PEM electrolysis cells for high-pressure hydrogen production by differential pressure electrolysis and frames for PEM electrolysis cell stacks
The frame design for PEM electrolysis cells, featuring coated anode and cathode frames with integrated flow channels, addresses airtightness and stability issues, enabling high-pressure operation with a hermetic seal and reduced component count, enhancing efficiency and cost-effectiveness.
Patent Information
- Application Number
- JP2024522459
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-04-27
- Filing Date
- 2022-10-12
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2042-10-12
AI Technical Summary
Classical PEM electrolysis cells face challenges with airtightness due to manufacturing tolerances, mechanical stability issues leading to frame deformation, and the formation of gaps between components, which compromise sealing under high or differential pressures, and the need for additional channels increases costs.
A frame design for PEM electrolysis cells with an anode and cathode frames coated with a sealing material, featuring a step for supporting the catalyst-coated membrane and integrated flow channels, ensuring mechanical stability and sealing efficacy without deformation under high pressures.
The frame design provides a hermetic seal and mechanical stability, allowing operation under high differential pressures up to 40 bar while reducing component count and assembly complexity, and enabling the use of thinner membranes, thus enhancing efficiency and reducing manufacturing costs.
Smart Images

Figure 2024536518000001_ABST
Abstract
Description
[Technical field]
[0001] The invention relates to a novel frame for a PEM electrolysis cell and a frame for a PEM electrolysis cell stack. The object of the invention is a frame according to the invention, a PEM electrolysis cell according to the invention and a PEM electrolysis cell stack according to the invention (= stack-type PEM electrolyzer), which comprises a frame according to the invention, a pre-assembled module, a method for manufacturing a pre-assembled module and a method for manufacturing a PEM electrolysis cell stack. The frame according to the invention, the PEM electrolysis cell according to the invention and the PEM electrolysis cell stack according to the invention are suitable for the production of high-pressure hydrogen by differential pressure electrolysis in combination with the use of thin proton exchange membranes. The invention is based on a new frame and seal concept. The invention also relates to a cover for a stack-type PEM electrolyzer.
[0002] Proton exchange membrane (PEM) water electrolysis is an attractive technology to produce hydrogen using electricity from renewable energy sources. This means that the energy of the energy carrier hydrogen can be stored in case the electricity available from renewable sources is not sufficient, thus contributing to decarbonization. An important advantage of PEM electrolysis is that hydrogen can be produced under pressure. For all potential applications, hydrogen must be available in compressed form. This means that PEM systems (such as PEM electrolysis cells and PEM electrolysis cell stacks) are particularly suited to the needs of industry. To save energy, it is advantageous to carry out PEM electrolysis directly under pressure. As usually only hydrogen is used, oxygen can be produced cheaply without pressure, which is called differential pressure electrolysis. A differential pressure of at least 30 bar is the current state of the art, but this is currently only possible with electrolyte membranes at least about 120 μm thick.
[0003] To produce as much hydrogen as possible with the available electricity, the efficiency of the PEM electrolysis cell is of utmost importance. A significant part of the energy loss is caused especially by the ohmic resistance of the electrolyte membrane. Catalyst-coated membranes (CCMs) are used for the PEM membranes. By using thin PEM membranes, the membrane resistance can be significantly reduced.
[0004] The classical structure of a PEM electrolysis cell is shown in Figure 1.
[0005] A classical PEM electrolyser consists of a catalyst-coated membrane (CCM) where the reaction takes place. On the anode and cathode sides, porous transport layers (PTLs) transport water towards the CCM and porous transport layers (PTLs) transport the product gas away from the CCM. Bipolar plates (BPPs) spatially separate the anode and cathode sides. The inflow and outflow of gas and water is ensured by a frame made of conventional metal or high-strength plastic (PEEK). The CCM and PTL components are inserted into this frame. The frame is laterally sealed by O-rings or other seals such as flat gaskets or injection seals, which prevent gas from exiting the PEM electrolysis cell.
[0006] PEM electrolysis cell stacks, consisting of PEM electrolysis cells and frames, are known in the art.
[0007] US 6,669,826 B1 discloses a method for achieving sealing of a PEM electrolysis cell stack by applying uniform contact pressure to the electrolysis cells, in which sub-stacks, each consisting of a number of PEM electrolysis cells arranged in series in a bipolar configuration, are compressed with the aid of end plates, intermediate supports, tie rods and prestressing means.
[0008] US 6,852,441 B1 discloses stabilizing the frame of a PEM electrolysis cell in an electrolysis cell stack by means of a reinforcing element surrounding the periphery of the electrolysis cell stack.
[0009] EP 1 356 134 B1 discloses a frame for PEM electrolysis cells, in which the electrolysis cells are compactly stacked in a bipolar arrangement, the stacked frames being separated by a partition wall. The frame has two opposing planar faces and an opening through which the membrane is held in the frame by thermocompression of polyphenylene oxide strips, as well as holes for the inlet of the electrolyte and the outlet of the product gas. The gas and electrolyte are sealed by sealing rings, and the stack is sealed by sealing rings located in grooves in each frame. To maintain the integrity of the sealing rings between adjacent frames in the stack against internal pressure, the PEM electrolysis cell stack is enclosed and compressed between two stainless steel plates held together by a threaded connecting rod.
[0010] US 8,282,811 B2 discloses an electrolysis cell for generating hydrogen at high pressure, in which a frame is placed between the membrane electrode assembly and a separator acting as a hydrogen or oxygen separator, with openings for the flow of water, oxygen and hydrogen. A gasket seals the frame to the separator, and the membrane seals the frame on the opposite side. Pressure pads between adjacent separators and a plastic manifold gasket surrounding the pressure pads seal the openings between the individual electrolysis cells in the stack.
[0011] US 7,507,493 B2 discloses a PEM electrolysis cell including a bipolar plate with a seal. The seal is arranged between the frame and the end of the porous gas diffusion layer. Furthermore, the electrolysis cell is provided with a protection element between the seal and the membrane electrode arrangement to protect the proton exchange membrane. This should enable the cell to operate at sustained high pressures, low resistivity and improved creep protection.
[0012] US 8,349,151 B2 discloses frames for use as anode and cathode frames of water electrolyzers, the anode and cathode frames being of identical construction and consisting of a universal cell frame having a central opening and a plurality of lateral openings, where mating sets of lateral openings are spaced approximately 90 degrees or 180 degrees apart and each are fluidly connected or disconnected to the central opening by at least one internal radial passage, the anode and cathode frames being rotated 90 degrees relative to each other such that a series of electrolyzers are fluidly interconnected through the openings.
[0013] EP 3 462 528 A1 discloses an electrochemical cell for high pressure hydrogen production comprising a membrane electrode arrangement and a flow structure having flat surfaces on either side of the membrane electrode arrangement, one flat surface being larger than the other, a bipolar plate, a reinforcing layer and a seal having a sealing ring arranged between the bipolar plate and the electrolyte membrane adjacent to the flow structure having the smaller surface.
[0014] DE 10 2014 010 813 A1 discloses a frame for a stacked electrolyser for producing high pressure hydrogen, which frame comprises an integrated reinforcement disposed between a fluid guide and an outer edge, embedded in the frame structure, and a recess disposed radially between the reinforcement and the fluid guide for receiving a seal.
[0015] EP 3 699 323 A1 relates for example to electrode supplies for electrode stacks of electrolytic cells.
[0016] DE 25 33 728 A1 relates to an electrolysis cell with bipolar electrodes arranged side by side and an outer frame which surrounds at least one chamber of the electrolysis cell.
[0017] EP 3 770 303 A1 relates to an electrode packing unit for a stack structure of an electrochemical reactor comprising a bipolar plate, two electrode plates and two current transfer structures arranged between the bipolar plate and the electrode plates.
[0018] WO 2020 / 039218 A1 relates to a stacked electrolysis device for the electrolysis of water having a cathode plate, an anode plate, an electrolysis stack, end plates and a flow channel sealing arrangement.
[0019] US 202009906 A1 relates to a catalytically coated membrane for a water electrolyzer.
[0020] Difficulties commonly encountered with classical PEM electrolysis cells include: 1. In PEM electrolysis cell stacks, i.e. stack-type PEM electrolysis equipment, the frames of many PEM electrolysis cells are stacked, and airtightness is an issue because each material used for the frame and other parts has manufacturing tolerances. As a result, the O-rings and other seals used may not have sufficient contact pressure at some points on the frame. Especially when hydrogen is produced under pressure or differential pressure, it is difficult or impossible for known seals to achieve tightness. 2. Mechanical stability of the frame When high-pressure hydrogen is generated, the plastic frame will deform (Figure 2). 3. A small gap 17 remains between the PTL and the frame 1. The CCMs 13 are forced into this gap 17 in a compression mode. This results in the CCMs 13 creeping out 24 into the gap 17 (so-called viscoelastic behavior). If the frame 1 is deformed due to its low mechanical stability (see point 2), this effect is intensified and the gap 17 becomes larger (Figure 2). 4. The frame has channels for the supply and removal of water and gas. The channels are cut out of the frame, i.e. from metal or plastic parts, which increases the cost.
[0021] In order to produce industrial hydrogen at high pressure using PEM electrolysis, an improved PEM electrolysis cell is needed that can operate under high and differential pressures and that does not suffer from the drawbacks mentioned above.
[0022] This problem is solved by the invention according to claims 1 to 21.
[0023] The subject of the invention is a frame 1 for a PEM electrolysis cell 2 for a stacked type 23 PEM electrolysis apparatus, the frame 1 comprising a first side 4 having a planar first surface, a second side 5 opposite the first side 4 having a planar second surface, an anode frame 8 and a cathode frame 11. Here, the anode frame comprises a first side 4, an opposite side of the anode frame 4″ from the first side 4, and a first opening 6 for receiving a porous transport layer (PTL) anode 7, the first opening 6 extending from the first side 4 to the opposite side of the anode frame 4″. Here, the cathode frame 11 has a second side 5, a side of the cathode frame 5″ opposite the second side 5, and a second opening 9 for receiving a PTL cathode 10, the second opening 9 extending from the second side 5 to the opposite side of the cathode frame 5″. Here, a side surface of the anode frame 4″ facing the first side surface 4 and a side surface of the cathode frame 5″ facing the second side surface 5 are disposed adjacent to each other. The anode frame 8 and the cathode frame 11 are connected to each other. Here, the first opening 6 and the second opening 9 are connected to each other. Here, the first opening 6 is larger than the second opening 9, and the anode frame 8 and the cathode frame 11 are arranged such that the side facing the first side 4 of the anode frame 4'' and the side facing the second side 5 of the cathode frame 5'' form a step 12 at the transition from the anode frame 8 to the cathode frame 11.
[0024] In the frame 1 according to the invention, the step 12 is preferably part of the cathode frame 11. In the frame 1 according to the invention, the step 12 is preferably adjacent to the second opening 9. In the frame 1 according to the invention, the step 12 preferably borders the second opening 9. In the frame 1 according to the invention, the step 12 preferably forms a planar third surface as a support surface for the catalyst coated membrane (CCM) 13. In the frame 1 according to the invention, the step 12 is preferably part of the cathode frame 11 and forms a planar third surface as a support surface for the membrane 13. In the frame 1 according to the invention, the step 12 is preferably part of the cathode frame 11 and forms a planar third surface adjacent to the second opening 9, borders the second opening 9 and forms a planar third surface as a support surface for the catalyst coated membrane (CCM) 13.
[0025] The anode frame 8 comprises a core 21 and a coating of a seal material 22. Preferably, the anode frame 8 comprises a core 21 of metal or other suitable material, preferably the anode frame 8 comprises a coating of a seal material 22, which is preferably rubber (= core 21 with a coating of rubber). The cathode frame 11 comprises a core 21 and a coating of a seal material 22. Preferably, the cathode frame 11 comprises a core 21 of metal or other suitable material, and a coating of a seal material 22, which is preferably rubber (= core 21 with a coating of rubber). As a coating of the metallic core 21 any seal material is suitable, for example rubber, in particular ethylene propylene diene rubber (EPDM). The coating of the seal material 22 is preferably a seal or serves as a seal of the PEM electrolysis cell 2 or of the stacked PEM electrolysis device 23.
[0026] The subject of the invention is a frame 1 for a PEM electrolysis cell 2 with a core 21, preferably made of metal, which is covered with a sealing material, preferably rubber, for example EPDM (Figures 3a and 3b). The core 21 of the anode frame 8 is completely or partially covered with a sealing material 22, in particular a seal. The core 21 of the cathode frame 11 is completely or partially covered with a sealing material 22, in particular a seal. As a sealing material any sealing material is suitable, for example rubber, in particular ethylene propylene diene rubber (EPDM). For example, the seal consists of EPDM or consists of EPDM.
[0027] The core 21 of the anode frame 8 is preferably made of or consists of metal. The core 21 of the cathode frame 11 is preferably made of or consists of metal. A metallic core 21 provides good mechanical stability. Alternatively, other materials with similar mechanical properties can be used for the core 21, for example polytetrafluoroethylene (PTFE), in particular reinforced PTFE or molecular reinforced PTFE. The sealant 22, preferably a coating made of rubber, for example ethylene propylene diene rubber (EPDM), creates a sealing effect, i.e. the sealant acts as a seal.
[0028] In a preferred embodiment, the entire surface of the core 21 of the anode frame 8 is covered with a coating of the seal material 22. In a further preferred embodiment, at least 90%, preferably at least 95% or more of the surface of the core 21 of the anode frame 8 is covered with a coating of the seal material 22. In a preferred embodiment, the entire surface of the core 21 of the cathode frame 11 is covered with a coating of the seal material 22. In a further preferred embodiment, at least 90%, preferably at least 95% or more of the surface of the core 21 of the cathode frame 11 is covered with a coating of the seal material 22. In these embodiments, the sealing surface is very large.
[0029] In alternative embodiments, less than 90% of the surface of the core 21 of the anode frame 8 is covered with a coating of the sealant 22. In further alternative embodiments, less than 90% of the surface of the core 21 of the cathode frame 11 is covered with a coating of the sealant 22. However, in these alternative embodiments, the area of the surface of the core 21 of the anode frame 8 and / or the core 21 of the cathode frame 11 is covered with a coating of the sealant 22 necessary to provide a complete seal of the PEM electrolysis cell 2. Preferably, in these alternative embodiments, at least the area of the surface of the core 21 of the anode frame 8 and / or the core 21 of the cathode frame 11 surrounding the first opening 6 and / or the second opening 9 is covered with a coating of the sealant 22. For example, an area of 0.5 cm to 2.5 cm, preferably 1 cm to 2 cm, e.g. 1.5 cm, of the surface of the core 21 of the anode frame 8 directly surrounding the first opening 6 (see Figures 10b to 10d and 14). For example, the area of the surface of the core 21 of the cathode frame 11 immediately surrounding the second opening 9 is 0.5 cm to 2.5 cm, preferably 1 cm to 2 cm, for example 1.5 cm.
[0030] The metal provides good mechanical stability, while the sealing material 22, preferably a coating made of rubber, for example EPDM, provides the sealing effect. The fact that preferably the entire or at least 90%, for example at least 95% or more of the surface of the metallic core 21 of the anode frame 8 or preferably the entire or at least 90%, for example at least 95% or more of the surface of the metallic core 21 of the cathode frame 11 is covered with a sealing material, preferably rubber, for example EPDM, means that the sealing surface is very large.
[0031] A further advantage of the coating, e.g. made of a metal stable core 21 and sealant 22, is that components such as the PTL anode 7 and the PTL cathode 10 can be press-fitted into the frame 1, in particular the anode frame 8 and the cathode frame 11, so that during electrolysis under high pressure or differential pressure, e.g. up to 40 bar differential pressure, in the PEM electrolysis cell 2 or stacked PEM electrolyser 23, there is no deformation of the frame 1 and no larger gaps 17 are formed between the individual components in the frame 1, e.g. between the PTL cathode 10 and the frame 1 and / or between the PTL anode 7 and the frame 1 (Figure 8).
[0032] The metal used for the core 21 of the anode frame 8 and / or the cathode frame 11 can be stainless steel, for example stainless steel with a thickness of 0.5 mm. The thickness of the coated core 21 of the anode frame 8, i.e. the coating consisting of the core 21 and the sealant 22, combined, can be 1-5 mm, preferably 2-3 mm, for example 2.2 mm. The thickness of the coated core 21 of the cathode frame 11, i.e. the coating consisting of the core 21 and the sealant 22, combined, can be 1-5 mm, preferably 2-3 mm, for example 2.2 mm. Materials with comparable properties are also suitable for the core 21, for example highly reinforced plastics, for example PTFE, molecular reinforced PTFE.
[0033] The coating made of the seal material 22 has a thickness. The thickness of the coating made of the seal material 22 is, for example, 1 to 4.5 mm, for example, 2 to 3 mm. Preferably, the thickness of the coating made of the seal material 22 surrounding the core 21 of the anode frame 8 is the same everywhere. Preferably, the thickness of the coating made of the seal material 22 surrounding the core 21 of the positive electrode frame 11 is the same everywhere. In a specific embodiment, the core 21 of the anode frame 8 has a region 22'' in which the thickness of the coating made of the seal material 22 is reduced compared to the thickness of the coating made of the seal material 22 (Figures 10b to 10d, Figure 14). In a specific embodiment, the core 21 of the positive electrode frame 11 has a region in which the thickness of the coating made of the seal material 22 is reduced compared to the thickness of the coating made of the seal material 22''. For example, the thickness of the coating made of the seal material 22''. The thickness of the coating made of the seal material 22 is reduced by 1 mm compared to the thickness of the coating made of the seal material 22. For example, the thickness of the coating made of the sealing material 22 is 4 mm, and the reduced thickness of the coating made of the sealing material 22'' is 3 mm. For example, the thickness of the coating made of the sealing material 22 is 10 mm or less, preferably 5 mm, 3 mm, 2 mm or less, 1.5 mm or less, 1 mm or less. For example, the reduced thickness of the coating made of the sealing material 22 is 9 mm or less, preferably 4 mm, 2.8 mm, 1.9 mm or less, 1.45 mm, 0.95 mm or less. For example, the difference in thickness between the coating thickness made of the sealing material 22 and the reduced thickness of the coating made of the sealing material 22'' is 1 mm, 0.7 mm, 0.5 mm or less, for example, 0.3 mm, 0.2 mm, 0.1 mm, 0.05 mm or less.
[0034] For example, the first opening 6 is at least 0.5 mm or 1 mm, for example 2 mm or more, 0.5 cm, preferably 1 cm, particularly preferably 1.5 cm or more, larger than the second opening 9, and preferably the step 12 formed on the inside of the cathode frame 11 by the larger first opening 6 and the smaller second opening 9 has the same width everywhere (FIG. 7b, FIG. 11). Alternatively, the step 12 can have different widths at various places. The width of the step 12, and therefore the width of the planar third surface for holding the CCM 13, can have the same width or different widths at various places.
[0035] The anode frame 8 may have, for example, outer dimensions of 20-70 cm x 20-70 cm, for example 50 cm x 50 cm or 35 cm x 35 cm. The first opening 6 may have, for example, dimensions of 11-51 cm x 11-51 cm, for example 21 cm x 21 cm or 15 cm x 15 cm (Fig. 9b). The cathode frame 11 may have, for example, outer dimensions of 20-70 cm x 20-70 cm, for example 50 cm x 50 cm or 35 cm x 35 cm. The second opening 9 may have dimensions of 10-50 cm x 10-50 cm, for example 20 cm x 20 cm or 14 cm x 14 cm (Fig. 9a). Preferably, the same outer dimensions are selected for the anode frame 8 and the cathode frame 11. The dimensions of the first opening 6 and the second opening 9 are selected such that the first opening 9 is larger than the second opening 9, such that when the anode frame 8 and the cathode frame 1 interact as a frame 1, a step 12 is formed; Various frame shapes are known to the person skilled in the art, and the frame 1, the anode frame 8 and the cathode frame 11 can be designed, for example, square, rectangular or circular. Due to the fact that the shape of the frame 1 can be freely selected, the contact pressure in certain areas of the frame 1 can be adjusted by increasing or decreasing the thickness of the frame, preferably by decreasing the thickness of the coating made of the sealant 22. The thickness of the coating made of the sealant 22 can also be increased. This allows forming areas in which the layer thickness of the coating made of the sealant 22 on the core 21 is thicker than in other areas of the anode frame 8 or the cathode frame 11. The layer thickness of the coating made of the sealant 22 can be reduced. As a result, it is possible to form areas in which the layer thickness of the coating made of the sealant 22 on the core 21 is smaller than in other areas of the anode frame 8 or the cathode frame 11. Areas with different layer thicknesses of the coating made of the sealant 22 can take over the function of the frame 1 according to the invention.
[0036] To avoid side leakage, the pressure on the active area can be increased by a circumferential height 26'' in the thickness of the coating of the seal material 22, e.g. an increase in rubber in the circumferential direction. The circumferential height 26'' in the thickness of the coating of the seal material 22 can have a width of e.g. 1 mm. The thickness difference between the coating of the seal material 22 and the circumferential ridge 26'' can be e.g. 1 mm, 0.5 mm, 0.1 mm, 0.05 mm.
[0037] The subject of the present invention is a frame 1 in which the coating of sealing material 22 in certain areas of the anode frame 8 and / or in certain areas of the cathode frame 11 has a reduced layer thickness 22'' compared to the layer thickness of the coating of sealing material 22, for example to reduce the contact pressure.
[0038] The subject of the invention is a frame 1, in which in a specific region of the anode frame 8, a coating of a sealing material 22 has a circumferential height 26'' surrounding the first opening 6, for example to enhance the sealing effect. The subject of the invention is a frame 1, in which in a specific region of the cathode frame 11, a coating of a sealing material 22 has a circumferential ridge 26'' surrounding the second opening 9, for example to enhance the sealing effect.
[0039] In a square anode frame 8, the first opening 6 may be defined by a first side 27, a second side 28, a third side 29, and a fourth side 30. In a square cathode frame 11, the second opening 9 may be defined by a first side 27'', a second side 28'', a third side 29'', and a fourth side 30''.
[0040] Further components which are part of the PEM electrolysis cell 2 or the stack-type PEM electrolysis device 23 can be saved by being installed as structures on the frame 1, the anode frame 8, the cathode frame 11, in particular by using a coating of sealing material 22 on which the cores 21 of the anode frame 8 and the cathode frame 11 are coated. For example, the coating of sealing material 22 can be a coating of rubber and for example consists of a rubber lip 25 which is arranged in the area of the connections for the individual voltage measurements. In this way, insulating foils can be saved. The invention relates to a frame 1 in which the coating of sealing material 22 of the anode frame 8 and / or the coating of sealing material 22 of the cathode frame 11 take over further functions in addition to the sealing function. For this purpose, the coating of sealing material 22 of the anode frame 8 and / or the cathode frame 11 consists of a corresponding embodiment, for example of a rubber lip 25.
[0041] The number of individual parts required to manufacture a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23 can be reduced, since other necessary parts can be manufactured directly from the coating of sealing material 22. This significantly reduces the effort required to assemble a PEM electrolysis device of stack type 23. Similarly, by inserting the means for connecting the anode frame 8 and the cathode frame 11, such as the pins 19 and holes 18 into the anode frame 8 and / or the cathode frame 11, no additional assembly aids are required.
[0042] In a preferred embodiment, the coating of the sealing material 22 comprises one or more channels type II 15. The channel type II 15 is designed as an area of the coating of the sealing material 22 with a reduced layer thickness compared to the layer thickness of the coating of the sealing material 22. The channel type II 15 is therefore a depression or recess of the coating made of the sealing material 22 that does not contribute to the sealing effect. Adjacent individual channels type II 15 are separated by plateaus 26. Plateaus 26 are, for example, areas between two adjacent channels type II 15, in which the core 21 has a coating of the sealing material 22 without a reduced layer thickness. The reduced layer thickness of the coating of the sealing material 22'' in the areas where the individual channels type II 15 are located can be selected independently of the reduced layer thickness of the coating of the sealing material 22'' in other areas of the coating surrounding the core 21, which areas can have a reduced layer thickness of the coating. In certain embodiments, the core 21 does not have a coating of sealant 22 in one or more areas representing one or more channel type II 15 .
[0043] In a preferred embodiment, the first opening 6, bordered by the anode frame 8, and the second opening 9, bordered by the cathode frame 11, are of different sizes (Figs. 7b, 8, 9a and 9b). For example, the cathode frame 11 is small and the anode frame 8 is large. This means that a pressure difference, e.g. 40 bar, i.e. if only the cathode side of the electrochemical cell 2 is operated under pressure, or if only the cathode side of the stacked 23 PEM electrolyser is operated under pressure, the hydrogen pressure generated at the cathode during PEM electrolysis does not or cannot press the gap 17 between the anode frame 8 and the PTL anode 7. The CCM 13 is only pressed against the PTL anode 7 and mechanically supported by the PTL anode 7. In this way, creeping 24 of the CCM 13 into the gap 17 between the frame 1, e.g. the anode frame 8 and the PTL anode 7, can be prevented.
[0044] In a preferred embodiment, the frame 1 according to the invention comprises two different types of flow channels for the supply and removal of water and gas. Preferably, the frame 1 comprises one or more flow channels type I 14c for transporting water into the frame 1 and for transporting water and gas from the frame 1. Preferably, the I-type flow channels 14 are not directly connected to the first opening 6 of the anode frame 8 or to the second opening 9 of the cathode frame 11. Preferably, the core 21 of the anode frame 8 consists of one or more channels type I 14. Preferably, the core 21 of the cathode frame 11 consists of one or more I-type channels 14. Preferably, the I-type channels 14 are covered with a coating made of a sealant 22.
[0045] Furthermore, the frame 1 preferably comprises one or more channels type II 15 for transporting water to the first opening 6, water and oxygen from the first opening 6, and hydrogen from the second opening 9. Preferably, the type II channels 15 connect the type I channels 14 to the first opening 6. Preferably, the type II channels 15 connect the type I channels 14 to the second opening 9.
[0046] In a preferred embodiment, the covering of the seal material 22, which is entirely or partially covered by the anode frame 8, consists of one or more type II channels 15. In another embodiment, the core 21 of the anode frame 8 consists of one or more type II channels 15. In a preferred embodiment, the covering of the seal material 22, which is entirely or partially covered by the cathode frame 11, consists of one or more type II channels 15. In another embodiment, the core 21 of the cathode frame 11 consists of one or more type II channels 15. The advantage of this embodiment is the manufacturing costs. In a preferred embodiment, the channel type II 15 is not milled out of each anode frame 8 and each cathode frame 11, but is transferred once to a tool. A suitable tool is, for example, a negative of the anode frame 8 or a negative of the cathode frame 11. For example, the arrangement, diameter, length and, if necessary, other parameters of the channel type II 15 are transferred to the tool. The tool can be used, for example, to transfer the channel type II 15 to the seal 22, as if it were stamped into the seal material, preferably rubber, for example EPDM, using a stamp. A tool is used to vulcanize the core 21 of the anode frame 8 or the core 21 of the cathode frame 11 .
[0047] In a preferred embodiment, the anode frame 8 includes, on the surface of the first side 4, one or more type II channels 15 that are connected to one or more type I channels 14, connect the type I channel(s) 14 to the first opening 6, and are arranged in a direction towards the bipolar plate (BPP) 16 when the frame 1 is installed in the PEM electrolysis cell 2 or stacked PEM electrolysis apparatus 23, and the side opposite the first side 4 of the anode frame 4'' does not have any type II channels 15.
[0048] In a preferred embodiment, the cathode frame 11 is connected on the surface of the second side 5 with one or more channels type I 14, which connect the channels type I 14 to the second openings 9 and constitute one or more channels type II 15 which are arranged towards the bipolar plate (BPP) 16 when the frame 1 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, and the side of the cathode frame 5'' opposite the second side 5 does not have channels type II 15.
[0049] In a preferred embodiment, the frame 1 according to the invention comprises one or more channels type I 14 for supplying and removing water and gases and one or more channels type II 15, the channels type I 14 being not connected to the first opening 6 of the anode frame 8 or to the second opening 9 of the cathode frame 11. In a preferred embodiment of the frame 1, the anode frame 8 comprises, on the surface of the first side 4, one or more channels type II 15 which are connected to the channels type I 14 and which connect the channels type I 14 to the first opening 6 and which are arranged in a direction towards the BPP 16 when the frame 1 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, and the side opposite to the first side 4 of the anode frame 4'' does not comprise channels type II 15. In a preferred embodiment of the frame 1, the cathode frame 11 is connected on the surface of the second side 5 with one or more channels type I 14, which connect the channels type I 14 to the second openings 9 and constitute channels type II 15 which are arranged in a direction towards the BPP 16 when the frame 1 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, and the side of the cathode frame 5'' opposite the second side 5 is devoid of channels type II 15.
[0050] In a preferred embodiment, the frame 1 according to the invention comprises at least two channels type I 14 for supplying and removing water and gases and at least two channels type II 15, the channels type I 14 being not connected to the first opening 6 of the anode frame 8 or to the second opening 9 of the cathode frame 11. In a preferred embodiment of the frame 1, the anode frame 8 comprises, on the surface of the first side 4, at least two channels type II 15, which are connected to the at least two channels type I 14 and connect the channels type I 14 to the first opening 6 and are arranged in a direction towards the BPP 16 when the frame 1 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, the side opposite to the first side 4 of the anode frame 4 ″ does not contain channels type II 15. Preferably, a plurality of channels type II 15 arranged on the first side 4 of the anode frame 7 connect the channels type I 14 to the first opening 6. In a preferred embodiment of the frame 1, the cathode frame 11 comprises at least two channels type II 15 arranged on the surface of the second side 5, connected to at least two channels type I 14, connecting the channel type I 14 to the second opening 9, and arranged in a direction towards the BPP 16 when the frame 1 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, and the side of the cathode frame 5″ opposite to the second side 5 does not include a channel type II 15. Preferably, the multiple channels type II 15 arranged on the second side 5 of the cathode frame 11 connect the channel type I 14 to the second opening 9.
[0051] The type II channel 15 connecting the type I channel 14 with the first opening 6 and the second opening 9, i.e., the type II channel 15 connecting the PTL anode 7 and the PTL cathode 10 with the type I channel 14 for supplying and removing water and gas in the PEM electrolysis cell, is arranged in the anode frame 8 and / or the cathode frame 11 so as to face the BPP 16 and not to face the CCM 13. The type II channel 15, i.e., the CCM 13, is arranged on the side of the anode frame 7 and the side of the cathode frame 11 on which the CCM 13 is placed, and since there is no flow path in the immediate vicinity of the first opening 6 or the second opening 9 in the area exposed to a differential pressure of up to 40 bar during electrolysis, the CCM 13 is not affected even if gas and water flow through the flow path of the type I 14 during electrolysis. The CCM 13 is placed on a smooth flat surface without grooves, so that it is sufficiently supported even under a differential pressure of up to 40 bar. At the same time, the anode chamber (the anode chamber is formed by the anode frame 7, the CCM 13 and the BPP 16), the cathode chamber (the cathode chamber is formed by the cathode frame 11, the CCM 13 and the BPP 16) and the entire PEM electrolysis cell 2 are completely sealed even at a differential pressure of up to 40 bar, and no gas or water will leak out.
[0052] In an exemplary embodiment, the frame 1 is comprised of from 2 to 1000 or more channels type II 15, such as at least 100 channels type II 15, preferably at least 200 channels type II 15, or more or less, such as less than 50 channels type II 15. Preferably, at least half of the type I channels 14 are connected to the first opening 6 or the second opening 9 by type II channels 15.
[0053] Preferably, at least two or more, e.g., four, ten or more, type II channels 15 connect the type I channels 14 to the first opening 6. Preferably, at least two or more, e.g., four, ten or more, type II channels 15 connect the type I channels 14 to the second opening 9.
[0054] For example, the channel type II 15 connected to the first opening 6 are arranged adjacent to each other on the first side of the frame 4. The distance between two adjacent channel type II 15 is, for example, ≦5 mm, ≦3 mm, preferably ≦2 mm or less. For example, the channel type II 15 between the channel type I 14 and the first opening 6 are arranged in a fan shape on the first side of the frame 4.
[0055] For example, the channel type II 15 connected to the second opening 9 are arranged adjacent to each other on the second side of the frame 5. The distance between two adjacent channel type II 15 is, for example, ≦5 mm, ≦3 mm, preferably ≦2 mm or less. For example, the channel type II 15 between the channel type I 14 and the second opening 9 are arranged in a fan shape on the second side of the frame 5.
[0056] The flow paths of the frame 1 are designed such that the liquid is distributed within the stack type 23 PEM electrolyser via flow paths type I 14 and enters the individual PEM electrolysis cells 2 via flow paths type II 15. The flow paths type I 14 are preferably arranged at regular intervals along or parallel to the first opening 6 of the anode frame 8. The I-type channels 14 are preferably arranged at regular intervals along or parallel to the second opening 9 of the cathode frame 11. For example, there are more than 20 or less, for example 5, I-type channels 14 on each side of the square first opening 6 or on each side of the square second opening 9.
[0057] In a particularly preferred embodiment, the flow channels type I 14 are arranged to supply water to the same parts, and therefore the same areas, of the first and second openings 6 and 9 of the electrochemical cell 2 or the first and second openings 6 and 9 of the PEM electrolyser of the stack type 23, respectively.
[0058] In a particularly preferred embodiment, a continuous channel type II 15 with a constant opening diameter, preferably 5 mm or less, particularly preferably <2 mm, leads from each channel type I 14 or part of the channel type I 14 to the first opening 6 or the second opening 9. These channels type II 15 are arranged, for example, in the shape of a fan, so that the channels type II 15 are evenly distributed over the first opening 6 or the second opening 9. Other arrangements of the channels type II 15 in the area between the first opening 6 or the second opening and the channel type I 14 passing through the channel type II 15 are also possible. By limiting the width of the channel type II 15 to 5 mm or less, preferably 2 mm or less, a sufficient contact pressure is transmitted to the counter frame 1 in the area of the channel type II 15.
[0059] The uniform distribution of channels type I 14 and type II 15 along the first opening 6 or along the second opening 9 across the entire width of the frame 1, for example along the entire width of the first side of the first opening 27 and along the entire width of the third side of the first opening 29 (Fig. 10a), provides a particularly good distribution of water across the entire active cell area (=first opening 6 + second opening 9) of the electrochemical cell 2. Water flows uniformly in the PEM electrolysis cell 2. Since most of the incoming water is used for cooling, the uniform distribution of type II channels 15 leads to homogeneous heat dissipation. Such an arrangement of channels type II 15 allows the heat generated during PEM electrolysis to be dissipated uniformly. Dissipation of reaction heat is an important parameter for PEM electrolysis cells 2 or PEM electrolysis devices of stack type 23.
[0060] The present invention includes stack type 23 PEM electrolyzers of different designs and constructions.
[0061] The frame 1, the PEM electrolysis cell 2, the pre-assembled module 20, the PEM electrolysis device of stack type 23 are included, and each individual flow channel type II 15 is adapted to provide a higher or lower pressure loss in the flow of water compared to the other flow channels type II 15 of the respective frame 1, respective electrochemical cell 2, respective PEM electrolysis device of stack type 23. For example, the external flow channels type II 15 are adapted accordingly, for example the flow channel type II 15 arranged at the end of the arrangement of flow channels type II 15 on the first side of the frame 4, for example the flow channel type II 15 arranged at the end of the arrangement of flow channels type II 15 with respect to the first side of the first opening 27, is adapted to provide either a higher or lower pressure loss in the flowing water compared to the other flow channels type II 15 of the PEM electrolysis device of frame 1, electrochemical cell 2, pre-assembled module 20, stack type 23. This can be achieved, for example, by reducing the opening cross section of the type II flow channels 15. This is necessary, for example, if the pressure loss in the channels type I 14 is not uniform, but the channels type II 15 is uniform, and a certain area of the active cell area (active cell area = first opening 6 + second opening 9) with a higher volumetric flow rate of water through said channels type II 15 is connected to a channel type I 14 where the flowing water has a higher pressure. Without adapting the type II channels 15, the cooling of the active cell area may be more uneven, for example, due to the water flowing through them. This can be compensated for by adapting the type II channels 15. The cross-sectional area of the channels type II 15 can be reduced, for example, to compensate for differences in water pressure in the channels type I 14. Preferably, a uniform or homogeneous water pressure is generated over the entire active cell area. With channels type II 15, for example, individually adapted and with, for example, different opening cross-sectional areas, the different pressure losses in the channels type I 14 can be compensated for and the flow through all channels type II 15 can be homogenized.
[0062] The subject of the present invention are frames 1, PEM electrolysis cells 2, preassembled modules 20 and PEM electrolysis devices of stack type 23, in which the individual flow channels type II 15 of the corresponding frame 1, the corresponding electrochemical cells 2, the corresponding preassembled modules 20 and the corresponding PEM electrolysis device of stack type 23 are arranged in such a way that each flow channel type II 15 supplies water to an area as large as the active cell area.
[0063] The present invention concerns a frame 1, a PEM electrolysis cell 2, a preassembled module 20 and a PEM electrolysis device of stack type 23, in which the individual channels type II 15 of each frame 1, each PEM electrolysis cell 2, each preassembled module 20 and each PEM electrolysis device of stack type 23 are designed in such a way that all channels type II 15 can simultaneously transport the same amount of water, i.e. all channels type II 15 are identical. This can be achieved, for example, by all channels type II 15 having the same cross section through which water can flow. Preferably, the channels type II 15 are arranged in such a way that each channel type II 15 supplies water to an area of the same size as the active cell area. Particularly preferably, the channels type II 15 are arranged in such a way that each channel type II 15 supplies water to an area of the same size of the active cell area and all channels type II 15 are identical. In this way, water can be evenly supplied to the entire active cell area.
[0064] The number, shape and arrangement of type I channels 14, as well as other parameters thereof, and the number, shape and arrangement of type II channels 15, as well as other parameters thereof, may be adapted as necessary, for example to suit the frame shape used.
[0065] In the frame 1 according to the invention, the anode frame 8 and the cathode frame 11 are connected to each other via connecting elements. Corresponding connecting elements are known to the person skilled in the art. In a preferred embodiment of the frame 1, the anode frame 8 is composed of one or more connecting elements, for example pins 19, and the cathode frame 11 is composed of one or more connecting elements, for example holes 18, the pins or pins 19 and the holes or holes 18 being arranged in such a way that the holes or holes 18 of the cathode frame 11 can be inserted into the pins or pins 19 of the anode frame 8, and the anode frame 8 and the cathode frame 11 can be connected to each other thereby.
[0066] The subject of the invention is a PEM electrolysis cell 2 operating under a differential pressure of up to 40 bar for the production of high pressure hydrogen, comprising a PEM membrane electrode arrangement with a CCM 13, a PTL anode 7 and a PTL cathode 10, the PEM electrolysis cell 2 constituting a frame 1 according to the invention, the first opening 6 of the anode frame 8 constituting the PTL anode 7, the second opening 9 of the cathode frame 11 constituting the PTL cathode 10, the CCM 13 being arranged between the side of the anode frame 4 ″ facing the first side 4 and the side of the cathode frame 5 ″ facing the second side 5, one side of the CCM 13 resting on the PTL anode 7 and the other side of the CCM 13 resting on the step 12 and the PTL cathode 10 (Figures 7b and 7c). When the PEM electrolysis cell 2 is operated under differential pressure, in the region of the gap 17 between the anode frame 8 and the PTL anode 7, no differential pressure acts on the CCM 13. This prevents the CCM 13 from creeping 24 into the gap 7 (FIGS. 8 and 8a).
[0067] In a preferred embodiment, a PEM electrolysis cell 2 according to the invention comprises a CCM 13 having a thickness of 80 μm or less, for example a CCM 13 having a thickness of 50 μm or less.
[0068] In the PEM electrolysis cell 2 according to the invention, the seal 22 of the anode frame 8, for example a coating made of rubber, preferably a coating made of EPDM, the seal 22 of the cathode frame 11, for example a coating made of rubber, preferably a coating made of EPDM, the seal 22 of the cathode frame 11, for example a coating made of rubber, preferably a coating made of EPDM, the step 12 interact with the CCM 13 (Fig. 7c and Fig. 8a) and completely seal the PEM electrolysis cell 2 and the anode and cathode compartments without the crawl 24 of the CCM 13 entering the gap 17 between the anode frame 8 and the PTL anode 7. The special arrangement of the type II channels 15 completely guarantees both the supply and removal of water and gases, as well as the stability of the CCM 13 and the complete sealing of the electrolyte membrane cell 2. The frame 1 according to the invention therefore allows the use of a CCM 13 with a thickness of 80 μm or less, for example a thickness of 50 μm or less (=thin CCM 13). The frame 1 according to the invention allows the PEM electrolysis cell 2 to be manufactured with a thinner CCM 13 than usual in the prior art. Furthermore, these PEM electrolysis cells 2 can be operated to accumulate hydrogen to create a differential pressure of up to 40 bar on the cathode side without damaging the CCM 13 or causing the PEM electrolysis cells 2 to leak.
[0069] In a preferred embodiment, the anode 7 is designed such that the BPP 16 is connected to the anode 7, which is called BPP / anode 36 according to the invention. The use of the BPP / anode 36 not only facilitates assembly, but also reduces the contact resistance between the individual parts. In a preferred embodiment, the anode 7 comprises at least one coarse distributor and at least one fine distributor for the process medium, in particular water. The coarse distributor distributes the water efficiently over the entire cell area (i.e. the first opening and the second opening 6+9). The fine distributor transports the water to the CCM 13, allows good electrical contact with the CCM 13 and at the same time mechanically supports the latter. As a coarse distributor for the PTL anode 7, for example, an expanded metal can be used. As a fine distributor for the PTL anode 7, for example, a plate made of sintered powder can be used. The coarse and fine distributors, for example expanded metal and sintered metal, can be joined, for example, by resistance welding, to produce the PTL anode 7. Alternatively, the powder can be sintered directly onto the expanded metal to produce the PTL anode 7. The PTL anode 7 can be connected to the BPP 16. Preferably, the BPP 16 is made of the same material as the PTL anode 7. In a particularly preferred embodiment, the BPP 16 and the PTL anode 7 are made of titanium. In an alternative preferred embodiment, the BPP 16 and the PTL anode 7 are made of at least 80% of the same material, for example titanium. The connection between the BPP 16 and the PTL anode 7 can be realized, for example by resistance welding, preferably in several places. In the BPP / PTL anode 36, the surface of the BPP 16 corresponds to the outer surface of the frame 1, or the surface of the BPP / PTL anode 36 essentially corresponds to the outer surface of the frame 1. The surface of the PTL anode 7 of the BPP / PTL anode 36 is adapted to fill or fit into the first opening 6. Instead of two parts (BPP 16 and PTL anode 7), only one part, the BPP / PTL anode 36, is required for assembly. This means you save one part.
[0070] Depending on whether water or gas is transported through the electrode, the channel type I14 on one or both sides along the first opening 6 of the anode frame 8 can also be significantly smaller than the channel type I14 on the other side along the first opening 6 of the anode frame 8 (see FIG. 10b). For example, the channel type I14 on the positive electrode side can be significantly smaller than the negative electrode side (see FIGS. 10b-10d). To save space and ensure the mechanical stability of the frame 1, the channel type I14 can be designed, for example, as a slot instead of a round hole. Various shapes and corresponding adaptations are possible for the I-type channels 14.
[0071] The object of the invention is a pre-assembled sub-module 20 for producing an electrolysis device of stack type 23, consisting of a frame 1 according to the invention. The object of the invention is a pre-assembled module 20 for producing an electrolysis device of stack type 23, consisting of, for example, an anode frame 8, a cathode frame 11, a BPP 16, a PTL anode 7 and a PTL cathode 10, Here, the anode frame 8 comprises a first side 4 of the frame 1 having a planar first surface, an opposite side to the first side 4 of the anode frame 4″, and a first opening 6 for receiving a PTL anode 7, the first opening 6 extending from the first side 4 to the opposite side of the anode frame 4″ to the first side 4, the first opening 6 being surrounded by the anode frame 8, the anode frame 8 comprising at least one connection element, e.g. a pin 19, for connection to a cathode frame 11, Here, the cathode frame 11 comprises a second side 5 of the frame 1 having a planar second surface, a side opposite to the first side 5 of the cathode frame 5″, and a second opening 9 for receiving the PTL cathode 10, where the second opening 9 extends from the second side 5 to the side opposite to the second side 5 of the cathode frame 5″ and is surrounded by the cathode frame 10, and the cathode frame 11 is composed of at least one connection element for connection to the anode frame 8, for example a hole 18 for receiving a pin 19 of the anode frame 8, Here, the BPP 16 is disposed between the first side 4 of the frame 1 and the second side 5 of the frame 1, and the BPP 16 may be part of the BPP / PTL anode 36. an anode frame 8, which consists of a core 21, e.g. made of metal or made of metal, and a coating made of a sealant 22, e.g. a coating made of rubber, preferably a coating made of EPDM, the core 21 being fully or partially covered with the coating made of the sealant 22, and preferably a BPP 16 is connected to a PTL anode 7 to form a BPP / PTL anode 36, the PTL anode 7 or the BPP / PTL anode 36 being inserted or pressed into the first opening 6, the PTL anode 7 being framed by the anode frame 8, The cathode frame 10 consists of a core 21, for example made of metal or made of metal, and a coating made of a sealant 22, for example a coating made of rubber, preferably a coating made of EPDM, the core 21 is completely or partially covered with the coating made of the sealant 22, the PTL cathode 10 is inserted or pressed into the second opening 9 and framed by the cathode frame 11, Here, the anode frame 8 and the cathode frame 11 are connected via the connecting elements of the anode frame 8 and the cathode frame 11, for example, the pins 19 of the anode frame 8 are inserted into the holes 18 of the cathode frame 11, and the anode frame 8 and the cathode frame 11 are thereby connected to each other; Here, the first opening 6 is larger than the second opening 9, the anode frame 8 and the cathode frame 11 are arranged such that the first side 4 and the second side 5 form a step 12 at the transition from the anode frame 8 to the cathode frame 11, where the step 12 is preferably the part of the cathode frame 11 adjacent to and preferably bordering the second opening 9, the step 12 preferably forms a planar third surface as a support surface for the CCM 13, and the BPP 16 or BPP 16 of the BPP / PTL anode 36 rests on one side on the PTL anode 7 and anode frame 8 and on the other side on the PTL cathode 10, the cathode frame 11 and the step 12. The pre-assembled module 20 is preferably comprised of flow channels type I 14 and type II 15 as described herein for the supply and removal of water and gas, which can be arranged as described.
[0072] The subject of the invention is a method for manufacturing an assembled module 20 consisting of a frame 1 according to the invention. The subject of the invention is, for example, a method for manufacturing an assembled module 20, comprising the following steps: a) For the anode frame 8, a core 21, preferably made of metal, is manufactured, which comprises a first side 4 with a planar first surface and a side opposite to the first side 4 of the anode frame 4'', the first side 4 and the side opposite to the first side 4 of the anode frame 4'' constitute a first opening 6 extending from the first side 4 to the side opposite to the first side 4 of the anode frame 4'' and bordered by the anode frame 8, and which comprises one, two or more I-shaped channels 14 for the supply and removal of water and gas, the I-shaped channels 14 being not connected to the first opening 6 of the anode frame 8, the anode frame 8 being provided with at least one connection element, e.g. a pin 19, for connection to the cathode frame 11, e.g. a pin 19, b) the surface of the core 21 produced according to a) for the anode frame 8 is completely or partially, for example at least 90%, coated with natural or synthetic rubber and then vulcanized in order to produce a coating of rubber as a coating of the sealant 22 by vulcanization, whereby a coating of rubber is produced on the entire surface or on a part of the surface of the core 21, preferably a coating of EPDM, in which in the coating of rubber 1. one, two or more channels 14 of type I are generated on the surface of the first side 4, connecting the one or more channels 14 of type I with the first opening 6; if the anode frame 8 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, then it is arranged in the direction of the BPP side of the BPP 16 or BPP / PTL anode 36, in the coating of rubber on the side facing the first side 4 of the anode frame 4″, no channels of type II 15 are generated; c) the PTL anode 7 and the BPP 16 or the BPP / PTL anode 36 are placed or pressed into the anode frame 8 produced according to a) and b); d) a core 21, preferably made of metal, is manufactured for the cathode frame 11, the core 21 having a second side 5 with a planar second surface and a side opposite to the second side 5 of the cathode frame 5'', the second side 5 and the side opposite to the second side 5 of the cathode frame 5'' are provided with one, two or more I-shaped channels 14 for the supply and removal of water and gases, which extend from the second side 5 to the side opposite to the second side 5 of the cathode frame 5'' and constitute a second opening 9 bordered by the cathode frame 11, the I-shaped channels 14 being not connected to the second opening 9 of the cathode frame 11, the cathode frame 11 being provided with at least one connection element, such as for example a hole 18, for connection to the anode frame 8, e) the surface of the core 21 for the cathode frame 11 produced according to d) is completely or partially, for example at least 90%, coated with natural or synthetic rubber and then vulcanized to produce a rubber coating as a coating of the sealant 22 by vulcanization, whereby a rubber coating, preferably a coating of EPDM, is produced on the entire surface or part of the surface of the core 21, in which two or more channels 15 of type II are generated on the surface of the second side 5, which are connected to one, two or more channels 14 of type I and connect the one or more channels 14 of type I with the second opening 9, if the cathode frame 11 is installed in a PEM electrolysis cell 2 or a PEM electrolysis device of stack type 23, arranged in the direction of the BPP side of the BPP 16 or BPP / PTL anode 36, and in the rubber coating on the side opposite to the second side 5 of the cathode frame 5 ″, no channels of type II 15 are generated; f) The cathode frame 11 manufactured according to d) and e) is connected to the anode frame 8, for example, by inserting the cathode frame 11 into the anode frame 8, placing the BPP 16 between the first side 4 and the second side 5, and then inserting or pushing the PTL cathode 10 into the cathode frame 11.
[0073] The subject of the present invention is a method for producing a PEM electrolyser of stack type 23 operating under differential pressure to produce high pressure hydrogen, comprising a frame 1 according to the invention, a preassembled module 20 according to the invention and an electrochemical cell 2. The subject of the present invention is, for example, a method for producing a PEM electrolyser of stack type 23 operating under differential pressure to produce high pressure hydrogen, comprising the method steps: a) at least x preassembled modules 20 according to the present invention and at least x+1 CCMs 13 are stacked one on top of the other to produce a stack of preassembled modules 3, in which one preassembled module 20 and one CCM 13 are stacked one on top of the other in the stack of preassembled modules 3, one CCM 13 is arranged on the upper side and one CCM 13 is arranged on the lower side of the stack of preassembled modules 3, and one CCM 13 is arranged between every two adjacent preassembled modules 20; and b) then a single anode, preferably a single PTL anode 7', is placed parallel to the outer CCM 13 on one side of the stack of pre-assembled modules 3, and a single cathode, preferably a single PTL cathode 10', is placed parallel to the outer CCM 13 on the other side of the stack of pre-assembled modules 3; c) end plates 33 are placed parallel to a single anode and parallel to a single cathode, and the resulting stack is compressed between the two end plates 33 to form a stack type 23 PEM electrolysis device, where x is an integer number and is ≧2.
[0074] In a preferred embodiment of the method for manufacturing a stacked 23 PEM electrolyser according to the invention, one, or preferably each, of the x+1 CCMs 13 in the stacked 23 PEM electrolyser has a thickness of less than or equal to 80 μm, x being an integer and ≧2. Particularly preferred, a plurality, or preferably each, of the x+1 CCMs 13 in the stacked 23 PEM electrolyser has a thickness of less than or equal to 50 μm, x being an integer and ≧2.
[0075] The subject of the invention is a PEM electrolyser of stack type 23 operating under differential pressure for producing high pressure hydrogen, which comprises one or more frames 1 according to the invention. The subject of the invention is a PEM electrolyser of stack type 23 comprising one or more preassembled modules 20 according to the invention. The subject of the invention is a PEM electrolyser of stack type 23 consisting of one or more PEM electrolysis cells 2 according to the invention.
[0076] The subject of the invention is a PEM electrolyser of stack type 23, operating under differential pressure, for example for producing high pressure hydrogen, comprising x preassembled modules 20 according to the invention, x+1 CCMs 13, a single anode, a single cathode and two end plates 33, whereby x preassembled modules 20 and x+1 CCMs 13 are stacked alternately on top of each other to form a stack of preassembled modules 3, whereby one preassembled module 20 and one CCM 13 are stacked alternately on top of each other in the stack of preassembled modules 3, whereby one CCM 13 is arranged on the upper and lower sides of the stack of preassembled modules 3 and one CCM 13 is arranged between two adjacent preassembled modules 20, whereby a single anode, preferably a single PTL anode 7', is arranged on one side of the stack of preassembled modules 3 parallel to the outer CCM 13 and a single cathode, preferably a single PTL cathode 10', is arranged on the other side of the stack of preassembled modules 3 parallel to the outer CCM 13, Here, one end plate 33 is placed parallel to a single anode and one end plate 33 is placed parallel to a single cathode, and the resulting stack is compressed between the two end plates 33 to form a stack type 23 PEM electrolysis device, where x is an integer and is ≧2.
[0077] In a preferred embodiment of the stacked 23 PEM electrolyser according to the invention, one or more, preferably each, of the x+1 CCMs 13 in the stacked 23 PEM electrolyser has a thickness of 80 μm or less, preferably a thickness of 50 μm or less, where x is an integer number ≧2.
[0078] Depending on requirements, further components can be installed at suitable positions in the PEM electrolyser of stack type 23, for example insulating plates 32 can be installed between the CCM 13 and the end plates 33. The insulating plates 32 in these positions prevent the end plates 33 from shorting out, for example when screws are used. Corresponding parts are known to those skilled in the art. The skilled person can adapt the manufacturing method accordingly.
[0079] The subject of the present invention is a PEM electrolyser of stack type 23 for operation under differential pressure to produce high pressure hydrogen, comprising x preassembled modules 20 according to the invention, x+1 CCMs 13, a single anode, preferably a single PTL anode 7', a single cathode, preferably a single PTL cathode 10' and two end plates 33, wherein the x preassembled modules 20 and the x+1 CCMs 13 are stacked alternately on top of each other to form a stack of preassembled modules 3, wherein the preassembled modules 20 and the x+1 CCMs 13 are stacked alternately on top of each other to form a stack of preassembled modules 3, In the stack of assembled modules 3, in each case one assembled module 20 and one CCM 13 are stacked one on top of the other, in each case one CCM 13 is arranged on the upper and lower sides of the stack of assembled modules 3, in each case one CCM 13 is arranged between two adjacent assembled modules 20; a single anode is arranged parallel to the outer CCM 13 on one side of the stack of assembled modules 3 and a single cathode is arranged parallel to the outer CCM 13 on the other side of the stack of assembled modules 3; Here, the end plates 33 are arranged parallel to a single anode and parallel to a single cathode, respectively, and the resulting stack is compressed between the two end plates 33 to form a stack type 23 PEM electrolysis device, where x is an integer number and is ≧2.
[0080] A half-cell anode is comprised only of the anode side of an electrochemical cell 2, and not the cathode side of the electrochemical cell 2. In a preferred embodiment, the half-cell anode is comprised of a single anode 7' and an anode frame 8. In a preferred embodiment, the half-cell anode is comprised of a single anode 7' and an anode frame 8. The half-cell anode completes an electrochemical cell 2 in an assembled module 20 or a stack of assembled modules 3.
[0081] The half-cell cathode constitutes only the cathode side of the electrochemical cell 2, and not the anode side of the electrochemical cell 2. In a preferred embodiment, the half-cell cathode is comprised of a single cathode 10' and a cathode frame 11. In a preferred embodiment, the half-cell cathode is comprised of a single cathode 10' and a cathode frame 8. The half-cell cathode completes an electrochemical cell 2 in an assembled module 20 or a stack of assembled modules 3.
[0082] In a preferred embodiment, a PEM electrolyser of stack type 23 is composed of at least 2 or 3 or 5 or more, e.g. 10, 50, 100, 500, 1000 or more preassembled modules 20 according to the invention. Preferably, a PEM electrolyser of stack type 23 according to the invention comprises, in addition to x preassembled modules 20 according to the invention (x being an integer and ≧2), a cathode frame 11, a CCM 13, an anode frame 8 and two end plates 33. Preferably, in a PEM electrolyser of stack type 23 according to the invention, the first PEM electrolyser cell 2 and the last PEM electrolyser cell 2 are different from the one located between them. For example, to manufacture a PEM electrolyser of stack type 23, a CCM 13 is placed on the cathode frame 11, and x preassembled modules 20 and x CCMs 13 are alternately stacked on the CCM 13, and an anode frame 8 is stacked on top of it. The stack is compressed between end plates 33 to form a stacked 23 PEM electrolyser, where x is an integer number and ≧2.
[0083] In a stack type 23 PEM electrolyser, preferably one of the two end plates 33 is, for example, an upper end plate 38 arranged at the top in the stack type 23 PEM electrolyser. In a stack type 23 PEM electrolyser, preferably one of the two end plates 33 is, for example, a lower end plate 44 arranged at the bottom in the stack type 23 PEM electrolyser.
[0084] The PEM electrolyser of stack type 23 is operated as a flow reactor in electrolysis mode. Water is continuously fed to the PEM electrolyser of stack type 23 and water is discharged from the PEM electrolyser cells of stack type 23. Water has to be distributed from the water inlet (= water inlet) 39 of the PEM electrolyser of stack type 23 to the flow channel type I 14. At the same time, water has to be sent from the I-type water channel 14 to the water inlet (= water inlet) 40 for discharging the water. This requires space that may not be available for e.g. end plates 33 because they would be too thick and the PEM electrolyser of stack type 23 would be too heavy if the end plates 33 were too thick.
[0085] Problem to be solved by the invention The present invention is a lid 37 for a PEM electrolyzer of stack type 23. The lid 37 according to the present invention has a structure that creates as much space as possible for water without making the entire end plate 33 unnecessarily thick.
[0086] The subject of the present invention is a lid 37 for a PEM electrolyser of stack type 23, in which an end plate 33, for example an upper end plate 38, is provided with at least one water connection 39 for the introduction of water, at least one water connection 40 for the discharge of water and at least two distributor covers 41, the upper end plate 38 for forming a space for water has at least two spaces for water distribution in the end plate 42, each of the at least two distributor covers 41 having a space for water distribution in the distributor cover 43, at least one distributor cover 43 for the introduction of water into the PEM electrolyser of stack type 23 is connected to the at least one water connection 39 for the introduction of water and to the space for water distribution in the end plate 42, and at least one further distributor cover 43 for the discharge of water from the PEM electrolyser of stack type 23 is connected to the at least one water connection 40 for the discharge of water and to the space for water distribution in the end plate 42.
[0087] The subject of the invention is a PEM electrolyser of the stack type 23 according to the invention, which comprises a lid 37 according to the invention. The subject of the invention is a PEM electrolyser of the stack type 23 according to the invention, which comprises a lid 37 according to the invention.
[0088] In order to completely seal the individual frames 1 of the electrochemical cells 2 and the individual frames 1 of the PEM electrolyser of the stack type 23, especially at high pressures or high differential pressures, the end plates 33 or the upper end plate 38 and the lower end plate 44 must be supported with sufficient bolt force or contact pressure. The coating of the sealing material 22 then acts as a seal and completely seals the individual frames 1, the anode frame 8 and the cathode frame 11. If frames 1 with large frame surfaces are used, the contact pressure required to clamp the end plates 33 completely and seal them is even higher. In the case of frames 1 with large frame areas, the contact pressure is particularly high if the cores 21 of the anode frame and the cores 21 of the cathode frame are completely covered with the coating of the sealing material 22, i.e. if the area of the coating of the sealing material 22 on the first face 4 of the anode frame 8 is large and if the frames 1 have large first openings 6, i.e. if the first face of the first openings 27 is long and possibly also if the second face of the first openings 28 is long. A large frame area is, for example, 1600 cm 2or more. In a preferred embodiment, not the entire frame surface of the anode frame 8 is required for sealing. In a particular embodiment, not the entire frame surface of the cathode frame 11 is required for sealing. In order to reduce the contact pressure, the thickness of the coating of the seal material 22 can be reduced in the areas of the surface of the core 21 that are not required for sealing. The corresponding anode frame 8 or cathode frame 11 is composed of areas on the core 21 where the coating of the seal material 22 has a layer thickness and areas on the core 21 where the coating of the seal material 22'' has a reduced layer thickness compared to the layer thickness of the coating of the seal material 22 (FIG. 10b, FIG. 14). The layer thickness of the coating of the seal material 22'' in the areas of the surface of the core 21 that are not required for sealing is at least 0.05 mm, for example at least 0.1 mm, preferably at least 0.2 mm, less than the layer thickness of the coating of the seal material 22 in the areas of the surface of the core 21 that are required for sealing the active areas (active area = first and second openings 6 + 9) and the channels type I and type II 14 + 15. In order to reduce the contact pressure, the thickness of the coating of sealant 22 can be reduced in areas of the surface of the core 21 for the positive frame 11 or the negative frame 8 that are not required for sealing, for example in the following areas: For example, in the areas of the surface of the core 21 that are not required for sealing the active areas (first and second openings 6+9) and the channels type I and type II 14+15, the layer thickness of the coating of sealant 22″ is reduced by at least 0.05 mm, for example by at least 0.1 mm, preferably by at least 0.2 mm.
[0089] The areas of the surface of the core metal 21 of the anode frame 8 and / or the cathode frame 11 where the layer thickness of the coating made of the sealing material 22 is not reduced are mainly subjected to pressure when the stack-type electrolysis device 23 is clamped (Fig. 1, 10-15 MPa). The sealing areas where the coating made of the sealing material 22 on the surface of the core 21 has a layer thickness that is not reduced can be defined as areas of the surface of the core 21 that are located at a distance of 0.2 mm or more, for example 0.5 mm or 1 mm or more, preferably 1.5 mm or 2 mm or more, around the first inner opening 6 or the second inner opening 9, and around the channel type I 14 and the channel type II 15 (Fig. 10b, Fig. 14). The distances are various. The arrangement of the first opening 6, the second opening 9, the I-type flow channel 14, the distance to the II-type flow channel 15 may be the same or different, if the coating made of the sealing material 22 has a non-reduced layer thickness. In a particular embodiment, the coating of sealing material 22 can have a zero layer thickness in areas or parts of areas of the surface of the core 21 of the anode frame 8 or cathode frame 11 where the coating of sealing material 22″ has a reduced layer thickness, i.e. in a particular embodiment, in this area of the surface, the core 21 is not covered with the coating of sealing material 22″. By reducing the layer thickness of the coating of sealing material 22″ in a particular area of the surface of the core 21 of the anode frame 8 or cathode frame 11, the area that has to be compressed can be reduced by, for example, 50% compared to a coating of sealing material 22 completely covering the surface of the core 21 with the same layer thickness. This also reduces the contact pressure required to press the frame 1 of the PEM electrolyser of the stack type 23 by up to 50%.
[0090] A further advantage of the advantageous embodiment of the invention is the production costs. The channels type II 15 are not milled out of each anode frame 8 and each cathode frame 11, but are transferred once to a tool. One tool is the negative of the anode frame 8, another tool is the negative of the cathode frame 11. The type II channels 15 are transferred to the tool and virtually inserted, like a stamp, into a coating of a sealant 22, preferably rubber, for example EPDM. With the help of the tool, the metal core 21 is coated by vulcanization with a sealant, preferably rubber, for example EPDM, and the channels type II 15 are simultaneously produced in the desired areas of the anode frame 8 and / or cathode frame 11 according to the invention. The molded parts or rubber molded parts produced by vulcanization of the anode frame 8 and / or cathode frame 11 can be used directly and can be produced in large quantities at low cost. Alternatively, for example injection molding or 3D printing are known.
[0091] The PEM electrolyser of stack type 23 is preferably designed in such a way that all components have a smooth and homogeneous surface so that no voltage peaks arise in the CCM 13. In order to prevent the CCM 13 from creeping into the pores 24 of the PTL anode 7 and / or PTL cathode 10 under gas pressure, for example PTL anodes 7 and / or PTL cathodes 10 with pore diameters <0.1 mm are used. For example, so-called "microporous layers", i.e. PTLs with a particularly homogeneous surface, can be used as PTL anodes 7 and / or PTL cathodes 10.
[0092] Preferably, the PEM electrolyser of stack type 23 according to the invention is used for the electrolysis of water in the temperature range of 10 to 95 degrees Celsius, preferably in the temperature range of 40 to 80 degrees Celsius, particularly preferably in the temperature range of 68 to 72 degrees Celsius. The PEM electrolyser of stack type 23 according to the invention also has the advantage that the temperature difference from one side of the stack to the other is preferably at most 0-10°C, preferably at most 3-7°C, particularly preferably at most 4°C.
[0093] The anode frame 8 and the cathode frame 11 can be easily joined to form the assembled module 20, since the sealing and anode frame 8 or the sealing and cathode frame 11 are each made of one part. Preferably, the BPP 16 connected to the PTL anode 7, i.e. the BPP / anode 36, is used to manufacture the assembled module 20. For example, the BPP 16 and the PTL anode 7 are welded together, and the BPP 16 and the PTL anode 7 are present as one part BPP / PTL anode 36. To manufacture the assembled module 20, first the anode frame 8 is inserted or pressed onto the anode 7 or the PTL anode 7 of the BPP / PTL anode 36. For example, the anode frame 8, in addition to the first pin 19 as a means of connection to the cathode frame 11, can also have a second pin 19 as a means of connection to the BPP 16 or the BPP / PTL anode 36, which can be inserted into the BPP 16. For this purpose, the BPP 16 of the BPP 16 or BPP / PTL anode 36 is provided with corresponding means, preferably holes 18, for connection to the anode frame 8. The anode frame 8 with the inserted or pressed-in PTL anode 7 and the BPP 16 or BPP / PTL anode 36 is then turned over and the cathode frame 11 is also inserted on the other side of the anode frame 8 with its connection means to the anode frame, preferably holes 18, so that it can be connected to the anode frame 8. The PTL cathode 10 is then inserted or pressed into the cathode frame 11 (FIG. 6). An assembled module 20 is obtained. The assembled modules 20 can be stacked alternately with the CCMs 13, for example via centering pins, in order to produce a stack of assembled modules 3 or a PEM electrolyser of stack type 23.
[0094] Reference sign Frame 1 PEM electrolysis cell 2 Stack of 20 pre-assembled modules 3 Frame 1, Side 1 4 The surface 4'' opposite to the first surface 4 of the anode frame 8 Frame 1, Side 2 5 A surface 5'' opposite to the second surface 5 of the cathode frame 11 First Opening 6 Porous transport layer (PTL) anode 7 Single PTL Anode 7' Anode Frame 8 Second Opening 9 Porous Transport Layer (PTL) Cathode 10 Single PTL cathode 10' Cathode Frame 11 Step 12 Catalyst Coated Membrane (CCM) 13 Channel Type I 14 Channel Type II 15 Bipolar Plate (BPP) 16 Gap 17 Holes 18 Pin 19 Pre-assembled Modules 20 Core 21 Coating with sealant 22 The thickness of the coating of the sealant 22 was reduced. Stacked PEM electrolysis equipment 23 Crawl 24 Rubber Lip 25 Elevation between two waterways Type II 15 26 Circumferential ridges for improved sealing around active areas 26 26'' First side surface 27 of first opening 6 of anode frame 8 A first side surface 27' of the second opening 9 of the cathode frame 11 A second side surface 28 of the first opening 6 of the anode frame 8 A second side surface 28' of the second opening 9 of the cathode frame 11 Third side surface 29 of first opening 6 of anode frame 8 The third side surface 29' of the second opening 9 of the cathode frame 11 The fourth side surface 30 of the first opening 6 of the anode frame 8 The fourth side surface 30' of the second opening 9 of the positive electrode frame 11 Channel Edge Type I14 31 Insulation Panels 32 End Plate 33 Tie rod 34 Current collector 35 BPP 16 and PTL anode 7 are connected (= BPP / PTL anode) 36 Lid for stacked PEM electrolysis unit 23 37 Upper end plate 38 Water connection for water introduction (=water connection input) 39 Discharge water connection port (= water connection port) 40 Distributor cover 41 Water distribution space 42 on upper end plate 38 Water distribution space inside distributor cover 43 Lower end plate 44 [Brief description of the drawings]
[0095] [Figure 1] Classical structure of a PEM electrolysis cell according to state of the art with a frame 1, a catalyst coated membrane (CCM) 13, a bipolar plate (BPP) 16, a PTL anode 7, a PTL cathode 10 with a gap 17 between the frame 1 and the PTL anode 7 and between the frame 1 and the PTL cathode 10. The frame 1 is provided with I-shaped channels 14 for supplying and removing water and gases. [Diagram 2] Frame 1 was deformed, large gaps 17 were formed between frame 1 and PTL anode 7 and between frame 1 and PTL cathode 10, and crawling 24 of CCM 13 entered into the enlarged gaps 17 between frame 1 and PTL anode 7 and between frame 1 and PTL cathode 10 of frame 1 according to FIG. [Figure 3a] FIG. 1 shows a part of a frame 1 according to the invention, which consists of a core 21 covered with a coating of sealing material 22 in which a channel type II 15 is formed. [Figure 3b] 1 shows a part of a frame 1 according to the invention. The frame 1 consists of a core 21 coated with a coating made of a sealant 22 and a part 15 of a channel type II in the coating made of the sealant 22. [Figure 4] The cathode frame 11 according to the invention shown here has a second opening 9 bordered by a first side 27', a second side 28', a third side 29' and a fourth side 30' of the cathode frame 11. The cathode frame 11 consists of two holes 18 as connecting elements for connecting with the anode frame 8 and 20 channels of type I 14. On the second side 5, the cathode frame 11 has a number of channels of type II 15 connecting the second opening 9 to ten channels of type I 14, each of which is connected to the second opening 9 by a number of channels of type II 15. On the side of the cathode frame 5'' opposite to the second side 5, there are no type II channels 15 connecting the I-type channels 14 with the second opening 9. [Diagram 5] The anode frame 8 according to the invention shown here has a first opening 6 bordered by a first side 27, a second side 28, a third side 29 and a fourth side 30 of the anode frame 8. The anode frame 8 comprises two pins 19 as connecting elements for connection to the cathode frame 11 and, in this embodiment, furthermore 20 channels of type I 14, arranged so that when the anode frame 8 and the cathode frame 11 are connected, they can interact with the 20 channels of type I 14 of the cathode frame 11 for the supply and removal of water and gas. The anode frame 8 comprises II-type channels 15 on the first side 4, connecting the first opening 6 with the ten channels of type I 14. On the side opposite to the first side 4 of the anode frame 4 ″, there are no II-type channels 15 connecting the I-type channels 14 with the first opening 6. The anode frame 8 comprises a coating of a sealant 22, preferably made of rubber. The anode frame 8 is provided with a lip 25 made of a sealing material, preferably rubber. [Figure 6]Schematic showing a method for manufacturing an assembled module 20 with process steps: a) initial position; b) first step: inserting pins 19 of anode frame 8 into holes 19 of BPP / PTL anode 36; c) second step: turning over the arrangement from b) reveals the BPP 16 side of BPP / PTL anode 36; d) third step: inserting cathode frame 11 into arrangement; e) fourth step: inserting PTL cathode 10 into second opening 9. [Figure 7] Exploded perspective view of the assembled module 20. The parts that make up the assembled module 20 are visible: cathode frame 11, anode frame 8, BPP / PTL anode 36, PTL cathode 10. The arrangement of the cathode frame 11, anode frame 8, BPP / PTL anode 36, PTL cathode 10 in the assembled module 20 is shown. The order in which the individual parts are preferably assembled is also shown. The type II channels 15 of the cathode frame 11 are arranged on the side opposite to the visible side of the cathode frame 11. This is the second side of the frame 5. They are not visible from this point of view. Their arrangement on the second side of the frame 5 is shown in light grey on the side opposite to the second side of the cathode frame 5''. [Figure 7a] The assembled module 20 is shown in plan view. All four parts belonging to the assembled module 20 are visible: cathode frame 11, anode frame 8, BPP / PTL anode (36), PTL cathode 10. The type II channels 15 are not visible in the assembled module 20, since they are all arranged towards the BPP / PTL anode 36 and therefore inside the assembled module 20. The arrangement of the channels type II 15 inside the module 20 is shown in light grey on the visible side of the cathode frame 11 (= second side of the cathode frame = side of the frame opposite to 5''). [Figure 7b]Side view of assembled module 20. Anode frame 8 and cathode frame 11 are connected. PTL anode 7 is inserted into anode frame 8 and PTL cathode 10 is inserted into cathode frame 11. BPP 16 is placed between anode frame 8 and cathode frame 11. Anode frame 8 and cathode frame 11 form a step 12 because first opening 6 is larger than second opening 9. BPP 16 is placed on PTL cathode 10, step 12 and cathode frame 11 and rests its other side on PTL anode 7 and anode frame 8. [Figure 7c] FIG. 7b is an enlarged cross-sectional view of a portion of assembled module 20, clearly showing step 12. [Figure 8] Figure 1 shows a cross-section of the schematic structure of a stack-type PEM electrolyser according to the invention, i.e. a stack of assembled modules 3. The arrangement shows a stack with three PEM electrolysis cells 2. The arrows indicate the direction of gas pressure during high-pressure hydrogen electrolysis, which is carried out under a differential pressure of 40 bar. [Figure 8a] FIG. 1 is an enlarged cross-sectional view of a portion of a PEM electrolyser 2 having a step 12. The arrows indicate the direction in which increased pressure acts on a CCM 13 due to a pressure difference. [Figure 9a] Exemplary dimensions of the cathode frame 11. Channel type II 15 connects the second opening 9 with channel type I 14, which are arranged along the second side of the second opening 28' and along the fourth side of the second opening 30'. In each case, multiple type II channels 15 connect the second opening 9 with the type I channels 14. The individual type II channels 15 are separated from each other by pedestals 26. [Figure 9b] Exemplary dimensions of the anode frame 8, which corresponds to the cathode frame 11 shown in Fig. 9a. The channel type II 15 connects the first openings 6 with the channel type I 14, which are arranged along a first side of the first openings 27 and along a third side of the first openings 29. In each case several type II channels 15 connect the first openings 6 and the type I channels 14. The individual type II channels 15 are separated from each other by pedestals 26. [Figure 10a] 1 shows an embodiment of an anode frame 8. The anode frame 8 is composed of a type I channel 14 and a type II channel 15, with the type II channels 14 arranged in a sector shape on the first side of the frame 4. In this embodiment, the anode frame 8 is rectangular and composed of a rectangular first opening 6 and 20 channels of type I 14, with 5 of the channel types I 14 arranged on each of the four sides of the anode frame, i.e., the first side of the first opening 27 is composed of 5 channels of type I 14, the second side of the first opening 28 is composed of 5 channels of type I 14, the third side of the first opening 29 is composed of 5 channels of type I 14, and the fourth side of the first opening 30 is composed of 5 channels of type I 14. On two opposite sides of the anode frame 8, the 5 channels of type II 14 are each connected to 8 channels of type II 15. Each channel type II 15 is connected to a channel type I 14 and a first opening 6. The type II channels 15 are arranged in a fan shape on the first side surface of the frame 4 , and are equally spaced apart along the first side surface of the first opening 27 and the third side surface of the first opening 29 . [Figure 10b]The anode frame 8 is shown. The anode frame 8 is made of channels type I 14, some of which have a circular shape and some of which have an elliptical shape. The anode frame 8 is provided with a coating 22 of sealant arranged on a core 21 (core not shown) of the anode frame 8. The coating of sealant 22 has a layer thickness, which is shown as a bordered area. The line surrounding the bordered area is a circumferential height 26 for enhancing the sealing effect around the active area 26''. The area of the anode frame 8 surrounding the channels type I 14 and II 15 and the first opening 6 is covered with a coating of sealant 22 with a layer thickness. The thickness of the coating 22 of sealant on the core 21 in this area of the anode frame 8 is 1.2 mm. The remaining part of the core 21 of the anode frame 6 (shown outside the border and labeled 22') has a reduced thickness 22'' of the coating of the sealant 22 compared to the thickness of the coating of the sealant 22. The reduced thickness of the coating of the sealant 22'' on the core 21 in this region of the anode frame 8 is 0.3 mm. [Figure 10c] The anode frame 8 is shown in a perspective side view. It shows the channel type II 15, which is designed as a recess in a coating made of a sealant 22 with a defined layer thickness in this area of the anode frame 8. The individual adjacent channels of type II 15 are separated by plateaus (= areas with a coating made of a sealant 22 with a defined layer thickness). [Figure 10d] A cross section of the anode frame 8 is shown in FIG. 10c. [Figure 10e] 1 shows a cathode frame 11. The cathode frame 11 consists of an I-shaped channel 14, some of which have a round shape and some of which have an elliptical shape. The elliptical I-shaped channel 14 is connected to a second opening 9 through a II-shaped channel 15. The cathode frame 11 consists of a rubber lip 25 to isolate a single voltage measurement. The anode frame 8 can have a similar arrangement. [Figure 11]An embodiment of an assembled module 20 (shown without the PTL cathode 10 and without the CCM 13) consisting of a cathode frame 11 and an anode frame 8 is shown. A step 12 is formed by the difference in size between the first opening 6 and the second opening 9. A type II channel 15 is located in part of the step 12, but is only partially visible because it is covered by the anode frame 11. [Figure 12] A PEM electrolyser of stack type 23 according to the invention is shown, comprising a stack of PEM electrolyser cells 2, insulating plates 32, end plates 33, tie rods 34 and current collecting plates 35. [Figure 13] A preferred embodiment of a PTL anode 7 is shown, where a BPP 16 is connected to the anode 7 to form a BPP / PTL anode 36 . [Figure 14] 10b shows the pressure distribution in a PEM electrolysis cell 2 according to the invention with an anode frame 8 as shown. The cell was clamped with a defined torque between two end plates 33. Instead of the CCM 13, a pressure-sensitive foil was placed between the anode frame 8 and the matching cathode frame 11, which triggers differently at different pressures. By evaluating the pressure-sensitive foil, it was determined which pressures prevail in which areas of the anode frame 8. The highest pressures of 10-15 MPa are in the areas of the anode frame 8 where the core 21 is covered with a coating made of sealing material 22, i.e., for example, along the first side of the first opening 27 and along the second side of the first opening 29 and in the area around the channel type I 14. This area of the anode frame 8 has a layer thickness of 0.2 mm greater than the areas with a reduced layer thickness of the coating made of sealing material 22 ″. The channel type II 15 connecting the first opening 6 to the channel type I 14 and the area where the plateau 26 is located are excluded from this. In this region, the pressure is only 1-2 MPa. At the outer edge of the anode frame 8, in the region where the core 21 is coated with a reduced layer thickness compared to the coating of the sealing material 22 (=reduced layer thickness of the coating of the sealing material 22″), the pressure is even lower, at 0.1-0.5 MPa. [Figure 15a]A lid 37 according to the invention for a PEM electrolyser of stack type 23 is shown. The lid 37 consists of an end plate 33, e.g. an upper end plate 38, which is connected to two distributor covers 41, one distributor cover 41 constituting the water connection for the input 39 and the other distributor cover 41 constituting the water connection for the outlet 40. [Figure 15b] The lid 37 of the PEM electrolyser of stack type 23 is shown with the distributor cover 41 removed so that the water distribution space in the end plate 42 and the I-shaped flow path 14 connected to the water distribution space in the end plate 42 are visible in the end plate 33. [Figure 15c] FIG. 2 shows a distributor cover 41 for a lid 37 according to the invention for a PEM electrolyser of stack type 23, where the space for water distribution in the distributor cover 43 is visible. [Figure 15d] A simulation of how water is distributed in the lid 37 according to the invention, also showing the different flow rates at different points of the lid 37 and at the transition to the I-channel 14. [Figure 16] 1 shows an anode frame 7 with type I channels 14 and type II channels 15 arranged thereon, as well as areas coated with a sealant 22 and areas coated with a reduced thickness sealant 22''. The type II channels 15 connect a portion of the type I channels 14 to the first opening 6. The channels are spaced apart along a first side of the first opening 27 and along a third side of the first opening 29, such that each channel type II 15 introduces water or expels water and gas to the same area of the first opening 6 or active area. [Figure 16a] FIG. 17 is an enlarged cross-sectional view of the anode frame of FIG. 16. [Figure 16b] FIG. 17 is an enlarged cross-sectional view of the anode frame of FIG. 16. [Figure 16c] FIG. 17 is an enlarged cross-sectional view of the anode frame of FIG. 16. [Figure 17]A cathode frame 11 is shown with type I channels 14 and type II channels 15, as well as areas coated with a sealant 22 and areas coated with a reduced thickness sealant 22''. The type II channels 15 connect parts of the type I channels 14 to the second opening 9. They are spaced apart along a second side of the second opening 28' and along a fourth side of the second opening 30' such that each channel type II 15 introduces water or expels water and gas to the same area of the first opening 6 or active area.
Claims
1. A frame (1) for a PEM electrolysis cell (2) for a stacked PEM electrolysis device (23), comprising: The frame (1) comprises a first side (4) having a planar first surface, a second side (5) opposite the first side (4) having a planar second surface, an anode frame (8) and a cathode frame (11); the anode frame having a first side (4), a side of the anode frame (4'') opposite the first side (4), and a first opening (6) for receiving a porous transport layer (PTL) anode (7), the first opening (6) extending from the first side (4) to the opposite side of the anode frame (4''); the cathode frame (11) has a second surface (5), a side opposite the second side (5) of the cathode frame (5''), and a second opening (9) for receiving the PTL cathode (10), the second opening (9) extending from the second side (5) to the opposite side of the cathode frame (5''); a side of the anode frame (4'') facing the first side (4) and a side of the cathode frame (5'') facing the second side (5) are disposed adjacent to each other; The anode frame (8) and the cathode frame (11) are connected to each other, The first opening (6) and the second opening (9) are connected to each other; 1. A frame (1), characterized in that the first opening (6) is larger than the second opening (9), the anode frame (8) and the cathode frame (11) are arranged such that a side facing the first side (4) of the anode frame (4'') and a side facing the second side (5) of the cathode frame (5'') form a step (12) at the transition from the anode frame (8) to the cathode frame (11), the step (12) forming a planar third surface as a support surface for a catalytically coated membrane (CCM) (13), the anode frame (8) consisting of a coating made of a core (21') and a sealing material (22) and the cathode frame (11) consisting of a coating made of a core (21'') and a sealing material (22).
2. It comprises one or more type I channels (14) for transporting water into the frame (1) and water and gas out of the frame (1), and one or more type II channels (15) for transporting water into the first opening (6) and water and oxygen out of the first opening (6), wherein the type I channels (14) are not connected to the first opening (6) of the anode frame (8) or the second opening (9) of the cathode frame (11), 2. The frame (1) according to claim 1, wherein the anode frame (8) comprises, on a surface of the first side (4), one or more channels type II (15) connected to one or more channels type I (14) and connecting the channels type I (14) with the first opening (6), and arranged towards the bipolar plates (BPPs) (16) when the frame (1) is installed in a PEM electrolysis cell (2) or a stacked PEM electrolysis device (23), the side opposite to the first side (4) of the anode frame (4'') being devoid of channels type II (15).
3. one or more type I channels (14) for the transport of water into the frame (1) and water and gas out of the frame (1) and one or more type II channels (15) for the transport of hydrogen from the second opening (9), the type I channels (14) being not connected to the first opening (6) of the anode frame (8) or the second opening (9) of the cathode frame (11); 3. A frame (1) according to claim 1 or 2, wherein the cathode frame (11) comprises, on the surface of the second side (5), one or more channels type II (15) connected to one or more channels type I (14) and connecting the channels type I (14) with the second opening (9), and arranged towards the bipolar plates (BPP) (16) when the frame (1) is installed in a PEM electrolysis cell (2) or a stacked PEM electrolysis device (23), and wherein there are no channels type II (15) on the side facing the second side (5) of the cathode frame (5'').
4. a first opening (6) defined by a first side (27), a second side (28), a third side (29) and a fourth side (30); For a uniform flow of water through the first openings (6) and for a constant removal of heat of reaction from the first openings (6), each type I channel (14) connected to the first openings (6) is connected to the first openings (6) by at least two type II channels (15), 4. A frame (1) according to claim 2 or 3, wherein the channels type II (15) are arranged adjacent to each other on a first side (4) of the frame, the distance between two adjacent channels type II (15) on a first side (27) of the first opening being ≦3 mm and the distance between two adjacent channels type II (15) on a third side (29) of the first opening being ≦3 mm.
5. a second opening (9) is formed by a first side (27'), a second side (28'), a third side (29') and a fourth side (30'), and each type I channel (14) connected to the second opening (9) is connected to the second opening (9) by at least two type II channels (15) for a uniform flow of water through the second opening (9) and for a constant removal of heat of reaction from the second opening (9); 5. A frame (1) according to claim 2, wherein the channels type II (15) are arranged adjacent to each other on the second side (5) of the frame, the distance between two adjacent channels type II (15) on the second side (28') of the second opening being ≦3 mm and the distance between two adjacent channels type II (15) on the fourth side (30') of the second opening being ≦3 mm.
6. 6. A frame (1) according to claim 4 or 5, wherein the distances between adjacent channels type II (15) on the first side (27) of the first opening and on the third side (29) of the first opening are equal, and optionally the distances between adjacent channels type II (15) on the second side (28') of the second opening and on the fourth side (30') of the second opening are equal.
7. at least two type II channels (15) between a first side (27) of the first opening and a type I channel (14) connected to the first opening (6) by said at least two type II channels (15) are arranged in a sector shape; at least two type II channels (15) between a third side (29) of the first opening and a type I channel (14) connected to the first opening (6) by said at least two type II channels (15) are arranged in a sector shape; Optionally, at least two type II channels (15) between the second side (28') of the second opening and the type I channel (14) connected to the second opening (9) by these at least two type II channels (15) are arranged in a fan shape; 7. The frame (1) according to any one of claims 4 to 6, wherein the at least two channels type II (15) between the fourth side (30') of the second opening and the channel type I (14) connected to the second opening (9) by these at least two channels type II (15) are arranged in a fan shape.
8. The core (21) of the anode frame (8) is made of metal, and the core (21) of the cathode frame (11) is made of metal; 8. A frame (1) according to any one of the preceding claims, wherein the anode frame (8) comprises a sealing material coating (22) which is a rubber coating and the cathode frame (11) comprises a sealing material coating (22) which is a rubber coating.
9. 9. A frame (1) according to any one of claims 1 to 8, wherein in order to reduce the contact pressure, a portion of the sealant coating (22) of the anode frame (8) has a reduced layer thickness of the sealant coating (22'') compared to the layer thickness of the sealant coating (22) and / or in order to reduce the contact pressure, a portion of the sealant coating (22) of the cathode frame (11) has a reduced layer thickness of the sealant coating (22'') compared to the layer thickness of the sealant coating (22).
10. 10. The frame (1) according to claim 9, wherein the sealing material coating (22) on the part of the anode frame (8) has a circumferential height (26') to enhance the sealing effect, said circumferential height (26') surrounding the first opening (6) and / or the sealing material coating (22) on the part of the cathode frame (11) has a circumferential height (26') to enhance the sealing effect, said circumferential height (26') surrounding the second opening (9).
11. The anode frame (8) comprises one or more connection elements, e.g. one or more pins (19), for connection to the cathode frame (11), and the cathode frame (11) comprises one or more connection elements, e.g. one or more holes (18), for connection to the anode frame (8); A frame (1) according to any one of claims 1 to 10, wherein the connecting elements are arranged such that the anode frame (8) and the cathode frame (11) can be connected to each other, for example the pins (19) and holes (18) are arranged such that the holes (18) of the cathode frame (11) can be connected to the pins (19) of the anode frame (8), thereby allowing the anode frame (8) and the cathode frame (11) to be connected to each other.
12. A PEM electrolysis cell (2) for producing high pressure hydrogen, comprising a CCM (13), a PTL anode (7) and a PTL cathode (10), the PEM electrolysis cell (2) operating under a differential pressure of up to 40 bar, A PEM electrolysis cell (2) comprising a frame (1) according to any one of claims 1 to 11, the first opening (6) of the anode frame (8) constitutes a PTL anode (7), the second opening (9) of the cathode frame (11) constitutes a PTL cathode (10), and the CCM (13) is disposed between a side of the anode frame (4'') facing the first side (4) and a side of the cathode frame (5'') facing the second side (5); A PEM electrolysis cell (2), characterized in that one side of the CCM (13) rests on a PTL anode (7) and the other side of the CCM (13) rests on a step (12) and a PTL cathode (10).
13. 13. The PEM electrolysis cell (2) of claim 12, wherein the CCM (13) has a thickness of 80 μm or less, such as 50 μm or less.
14. A pre-assembled module (20) for manufacturing a stacked electrolysis device (23) consisting of an anode frame (8), a cathode frame (11), a BPP (16), a PTL anode (7) and a PTL cathode (10), the anode frame (8) comprises a first side (4) having a planar first surface, a side of the anode frame (4'') opposite the first side (4), and a first opening (6) for receiving a PTL anode (7), the first opening (6) extending from the first side (4) to a side of the anode frame (4'') opposite the first side (4), the first opening (6) being bordered by the anode frame (8), the anode frame (8) comprising at least one connection element, preferably a pin (19), for connection to a cathode frame (11); a cathode frame (11) having a second side (5) with a planar second surface, a side of the cathode frame (5'') opposite the second side (5), and a second opening (9) for receiving a PTL cathode (10), the second opening (9) extending from the second side (5) to a side of the cathode frame (5'') opposite the second side (5), the second opening (9) being bordered by the cathode frame (10), the cathode frame (11) comprising a hole (18) for receiving at least one connection element, preferably a pin (19), for connection to the anode frame (8); The BPP (16) is disposed between the first side (4) and the second side (5); The anode frame (8) comprises a core (21) and a sealing material coating (22), preferably a rubber coating, preferably a BPP (16) connected to a PTL anode (7) to form a BPP / PTL anode (36), the PTL anode (7) being inserted or pressed into the first opening (6) and framed by the anode frame (8); The cathode frame (10) comprises a core (21) and a sealing material coating (22), preferably a rubber coating, and the PTL cathode (10) is inserted or pressed into the second opening (9) and is framed by the cathode frame (11); the connecting elements of the anode frame (8) are connected to the connecting elements of the cathode frame (11), preferably with at least one pin (19) inserted into at least one hole (18), the anode frame (8) and the cathode frame (11) being thereby connected to each other; the first opening (6) is larger than the second opening (9), the anode frame (8) and the cathode frame (11) are arranged such that the first side (4) and the second side (5) form a step (12) at the transition from the anode frame (8) to the cathode frame (11), the step (12) forming a planar third surface as a support surface for the CCM (13); An assembled module (20) characterized in that the BPP (16) rests on the one hand on the PTL anode (7) and the anode frame (8) and on the other hand on the PTL cathode (10), the cathode frame (11) and the step (12).
15. A method for manufacturing an assembled module (20), comprising the steps of: a) forming a first insulating layer on the first substrate; a) a metallic core (21) is manufactured for an anode frame (8), the core (21) comprising a first side (4) having a planar first surface and a side facing the first side (4) of the anode frame (4''), the first side (4) of the anode frame (4'') and the side facing the first side (4) defining a first opening (6) extending from the first side (4) to the side facing the first side (4) of the anode frame (4'') and bordered by the anode frame (8), in which one or more channels type I (14) for the supply and removal of water and gases are formed, the channels type I (14) being not connected to the first opening (6) of the anode frame (8), the anode frame (8) comprising at least one connection element, preferably at least one pin (19), for connection to a cathode frame (11), b) all or part of the surface of the metallic core (21) produced according to a), preferably at least 90% of the surface of the metallic core (21) produced according to a), is fully or partially coated with natural or synthetic rubber for the anode frame (8) for forming a rubber coating by vulcanization and then vulcanized, whereby a rubber coating is formed on the metallic core (21) as a sealant (22), in which one or more type II channels (15) are formed on the surface of the first side (4), which type II channels (15) are connected to one or more type I channels (14) and connect the type I channels (14) with the first opening (6), and are arranged in the direction of the BPP (16) when the anode frame (8) is installed in the PEM electrolysis cell (2) or stacked PEM electrolysis device (23), and no type II channels (15') are formed in the rubber coating on the side facing the first side (4) of the anode frame (4''); c) placing or pressing a PTL anode (7) into the anode frame (8) produced according to a) and b), the PTL anode (7) being preferably connected to a BPP (16) to form a BPP / PTL anode (36); d) a metallic core (21) is manufactured for a cathode frame (11), the metallic core (21) comprising a second side (5) having a planar second surface and a side facing the second side (5) of the cathode frame (5''), the second side (5) and the side facing the second side (5) of the cathode frame (5'') constituting a second opening (9) extending from the second side (5) to the side facing the second side (5) of the cathode frame (5'') and bordered by the cathode frame (11), in which one or more channels type I (14) for the supply and removal of water and gases are formed, the channels type I (14) being not connected to the second opening (9) of the cathode frame (11), the cathode frame (11) comprising at least one connection element, preferably at least one hole (18), for connection to an anode frame (8); e) all or part of the surface of the metal core (21) produced according to d), preferably at least 90% of the surface of the metal core (21) produced according to d) for a cathode frame (11) for forming a rubber coating by vulcanization, is fully or partially coated with natural or synthetic rubber and then vulcanized, whereby a rubber coating is formed on the metal core (21) as a sealant (22), in which one or more type II channels (15'') are formed on the surface of the second side (5), which type II channels are connected to one or more type I channels (14) and connect the type I channels (14) with the second opening (9), the cathode frame (11) being arranged in the direction of the BPP (16) when installed in the PEM electrolysis cell (2) or stacked PEM electrolysis device (23), and no type II channels (15'') are formed in the rubber coating on the side of the cathode frame (5'') facing the second side (5); f) the cathode frame (11) manufactured according to d) and e) is connected to the anode frame (8) manufactured according to a) to c) by at least one connecting element of the cathode frame (11), preferably at least one hole (19), by at least one connecting element of the anode frame (8), preferably at least one pin (18), preferably at least one hole (19) being plugged onto at least one pin (18), the cathode frame (11) thereby being connected to the anode frame (8), a BPP (16) is placed between the first side (4) and the second side (5), a PTL cathode (10) is inserted or pressed into the cathode frame (11), the first opening (6) is larger than the second opening (9), and the anode frame (8) and the cathode frame (11) are arranged such that the side of the anode frame (4) facing the first side (4'') and the side of the cathode frame (5) facing the second side (5'') form a step (12) at the transition from the anode frame (8) to the cathode frame (11).
16. A method for producing a stacked PEM electrolysis device (23) operated under a pressure difference to produce high-pressure hydrogen, comprising the steps of: a) at least x preassembled modules (20) according to claim 14 or at least x+1 manufacturable CCMs (13) according to claim 15 are stacked alternately on top of one another to produce a stack (3) of preassembled modules, in which one preassembled module (20) and one CCM (13) are stacked alternately on top of one another in the stack of preassembled modules (3), one CCM (13) is arranged on the upper and lower sides of the stack of preassembled modules (3) and one CCM (13) is arranged between every two adjacent preassembled modules (20), b) a half-cell anode, preferably a single anode (7') and anode frame (8) are arranged parallel to the outer CCM (13) on one side of the stack of assembled modules (3) and a half-cell cathode, preferably a single cathode (10') and cathode frame (11) are arranged parallel to the outer CCM (13) on the other side of the stack of assembled modules (3); c) end plates (33) are placed parallel to the half-cell anode and parallel to the half-cell cathode, and the formed stack is compressed between the two end plates (33) to form a stacked device (23); where x is an integer, ≧2.
17. A stacked PEM electrolyser (23) operating under differential pressure to produce high pressure hydrogen, comprising: A system comprising: x preassembled modules (20) according to claim 14; or x+1 manufacturable CCMs (13) according to claim 15; a single anode; a single cathode; and two end plates (33); x assembled modules (20) and x+1 CCMs (13) are stacked alternately on top of each other to form a stack of assembled modules (3), one assembled module (20) and one CCM (13) being stacked alternately one on top of the other in the stack of assembled modules (3); One CCM (13) is disposed on each of the upper and lower sides of the stack of assembled modules (3), and one CCM (13) is disposed between two adjacent assembled modules (20); A single anode is disposed parallel to the outer CCM (13) on one side of the stack of assembled modules (3) and a single cathode is disposed parallel to the outer CCM (13) on the other side of the stack of assembled modules (3); Stacked PEM electrolyser (23), characterized in that the end plates (33) are each arranged parallel to a single anode and parallel to a single cathode, and the formed stack is compressed between the two end plates (33) to form a stacked PEM electrolyser (23). where x is an integer and is ≧2.
18. A stack-type electrolysis device (23) operating under differential pressure for producing high-pressure hydrogen, comprising:
14. A system comprising: x+1 PEM electrolysis cells (2) according to claim 12 or 13, said PEM cells (2) having x+1 CCMs (13) and x-1 BPPs (16), and upper and lower end plates (38 and 44); x+1 PEM electrolysis cells (2) and x-1 BPPs (16) are alternately stacked one on top of the other in a stack, one PEM electrolysis cell (2) and one BPP (16) are alternately stacked on top of each other in the stack, one BPP (16) is located at the top and bottom of the stack, and one BPP (16) is located between two adjacent PEM electrolysis cells (2); A stacked PEM electrolyser (23), characterized in that an upper end plate (38) is arranged parallel to the BPP (16) above the stack, and a lower end plate (44) is arranged parallel to the BPP (16) below the stack, and the formed stack is compressed between the upper end plate (38) and the lower end plate (44) to form a stacked PEM electrolyser (23). where x is an integer, ≧2.
19. A stacked PEM electrolyser (23) according to claim 17 or 18 or producible according to claim 16, A stacked PEM electrolyser (23), wherein each of the x+1 CCMs (13) in the stacked PEM electrolyser (23) has a thickness of 80 μm or less, and preferably has a thickness of 50 μm or less.
20. It consists of two end plates (33), preferably an upper end plate (38) arranged on the upper side of the stack and a lower end plate (44) arranged on the lower side of the stack, at least one end plate (33), preferably the upper end plate (38), is provided with at least one water connection (39) for the introduction of water and at least one water connection (40) for the discharge of water and at least two distributor covers (41), At least one end plate (33) for providing a space for water has at least two spaces for water distribution within the at least one end plate (33); Each of the at least two distributor covers (41) has a space for distributing water within the distributor cover (43); At least one distributor cover (43) for the introduction of water into the stacked PEM electrolysis device (23) is connected to at least one water connection (39) for the introduction of water and to a space for the distribution of water in the end plate (42); 20. The stacked PEM electrolyser (23) according to any one of claims 17 to 19, wherein at least one further distributor cover (43) for the discharge of water from the stacked PEM electrolyser (23) is connected to at least one water connection (40) for the discharge of water and to the space for water distribution in the end plate (42).
21. A lid (37) for a stacked PEM electrolyser according to any one of claims 17 to 19, wherein an end plate (33), e.g. an upper end plate (38), comprises at least one water connection (39) for introducing water into the stacked PEM electrolyser (23), at least one water connection (40) for draining water from the stacked PEM electrolyser (23), and at least two distributor covers (41), The end plate (33) is provided with at least two distribution spaces to provide space for water; Each of the at least two distributor covers (41) has a space for distributing water within the distributor cover (43); At least one distributor cover (43) for the introduction of water into the stacked PEM electrolysis device (23) has at least one water connection (39) for the introduction of water and a space for the distribution of water in the end plate (33); At least one further distributor cover (43) for the discharge of water from the stacked PEM electrolyser (23) is connected to at least one water connection (40) for the discharge of water and to a space for the distribution of water in the end plate (33).
Citation Information
Patent Citations
High -performance oxyhydrogen generator
CN207079283U
Electrode system
EP3699323A1
2 denkyokuzaiojusurudenkaiso
JP1976044571A
Holder for ion exchange membrane
JP1978146272A
Ion-exchange membrane electrolytic cell equipped with gas diffusion electrode
JP2004285427A
Cited By
Method for producing plate assemblies, plate assemblies, and corresponding electrochemical cells
JP2026517932A
