Method for manufacturing light-emitting element

The method enhances light extraction efficiency in light emitting devices by forming a laminated transparent conductive layer with aligned crystal grains, addressing the challenge of light transmission in semiconductor-based devices.

JP7554385B2Active Publication Date: 2024-09-20NICHIA CORP
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2022038338
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-03-11
Publication Date
2024-09-20
Estimated Expiration
2042-03-11

AI Technical Summary

Technical Problem

Existing light emitting devices using semiconductor materials face challenges in improving light extraction efficiency, particularly due to the use of conductive layers that hinder light transmission.

Method used

A manufacturing method involving the formation of a transparent conductive layer with a laminated structure, where a first layer is formed at a low temperature and then heat-treated to align crystal orientation, followed by a thicker second layer to enhance transparency and reduce resistivity.

Benefits of technology

The method results in a transparent conductive layer with low resistivity and high light transmittance, leading to improved light extraction efficiency in the light emitting device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554385000003
    Figure 0007554385000003
  • Figure 0007554385000011
    Figure 0007554385000011
  • Figure 0007554385000017
    Figure 0007554385000017
Patent Text Reader

Abstract

To provide a method for manufacturing a light emitting element improved in light extraction efficiency.SOLUTION: A method for manufacturing a light emitting element 100 includes the steps of: preparing a semiconductor structure 10 including a first semiconductor layer 11, a second semiconductor layer 12, and an active layer 13 located between the first semiconductor layer 11 and the second semiconductor layer 12; forming a first light-transmitting conductive layer 21 with a first film thickness at a first temperature, on the second semiconductor layer 12; heating the first light-transmitting conductive layer 21 at a second temperature higher than the first temperature in an oxygen-containing atmosphere; and, after the step of heating, forming a second light-transmitting conductive layer 22 having a second film thickness thicker than the first film thickness at a third temperature higher than the first temperature, on the first light-transmitting conductive layer 21.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a light-emitting device. [Background technology]

[0002] Patent Document 1 discloses that in a light-emitting device using a semiconductor such as a nitride semiconductor, a light-transmitting conductive layer such as ITO is disposed on a semiconductor layer. In such a light-emitting device, it is desired to dispose a conductive layer having high light transmittance to improve the light extraction efficiency. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2012-156312 A Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the present invention is to provide a method for manufacturing a light-emitting device having improved light extraction efficiency. [Means for solving the problem]

[0005] A method for manufacturing a light-emitting element according to one embodiment of the present invention includes the steps of: preparing a semiconductor structure including a first semiconductor layer, a second semiconductor layer, and an active layer located between the first semiconductor layer and the second semiconductor layer; forming a first light-transmitting conductive layer having a first thickness on the second semiconductor layer at a first temperature; heating the first light-transmitting conductive layer at a second temperature higher than the first temperature in an oxygen-containing atmosphere; and, after the heating step, forming a second light-transmitting conductive layer having a second thickness thicker than the first thickness on the first light-transmitting conductive layer at a third temperature higher than the first temperature. Effect of the Invention

[0006] According to the method for manufacturing a light-emitting element according to one embodiment of the present invention, a light-transmitting conductive layer having low resistivity and high light transmittance is formed, making it possible to provide a light-emitting element with improved light extraction efficiency. [Brief description of the drawings]

[0007] [Figure 1] 1 is a schematic cross-sectional view showing a light-emitting element according to one embodiment of the present invention. [Diagram 2] 1 is a flowchart showing a method for manufacturing a light emitting device. [Diagram 3] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 4] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Diagram 5] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 6] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 7] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 8] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 9] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 10] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 11] 1A to 1C are cross-sectional views illustrating a manufacturing process of the light emitting device. [Figure 12] 1 is a graph showing the results of XRD measurement of the translucent conductive layers of Example 1, Comparative Example 1, and Comparative Example 2. [Figure 13] 3 is an AFM photograph of the transparent conductive layer according to Example 1. [Figure 14] 1 is an AFM photograph of a transparent conductive layer according to Comparative Example 1. [Figure 15] 11 is an AFM photograph of a transparent conductive layer according to Comparative Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The present invention will be described in more detail below with reference to the drawings. In the following description, terms indicating specific directions or positions (e.g., "upper", "lower", and other terms including these terms) are used as necessary, but the use of these terms is for the purpose of facilitating understanding of the invention with reference to the drawings, and the meaning of these terms does not limit the technical scope of the present invention. In addition, parts with the same reference numerals appearing in multiple drawings indicate the same or equivalent parts or members.

[0009] Furthermore, the embodiments shown below are specific examples of the technical ideas of the present invention, and do not limit the present invention to the following. Furthermore, unless otherwise specified, the dimensions, materials, shapes, relative positions, etc. of the components described below are intended to be illustrative and not to limit the scope of the present invention. Furthermore, the sizes and positional relationships of the components shown in the drawings may be exaggerated to clarify the explanation. [Embodiment 1]

[0010] A schematic cross-sectional view of a light-emitting device according to embodiment 1 is shown in Fig. 1. The light-emitting device 100 shown in this figure includes a substrate 1, a semiconductor structure 10, a light-transmitting conductive layer 20, and an electrode 30. The semiconductor structure 10 includes a first semiconductor layer 11, a second semiconductor layer 12, and an active layer 13 located between the first semiconductor layer 11 and the second semiconductor layer 12. The light-transmitting conductive layer 20 includes a first light-transmitting conductive layer 21 and a second light-transmitting conductive layer 22. The electrode 30 includes a first electrode 31 and a second electrode 32. (Substrate 1)

[0011] The substrate 1 supports the semiconductor structure 10. The substrate 1 may be a growth substrate for epitaxially growing the semiconductor structure 10. For example, when a nitride semiconductor is used for the semiconductor structure 10, the substrate 1 may be a sapphire (Al2O3) substrate, a gallium nitride substrate, a SiC substrate, or the like. The semiconductor structure 10 is disposed on, for example, the C-plane of the sapphire substrate. (Semiconductor structure 10)

[0012] The semiconductor structure 10 is disposed on the upper surface of the substrate 1. The semiconductor structure 10 has a first semiconductor layer 11 of a first conductivity type, a second semiconductor layer 12 of a second conductivity type, and an active layer 13 located between the first semiconductor layer 11 and the second semiconductor layer 12. The first conductivity type is n-type or p-type. The second conductivity type is a conductivity type different from the first conductivity type, and is p-type or n-type. In this embodiment, the first conductivity type is n-type, and the second conductivity type is p-type. By applying a voltage between a first electrode 31 disposed on the first semiconductor layer 11 and a second electrode 32 disposed on the second semiconductor layer 12, the active layer 13 emits light. The light from the active layer 13 is, for example, ultraviolet light or visible light. The emission peak wavelength of the active layer 13 is, for example, 400 nm or more and 540 nm or less.

[0013] The first semiconductor layer 11 has an exposed portion exposed from the second semiconductor layer 12 and the active layer 13. The second semiconductor layer 12 and the active layer 13 are not disposed on the exposed portion of the first semiconductor layer 11.

[0014] The semiconductor structure 10 is, for example, a laminate in which a plurality of semiconductor layers made of nitride semiconductors are laminated. Here, the term "nitride semiconductor" refers to a semiconductor containing nitrogen, typically In. x Al y Ga 1-x-y It includes all semiconductors with compositions in which the composition ratios x and y in the chemical formula N (0≦x≦1, 0≦y≦1, x+y≦1) are changed within the respective ranges. (Dielectric layer 40)

[0015] The dielectric layer 40 is disposed on a part of the upper surface of the first semiconductor layer 11 and a part of the upper surface of the second semiconductor layer 12. The dielectric layer 40 is disposed between the first semiconductor layer 11 and the first electrode 31, and between the second semiconductor layer and the second electrode 32. The dielectric layer 40 is disposed to totally reflect the light from the active layer 13 toward the first electrode 31 or the second electrode 32 at the interface between the semiconductor structure 10 and the dielectric layer 40, thereby improving the light extraction efficiency. For the dielectric layer 40, for example, an insulating material such as silicon oxide, silicon nitride, or silicon oxynitride can be used. The dielectric layer 40 may not be disposed. (Transparent conductive layer 20)

[0016] The translucent conductive layer 20 is disposed on the second semiconductor layer 12. The translucent conductive layer 20 has a laminated structure in which a first translucent conductive layer 21 and a second translucent conductive layer 22 are laminated in this order from the second semiconductor layer 12 side. The translucent conductive layer 20 is electrically connected to the second semiconductor layer 12. The translucent conductive layer 20 is provided so as to cover substantially the entire upper surface of the second semiconductor layer 12, and can diffuse the current supplied to the second electrode 32 over a wider range of the second semiconductor layer 12.

[0017] The translucent conductive layer 20 may be made of, for example, a metal oxide having electrical conductivity. The translucent conductive layer 20 may be made of, for example, an oxide containing at least one element selected from the group consisting of Zn, In, Sn, Ga, and Ti. For example, the translucent conductive layer 20 may be made of ITO or ZnO. ITO and ZnO are materials with low electrical resistivity, and therefore are suitable materials for covering substantially the entire upper surface of the first semiconductor layer 11. (First transparent conductive layer 21)

[0018] The first translucent conductive layer 21 is disposed on the second semiconductor layer 12. The first translucent conductive layer 21 is disposed, for example, so as to cover the second semiconductor layer 12 and the dielectric layer 40. The film thickness of the first translucent conductive layer 21 is defined as a first film thickness. The first film thickness is preferably, for example, 2 nm or more and 8 nm or less. By reducing the film thickness of the first translucent conductive layer 21, it is possible to reduce light absorption by the first translucent conductive layer 21. (Second transparent conductive layer 22)

[0019] The second translucent conductive layer 22 is disposed on the first translucent conductive layer 21. The second translucent conductive layer 22 has a second film thickness that is thicker than the first film thickness, which is the film thickness of the first translucent conductive layer 21.

[0020] The average diameter of the crystal grains of the first translucent conductive layer 21 and the second translucent conductive layer 22 is, for example, preferably 1 μm or more, and more preferably 1 μm or more and 10 μm or less. The larger average diameter of the crystal grains of the translucent conductive layer 20 improves the translucency of the translucent conductive layer 20. The light transmittance of the translucent conductive layer 20 including the first translucent conductive layer 21 and the second translucent conductive layer 22 can be, for example, 60% or more, and preferably 70% or more.

[0021] Furthermore, the second film thickness is preferably 5 to 40 times the first film thickness. Specifically, the second film thickness is preferably 40 to 300 nm. By reducing the film thickness of the second translucent conductive layer 22, an increase in the resistivity of the translucent conductive layer 20 can be reduced. The resistivity of the translucent conductive layer 20 including the first translucent conductive layer 21 and the second translucent conductive layer 22 can be 150 μΩ·cm or less.

[0022] The first electrode 31 is disposed on the first semiconductor layer 11 and is electrically connected to the first semiconductor layer 11. The first electrode 31 may be made of, for example, Cu, Au, or an alloy containing these metals as a main component, so as to be suitable for connection to the outside by wire bonding or the like. The first electrode 31 may have a laminated structure including multiple metal layers.

[0023] The second electrode 32 is disposed on the second translucent conductive layer 22 and is electrically connected to the second semiconductor layer 12 via the first translucent conductive layer 21 and the second translucent conductive layer 22. The second electrode 32 may be made of, for example, Cu, Au, or an alloy containing these metals as a main component, so as to be suitable for connection to the outside by wire bonding or the like. The second electrode 32 may have a laminated structure including multiple metal layers.

[0024] The surface of the light-emitting element 100 is covered with a protective film 60. The protective film 60 has openings that expose a part of the upper surface of the p-side electrode 32b and a part of the upper surface of the second n-side electrode 31b. Through the openings of the protective film 60, the first electrode 31 and the second electrode 32 are electrically connected to the outside. The protective film 60 may be made of an insulating material such as silicon oxide, silicon nitride, or silicon oxynitride. The protective film 60 does not necessarily have to be provided. [Method of manufacturing light-emitting element]

[0025] A method for manufacturing the light-emitting device of the first embodiment will be described with reference to Figs. 1 to 11. First, a step S1 is performed to prepare a semiconductor structure 10. For example, as shown in Fig. 3, a sapphire substrate is prepared as a substrate 1, and the semiconductor structure 10 including a first semiconductor layer 11, an active layer 13, and a second semiconductor layer 12 is formed on the substrate 1 to prepare the semiconductor structure 10. The semiconductor structure 10 is formed, for example, by forming an n-type semiconductor layer as the first semiconductor layer 11 on the substrate 1, forming the active layer 13 on the n-type semiconductor layer, and further forming a p-type semiconductor layer as the second semiconductor layer 12 on the active layer 13 in this order. Such a semiconductor structure 10 can be formed by a liquid phase growth method, a hydride vapor phase epitaxy (HVPE) method, or a metal organic chemical vapor deposition (MOCVD) method.

[0026] Next, as shown in Fig. 4, a part of the second semiconductor layer 12, a part of the active layer 13, and a part of the first semiconductor layer 11 are removed from the second semiconductor layer 12 side by etching or the like to expose a part of the first semiconductor layer 11 from the second semiconductor layer 12 and the active layer 13. Next, as shown in Fig. 5, a dielectric layer 40 is partially formed on the second semiconductor layer 12 and on the exposed first semiconductor layer 11, respectively. The dielectric layer 40 can be formed by, for example, a vapor deposition method or a sputtering method. Note that in this specification, preparing the semiconductor structure 10 also includes obtaining a ready-made semiconductor structure.

[0027] Next, in step S2, a process of forming a first translucent conductive layer 21 having a first thickness on the second semiconductor layer 12 at a first temperature is performed. The first translucent conductive layer 21 is formed so as to cover the second semiconductor layer 12, the first semiconductor layer 11, and the dielectric layer 40, as shown in Fig. 6, for example. By forming it at the first temperature, the first translucent conductive layer 21 is formed in an amorphous state. The first temperature is, for example, 25°C or more and 35°C or less.

[0028] The first translucent conductive layer 21 can be formed by, for example, a vapor deposition method or a sputtering method. For example, a reactive plasma deposition (RPD) method, which is one of the vapor deposition methods, can be used to form the first translucent conductive layer 21. In addition, when forming the first translucent conductive layer 21, it is preferable to use a vacuum vapor deposition method in which vapor deposition is performed in a vacuum. In consideration of damage to the second semiconductor layer 12 when forming the first translucent conductive layer 21, it is preferable to form the first translucent conductive layer 21 by a vapor deposition method rather than a sputtering method. On the other hand, the sputtering method can also be used to form the second translucent conductive layer 22 described later, and is therefore preferable in terms of improving productivity.

[0029] Next, in step S3, the first translucent conductive layer 21 is heated at a second temperature higher than the first temperature in an oxygen-containing atmosphere. The second temperature is preferably 200° C. or more and 500° C. or less. In this way, the first translucent conductive layer 21 is formed in an amorphous state at a relatively low first temperature, and then heated at a second temperature higher than the first temperature. In this way, the first translucent conductive layer 21 is formed in an uncrystallized state and heated in an oxygen-containing atmosphere, thereby forming large crystal grains on the surface of the first translucent conductive layer 21. In addition, the first translucent conductive layer 21 after being formed at the first temperature tends to have a poor crystal orientation, and the first translucent conductive layer 21 tends to have a uniform crystal orientation by heating it at the second temperature. In this way, the crystal orientation can be uniformed by heating the first translucent conductive layer 21 after its formation, so that the electron mobility in the first translucent conductive layer 21 can be increased and the sheet resistance can be reduced.

[0030] Next, in step S4, a process of forming a second translucent conductive layer 22 having a second thickness at a third temperature is performed on the first translucent conductive layer 21. The second translucent conductive layer 22 is formed on the first translucent conductive layer 21 formed on the second semiconductor layer 12 and the first semiconductor layer 11, as shown in Fig. 7, for example. The third temperature is a temperature higher than the first temperature. The third temperature is, for example, 200°C or higher and 500°C or lower.

[0031] The second light-transmitting conductive layer 22 can be formed by, for example, a vapor deposition method or a sputtering method. The thickness of the second light-transmitting conductive layer 22 is thicker than the first thickness. The second thickness is, for example, 40 nm or more and 80 nm or less.

[0032] As described above, the second translucent conductive layer 22 is formed at a third temperature higher than the first temperature on the first translucent conductive layer 21, which has relatively large crystal grains formed on its surface by heating. This makes it possible to form the second translucent conductive layer 22, which has undergone crystal growth while inheriting the crystalline state of the surface of the first translucent conductive layer 21.

[0033] The manufacturing method of the light emitting device 100 according to the present embodiment can form the highly light transmissive conductive layer 20 including the first light transmissive conductive layer 21 and the second light transmissive conductive layer 22, and therefore can obtain a light emitting device with improved light extraction efficiency. By reducing the thickness of the first light transmissive conductive layer 21, which has a higher resistivity than the second light transmissive conductive layer 22, it is possible to reduce deterioration of the resistivity of the light transmissive conductive layer 20. In addition, by forming the second light transmissive conductive layer 22 on the heated first light transmissive conductive layer 21, the crystal grains in the first light transmissive conductive layer 21 and the second light transmissive conductive layer 22 are enlarged, and a light transmissive conductive layer 20 that has both low resistivity and high light transmissivity is realized.

[0034] Next, in step S5, a process of removing a part of the first translucent conductive layer 21 and a part of the second translucent conductive layer 22 is performed. Specifically, as shown in FIG. 8, a resist mask 50 is formed on a part of the second translucent conductive layer 22 located above the second semiconductor layer 12. In this state, as shown in FIG. 9, a part of the first translucent conductive layer 21 and a part of the second translucent conductive layer 22 are etched through the resist mask 50. Thereafter, the resist mask 50 is removed to form the translucent conductive layer 20 formed on a part of the second semiconductor layer 12. In this manner, a translucent conductive layer 20 having low resistivity and high translucency can be formed.

[0035] Next, in step S6, a process of forming electrodes is performed. Specifically, as shown in Fig. 10, a first n-side electrode 31a is formed on the exposed upper surface of the first semiconductor layer 11 to cover the dielectric layer 40. Next, as shown in Fig. 11, a p-side electrode 32b is formed on the upper surface of the second translucent conductive layer 22, and a second n-side electrode 31b is formed on the upper surface of the first n-side electrode 31a. The electrodes can be formed by, for example, a vapor deposition method or a sputtering method.

[0036] Finally, in step S7, the protective film 60 is formed. Specifically, as shown in FIG. 1, the protective film 60 is formed so as to cover the semiconductor structure 10, the light-transmitting conductive layer 20, the first n-side electrode 31a, the second n-side electrode 31b, and the p-side electrode 32b. As shown in FIG. 1, the protective film 60 has openings that expose a part of the upper surface of the p-side electrode 32b and a part of the upper surface of the second n-side electrode 31b. The protective film 60 can be formed by, for example, a vapor deposition method or a sputtering method. In this manner, the light-emitting device 100 according to Example 1 is obtained. [Example 1]

[0037] Next, in order to confirm the effect of the present invention, a translucent conductive layer according to Example 1 was prepared and compared with the translucent conductive layers according to Comparative Examples 1 and 2. As the translucent conductive layer according to Example 1, a translucent conductive layer including a first translucent conductive layer and a second translucent conductive layer was formed. First, an ITO layer having a thickness of 3 nm was formed as the first translucent conductive layer on a sapphire substrate. The first translucent conductive layer was formed by a vacuum deposition method at a temperature of 30°C.

[0038] Next, the first light-transmitting conductive layer was heated at a temperature of 250° C. in an atmosphere containing oxygen.

[0039] Furthermore, a second translucent conductive layer was formed at a third temperature on the heated first translucent conductive layer. An ITO layer having a thickness of 57 nm was formed as the second translucent conductive layer. The second translucent conductive layer was formed by a vacuum deposition method at a temperature of 250° C. In this manner, the translucent conductive layer according to Example 1 was formed. [Comparative Example 1]

[0040] In Comparative Example 1, an ITO layer having a thickness of 60 nm was formed as the translucent conductive layer. The translucent conductive layer according to Comparative Example 1 was formed by sputtering at a temperature of 30°C. [Comparative Example 2]

[0041] In Comparative Example 2, a 60 nm ITO layer was formed as the translucent conductive layer in the same manner as in Comparative Example 1. The translucent conductive layer in Comparative Example 2 was formed by the same film formation method and at the same temperature as the second translucent conductive layer in Example 1. (Comparative Test)

[0042] The resistivity, light transmittance, and XRD were measured for the thus obtained translucent conductive layers according to Example 1 and Comparative Examples 1 and 2. The measurements were performed after the translucent conductive layers according to Example 1 and Comparative Examples 1 and 2 were subjected to a heat treatment at 455° C. in an oxygen-containing atmosphere and a heat treatment at 400° C. in a vacuum.

[0043] The resistivity of the translucent conductive layers according to Example 1 and Comparative Examples 1 and 2 was measured. The measurements were performed using a Loresta-GP device manufactured by Mitsubishi Chemical Corporation. The results are shown in Table 1. The rate of change in resistivity in Table 1 indicates the rate of change in resistivity for Comparative Example 2 and Example 1, respectively, when the resistivity for Comparative Example 1 is used as the reference. [Table 1]

[0044] As shown in Table 1, it was confirmed that the resistivity of Example 1 was reduced more than that of Comparative Example 1 and Comparative Example 2. In particular, the resistivity of Example 1 was reduced to about half that of Comparative Example 1. In addition, in comparison with Comparative Example 2, it was confirmed that Example 1, in which the first translucent conductive layer was formed by a deposition method, and then the first translucent conductive layer was heat-treated, and then the second translucent conductive layer was formed by a deposition method, was more effective in reducing the resistivity than Comparative Example 2, in which the translucent conductive layer was formed only by a deposition method.

[0045] Next, the light transmittance of the light-transmitting conductive layers according to Example 1 and Comparative Examples 1 and 2 was measured. The measurements were performed using an ARM-500 device manufactured by JASCO Corporation. The results are shown in Table 2. The rate of change in transmittance in Table 2 indicates the rate of change in transmittance of Comparative Example 2 and Example 1, respectively, when the transmittance of Comparative Example 1 is used as the reference. [Table 2]

[0046] As shown in Table 2, it was confirmed that the transmittance of Example 1 was improved compared to Comparative Examples 1 and 2. In addition, no significant difference in transmittance was confirmed between Comparative Examples 1 and 2.

[0047] Next, in order to confirm the crystallinity, the XRD (2θ-ω) of the transparent conductive layers according to Example 1, Comparative Examples 1 and 2 was measured. The measurement was performed using an X'Pert PRO device manufactured by PANalytical. The results are shown in the graph of FIG. 12. FIG. 12 shows the measurement waveforms of Example 1, Comparative Example 1 and Comparative Example 2, which are shifted vertically. As shown in FIG. 12, it was confirmed that the (400) of In2O3 was more prominent in Example 1 than in Comparative Examples 1 and 2. On the other hand, it was confirmed that the (222) of In2O3 was prominent in Comparative Example 2. In addition, it was confirmed that the peak at (400) of In2O3 was higher in Example 1 than in Comparative Example 1, and the crystal orientation of ITO was more uniform than in Comparative Example 1.

[0048] Finally, in order to confirm the size of the crystal grains, AFM images of the transparent conductive layers according to Example 1 and Comparative Examples 1 and 2 were observed. Here, the transparent conductive layers according to Example 1 and Comparative Examples 1 and 2 were subjected to a heat treatment at 455°C in an oxygen-containing atmosphere and a heat treatment at 400°C in a vacuum, and then the surface of the transparent conductive layer was etched with hydrochloric acid for 30 seconds, and then the observation was performed. The observation was performed using a DIMENSION FastScan device manufactured by BRUKER. The results are shown in Figures 13, 14, and 15. In these figures, Figure 13 shows a photograph of Example 1, Figure 14 shows a photograph of Comparative Example 1, and Figure 15 shows a photograph of Comparative Example 2.

[0049] When the size of a single crystal grain formed on the surface of the translucent conductive layer according to Example 1 and Comparative Examples 1 and 2 was measured, multiple crystal grains with a size of 2 μm or more were confirmed in Example 1. Crystal grains with a size of 1 μm or less were confirmed in Comparative Example 1, and crystal grains with a size of 0.1 μm or less were confirmed in Comparative Example 2. From these findings, it was confirmed that larger crystal grains were formed in Example 1 than in Comparative Examples 1 and 2. [Explanation of symbols]

[0050] 100...Light emitting element 1...Substrate 10...Semiconductor structure 11...First semiconductor layer 12...Second semiconductor layer 13…Active layer 20...Transparent conductive layer 21...First transparent conductive layer 22...Second transparent conductive layer 30...electrode 31...first electrode; 31a...first n-side electrode; 31b...second n-side electrode 32...second electrode; 32b...p side electrode 40...Dielectric layer 50...Resist mask 60...Protective film

Claims

1. A first semiconductor layer; A second semiconductor layer; an active layer located between the first semiconductor layer and the second semiconductor layer; providing a semiconductor structure comprising: forming a first light-transmitting conductive layer of indium tin oxide having a first thickness in an amorphous state at a first temperature on the second semiconductor layer; heating the first light-transmitting conductive layer in an oxygen-containing atmosphere at a second temperature higher than the first temperature; forming a second light-transmitting conductive layer, which is indium tin oxide and has a second thickness greater than the first thickness, on the first light-transmitting conductive layer after the heating step at a third temperature greater than the first temperature; A method for manufacturing a light-emitting device comprising the steps of:

2. A method for producing the light-emitting device according to claim 1, comprising the steps of: The method for manufacturing a light-emitting device, wherein the first light-transmitting conductive layer is formed by a vapor deposition method.

3. A method for producing the light-emitting device according to claim 1 or 2, comprising the steps of: The second light-transmitting conductive layer is formed by a sputtering method or a vapor deposition method.

4. A method for producing the light-emitting device according to any one of claims 1 to 3, comprising the steps of: The second temperature is 200° C. or higher and 500° C. or lower.

5. A method for producing the light-emitting device according to any one of claims 1 to 4, comprising the steps of: The method for manufacturing a light-emitting device, wherein the second film thickness is 5 to 40 times the first film thickness.

6. A method for producing the light-emitting device according to any one of claims 1 to 5, comprising the steps of: The method for manufacturing a light-emitting element, wherein the first film thickness is 2 nm or more and 8 nm or less.

7. A method for producing the light-emitting device according to any one of claims 1 to 6, comprising the steps of: The method for manufacturing a light-emitting element, wherein the second film thickness is 40 nm or more and 80 nm or less.

8. A method for producing the light-emitting device according to any one of claims 1 to 7, comprising the steps of: The method for manufacturing a light-emitting element, wherein the first temperature is 25° C. or higher and 35° C. or lower.

Citation Information

Patent Citations

  • Preparation method of laminated transparent conducting layer LED (light emitting diode) chip

    CN102832299A

  • Semiconductor light emitting element and its manufacturing method

    JP2001085742A

  • Gallium nitride semiconductor light emitting element and manufacturing method therefor

    JP2001210867A

  • Method of manufacturing light-emitting element

    JP2008140918A

  • Gallium nitride compound semiconductor light-emitting device and method for manufacturing the same

    JP2008177514A