Biomedical Devices

JP2024511728A5Active Publication Date: 2024-10-25BAUSCH & LOMB IRELAND LIMITED
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023554393
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-03-15
Filing Date
2022-03-14
Publication Date
2024-10-25
Estimated Expiration
2042-03-14

AI Technical Summary

Technical Problem

Biomedical devices such as ophthalmic lenses made from siloxy-containing materials often have hydrophobic surfaces and inadequate wettability, which can lead to discomfort and reduced oxygen permeability, necessitating a balance of properties for improved wearability and functionality.

Method used

The development of thermoplastic or thermoset polyoxazoline-based silicone-containing polyurethane materials, comprising difunctional isocyanates, polyalcohols, dihydroxy-terminated polysiloxane prepolymers, and polyoxazoline polyols, which are polymerized and hydrated to create biomedical devices with enhanced oxygen permeability and wettability.

Benefits of technology

The resulting materials exhibit improved oxygen permeability and wettability, suitable for high-throughput production of contact lenses, ensuring comfort and functionality by balancing key physical properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2022194737000001
    Figure 2022194737000001
  • Figure 2022194737000002
    Figure 2022194737000002
  • Figure 2022194737000003
    Figure 2022194737000003
Patent Text Reader

Abstract

A biomedical device is disclosed that is the polymerization product of a mixture comprising: (a) one or more difunctional isocyanates; (b) one or more polyalcohols; (c) one or more dihydroxy-terminated polysiloxane prepolymers; and (d) one or more polyoxazoline polyols having a weight average molecular weight of about 1000 Daltons or greater.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Claiming priority This application claims priority to U.S. Provisional Patent Application No. 63 / 161,002, entitled "Biomedical Devices," filed March 15, 2021, the contents of which are incorporated by reference herein in their entirety. [Background technology]

[0002] Biomedical devices such as ophthalmic lenses made from siloxy-containing materials have been investigated for several years. Such materials can generally be subdivided into two main types: hydrogels and non-hydrogels. Hydrogels can absorb and retain water in equilibrium, whereas non-hydrogels do not absorb significant amounts of water. Regardless of their water content, both hydrogel and non-hydrogel siloxy and / or fluorinated contact lenses tend to be relatively hydrophobic and have non-wetting surfaces.

[0003] Hydrogels represent a desirable class of materials for many biomedical applications, including contact lenses and intraocular lenses. Hydrogels are hydrated crosslinked polymer systems that contain water in equilibrium. Silicone hydrogels are a known class of hydrogels, characterized by the inclusion of siloxy-containing materials. The advantage of silicone hydrogels over non-silicone hydrogels is that they typically have higher oxygen permeability due to the inclusion of siloxy-containing monomers. Most existing hydrogels are based on the free radical polymerization of monomers that contain crosslinkers, and therefore these materials are thermosetting polymers.

[0004] In the field of biomedical devices such as contact lenses, various physical and chemical properties, such as oxygen permeability, wettability, material strength and stability, are just some of the factors that must be carefully balanced to provide a usable contact lens. For example, the cornea receives its oxygen supply from contact with the atmosphere, so good oxygen permeability is an important feature for certain contact lens materials. Wettability is also important in that if the lens is not wettable enough, it will not remain lubricated and therefore cannot be worn comfortably on the eye. Thus, an optimal contact lens will have at least both good oxygen permeability and good tear wettability. Summary of the Invention

[0005] According to an exemplary embodiment, the biomedical device is a polymerization product of a mixture comprising: (a) one or more difunctional isocyanates; (b) one or more polyalcohols; (c) one or more dihydroxy-terminated polysiloxane prepolymers; and (d) one or more polyoxazoline polyols having a weight average molecular weight of about 1000 Daltons or greater.

[0006] According to another exemplary embodiment, there is provided a method for making a biomedical device comprising: (a) providing a mixture comprising (i) one or more difunctional isocyanates, (ii) one or more polyalcohols, (iii) one or more dihydroxy-terminated polysiloxane prepolymers, and (iv) one or more polyoxazoline polyols having a weight average molecular weight of about 1000 Daltons or greater; (b) subjecting the mixture to polymerization conditions to provide a polymerized device; and (c) hydrating the polymerized device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Various exemplary embodiments described herein are directed to biomedical devices obtained from thermosetting or thermoplastic polyoxazoline-based silicone-containing polyurethane materials. The polyoxazoline-based silicone-containing polyurethane materials described herein in non-limiting exemplary embodiments are particularly suitable for use in the contact lens industry. In addition, the polyoxazoline-based silicone-containing polyurethane materials are thermoplastic or thermosetting materials that exhibit exemplary physical properties, particularly in terms of oxygen permeability and light permeability. Advantageously, the thermoplastic or thermosetting materials described herein are suitable for use in conventional molding equipment, thereby enabling high-throughput production of contact lenses.

[0008] Thermoplastic polyurethanes have minimal crosslinking, and any bonds within the polymer network are primarily through hydrogen bonds or other physical mechanisms. Due to the low level of crosslinking, thermoplastic polyurethanes are relatively flexible. The crosslinks in thermoplastic polyurethanes can be reversibly broken by increasing temperatures, such as during molding or extrusion. That is, the thermoplastic material softens when exposed to heat and returns to its original state when cooled. Thermoset polyurethanes, on the other hand, are irreversibly fixed when cured. The crosslinks are irreversibly fixed and do not break when exposed to heat. Thus, thermoset polyurethanes, which typically have a high level of crosslinking, are relatively rigid. Thus, as used herein, the term "thermoplastic" refers to a material that melts at a temperature below its decomposition temperature. As used herein, the term "thermoset" refers to a material that melts at a temperature above its decomposition temperature.

[0009] The biomedical devices disclosed herein are intended to be in direct contact with body tissues or fluids. As used herein, the term "biomedical device" refers to any article designed to be used in or on mammalian tissues or fluids, preferably in or on human tissues or fluids. Representative examples of biomedical devices include, but are not limited to, artificial ureters, diaphragms, intrauterine contraceptive devices, heart valves, catheters, denture liners, prosthetic devices, and ophthalmic lens applications, where the lenses are intended to be placed directly in or on the eye, such as, for example, intraocular devices and contact lenses. In an exemplary embodiment, the biomedical device is an ophthalmic device, in particular a contact lens, more particularly a contact lens made from silicone hydrogel.

[0010] As used herein, the term "ophthalmic device" refers to devices that reside in and on the eye. These devices can provide optical correction, wound care, drug delivery, diagnostic functions, or cosmetic enhancements or effects, or a combination of these properties. Useful ophthalmic devices include, but are not limited to, ophthalmic lenses, such as soft contact lenses (e.g., hydrogel soft lenses, and non-hydrogel soft lenses), hard contact lenses (e.g., gas permeable hard lens materials), intraocular lenses, overlay lenses, intraocular inserts, optical inserts, and the like. As will be understood by those skilled in the art, a lens is considered to be "soft" if it can fold back on itself without breaking.

[0011] In an exemplary embodiment, the ophthalmic device may be a high water content ophthalmic device. In an exemplary embodiment, the high water content ophthalmic device will have an equilibrium water content of at least about 65 weight percent. In another exemplary embodiment, the high water content ophthalmic device will have an equilibrium water content of at least about 70 weight percent. In another exemplary embodiment, the high water content ophthalmic device will have an equilibrium water content of at least about 75 weight percent.

[0012] In an exemplary, non-limiting embodiment, the biomedical devices disclosed herein are formed from the polymerization product of a mixture comprising: (a) one or more difunctional isocyanates; (b) one or more polyalcohols; (c) one or more dihydroxy-terminated polysiloxane prepolymers; and (d) one or more polyoxazoline polyols having a weight average molecular weight of about 1000 Daltons or greater.

[0013] Suitable one or more difunctional isocyanates include, for example, any aliphatic, cycloaliphatic, or aromatic isocyanate.Suitable aromatic diisocyanates that can be used herein include, for example, toluene 2,4-diisocyanate (TDI), toluene 2,6-diisocyanate (TDI), 4,4'-methylenediphenyl diisocyanate (MDI), 2,4'-methylenediphenyl diisocyanate (MDI), polymeric methylenediphenyl diisocyanate (PMDI), p-phenylene diisocyanate (PPDI), m-phenylene diisocyanate (PDI), naphthalene 1,5-diisocyanate (NDI), naphthalene 2,4-diisocyanate (NDI), p-xylene diisocyanate (XDI), and homopolymers and copolymers and blends thereof. Suitable aliphatic diisocyanates that may be used herein include, for example, isophorone diisocyanate (IPDI), 1,6-hexamethylene diisocyanate (HDI), 4,4'-dicyclohexylmethane diisocyanate ("HDI"). 12 Suitable polyfunctional isocyanates include HDI or HMI, meta-tetramethylxylene diisocyanate (TMXDI), trans-cyclohexane diisocyanate (CHDI), and homopolymers and copolymers and blends thereof. 12 This includes trimers, oligomers, or other derivatives of MDI. As used herein, the term "difunctional" means that the average functionality of the isocyanate composition and the polyhydroxy compound is about 2.

[0014] In an exemplary embodiment, the one or more difunctional isocyanates have the formula OCN-R 1 -NCO, wherein R 1 Linear or branched C3-C 18 -Alkylene, unsubstituted or substituted C6-C 10 -Arylene, unsubstituted or substituted C7-C 18 -Aralkylene, unsubstituted or substituted C6-C 10 -Arylene-C1~C2-Alkylene-C6~C 10 -arylene, unsubstituted or substituted C3-C8-cycloalkylene, unsubstituted or substituted C3-C8-cycloalkylene-C1-C6-alkylene, unsubstituted or substituted C3-C8-cycloalkylene-C1-C6-alkylene-C3-C8-cycloalkylene, or unsubstituted or substituted C1-C6-alkylene-C3-C8-cyclo-alkylene-C1-C6-alkylene.

[0015] In an exemplary embodiment, the one or more difunctional isocyanates may be present in the mixture in an amount ranging from about 20 to about 60 weight percent, based on the total weight of the mixture. In an exemplary embodiment, the amount of the one or more difunctional isocyanates in the mixture may be in the range of about 30 to about 45 weight percent, based on the total weight of the mixture.

[0016] The mixture further comprises one or more polyalcohols. Suitable polyalcohols include, for example, linear or branched aliphatic or aromatic diols, triols, higher functional polyols having an average functionality of more than three, tertiary amine polyalcohols, alkoxylated polyalcohols, polyether polyalcohols, and mixtures thereof. In an exemplary embodiment, the one or more polyalcohols may have, for example, from about 2 to about 1000 carbon atoms and from 2 to about 10 hydroxy groups. In another embodiment, the one or more polyalcohols may have up to about 1000 carbon atoms, or up to about 750 carbon atoms, or up to about 650 carbon atoms, or up to about 550 carbon atoms, or up to about 450 carbon atoms, or up to about 350 carbon atoms, or up to about 250 carbon atoms, or up to about 150 carbon atoms, or up to about 100 carbon atoms, or up to about 50 carbon atoms, and from 2 to about 10 hydroxy groups. In one embodiment, the one or more polyalcohols can have at least 2 carbon atoms, or at least about 5 carbon atoms, or at least about 10 carbon atoms, or at least about 15 carbon atoms, or at least about 20 carbon atoms, or at least about 25 carbon atoms, or at least about 30 carbon atoms, or at least about 40 carbon atoms, or at least about 50 carbon atoms, or at least about 100 carbon atoms, and from 2 to about 10 hydroxy groups. As one of ordinary skill in the art would readily appreciate, any of the foregoing lower limits can be combined with any of the upper limits.

[0017] In exemplary embodiments, the one or more polyalcohols can have, for example, about 1 to about 50 carbon atoms and 2 to 10 hydroxy groups. In exemplary embodiments, the one or more polyalcohols can have, for example, about 2 to about 50 carbon atoms and 2 to 10 hydroxy groups. When used as a chain extender, the one or more polyalcohols can have, for example, about 2 to about 20 carbon atoms, or about 2 to about 10 carbon atoms, or about 2 to about 5 carbon atoms, and 2 to 10 hydroxy groups, or 2 to 4 hydroxy groups.

[0018] Suitable diols include, for example, ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, dipropylene glycol, trimethylene glycol, butylene glycol, neopentyl glycol, 2,2-dimethyl-1,3-propanediol, 1,6-hexanediol, 2-methyl-1,3-propanediol, 1,3-propaneglycol, 1,3-butanediol, 1,4-butanediol, 1,5-pentanediol, 3-hydroxy-2,2-dimethylpropyl-3-hydroxy-2,2-dimethylpropanoate (HPHP), 1,2-cyclohexanediol, 1,3-cyclohexanediol, 1,3-cyclohexanedimethanol, 1,4-cyclohexanedimethanol, resorcinol, hydroquinone, and poly(oxyalkylene) polyols derived from the condensation of ethylene oxide, propylene oxide, or combinations thereof. Mixtures of any of the diols are also contemplated. The polyalcohol component may also include triols, higher functionality polyols having an average functionality greater than three, or mixtures thereof.

[0019] Suitable triols and higher functional polyalcohols include, for example, glycerol, diglycerol, trimethylolpropane, pentaerythritol, dipentaerythritol, sugars (e.g., sucrose, glucose, and fructose), sugar alcohols (e.g., sorbitol and mannitol), and combinations of any of the foregoing. For some embodiments, mixtures of diols, triols, and / or higher functional polyalcohols are also contemplated.

[0020] Suitable tertiary amine polyalcohols include, for example, compounds having at least two hydroxyl groups and at least one tertiary amine group. In one embodiment, the tertiary amine polyalcohol may have, for example, about 2 to about 50 carbon atoms, or about 2 to about 20 carbon atoms, or about 2 to about 10 carbon atoms, or about 2 to about 5 carbon atoms, and 2 to 10 hydroxy groups, or 2 to 4 hydroxy groups. Representative examples of suitable tertiary amine polyalcohols include triethanolamine, N-methyldiethanolamine, N-ethyldiethanolamine, N-propyldiethanolamine, Nn-butyldiethanolamine, N-tert-butyldiethanolamine, N-bis(2-hydroxyethyl)octadecylamine, bis(2-hydroxyethyl)cocoalkylamine, bis(2-hydroxyethyl)oleylamine, ethoxylated (EO), propoxylated (PO), and mixed EO / PO tertiary amines, such as ethoxylated triethanolamine, and mixtures thereof.

[0021] Suitable alkoxylated polyalcohols may have, for example, about 2 to about 20 carbon atoms, or about 3 to about 20 carbon atoms, or about 4 to about 20 carbon atoms, or about 2 to about 10 carbon atoms, and 2 to 10 hydroxy groups, or 2 to 4 hydroxy groups. In one embodiment, the alkoxylated polyalcohol may have a number average molecular weight of 200 to 5,000 grams / mole. In one embodiment, a suitable alkoxylated polyalcohol may be polyoxyethylene glycol, i.e., "PEG," which is used to describe polyoxyethylene, followed by a number indicating the PEG moiety having the approximate molecular weight equal to that number. Representative examples of PEG for use herein include PEG 350, PEG 4000, PEG 6000, PEG 8000, and PEG 10000 (which is the PEG moiety having the approximate molecular weight of 10,000 daltons).

[0022] Representative examples of suitable alkoxylated polyalcohols include ethoxylated diols, ethoxylated triols, ethoxylated tetrols, ethoxylated pentaols, ethoxylated hexaols, propoxylated diols, propoxylated triols, propoxylated tetrols, propoxylated pentaols, propoxylated hexaols, butoxylated diols, butoxylated triols, butoxylated tetrols, butoxylated pentaols, butoxylated hexaols, etc. Representative examples of ethoxylated polyalcohols are ethoxylated glycerols, ethoxylated pentaerythritols, ethoxylated trimethylolpropanes, ethoxylated glucosides, and ethoxylated glucoses.

[0023] Suitable polyether polyalcohols include, for example, polyether polyalcohols that contain one or more chains or polymeric moieties having one or more (-OR-) repeating units, where R is an alkylene or arylene group having from 2 to about 6 carbon atoms. The polyethers may be derived from block copolymers formed from different ratios of ethylene oxide (EO) and propylene oxide (PO) moieties. Such polyethers and each of their component segments may contain different attached hydrophobic and hydrophilic chemical functional moieties and segments.

[0024] Representative examples of suitable polyether polyalcohols are the poloxamer block copolymers. One particular type of poloxamer block copolymer is available under the trademark Pluronic® (BASF Wyandotte Corp., Wyandotte, Mich.). Poloxamers include Pluronics and reverse Pluronics. Pluronics generally have the formula (I): HO(C2H4O) a (C3H6O) b (C2H4O) a H (I) (wherein a is independently at least 1 and b is at least 1),

[0025] Reverse Pluronics generally have the formula (II) HO(C3H6O) b (C2H4O) a (C3H6O) b H (II) The poloxamers in the series are each composed of a poly(propylene oxide)-poly(ethylene oxide)-poly(propylene oxide) block represented by the formula: (wherein a is at least 1 and b is independently at least 1). The poly(ethylene oxide) (PEO) block is hydrophilic, whereas the poly(propylene oxide) (PPO) block is hydrophobic in nature. The poloxamers in each series have different ratios of PEO to PPO, which ultimately determines the hydrophilic-lipophilic balance (HLB) of the material, i.e., the different HLB values ​​are based on different values ​​of a and b, where a represents the number of hydrophilic poly(ethylene oxide) units (PEO) present in the molecule, and b represents the number of hydrophobic poly(propylene oxide) units (PPO) present in the molecule.

[0026] Another example of a suitable polyether polyalcohol may be a poloxamine block copolymer. The term block copolymer as used herein should be understood to mean a poloxamer and / or poloxamine having two or more blocks in the polymer backbone. While poloxamers and reverse poloxamers are considered to be difunctional molecules (based on the terminal hydroxyl groups), poloxamines are in tetrafunctional form, i.e., these molecules are tetrafunctional block copolymers terminated with primary hydroxyl groups and linked by a central diamine. One particular type of poloxamine block copolymer is available under the trademark Tetronic (BASF). Poloxamines include Tetronics and reverse Tetronics. Poloxamines are represented by the following formula (III): [ka] wherein a is independently at least 1 and b is independently at least 1.

[0027] The one or more polyalcohols described above may be present in the mixture in an amount ranging from about 10 to about 70 weight percent, based on the total weight of the mixture. In an exemplary embodiment, the amount of the one or more polyalcohols in the mixture may range from about 12 to about 20 weight percent, based on the total weight of the mixture.

[0028] The mixture further comprises one or more hydroxy-terminated polysiloxane prepolymers. In an exemplary embodiment, the hydroxy-terminated polysiloxane prepolymer has the structure of formula (IV): [ka] wherein each R is independently a hydroxyl-containing reactive functional end group; R 1 ~R 6 are independently hydrocarbyl groups, e.g., linear or branched, substituted or unsubstituted C1-C 30Alkyl groups, substituted or unsubstituted C3-C 30 Cycloalkyl groups, substituted or unsubstituted C4-C 30 Cycloalkylalkyl groups, substituted or unsubstituted C3-C 30 Cycloalkenyl groups, substituted or unsubstituted C6-C 30 Aryl groups and substituted or unsubstituted C7-C 30 It is an arylalkyl group, L is independently a linking group, and x is 3 to 200.

[0029] A hydroxyl-containing reactive functional end group for use herein is a group that contains at least one hydroxyl group. Representative examples of hydroxyl-containing reactive functional end groups for use herein include, by way of example, those of the following general formula -R 7 (OH), where R 7 are independently alkyl, aryl, and cycloalkyl groups, etc., as defined herein.

[0030] The linking groups L are independently straight or branched, substituted or unsubstituted alkyl groups, substituted or unsubstituted cycloalkyl groups, substituted or unsubstituted aryl groups, substituted or unsubstituted ether or polyether groups, and substituted or unsubstituted ester groups.

[0031] Representative examples of alkyl groups for use herein include, by way of example, straight or branched alkyl chain groups containing carbon and hydrogen atoms having from 1 to about 30 carbon atoms, or from 1 to about 12 carbon atoms, or from 1 to about 6 carbon atoms, relative to the remainder of the molecule, with or without unsaturation, such as methyl, ethyl, n-propyl, 1-methylethyl (isopropyl), n-butyl, n-pentyl, methylene, ethylene, and the like.

[0032] Representative examples of cycloalkyl groups for use herein include, by way of example, substituted or unsubstituted non-aromatic monocyclic or polycyclic ring systems of about 3 to about 30 carbon atoms, or 3 to about 6 carbon atoms, such as cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, perhydronaphthyl, adamantyl, and norbornyl groups, bridged cyclic or spiro bicyclic groups, such as spiro-(4,4)-non-2-yl, and the like, optionally containing one or more heteroatoms, such as, for example, O and N.

[0033] Representative examples of cycloalkylalkyl groups for use herein include, by way of example, substituted or unsubstituted cyclic ring-containing groups containing from about 4 to about 30 carbon atoms, or from 3 to about 6 carbon atoms, which are attached directly to the alkyl group and then attached to the main structure of the monomer at any carbon from the alkyl group to produce a stable structure, such as, for example, cyclopropylmethyl, cyclobutylethyl, cyclopentylethyl, and the like, and the cyclic ring may optionally contain one or more heteroatoms, such as, for example, O and N.

[0034] Representative examples of cycloalkenyl groups for use herein include, by way of example, substituted or unsubstituted cyclic ring-containing groups containing from about 3 to about 30 carbon atoms, or from 3 to about 6 carbon atoms, and having at least one carbon-carbon double bond, such as cyclopropenyl, cyclobutenyl, cyclopentenyl, and the like, wherein the cyclic ring can optionally contain one or more heteroatoms, such as, for example, O and N.

[0035] Representative examples of aryl groups for use herein include, by way of example, substituted or unsubstituted monocyclic or polycyclic aromatic groups containing from about 6 to about 30 carbon atoms, e.g., phenyl, naphthyl, tetrahydronaphthyl, indenyl, biphenyl, and the like, optionally containing one or more heteroatoms such as, for example, O and N.

[0036] Representative examples of arylalkyl groups for use herein include, by way of example, a substituted or unsubstituted aryl group, as defined herein, directly bonded to an alkyl group, as defined herein, such as, for example, -CH2C6H5, -C2H4C6H5, and the like, where the aryl group may optionally contain one or more heteroatoms, such as, for example, O and N.

[0037] Representative examples of ester groups for use herein include, by way of example, carboxylic acid esters having 1 to 20 carbon atoms.

[0038] Representative examples of ether- or polyether-containing groups for use herein include, by way of example, alkyl ethers, cycloalkyl ethers, cycloalkylalkyl ethers, cycloalkenyl ethers, aryl ethers, arylalkyl ethers, where alkyl, cycloalkyl, cycloalkylalkyl, cycloalkenyl, aryl, and arylalkyl groups are as defined herein. Exemplary ether- or polyether-containing groups include, by way of example, alkylene oxides, poly(alkylene oxides), such as ethylene oxide, propylene oxide, butylene oxide, poly(ethylene oxide), poly(ethylene glycol), poly(propylene oxide), poly(butylene oxide), and mixtures or copolymers thereof, alkylene oxides of the general formula -(R 14 OR 15 ) t An ether group or a polyether group represented by the formula: 14 is a bond, a substituted or unsubstituted alkyl, cycloalkyl, or aryl group as defined herein, and R 15 is a substituted or unsubstituted alkyl, cycloalkyl, or aryl group as defined herein, and t is at least 1.

[0039] In an exemplary embodiment, the hydroxy-terminated polysiloxane prepolymer has the structure of formula (V): [ka] In the formula, each R, R 1 , R 2 , R 3 and R 4 The groups are independently H or hydrocarbyl groups, e.g., linear or branched, substituted or unsubstituted C1-C 12 represents an alkyl group, p is an integer from 0 to 40, for example, 1 to 10, q is an integer from 0 to 40, for example, 1 to 10, z is an integer from 2 to 50, for example, 2 to 10 or 2, u is an integer from 1 to 100, for example, 10 to 40, y is an integer from 0 to 40, for example, 1 to 10, w is an integer from 0 to 40, for example, 1 to 10, and v is an integer from 2 to 50, for example, 2 to 10, and each Q group independently represents a hydroxyl-containing reactive functional end group.

[0040] In an exemplary embodiment, at least one R 1 group represents a hydrocarbyl group, p represents an integer from 1 to 40, or at least one R 2 group represents a hydrocarbyl group, q represents an integer from 1 to 40, and at least one R 3 group represents a hydrocarbyl group, w represents an integer from 1 to 40, or at least one R 4 The group represents a hydrocarbyl group, and y represents an integer of 1 to 40.

[0041] In an exemplary embodiment, each R, R 1 , R 2 , R 3 and R 4 The groups independently represent H or an alkyl group, such as a methyl, ethyl, or propyl group.

[0042] In an exemplary embodiment, at least one R 1 group and at least one R 4 The group represents a hydrocarbyl group, p represents an integer of 1 to 40, and y represents an integer of 1 to 40.

[0043] In an exemplary embodiment, at least one R 2 group and at least one R3 The group represents a hydrocarbyl group, q represents an integer of 1 to 40, and w represents an integer of 1 to 40.

[0044] In an exemplary embodiment, the silicone-containing compounds are symmetrical, however, asymmetrical structures with silicone compounds can also be used.

[0045] In an exemplary embodiment, 1 and / or R 4 represents a hydrocarbyl group, p and q each independently represent an integer of 1 to 5, and w and y each independently represent an integer of 1 to 10 or 5 to 10.

[0046] In an exemplary embodiment, 3 and / or R 4 represents a hydrocarbyl group, w and y each independently represent an integer of 1 to 5, and p and q each independently represent an integer of 1 to 10 or 5 to 10.

[0047] In an exemplary embodiment, Q is OH.

[0048] In another exemplary embodiment, the hydroxy-terminated polysiloxane prepolymer has the structure of formula (Va): [ka] wherein R1 and R4 are hydrocarbyl groups, such as linear or branched, substituted or unsubstituted C1-C 12 represents an alkyl group, for example, methyl, ethyl, or propyl; p represents an integer of 1 to 40, for example, 1 to 10; y represents an integer of 1 to 40, for example, 1 to 10; q represents an integer of 1 to 40, for example, 5 to 10; w represents an integer of 1 to 40, for example, 5 to 10; and Q, z, R, u, and v are as defined above.

[0049] In another exemplary embodiment, the hydroxy-terminated polysiloxane prepolymer has the structure of formula (Vb): [ka] wherein R 2 and R 3 is a hydrocarbyl group, for example a linear or branched, substituted or unsubstituted C1-C 12 represents an alkyl group, for example, methyl, ethyl, or propyl; p represents an integer of 1 to 40, for example, 1 to 10; y represents an integer of 1 to 40, for example, 1 to 10; q represents an integer of 1 to 40, for example, 5 to 10; w represents an integer of 1 to 40, for example, 5 to 10; and Q, z, R, u, and v are as defined above.

[0050] In another exemplary embodiment, the hydroxy-terminated polysiloxane prepolymer has the structure of formula (Vc): [ka] where each R group is an alkyl group, e.g., methyl, ethyl, or propyl, and p, q, z, u, v, w, and y are as defined above. An example of a compound of formula (Vc) is Silsurf® 2510 available from Siltech Corporation, where each R group represents a methyl group, z is 25, p is 10, and y is 10.

[0051] In exemplary embodiments, the one or more hydroxy-terminated polysiloxane prepolymers can have a number average molecular weight of about 500 to about 5000 Daltons, as determined, for example, by size exclusion chromatography (i.e., gel permeation chromatography). In exemplary embodiments, the one or more hydroxy-terminated polysiloxane prepolymers can have a number average molecular weight of about 500 to about 3500 Daltons. In exemplary embodiments, the one or more hydroxy-terminated polysiloxane prepolymers can have a number average molecular weight of about 800 to about 3000 Daltons.

[0052] Methods for making one or more hydroxy-terminated polysiloxane prepolymers are well known and within the purview of one skilled in the art. Additionally, polysiloxane prepolymers are also commercially available from sources such as, for example, Gelest, Silar, Shin-Etsu, Momentive, and Siltech.

[0053] The one or more hydroxy-terminated polysiloxane prepolymers may be present in the mixture in an amount ranging from about 3 to about 60 weight percent, based on the total weight of the mixture. In an exemplary embodiment, the amount of the one or more hydroxy-terminated polysiloxane prepolymers in the mixture may range from about 10 to about 50 weight percent, based on the total weight of the mixture.

[0054] The mixture further comprises one or more polyoxazoline polyols having a weight average molecular weight of about 1000 Daltons or greater, as determined, for example, by size exclusion chromatography (i.e., gel permeation chromatography). In an exemplary embodiment, the one or more polyoxazoline polyols can have a weight average molecular weight of about 1000 Daltons or greater, and up to about 50,000,000 Daltons. In exemplary embodiments, the one or more polyoxazoline polyols may have a weight average molecular weight of about 1000 daltons or greater, or greater than 10,000 daltons, or greater than 25,000 daltons, or greater than 50,000 daltons, or greater than 100,000 daltons, or greater than 250,000 daltons, or greater than 500,000 daltons, or greater than 750,000 daltons, or greater than 1,000,000 daltons, or greater than 2,500,000 daltons, or greater than 5,000,000 daltons, or greater than 10,000,000 daltons, or greater than 25,000,000 daltons, up to about 50,000,000 daltons. In exemplary embodiments, the one or more polyoxazoline polyols may have a weight average molecular weight of less than about 50,000,000 daltons, or less than 25,000,000 daltons, or less than 10,000,000 daltons, or less than 5,000,000 daltons, or less than 2,500,000 daltons, or less than 1,000,000 daltons, or less than 750,000 daltons, or less than 500,000 daltons, or less than 250,000 daltons, or less than 100,000 daltons.

[0055] In an exemplary embodiment, the one or more polyoxazoline polyols are difunctional, trifunctional, or tetrafunctional polyoxazoline polyols. In an exemplary embodiment, a difunctional polyoxazoline polyol is a C1-C 1,2-dioxazoline polyol having two oxazoline-containing hydroxyl groups per alkyl molecule, the alkyl molecule optionally containing one or more of an ether linkage and / or an ester linkage. 12Alkyl polyoxazoline polyols, C6-C, with two oxazoline-containing hydroxyl groups per aromatic molecule 30 Aromatic polyoxazoline polyols, C3-C oxazoline-containing hydroxyl groups per cycloalkyl molecule. 20 In one embodiment, the aryl group is phenyl. For example, in one embodiment, the one or more polyoxazoline polyols are of the structure of formula (VI): [ka] where each R is a hydroxyl group, each R' is independently a hydrocarbyl group, such as, for example, an alkyl group, a haloalkyl group, an alkene group, an alkyne group, a cycloalkyl group, a halocycloalkyl group, an aryl group, a haloaryl group, an aralkyl group, and a haloaralkyl group, Z is a divalent bond, and each of x and y is independently at least 1, for example, from 1 up to about 200. Representative Z bonds include single bonds, C1-C aryl groups, optionally including ether bonds. 12 Alkylene group, C6-C 30 Arylene group, C7-C 30 Alkarylene group, and C3-C 20 Cycloalkylene groups are included.

[0056] In another exemplary embodiment, the trifunctional polyoxazoline polyol is a C1-C aryloxy group-containing polyoxazoline having three oxazoline-containing hydroxyl groups per alkyl molecule, the alkyl molecule optionally containing one or more of an ether linkage and / or an ester linkage. 12 In an exemplary embodiment, the polyoxazoline polyol is a C1-C 12The alkyl moiety may be a straight or branched alkyl chain molecule containing carbon and hydrogen atoms of 1 to 12 carbon atoms, or 1 to about 6 carbon atoms, relative to the remainder of the molecule, with or without unsaturation. The three oxazoline-containing hydroxyl groups may be the same or different and may be provided at any point of attachment to the alkyl moiety.

[0057] In another exemplary embodiment, the trifunctional polyoxazoline polyol is a C-C oxazoline-containing hydroxyl group-containing polyol having three oxazoline-containing hydroxyl groups per aromatic molecule. 30 In an exemplary embodiment, the aromatic polyoxazoline polyol is a C6-C 30 The aromatic may be a substituted or unsubstituted monocyclic or polycyclic aromatic group containing about 6 to about 30 carbon atoms, or 6 to 12 carbon atoms, such as phenyl, naphthyl, tetrahydronaphthyl, indenyl, biphenyl, and the like, optionally containing one or more heteroatoms, such as O and N. The three oxazoline-containing hydroxyl groups may be the same or different and may be provided at any point of attachment to the aromatic molecule. In one embodiment, the aromatic molecule is phenyl.

[0058] In another exemplary embodiment, the trifunctional polyoxazoline polyol is a C-C cycloalkyl polyol having three oxazoline-containing hydroxyl groups per cycloalkyl molecule. 20 In an exemplary embodiment, the polyoxazoline polyol is a cycloalkyl polyoxazoline polyol. 20The cycloalkyl molecule may be a substituted or unsubstituted non-aromatic monocyclic or polycyclic ring system of about 3 to about 20 carbon atoms, or 3 to about 6 carbon atoms, such as cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, perhydronaphthyl, adamantyl, and norbornyl groups, bridged cyclic or spiro bicyclic groups, such as spiro-(4,4)-non-2-yl, and the like, optionally containing one or more heteroatoms, such as, for example, O and N. The three oxazoline-containing hydroxyl groups may be the same or different and may be provided at any point of attachment to the cycloalkyl molecule.

[0059] In another exemplary embodiment, the tetrafunctional polyoxazoline polyol is a C1-C aryloxy group-containing polyoxazoline having four oxazoline-containing hydroxyl groups per alkyl molecule, the alkyl molecule optionally containing one or more of an ether linkage and / or an ester linkage. 12 Alkyl polyoxazoline polyols, C6-C, with four oxazoline-containing hydroxyl groups per aromatic molecule 30 Aromatic polyoxazoline polyols, C3-C oxazoline-containing hydroxyl groups per cycloalkyl molecule 20 In one embodiment, the aryl group is phenyl. 12 Alkyl molecules, C6-C 30 aromatic molecules, and C3~C 20 The cycloalkyl moiety can be any of those described above. In an exemplary embodiment, the four oxazoline-containing hydroxyl groups can be the same or different and can be provided at any point of attachment to the alkyl moiety, the aromatic moiety, and the cycloalkyl moiety.

[0060] One or more of the polyoxazoline polyols described above having a weight average molecular weight of about 1000 Daltons or greater can be prepared by methods known in the art.

[0061] In one embodiment, the one or more polyoxazoline polyols are For example, bromo-containing initiator (A-2) (Br) a -Z (A-2) (wherein Z is a hydrocarbyl group and a is an integer from 2 to 4) to form a 2-substituted-2-oxazoline (A-1) [ka] to catalytic ring-opening polymerization, followed by reaction of the resulting product with a water / sodium carbonate mixture or other suitable terminating agent to prepare a polyoxazoline polyol. The Z hydrocarbyl group of the bromo-containing initiator can be any C1-C 30 Alkyl groups, C6-C 30 Aromatic group, C3~C 20 Cycloalkyl, C1-C 20 Ester-containing groups, C1-C 20 It may be a polyether-containing group, etc. 30 Alkyl groups, C6-C 30 Aromatic group, C3~C 20 Cycloalkyl, C1-C 20 Ester-containing groups, and C1-C 20 The polyether-containing group can be any of those described herein above. Suitable terminating agents other than water / sodium carbonate mixtures can be used, including, for example, glycolic acid, lactic acid, ethylene glycol, propylene glycol, and the like, in the presence of a base such as triazabicyclodecene.

[0062] In an exemplary embodiment, the one or more polyoxazoline polyols described above can be obtained by subjecting a 2-substituted-2-oxazoline (A-1) to a catalytic ring-opening polymerization process as shown below. [ka]

[0063] In another exemplary embodiment, the one or more polyoxazoline polyols described above can be obtained by subjecting a 2-substituted-2-oxazoline (A-1) to a catalytic ring-opening polymerization process as shown below. [ka]

[0064] Thus, suitable alkyl substituted oxazolines for use herein are of the formula: [ka] In an exemplary non-limiting embodiment, the 2-alkyl substituted oxazoline for use herein is 2-isopropenyl-2-oxazoline. Thus, in an exemplary embodiment, the poly(2-alkyloxazoline) repeat unit as shown above in the catalytic ring-opening polymerization process is represented by the following: [ka]

[0065] where R is an alkyl group of 1 to 12 carbon atoms.

[0066] The one or more polyoxazoline polyols may be present in the mixture in an amount ranging from about 5 to about 65 weight percent, based on the total weight of the mixture. In an exemplary embodiment, the amount of the one or more polyoxazoline polyols in the mixture may range from about 10 to about 45 weight percent, based on the total weight of the mixture.

[0067] In an exemplary embodiment, the mixture further contains a catalyst for carrying out the reaction to prepare the polymerization product. Suitable urethane catalysts include, for example, stannous salts of carboxylic acids such as stannous octoate, stannous oleate, stannous acetate, and stannous laurate, dialkyltin dicarboxylates such as dibutyltin dilaurate and dibutyltin diacetate (which are known in the art as urethane catalysts and as tertiary amines), and tin mercaptides.

[0068] The amount of catalyst used is generally from about 0.005 to about 5 weight percent of the mixture being catalyzed, depending on the nature of the isocyanate.

[0069] The mixture may further contain other monomers. In an exemplary embodiment, the mixture may further include one or more antioxidants. Suitable antioxidants may be any of those commonly used in polyurethanes, such as, for example, BHA (butylated hydroxyl anisole), BHT (butylated hydroxytoluene), and ascorbic acid. The one or more antioxidants may be used in an amount of about 0.01 to about 10 weight percent, or about 0.1 to about 5 weight percent, or about 0.2 to about 1 weight percent, based on the total weight of the mixture.

[0070] In another exemplary embodiment, the mixture may further comprise one or more end-functionalized surfactants. Suitable end-functionalized surfactants include, by way of example, poloxamers, such as the Pluronics and reverse Pluronics, and poloxamines, such as the Tetronics and reverse Tetronics described above.

[0071] Poloxamers and reverse poloxamers have terminal hydroxyl groups that can be end-functionalized. One example of an end-functionalized poloxamer is poloxamer dimethacrylate (e.g., Pluronic® F127 dimethacrylate), disclosed in U.S. Patent Application Publication No. 2003 / 0044468. Other examples include glycidyl-terminated copolymers of polyethylene glycol and polypropylene glycol, disclosed in U.S. Patent No. 6,517,933.

[0072] The poloxamers and / or poloxamines can be functionalized to provide the desired reactivity at the ends of the molecules. The functionality can vary and is determined based on the intended use of the functionalized PEO- and PPO-containing block copolymers. That is, the PEO- and PPO-containing block copolymers are reacted to provide terminal functionality complementary to the intended device-forming mixture.

[0073] Representative examples of reaction sequences by which the PEO- and PPO-containing block copolymers can be end-functionalized are set forth below. [ka]

[0074] The above reaction sequences are merely illustrative and non-limiting examples of reactions that provide functionalized ends for PEO- and PPO-containing block copolymers. It should be understood that one skilled in the art can determine other reaction methods without undue experimentation. It should also be understood that any particular block copolymer molecule shown is only one chain length of a polydispersed population of the referenced material.

[0075] In one embodiment, the end-functionalized surfactant is selected from the group consisting of a poloxamer having at least one end end that is end-functionalized, a reverse poloxamer having at least one end end that is end-functionalized, a poloxamine having at least one end end that is end-functionalized, a reverse poloxamine having at least one end end that is end-functionalized, and mixtures thereof.

[0076] Generally, the end-functionalized surfactant will be present in the mixture in an amount ranging from about 0.01 to about 20 weight percent, or from about 1 to about 10 weight percent, or from about 3 to about 6 weight percent, based on the total weight of the mixture.

[0077] The mixture may further contain, if necessary, various additives, such as one or more ultraviolet (UV) blocking agents, colorants, lubricating internal wetting agents, and reinforcing agents, as well as other components well known in the art, within the limits that do not impair the purpose and effect of the exemplary embodiments disclosed herein.

[0078] Exemplary embodiment biomedical devices, such as contact lenses or intraocular lenses, can be prepared by polymerizing the above-described mixture to form a product that can then be formed into the appropriate shape by lathing, injection molding, compression molding, cutting, etc. For example, in manufacturing contact lenses, the initial mixture may be polymerized in a tube to provide rod-shaped articles that are then cut into buttons. The buttons may then be lathed into contact lenses.

[0079] Alternatively, biomedical devices such as contact lenses may be cast directly from the mixture into a mold, e.g., a polypropylene mold, by, for example, spin casting and static casting. Spin casting is disclosed in U.S. Pat. Nos. 3,408,429 and 3,660,545, and static casting is disclosed in U.S. Pat. Nos. 4,113,224, 4,197,266, and 5,271,875. Spin casting involves filling a mold with the mixture to be polymerized and rotating the mold in a controlled manner while exposing the mixture to a radiation source such as UV light. Static casting involves casting the mixture between two mold sections, one mold section shaped to form the anterior surface of the lens and the other mold section shaped to form the posterior surface of the lens, and curing the mixture while held in the mold assembly to form the lens. No. 5,271,875 describes a static casting method that allows for the molding of a finished lens in a mold cavity defined by a posterior mold and an anterior mold.As an additional method, U.S. Pat. No. 4,555,732 discloses a process in which an excess of a monomer mixture is cured by spin casting in a mold to form a molded article having a lens anterior surface and a relatively large thickness, and the posterior surface of the cured spin cast article is subsequently lathed to provide a contact lens having a desired thickness and lens posterior surface.

[0080] The polymerization can be carried out in a reaction medium, such as a solution or dispersion using a suitable solvent. Generally, the polymerization can be carried out for about 15 minutes to about 72 hours. If desired, the resulting polymerization product can be dried under high vacuum, for example, for about 5 to about 72 hours, or left in an aqueous solution before use.

[0081] Polymerization of the mixture results in a polymer that, when hydrated, preferably forms a hydrogel. When producing hydrogel lenses, the mixture may further include at least a diluent (e.g., a PEG-ether diluent) that is ultimately replaced by water when the polymerization product is hydrated to form a hydrogel. The maximum amount of diluent that can be used will depend on the amount of swelling that the diluent causes in the final polymer. Excessive swelling may cause or disintegrate the copolymer when the diluent is replaced by water upon hydration. In general, the water content of the hydrogel is as described herein above. The amount of diluent used should be less than about 50 weight percent, and in most cases the diluent content is less than about 30 weight percent. However, for a particular polymer system, the practical limit will be dictated by the solubility of the various monomers in the diluent. To produce an optically clear copolymer, it is important that no phase separation occurs between the comonomer and the diluent, or between the diluent and the final copolymer, which would cause visual opacity.

[0082] It may be desirable to remove residual diluent from the lens prior to the edge finishing operation, which can be accomplished by evaporation at or near ambient pressure, or under high vacuum, if desired. High temperatures can be used to reduce the time required to evaporate the diluent. The time, temperature, and pressure conditions for the solvent removal step will vary depending on factors such as the volatility of the diluent and the particular monomeric components, as can be readily determined by one of ordinary skill in the art. If desired, the mixture used to make the hydrogel lens may further include crosslinkers and wetting agents known in the prior art for making hydrogel materials.

[0083] The biomedical devices, such as contact lenses obtained herein, may be subjected to optional machining operations. For example, other optional machining steps may include buffing or polishing of the lens edges and / or surfaces. In general, such machining processes may be performed before or after the product is released from the mold parts, for example, the lens is dry demolded from the mold by lifting the lens from the mold with high vacuum tweezers, after which the lens is transferred by mechanical tweezers to a second set of high vacuum tweezers and placed against a rotating surface to smooth the surface or edges. The lens may then be flipped over to machine the other side of the lens.

[0084] The lenses may then be transferred to individual lens packages containing a buffered saline solution. Saline may be added to the package either before or after transfer of the lenses. Suitable package designs and materials are known in the art. The plastic package is peelably sealed with a film. Suitable sealing films are known in the art and include foils, polymeric films, and mixtures thereof. The sealed package containing the lenses is then sterilized to ensure a sterile product.

[0085] As one of ordinary skill in the art would readily appreciate, other steps can be included in the above-described molding and packaging process, including, for example, coating the formed lenses, surface treating the lenses during formation (e.g., via mold transfer), inspecting the lenses, discarding defective lenses, cleaning mold halves, reusing mold halves, and the like, as well as combinations thereof.

[0086] The following examples are provided to enable one of ordinary skill in the art to practice the invention and are merely illustrative and should not be construed as limiting the scope of the invention, which is defined in the claims.

[0087] Example 1 A polyoxazoline having a number average molecular weight of 400 Daltons and a weight average molecular weight of 1900 Daltons was prepared according to the following reaction scheme. [ka]

[0088] To a flame-dried, two-necked, 250 mL round-bottom flask equipped with a stopper, stir bar, and condenser was added via syringe 2-ethyl-2-oxazoline (25 mL), ethylene glycol bis(2-bromoprionate) (0.568 grams), and acetonitrile (55 mL). The flask was filled with N 2(g) The mixture was placed in an oil bath at 80° C. under reduced pressure and stirred overnight. The reaction was quenched by adding sodium bicarbonate (0.12 grams) and deionized (DI) water (0.2 mL) and stirred for 1 hour. The resulting polymer was precipitated into approximately 1500 mL of diethyl ether, filtered, and dried in a high vacuum oven.

[0089] Example 2 A polyoxazoline having a number average molecular weight of 5,000 daltons was prepared according to the following reaction scheme. [ka]

[0090] To a flame-dried, two-necked, 250 mL round-bottom flask equipped with a stopper, stir bar, and condenser was added via syringe 2-ethyl-2-oxazoline (25 mL), α,α'-dibromo-p-xylene (0.45 grams), and acetonitrile (55 mL). The flask was filled with N 2(g) The mixture was placed in an oil bath at 80° C. under reduced pressure and stirred overnight. The reaction was quenched by adding sodium bicarbonate (0.12 grams) and DI water (0.2 mL) and stirred for 1 hour. The resulting polymer was precipitated into approximately 1500 mL of diethyl ether, filtered, and dried in a high vacuum oven.

[0091] Example 3 A polyoxazoline having a number average molecular weight of 700 Daltons and a weight average molecular weight of 7700 Daltons was prepared according to the following reaction scheme. [ka]

[0092] To a flame-dried, two-necked, 250 mL round-bottom flask equipped with a stopper, stir bar, and condenser was added 2-ethyl-2-oxazoline (25 mL), 1,6-dibromohexane (0.26 mL), and acetonitrile (55 mL) via syringe. The flask was filled with N 2(g) The mixture was placed in an oil bath at 80° C. under reduced pressure and stirred overnight. The reaction was quenched by adding sodium bicarbonate (0.12 grams) and DI water (0.2 mL) and stirred for 1 hour. The resulting polymer was precipitated into approximately 1500 mL of diethyl ether, filtered, and dried in a high vacuum oven.

[0093] Example 4 A polyoxazoline having a number average molecular weight of 800 Daltons and a weight average molecular weight of 14400 Daltons was prepared according to the following reaction scheme. [ka]

[0094] To a flame-dried, two-necked, 250 mL round-bottom flask equipped with a stopper, stir bar, and condenser was added via syringe 2-ethyl-2-oxazoline (25 mL), 1,2,5,6-tetrakis(bromomethyl)benzene (0.77 grams), and acetonitrile (55 mL). The flask was flushed with N 2(g) The mixture was placed in an oil bath at 80° C. under reduced pressure and stirred overnight. The reaction was quenched by adding sodium bicarbonate (0.12 grams) and DI water (0.2 mL) and stirred for 1 hour. The resulting polymer was precipitated into approximately 1500 mL of diethyl ether, filtered, and dried in a high vacuum oven.

[0095] Example 5 A polyoxazoline having a number average molecular weight of 4,900 daltons and a weight average molecular weight of 9,135 daltons was prepared according to the following reaction scheme. [ka]

[0096] To a flame-dried, two-necked, 250 mL round bottom flask was added 4,4'-bis(bromomethyl)biphenyl (0.54 g, 0.0016 mol) and 20 mL of anhydrous acetonitrile. 2-Ethyl-2-oxazoline (24.55 g, 0.2476 mol) was then added via syringe. The flask was placed in a preheated oil bath at 80° C. for approximately 6 hours to form the polymer in ether and then cooled. Glycolic acid (2.20 g, 0.037 mol) and triethylamine (1.24 g, 0.012 mol) were added sequentially and placed in a preheated oil bath at 50° C. overnight. Additional solvent (approximately 5 mL) was added to keep the reaction stirring.

[0097] The mixture was cooled, diluted with dichloromethane (400 mL) and washed with saturated aqueous sodium bicarbonate (2×300 mL) and saturated aqueous sodium chloride (1×300 mL). The combined bicarbonate extracts were back-extracted with 1×400 mL of dichloromethane. The combined organics were dried over magnesium sulfate and evaporated. Dichloromethane (ca. 100 mL) was then added to the residue and precipitated in ether. The polymer was collected, dried, redissolved in dichloromethane and precipitated in ether. The solid was filtered, rinsed and dried at room temperature in a household high vacuum oven for several days. A white solid (18.60 g) (76%) was recovered.

[0098] Example 6 Preparation of polyoxazoline-based silicone-containing polyurethanes.

[0099] To a flame-dried, two-necked, 250 mL round bottom flask equipped with a stopper, stir bar, addition funnel, and condenser, under nitrogen to maintain a dry environment, was added the polyoxazoline polymer of Example 2 (6.43 grams) and 1,2-dichloroethane (76 mL / 100 grams of mixture). After the polymer was dissolved, Silsurf® 2510 (45.89 grams), triethylene glycol (13.14 grams), and dibutyltin dilaurate (0.05 grams) were added. The flask was placed in a heated oil bath (80° C.) and stirred to combine the ingredients. Next, 4,4′-methylenebis(cyclohexyl isocyanate) (34.50 grams) was added via syringe. The reaction mixture was stirred under nitrogen for at least 2 hours while maintaining the temperature at 80° C. The reaction mixture was then cooled to room temperature and poured onto a treated glass plate to produce a thin film. The solvent was allowed to evaporate overnight in a hood.

[0100] For the sake of brevity, various features disclosed herein are described in the context of a single embodiment, but may also be provided separately or in any suitable subcombination.All combinations of the embodiments are specifically encompassed by the exemplary embodiments disclosed herein, as if each and every combination were individually and expressly disclosed herein.In addition, all subcombinations listed in the embodiments that describe such variables are also specifically encompassed by the formulation, and are disclosed herein, as if each and every such subcombination were individually and expressly disclosed herein.

[0101] It will be understood that various modifications can be made to the embodiments disclosed herein. Therefore, the above description should not be interpreted as limiting, but only as an example of a preferred embodiment. For example, the functions implemented as the best mode for operating the embodiments disclosed herein, described above, are for illustrative purposes only. Those skilled in the art can implement other configurations and methods without departing from the scope and spirit of the present invention. Moreover, those skilled in the art will envision other modifications within the scope and spirit of the features and advantages added herein.

Claims

1. a biomedical device that is a polymerization product of the mixture, (a) one or more difunctional isocyanates; (b) one or more polyalcohols; (c) one or more hydroxy-terminated polysiloxane prepolymers; and (d) one or more polyoxazoline polyols having a weight average molecular weight of 1000 Daltons or greater.

2. the one or more difunctional isocyanates include aliphatic isocyanates, cycloaliphatic isocyanates, and aromatic isocyanates; 10. The biomedical device of claim 1, wherein said one or more polyalcohols have 2 to 50 carbon atoms and at least two hydroxy groups.

3. The one or more difunctional isocyanates are represented by the formula OCN-R 1 —NCO, wherein R 1 is a linear or branched chain C 3 ~C 18 - alkylene group, unsubstituted or substituted C 6 ~C 10 - an arylene group, unsubstituted or substituted C 7 ~C 18 -aralkylene group, C 6 ~C 10 -Arylene-C 1 ~C 2 -Alkylene-C 6 ~C 10 - an arylene group, C 3 ~C 8 -cycloalkylene group, C 3 ~C 8 -Cycloalkylene-C 1 ~C 6 - alkylene group, C 3 ~C 8 -Cycloalkylene-C 1 ~C 6 -Alkylene-C 3 ~C 8 -cycloalkylene group, or C 1 ~C 6 -Alkylene-C 3 ~C 8 -cyclo-alkylene-C 1 ~C 6 - is an alkylene group, 3. The biomedical device of claim 1 or 2, wherein the one or more polyalcohols are selected from the group consisting of diols, triols, tertiary amine polyalcohols, alkoxylated polyalcohols, polyether polyalcohols, and mixtures thereof.

4. The one or more hydroxy-terminated polysiloxane prepolymers have the formula: 【V】 wherein each R, R 1 , R 2 , R 3 and R 4 4. The biomedical device of any one of claims 1 to 3, wherein groups independently represent H or a hydrocarbyl group, p is an integer from 0 to 40, q is an integer from 0 to 40, z is an integer from 2 to 50, u is an integer from 1 to 100, y is an integer from 0 to 40, w is an integer from 0 to 40, and v is an integer from 2 to 50, and each Q group independently represents a hydroxyl-containing reactive functional end group.

5. 5. The biomedical device of any one of claims 1 to 4, wherein the one or more polyoxazoline polyols comprise one or more di-, tri-, and tetra-functional polyoxazoline polyols.

6. The one or more polyoxazoline polyols have the formula: 【Chemical VI】 6. The biomedical device of any one of claims 1-5, wherein each R is a hydroxyl group, each R' is independently an alkyl group, a haloalkyl group, an alkene group, an alkyne group, a cycloalkyl group, a halocycloalkyl group, an aryl group, a haloaryl group, an aralkyl group, and a haloaralkyl group, Z is a divalent bond, and each of x and y is independently at least 1.

7. The mixture is (a) 20 to 60 weight percent of the one or more difunctional isocyanates, based on the total weight of the mixture; (b) 10 to 70 weight percent of said one or more polyalcohols, based on the total weight of the mixture; (c) 3 to 60 weight percent of said one or more hydroxy-terminated polysiloxane prepolymers, based on the total weight of said mixture; 7. The biomedical device of any one of claims 1-6, comprising: (d) 5 to 65 weight percent of the one or more polyoxazoline polyols having a weight average molecular weight of 1000 Daltons or greater, based on the total weight of the mixture.

8. The biomedical device according to any one of claims 1 to 7, which is one of a contact lens or an intraocular lens.

9. The biomedical device of any one of claims 1 to 8, wherein the polymerization product is a thermosetting polymerization product.

10. 1. A method of making a biomedical device, the method comprising: (a) providing a mixture comprising: (i) one or more difunctional isocyanates; (ii) one or more polyalcohols; (iii) one or more hydroxy-terminated polysiloxane prepolymers; and (iv) one or more polyoxazoline polyols having a weight average molecular weight of 1000 Daltons or greater; (b) subjecting the mixture to polymerization conditions to provide a polymerized device; (c) hydrating the polymerized device.