Light emitting device

By employing a layered structure with strategically aligned triplet excited state energy levels and a separation layer, the luminous efficiency of organic electroluminescent devices is enhanced, addressing the inefficiencies in existing technologies and enabling high-efficiency white light emission.

JP2024167384AInactive Publication Date: 2024-12-03SEMICON ENERGY LAB CO LTD
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
JP2024151982
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2014-11-28
Filing Date
2024-09-04
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing organic electroluminescent devices face challenges in achieving high luminous efficiency due to limitations in the energy transfer processes between host and luminescent materials, particularly with fluorescent materials where triplet excited states are not effectively utilized.

Method used

The introduction of a layered structure with overlapping light-emitting layers, each containing specific host and luminescent materials, where the triplet excited state energy levels are strategically aligned to enhance energy transfer, including the use of fluorescent and phosphorescent materials, and an optional separation layer to prevent triplet energy transfer.

Benefits of technology

This configuration results in a highly efficient light-emitting device with improved luminous efficiency, capable of emitting white light with high color rendering properties and maintaining reliability under various operational conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024167384000001_ABST
    Figure 2024167384000001_ABST
Patent Text Reader

Abstract

To increase the light emission efficiency of a light-emitting element.SOLUTION: A light-emitting element is provided, which comprises a first electrode, a second electrode over the first electrode, and a first luminescent layer and a second luminescent layer which are provided between the first and second electrodes. The first luminescent layer and the second luminescent layer have regions overlapping with each other. The first luminescent layer has a first host material and a first luminescent material. The second luminescent layer has a second host material and a second luminescent material. The first luminescent material is a fluorescent material. The second luminescent material is a phosphorescent material. The lowest level (T1 level) of a triplet excited state of the first luminescent material is higher than T1 level of the first host material. A light emitting device, a unit of electronic equipment and a light-emitting device, each comprising the light-emitting element are provided.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention is a light-emitting element, a light-emitting device having a light-emitting element, a display device, an electronic device, and The present invention also relates to a semiconductor device having a light-emitting element and a lighting device. Apparatus and methods for manufacturing the same are included. [Background technology]

[0002] A light-emitting element having a layer containing an organic compound between a pair of electrodes, and a light-emitting device including the light-emitting element These are called organic electroluminescent elements and organic electroluminescent devices, respectively. The present invention can be applied to lighting devices and the like (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] US Patent Application Publication No. 2012 / 0205632 Summary of the Invention [Problem to be solved by the invention]

[0004] One object of one embodiment of the present invention is to improve the emission efficiency of a light-emitting element. One object of one embodiment of the present invention is to provide a light-emitting device or a semiconductor device including the light-emitting device. The description of these issues does not preclude the existence of other issues. An embodiment of the invention does not necessarily have to solve all of these problems. Other problems will be obvious from the description, drawings, claims, etc. It is possible to extract other issues from the detailed description, drawings, claims, etc. [Means for solving the problem]

[0005] One aspect of the present invention is a semiconductor device comprising a first electrode, a second electrode on the first electrode, and a first emitter. The light-emitting device has a first light-emitting layer and a second light-emitting layer. The first electrode and the second electrode are provided between each other, and have an overlapping area. The first light-emitting layer has a first host material and a first light-emitting material, and the second light-emitting layer has a second host material. The first light-emitting material is a fluorescent material and the second light-emitting material is a The light-emitting material is a phosphorescent material. The lowest triplet excited state level (T1 level) of the first light-emitting material is The T1 level is higher than the T1 level of the first host material.

[0006] Another aspect of the present invention is a semiconductor device comprising a first electrode, a second electrode on the first electrode, and a first The light-emitting element has a first light-emitting unit and a second light-emitting unit. and the second light-emitting unit are both disposed between the first electrode and the second electrode, and The first light-emitting unit and the second light-emitting unit have an overlapping region. An intermediate layer is provided between the first light-emitting unit and the second light-emitting unit. The first light-emitting unit includes a first light-emitting layer and a second light-emitting layer that overlap each other. The second light-emitting unit has a third light-emitting layer. The first light-emitting layer has a first host. The second light-emitting layer has a second host material and a first light-emitting material, and the second light-emitting layer has a second host material and a second light-emitting material. The third light-emitting layer has a third host material and a third light-emitting material. The light emitting material is a fluorescent material, the second light emitting material is a phosphorescent material, and the third light emitting material is The T1 level of the first light-emitting material is one of a fluorescent material and a phosphorescent material. higher than the T1 level of the first host material.

[0007] In this specification and claims, the term "fluorescent material" refers to a material that emits light at the lowest level of a singlet excited state ( A material that emits light in the visible light range when it relaxes from the S1 level to the ground state. This refers to a material that emits light in the visible light region at room temperature when relaxing from the T1 level to the ground state. In other words, a phosphorescent material is a material that can convert triplet excitation energy into visible light. be.

[0008] In each of the first light-emitting layer, the second light-emitting layer, and the third light-emitting layer, The second host material and the third host material are present in the greatest amounts by weight.

[0009] The second host material preferably has a higher T1 level than the first host material.

[0010] The first light-emitting layer and the second light-emitting layer may have a region where they are in contact with each other.

[0011] The first light-emitting layer and the second light-emitting layer may be separated from each other. In that case, a hole transport A layer having a mixture of a polarizing material and an electron transporting material, or a layer having a bipolar material, is provided between the polarizing material and the electron transporting material. One of the hole transporting material and the electron transporting material may be the second The bipolar material may be the same as the second host material. stomach.

[0012] The second light-emitting layer may be provided on the first light-emitting layer, and the first light-emitting layer may be disposed on the second light-emitting layer. It may be provided on the top.

[0013] The second light-emitting unit may be disposed on the first light-emitting unit, and the first light-emitting unit The light emitting unit may be provided on the second light emitting unit.

[0014] One embodiment of the present invention is a light-emitting element having a plurality of light-emitting elements having the above-described structures, It is a light emitting device.

[0015] One embodiment of the present invention is an electronic device including a light-emitting device having any of the above structures.

[0016] One embodiment of the present invention is a lighting device including a light-emitting device having any of the above structures and a housing or a support. It is.

[0017] In this specification and claims, the term "light emitting device" refers to an image display device or an image Refers to the light source used in display devices. Also, when a connector, such as FPC (F flexible printed circuit), TCP (Tape Carrier) A module with a printed wiring board attached to the end of the TCP. The COG (Chip On Glass) method is used for the installed module or light emitting device. Furthermore, any module on which an IC (integrated circuit) is directly mounted is also included in the light emitting device. Effect of the Invention

[0018] According to one embodiment of the present invention, a highly efficient light-emitting element, light-emitting device, electronic device, or lighting device is provided. The description of these effects does not preclude the existence of other effects. Note that one embodiment of the present invention does not necessarily have all of these effects. Effects other than those mentioned above will become apparent from the description, drawings, claims, etc. It is possible to extract other effects from the description, drawings, claims, etc. It is. [Brief description of the drawings]

[0019] [Figure 1] 1 illustrates a configuration example of a light-emitting element according to one embodiment of the present invention. [Diagram 2] 1 shows a light-emitting mechanism of a light-emitting element according to one embodiment of the present invention. [Diagram 3] 1 illustrates a configuration example of a light-emitting element according to one embodiment of the present invention. [Figure 4] 1 illustrates a configuration example of a light-emitting device according to one embodiment of the present invention. [Diagram 5] 1 illustrates a configuration example of a light-emitting device according to one embodiment of the present invention. [Figure 6] 1 shows an example of an electronic device according to an embodiment of the present invention. [Figure 7] 1 shows an example of an electronic device according to an embodiment of the present invention. [Figure 8] 1 shows an example of a lighting device according to one embodiment of the present invention. [Figure 9] 1A and 1B are schematic diagrams of a light-emitting element 1 and a light-emitting element 2 in Examples 1 and 2. [Figure 10] 3 shows a voltage-luminance curve of the light-emitting element 1 in Example 1. [Figure 11] 3 shows a luminance-current efficiency curve and a luminance-external quantum efficiency curve of the light-emitting element 1 in Example 1. [Figure 12] 3 shows a luminance-power efficiency curve of the light-emitting element 1 in Example 1. [Figure 13] 3 shows an electroluminescence spectrum of the light-emitting element 1 in Example 1. [Figure 14] 11 is a voltage-luminance curve of the light-emitting element 2 in Example 2. [Figure 15] 11 shows a luminance-current efficiency curve and a luminance-external quantum efficiency curve of the light-emitting element 2 in Example 2. [Figure 16] 10 shows a luminance-power efficiency curve of the light-emitting element 2 in Example 2. [Figure 17] 4 shows an electroluminescence spectrum of the light-emitting element 2 in Example 2. [Figure 18] 1A to 1C are schematic views of light-emitting elements 3 to 6 in Reference Example 1. [Figure 19] 1 shows luminance-current efficiency curves of light-emitting elements 3 to 6 in Reference Example 1. [Figure 20] 1 shows voltage-luminance curves of light-emitting elements 3 to 6 in Reference Example 1. [Figure 21] 1 shows luminance vs. external quantum efficiency curves of the light-emitting elements 3 to 6 in Reference Example 1. [Figure 22] 1 shows electroluminescence spectra of light-emitting elements 3 to 6 in Reference Example 1. [Figure 23] 1 shows reliability test results of light-emitting elements 3 to 6 in Reference Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] Hereinafter, the embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the above description, and may be modified in various forms and without departing from the spirit and scope of the present invention. The details can be changed in various ways. Therefore, the present invention is limited to the following embodiments. It should not be construed as being limited to the contents listed.

[0021] (Embodiment 1) 1. Example of light-emitting element configuration A structural example of a light-emitting element according to one embodiment of the present invention will be described with reference to FIG. The element includes a first electrode 100, a second electrode 102, and a first light-emitting element disposed between them. The first light-emitting layer 120 and the second light-emitting layer 122 are In the following description, the first electrode 100 is an anode and the second electrode 102 is a cathode. .

[0022] 1-1. Electrode The first electrode 100 and the second electrode 102 are connected to the first light-emitting layer 120 and the second light-emitting layer 122. They have the function of injecting holes and electrons, respectively. These electrodes are made of metals, alloys, and conductive compounds. The metal can be aluminum, or a mixture or laminate of these metals. Typical examples are aluminum (Al) and silver (Ag), as well as tungsten, chromium, molybdenum, etc. transition metals such as tin, copper, and titanium; alkali metals such as lithium (Li) and cesium; Group 2 metals such as calcium and magnesium (Mg) can be used. As the alloy, an alloy containing the above metals can be used. Examples of conductive compounds include indium oxide, for example, MgAg, AlLi, etc. - Metal oxides such as indium tin oxide. As the reactive compound, an inorganic carbon-based material such as graphene may be used. By stacking a plurality of these materials, the first electrode 100 or the second electrode 102, Alternatively, both may be formed.

[0023] The light emitted from the first light-emitting layer 120 and the second light-emitting layer 122 is The electric field is then extracted through the first electrode 102, the second electrode 102, or both of these electrodes. At least one of them transmits visible light. The electrode that extracts the light is made of a light-transmitting material such as a metal or alloy. When a material with a low optical transmittance is used, the first electrode 100 or The first electrode 102 or a part of the first electrode 102 may be formed. The film is formed to a thickness of 10 nm or more.

[0024] 1-2. First light-emitting layer The first light-emitting layer 120 includes a first host material and a first light-emitting material, the first light-emitting material being a phosphor. In the first light-emitting layer 120, the first host material is present in the largest amount by weight. The first light-emitting material is dispersed in the first host material. The T1 level of the first light-emitting material is The S1 level of the first host material is higher than the S It is preferable that the level is higher than level 1. The light emitting mechanism of the first light emitting layer 120 will be described later.

[0025] The first host material is preferably an anthracene derivative or a tetracene derivative. These derivatives have high S1 levels and low T1 levels. Nyl-3-[4-(10-phenyl-9-anthryl)phenyl]-9H-carbazole (PCzPA), 3-[4-(1-naphthyl)-phenyl]-9-phenyl-9H-carbazone Pazol (PCPN), 9-[4-(10-phenyl-9-anthracenyl)phenyl] -9H-Carbazole (CzPA), 7-[4-(10-phenyl-9-anthryl)phenyl] phenyl]-7H-dibenzo[c,g]carbazole (cgDBCzPA), 6-[3-( 9,10-diphenyl-2-anthryl)phenyl]-benzo[b]naphtho[1,2-d ]furan (2mBnfPPA), 9-phenyl-10-{4-(9-phenyl-9H-furan {fluorophenyl-9-yl}biphenyl-4'-yl}anthracene (FLPPA) Alternatively, 5,12-diphenyltetracene, 5,12-bis(biphenyl-2 -yl)tetracene and the like.

[0026] The first light-emitting material may be a pyrene derivative, an anthracene derivative, or a triphenylene derivative. , fluorene derivatives, carbazole derivatives, dibenzothiophene derivatives, dibenzofuran Derivatives, dibenzoquinoxaline derivatives, quinoxaline derivatives, pyridine derivatives, pyrimidin Examples include pyrene derivatives, phenanthrene derivatives, and naphthalene derivatives. The pyrene derivative is preferably used because it has a high luminescence quantum yield. (3-methylphenyl)-N,N'-bis[3-(9-phenyl-9H-fluorene-9 -yl)phenyl]pyrene-1,6-diamine (1,6mMemFLPAPrn), N, N'-Bis[4-(9-phenyl-9H-fluoren-9-yl)phenyl]-N,N' -Diphenylpyrene-1,6-diamine (1,6FLPAPrn), N,N'-bis(di Benzofuran-2-yl)-N,N'-diphenylpyrene-1,6-diamine (1,6F rAPrn), N,N'-bis(dibenzothiophen-2-yl)-N,N'-diphenyl Examples include ruthenium-1,6-diamine (1,6ThAPrn).

[0027] 1-3. Second light-emitting layer The second light-emitting layer 122 includes a second host material and a second light-emitting material, the second light-emitting material being phosphorus. In the second light-emitting layer 122, the second host material is present in the largest amount by weight. The second light-emitting material is dispersed in the second host material. The T1 level of the second host material is It is preferable that the T1 level of the second light-emitting material is higher than that of the first light-emitting material.

[0028] The second luminescent material may be an organometallic complex of iridium, rhodium, or platinum. In particular, organic iridium complexes, such as iridium ortho-metal complexes, The orthometalating ligands are preferably 4H-triazole ligands, 1H -Triazole ligand, imidazole ligand, pyridine ligand, pyrimidine ligand, pyra The metal complexes include porphyrin ligands and isoquinoline ligands. and platinum complexes having a fluorine ligand.

[0029] As the second host material, zinc and aluminum-based metal complexes as well as oxadiazole derivatives are used. Conductors, triazole derivatives, benzimidazole derivatives, quinoxaline derivatives, dibenzo Quinoxaline derivatives, dibenzothiophene derivatives, dibenzofuran derivatives, pyrimidine derivatives Conductors, triazine derivatives, pyridine derivatives, bipyridine derivatives, phenanthroline derivatives Other examples include aromatic amines and carbazole derivatives. do.

[0030] The second light-emitting layer 122 contains a second host material and an exciplex (i.e., a hetero The compound may further contain an additive capable of forming an excimer. The emission peak of the first emitting material is the triplet MLCT (Metal to Ligand) of the second emitting material. d Charge Transfer) transition absorption band, more specifically, the longest wavelength side Selecting the second host material, the additive, and the second emissive material to overlap the absorption bands. This makes it possible to provide a light-emitting element with dramatically improved luminous efficiency.

[0031] There is no limitation on the emission colors of the first and second light-emitting materials, and they may be the same or different. The light emitted from each is mixed and taken out of the device, so for example, When the colors are complementary to each other, the light emitting elements can provide white light. In consideration of reliability, the emission peak wavelength of the first luminescent material is shorter than that of the second luminescent material. For example, it is preferable that the first light-emitting material emits blue light and the second light-emitting material emits green and yellow light. Alternatively, it is preferable that the light emitted is red.

[0032] The second light-emitting layer 122 may have a structure in which multiple layers are laminated. Different structures and materials may be used in several layers.

[0033] The first light-emitting layer 120 and the second light-emitting layer 122 are formed by deposition (including vacuum deposition). The insulating layer 11 can be formed by a method such as an ink jet method, a coating method, or a gravure printing method.

[0034] 1-4. Other layers As shown in FIG. 1A, a light-emitting element according to one embodiment of the present invention includes the first light-emitting layer 120 and The second light-emitting layer 122 may have layers other than the second light-emitting layer 122. For example, a hole injection layer, a hole transport layer, an electrode The layer may include a electron blocking layer, a hole blocking layer, an electron transport layer, an electron injection layer, etc. Each of the layers may be formed of multiple layers. These layers reduce the carrier injection barrier. It is possible to improve the carrier transport property or suppress the quenching phenomenon caused by the electrode, and thus the luminescence This contributes to improving efficiency and reducing driving voltage. In addition to the optical layer 122, a hole injection layer 124, a hole transport layer 126, an electron transport layer 128, and an electron injection layer In the present specification and claims, the first electrode The entire layer between the first electrode 100 and the second electrode 102 is defined as an EL layer. In FIG. 1(A), a hole injection layer 124, a hole transport layer 126, a first light-emitting layer 120, a second light-emitting layer 122, and a The stack including layer 122, electron transport layer 128, and electron injection layer 130 is the EL layer.

[0035] 1-4-1. Hole injection layer The hole injection layer 124 reduces the hole injection barrier from the first electrode 100, thereby It has a function of promoting injection, and is, for example, a transition metal oxide, a phthalocyanine derivative, or an aromatic It is formed from aromatic amines, etc. Transition metal oxides include molybdenum oxide and vanadium oxide. Examples of the oxides include zinc oxide, ruthenium oxide, tungsten oxide, and manganese oxide. Phthalocyanine derivatives include phthalocyanine and metal phthalocyanine. Examples of aromatic amines include benzidine derivatives and phenylenediamine derivatives. Polymer compounds such as polythiophene and polyaniline can also be used. Poly(ethylenedioxythiophene) / poly(styrene)-coated polythiophenes Sulfonic acid) is a typical example.

[0036] The hole injection layer 124 is formed by mixing a hole transporting material and a material that has an electron accepting property. Alternatively, a layer including a material exhibiting electron accepting properties and a layer including a material exhibiting hole transporting properties may be used. A stack of layers containing these materials may be used. Materials that exhibit electron-accepting properties include quinodimethane derivatives and Examples of organic acceptors include chloranil derivatives and hexaazatriphenylene derivatives. Specifically, 7,7,8,8-tetracyano-2,3,5,6-tetrafluoro Oroquinodimethane (abbreviation: F4-TCNQ), chloranil, 2,3,6,7,10,11 -Hexacyano-1,4,5,8,9,12-hexaazatriphenylene (abbreviation: HAT -CN) and other electron-withdrawing groups (halogen groups and cyano groups). Oxides, for example oxides of metals in Groups 4 to 8, can be used. Vanadium oxide, niobium oxide, tantalum oxide, chromium oxide, molybdenum oxide, tungsten oxide Among them, molybdenum oxide is stable in the air and It is preferred because it has low hygroscopicity and is easy to handle.

[0037] As the hole transporting material, a material having a higher hole transporting property than an electron transporting property can be used. ×10 -6 cm 2 It is preferable that the material has a hole mobility of 1 / Vs or more. The compounds are made using aromatic amines, carbazole derivatives, aromatic hydrocarbons, stilbene derivatives, etc. The hole transporting material may be a polymer compound.

[0038] 1-4-2. Hole transport layer The hole transport layer 126 is a layer containing a hole transporting material. The hole transport layer 126 can be formed by injecting the hole into the hole injection layer 124. Since it has the function of transporting holes to the first light-emitting layer 120, the highest occupied track of the hole injection layer 124 Road(HOMO:Highest Occupied Molecular Orbita l) It is preferred that the HOMO level is the same as or close to the HOMO level.

[0039] 1-4-3. Electron injection layer The electron injection layer 130 reduces the barrier for electron injection from the second electrode 102, thereby improving electron injection. For example, Group 1 metals, Group 2 metals, or their oxides, halides, etc. In addition, electron transport materials (described later) and their corresponding A mixed layer of materials exhibiting electron donating properties may also be used. The metals include Group 1 metals, Group 2 metals, and oxides thereof.

[0040] 1-4-4. Electron transport layer The electron transport layer 128 transports electrons injected from the second electrode 102 through the electron injection layer 130. The electron transporting material has a function of transporting electrons rather than holes to the second light-emitting layer 122. Materials with high transport properties of 1×10 -6 cm 2 / Vs or higher electron mobility Specifically, it is preferable that the material has a quinoline ligand or a benzoquinoline ligand. , metal complexes having oxazole or thiazole ligands, oxadiazole Derivatives, triazole derivatives, phenanthroline derivatives, pyridine derivatives, bipyridine derivatives Conductors and the like.

[0041] The hole injection layer 124, the hole transport layer 126, the electron injection layer 130, and the electron transport layer 126 are The transfer layer 128 can be formed by a deposition method (including a vacuum deposition method), an inkjet method, a coating method, a graphite method, or the like. The vias can be formed by a method such as via printing.

[0042] In addition, the hole injection layer 124, the hole transport layer 126, the electron injection layer 130, and the electron transport layer 12 In addition to the above-mentioned materials, 8 also includes inorganic compounds or polymer compounds (oligomers, dendrimers, etc.) , polymers, etc.) may also be used.

[0043] 2. Other configuration examples of light-emitting elements In the light-emitting element shown in FIG. 1(A), the second light-emitting layer 122 is provided on the first light-emitting layer 120. However, one embodiment of the present invention is not limited to this structure. The first light-emitting layer 120 may be located above the second light-emitting layer 122 .

[0044] 3. Light Emitting Mechanism of the First Light Emitting Layer 120 The correlation between the energy levels of the first host material and the first light-emitting material is shown in FIG. The symbols are as follows: S 0(h) : Ground state level of the first host material S 0(g) : Ground state level of the first light-emitting material S 1(h) : The lowest level of the singlet excited state of the first host material S 1(g) : The lowest level of the singlet excited state of the first light-emitting material T 1(h) : the lowest triplet excited state level of the first host material T 1(g) : The lowest triplet excited state level of the first light-emitting material

[0045] As described above, the first light-emitting layer 120 is made of a first host material and a luminescent layer having a higher T1 level than the first host material. Therefore, T 1(g) is T 1(h) Also, the first In the light-emitting layer 120, the first host material is present in a large amount compared to the first light-emitting material. In FIG. 2, the energy levels of two molecules of the first host material and one molecule of the first emitting material are shown. is.

[0046] Carrier recombination creates excited states in the first light-emitting layer 120. Since the first host material is present in a large amount compared to the first host material, the excited state is almost entirely in the first host material. Here, the singlet excited state and the triplet excited state that arise from carrier recombination are The ratio of the doublet excited states (hereinafter, the exciton generation probability) is about 1:3. That is, S 1(h) of The singlet excited state has a temperature of about 1, T 1(h) The triplet excited state with do.

[0047] S 1(g) S 1(h) When the first host material is in a singlet excited state, the first Energy is rapidly transferred to the luminescent material (singlet energy transfer, process (a)) to form the first A singlet excited state of the luminescent material is generated, which relaxes to the ground state by a radiative process (process (b )) to obtain light emission. 1(h) T 1(g) than When the triplet excited state of the first host material is high, the energy is rapidly transferred to the first light-emitting material. A transfer (triplet energy transfer) occurs and a triplet excited state of the first emissive material is formed. However, since the first light-emitting material is a fluorescent material, the triplet excited state emits light in the visible light region. Therefore, the triplet excited state of the first host material can be utilized for light emission. Therefore, T 1(h) T 1(g) When the temperature is higher than 1000 K, only the emission by process (a) occurs. As a result, only about 25% of the injected carriers are released. It cannot be used for light.

[0048] On the other hand, as shown in FIG. 2, in the light-emitting element of one embodiment of the present invention, T 1(g) is T 1(h) twist Therefore, the triplet energy transfer from the first host material to the first emitting material (process (c)) does not occur or is negligible. In this case, the three The singlet state can decay to the ground state by a non-radiative process (process (d)) or by a triplet-triplet decay (process (c)). Triplet-Triplet Annihilation (TTA) The processes of generating the singlet excited state of the first host material compete with each other. From the singlet excited state of the first host material, the lower level S 1(g) Hey! Since energy transfer (process (e)) occurs, the first light-emitting material is given a singlet excited state. can be done.

[0049] That is, in the first light-emitting layer 120, (1) the first (a) Energy transfer process from the singlet excited state of the host material, and (2) TTA (e) an energy transfer process from the singlet excited state of the first host material generated by the The singlet excited state of the first light-emitting material is formed through two processes. 1(g) T 1(h) If the temperature is lower than , only the former process can be used, The efficiency of a light-emitting device is governed by the probability of exciton generation. Like T 1(g) T 1(h) If the temperature is higher than Therefore, it is possible to obtain a luminous efficiency exceeding the exciton generation probability, thereby providing a highly efficient light-emitting device. It is possible.

[0050] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0051] (Embodiment 2) In this embodiment, a light-emitting element which is one embodiment of the present invention will be described with reference to FIG. The light emitting device of the present embodiment has a separation layer between the first light emitting layer 120 and the second light emitting layer 122. The light-emitting element of the present embodiment differs from that of the first embodiment in that it has a separation layer 135. The separation layer 135 is a first light-emitting The layer 120 and the second light-emitting layer 122 are in contact with each other. The structure of the other layers is the same as that of the first embodiment. Therefore, the description will be omitted.

[0052] The separation layer 135 is a layer that absorbs the excited state of the second host material and the second emissive state generated in the second emitting layer 122. to the first host material or the first light-emitting material in the first light-emitting layer 120. It is designed to prevent energy transfer (especially triplet energy transfer) by the Dexter mechanism. Therefore, the separation layer only needs to be a few nm thick. 20 nm or less, or 1 nm to 10 nm, or 1 nm to 5 nm .

[0053] The separation layer 135 may be made of a single material, but may be made of a hole transport material and an electron transport material. If it is made of a single material, a bipolar material may be used. Here, the bipolar material is a material in which the ratio of the mobility of electrons to the mobility of holes is 100 or less. The material contained in the separation layer 135 may be any of the hole transporting materials exemplified in Embodiment 1 and Alternatively, the material contained in the separation layer 135 may be an electron transporting material. Alternatively, at least one of them may be formed of the same material as the second host material. This makes it easier to fabricate the light-emitting element and reduces the driving voltage.

[0054] Alternatively, the materials contained in the separation layer 135, or at least one of them, may be a second The T1 level may be higher than that of the host material.

[0055] By adjusting the mixing ratio of the hole transport material and the electron transport material in the separation layer 135, The binding area can be adjusted, which allows control of the color of emitted light. For example, When the first electrode 100 and the second electrode 102 are an anode and a cathode, respectively, the separation layer 135 By increasing the proportion of the hole transport material, the recombination region is expanded from the first electrode 100 side to the second electrode 1 02 side. This allows the contribution of light emitted from the second light-emitting layer 122 to be Conversely, by increasing the proportion of the electron transporting material in the separation layer 135, the re- The coupling region can be shifted from the second electrode 102 side to the first electrode 100 side, and the first The contribution of light emitted from the light-emitting layer 120 can be increased. When the color of light emitted from the light-emitting layer 122 is different, the recombination region can be adjusted to change the color of the light-emitting element as a whole. The emission color can be changed.

[0056] The hole transport material and the electron transport material form exciplexes in the separation layer 135. This can effectively prevent the diffusion of excitons. The excited state of the host material or the excited state of the second light-emitting material is converted into the excited state of the first host material or can prevent energy transfer to the first light-emitting material.

[0057] As in the light-emitting element shown in the first embodiment, as shown in FIG. may be located on the second light-emitting layer 122. In this case, the second light-emitting layer may be located on the hole-transporting layer 126. An optical layer 122 is provided, and a first light-emitting layer 120 is provided thereon via a separation layer 135. .

[0058] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0059] (Embodiment 3) In this embodiment, a light-emitting element which is one embodiment of the present invention will be described with reference to FIG. do.

[0060] 1. Example of light-emitting element configuration The light-emitting element shown in this embodiment has a first electrode 100, a second electrode 101, and a The electrode 102, the first light-emitting unit 140-1 and the second light-emitting The first light-emitting unit 140-1 and the second light-emitting unit 14 0-2 are overlapped with each other, and an intermediate layer 150 is provided between them. In the following description, the first electrode 100 is an anode and the second electrode 102 is a cathode. The components having the same reference numerals or names as those in the first and second embodiments, such as 102, are the same as those in the first and second embodiments. Since this is similar to that of forms 1 and 2, detailed explanation will be omitted.

[0061] 1-1. First light-emitting unit The first light-emitting unit 140-1 has a first light-emitting layer 120 and a second light-emitting layer 122. The structures and materials of these layers are the same as those shown in the first embodiment. In the light-emitting device shown in FIG. 1, a second light-emitting layer 122 is disposed on a first light-emitting layer 120. However, the first light-emitting layer 120 may be provided on the second light-emitting layer 122. As shown in FIG. 1, a hole injection layer 124, a hole transport layer 126-1, and an electron transport layer 128-1 are provided. As these layers, the hole injection layer 124 and the hole transport layer 125 shown in the first embodiment may be used. The same material as the electron transport layer 126 and the electron transport layer 128 can be used. As shown in the second embodiment, a separation layer 1 is provided between the first light-emitting layer 120 and the second light-emitting layer 122. 35 may be set.

[0062] 1-2. Middle class When a voltage is applied between the first electrode 100 and the second electrode 102, the intermediate layer 150 Electrons are injected into the first light-emitting unit 140-1 and holes are injected into the second light-emitting unit 140-2. It also has the ability to transmit visible light and has a transmittance of 40% or more. Here, the intermediate layer 150 is preferably composed of a first layer 150-1 and a second layer 150-2. The first layer 150-1 is provided on the first light-emitting unit 140-1 side, and the second layer 1 50-2 is provided on the side of the second light emitting unit 140-2.

[0063] The first layer 150-1 is made of, for example, a Group 1 metal, a Group 2 metal, or a compound thereof (such as an oxide). Alternatively, the compounds shown in the first embodiment may be used. It is also possible to use a mixed layer of an electron transporting material and a material that exhibits electron donating properties. do.

[0064] The second layer 150-2 may be a layer having the transition metal oxide shown in the first embodiment. Alternatively, a mixed layer of a hole transporting material and a material that exhibits electron accepting properties can be formed. Alternatively, a laminate of a layer containing a material exhibiting electron accepting properties and a layer containing a material having hole transporting properties can be used. Specifically, the mixture usable as the hole injection layer 124 shown in the first embodiment can be used. Interleaving or lamination may be used.

[0065] Although not shown, a buffer layer is provided between the first layer 150-1 and the second layer 150-2. This allows the first layer 150-1 and the second layer 150-2 to be made of the same material. The buffer layer is a layer containing an electron transport material. Examples of electron transporting materials include perylene derivatives and nitrogen-containing condensed aromatic compounds. Some examples include:

[0066] The intermediate layer 150 can be formed by a deposition method (including a vacuum deposition method), an inkjet method, a coating method, a gravure method, or the like. It can be formed by a method such as a printing method.

[0067] 1-3. Second light-emitting unit The second light-emitting unit 140-2 includes a third light-emitting layer 132. The third light-emitting layer 132 includes The third host material and the third light-emitting material are a fluorescent material or a phosphorescent material. In the third light-emitting layer 132, the third host material is present in the largest amount by weight, and the third The light-emitting material is dispersed in a third host material. The third host material is the same as that shown in the first embodiment. The same materials as the first host material and the second host material described above can be used. The third host material may be the same as or different from the first host material or the second host material. When a fluorescent material is used as the third emitting material, the S1 level of the third host material is It is preferable that the third light-emitting material has a higher light-emitting capacity than the phosphorescent material. In the case of using the third host material, the T1 level of the third light-emitting material is higher than that of the third light-emitting material. As the third light-emitting material, the first light-emitting material or the second light-emitting material shown in the embodiment mode 1 may be used. Materials similar to optical materials can be used.

[0068] The third luminescent material may be the same as the first luminescent material or the second luminescent material, or may be different. For example, a red luminescent material can be produced by using the first luminescent material, the second luminescent material, and the third luminescent material. By providing the three primary colors of light, blue, and green, it is possible to emit white light with high color rendering from the light emitting element. It can be taken out.

[0069] In the light-emitting device shown in FIG. 3A, the second light-emitting unit 140-2 further includes a hole-transporting The layer 126-2, the electron transport layer 128-2, and the electron injection layer 130 are also formed. The same as that shown in the first embodiment can be used.

[0070] In comparison with the light-emitting elements shown in the first and second embodiments, the driving voltage of the light-emitting element shown in this embodiment is Although the electromotive voltage increases, the current efficiency is doubled or more at the same current density. It is possible to obtain a highly efficient light emitting device.

[0071] 2. Other configuration examples of light-emitting elements The light-emitting element shown in FIG. 3A has a first light-emitting layer 120 and a second light-emitting layer 122. A light-emitting unit (first light-emitting unit 140-1) is formed on the first electrode 100 side. However, as shown in FIG. 3B, it may be formed on the second electrode 102 side. In this case, similarly to the second embodiment, a separation layer 13 is provided between the first light-emitting layer 120 and the second light-emitting layer 122. 5 may also be set.

[0072] Here, a light-emitting element having two light-emitting units will be described with reference to FIGS. 3(A) and 3(B). As shown in FIG. 3(C), n (n is an integer of 3 or more) light-emitting units (1 The light emitting device in which the layers 40-1 to 140-n are stacked is also included in the embodiments of the present invention. Intermediate layers (150(1) to 150(n-1)) are provided between adjacent light-emitting units. At least one of the n light-emitting units has the same configuration as the first light-emitting unit. It is sufficient that at least one of the light emitting units has a similar configuration to that of the second light emitting unit.

[0073] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0074] (Embodiment 4) In this embodiment, an active layer is used as an example of a light-emitting device including a light-emitting element of one embodiment of the present invention. A positive matrix type light emitting device will be described with reference to FIG. 4. FIG. 4(A) shows the top of a light emitting device. 4(B) is a cross-sectional view taken along line AA' of FIG. 4(A).

[0075] As shown in FIG. 4(A) and FIG. 4(B), the light emitting device has a source side driving circuit 40 on an element substrate 401. 3, a pixel portion 402, and gate side driving circuits 404a and 404b. 406 is a sealing substrate. Reference numeral 405 denotes a sealant, and the inside surrounded by the sealant 405 is a region 418. The child substrate 401 and the sealing substrate 406 may be made of glass or quartz substrate, or FRP (Fiberglass) substrate. Reinforced Plastics), PVF (Polyvinyl Fluoride), Poly A flexible substrate made of ester, acrylic, or the like can be used. It receives various signals from the FPC 408 and the source side driver circuit 403 and The FPC is connected to a printed wiring board (PW B) may be attached.

[0076] For the sake of simplicity, FIG. 4B shows a part of the source side driver circuit 403 and one of the pixel portions 402. As shown in FIG. 4B, the source side driver circuit 403 has an n-channel A CMOS circuit is formed by combining a p-channel transistor 409 and a p-channel transistor 410. A circuit is formed, but other circuits, such as a PMOS circuit or an NMOS circuit, are also formed. In addition, the source side driver circuit 403 and the gate side driver circuits 404a and 404b may be entirely Alternatively, a part of the transistor may be formed outside the substrate, not on the substrate. The staggered type may be used, or the inverted staggered type may be used. Examples include group 14 elements such as silicon and germanium, gallium arsenide and indium lithium. Materials that exhibit semiconducting properties, such as compounds such as tin oxide and zinc oxide, or oxides such as zinc oxide and tin oxide. As long as the material is an oxide that exhibits semiconductor properties (oxide semiconductor), The oxides are made of a composite of elements selected from indium, gallium, aluminum, zinc and tin. The semiconductor layer may be either crystalline or amorphous. Specific examples of the semiconductor include a single crystal semiconductor, a polycrystalline semiconductor, and a microcrystalline semiconductor. can be.

[0077] The pixel portion 402 includes a switching transistor 411 and a current control transistor 412. and a first electrode 413 electrically connected to a current control transistor 412. An insulator 414 is formed to cover the edge of the first electrode 413. There are.

[0078] The structure of the light-emitting element shown in the embodiment mode 1, 2, or 3 is applied to the opening of the insulator 414. That is, the light-emitting element 417 has a first electrode 413, an EL The EL layer 415 has at least a first emitting layer, and a second electrode 416. The light-emitting device includes a first light-emitting layer and a second light-emitting layer, and may further include a third light-emitting layer. A plurality of light emitting elements are formed in the pixel portion 402, and the light emitting elements described in the first to third embodiments are formed in a part of the pixel portion 402. Light-emitting elements having a different configuration from the light-emitting elements described above may be included.

[0079] The sealing substrate 406 and the element substrate 401 are bonded together by the sealing material 405. The light emitting element 417 is disposed in the region 418. The region 418 is filled with an inert gas, or a resin or a desiccant. The sealing material 405 is made of epoxy resin or glass frit. It is preferable to have

[0080] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0081] (Embodiment 5) In this embodiment, a passive element is used as an example of a light-emitting device having a light-emitting element of one embodiment of the present invention. The matrix type light emitting device will be described with reference to FIG. 5. FIG. 5(A) shows a light emitting device. FIG. 5(B) is a perspective view and an XY cross-sectional view of FIG. 5(A).

[0082] The light emitting device includes a substrate 551, a first electrode 552, a second electrode 556, and an EL layer 555. The EL layer 555 has the first light-emitting layer 120 and the second light-emitting layer 122 shown in the first, second, or third embodiment. The light-emitting layer 122 is formed of the first electrode 552. A part of the first electrode 552 is covered with an insulating layer 553. A partition layer 554 is provided on the layer 553. The partition layer 554 is spaced apart from the substrate 551. In other words, the cross section of the partition layer 554 in the short side direction is a trapezoid, and The bottom side in contact with the edge layer 553 is shorter than the top side. It can prevent child defects.

[0083] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0084] (Embodiment 6) In this embodiment, an electronic device including a light-emitting device having a light-emitting element according to one embodiment of the present invention will be described. An example will be described with reference to FIGS.

[0085] Examples of electronic devices include television sets, computers, and cameras (digital cameras). and digital video cameras), digital photo frames, mobile phones, personal digital assistants, games Examples of such electronic devices include music players, audio players, etc. Specific examples of these electronic devices are shown in Figure 6.

[0086] FIG. 6A shows an example of a television device. The television device 6100 has a housing A display unit 6103 is incorporated in the display unit 6101. The display unit 6103 is a display unit as described in the first and second embodiments. 3 or 3. A light emitting device including the light emitting element shown in FIG.

[0087] FIG. 6B shows an example of a computer. The computer includes a main body 6201 and a housing 6 202, display unit 6203, keyboard 6204, external connection port 6205, pointing The display unit 6203 includes a display device 6206 and the like. A light emitting device is provided that includes the light emitting element shown.

[0088] FIG. 6C shows an example of a smart watch. The smart watch includes a housing 6302. , a display panel 6304, operation buttons 6311, 6312, a connection terminal 6313, and a band 63 21, a clasp 6322, etc. The display panel 6304 has the display panel 6304 shown in FIG. The display panel 6304 is provided with a light-emitting device including the light-emitting element shown in FIG. It has a rectangular display area, and includes an icon 6305 representing the time and other icons 630 6, etc. can be displayed.

[0089] FIG. 6D shows an example of a mobile phone. A mobile phone 6400 is provided in a housing 6401. In addition to the built-in display unit 6402, operation buttons 6403, external connection port 6404, The display unit 6402 includes a speaker 6405, a microphone 6406, and the like. A light-emitting device including the light-emitting element shown in FIG. 2 or FIG. 3 is provided. The display portion 6402 is provided with a touch panel, and when the display portion 6402 is touched with a finger or the like, This allows the user to operate the mobile phone 6400 or input information to the mobile phone 6400. In addition, an image sensor may be mounted on the display portion 6402 to provide an imaging function.

[0090] FIG. 7 shows an example of a foldable tablet terminal. The tablet terminal includes a housing 730, a display unit 731a, and a display unit 731b. , a display mode changeover switch 734, a power switch 735, a power saving mode changeover switch The display unit 731a and the display unit 731b include a switch 736, a fastener 733, and an operation switch 738. One or both of 731b may include the light-emitting element shown in the first, second, or third embodiment. The tablet device can be folded in half, so the case can be folded when not in use. By closing the body 730, the display units 731a and 731b can be protected. .

[0091] The display unit 731a and the display unit 731b are partially or entirely configured as touch panel areas 732a and 732b. 32b, and the user can touch the displayed operation keys 737 and operation switches 739. Various operations such as data input may be performed using the above.

[0092] The display mode changeover switch 734 allows the user to change the display orientation between portrait and landscape. You can select between black and white and color display. The tablet device detects the amount of external light detected by the light sensor built into the device. The brightness of the display can be optimized.

[0093] FIG. 7A shows an example in which the display areas of the display units 731a and 731b are the same. The products may be different from each other and the display specifications may be different. For example, one may be It may be of higher resolution than the above.

[0094] FIG. 7B shows the tablet terminal in a closed state, with a solar cell 750 and a charge / discharge control circuit. A control circuit 752, a battery 754, a DC-DC converter 756, etc. are shown. Power can be supplied to the tablet terminal by a solar cell 750. 750 may be provided on one or both sides of the housing 730 .

[0095] As described above, an electronic device can be obtained by using a light-emitting device which is one embodiment of the present invention. The light-emitting device has a very wide range of applications and can be used in electronic devices in a wide range of fields. do.

[0096] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done.

[0097] (Embodiment 7) In this embodiment, a lighting device including a light-emitting device having a light-emitting element according to one embodiment of the present invention will be described. An example will be described with reference to FIG.

[0098] FIG. 8 shows a lighting device 801 installed on the ceiling, a lighting device 803 installed on a wall, and a lighting device 804 installed on a curved surface. 8 shows a lighting device 802 installed on a table or other furniture, and a lighting device 804 installed on a table or other furniture. The lighting device 801 includes a housing 821, a light-emitting device 811 installed in the housing 821, and The lighting device 802 also includes a support 822 and a light-emitting device 812 on the support 822. The lighting device 803 has a light-emitting device 813 installed on a wall surface. The light emitting device 804 includes a support 824 and a light emitting device 814 on the support 824. The light-emitting element shown in the first, second or third embodiment is applied to the light-emitting device of the lighting device. It is possible.

[0099] The structure described in this embodiment mode may be used in appropriate combination with structures described in other embodiments. This can be done. EXAMPLES

[0100] In this example, a manufacturing example of a light-emitting element according to one embodiment of the present invention will be described. A schematic diagram of the optical element (light-emitting element 1) is shown in Figure 9(A), details of the element structure are shown in Table 1, and the compounds used are shown in Table 1. The structures and abbreviations of the objects are shown below. [ka] [ka] [Table 1]

[0101] 1. Fabrication of Light-Emitting Device 1 Indium tin oxide (ITSO) with silicon oxide formed on a glass substrate m Tin SiO2Doped Oxide), film thickness 110nm, area 4mm 2 (2 A 1,3,5-tri(dibenzothiophene) film was placed on the first electrode 100. DBT3P-II and molybdenum oxide were mixed in a weight ratio of A hole injection layer 124 is formed by co-evaporating a mixture of 2:1 (II:MoO3) and a thickness of 30 nm. was formed.

[0102] On the hole injection layer 124, 3-[4-(9-phenanthryl)-phenyl]-9-phenyl -9H-carbazole (PCPPn) was evaporated to a thickness of 20 nm to form a hole transport layer. 126 was formed.

[0103] On the hole transport layer 126, 7-[4-(10-phenyl-9-anthryl)phenyl]-7 H-Dibenzo[c,g]carbazole (cgDBCzPA), 9-phenyl-3-[4- (10-phenyl-9-anthryl)phenyl]-9H-carbazole (PCzPA), and N,N'-bis(3-methylphenyl)-N,N'-bis[3-(9-phenyl- 9H-fluoren-9-yl)phenyl]pyrene-1,6-diamine (1,6mMemF LPAPrn) by weight ratio (cgDBCzPA:PCzPA:1,6mMemFLPAPr n) at 0.3:0.7:0.05 and a thickness of 20 nm to form a first light-emitting layer. 120 was formed.

[0104] On the first light-emitting layer 120, 2-[3′-(dibenzothiophen-4-yl)biphenyl- 3-yl]dibenzo[f,h]quinoxaline (2mDBTBPDBq-II), N-(1 ,1'-biphenyl-4-yl)-9,9-dimethyl-N-[4-(9-phenyl-9H -carbazol-3-yl)phenyl]-9H-fluoren-2-amine (PCBBiF ), and bis(2,3,5-triphenylpyrazine)(dipivaloylmethanate)yl Ir(tppr)2(dpm) was added in a weight ratio of 2mDBTBPDBq- II: PCBBiF:Ir(tppr)2(dpm)) 0.5:0.5:0.05, membrane The first layer 122(1) of the second light-emitting layer 122 is formed by co-evaporation to a thickness of 10 nm. Ta.

[0105] On top of this, 2mDBTBPDBq-II, PCBBiF, and bis[2-(6-tert-butyl) t-Butyl-4-pyrimidinyl-κN3)phenyl-κC](2,4-pentanedionate -κ 2 O,O') Iridium(III) (Ir(tBuppm)2(acac)) by weight Ratio(2mDBTBPDBq-II:PCBBiF:Ir(tBuppm)2(acac) ) in a ratio of 0.7:0.3:0.05 to a thickness of 20 nm to form a second light-emitting layer 1. A second layer 122(2) was formed.

[0106] On top of this, 2mDBTBPDBq-II and bathophenanthroline (Bphen) were added. The electron transport layer (128(1), 128(2)) was deposited in this order to have a thickness of 10 nm and 15 nm. 8(2)) was formed on the electron transport layer (128(1), 128(2)). LiF is evaporated to a thickness of 1 nm to form the electron injection layer 130, and then Al is evaporated. Aluminum (Al) was evaporated to a thickness of 200 nm to form the second electrode 102. The opposing glass substrate is fixed onto the glass substrate using a sealant in a nitrogen atmosphere to seal the device. Thus, the light-emitting element 1 was obtained.

[0107] 2. Characteristics of Light-Emitting Element 1 10 to 13 show the initial characteristics of the light-emitting element 1. As shown in FIG. Light emission begins at around 2.4V, and at 5.0V it reaches 8000cd / m 2 Shows brightness exceeding This shows that it can be driven at a low voltage. 2 In the current The efficiency and external quantum efficiency were 20.4cd / A and 10.7%, respectively (see Figure 11). The efficiency was 16.9lm / W (see Figure 12), which confirmed its high efficiency. The light-emitting element 1 includes a blue-emitting fluorescent material (1,6mMemFLPAPrn) as a first The red-emitting phosphorescent material (Ir(tppr)2(dpm)) is added to the light-emitting layer 120 of the first light-emitting layer. The first layer 122(1) of the 122 is a green light-emitting phosphorescent material (Ir(tBuppm)2(a cac)) is contained in the second layer 122(2) of the second light-emitting layer 122. Optical element 500cd / m 2 The electroluminescence spectrum at red, blue, and green wavelengths is shown. Since the peaks were observed for each, it was found that light was emitted simultaneously from these three luminescent materials. In fact, 1000cd / m 2 The chromaticity of the light emitted at (x, y) = (0 .38, 0.36), which shows that white light was obtained. EXAMPLES

[0108] In this example, a manufacturing example of a light-emitting element according to one embodiment of the present invention will be described. The schematic diagram of the optical element (light-emitting element 2) is shown in Figure 9(B), the details of the element structure are shown in Table 2, and the compounds used are shown in Table 2. The structures and abbreviations of the compounds used in the light-emitting element 1 described in Example 1 are shown below. Structure and abbreviations are omitted. [ka] [Table 2]

[0109] 1. Fabrication of Light-Emitting Device 2 Similar to the light-emitting element 1, a hole injection layer 124 and a hole transport layer 126 are formed on the first electrode 100. After that, PCzPA and 1,6mMemFLPAPrn were mixed in a weight ratio (PCzPA: 1,6mMe emFLPAPrn) was co-evaporated at 1:0.05 to a thickness of 10 nm to form the first layer. An optical layer 120 was formed.

[0110] On the first light-emitting layer 120, 2mDBTBPDBq-II and PCBBiF were added in a weight ratio (2mD The ratio of BTBPDBq-II:PCBBiF was 0.6:0.4, and the film thickness was 2 nm. Separation layer 135 was formed by evaporation.

[0111] On top of this, 2mDBTBPDBq-II, PCBBiF, and bis{2-[6-(2, 6-Dimethylphenyl)-4-pyrimidinyl-κN3]phenyl-κC}(2,4-pentane Tandonato-κO,O')iridium(III) (Ir(ppm-dmp)2(aca c)) by weight ratio (2mDBTBPDBq-II:PCBBiF:Ir (ppm-dmp) 2(acac)) in a ratio of 0.8:0.2:0.05 was co-evaporated to a thickness of 20 nm. The second light-emitting layer 122 was formed.

[0112] On top of this, 2mDBTBPDBq-II and Bphen were applied to thicknesses of 10 nm and 15 nm, respectively. The electron transport layers (128(1), 128(2)) were formed by sequentially depositing the layers so that the thickness of each layer became 128(1) and 128(2). Lithium fluoride is deposited on the electron transport layer (128(1), 128(2)) to a thickness of 1 nm. The electron injection layer 130 was formed by vapor deposition of an alloy of silver and magnesium in a volume ratio (A The film was then co-evaporated to a thickness of 1 nm with a ratio of 0.6:0.2 (Al:Mg), and 200 nm of silver was then deposited on top. The second electrode 102 was formed by deposition so as to have a thickness of 100 μm. The light-emitting element 2 was obtained by sealing.

[0113] 2. Characteristics of Light-Emitting Element 2 14 to 17 show the initial characteristics of the light-emitting element 2. As shown in FIG. Light emission begins at around 2.6V, and reaches 10,000cd / m at 4.3V. 2 More than This shows that it can be driven at a low voltage. 2 In The current efficiency and external quantum efficiency were 55.3cd / A and 17.2%, respectively (see Figure 15). The efficiency is 52.6lm / W (see Figure 16), which confirms that the efficiency is high. The light-emitting element 2 has a blue-emitting fluorescent material (1,6mMemFLPAPrn) in the first light-emitting layer 1. 20, a yellow light-emitting phosphorescent material (Ir(ppm-dmp)2(acac)) is formed as a second light-emitting layer 1 22. In Figure 17, 1000 cd / m 2 Electroluminescence spectrum of light-emitting element 2 at The peaks are observed in the blue and yellow wavelength regions, respectively. It can be seen that light is emitted simultaneously from two luminescent materials. 2 In The chromaticity of the emission was (x, y) = (0.41, 0.49).

[0114] As described above, the light-emitting element of this embodiment exhibits high current efficiency and can be driven at a low driving voltage. The configuration shown in this embodiment can be used in appropriate combination with other embodiments and mode of implementation. It is possible to do so. (Reference example 1)

[0115] As described in the first embodiment, an additive is added to the second light-emitting layer 122 to form an exciplex. The luminous efficiency can be significantly increased by forming a luminous flux. The optical elements are shown as 3 to 6. The details of the element structure are shown in Table 3. The structures of the compounds used are also shown in Table 3. The names are as follows. FIG. 18(A) is a schematic cross-sectional view of the light-emitting element 3 and the light-emitting element 5, and FIG. 2 is a schematic cross-sectional view of the light-emitting element 4 and the light-emitting element 6.

[0116] [ka]

[0117] [Table 3]

[0118] 1. Fabrication of Light-Emitting Device 3 As the first electrode 1100, an ITSO film was formed on a glass substrate to a thickness of 110 nm. The electrode area of ​​the first electrode 1100 was 4 mm 2 (2mm x 2mm) It was decided.

[0119] Next, a hole injection layer 1124 was formed on the first electrode 1100 using DBT3P-II and Mo The weight ratio of DBT3P-II to MoO3 is 1:0.5, and the thickness is 50 nm. The resulting mixture was co-evaporated.

[0120] Next, 4-phenyl-4'-(9 -phenylfluoren-9-yl)triphenylamine (abbreviation: BPAFLP) with a thickness of 2 The deposition was carried out so as to give a thickness of 0 nm.

[0121] Next, 2 mD was deposited on the hole transport layer 1126 as the light emitting layers 1122(1) and 1122(2). BTBPDBq-II, PCBBiF, and Ir(tBuppm)2(acac), Weight ratio (2mDBTBPDBq-II:PCBBiF:Ir(tBuppm)2(aca c)) were co-evaporated in a ratio of 0.7:0.3:0.05 to a thickness of 20 nm, and then Amount ratio (2mDBTBPDBq-II:PCBBiF:Ir(tBuppm)2(acac The mixture was co-deposited at a ratio of 0.8:0.2:0.05 to a thickness of 20 nm. In layer 1122, 2mDBTBPDBq-II is the host material and PCBBiF is It is an additive that can form an exciplex with the host material, and Ir(tBuppm)2( acac) is the luminescent material.

[0122] Next, the electron transport layers 1128(1), 1128(2), and the electron As the child injection layer 1130, 2mDBTBPDBq-II, Bphen, and LiF are used. The layers were deposited in sequence to thicknesses of 20 nm, 10 nm, and 1 nm, respectively.

[0123] Next, aluminum (Al) was deposited on the electron injection layer 1130 to a thickness as a second electrode 1102. The thickness was formed to be 200 nm.

[0124] Through the above steps, the light-emitting element 3 formed on the glass substrate was fabricated. In the film formation process, the deposition was all performed using a resistance heating method.

[0125] Next, in a glove box with a nitrogen atmosphere, the sealing substrate is sealed using an organic EL sealing material. The light-emitting element 3 was sealed by fixing the sealing material on the glass substrate. The glass substrate and the sealing substrate are then bonded together, and 365 nm ultraviolet light is applied at 6 J / cm2 The light-emitting element 3 was obtained by irradiating the light with light and then heat-treating it for 1 hour at 80° C.

[0126] 2. Fabrication of Light-Emitting Device 4 The fabrication process of the light-emitting element 4 is different from that of the light-emitting element 3 described above only in the following steps. The fabrication method was the same as that for the light-emitting element 3.

[0127] As the hole injection layer 1124 on the first electrode 1100, DBT3P-II, MoO3, and The weight ratio (DBT3P-II:MoO3) was 1:0.5 and the thickness was 10 nm. I arrived.

[0128] On the hole transport layer 1126, 2mDBTBPDBq-II and PC BBiF and bis{2-[5-methyl-6-(2-methylphenyl)-4-pyrimidinyl -κN3]phenyl-κC}(2,4-pentanedionato-κ 2 O,O') Iridium ( III) (Ir(mpmppm)2(acac)) in a weight ratio of (2mDBTBPDBq -II:PCBBiF:Ir(mpmppm)2(acac)) is 0.8:0.2:0. 06, and the thickness was 40 nm. BTBPDBq-II is the host material, and PCBBiF is the host material and the exciton The additive is capable of forming a luminescent compound, and Ir(mpmppm)2(acac) is the luminescent material. .

[0129] Next, 2 mD was deposited on the light-emitting layer 1122 as the electron transport layers 1128(1) and 1128(2). BTBPDBq-II and Bphen are prepared with thicknesses of 15 nm and 20 nm, respectively. The deposition was carried out in the following order.

[0130] 3. Fabrication of Light-Emitting Device 5 The light-emitting element 5 is fabricated in the following steps, which are different from the light-emitting element 3 described above. The fabrication method was the same as that for the light-emitting element 3.

[0131] As the hole injection layer 1124 on the first electrode 1100, DBT3P-II, MoO3, and The weight ratio (DBT3P-II:MoO3) was 1:0.5 and the thickness was 20 nm. I arrived.

[0132] On the hole transport layer 1126, 2mDBTB was formed as the light emitting layers 1122(1) and 1122(2). PDBq-II, PCBBiF, and (acetylacetonato)bis(4,6-diphenyl pyrimidinato)iridium(III) (abbreviation: Ir(dppm)2(acac)) Weight ratio (2mDBTBPDBq-II:PCBBiF:Ir(dppm)2(acac) ) were co-deposited in a ratio of 0.7:0.3:0.05 to a thickness of 20 nm, and then the weight ratio was (2mDBTBPDBq-II:PCBBiF:Ir(dppm)2(acac)) is 0 The light-emitting layer 112 was co-deposited at a ratio of 0.8:0.2:0.05 to a thickness of 20 nm. In 2, 2mDBTBPDBq-II is the host material, and PCBBiF is the host material. It is an additive that can form an exciplex with the material, and Ir(dppm)2(acac) is It is a light-emitting material.

[0133] Next, electron transport layers 1128(1) and 1128(2) are formed on the light emitting layer 1122(2). 2mDBTBPDBq-II and Bphen were arranged in order so that the thickness was 20 nm. Next, deposition was performed.

[0134] 4. Fabrication of Light-Emitting Device 6 The light-emitting element 6 is fabricated in the following steps, which are different from the light-emitting element 3 described above. The fabrication method was the same as that for the light-emitting element 3.

[0135] As the first electrode 1100, an ITSO film was formed on a glass substrate to a thickness of 70 nm. Successful.

[0136] Next, as the hole injection layer 1124 on the first electrode 1100, BPAFLP and MoO3 and MoO3) were co-evaporated to a thickness of 60 nm with a weight ratio (BPAFLP:MoO3) of 1:0.5. did.

[0137] On the hole transport layer 1126, 2mDBTBPDBq-II and PC BBiF and Ir(tppr)2(dpm) were mixed in a weight ratio of (2mDBTBPDBq-II : PCBBiF:Ir(tppr)2(dpm)) is 0.8:0.2:0.05, thickness is The luminescent layer 1122 was formed by co-evaporation to a thickness of 40 nm. q-II is the host material, and PCBBiF can form an exciplex with the host material. The additive is Ir(tppr)2(dpm), which is the luminescent material.

[0138] Next, 2 mD was deposited on the light-emitting layer 1122 as the electron transport layers 1128(1) and 1128(2). BTBPDBq-II and Bphen are prepared with thicknesses of 20 nm and 15 nm, respectively. The deposition was carried out in the following order.

[0139] 5. Characteristics of Light-Emitting Elements 3 to 6 Next, luminance-current efficiency curves of the thus fabricated Light-emitting Elements 3 to 6 are shown in FIG. Moreover, a voltage-luminance curve is shown in Figure 20. Moreover, a luminance-external quantum efficiency curve is shown in Figure 21. The measurements of each light-emitting device were carried out at room temperature (an atmosphere maintained at 23° C.).

[0140] Also, 1000cd / m 2 The element characteristics of the light-emitting elements 3 to 6 in the vicinity are shown in Table 4. The external quantum efficiency in Figure 21 and Table 4 was calculated taking into account the light distribution characteristics of the emitted light. It is.

[0141] [Table 4]

[0142] Furthermore, the light-emitting elements 3 to 6 were supplied with 2.5 mA / cm 2 When a current is applied at a current density of The electroluminescence spectra are shown in Figure 22. Light-emitting element 3 emits green light, and light-emitting element 4 emits yellow light. The light emitting element 5 emits orange light, and the light emitting element 6 emits red light.

[0143] As shown in FIG. 19 to FIG. 22 and Table 4, the light-emitting elements 3 to 6 exhibited high The light emission was achieved with a high current efficiency, a high external quantum efficiency, and a low driving voltage. The light-emitting elements 3 to 6 have little decrease in efficiency even in a high brightness region, and have high luminous efficiency. It maintains that.

[0144] Next, the measurement results of the reliability test of the light-emitting elements 3 to 6 are shown in FIG. The performance test was performed by setting the initial luminance of the light-emitting element to 5000 cd / m 2 The current density is set to constant. The light emitting element 3 to the light emitting element 6 were driven.

[0145] As a result, the time (LT90) at which the luminance of the light-emitting elements 3 to 6 deteriorated to 90% of the initial luminance are 1000 hours for light-emitting element 3, 1300 hours for light-emitting element 4, and 2000 hours for light-emitting element 5, respectively. The estimated life span of the first light-emitting element was 800 hours, and that of the light-emitting element 6 was 560 hours, showing excellent reliability.

[0146] Therefore, an additive capable of forming an exciplex with the host material is added to the light-emitting layer 1122. By using the exciplex as a medium for energy transfer, Regardless of the emission color, it has high current efficiency, high external quantum efficiency, and low driving voltage. It is also possible to obtain a light emitting element that emits light with excellent reliability. can be done.

[0147] (Reference example 2) The synthesis method of Ir(ppm-dmp)2(acac) used in Example 2 is described below. The teams are as follows: [ka]

[0148] 1. Synthesis of 4-chloro-6-phenylpyrimidine 4,6-Dichloropyrimidine 5.0g, Phenylboronic acid 4.9g, Sodium carbonate 7g .1g, bis(triphenylphosphine)palladium(II) dichloride (PdCl2( A mixture of 0.34 g of PPh3)2), 20 mL of acetonitrile, and 20 mL of water was The mixture was heated under reflux for 1 hour by irradiation with microwaves (2.45 GHz, 100 W) under a stream of argon. The resulting mixture was extracted with dichloromethane and subjected to silica gel column chromatography (eluent). By purifying the mixture in a solvent of dichloromethane, 4-chloro-6-phenylpyrimidine was obtained in 1 The product was obtained in an amount of 0.6 g (yield: 23%, pale yellow solid). A microwave synthesis apparatus (CEM Discover) was used.

[0149] 2,4-Phenyl-6-(2,6-dimethylphenyl)pyrimidine (HPPM-DMP) Synthesis of 4-Chloro-6-phenylpyrimidine 1.6g, 2,6-dimethylphenylboronic acid 1 .5g, sodium carbonate 1.8g, PdCl2(PPh3) 259mg, N,N-dimethyl A mixture of 20 mL of diethyl ether and 20 mL of water was heated in a microwave oven (2 The mixture was heated to reflux by irradiation with a 100 W (1.45 GHz, 100 W) for 2 hours. Extraction with ethyl acetate and silica gel column chromatography (eluent: ethyl acetate:hexane) The mixture was purified by hexane (1:5) to give 0.50 g of Hppm-dmp (yield: 23%, pure). (light yellow oil).

[0150] 3. Di-μ-chloro-tetrakis{2-[6-(2,6-dimethylphenyl)-4-pyridyl {rimidinyl-κN3]phenyl-κC}diiridium(III) ([Ir(ppm-dm Synthesis of p)2Cl2) Hppm-dmp 1.0g, iridium(III) chloride hydrate 0.57g, 2-ethoxy A mixture of 20 mL of ethanol and 20 mL of water was heated in a microwave oven under an argon stream (2. The mixture was heated under reflux for 3 hours under irradiation with a 45 GHz (100 W). The mixture was filtered. The solid was washed with methanol to obtain 1.1 g of [Ir(ppm-dmp)2Cl]2. Obtained (yield: 74%, orange solid).

[0151] 4. Synthesis of Ir(ppm-dmp)2(acac) [Ir(ppm-dmp)2Cl]21.1g, sodium carbonate 0.77g, acetyl For a mixture of 0.23 g of acetone (Hacac) and 30 mL of 2-ethoxyethanol, Heating by irradiating with microwaves (2.45GHz, 120W) for 2 hours under an argon atmosphere The mixture was filtered, and the insoluble matter was washed with methanol. The residue was purified by silica gel column chromatography (eluent: ethyl acetate:hexane= The solid was purified with a hexane dilution of 1:5, and the resulting solid was recrystallized with hexane to obtain Ir(ppm- dmp)2(acac) was obtained (yield: 59%, orange powder solid). 0.21g was purified by train sublimation to obtain the desired orange solid. The recovery rate was 48%. The sublimation purification conditions were a pressure of 2.7 Pa and an argon gas flow rate of 5.0 mL / m The temperature was 240°C. The Ir(ppm-dmp)2(acac) 1 H-NM The R (nuclear magnetic resonance) spectrum data is shown below.

[0152] 1 H-NMR.δ(CDCl3):1.85(s,6H),2.26(s,12H), 5.35(s,1H),6.46-6.48(dd,2H),6.83-6.90(dm ,4H),7.20-7.22(d,4H),7.29-7.32(t,2H),7.6 3-7.65(dd,2H),7.72(ds,2H),9.24(ds,2H). [Explanation of symbols]

[0153] 100 First electrode 102 Second electrode 120 First light-emitting layer 122 Second light-emitting layer 122(1) First layer of the second light-emitting layer 122 122(2) Second layer of the second light-emitting layer 122 124 Hole injection layer 126 Hole transport layer 126-1 Hole transport layer 126-2 Hole transport layer 128 Electron transport layer 128-1 Electron transport layer 128-2 Electron transport layer 128(1) Electron transport layer 128(2) Electron transport layer 130 Electron injection layer 132 Light-emitting layer 135 Separation layer 140-1 First light emitting unit 140-2 Second light emitting unit 150 Middle Class 401 Element substrate 402 Pixel section 403 Source side driver circuit 404a Gate side drive circuit 404b Gate side drive circuit 405 Sealing material 406 Sealing substrate 407 Wiring 408 FPC 409 n-channel transistor 410 p-channel transistor 411 Switching Transistors 412 Current Control Transistor 413 First electrode 414 Insulation 415 EL layer 416 Second Electrode 417 Light-emitting element 418 areas 551 Substrate 552 First electrode 553 Insulation Layer 554 Partition layer 555 EL layer 556 Second Electrode 730 Case 731a Display section 731b Display section 732a Touch panel area 732b Touch panel area 733 Fasteners 734 Display mode change switch 735 Power Switch 736 Power saving mode switch 737 Operation Key 738 Operation Switch 739 Operation Switch 750 Solar Cells 752 Charge / discharge control circuit 754 Battery 756 DC-DC Converter 801 Lighting Equipment 802 Lighting equipment 803 Lighting Equipment 804 Lighting Equipment 811 Light emitting device 812 Light emitting device 813 Light emitting device 814 Light-emitting device 821 Case 822 Support 824 Support 1100 First electrode 1102 Second electrode 1122 Light-emitting layer 1122(1) Emitting layer 1122(2) Emitting layer 1124 Hole injection layer 1126 Hole transport layer 1128(1) Electron transport layer 1128(2) Electron transport layer 1130 Electron injection layer 6100 Television equipment 6101 Housing 6103 Display section 6201 Main unit 6202 Case 6203 Display section 6204 Keyboard 6205 External connection port 6206 Pointing Device 6302 Case 6304 Display Panel 6305 Icon 6306 Icon 6311 Operation button 6312 Operation button 6313 Connection terminal 6321 Band 6322 Clasp 6400 Mobile Phone 6401 Case 6402 Display section 6403 Operation button 6404 External connection port 6405 Speaker 6406 Mike

Claims

1. a light-emitting element having a first electrode, a second electrode, a first light-emitting layer, a second light-emitting layer, and a third light-emitting layer; the first light-emitting layer includes a first fluorescent material and a first host material; T of the first fluorescent material 1 The level is the T 1 Higher than the level, S of the first host material 1 The level is S of the first fluorescent material. 1 Higher than the level, the second light-emitting layer includes a first phosphorescent material, a second host material, and a second material capable of forming an exciplex with the second host material; the third light-emitting layer comprises a second fluorescent material and a third host material; T of the second fluorescent material 1 The level is the T 1 Higher than the level, S of the third host material 1 The level is S of the second fluorescent material. 1 A light-emitting device, higher than the level.

2. In claim 1, The emission peak wavelength of the first fluorescent material is shorter than the emission peak wavelength of the first phosphorescent material; A light emitting device, wherein the emission peak wavelength of the second fluorescent material is shorter than the emission peak wavelength of the first phosphorescent material.

3. In claim 1 or 2, the emission color of the first fluorescent material is blue; the emission color of the second fluorescent material is blue; The light emitting device, wherein the emission color of the first phosphorescent material is green, yellow, or red.

4. In any one of claims 1 to 3, a first light-emitting layer and a second light-emitting layer, the first light-emitting layer being separated from the first light-emitting layer by a first electron-transporting material, a first hole-transporting material, and a first acceptor; and

5. In any one of claims 1 to 4, a second electron transport material, a second hole transport material, and a second acceptor, the second light emitting layer and the third light emitting layer being separated from each other by a second electron transport material, a second hole transport material, and a second acceptor.

Citation Information

Patent Citations

  • Light-emitting element, display, and electronic equipment

    JP2009129711A

  • Light-emitting element, light-emitting apparatus, electronic device, and illumination apparatus

    JP2011228277A

  • Light-emitting element, light-emitting device, electronics, and lighting device

    JP2011228278A

  • Light-emitting element

    JP2012186461A

  • Luminous element, light-emitting device, electronic apparatus and light device

    JP2013219024A