a device using 10um pixels. Therefore, to balance image sharpness with overall lighting intensity for a particular application, A combination of micropixelation and traditional subpixelation can be used. .
[0059] An alternative SFF system for digital production of parts is described in Figures 34 and 35. There are three important processes carried out in the system: powder deposition, powder injection, and irradiation. The powder measuring module (302) may be used for the first step. Optionally, the implantation platform (304) may be used for the second step, and the projection unit may be used for the second step. The powder measuring module (302) may be used for the third step. In general, any system capable of depositing a controlled amount of powder to produce a smooth layer. The injection platform (304) may be a powder deposition module having a porous upper surface (306). and a resin passage (308) for supplying resin to the powder deposited by the mold (302). In this system, a combination of capillary action and the applied pumping pressure drives the resin into the powder. The resin is then hardened by the projection unit (106) to bond the powder together. The powder composite components may be delaminated and sintered to produce powder composite components. The powder feedstock may then be post-processed to produce proximate solid objects fabricated from the powder feedstock.
[0060] Figures 36-39 explain this process in more detail. A first layer of powder (310) is placed on the injection platform. After being deposited on the platform (304), a resin is provided (312) to infuse the powder (310). Typically, this resin (312) holds the powder layers (310) together without interfering with further layers of powder. A second layer of powder (314) is deposited on the first layer (310). The resin level (312) can be increased by additional injection. The process can be repeated until the build process is complete.
[0061] Figures 40-43 show alternative approaches to achieve the goal of rapid production of dense powder composite parts. The figures depict several systems that use a dry powder approach that is then infused with resin. Instead of depositing, a low-density slurry is deposited on the build platform and the slurry is then The density of the slurry is determined by exposing it to an image that hardens parts of the slurry and bonds the powders therein together. Figure 40 shows one system for implementing this process.
[0062] In this system, a material deposition module (302) moves across a build platform (304). The fixed rollers (318, 326) are mounted so that each fixed roller (318 The material deposition module (302) is attached to both sides of the material deposition module (302) using films (320, 328) connected to the Each of these films (320, 328) is attached to the leveling rollers (322, 324). The material is then wound around the reels (314, 316) which automatically retract. As the stacking module (302) traverses the platform, one reel dispenses the film, The other retracts it. The slurry material is deposited on the platform by the material deposition module (302). The slurry can then be deposited on a flat surface (304) by a film. The film is flattened into a layer and kept flat by tension within the film. (302) simply uses a recoating blade on either side of the material deposition system (302). , and flatten the layer of slurry. In this case, the hardening process is performed by pressing the slurry into a flat layer, which allows the hardening process to occur. An image-forming unit that projects light through a film that transmits the appropriate amount of light at the relevant wavelengths to produce a The process may begin with an image from unit (106).
[0063] Another layer production system is shown in Figures 42-43. Depending on the layer thickness, it can produce flat layers. This can make it difficult to use the tensioned film system. is inadequate for controlling layer variations over large areas, especially when the layers in question are thin. In the system shown in Figures 42-43, the film (336) is During the flattening process, vacuum pressure is applied through holes (338) in the rigid block (334). In FIG. 43, the film (336) is held on a rigid block (334). The film (336) is attached to a round film mount. The assembly is held in place at both ends by the material deposition module (30 2) The deposited slurry material can be flattened and distributed in bulk. Once this is done, the vacuum source is turned off and the rigid block (334) is retracted, allowing the film (336) to pass through. This can enable imaging of the slurry material.
[0064] 44-48 show schematic diagrams of the material handling methods described in the previous system. Similar to the 3D model, the perforated build platform provides a high degree of thermal conductivity for both the platform and the part being built. This will be used to construct porous areas that allow fluid flow through the In these systems, a low-density blend of powder (310) and resin (312) is deposited on the build surface (304). The excess resin (312) is removed, increasing the effective powder packing density of the slurry, and The slurry is then pumped through the porous build surface (304) to densify the powder (310). Applying vacuum pressure to the fluid output of the build platform (304) is one option, but generally, the upper area of the build area and the build platform (304) Any means of creating a pressure differential between the lower / inner region of the For example, positive pressure can be applied to an enclosed build area. As shown in FIG. 46, all the excess resin (312) is removed by the resin (312) at the contact points between the powder particles (310). In this case, the lattice image generation technique described below may be used to This is not necessary, as the fluid evacuation process leaves an inherently porous structure, so that the fluid paths within the part Even if a solid hardened image is used, it remains available. As has been shown, multiple layers of material can be produced in a similar manner to produce a complete object. It can then be sintered to remove the binder and produce a metal or ceramic It is possible to produce closely spaced solid objects of material. Furthermore, this type of deposition process Ultrasonic agitation sources include recoater blades, filter blades, and a film, a reinforcement mechanism for the film, or a build surface (304) or another source. Good too.
[0065] In Figures 44-46, the slurry is exposed to the open atmosphere, whereas in many of the systems mentioned above, the slurry A film is used to flatten the lees, and the image is formed through this film. To carry out the processes described in Figures 44-46, a material deposition system and A recoating blade will be used. Note that the slurry is deposited in an open atmosphere. In this case, it may be possible to densify the slurry without applying vacuum pressure. If the slurry contains viscosity reducing additives (VRAs), the build area must be cooled to prevent evaporation of such ingredients. In this case, the VRA is heated to increase the deposition rate. It is possible that the organic solvent reduces the viscosity of the solution and then the viscosity of the deposited material layer. It may evaporate to promote field densification.
[0066] 47 and 48 show a film (340) used to level and distribute a layer of slurry material. The layer densification is essentially the same as previously described, with the main difference being The advantage is that the film can limit the escape of the resin after the powder has solidified. This resistance can be detected by the print system and indicates that powder compaction has occurred. This feedback mechanism can be used to determine the specific Depending on the implementation, it may be useful to have the film cured before another layer can be produced. These prints must be peeled off the applied material, which can slow down the printing speed. The merits of each of the processes will depend heavily on the specific implementation for a particular application.
[0067] FIG. 49 illustrates a system that utilizes an alternative approach to producing powder composite components. The feed reel (344), guide rollers (348, 350), and feed reel (342) are The film (346) is generally positioned to deliver a film (346) to the build surface (304). A blend of at least one monomer and at least one photoinitiator, and one or more plasticizers. , as well as a material that is solid at room temperature but melts when exposed to a heated build platform (304). With the possible addition of powder feedstock that can be melted. At least a portion of the film (346) that is in contact with the substrate (320) may be melted, while the remainder of the film (346) may remain solid. As a result, the outgoing reel (342) picks up the unused film (346) and The film (346) may be retracted into the build area to allow for the construction of additional layers. The fabrication of the part from the film is similar to that described above, especially in Figs. Once at least some of the material is melted, the process proceeds according to Figures 44-46. However, it is possible to at least partially undergo a phase transition for the purpose of generating a photodefinable three-dimensional object. The emergence of a solid feedstock that can be used for this purpose is itself a novel system. The part has excess material removed while at elevated temperature to keep the uncured material in a liquid state. It can dissolve unmodified (e.g., unpolymerized) materials but has no effect on polymerized materials. An exemplary monomer for this purpose is norbornene. It is a solid at room temperature, has a viscosity of about 0.75 mPa*s at 50°C, and when polymerized, has a viscosity of about 300°C. Further, the acrylate or epoxide or Other polymerizable monomers are solid under normal storage conditions of the material, but at some temperature, ideally Typically used in combination with non-reactive components that become fluid when heated to temperatures between 60 and 100°C. For example, paraffin wax is solid at 25°C but non-solid at 100°C. It is always a low viscosity liquid. High molecular weight polyethylene glycol and polypropylene glycol Coal is also a viable option for this type of material blend. It is solid at storage temperatures and liquid at higher operating temperatures and contains a photopolymerizable monomer component. Any material is considered an embodiment of the present subject matter. In such systems, the binder formulation generally contains less than 70% by weight of non-reactive diluent, PI system. It may be understood that the composition comprises at least 2% by weight of one or more of the ingredients used, and the remainder of the composition is The copolymer may be one or more monomers or oligomers that can be polymerized by the PI system, where The mixture is solid at a first storage temperature below 35° C. and is solid for 20 minutes at a second operating temperature above 35° C. Such bonding agents have a viscosity of less than 100 cps for the purpose of producing metal or ceramic components. The raw materials compounded from the additives are generally less than 45% when in-situ densification is used as described above. It is understood that the powder has a volumetric powder loading of more than 45% after in situ densification. is achievable, or if in-situ densification is not used, a volumetric powder loading of over 40% is achievable.
[0068] It is also possible to use a double membrane in the system illustrated in FIG. and the other layers may be made of the photopolymerizable materials mentioned above. In this case, the process is similar to the system shown in Figures 47-48, except that the transparent film is A build material is used as the imaging window where it is hardened by incident radiation.
[0069] 50-51 show an alternative embodiment of the system of FIG. 49, with infeed and outfeed relays. Instead of using a roller, this system uses two feed rollers (364, 366) to heat the A single feed is loaded with a thicker film (360) that is fed to the build surface (304). The melt pool (368) is formed by melting the film (360) against the build surface (304). The blade (372) is used to create a uniform layer of the slurry (370). The use of a solid feedstock is generally used to flatten the molten pool (368) in order to reduce the melting temperature. , easily switched for other materials, and powder media more effectively than liquid slurries during storage It is possible to provide a build material that can keep the film suspended. Although depicted as a solid feedstock, pellets or other form factors may generally be used. Although this may be advantageous, the principle of operation remains the same.
[0070] Additionally, a powder feedstock is used that comprises a metal powder having a solid coating of a binder material. By doing so, a system having similar advantages to those described in Figs. 50-51 can be implemented. The binder material may generally be of the type described above, where undergoes a phase change before being irradiated to initiate the polymerization process, resulting in the release of excess unpolymerized material. The powder may be removed by a solvent, possibly while at high temperature. The use of powder has the advantage of enabling the use of electrostatic powder deposition, which is generally , which is non-conductive in nature or has at least a coating which is non-conductive in nature. Furthermore, the thickness of the coating is limited to the powder material that is heated in the build-up. When the binder material melts, the layer solidifies under the weight of the powder and In an alternative configuration, a thicker core may be used such that no additional densification is required. Coatings can be used and densification can also be carried out, thus reducing the size of the particles in the raw material. By increasing the size, agglomeration can be reduced and the rheological properties of the feedstock can be improved. can be improved.
[0071] FIG. 52 illustrates a generalized view of the manufacturing process shown in many of the various embodiments of the previous figures. To overcome the inherent viscosity / speed limitations of traditional slurry-based SLA manufacturing, To achieve this, a slurry is deposited to produce a layer of material, which is then evaporated by evaporation of one or more components of the slurry. Removal of part of the liquid component of the slurry by suction or removal of the liquid component of the slurry by suction by any of several methods, including, but not limited to, removal of a substantial majority of Following the density change, an image is projected onto the build area. At least a portion of the slurry is selectively modified to solidify the liquid components of the slurry, The process is repeated to build the part in layers.
[0072] FIG. 53 illustrates a component (400) that can be manufactured using one or more of the systems described above. 54 and 55 show how powders are bonded together to form a part (400) and how resin is bonded next to the powder. A curing pattern (404) may be used to form a lattice structure that allows the layer of In some cases, more or less resin is allowed to flow to the subsequent layers. In order to achieve this, it is desirable to change the lattice structure of the assembled object during the assembly process. Figures 56-58 show one way to do this. Figure 56 shows the build surface (40 FIG. 57 shows the lattice structure (408) projected onto the resin acceleration zone (410). In this zone, it is desirable to increase the flow of resin to the subsequent layers. Figure 58 shows the 4 shows a modified lattice pattern (412) that allows for increased resin flow within (410). Local changes to the lattice pattern within a given layer are applied before the build process begins, during the build phase. Either during the process but before the layer in question is produced, or during the process of producing the layer in question. It is possible.
[0073] FIG. 59 illustrates additional imaging methods that can control fluid flow in the build process. Adding flow restricting features (414) to the outer areas of the part being built reduces the fluid flow rate. This helps regulate the fluid flow rate across the build area so that the flow rate is more uniform across this area. In some of the above systems, the fluid flows through a porous powder composite part. In either case, it is desirable to adjust the fluid flow rate to optimize uniformity, and a flow restriction mechanism (4 The feature of 14) is one way to achieve this end. In general, the flow restrictor (414) The effect is to reduce the effective area through which fluid can flow without being interconnected. As a result, additional objects are created and then removed during a cleaning step after the build process is complete. The flow restrictor must be located within a given layer and from one layer to the next. Any flow restrictor geometry can be used to achieve this flow regime as long as the and are strictly prime to each other. In this way, comparative It is relatively easy to wash away because it is easily washed away during the cleaning process. The material effectively behaves as an unbound material because The bonding process is sufficient to produce a bound volume of material that has some significant structural integrity. This is because they are not given a proper structure.
[0074] Additionally, FIG. 59 illustrates a method for confining fluid flow generally within a print area. The boundary feature (416) may be a boundary feature that may be injected after dry powder deposition. In this way, the flow of fluid to the excess powder can be restricted, and a low density slurry is precipitated, which is then They serve to provide separate flow paths during layer densification, such as when densified by a pressure gradient. or generally controls flow to a target build area or sub-area of that area. This boundary can be used to limit the size of the part or components as they are constructed. As it is constructed from a single powder bed, there is no need to use a build platform, as is common with existing powder bed fusion systems. Powder deposition in the relevant build area as it exists in a system where the mass is a containing piston There are no disturbing edge effects.
[0075] 60-78 show a number of systems for material handling that can improve upon the above-mentioned system. Generally, the system is used to produce flat layers that meet the requirements of SFF systems. The weighing powder for manufacturing may or may not be feasible in a single module. FIG. 60 shows a powder metering system (502) and a powder metering system (506) for producing a flat layer. A pair of rollers (530) that can be used to condition the powder deposited by the roller (502). , 532). By having two rollers (530, 532), the assembly The powder can be adjusted regardless of which direction it is moving relative to the build surface (520). This can expedite the material handling process.
[0076] Figure 61 can be used in any of the previously mentioned systems that require the deposition of a layer of powder. In general, there are design constraints that must be considered in a powder deposition system. There are several factors to consider, including speed, reliability, quality, and potential impact on the parts and machines being built. In the above mentioned systems, the powder metering system creates a layer of powder. However, the powder dissolves too quickly and is difficult to measure. If dispensed, the powder may aerosolize as it is gravity fed onto the build surface. FIG. 61 illustrates a method for restricting (506) the flow of aerosolized powder as it is deposited onto a build surface (520), A flat layer of powder (508) that has already been partially conditioned is produced, which is then rolled by a roller (530). The powder can be further compressed to produce a uniform layer of powder (510) having a high density. A powder metering system (502) having an exit shroud (504) is shown. By using a 100% sieve, the powder (506) can be pumped through the system while increasing the allowable speed at which the system can operate. Avoid allowing electrical wiring to escape from the build area and interfere with other mechanical and / or electrical systems. The advantage of this shroud (504) is that it provides an air gap for preconditioning the layer of powder (508). The presence of the edge and the fact that the deposited powder (506) is completely surrounded by the shroud This comes from two aspects: providing confinement on one side, but allowing the powder to be generally constructed. A regular doctor would leave it exposed to the environment and allow for a greater degree of aerosolization. Unlike blades, the complete enclosure provides preconditioning and potentially aerosol protection. This is combined with a greater degree of containment of the encapsulated powder.
[0077] FIG. 62 shows another improvement to the previously described system that allows for better powder containment. The modified build platform (520) is configured such that the aerosolized powder is vents (522) that can suck in the surrounding environment to prevent air from escaping from the room, as well as The nozzle has a powder collection pocket (524) for collecting any excess powder that is deposited in the nozzle. These further improvements control where powder is allowed in the overall manufacturing system, Therefore, any damage that may occur from powder ingress into the operating / control elements of the system is prevented. Stop.
[0078] In some cases, materials that are fibrous in nature or contain non-spherical particles are used. For example, some ceramics may be made with elongated grains. Rather, the orientation of these grains in the manufactured component produces specific anisotropic mechanical properties. FIG. 63 shows a method for adjusting layers of material to align elongated particles. In this example, raised rollers (534, 536) are used to provide a system more suited to this class of material. Typically designed to interact with and align ridges, combs, or elongated particles. Any roller configured with other mechanisms may be used herein.
[0079] FIG. 64 illustrates the imaging unit (106) and / or injection platform (50) shown in the previous figures. 04) This scenario describes a much more sophisticated material handling system that eliminates the need for In the stem, a powder metering system (502) deposits the powder and rollers (530, 532) regulate the powder layer. Then, the vapor phase resin module (540, 542) injects resin into the powder, and the micro LED array (550, 552) The resin hardens and bonds the powdered raw materials. This system The material deposition is to the right of the build surface (520). When moving, the primary roller (530), the primary vapor phase resin module (540), and the primary micro LED As the material deposition system moves left relative to the build surface (520), a secondary roller (532), a secondary vapor phase resin module (542), and a secondary micro LED array (552) In this way, the material deposition module does not require a delay between the production of successive layers. Without the need for a traverse, the build surface (520) may be traversed back and forth.
[0080] Figures 65-67 show the primary micro LED array (550) in more detail. The light source is composed of an array of micro LEDs (554) and an array of micro lenses (556). As such, each LED can produce a spot that is substantially smaller than the LED itself. Each row of microLEDs is laterally shifted by at most one spot width relative to the previous row, The number is such that the entire construction area can be imaged. The image is shown in Figure 68. Each row is coupled with the movement of the entire array across the platform. The lateral shift of replaces the shift effect of the refractive pixel shifting system described above. In addition, the system uses the astigmatic optics previously mentioned to optimize resolution and curing response. FIG. 69 shows an array of astigmatism micro LED systems according to this embodiment. The image generated by the above is shown.
[0081] FIG. 70 shows the primary gas phase resin module (540). This module converts liquid resin into a vapor. The vapors can then be absorbed by a layer of powder where the resin condenses. The powder returns to a liquid form, which can then be irradiated to bond the powder ingredients together. By using the system, the amount of resin required by the process is reduced, It may be possible to expedite the entire feed processing process. In this embodiment, the resin supply line The resin is then transferred to the module (540) by the nozzle (544). The resin is then evenly applied to the evaporation element (549). The vaporized elements are distributed from a central resin channel (546) into a number of channels (548) to Generally, the resin is subjected to ultrasonic vibration, thermal energy, or vaporizing elements (549) in close contact with the resin. It may be actuated by other means of converting the liquid state to a proximate vapor state. The vapor is then charged by a voltage applied to the vaporizing element (549) and a voltage applied to the secondary charging element to which the vapor is exposed. This can be achieved by applying a voltage to the build area, exposure to an electron gun or other charge source, or electrostatically attracting vapor droplets to the build area. The build area may be electrostatically charged by any other available means for charging the build area. Generally, it can be electrically grounded or otherwise electrically manipulated to achieve a desired behavior. may be generated.
[0082] FIG. 71 shows the powder metering system from either the primary powder metering system (502) or the secondary powder metering system (503). A material deposition system in which a gas phase resin module (540) deposits resin prior to depositing powder. The powder bed is moved by the primary roller (330) depending on the direction of travel of the material deposition system. or the secondary roller (532). A resin vapor phase is deposited on the build surface (520) before the powder, and the resin vapor phase is coalesced before the application of the powder layer. The resin is then mixed into a liquid film using the weight of the powder and the force of the rollers (530, 532). This allows the powder to be infiltrated in a bottom-up manner, facilitating the injection process.
[0083] Figures 72-75 show in more detail the process carried out in the system of Figure 71. As the film is deposited on the build surface (520), followed by the deposition of a first layer of powder (592), The resin (590) is injected through the powder layer (592). Generally, the thickness of the resin film (590) is such that it substantially overlaps the powder layer (592). The thickness of the powder layer (592) should be less than the thickness of the powder layer (592) so that only enough resin (590) is provided to bond to the powder. After part of the layer is cured, additional resin (594) is deposited, forming a second layer of powder. The resin level is raised so that (596) can be deposited and injected. This is the build process. This may be repeated with further deposition of resin and powder until completion.
[0084] FIG. 76 shows a configuration similar to that of FIG. 71 in that resin deposition occurs before powder deposition. The key difference is that rather than a gas-phase resin module (540), a resin microdroplet deposition array (560) is utilized. The resin microdroplet deposition array (560) is shown in more detail in FIG. An array of microdroplet dispensers (562) are arranged to move the system across the build surface (520). This is used to deposit droplets of resin when the resin is applied to a given area. It provides some control over the amount of resin, allowing for greater control over the depth of resin in specific areas of the build area. The thickness can be controlled to produce uneven amounts of pouring in a given powder layer. This is To improve vertical print resolution by effectively allowing It can be useful to limit the exposure of the area and therefore the cure depth of the resin binder. By doing so, it is relatively easy to print a partial layer on top of a normal layer, It is typically not possible to print a partial layer on the bottom of a normal layer. The system makes it possible to achieve this type of hardening behavior. Figure 78 shows the process The results show that the resin boundary (580) varies across the build surface (520) and at different levels. The powder particles (570) are bonded together. This depiction is intended to be a schematic representation of the process, as well as a representation of the build process. For most powders used in the process, the maximum particle size is generally smaller than the thickness of the powder layer. Now, recognizing that the resin has a different particle size distribution, this varying resin boundary (580) is Generally, this translates to a similarly varying boundary of the printed part.
[0085] The limitations of the droplet size achievable in conventional microdroplet deposition systems mean that evaporation during deposition The resin droplets are mixed together to deposit microdroplets consisting of a suspension of resin droplets in a carrier medium that can be volatilized. It may be advantageous to fuse the droplets together into a film. For example, droplet ejection systems typically Although the size of the droplets may be limited to picoliters, there are concerns over the femtoliter range. It may be possible to generate droplets in a suspension. In this way, a microdroplet deposition system This allows for the production of thinner resin films than is possible by direct deposition from a polymer.
[0086] In the previous figures, a method for producing fractional layers was described, which depends on the binder composition, By controlling the curing atmosphere and the wavelength of light used to cure the binder material, Therefore, it may be achieved by other means. In general, shorter wavelength light is more effective at overcoming oxygen inhibition. Due to its superior ability to resist heat, it is more effective at curing the surface of photosensitive materials. Therefore, the top part of the layer can be cured by short exposure to high intensity short wavelength UV light. Deeper parts of the layer can be etched by longer exposure to lower intensity long wavelength UV light. In addition, the fluorescent catalyst can be added to the binder. Addition of fluorine to mixtures to increase the depth of cure and allow selective cure of different depths of layers of material. It is possible.
[0087] Coumarin dyes are particularly effective in the UV and blue portions of the spectrum and have It has a higher quantum yield and both absorption and emission peaks below 500 nm. utilizing photoinitiators, fluorescent dyes, and single- or multi-color imaging systems that are sensitive to Many configurations are possible, each with beneficial effects. In the simplest case, a photoinitiator A formulation having a PI system, a fluorescent dye, and a monomer system, wherein the PI system is a Such a system is sensitive in both the absorption and emission regions of the spectrum. When used, it is particularly useful as a binder for powdered raw materials with very high volume loadings. If used, direct visibility to all areas that need to be cured in a given layer is required. Lines are not possible and the fluorescent dye can reach further areas of the binder that would otherwise be inaccessible. In this way, fluorescent dyes can be used as optical catalysts to By using a fluorine-containing ... It may also reduce the exposure time required to bond layers of materials together. In systems such as those described above, the formulations generally contain less than 0.25% by weight of fluorescent dye, e.g., PI systems. It may be understood that the composition contains at least 2% by weight of one or more of the ingredients used, the remainder of the composition being , may be one or more monomers or oligomers that can be polymerized by the PI system.
[0088] Another configuration is one in which polymerization can occur in at least two wavelength regions, with absorption between these two regions. The fluorescent dye has an emission peak within the long wavelength region of the PI system. The shorter wavelength PIs are generally due to the free radicals at the surface of the binder material. This system is not significantly affected by the oxygen inhibition effects that are common in ethanol systems. , which is less than the absorption region of the fluorescent dye but is a first of at least two wavelength regions of the PI system Exposure to short wavelengths within the wavelength range causes polymerization at the surface of the layer of material, and the result of this exposure The timing may be controlled so that only the top portion of the layer is cured. Exposure to wavelengths within the absorption band is utilized to cure the material in the bottom section of the layer. while oxygen inhibition prevents polymerization in the upper sections of the layer. Polymerization of discrete layers can be achieved. In systems such as those described herein, The formulation generally contains less than 0.25% by weight of a fluorescent dye that can be excited at a first wavelength, substantially at least 0.1% by weight of the a first photoinitiator, sensitive at a third wavelength longer than either of the first and second wavelengths, At least 0.1 wt. % of a second photoinitiator substantially contained within the emission band of the dye, and PI. It may be understood to include at least one monomer or oligomer that can be polymerized by the system. do.
[0089] Another method to achieve fractional phase control is to use PI systems and monomers with multiple functional groups. For example, it may be polymerized by ring-opening polymerization or other means using a cationic system. Polymerizable by free radical systems with epoxides, oxetanes, or other monomers Mixtures of acrylate monomers or other monomers can be used to produce free radical and cationic acrylates. In this system, the cationic PI may be used in combination with a PI system containing both PIs. If the PI is sensitive at short wavelengths and the free radical PI is sensitive at longer wavelengths, as described above A behavior similar to that described above can be achieved. Exposure to short wavelengths initiates polymerization at the surface of the layer. while exposure to longer wavelengths can be used to cure below the surface of the layer. It has an absorption band at a wavelength longer than the absorption region of cationic PIs and is in the absorption region of free radical PIs. Fluorescent dyes having emission bands within them can also be used to enhance the curing of the bottom regions of the layer. A hybrid having both acrylate and epoxide functional groups (or other similar groups) Lid monomers may also be used in this context.
[0090] Figures 79-87 show how to process printed parts that can improve such parts in various ways. Figures 79-81 illustrate several methods that can improve the surface finish. Generally, a method for producing powder composite parts that can be printed and then sintered is presented. Many of these methods require larger geometric dimensions than would be nominally acceptable based on the powder particle size within the print. It is possible to provide imaging resolution to provide finer control over target shape. Figure 79 shows one object (600) where this behavior can be observed. Figure 80 shows the object (600) The cross section of the powder (602) is used to bond together the powder (602) to print the object (600). As can be seen in this figure, some of the powder particles (60 2) protrudes beyond the surface of the object defined by the cured pattern (604). In this case, The boundaries of the cured pattern (604) can act as a mask, and the part can be etched by applying a mask to the surface of the part (600). It may be electropolished to remove the portions of the powder particles (602) that protrude beyond the surface. The result of this process is shown in FIG. 81 and may include, in some cases, the optically defined portion of the part (600). The surface itself may be porous, so that in order to prevent penetration into the part (600), An electrolyte must be selected that has suitable viscosity and surface tension characteristics. The charges are minimal and well masked, so the process is quick and with minimal additional charges. This can be achieved at additional manufacturing costs.
[0091] FIG. 82 illustrates a part (610) that can be manufactured by any of the aforementioned systems, and Shown in FIG. 6 is a support structure (612) that can be manufactured separately or in conjunction with the part (610). The portion (610) includes protrusions that will significantly deform if not supported during sintering. 2) is coated with a sintering inhibiting solution and positioned under the overhang of the part (610). By so doing, the support structure (612) supports the overhang of the part (610) during sintering. An oxidizing agent can be applied to the top surface (614) of the support structure (612) to aid in the oxidation of this surface. The surface (614) is oxidized to prevent adhesion to the part (610) during sintering while preventing deformation of the part (610). This can also be prevented.
[0092] Figures 83-84 show automated cleaning and sintering of parts printed via any of the methods mentioned above. FIG. 83 shows a method for improving the solubility of a batch-printed polymer in combination with a support structure (630). Figure 84 shows an array of printed parts (620). Figure 84 shows the removal of excess build material from the parts after printing. In many of the above devices, additional support structures (632) are shown that can aid in the process of After the printing process is complete, there is uncured material surrounding the printed part. can be removed by washing in a solvent bath. In the system depicted in Figure 84, The two support structures (630, 632) are not attached to the part (620) and hold the part (620) in place during cleaning. It also acts as a rack that can be used for simple pick-and-place automation. The sintering system can then move them to another rack for sintering. In addition, the lower support structure (630) is treated in the manner described in FIG. If so, it may be used as a support during sintering, and generally allows post-processing of many parts simultaneously. For ease of use, any non-adhesive support structures may be printed in conjunction with the array of parts. Thus, manufacturing efficiency is improved.
[0093] FIG. 85 shows as a schematic flow chart the process used in FIG. 82, in which the support structure is It may be printed integrally with one or more parts or separately and adheres to the part during sintering. It is treated to inhibit the sintering process and is used as a support during the sintering process. Effectively increasing the types of geometric shapes that can be produced by the stamping and sintering process It is possible.
[0094] FIG. 86 shows additional methods for post-processing printed parts. Traditionally, green The part is subjected to a sintering process to remove a substantial portion of the binder material to prepare the part for sintering. In particular, the binder material is treated thermally, with a solvent, or with a catalytic process. If some of the components in the binder have a higher volatility than the other components, exposure to vacuum pressure can This may be possible in any of the previously mentioned systems by removing some of the binder. This method provides a fast, low-temperature system for desorption even in Particularly applicable to the above-mentioned systems in which perforated parts are manufactured, the perforations incorporated in the parts The flexible structure allows for rapid release of volatilized binder material without distortion or destruction of the part. .
[0095] Figure 87 shows an additional method for post-processing printed parts. The system described above can potentially use a wide variety of binder formulations, but is not limited to multiple types. It may be advantageous to use specific blends of types of monomers and multiple curing treatments. In particular, at least one monomer in the formulation is photopolymerized by a photopolymerization process (primary monomer). A second monomer may be polymerized by a thermal process, and another monomer (secondary monomer) may be polymerized by a thermal process. The polymer formed by curing the secondary monomer (primary polymer) is The polymer formed by the polymerization (secondary polymer) is not water-soluble, is soluble in a solvent that has the ability to decompose cleanly in an inert or reducing atmosphere. When used in combination with a variety of reactive metal powders, it can be used to produce sintered metal parts. One such example uses an acrylate-based first monomer / polymer and The second monomer / polymer may be olefinic. Solvent debinding agents include: One option for removing the primary polymer in such formulations is to remove the secondary polymer. Any formulation that allows removal of the primary polymer without adversely affecting the composition is advantageous. This is especially true for metals that cannot be exposed to oxygen during sintering. The most interesting and easily photopolymerizable materials are those used for processing metals in sintering processes. If decomposition is not possible in an inert or reducing atmosphere, which is typical of There is.
[0096] Although a specific combination of systems is shown herein, any combination of the aforementioned subsystems may be used. According to any of the methods or systems described above, Any system that provides powder deposition, powder injection, and irradiation is an embodiment of the present subject matter. It can be understood that.
[0097] The subject matter may be embodied in other forms without departing from its spirit or essential characteristics. The described embodiments are therefore considered in all respects to be illustrative and not restrictive. The present subject matter has been described with respect to certain preferred embodiments. However, other embodiments apparent to those skilled in the art are within the scope of the present subject matter.
Claims
1. A method for manufacturing a three-dimensional object, comprising the steps of: delivering a build material to a build surface, the build material comprising a mixed composition of a powder material and a binder material; Increasing the powder loading density of the build material provided to the build surface; Selectively irradiating the build material to change a physical state of a portion of the build material. 、 The method according to claim 1,
2. 2. The method of claim 1, wherein applying the build material to the build surface comprises: The method comprising providing the build material as a pre-mixed slurry.
3. 10. The method of claim 1, comprising the steps of sequentially producing a plurality of layers of material, and The method comprises emitting a layer to produce an object.
4. 4. The method of claim 3, wherein the step of selectively irradiating the build material comprises: radiating the build material in a radiation pattern having a structure that allows fluid to flow therethrough. Includes, a method.
5. 3. The method of claim 2, wherein the step of delivering the build material to the build surface comprises: lowering the build material into a vat of build material; moving the build surface incrementally away from the vat of build material; The method includes:
6. 3. The method of claim 2, wherein the step of delivering the build material to the build surface comprises: providing a layer of material on the build surface; moving the build surface in a stepwise manner away from an imaging system; The method includes:
7. 7. The method of claim 6, further comprising applying a coating of a coating material to the build surface using a doctor blade. adjusting the conditions of the build material being heated.
8. 7. The method of claim 6, wherein the build is applied to the build surface using a membrane. The method comprises adjusting the condition of the material.
9. 9. The method of claim 8, further comprising the step of stabilizing the membrane with a rigid surface during layer generation. How to do it.
10. 5. The method of claim 4, wherein increasing the powder loading density of the build material comprises: The method includes flowing a fluid across the build surface.
11. 11. The method of claim 10, wherein increasing the powder loading density of the build material comprises: , flowing a fluid through the object being built.
12. 3. The method of claim 2, wherein increasing the powder loading density of the build material comprises: densifying said powder material using ultrasonic agitation.
13. 3. The method of claim 2, wherein increasing the powder loading density of the build material comprises: volatilizing at least a portion of at least one component of said binder material. 。
14. 14. The method of claim 13, wherein the at least one component is a volatile organic solvent. ,method.
15. 4. The method of claim 3, wherein increasing the powder loading density of the build material comprises: removing an amount of binder from a given layer so that said layer has a porous structure; Including floor, method. wherein
16. each configured to generate an image within a respective pixel region of the target surface, The illuminated area covered by the generated image is the sum of the sizes of the respective pixel areas. an array of selectively actuated illumination sources at least 20% smaller than an image shifting device for shifting the position of each image within said respective pixel area; An image generating system comprising:
17. 17. The imaging system of claim 16, wherein the image shifting device comprises at least one An image generating system having a rotatable refractive element.
18. 18. The imaging system of claim 17, wherein the image shifting device shifts the image along each of the different axes. and a second rotatable refractive element for moving said image through said first rotatable refractive element.
19. 20. The imaging system of claim 17, the image shifting device has at least two refractive elements; The at least two refractive elements are calibrated to reduce chromatic aberration in each image. With various refractive indices, Image generation system.
20. 20. The imaging system of claim 19, wherein the image shifting device is arranged to shift the image along two axes. Image forming system having four rotatable refractive elements configured for achromatic shift Hmm.
21. 17. The imaging system of claim 16, The array of illumination sources comprises: a DMD chip configured to reflect radiation from an incident light source; A microlens configured to direct radiation from the DMD chip to the surface. array, An image generating system comprising:
22. 17. The imaging system of claim 16, wherein the array of illumination sources is a micro LED array. An image generating system having a ray.
23. 17. The imaging system of claim 16, wherein the array of illumination sources comprises a large source and an LCD. An image generating system having a combination of masks.
24. 21. An image generating system according to claim 17, wherein the image shifting device comprises: The position of each image is moved by a minimum movement amount smaller than the maximum dimension of each pixel area. The image generating system is configured as follows.
25. 1. A method for manufacturing a 3D object, comprising: delivering a build material to a build surface, the build material comprising a solid mixture of a powder material and a binder material; changing the state of the binder material; Selectively irradiating the build material to change a physical state of a portion of the build material. 、 The method according to claim 1,
26. 26. The method of claim 25, wherein the solid mixture comprises the powder material and the binder material. The method of claim 1, further comprising:
27. 27. The method of claim 26, The membrane has a plurality of layers; One layer has a non-reactive, semi-transparent imaging window; method.
28. 27. The method of claim 26, wherein the step of changing the state of the binder material comprises forming a uniform layer. generating an in-situ regulated molten pool from the film on the build surface.
29. 26. The method of claim 25, wherein the solid mixture comprises the powder material and the binder material. The method of claim 1, further comprising:
30. 26. The method of claim 25, wherein the solid mixtures are each coated in the binder material. having particles of said powder material being coated thereon.
31. The method according to any one of claims 26 to 30, further comprising changing the state of the binder material. increasing a powder loading density of the build material after
32. 31. The method of claim 30, wherein the step of changing the state of the binder material comprises: A method for increasing the powder loading density of a powdered material.
33. 26. The method of claim 25, wherein the build material is left unchanged after irradiation of the build material. removing the activating moiety.
34. 1. A method for manufacturing a 3D object, comprising: delivering a build material to a build surface, the build material comprising a mixture of a powder material and a binder material; The build material is selectively irradiated to form a lattice pattern that allows fluid to flow therethrough. generating a layer or layers; Monitoring the rate of flow of fluid through one or more of the layers provides filtering to a fluid control system. providing feedback; The modification of the grid pattern of a given layer is based on the observed flow of fluid in at least a portion of a past layer. Phases according to quantity, The method according to claim 1,
35. 35. The method of claim 34, wherein the step of providing build material comprises: delivering the powder material to the build surface; injecting said binder material into said powder material; The method comprising:
36. 35. The method of claim 34, wherein the step of providing the build material comprises: applying a slurry containing the mixture of binder materials to the build surface. Law.
37. 1. A method for manufacturing a 3D object, comprising: Delivering a build material to the build platform, the build material including a mixture of a powder material and a binder material. Stages and Selectively irradiating the build material to form selected parts within the build platform. Producing one or more layers having boundaries configured to contain fluid flow within the lint region. Floor, The method according to claim 1,
38. 38. The method of claim 37, wherein the boundary is selected to reduce the flow of the binder material. The method is configured to confine the print area to within the print area.
39. 38. The method of claim 37, The step of applying the build material may include applying a powder of the build material to the build surface. increasing the loading density; The interface has a flow path through which the binder material is drawn from the powder material. 、 method.
40. 38. The method of claim 37, wherein the step of providing build material comprises: depositing the powder material on the build surface; injecting said binder material into said powder material; The method comprising:
41. 1. A method for manufacturing a 3D object, comprising: delivering a build material to a build surface, the build material comprising a mixture of a powder material and a binder material; The build material is selectively irradiated to form a grid pattern that allows fluid to flow therethrough. generating one or more layers of the object; and curing a pattern of a plurality of discrete flow control portions within an area exterior to the object to form the one or more layers. controlling fluid flow through the layer; The method according to claim 1,
42. 42. The method of claim 41, wherein the step of providing build material comprises: depositing the powder material onto the build surface; injecting said binder material into said powder material; The method comprising:
43. 42. The method of claim 41, wherein the step of providing the build material comprises: applying a slurry containing the mixture of binder materials to the build surface. Law.
44. 1. A system for manufacturing a 3D object, comprising: A build surface; configured to deliver powder material to the build surface and precondition the powder material; A one-piece powder blade configured to hold the powder material in a manner that prevents aerosolization. a material supply system having a powder metering system with a shroud or cover structure; A system comprising:
45. 45. The system of claim 44, wherein the material supply system adjusts the powder material. The system includes a roller configured to:
46. 1. A system for manufacturing a 3D object, comprising: A build surface; a powder delivery system configured to deliver powder material to the build surface; a binder delivery system configured to introduce a liquid binder into at least a portion of the powder material. Stem and Airborne aerosol powder can detach from the build surface and interfere with other electromechanical systems. and a plurality of flow channels integrated around the periphery of the build surface configured to prevent 、 A system comprising:
47. 1. A system for manufacturing a 3D object, comprising: A build surface; a powder delivery system configured to deliver powder material to the build surface; a binder supply system configured to supply a liquid binder to the powder material; a powder metering system and at least one roller configured to condition the layer; Equipped with The roller is configured to align substantially elliptical, fibrous, or dendritic powder particles. having system.
48. 48. The system of claim 47, wherein the roller portion comprises a ridge. 。
49. 48. The system of claim 47, wherein the portion of the roller includes a plurality of teeth. Hmm.
50. 1. A method for manufacturing a 3D object, comprising: applying a layer of liquid binder to a build surface; Delivering powder material to the build surface fills the powder material with the liquid binder. and Selectively operating an imaging system to irradiate the liquid binder to image the powder material. forming a layer of said object by bonding at least some of said layers together; The method according to claim 1,
51. 51. The method of claim 50, The step of applying a layer of liquid binder may include the step of metering an amount of applied liquid binder. death, The step of supplying the powder material includes applying the powder material to a desired position in the powder layer with the liquid binder.
3. Fill the space between the layers so that the effective vertical resolution of the imaging system is narrower than the thickness of the layer. step, The method according to claim 1,
52. 51. The method of claim 50, wherein the step of applying the layer of liquid binder comprises applying a jetting head providing droplets of said liquid binder using
53. 51. The method of claim 50, wherein the step of applying a layer of liquid bonding agent comprises applying an ultrasonic spray to the surface of the substrate. applying droplets of said liquid binder using a laser system.
54. 51. The method of claim 50, wherein the step of applying a layer of liquid binder comprises: A method comprising providing a vapor of a binder that condenses on a surface.
55. 1. A method for manufacturing a 3D object, comprising: applying a build material to a build surface; selectively irradiating the build material to produce layers of the object; The step of selectively irradiating the build material produces an array of images in a plurality of rows on the surface of each layer. [0023] Including the use of an array of illumination sources to generate a center-to-center distance between said array of images is greater than a width of each image; Each of the plurality of rows of the image is offset from an adjacent row by a distance not exceeding the width of each image. R, The rows are linearly translated across a target area to completely image the target area. have a sufficient number of columns to generate method.
56. 56. The method of claim 55, the build material having a mixed composition of a powder material and a binder material; The step of selectively irradiating the build material bonds at least a portion of the powder material to [0023] Combining to generate a layer. method.
57. 56. The method of claim 55, wherein the step of providing build material comprises: depositing the binder material on the build surface; injecting said binder material into said powder material; The method includes:
58. 56. The method of claim 55, wherein the step of depositing the binder material comprises: depositing a slurry containing the mixture of binder materials onto the build surface. method.
59. 1. A binder material for use in the manufacture of 3D objects, comprising: at least one reactive monomer; one or more photoinitiators; Fluorescent material selected to function as a photocatalyst and not exceeding 0.5% by weight of said binder material It has photopigments, configured to be mixed with a powder material to generate a composite part; Binder material.
60. 60. The binder material of claim 59, wherein the fluorescent dye is a coumarin derivative. Agent materials.
61. 60. The binder material of claim 59, wherein at least one of the one or more photoinitiators A binder material, wherein one absorption band includes both the excitation band and the emission band of said fluorescent dye.
62. 60. The binder material of claim 59, the one or more photoinitiators include a first photoinitiator and a second photoinitiator; The first photoinitiator has a first absorption band and the second photoinitiator is substantially away from the first absorption band. a second absorption band distant from The fluorescent dye has a third absorption band substantially separate from both the first absorption band and the second absorption band. A band is provided. The fluorescent dye has a band that substantially intersects one or both of the first and second absorption bands. having an emission band, Binder material.
63. 60. The binder material of claim 59, the one or more photoinitiators include a first photoinitiator and a second photoinitiator; The first photoinitiator has a first absorption band and the second photoinitiator is substantially away from the first absorption band. a second absorption band distant from The first photoinitiator is sensitive to oxygen inhibition and the second photoinitiator is resistant to oxygen inhibition. Not susceptible to Binder material.
64. 64. The binder material of claim 63, wherein the at least one reactive monomer is a first reactive monomer that is specifically polymerized by the first photoinitiator and a second reactive monomer that is specifically polymerized by the second photoinitiator; and a second reactive monomer that is specifically polymerized by the polymerization of said monomer.
65. 64. The binder material of claim 63, wherein the at least one reactive monomer is A polymer having a functional group that can be polymerized by either the first photoinitiator or the second photoinitiator. A binder material comprising a hybrid monomer.
66. 1. A binder material for use in the manufacture of 3D objects, comprising: one or more reactive monomers; One or more photoinitiators having It is solid at storage temperatures below 35° C. and converts to a liquid state at operating temperatures above 35° C.; configured to be mixed with a powder material to produce a composite part; Binder material.
67. 67. The binder material of claim 66, wherein at least one of the one or more reactive monomers at least one of the binder materials is norbornene or a norbornene derivative.
68. 67. The binder material of claim 66, wherein at least one of the one or more reactive monomers At least one binder material is a functionalized derivative of cyanuric acid.
69. 67. A binder material according to claim 66, comprising a binder material adapted to modify the mechanical properties of the binder material. The binder material includes a non-reactive diluent configured as follows:
70. 70. The binder material of claim 69, wherein the non-reactive diluent is a plasticizer. material.
71. 70. The binder material of claim 69, wherein the non-reactive diluent has a storage temperature of less than 35°C. A binder material that is solid at room temperature and liquid at operating temperatures above 35°C.
72. 72. The binder material of claim 71, wherein the diluent is a wax.
73. 72. The binder material of claim 71, wherein the diluent has an average molecular weight greater than 1000. The binder material is polyethylene glycol having a molecular weight of 1.5 to 1.
5.
74. 72. The binder material of claim 71, wherein the diluent has an average molecular weight greater than 1000. The binder material is polypropylene glycol having a molecular weight of 1.5 to 1.
5.
75. 1. A method for producing a powder composite component, comprising the steps of: depositing a mixture of binder material and powder material onto a build surface; Selectively irradiating the binder material with a resolution finer than the nominal size of the powder material. bonding the powder materials together to form the powder composite part; and The powder composite member is then removed so as to remove the portion of the powder material protruding from the surface of the powder composite member. treating the composite material; The method according to claim 1,
76. 76. The method of claim 75, wherein the step of treating the powder composite component comprises electrochemical treatment. A method comprising the step of applying.
77. 77. The method of claim 76, wherein the step of applying an electrochemical treatment is performed at a rate of more than 10 cps. applying an electrolyte having a viscosity of
78. 77. The method of claim 76, wherein the step of applying an electrochemical treatment is more than 50 cps. applying an electrolyte having a viscosity of
79. 77. The method of claim 76, wherein the step of applying an electrochemical treatment comprises applying a pressure of 100 cps. The method includes applying a highly viscous electrolyte.
80. 77. The method of claim 76, wherein the step of applying an electrochemical treatment comprises applying a 500 cps The method includes applying a highly viscous electrolyte.
81. 77. The method of claim 76, wherein the step of applying an electrochemical treatment comprises applying a s。 Applying an electrolyte having a viscosity of greater than s.
82. 1. A method for producing a powder composite component, comprising the steps of: delivering a mixture of binder material and powder material to a build surface; Selectively irradiating the binder material to bond the powder materials together to form the powder composite. generating a component; producing a support structure configured to support at least a portion of the powder composite material; Floor and At least the contact surface of the support structure is treated to prevent bonding with the powder composite member. and Sintering the powder composite to fuse with the powder material and remove the binder material. step, The method according to claim 1,
83. 83. The method of claim 82, wherein the step of treating the contact surface of the support structure comprises: The method comprises the step of oxidizing the contact surface.
84. 83. The method of claim 82, further comprising the step of simultaneously producing a plurality of powder composite components. Has The step of fabricating a support structure may include providing support for all of the plurality of powder composite members during sintering. manufacturing a unitary support structure configured to method.
85. 83. The method of claim 82, further comprising the step of simultaneously producing a plurality of powder composite components. Has The step of fabricating the support structure may further comprise the step of: and two or more support structures adapted to support the plurality of powder composite members during sintering. manufacturing method.
86. 83. The method of claim 82, wherein the support structure is manufactured integrally with the powder composite component. How to do it.
87. 1. A method for producing a powder composite component, comprising the steps of: combining a powder material with a binder material to produce a powder composite component; The powder composite is processed in a vacuum chamber to reduce the temperature of the powder composite. At least one of the binder materials is heated to a temperature above the glass transition temperature of the composite material. removing a portion thereof; heat treating the powder composite to sinter the powder materials together; The method according to claim 1,
88. 88. The method of claim 87, wherein the binder material is a binder having a melting point less than the melting point of the other components of the binder material. The method of claim 1, further comprising the step of:
89. 88. The method of claim 87, wherein the binder material is formed by decomposition of other components of the binder material. a wax having a boiling point below the temperature.
90. A method of manufacturing a component, comprising the steps of: A powder material is bonded to a binder material including at least a first polymerizable component and a second polymerizable component. combining the layers to produce one or more layers of material; The one or more layers of material are selectively irradiated to polymerize the first polymerizable component to form layers forming a precursor member by bonding together at least a portion of the heat treating the precursor member to polymerize the second polymerizable component; The method according to claim 1,
91. 91. The method of claim 90, further comprising removing the precursor member from the precursor member by treatment with a solvent.
1. The method comprising removing the polymerizable component.
92. 92. The method of claim 91, further comprising removing the second polymerizable component by heat treatment. A method having a floor.
Citation Information
Patent Citations
Use of thermoset polymer powder composition
JP2018529555A
Additive manufacturing method and apparatus
JP2018532613A