How to dispose of block ice

The method of heating and precipitating PVA from block ice using magnesium sulfate addresses the separation challenge of borax and PVA in nuclear reactor decommissioning, enabling efficient disposal of block ice components.

JP7553518B2Active Publication Date: 2024-09-18TAIHEI DENGYO KAISHA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2022136349
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-08-29
Publication Date
2024-09-18
Estimated Expiration
2042-08-29

AI Technical Summary

Technical Problem

The challenge during decommissioning of nuclear reactors with ice condensers is the separation and disposal of block ice composed of borax and polyvinyl alcohol (PVA) in the ice condenser.

Method used

A method involving heating and melting block ice, followed by adding magnesium sulfate to precipitate PVA from the solution, allowing separation of PVA and borax.

Benefits of technology

Effectively separates PVA from borax-containing solutions, facilitating proper disposal of block ice components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007553518000003
    Figure 0007553518000003
  • Figure 0007553518000001
    Figure 0007553518000001
  • Figure 0007553518000002
    Figure 0007553518000002
Patent Text Reader

Abstract

To provide a processing method for separating a block ice comprising ice containing borax (Na2B4O7 10H2O) and PVA covering the ice, into PVA and borax aqueous solution.SOLUTION: A block ice processing method disclosed herein comprises adding magnesium sulfate (MgSO4 7H2O) to a solution obtained by heating and melting block ice comprising ice containing borax (Na2B4O7 10H2O) and polyvinyl alcohol (PVA) covering the ice, and isolating precipitate in the solution from the solution.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This invention relates to a method for treating block ice contained in ice condensers that are installed in some nuclear reactor facilities to condense high-temperature steam that is generated in the event of an abnormality. [Background technology]

[0002] In some nuclear reactors, ice condensers containing multiple block ice are installed to condense high-temperature steam that fills the reactor containment vessel in the event of an abnormality. As disclosed in Patent Document 1, the block ice is composed of ice containing borax (Na2B4O7·10H2O) to promote neutron absorption, and water-soluble polymer polyvinyl alcohol (PVA) is attached to the outer periphery to prevent or suppress sublimation of the block ice body. The specifications of PVA are as follows: PVA polymerization degree = 1700, saponification degree = 88 mol%, 0.8 wt% borax added, and a thickness of about 15 μm is considered to be suitable. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 3876241 Summary of the Invention [Problem to be solved by the invention]

[0004] When a nuclear reactor equipped with an ice condenser is decommissioned, the block ice stored in the ice condenser must be separated into PVA and a dissolving liquid containing borax and then disposed of appropriately.

[0005] Therefore, an object of the present invention is to provide a processing method for separating block ice, which includes ice containing borax (Na2B4O7·10H2O) and PVA covering the ice, into PVA and a dissolving solution containing borax. [Means for solving the problem]

[0006] The present invention has been made to achieve the above object and has the following features.

[0007] The invention described in claim 1 is characterized by comprising a melting step of heating and melting block ice containing ice containing borax (Na2B4O7·10H2O) and polyvinyl alcohol (PVA) covering the ice, an adding step of adding magnesium sulfate (MgSO4·7H2O) to the melting solution obtained in the melting step, and a separating step of separating a precipitate in the melting solution obtained by adding the magnesium sulfate from the melting solution.

[0008] The invention described in claim 2 is a method for processing block ice described in claim 1, characterized in that the PVA has a PVA polymerization degree of 1700, a saponification degree of 88 mol%, and contains 0.8 wt% borax.

[0009] The invention described in claim 3 is a method for processing block ice described in claim 1 or 2, characterized in that in the adding step, 0.4 g of magnesium sulfate (MgSO4·7H2O) is added per 1 ml of the dissolving solution obtained in the dissolving step. Effect of the Invention

[0010] According to this invention, by adding magnesium sulfate (MgSO4·7H2O) to the solution obtained in the dissolving process, PVA is precipitated, and by separating this, the block ice can be separated into PVA and a solution containing borax. [Brief description of the drawings]

[0011] [Figure 1] (A)-(C) are diagrams showing part of the flow of a block ice processing method. [Diagram 2] 13(A) and 13(B) are diagrams showing a part of the flow of a method for processing block ice. [Diagram 3]1 is a flowchart illustrating an example of a method for processing block ice. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] An embodiment of the present invention will now be described with reference to the drawings.

[0013] First, we will explain the block ice to be treated. Block ice is cylindrical, and its main body is composed of ice containing borax (Na2B4O7·10H2O) to promote neutron absorption. Water-soluble polymer polyvinyl alcohol (hereafter abbreviated as PVA) is attached to the outer periphery of the ice to prevent or suppress the sublimation of the ice. A film made of PVA is attached to the outer surface of the ice by full or partial welding using heat treatment with a dryer, etc.

[0014] The film made of PVA is preferably a product with a PVA polymerization degree of 1700, a saponification degree of 88 mol%, 0.8% by weight of borax added, and a thickness of about 15 μm. In this embodiment, the block ice made by attaching a PVA with a PVA polymerization degree of 1700, a saponification degree of 88 mol%, 0.8% by weight of borax added, and a thickness of 15 μm to ice containing borax (Na2B4O7·10H2O) is treated, but the present invention is not limited to this specification of PVA, and may be applied to any water-soluble polymer polyvinyl alcohol (PVA) that can prevent or suppress the sublimation of the block ice body (ice).

[0015] Next, an example of a method for processing block ice will be described with reference to Figs.

[0016] As shown in FIG. 1(A), first, block ice B is put into a crusher 1, and the block ice B is crushed by the crusher 1 (step S1).

[0017] Next, the crushed block ice B is placed in an oil bath 2 and heated and melted in the oil bath 2 (step S2, an example of a "melting step"). At this time, the heating temperature in the oil bath 2 is set to about 80°C. This completely melts the PVA. As the oil bath 2, for example, an oil bath manufactured by Yazawa Scientific Co., Ltd. can be used. As shown in FIG. 2(B), the dissolving liquid in the oil bath 2 is stirred by a stirrer 4. If the block ice B can be melted in the oil bath 2 without being crushed, step S1 may be omitted.

[0018] Next, as shown in FIG. 1(C), the dissolving solution is transferred from the oil bath 2 to a treatment tank 3.

[0019] Next, as shown in FIG. 2(A), the dissolving solution in the treatment tank 3 is stirred by the stirrer 4. Magnesium sulfate (MgSO4·7H2O) is added while checking the pH of the dissolving solution with a pH meter (step S3, an example of an "adding step"). The pH is measured here to check the reaction in the aqueous solution. The PVA aqueous solution is weakly acidic (due to the partially saponified PVA), while the borax aqueous solution is weakly alkaline. The pH of the dissolving solution in which block ice B was dissolved was "9". When magnesium sulfate was added to this dissolving solution, the pH dropped to "7", which means that a compound of magnesium sulfate and borax was formed. By measuring the pH in this way, the degree of reaction in the dissolving solution can be confirmed. 0.4 g of magnesium sulfate (MgSO4·7H2O) is added per 1 ml of dissolving solution. However, the amount of magnesium sulfate (MgSO4·7H2O) added can be an amount that allows the PVA in the dissolving solution to be sufficiently precipitated.

[0020] By adding magnesium sulfate (MgSO4·7H2O) to the solution, the PVA in the solution becomes a precipitate. Here, the PVA in the solution (PVA solution) is a hydrophilic colloid, and the hydrophilic OH group of PVA strongly attracts water molecules through hydrogen bonds. When a large amount of electrolyte solution (magnesium sulfate, etc.) is added to the hydrocolloid solution, the added ions (Mg 2+ions), hydration occurs more strongly in the colloidal particles, and water molecules are separated from the hydrophilic groups on the surface of the colloidal particles. As a result, the PVA from which the water molecules have been separated aggregates (salting out) due to intermolecular forces, and the PVA separates from the PVA aqueous solution. Note that salting out can occur even at room temperature, but the higher the temperature of the aqueous solution, the faster the salting out reaction. The effect of salting out is stronger in salts containing ions with stronger hydration power, and ions with a smaller ionic radius have stronger hydration power for the same valence. That is, Mg 2+ >Ca 2+ >Sr 2+ >Ba 2+ In addition, among compounds containing divalent ions, sulfates and hydroxides containing Ca and Sr, except for Mg ions, are almost insoluble in water. The solubility of magnesium sulfate in water is 25.5g / 100mL (20℃), while the solubility of calcium sulfate in water is 0.24g / 100mL (20℃). Magnesium sulfate is a heptahydrate (MgSO4·7H2O), and 49% of MgSO4·7H2O is MgSO4. As half of the amount is water molecules, when adding MgSO4·7H2O to a PVA aqueous solution, it is possible to directly add MgSO4·7H2O crystal powder without the need to make it into an aqueous solution.

[0021] 2(B), the dissolving solution in the treatment tank 3 is poured into a waste can 6 equipped with a filter bag 7 to separate the precipitate in the dissolving solution from the dissolving solution (step S4, an example of a "separation process"). As a result, the precipitate (PVA) in the dissolving solution is taken out into the filter bag 7, and the dissolving solution containing borax (Na2B4O7·10H2O) from which the PVA has been separated is stored in the waste can 6.

[0022] As described above, the method for treating block ice in this embodiment includes a melting process in which block ice B, which includes ice containing borax (Na2B4O7·10H2O) and polyvinyl alcohol (PVA) covering the ice, is heated and melted, an adding process in which magnesium sulfate (MgSO4·7H2O) is added to the melting solution obtained in the melting process, and a separating process in which a precipitate in the melting solution obtained by adding magnesium sulfate is separated from the melting solution.

[0023] Therefore, according to the method for processing block ice B of this embodiment, magnesium sulfate (MgSO4·7H2O) is added to the solution obtained in the melting process to precipitate PVA, and by separating this, block ice B can be separated into PVA and a solution containing borax. [Explanation of symbols]

[0024] 1: Crusher 2: Oil bath 3: Treatment tank 4: Stirrer 6: Waste cans 7: Filtration bag B: Block ice

Claims

1. Borax (Na 2 B 4 O 7 ・10H 2 A melting step of heating and melting block ice including ice containing O and polyvinyl alcohol (PVA) covering the ice; The solution obtained in the dissolution step was treated with magnesium sulfate (MgSO 4 ・7H 2 O) is added; a separation step of separating a precipitate in the solution obtained by adding the magnesium sulfate from the solution; 1. A method for treating block ice, comprising:

2. 2. A method for treating block ice according to claim 1, comprising the steps of: A method for treating block ice, wherein the PVA has a degree of polymerization of 1700, a degree of saponification of 88 mol %, and contains 0.8% by weight of borax.

3. 3. A method for treating block ice according to claim 1 or 2, comprising the steps of: In the addition step, magnesium sulfate (MgSO 4 ・7H 2 A method for treating block ice, comprising adding 0.4 g of

Citation Information

Patent Citations

  • Ice condenser, sublimation preventive cooling body used therefor, and its production method

    JP2000147180A

  • Sublimation prevention cooling body manufacturing method

    JP3876241B2