Polymer composition comprising VDF polymer and graphite
A VDF polymer and graphite composition with specific properties addresses corrosion and mechanical degradation in offshore pipelines by reducing acidic gas permeation and enhancing mechanical properties, ensuring extended service life and ease of manufacturing.
Patent Information
- Application Number
- JP2021528977
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-11-26
- Filing Date
- 2019-11-25
- Publication Date
- 2024-09-17
- Estimated Expiration
- 2039-11-25
AI Technical Summary
Offshore pipelines face issues with corrosion due to the permeation of acidic gases like CO2 and H2S, which degrade mechanical properties and reduce service life, especially under high pressures and temperatures, and existing acid-grade steels are expensive and mechanically insufficient.
A polymer composition comprising VDF polymer and selected graphite with specific particle size and BET surface area is used to reduce acidic gas permeation and maintain mechanical integrity, featuring a thermoplastic VDF polymer blended with graphite particles of defined size and surface area, ensuring uniform distribution and improved mechanical properties.
The composition effectively reduces acidic gas permeation and maintains mechanical properties, enabling longer service life and ease of manufacturing, particularly in harsh environments with repeated mechanical deformations.
Smart Images

Figure 0007551613000001
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to European Patent Application No. 18208223.0, filed November 26, 2018, the entire contents of which are incorporated herein by reference for all purposes.
[0002] The present invention relates to a polymer composition comprising a vinylidene fluoride (VDF) polymer and a selected graphite grade. The composition according to the invention is particularly useful for the manufacture of tubular articles such as pipes for the oil / gas extraction industry, especially for applications in harsh conditions such as transporting hydrocarbons from offshore wells to floating offshore units. The composition according to the invention reduces the permeation of acid gases such as CO2 and H2S from the hydrocarbon stream through the layers of the pipe, thus preventing corrosion of its metallic outer armor layer. At the same time, the composition according to the invention has good mechanical properties such as elongation at break and yield strain that allow their application in situations involving significant repeated mechanical deformation. [Background technology]
[0003] Offshore pipelines, such as those used to pump crude oil and natural gas from offshore drilling rigs and terminals to land or to floating platforms, are required to be able to withstand very high pressures and temperatures and therefore typically include formations made of metals such as iron and steel.
[0004] Such pipelines are also required to be flexible to accommodate relative movement of source and destination and also to allow transportation and reuse in a rolled form. Flexibility is typically achieved by combining a metal layer, which provides structure and resistance to pressure, with a polymer layer that seals the tube and prevents migration of materials from the inside of the pipe to the outside.
[0005] Flexible pipes for transporting hydrocarbons, also known as flexible risers, are widely used and generally comprise, from the inside to the outside of the pipe, a metal frame, a pressure armor layer, a tensile armor layer and a polymer outer sheath, covered with a polymer inner sealing sheath for protecting the entire pipe, in particular to prevent seawater from penetrating its thickness. The metal frame and the pressure armor layer are usually made of longitudinal elements wound with a short pitch, giving the pipe the ability to withstand radial forces, while the tensile armor layer is usually made of metal wire wound with a long pitch to react to axial forces. Flexible risers can be bonded or unbonded. The present invention finds application in both types.
[0006] Polyvinylidene fluoride (PVDF) has been proposed as a material for fabricating such polymeric inner sealing sheaths due to its chemical resistance to hydrocarbons, typically at temperatures between 100°C and 130°C.
[0007] Under operating temperatures and pressures, carbon dioxide (CO2) and hydrogen sulfide (H2S) contained in the hydrocarbons can penetrate through the polymer inner sealing sheath into the tensile armor layer and, in the presence of water vapor, cause corrosion of these metallic reinforcements. These phenomena can affect the mechanical performance of the pipes, especially in ultra-deepwater applications, and consequently reduce their service life.
[0008] Acid-use steel grades for the pressure and tensile armor layers are sometimes used to prevent this corrosive effect, but such steel grades have the disadvantage of being expensive and having poor mechanical properties, and impose an increase in the section and weight of the metal parts in these pipes.
[0009] There is therefore a need for improved polymer compositions that can be used for the polymeric inner sealing sheath of such flexible pipes, which reduce the permeation of acid gases, thus making it possible to manufacture such pipes without the drawbacks mentioned above in relation to the use of acidic steel grades, and generally to extend the service life of such pipes. Such compositions should also maintain good mechanical properties to withstand the repeated strains and compression forces to which they are subjected during operation, in particular associated with winding / unwinding of rolls and with the relative movements of the hydrocarbon source and destination locations, for example when the destination is a floating platform. Under these conditions, one face of the pipe is typically stretched while the opposite face is compressed, and this stretching / compression cycle can be repeated many times in different directions.
[0010] For this reason, it is very important that the material used in the pipe has a sufficiently high elongation at break and a sufficiently high yield stress to withstand these stresses during the entire useful life of the pipe. Summary of the Invention
[0011] The present invention relates to a polymer composition comprising a VDF polymer and a selected graphitic material having a low particle size and a defined range of BET surface area, excluding materials with very low or very high BET surface area.
[0012] It has been found that the use of the composition according to the invention in flexible pipes, for example for gas / oil extraction, strongly reduces the permeation rate of acid gases, such as CO2 and H2S. The composition according to the invention has a lower permeation rate when compared to compositions using graphite materials with larger particle sizes, and is easier and cheaper to manufacture than compositions using graphite materials with smaller particle sizes and larger BET specific surface areas. Compositions containing graphite grades within the most preferred range also have improved mechanical properties. These properties allow for easy manufacture and distribution uniformity of the composition, as well as longer service life in harsh environments for articles containing the composition.
[0013] In one aspect, the present invention provides a polymer composition comprising at least one vinylidene fluoride (VDF) polymer, and a plurality of graphite particles, from 1 to 100 parts by weight, preferably from 2 to 50 parts by weight, more preferably from 2 to 30 parts by weight, and even more preferably from 3 to 20 parts by weight, per 100 parts by weight of the VDF polymer, wherein the graphite particles have a D90 particle size measured by laser scattering of less than 50 μm, preferably from 2 to 30 μm, more preferably from 2 to 20 μm, and even more preferably from 2 to 10 μm, and ...10 to 50 μm. 2 / g, preferably 15 to 35 m 2 / g.
[0014] In another aspect, the present invention relates to a tubular article comprising the composition described above.
[0015] In a further aspect, the present invention relates to a multi-layer pipe, in particular a flexible riser, comprising a tubular article as described above.
[0016] The present invention also relates to methods of making the compositions of the present invention and to methods of making tubular articles comprising the compositions of the present invention.
[0017] In another aspect, the present invention relates to the use of the compositions of the present invention for transporting hydrocarbons, and in particular in downhole or drilling operations, tubular articles and multi-layer pipes comprising the compositions of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] The polymer composition of the present invention is preferably a thermoplastic composition.
[0019] At least one vinylidene fluoride (VDF) polymer is used in the composition of the invention. Preferably, said VDF polymer is a thermoplastic VDF polymer, but also VDF thermoplastic elastomers can be used as detailed below.
[0020] For the purposes of the present invention, the term "thermoplastic" is intended to mean polymers and / or compositions that are solid at room or use temperature, soften when heated and harden again when cooled without appreciable changes in chemical and physical properties. Such a definition can be found, for example, in the encyclopedia called Polymer Science Dictionary, edited by MARK SM, ALGER. LONDON: ELSEVIER APPLIED SCIENCE, 1989. p. 476.
[0021] The expressions "vinylidene fluoride polymer" or "VDF polymer" are equivalent and are used within the framework of the present invention to denote a polymer essentially made up of repeating units, more than 50 mol % of which derive from vinylidene fluoride (VDF).
[0022] The VDF polymers useful in the present invention are preferably (a) at least 60 mol %, preferably at least 75 mol %, more preferably at least 85 mol % of repeat units derived from vinylidene fluoride (VDF); (b) optionally 0.1 to 15 mol %, preferably 0.1 to 12 mol %, more preferably 0.1 to 10 mol % of repeat units derived from a fluorinated monomer other than VDF; (c) optionally, 0.1 to 5 mol %, preferably 0.1 to 3 mol %, more preferably 0.1 to 1 mol % of repeating units derived from one or more hydrogen-containing comonomers; Including, All mole percentages above are based on the total moles of repeat units in the VDF polymer. It is a polymer.
[0023] Said fluorinated monomer different from VDF is advantageously selected from the group consisting of vinyl fluoride (VF1); trifluoroethylene (VF3); chlorotrifluoroethylene (CTFE); 1,2-difluoroethylene; tetrafluoroethylene (TFE); hexafluoropropylene (HFP); perfluoro(alkyl)vinyl ethers, such as perfluoro(methyl)vinyl ether (PMVE), perfluoro(ethyl)vinyl ether (PEVE) and perfluoro(propyl)vinyl ether (PPVE); perfluoro(1,3-dioxole); perfluoro(2,2-dimethyl-1,3-dioxole) (PDD). Preferably, possible additional fluorinated monomers are selected from chlorotrifluoroethylene (CTFE), hexafluoropropylene (HFP), trifluoroethylene (VF3) and tetrafluoroethylene (TFE).
[0024] The choice of said hydrogen-containing comonomer is not particularly limited; alpha-olefins, (meth)acrylic monomers, vinyl ether monomers, styrene monomonomers may be used.
[0025] Thus, the VDF polymer for use in the present invention is more preferably (a) at least 60 mol %, preferably at least 75 mol %, more preferably at least 85 mol %, of repeat units derived from vinylidene fluoride (VDF); (b) optionally 0.1 to 15 mol %, preferably 0.1 to 12 mol %, more preferably 0.1 to 10 mol % of a fluorinated monomer different from VDF; preferably, said fluorinated monomer is selected from the group consisting of vinyl fluoride (VF1), chlorotrifluoroethylene (CTFE), hexafluoropropene (HFP), tetrafluoroethylene (TFE), perfluoromethylvinylether (MVE), trifluoroethylene (TrFE) and mixtures thereof; It essentially consists of All the above mole percentages are based on the total moles of repeat units in the VDF polymer. It is a polymer.
[0026] Defects, end chains, impurities, chain inversions or branches etc. may further be present in the VDF copolymer in addition to said repeating units, without these constituents substantially altering the behaviour and properties of the VDF polymer.
[0027] Non-limiting examples of VDF polymers useful in the present invention include homopolymers of VDF, VDF / TFE copolymers, VDF / TFE / HFP copolymers, VDF / TFE / CTFE copolymers, VDF / TFE / TrFE copolymers, VDF / CTFE copolymers, VDF / HFP copolymers, VDF / TFE / HFP / CTFE copolymers, among others.
[0028] As mentioned above, the at least one VDF polymer may be a thermoplastic polymer. Optionally, the at least one VDF polymer may be a VDF-based fluorinated thermoplastic elastomer comprising at least one elastomeric "soft" block consisting of a sequence of repeating units, said sequence comprising repeating units derived from VDF and from at least one fluorinated monomer different from VDF, and at least one thermoplastic "hard" block consisting of a sequence of repeating units, said sequence comprising repeating units derived from VDF in an amount of at least 85 mol % relative to the total moles of repeating units of the block.
[0029] In the present invention, the composition may comprise two or more VDF polymers, in particular the composition may comprise a blend of at least one PVDF homopolymer and at least one VDF-containing copolymer.
[0030] Particularly preferred in the present invention are blends of a PVDF homopolymer with at least one VDF copolymer selected from the group consisting of VDF / CTFE copolymers and VDF / HFP copolymers.
[0031] The melt index of the VDF polymer in the composition (or of the combined VDF polymer mixture, in the case where two or more VDF polymers are present), measured according to ASTM test No. 1238, carried out at 230°C under a piston load of 2.16 kg, may advantageously be at least 0.01, preferably at least 0.05, more preferably at least 0.1 g / 10 min, and advantageously be less than 50, preferably less than 30, more preferably less than 20 g / 10 min.
[0032] When measured instead according to the same ASTM standard under a piston load of 5 kg, the melt index may advantageously be at least 1, preferably at least 2, more preferably at least 5 g / 10 min, and advantageously less than 70, preferably less than 50, more preferably less than 40 g / 10 min.
[0033] Each VDF polymer for use in the present invention preferably has a melting point (T) of at least 120° C., preferably at least 125° C., more preferably at least 130° C., and at most 190° C., preferably at most 185° C., more preferably at most 180° C., as measured by DSC at a heating rate of 10° C. / min according to ASTM D3418. m2 ).
[0034] Optionally, the composition of the present invention may comprise a fluoroelastomer in dispersed form, said fluoroelastomer consisting of a sequence of repeating units from VDF and repeating units derived from at least one fluorinated monomer different from VDF, said elastomer being chemically crosslinked, for example by dynamic vulcanization.
[0035] The composition of the present invention also comprises a plurality of graphite particles in an amount of 1-100 parts by weight, preferably 2-50 parts by weight, more preferably 2-30 parts by weight, and even more preferably 3-20 parts by weight, based on 100 parts by weight of the VDF polymer. The graphite particles in the present invention have a D90 particle size of less than 50 μm, preferably 2-30 μm, more preferably 2-20 μm, and even more preferably 2-10 μm, as measured by the laser scattering method described below in the experimental section. The graphite particles in the present invention also have a D90 particle size of less than 50 μm, preferably 2-30 μm, more preferably 2-20 μm, and even more preferably 2-10 μm, as measured by the laser scattering method described below in the experimental section. 2 / g, preferably 15 to 35 m 2 / g (as measured by the method described below in the experimental section).
[0036] Surprisingly, it has been found that the selection of a particular D90 size and BET specific surface area range significantly affects several properties of the compositions of the present invention.
[0037] As previously predicted, when considering the permeation rate of acid gases such as CO2 and H2S, it has been found that the use of graphite materials within a selected particle size range provides a stronger effect than that of larger particle size graphite materials, as shown in the experimental section below.
[0038] It has also been realised that by using a graphite material having a D90 particle size and BET specific surface area within the claimed ranges (as will be explained in more detail below), the compositions of the present invention can be easily manufactured by simply premixing the VDF polymer in divided form such as powder, pellets, granules or fibres with the graphite material to provide a premix, and then processing the premix in an extruder.
[0039] Both of these effects were even more pronounced by selecting the D90 particle size and BET specific surface area within the preferred ranges described herein.
[0040] When considering the mechanical properties of polymer compositions, it is expected that the addition of particulate fillers such as graphite will have a negative effect on the mechanical properties. "Elongation at break" and "yield strain" (measured according to ASTM D638) are important properties for the practical application of the compositions according to the present invention. In fact, when such compositions are formed into tubes or pipes, for example, when the pipes are wound and unwound, they are subjected to high levels of elastic deformation, and therefore it is also important that the pipes and pipe layers comprising the compositions of the present invention can not only prevent acid gas migration, but also be able to withstand such stresses many times without breaking or losing their elasticity.
[0041] However, it has been surprisingly found that by selecting a graphite material having a D90 particle size within the most preferred range claimed herein, the adverse effect of the presence of graphite particles on these mechanical properties is significantly reduced for compositions containing larger particle size graphite. Without being bound by theory, it is believed that a lower number of large particles improves these properties because larger particles may act as starting points for structural failure after mechanical stress.
[0042] Therefore, the compositions according to the invention can be easily manufactured and provide an optimal combination of barrier and mechanical properties that are the result of the specific combination of the selected fluoropolymer material and the selected graphite grade.
[0043] The polymer composition according to the invention can be produced by mixing one or more VDF polymers in the molten state with a plurality of graphite particles according to the invention. A preferred method for the industrial production of such a composition is to use an extruder capable of mixing the melt thoroughly and extrude the mixture of VDF polymer and graphite particles. This method can be carried out as is common in the art, but the applicant has found that certain process steps can further improve the properties of the resulting composition.
[0044] To achieve a better homogeneity of the composition, the VDF polymer can be provided in divided forms, such as pellets, granules, powder, beads or fibers. The polymer in divided form can be premixed in the dry state, typically without heating the mixture, with mechanical stirring. Premixing can be carried out directly in the feeder of an extruder that includes a blender unit at its main gate. The premix is preferably fed at the main gate of the extruder. In this way, the graphite particles are thoroughly mixed in the polymer matrix so that the individual particles are dispersed and do not agglomerate. Surprisingly, it has been found that the composition according to the invention produced in this way has a further improved yield strain and elongation at break when compared to a composition having the same composition but produced using a different method, such as feeding the graphite particles at the side feeder of the extruder.
[0045] Without being bound by theory, it is believed that this is the result of the fact that graphite materials within the selected range tend to homogeneously form a layer covering the VDF polymer particles, possibly due to electrostatic interactions, so that upon melting the graphite is well dispersed and homogeneously distributed in the composition with relatively little mixing in the molten phase. Instead, it has been observed that graphite materials with too large a particle size and low BET area tend to separate in the premix, making it difficult to distribute homogeneously in the composition, while graphite materials (as well as graphene and graphene-like materials) with too small a particle size and too large BET surface area tend to agglomerate, also making it difficult to achieve a homogeneous composition.
[0046] The preferred extruder for this operation is a twin screw extruder.
[0047] Once the raw materials of the composition of the present invention are fed into the extruder, the VDF polymer is melted and blended with the graphite particles. The mixture can be directly extruded in tubular form for its final use, but more preferably in divided forms such as pellets, granules, beads or fibers, which will be further processed at a later stage to produce the finished product.
[0048] The polymer composition according to the invention finds application, for example, in the construction of pipes for the oil and gas industry. The tubular article according to the invention can be obtained by extruding the composition according to the invention into a tube. A preferred method for producing a tubular article is to provide the composition according to the invention in a divided form, such as pellets, granules, powder, beads or fibers, and introduce it into an extruder capable of forming a tubular article, typically a single screw extruder being preferred for forming the composition of the invention into a tubular article. Such a tubular article can be extruded as a free-standing tube, or it can be extruded onto the top surface of a support, such as a rigid metal frame or other support.
[0049] Alternatively, tubular articles comprising the compositions of the present invention can be produced by extruding or otherwise forming the compositions of the present invention in the form of a film, layer or tape, and then wrapping said film, layer or tape around a support having a cylindrical shape. Such a support can be removed once the tubular article is formed or maintained as part of a structure. To form a tighter seal at the joints of the films, layers or tapes, heat can be applied to partially melt the composition as the tape, film or layer is formed into a tube, using methods common in the art.
[0050] The tubular articles according to the invention can be used as such or, more generally, can be incorporated into multi-layer pipes having at least one layer comprising or made from the composition of the invention.
[0051] Multi-layer pipes can be formed by known techniques, for example, a larger pipe can be introduced or formed on the outside of a smaller pipe. Alternatively, different polymer compositions can be co-extruded together to form concentric pipes with layers of different compositions. For example, the composition of the present invention can be co-extruded with a composition that includes one or more VDF polymers but does not include or is essentially free of graphite particles, thus forming a multi-layer pipe with one graphite-containing layer and one graphite-free layer, especially where the graphite-free layer is in an internal position. Such structures can be beneficial when hydrocarbons are transported under high pressure, such as in flexible risers for oil extraction, and can provide such flexible risers with a longer service life. Without being bound by theory, it is believed that gases at high pressure can permeate the first molecular layer of the polymer in direct contact with the flow. Such gases can expand and form blisters in such layers when the pressure is reduced to normal pressure. In this structure, the graphite-containing layer, which is less resistant to mechanical stresses than the graphite-free layer, is protected from blistering, and thus it does not contain possible initiation points that could trigger mechanical fracture.
[0052] As is known in the art, multi-layer pipes, such as those used in the oil and gas industry, can be "bonded" (i.e., where the surfaces of the various layers are bonded to one another) or "unbonded" (i.e., where the various layers are free to move somewhat independently within the multi-layer structure). In some cases, multi-layer pipes can include some layers that have "bonds" between them and other layers that are not bonded to others.
[0053] A preferred multi-layer pipe comprising the composition of the present invention is a pipe for recovering hydrocarbons, such as a flexible riser for oil and gas extraction. As mentioned above, typically such a flexible riser comprises, from the inside to the outside of the pipe, a metal frame covered with a polymeric inner sealing sheath, a pressure armor layer, a tensile armor layer and a polymeric outer sheath. A flexible riser according to the present invention comprises a polymeric inner sealing sheath comprising or made of a composition according to the present invention. In the case where the polymeric inner sheath comprises two or more layers, it may have at least one of its layers comprising or made of a composition according to the present invention. Such a pipe according to the present invention combines excellent resistance to acid gas permeation with very good mechanical properties that allow repeated winding and unwinding without damaging the pipe, even in harsh environments such as offshore boats and platforms. Such a pipe can withstand the strains occurring in those conditions much better than other pipes in which the polymeric outer sheath layer comprises different grades of graphite.
[0054] In a flexible riser according to the present invention, the polymeric outer sheath layer may comprise the polymer composition of the present invention, although it is preferred that such layers are made of other materials conventional for such applications as described in the art.
[0055] A particularly preferred configuration for a multi-layer pipe comprising one tubular article comprising, consisting essentially of or made of the composition of the present invention is one in which an additional tubular article comprising a VDF polymer layer and essentially free of graphite particles is concentric and more internal to the pipe than the layer comprising, consisting essentially of or made of the composition of the present invention.
[0056] In another aspect, the present invention relates to a method for transporting hydrocarbons (e.g. for recovering crude oil, especially in offshore drilling or downhole operations) comprising the use of a pipe comprising or made of the polymer composition of the present invention, or of a tubular article according to the present invention, or of a multi-layer pipe according to the present invention.
[0057] In a further aspect, the present invention relates to the use of a pipe comprising the polymer composition according to the invention, of a tubular article according to the invention or of a multi-layer pipe according to the invention in drilling operations or in downhole operations, the composition of the present invention providing the pipe with barrier and mechanical properties which extend the life of the pipe.
[0058] The present invention will now be described in more detail with reference to the following examples, the purpose of which is merely illustrative and is not intended to limit the scope of the invention.
[0059] raw materials SOLEF® VDF polymer S50515 from Solvay Specialty Polymers Italy SpA Graphite Timrex® KS4-D90 4.7 μm from Imerys Graphite Timrex® CT301-D90 30 μm from Imerys Graphite Timrex® CT001-D90 81 μm from Imerys
[0060] Measurement of CO2 transmission rate The CO2 permeability measurements were carried out using method ISO 15105-1 at 23°C and atmospheric pressure. The equipment used was a Versaperm Permeability Meter MK IV. CO2 CP Grade was used, T was 23°C and the tests were carried out at atmospheric pressure (990-1015 mbar). The permeability values reported in the table below are in cm 3 (STP)mm / m 2 It is expressed in barometric pressure days according to this method.
[0061] Measurement of yield strain and elongation at break The yield strain and elongation at break were measured according to ASTM D638 using Type V specimens at 23° C. with a deformation rate of 10 mm / min.
[0062] Measurement of graphite powder particle size D90 The particle size D90 of the graphite particles before incorporation into the polymer matrix was measured by laser diffraction according to method ISO 13390.
[0063] Measurement of BET specific surface area of graphite powder The BET specific surface area of the graphite was measured according to ASTM D6556-04. EXAMPLES
[0064] The compositions were prepared in a twin-screw extruder Brabender KETSE with a screw diameter of 20 mm and a length to diameter ratio of 40. A metering feeder was used to feed the polymer pellets at the main gate. In examples 2, 4 and 5, the graphite powder was dry blended with the VDF polymer by premixing the ingredients for 4 hours in a metering feeder at the main gate with mechanical stirring. In example 3, the graphite was introduced with a side feeder. Mixing and extrusion were carried out at a set temperature of 230° C. All compositions contained 14 parts by weight of graphite for 100 parts of VDF polymer (SOLEF® 50515).
[0065] TIFF0007551613000001.tif70170
[0066] The results show how large particle size graphite has no effect on permeability, while medium and small particle size graphite effectively prevent acid gas migration.
[0067] The results also show how only the small-sized graphite from Example 2, which, on the other hand, has the best profile in terms of permeability, also has the best profile in terms of maintaining mechanical properties, giving only a small drop in yield strain. The elongation at break for Example 2 is four times higher than that for the sample with larger-sized graphite particles. The elongation at break for Example 2 is also much lower than the control sample that does not contain any graphite, but this is of little practical importance since the value of 21% is sufficient to ensure suitability in practical applications in which graphite-free materials are used, because anyway strains exceeding 11% would change even the properties of the graphite-free material due to the yield strain limit. In contrast, the maximum elongation at break for the samples with intermediate and high graphite content is insufficient to replace graphite-free materials in all situations in which the material is exposed to significant mechanical stress.
[0068] The comparison between Examples 2 and 3 shows the important role played by the process by which the material is produced. In Example 2, the small size graphite and the polymer pellets are premixed in a dry state for 4 hours, and after this premixing operation, the resulting premix is introduced into the extruder at its main gate. In Example 3, only the polymer pellets are introduced at the main gate, while the small size graphite particles are introduced at the side feeder of the extruder. Surprisingly, the material obtained in Example 2 has much better mechanical properties than that obtained in Example 3, with improved yield strain and twice as much elongation at break.
[0069] To the extent that the disclosures of any patents, patent applications, and publications incorporated herein by reference conflict with the statements of this application to the extent that a term may be unclear, this statement shall control.
Claims
1. at least one vinylidene fluoride (VDF) polymer, - 2 to 50 parts by weight of graphite particles per 100 parts by weight of VDF polymer A polymer composition comprising: - the plurality of graphite particles have a D90 particle size as measured by laser scattering of less than 50 μm and a D90 particle size as measured by laser scattering of 15 to 50 μm 2 The polymer composition has a BET specific surface area of 100 / g.
2. The polymer composition of claim 1 , wherein said at least one VDF polymer is a thermoplastic polymer.
3. A tubular article comprising the composition of claim 1 or 2.
4. A multi-layer pipe, one of the layers being the tubular article of claim 3.
5. 5. A multi-layer pipe according to claim 4, wherein at least one layer comprising VDF polymer and free of graphite compounds is adhered to at least a portion of the inner surface of said tubular article.
6. 6. The multi-layer pipe according to claim 4 or 5, which is a bonded or unbonded flexible riser for oil and gas extraction, the flexible riser comprising, from the inside to the outside, an inner metal frame, a polymer inner sealing sheath, and a metal tensile armor layer.
7. 7. The multi-layer pipe of claim 6, wherein said polymeric inner sealing sheath comprises or is a tubular article according to claim 3.
8. - providing at least one vinylidene fluoride (VDF) polymer, A plurality of graphite particles, from 2 to 50 parts by weight per 100 parts by weight of VDF polymer, said plurality of graphite particles having a D90 particle size measured by laser scattering of less than 50 μm and a D90 particle size of 15 to 50 μm. 2 providing a plurality of graphite particles having a BET specific surface area of 1 / g; - introducing said VDF polymer and said graphite particles into an extruder; - extruding said VDF polymer and said plurality of graphite particles A method for producing the polymer composition according to claim 1 or 2, comprising:
9. 9. The method of claim 8, further comprising the steps of premixing the VDF polymer in divided form, such as pellets, granules, powder, beads or fibers, with the plurality of graphite particles to obtain a premix, and introducing the resulting premix into a main gate of the extruder.
10. A method for producing a tubular article according to claim 3, comprising the step of extruding the polymer composition according to claim 1 or 2 in the form of a tube.
11. 4. A method for producing a tubular article according to claim 3, comprising the steps of extruding the polymer composition according to claim 1 or 2 in the form of a film, layer or tape, thereafter wrapping said film, layer or tape around a support having a cylindrical shape, and then optionally removing said support.
12. 12. The method of claim 11 further comprising the step of applying heat to the wrapped film, layer or tape to at least partially melt it, thus forming a sealed tubular article.
13. Use of the polymer composition according to claim 1 or 2, or of the tubular article according to claim 3, or of the multi-layer pipe according to any one of claims 4 to 7, for transporting hydrocarbons.
14. Use of a polymer composition according to claim 1 or 2, or of a tubular article according to claim 3, or of a multi-layer pipe according to any one of claims 4 to 7, in downhole operations.
15. Use of a polymer composition according to claim 1 or 2, or of a tubular article according to claim 3, or of a multi-layer pipe according to any one of claims 4 to 7 in drilling operations.
16. at least one vinylidene fluoride (VDF) polymer, - 1 to 100 parts by weight of graphite particles per 100 parts by weight of VDF polymer 1. A polymeric composition for use in downhole or drilling operations comprising: said plurality of graphite particles having a D90 particle size as measured by laser scattering of less than 50 μm and a D90 particle size as measured by laser scattering of 10 to 50 μm; 2 The polymer composition has a BET specific surface area of 100 / g.
17. 17. A tubular article for use in downhole or drilling operations comprising the composition of claim 16.
18. 20. A multi-layer pipe for use in downhole or drilling operations, one of the layers being the tubular article of claim 17.
Citation Information
Patent Citations
Carbon-filler-containing vinylidene fluoride resin composition
JP1985168742A
PVDF-based PTC paint and its application for self-regulated heating system
JP2005054185A
Fluororubber composition
JP2016014092A
JPP3229635B
Peroxide-curable, electrically conductive fluoroelastomer composition
WO2009072606A1