Molybdenum Precursor Compounds

Molybdenum alkanoate compounds in combination with gases facilitate efficient deposition of high-purity molybdenum films on microelectronic substrates, addressing volatility and stability issues in existing deposition methods, enhancing semiconductor manufacturing efficiency.

JP2024544133AActive Publication Date: 2024-11-28ENTEGRIS INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024527439
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-10
Filing Date
2022-11-07
Publication Date
2024-11-28
Estimated Expiration
2042-11-07

AI Technical Summary

Technical Problem

Existing deposition methods for molybdenum-containing films face challenges with liquid and solid precursors, particularly in achieving sufficient volatility, thermal stability, reactivity, and compatibility for efficient vapor deposition in semiconductor manufacturing, necessitating improved molybdenum delivery reagents and process parameters.

Method used

The use of molybdenum-containing alkanoate compounds, represented by formula (I), in combination with reducing and oxidizing gases, allows for the deposition of high-purity molybdenum films through chemical vapor deposition (CVD) and atomic layer deposition (ALD) methods, ensuring high deposition rates and conformal step coverage on microelectronic device substrates.

Benefits of technology

The method enables the deposition of high-purity molybdenum films with controlled film resistivity, morphology, and stress, suitable for mass production of semiconductor products and flat panel displays, using compounds that are non-flammable, non-corrosive, and easy to handle.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024544133000001_ABST
    Figure 2024544133000001_ABST
Patent Text Reader

Abstract

The present invention provides certain molybdenum-containing compounds believed to be useful for the deposition of molybdenum-containing films on the surfaces of various microelectronic device substrates. In one aspect, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, comprising exposing the substrate to a compound of formula (I) as described herein in a reaction zone under deposition conditions.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Claiming priority This invention claims priority to U.S. Provisional Patent Application No. 63 / 277,829, filed November 10, 2021. This priority document is incorporated herein by reference.

[0002] The present invention relates to certain molybdenum compounds that are useful as precursors in the deposition of molybdenum-containing films on microelectronic device substrates. [Background technology]

[0003] Group 6 metals such as molybdenum, chromium, and tungsten are increasingly being utilized in the fabrication of semiconductor devices, including for use as diffusion barriers, electrodes, photomasks, power electronics substrates, low resistance gates, flat panel displays, and interconnects, due to their extremely high melting points, low coefficients of thermal expansion, low resistivity, and high thermal conductivity.

[0004] Such utility has motivated efforts to achieve deposition of molybdenum, chromium and tungsten films for such applications that are characterized by high conformality of the deposited films and high deposition rates to accommodate efficient high volume manufacturing operations. This has led to the development of improved molybdenum and tungsten delivery reagents useful in vapor deposition operations, and improved process parameters utilizing such reagents.

[0005] In atomic layer deposition (ALD) reactants and precursor molecules are introduced in alternating pulses into a reaction zone to form layers of the desired chemical composition. These precursors are delivered to the wafer in gaseous form. For precursors that are gaseous at standard temperatures and pressures, the method is well established. The precursor gas flows directly into the deposition chamber. The trend towards new interconnect materials requires a broader portfolio of precursors, many of which are liquids or solids at room temperature. These ALD precursors must have sufficient volatility, thermal stability, and reactivity with the substrate and the film being deposited. The vapor pressure of the precursor, whether liquid or solid, determines the process conditions.

[0006] Most liquid precursors are delivered at room temperature and vaporized by reducing the pressure. Liquids are generally easier to purify, handle and deliver than solid precursors. Therefore, many integrated device manufacturers (IDMs) prefer liquid delivery systems.

[0007] Solids are more difficult because the material and the gas lines that supply it must be heated. Ideally, the precursor should be non-flammable, non-corrosive, non-toxic, and easy and cheap to manufacture. Summary of the Invention

[0008] In summary, the present invention provides certain molybdenum-containing compounds believed to be useful for the deposition of molybdenum-containing films on the surfaces of various microelectronic device substrates. In one aspect, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, comprising reacting the substrate with a compound of formula (I) in a reaction zone under deposition conditions: TIFF2024544133000002.tif37170 [wherein each R is independently selected from (i) C1-C4 alkyl or (ii) C1-C4 alkyl substituted with one or more halogen atoms]; to thereby form a molybdenum-containing film on the substrate. [Brief description of the drawings]

[0009] [Figure 1] 1 is a graph showing a thermogravimetric analysis of a molybdenum (II) acetate dimer compound showing that 50% of the mass is evaporated by 310° C. [Diagram 2] FIG. 1 shows a thermogravimetric analysis of the common precursor HfCl4, showing that 50% of the mass is evaporated by 290° C.; therefore, molybdenum(II) acetate dimer can be delivered at similar temperatures in deposition techniques such as ALD. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless the content clearly dictates otherwise. As used in this specification and the appended claims, the term "or" is generally used in its sense including "and / or" unless the content clearly dictates otherwise.

[0011] The term "about" generally refers to a range of numbers that are considered equivalent to the stated value (e.g., having the same function or result). In many cases, the term "about" may include numbers that are rounded to the nearest significant figure.

[0012] Numeric ranges expressed using endpoints include all numbers subsumed within that range (eg, 1 to 5 includes 1, 1.5, 2, 2.75, 3, 3.80, 4, and 5).

[0013] In a first aspect, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, the method comprising exposing the substrate in a reaction zone to a compound of formula (I): TIFF2024544133000003.tif38170 [wherein each R is independently selected from (i) C1-C4 alkyl, or (ii) C1-C4 alkyl substituted with one or more halogen atoms; Under deposition conditions, a molybdenum-containing film forms on the substrate.

[0014] In one embodiment, each R is selected from methyl, tert-butyl, and trifluoromethyl.

[0015] The compounds of formula (I) shown above exist as dimers of molybdenum-containing alkanoates. In other words, the compounds of formula (I) have the empirical formula TIFF2024544133000004.tif20170 [wherein R is as defined above] has.

[0016] Many of the compounds of formula (I) are known and can be prepared by treating molybdenum hexacarbonyl (Mo(CO)6) with acetic acid (i.e., when R is methyl). Similarly, other carboxylic acids can be utilized for the corresponding R group of formula (I). (See, for example, Rhenium and Molybdenum Compounds Containing Quadruple Bonds, Alicia B. Brignole, FA Cotton, Z. Dori, Z. Dori, Z. Dori, G. Wilkinson; Book editor: FA Cotton; First edition: January 1, 1972; https: / / doi.org / 10.1002 / 9780470132449.ch15. Additionally, when R is methyl, the molybdenum(II) acetate dimer compound is commercially available from Sigma Aldrich (CAS number 14221-06-8).)

[0017] The compounds of formula (I) are believed to be useful for the chemical vapor deposition of molybdenum-containing films. In this regard, the term "molybdenum-containing" films are films comprised of one or more of molybdenum metal, molybdenum oxide, molybdenum carbide, and molybdenum nitride.

[0018] Chemical vapor deposition techniques include those referred to as chemical vapor deposition (CVD) and atomic layer deposition (ALD), including several derivative versions thereof, such as UV laser photodissociation CVD, plasma-assisted CVD, pulsed CVD, and plasma-assisted ALD, among others. In depositing high purity metals onto two-dimensional or three-dimensional microelectronic device substrates, these types of deposition techniques can be desirable due to the high purity of the deposited metal and the ability to provide good conformal step coverage over the often highly non-planar microelectronic device geometries.

[0019] In one embodiment, the molybdenum-containing film or layer deposited on the substrate surface can be formed, for example, by chemical vapor deposition, pulsed chemical vapor deposition (CVD) or atomic layer deposition (ALD), thus directly using vapor derived from the compound of formula (I).

[0020] In one embodiment, the compound of formula (I) is introduced together with a reducing gas into a reaction zone containing a microelectronic device substrate. The conditions of the reaction zone are selected such that the molybdenum contained in the precursor of formula (I) is deposited on the microelectronic device substrate as molybdenum metal. In one embodiment, the precursor and the reducing gas are continuously introduced into the reaction zone. In another embodiment, an oxidizing gas, such as oxygen, ozone, or a combination of water and hydrogen, can be introduced into the reaction zone to improve the composition of the deposited metal layer. Thus, the oxidizing gas is introduced in an amount and manner that reduces the amount of carbon deposited in the completed molybdenum layer. In one embodiment, the oxidizing gas is introduced intermittently in a pulsed manner. Further details of this technique can be found in U.S. Patent Publication No. 2020 / 0115798, which is incorporated herein by reference.

[0021] Thus, in one embodiment, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, comprising introducing a precursor of formula (I) into a reaction zone containing the microelectronic device substrate and simultaneously introducing a reducing gas into the reaction zone, hi another embodiment, the method further comprises intermittently introducing pulses of an oxidizing gas into the reaction zone.

[0022] In another embodiment, a molybdenum precursor of formula (I) can be introduced into a reaction zone containing a microelectronic device substrate, followed by pulsing an oxidizing gas (e.g., H2O vapor), followed by pulsing a reducing gas (e.g., H2). In this manner, a molybdenum metal film can be deposited on the surface of a microelectronic device substrate. Thus, in a further embodiment, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, comprising: (i) introducing a precursor of formula (I) into a reaction zone containing a microelectronic device substrate, while intermittently (ii) exposing the substrate to an oxidizing gas; and intermittently (iii) exposing the substrate to a reducing gas. In a particular embodiment, the precursor, the oxidizing gas, and the reducing gas are pulsed into the atomic layer deposition region.

[0023] In certain embodiments of the invention, the oxidizing gas is composed of a gas selected from H2O vapor, H2O2, O3, and N2O. In certain embodiments of the invention, the reducing gas is composed of a gas selected from H2, hydrazine (N2H4), methylhydrazine, t-butylhydrazine, 1,1-dimethylhydrazine, 1,2-dimethylhydrazine, and NH3. Given the oxidation potential of H2O2 and O3, it will be understood that such gases should not be utilized with hydrazine (N2H4), methylhydrazine, t-butylhydrazine, 1,1-dimethylhydrazine, or 1,2-dimethylhydrazine, or if utilized sequentially, any such gas remaining from such steps should be purged from the reactor prior to exposing the substrate to the other reactant. Further details regarding these techniques can be found in U.S. Patent Publication No. 2021 / 062331, which is incorporated herein by reference.

[0024] In certain cases, nitrogen-containing reducing gases such as ammonia (NH3), hydrazine (N2H4); C1-C4 alkyl hydrazines such as methylhydrazine, t-butylhydrazine, 1,1-dimethylhydrazine, and 1,2-dimethylhydrazine may be useful, but under some conditions will result in molybdenum-containing nitride films rather than pure metal films. Similarly, in certain embodiments, carbon-containing reducing gases such as carbon monoxide, alkanes, alkenes, and alkynes may be useful, but under some conditions will result in molybdenum carbide films rather than pure metal films. In one embodiment, the reducing gas is hydrogen.

[0025] The methods disclosed herein may include one or more purge gases as an optional step between the introduction of the metal precursor and the reducing and / or oxidizing gases, and the carrier gas. The purge or carrier gas, used either to purge out unconsumed reactants and / or reaction by-products, or to act as a diluent and carrier for the metal precursor and the reducing or oxidizing gas, is an inert gas that does not react with the precursor. Exemplary gases include, but are not limited to, argon, nitrogen, helium, neon, and mixtures thereof. In certain embodiments, a purge gas, such as Ar, is fed into the reactor at a flow rate ranging from about 10 to about 10,000 sccm for about 0.1 to 1000 seconds, thereby purging unreacted materials and any by-products that may remain in the reactor. Other such inert gases, as used herein, may be utilized as carrier gases to vary the concentration of the molybdenum precursor and / or the oxidizing and / or reducing gas injected into the reaction zone. The use of a carrier gas and its flow rate will ultimately depend on the configuration of the deposition tool, its scale of operation, and the particular precursors being utilized.

[0026] In one embodiment, a reducing gas can be utilized with the precursor of formula (I) to effect the formation of an elemental molybdenum-containing film. Alternatively, when using the precursors described herein as a means to deposit metal oxide thin films such as MoO2, an oxidizing gas (i.e., a co-reactant) such as oxygen can be added to the process.

[0027] In various embodiments, deposition conditions include an inert atmosphere, except for the optional presence of such reducing and / or oxidizing gases. In certain embodiments, the precursor vapor can be deposited in the substantial absence of other metal vapors.

[0028] In certain embodiments, the molybdenum-containing layer deposited on the substrate surface can be formed, for example, by chemical vapor deposition (CVD), pulsed chemical vapor deposition, atomic layer deposition (ALD), or other (thermal) vapor deposition methods without the prior formation of a nucleation layer. Each precursor vapor contact step can be alternately repeated for a desired number of cycles to form a desired thickness of the molybdenum-containing film. In various embodiments, the contact of the substrate (e.g., titanium nitride) layer with the vapor of the compound of formula (I) is performed at a temperature ranging from 200° C. to 750° C. for such deposition, and at a pressure of about 0.5 to about 500 Torr. The pulse introduction of the compound of formula (I), the reducing gas, and the oxidizing gas can range in duration from about 0.2 seconds to about 60 seconds in certain embodiments.

[0029] Molybdenum metal-containing materials can be directly deposited on a substrate to form bulk deposits of molybdenum metal, oxide, carbide, or nitride, as described above. When deposition of elemental molybdenum films is desired and H2 is utilized as the reducing gas, the concentration of H2 is important to the formation of molybdenum metal versus oxide, since metal formation requires more than 4 molar equivalents of H2, or excess H2. Below 4 molar equivalents of H2, varying amounts of molybdenum metal oxide are formed, and therefore further exposure to H2 is required to reduce the molybdenum oxide thus formed.

[0030] Process chemistries for depositing such molybdenum-containing materials according to the present disclosure can include the deposition of elemental molybdenum, Mo(0), via the reaction Mo2(O2CCH3)4+2H2→2Mo+4HOCCH3. Intermediate reactions may exist and are well known in the art.

[0031] The molybdenum-containing material deposited according to the method of the present invention can be characterized by any suitable metrics and parameters, such as the deposition rate of the molybdenum-containing material, the film resistivity of the deposited molybdenum-containing material, the film morphology of the deposited molybdenum-containing material, the film stress of the deposited molybdenum-containing material, the step coverage of the material, the film composition and purity, and the process window or process envelope of suitable process conditions. Any suitable metrics and parameters can be employed to characterize the deposited material and relate it to specific process conditions to enable mass production of corresponding semiconductor products and flat panel displays. Advantageously, it is believed that the method of the present invention can deposit high purity molybdenum metal films on microelectronic device substrates.

[0032] The substrate utilized in the deposition method of the present invention can be of any suitable type, and can include, for example, a microelectronic device substrate, such as a silicon substrate, a silicon dioxide substrate, or other silicon-based substrate. In various embodiments, the substrate can include one or more metal or dielectric substrates, such as Co, Cu, Al, W, WN, WC, TiN, Mo, MoC, SiO2, W, SiN, WCN, Al2O3, AlN, ZrO2, HfO2, SiO2, lanthanum oxide (La2O3), tantalum nitride (TaN), niobium nitride, ruthenium oxide (RuO2), iridium oxide (IrO2), niobium oxide (Nb2O3), yttrium oxide (Y2O3).

[0033] In certain embodiments, for example in the case of an oxide substrate such as silicon dioxide, or alternatively in the case of a silicon or polysilicon substrate, the substrate can be processed or manufactured to include a barrier layer thereon, such as titanium nitride, for subsequently deposited materials.

[0034] It will be appreciated that the method of the present invention can be carried out in many alternative ways and under a wide variety of process conditions. The microelectronic or semiconductor device can be of any suitable type and can include, for example, a DRAM device, a 3-D NAND device, or other device, i.e., device integrated structure. In various embodiments, the substrate can include vias into which the molybdenum-containing material is deposited. The device can have an aspect ratio of depth to lateral dimension ranging, for example, from 10:1 to 40:1. In other embodiments, the method can be carried out in the manufacture of microelectronic device products, such as mobile devices, logic devices, flat panel displays, or IC packaging components.

[0035] In the methods of the present invention, the precursor compounds can be reacted with the desired microelectronic device surface or substrate in any suitable manner, for example, in a single wafer chamber, a multi-wafer chamber, or in a furnace containing multiple wafers.

[0036] As used herein, the term "microelectronic device" corresponds to a semiconductor substrate, including 3D NAND structures, logic devices, DRAM, power devices, flat panel displays, and microelectromechanical systems (MEMS), that is manufactured for use in microelectronics, integrated circuit, or computer chip applications. It is to be understood that the term "microelectronic device" is not limiting in any way and includes any substrate that contains n-channel metal oxide semiconductor (nMOS) and / or p-channel metal oxide semiconductor (pMOS) transistors and that will ultimately become a microelectronic device or microelectronic assembly. Furthermore, the underlying substrate need not be silicon, but can be an insulator such as glass or sapphire, a high bandgap semiconductor such as SiC or GaN, or other materials useful in the manufacture of electrical circuits. Such microelectronic devices contain at least one substrate, which may be selected from, but is not limited to, silicon, SiO2, Si3N4, OSG, FSG, silicon carbide, hydrogenated silicon carbide, silicon nitride, hydrogenated silicon nitride, silicon carbonitride, hydrogenated silicon carbonitride, boron nitride, anti-reflective coatings, photoresists, germanium, germanium-containing, boron-containing, Ga / As, flexible substrates, porous inorganic materials, metals such as copper and aluminum, and diffusion barrier layers such as TiN, Ti(C)N, TaN, Ta(C)N, Ta, W, WN, etc. The films are compatible with various subsequent processing steps, such as, for example, chemical mechanical planarization (CMP) and anisotropic etching processes.

[0037] Aspects In a first aspect, the present invention provides a method for depositing a molybdenum-containing film on a microelectronic device substrate, the method comprising exposing the substrate in a reaction zone to a compound of formula (I): TIFF2024544133000005.tif38170 [wherein each R is independently selected from (i) C1-C4 alkyl or (ii) C1-C4 alkyl substituted with one or more halogen atoms; Under deposition conditions, a molybdenum-containing film forms on the substrate.

[0038] In a second aspect, the present invention provides the method of the first aspect, wherein each R is C1-C4 alkyl.

[0039] In a third aspect, the present invention provides the method of the first aspect, wherein each R is methyl.

[0040] In a fourth aspect, the present invention provides the method of the first or second aspect, wherein each R is tert-butyl.

[0041] In a fifth aspect, the present invention provides the method of the first aspect, wherein each R is trifluoromethyl.

[0042] In a sixth aspect, the present invention provides the method of any one of the first to fifth aspects, wherein the deposition conditions include a temperature of about 200° C. to about 750° C. and a pressure of about 0.5 to about 500 Torr.

[0043] In a seventh aspect, the invention provides the method of any one of the first to sixth aspects, wherein the deposition conditions comprise introducing a compound of formula (I) into a reaction zone containing a microelectronic device substrate and simultaneously introducing a reducing gas into the reaction zone.

[0044] In an eighth aspect, the present invention provides the method of the seventh aspect, wherein the deposition conditions further comprise intermittently introducing pulses of an oxidizing gas into the reaction zone.

[0045] In a ninth aspect, the invention provides the method of any one of the first to sixth aspects, wherein the deposition conditions comprise: (i) introducing a precursor of formula (I) to a reaction zone containing a microelectronic device substrate while intermittently (ii) exposing the substrate to an oxidizing gas; and intermittently (iii) exposing the substrate to a reducing gas.

[0046] In a tenth aspect, the present invention provides a method of the seventh or ninth aspect, wherein the reducing gas consists of a gas selected from H2, hydrazine, methylhydrazine, t-butylhydrazine, 1,2-dimethylhydrazine, 1,2-dimethylhydrazine, and NH3.

[0047] In an eleventh aspect, the present invention provides a method of the eighth or ninth aspect, wherein the oxidizing gas is selected from H2O (H2O) vapor, H2O2, O3, and N2O.

[0048] In a twelfth aspect, the present invention provides the method of any one of the first to eleventh aspects, wherein the substrate is selected from titanium nitride, tantalum nitride, aluminum nitride, aluminum oxide, zirconium oxide, hafnium oxide, silicon dioxide, silicon nitride, lanthanum oxide, ruthenium oxide, iridium oxide, niobium oxide, and yttrium oxide.

[0049] In a thirteenth aspect, the present invention provides the method of any one of the first to twelfth aspects, wherein the molybdenum-containing film is molybdenum metal.

[0050] Thus, while several illustrative embodiments of the disclosure have been described, those skilled in the art will readily appreciate that still other embodiments may be made and used within the scope of the claims appended hereto. Numerous advantages of the disclosure to which this document is directed have been set forth in the foregoing description. It will be understood, however, that the disclosure is, in many respects, only illustrative. The scope of the disclosure will, of course, be expressed in the language of the appended claims.

Claims

1. 1. A method for depositing a molybdenum-containing film on a microelectronic device substrate, comprising: reacting a compound of formula (I): [In the formula, each R is: (i) C 1 ~C 4 (ii) alkyl, or (iii) C substituted with one or more halogen atoms; 1 ~C 4 alkyl; thereby forming a molybdenum-containing film on the substrate.

2. Each R is C 1 ~C 4 The method of claim 1 , wherein the alkyl group is an alkyl group.

3. 2. The method of claim 1 , wherein each R is methyl.

4. 2. The method of claim 1 , wherein each R is tert-butyl.

5. The method of claim 1 , wherein each R is trifluoromethyl.

6. The method of claim 1, wherein the deposition conditions include a temperature of about 200° C. to about 750° C. and a pressure of about 0.5 to about 500 Torr.

7. 10. The method of claim 1, wherein the deposition conditions include introducing a compound of formula (I) into a reaction zone containing the microelectronic device substrate and simultaneously introducing a reducing gas into the reaction zone.

8. The method of claim 7 , wherein the deposition conditions further comprise intermittently introducing pulses of an oxidizing gas into the reaction zone.

9. 10. The method of claim 1 , wherein the deposition conditions include: (i) introducing a precursor of formula (I) into a reaction zone containing a microelectronic device substrate while intermittently (ii) exposing the substrate to an oxidizing gas; and intermittently (iii) exposing the substrate to a reducing gas.

10. The reducing gas is H 2 , hydrazine, methylhydrazine, t-butylhydrazine, 1,2-dimethylhydrazine, 1,2-dimethylhydrazine, and NH 3 10. The method of claim 7 or 9, wherein the gas is selected from the group consisting of:

11. The oxidizing gas is H 2 O (H 2 0) Steam, H 2 O 2 , O 3 , and N 2 The method of claim 8 or 9, wherein the amino acid is selected from the group consisting of aryl, aryloxy ...

12. 10. The method of claim 1, wherein the substrate is selected from titanium nitride, tantalum nitride, aluminum nitride, aluminum oxide, zirconium oxide, hafnium oxide, silicon dioxide, silicon nitride, lanthanum oxide, ruthenium oxide, iridium oxide, niobium oxide, and yttrium oxide.

13. The method of claim 1 , wherein the molybdenum-containing film is molybdenum metal.

Citation Information

Patent Citations

  • Formation of deposited film

    JP1987142779A

  • Lithium titanate powder for electrode of power storage device, material of active substance, electrode sheet arranged by use thereof, and power storage device

    JP2019220254A

  • Precursors for the deposition of molybdenum-containing coatings

    JP2022524041A

  • Precursors for deposition of molybdenum-containing films

    WO2020185618A1