Resist underlayer film forming composition and method for forming resist pattern using same
The resist underlayer film forming composition with a polymer having specific terminal structures addresses LWR and adhesion issues in EUV exposure, improving the uniformity and sensitivity of resist patterns in semiconductor manufacturing.
Patent Information
- Application Number
- JP2023067837
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-10-05
- Filing Date
- 2023-04-18
- Publication Date
- 2024-09-26
- Estimated Expiration
- 2039-10-01
AI Technical Summary
The formation of resist patterns in semiconductor manufacturing faces challenges such as line width roughness (LWR), pinholes, aggregation, and poor adhesion during EUV exposure, which affect the uniformity and sensitivity of the resist pattern.
A resist underlayer film forming composition containing a polymer with specific terminal structures and an organic solvent, optionally with a crosslinking agent, is used to form a resist underlayer film that enhances adhesion and reduces LWR, improving the rectangular shape and sensitivity of the resist pattern.
The composition effectively suppresses LWR and improves resist pattern formation sensitivity, ensuring uniform film formation without defects and enhancing the rectangular shape of the resist pattern.
Smart Images

Figure 0007556423000013 
Figure 0007556423000018 
Figure 0007556423000036
Abstract
Description
[Technical field]
[0001] The present invention relates to a resist underlayer film-forming composition for lithography, which is intended to suppress deterioration of LWR (Line Width Roughness, fluctuation in resist pattern line width) during resist pattern formation and to improve resist sensitivity in the lithography process during semiconductor device manufacturing, and a method for forming a resist pattern using the resist underlayer film-forming composition. [Background technology]
[0002] Conventionally, in the manufacture of semiconductor devices, microfabrication by lithography using a resist composition has been performed. The microfabrication is a processing method in which a thin film of a photoresist composition is formed on a semiconductor substrate such as a silicon wafer, and the thin film is irradiated with active light such as ultraviolet light through a mask pattern on which a device pattern is drawn, developed, and the substrate is etched using the obtained photoresist pattern as a protective film, thereby forming fine irregularities corresponding to the pattern on the substrate surface. In recent years, the integration density of semiconductor devices has increased, and the active light used has been studied for practical use in cutting-edge microfabrication in addition to the conventionally used i-line (wavelength 365 nm), KrF excimer laser (wavelength 248 nm), and ArF excimer laser (wavelength 193 nm). As a result, the diffuse reflection of the active light from the semiconductor substrate and the influence of standing waves have become major problems. Therefore, in order to solve this problem, a method of providing an anti-reflective coating (Bottom Anti-Reflective Coating: BARC) between the resist and the semiconductor substrate has been widely studied. The anti-reflective coating is also called a resist underlayer film. As such an anti-reflection film, organic anti-reflection films made of polymers having light-absorbing sites have been much investigated because of their ease of use. Patent Document 1 discloses an anti-reflective coating for semiconductors that contains a condensation polymer. Patent Document 2 discloses a resist underlayer coating for lithography that contains a polymer that has an optionally substituted aryl ester group at its terminal. Patent Document 3 discloses a resist underlayer coating forming composition that contains a polymer that has a sulfonyl group introduced at its terminal. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2005 / 098542 [Patent Document 2] International Publication No. 2015 / 046149 [Patent Document 3] International Publication No. 2015 / 163195 Summary of the Invention [Problem to be solved by the invention]
[0004] Required properties of the resist underlayer film include, for example, the absence of intermixing with the resist film formed on the upper layer (being insoluble in a resist solvent) and a faster dry etching rate than the resist film. In the case of lithography involving EUV exposure, the line width of the formed resist pattern is 32 nm or less, and the resist underlayer film for EUV exposure is formed to be thinner than conventional films. When forming such a thin film, pinholes and aggregation are likely to occur due to the influence of the substrate surface and the polymer used, making it difficult to form a uniform film without defects. On the other hand, when forming a resist pattern, a method may be adopted in which a solvent capable of dissolving the resist film, usually an organic solvent, is used to remove the unexposed portion of the resist film in the development step, leaving the exposed portion of the resist film as a resist pattern. In such a negative development process, improving the adhesion of the resist pattern is a major issue. There is also a demand for suppressing deterioration of LWR (Line Width Roughness) during resist pattern formation, forming resist patterns with good rectangular shapes, and improving resist sensitivity. An object of the present invention is to provide a composition for forming a resist underlayer film capable of forming a desired resist pattern, which has solved the above-mentioned problems, and a method for forming a resist pattern using the resist underlayer film-forming composition. [Means for solving the problem]
[0005] The present invention encompasses the following: [1] A resist underlayer film forming composition comprising a polymer having a structure represented by the following formula (1) or (2) at an end of the polymer chain, and an organic solvent: [ka] (In the above formulas (1) and (2), X is a divalent organic group, A is an aryl group having 6 to 40 carbon atoms, R1 is a halogen atom, an alkyl group having 1 to 10 carbon atoms, or an alkoxy group having 1 to 10 carbon atoms, R2 and R3 are each independently a hydrogen atom, a halogen atom, an alkyl group having 1 to 10 carbon atoms which may be substituted, or an aryl group having 6 to 40 carbon atoms which may be substituted, n1 and n3 are each independently an integer of 1 to 12, and n2 is an integer of 0 to 11.) [2] In the formulas (1) and (2), X is an ester bond or an ether bond. [3] In the formulas (1) and (2), A is a phenyl group, a naphthyl group, or an anthracenyl group. [4] The resist underlayer film forming composition according to [1], wherein in the formula (2), R2 and R3 are hydrogen atoms. [5] The resist underlayer film forming composition according to [1], wherein in the formula (1), n2 is 0.
[0006] [6] The resist underlayer film forming composition according to [1], wherein the polymer has a structural unit represented by the following formula (3): [ka] (In formula (3), A1, A2, A3, A4, A5 and A6 each independently represent a hydrogen atom, a methyl group or an ethyl group, and Y1 represents a group represented by formula (4), formula (5), formula (6) or formula (7): [ka] (In the formulas (4) to (7), R4 and R5 each independently represent a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; R4 and R5 may be bonded to each other to form a ring having 3 to 6 carbon atoms; R6 represents an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms), and Q represents a formula (8) or a formula (9): [ka] (In the formulas (8) and (9), Q1 represents an alkylene group having 1 to 10 carbon atoms, a phenylene group, a naphthylene group, or an anthrylene group, and the phenylene group, naphthylene group, and anthrylene group may each be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; n4 and n5 each independently represent an integer of 0 or 1; and Y2 represents the formula (4), the formula (5), or the formula (7).)
[0007] [7] The resist underlayer film forming composition according to [6], wherein the polymer having a structural unit represented by formula (3) is a polymer obtained by reacting a compound represented by formula (10) with a compound represented by formula (11). [ka] (In formulas (10) and (11), A1, A2, A3, A4, A5, A6, Y1 and Q have the same meanings as defined in [6].)
[0008] [8] The resist underlayer film forming composition according to [6], wherein the polymer having a structural unit represented by formula (3) is a polymer obtained by reacting a compound represented by formula (12) with a compound represented by formula (13). [ka] (In the formula, A1, A2, A3, A4, A5, A6, Y1 and Q have the same meanings as defined in [6]).
[0009] [9] The resist underlayer film forming composition according to any one of [1] to [8], further comprising a crosslinking acid catalyst.
[10] The resist underlayer film forming composition according to any one of [1] to [9], further comprising a crosslinking agent.
[11] A resist underlayer film, which is a fired product of a coating film comprising the resist underlayer film forming composition according to any one of [1] to
[10] .
[12] A method for producing a patterned substrate, comprising the steps of: applying the resist underlayer film forming composition according to any one of [1] to
[10] onto a semiconductor substrate and baking the composition to form a resist underlayer film; applying a resist onto the resist underlayer film and baking the composition to form a resist film; exposing the resist underlayer film and the semiconductor substrate coated with the resist to light; and developing and patterning the resist film after exposure.
[13] forming a resist underlayer film on a semiconductor substrate, the resist underlayer film being composed of the resist underlayer film forming composition according to any one of [1] to
[10] ; forming a resist film on the resist underlayer film; forming a resist pattern by irradiating the resist film with light or an electron beam and then developing it; forming a patterned resist underlayer film by etching the resist underlayer film through the formed resist pattern; processing a semiconductor substrate using the patterned resist underlayer film; A method for manufacturing a semiconductor device, comprising: Effect of the Invention
[0010] The resist underlayer film forming composition for lithography of the present invention is characterized in that the terminal of the polymer contained in the resist underlayer film forming composition is capped with the structure represented by the above formula (1) or (2), and is a composition containing such a polymer and an organic solvent, and preferably further a crosslinking agent and / or a compound that promotes a crosslinking reaction. The resist underlayer film forming composition for lithography of the present application has such a constitution, and thus can achieve suppression of deterioration of LWR and improvement of sensitivity during resist pattern formation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] <Resist underlayer film forming composition> The resist underlayer film forming composition of the present application contains a polymer having a structure represented by the following formula (1) or (2) at an end of the polymer chain, and an organic solvent. [ka] (In the above formulas (1) and (2), X is a divalent organic group, A is an aryl group having 6 to 40 carbon atoms, R1 is a halogen atom, an alkyl group having 1 to 40 carbon atoms, or an alkoxy group having 1 to 40 carbon atoms, R2 and R3 are each independently a hydrogen atom, a halogen atom, an alkyl group having 1 to 10 carbon atoms which may be substituted, or an aryl group having 6 to 40 carbon atoms which may be substituted, n1 and n3 are each independently an integer of 1 to 12, and n2 is an integer of 0 to 11.)
[0012] Specific examples of X include an ester bond, an ether bond, an amide bond, a urethane bond, and a urea bond, and among these, an ester bond or an ether bond is preferable. Specific examples of A are groups derived from benzene, naphthalene, anthracene, phenanthrene or pyrene, and among these, groups derived from benzene, naphthalene or anthracene are preferred. The halogen atom includes a fluorine atom, a chlorine atom, a bromine atom and an iodine atom. Specific examples of the alkyl group having 1 to 10 carbon atoms include a methyl group, an ethyl group, a propyl group, a butyl group, a hexyl group, and a pentyl group, and among these, a methyl group is preferable. Specific examples of the alkoxy group having 1 to 10 carbon atoms include a methoxy group, an ethoxy group, a propoxy group, a butoxy group, a hexoxy group, and a pentoxy group, and among these, a methoxy group is preferable. The term "optionally substituted" means that some or all of the hydrogen atoms in the alkyl group having 1 to 10 carbon atoms may be substituted with, for example, a fluoro group or a hydroxy group. Specific examples of the alkyl group having 1 to 10 carbon atoms include a methyl group, an ethyl group, a propyl group, a butyl group, a hexyl group, and a pentyl group, with a methyl group being preferred. Specific examples of the aryl group having 6 to 40 carbon atoms include a benzyl group, a naphthyl group, an anthracenyl group, a phenanthrenyl group, and a pyrenyl group, with a phenyl group being preferred among these. n1 and n3 each independently represent an integer of 1 to 12, preferably an integer of 1 to 6. n2 is an integer of 0 to 11, preferably an integer of 0 to 2. In the formula (2), R2 and R3 are preferably hydrogen atoms. In the above formula (1), n2 is preferably 0.
[0013] The compound having the partial structure represented by the above formula (1) is represented, for example, by the following formula (1-1). [ka] (In the above formula (1-1), X is a divalent organic group, A is an aryl group having 6 to 40 carbon atoms, R1 is a halogen atom, an alkyl group having 1 to 40 carbon atoms, or an alkoxy group having 1 to 40 carbon atoms, n1 is an integer of 1 to 12, and n2 is an integer of 0 to 11.)
[0014] In the above formula (1-1), preferred X, A, R1, n1 and n2 in the present invention are as defined above. Specific examples of the compound represented by the above formula (1-1) are as follows. The polymer contained in the resist underlayer film-forming composition of the present application can be produced by reacting the following compound with a terminal of a polymer by a method known per se.
[0015] [ka]
[0016] [ka]
[0017] [ka]
[0018] [ka]
[0019] [ka]
[0020] [ka]
[0021] The compound having the partial structure represented by the above formula (2) is represented, for example, by the following formula (2-1). [ka] (In the above formula (2-1), X is a divalent organic group, A is an aryl group having 6 to 40 carbon atoms, R2 and R3 each independently represent a hydrogen atom, an optionally substituted alkyl group having 1 to 10 carbon atoms, an optionally substituted aryl group having 6 to 40 carbon atoms, or a halogen atom, and n3 is an integer of 1 to 12.)
[0022] In the above formula (2-1), preferred X, A, R2, R3 and n3 in the present invention are as defined above. Specific examples of the compound represented by the above formula (2-1) are as follows. The polymer contained in the resist underlayer film-forming composition of the present application can be produced by reacting the following compound with a polymer terminal by a method known per se.
[0023] [ka]
[0024] The polymer is not particularly limited as long as it is a polymer known per se for use in a resist underlayer film-forming composition.Specific examples of the polymer include vinyl polymers reacted with olefins, polyamides, polyesters, polycarbonates, and polyurethanes, and preferably have a structural unit represented by the following formula (3). [ka] (In formula (3), A1, A2, A3, A4, A5 and A6 each independently represent a hydrogen atom, a methyl group or an ethyl group, and Y1 represents a group represented by formula (4), formula (5), formula (6) or formula (7):
[0025] [ka] (In formulas (4) to (7), R4 and R5 each independently represent a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; R4 and R5 may be bonded to each other to form a ring having 3 to 6 carbon atoms; R6 represents an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms), and Q represents formula (8) or formula (9):
[0026] [ka] (In the formulas (8) and (9), Q1 represents an alkylene group having 1 to 10 carbon atoms, a phenylene group, a naphthylene group, or an anthrylene group, and the phenylene group, naphthylene group, and an anthrylene group may each be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; n4 and n5 each independently represent the number 0 or 1; and Y2 represents the formula (4), the formula (5), or the formula (7)).
[0027] Specific examples of the alkyl group having 1 to 6 carbon atoms include a methyl group, an ethyl group, a propyl group, a butyl group, a hexyl group, and a pentyl group, and a methyl group is preferable. Specific examples of the alkenyl group having 3 to 6 carbon atoms include groups derived from propylene, isobutylene, and amylene, and preferably a propenyl group. Specific examples of the alkoxy group having 1 to 6 carbon atoms include a methoxy group, an ethoxy group, a propoxy group, a butoxy group, a hexoxy group, or a pentoxy group, and preferably a methoxy group. Specific examples of the alkylthio group having 1 to 6 carbon atoms include groups derived from dimethyl sulfide, diethyl sulfide, dimethyl disulfide, and diethyl disulfide, and preferably a group derived from diethyl disulfide. Specific examples of the ring having 3 to 6 carbon atoms include a cyclopropane ring, a cyclobutane ring, a cyclohexane ring, and a thiophene ring. Specific examples of the alkylene group having 1 to 10 carbon atoms include a methylene group, an ethylene group, a propylene group, a butylene group, a hexylene group, a pentylene group, a heptylene group, an octylene group, a nonylene group, and a decylene group, and preferably a methylene group, an ethylene group, a propylene group, or a butylene group.
[0028] The polymer may be used by reacting a compound having a specific structure with the polymer terminal described in Republished Publication No. 2005 / 098542. The polymer contained in the resist underlayer film forming composition of the present application is obtained by reacting a compound represented by formula (10) with a compound represented by formula (11) to obtain a copolymer, and then reacting a compound having a specific structure with the terminal of the copolymer. The polymer contained in the resist underlayer film forming composition of the present application may be a reaction product of a mixture of compounds including a compound represented by the following formula (10), a compound represented by the following formula (11), and a compound represented by the above formula (1-1) or formula (2-1).
[0029] [ka] In formula (10), A1, A2, A3, A4, A5, and A6 each independently represent a hydrogen atom, a methyl group, or an ethyl group, and Y1 represents a group represented by formula (4), formula (5), formula (6), or formula (7):
[0030] [ka] (In the formulas (4) to (7), R4 and R5 each independently represent a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; R4 and R5 may be bonded to each other to form a ring having 3 to 6 carbon atoms; R6 represents an alkyl group having 1 to 6 carbon atoms, an alkenyl group having 3 to 6 carbon atoms, a benzyl group, or a phenyl group, and the phenyl group may be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms), and Q represents a formula (8) or a formula (9):
[0031] [ka] (In formulas (8) and (9), Q1 represents an alkylene group having 1 to 10 carbon atoms, a phenylene group, a naphthylene group, or an anthrylene group, and the phenylene group, naphthylene group, and anthrylene group may each be substituted with at least one group selected from the group consisting of an alkyl group having 1 to 6 carbon atoms, a halogen atom, an alkoxy group having 1 to 6 carbon atoms, a nitro group, a cyano group, a hydroxyl group, and an alkylthio group having 1 to 6 carbon atoms; n4 and n5 each independently represent the number 0 or 1; and Y2 represents formula (4), formula (5), or formula (7)).
[0032] Specific examples of the alkyl group having 1 to 6 carbon atoms include a methyl group, an ethyl group, a propyl group, a butyl group, a hexyl group, and a pentyl group, and a methyl group is preferable. Specific examples of the alkenyl group having 3 to 6 carbon atoms include groups derived from propylene, isobutylene, and amylene, and preferably a propenyl group. Specific examples of the alkoxy group having 1 to 6 carbon atoms include a methoxy group, an ethoxy group, a propoxy group, a butoxy group, a hexoxy group, or a pentoxy group, and preferably a methoxy group. Specific examples of the alkylthio group having 1 to 6 carbon atoms include groups derived from dimethyl sulfide, diethyl sulfide, dimethyl disulfide, and diethyl disulfide, and preferably a group derived from diethyl disulfide. Specific examples of the ring having 3 to 6 carbon atoms include a cyclopropane ring, a cyclobutane ring, a cyclohexane ring, and a thiophene ring. Specific examples of the alkylene group having 1 to 10 carbon atoms include a methylene group, an ethylene group, a propylene group, a butylene group, a hexylene group, a pentylene group, a heptylene group, an octylene group, a nonylene group, and a decylene group, and preferably a methylene group, an ethylene group, a propylene group, or a butylene group.
[0033] The polymer contained in the resist underlayer film forming composition of the present application is obtained by reacting a compound represented by formula (12) with a compound represented by formula (13) to obtain a copolymer, and then reacting a compound having a specific structure with the terminal of the copolymer. The polymer contained in the resist underlayer film forming composition of the present application may be a polymer obtained by a reaction of a mixture of compounds including a compound represented by formula (12), a compound represented by formula (13), and a compound represented by formula (1-1) or formula (2-1) above.
[0034] [ka] (In the formula, A1, A2, A3, A4, A5, A6, Y1 and Q have the same meanings as defined above.)
[0035] The proportion of the polymer in the solid content of the resist underlayer film forming composition of the present invention is 50% by mass or more, preferably 60% by mass or more, for example, 50 to 100% by mass, or 60 to 99% by mass, or 70 to 95% by mass. The proportion of the solid content in the resist underlayer film forming composition of the present invention is not particularly limited as long as each component is uniformly dissolved in the solvent, but is, for example, 0.5 to 50% by mass, or 1 to 30% by mass, or 3 to 20% by mass. Here, the solid content is the total components of the resist underlayer film forming composition excluding the solvent component.
[0036] The molecular weight of the polymer contained in the resist underlayer film forming composition of the present invention is, for example, 1,000 to 200,000, or 1,200 to 100,000, or 1,500 to 30,000, or 2,000 to 20,000, or 2,000 to 4,000, as weight average molecular weight. The weight average molecular weight can be determined, for example, by the gel permeation chromatography (GPC) measurement method described in the Examples.
[0037] <Polymer manufacturing method> As an example of the polymerization method, the polymer contained in the resist underlayer film forming composition of the present application can be synthesized by adding a polymerization catalyst to a mixture of compounds including a compound represented by the following formula (10), a compound represented by the following formula (11), and a compound represented by the above formula (1-1) or formula (2-1), and performing heat polymerization. As an example of the polymerization method, the polymer contained in the resist underlayer film forming composition of the present application can be synthesized by adding a polymerization catalyst to a mixture of compounds including a compound represented by the following formula (12), a compound represented by the formula (13), and a compound represented by the above formula (1-1) or formula (2-1), and performing heat polymerization. The organic solvent used here can be appropriately selected from the preferred examples of organic solvents contained in the resist underlayer film forming composition for lithography of the present invention described later. Examples of the polymerization catalyst include benzyltriethylammonium chloride and ethyltriphenylphosphonium bromide, and the polymerization can be performed by heating to, for example, 50° C. to 160° C., preferably 70° C. to 130° C. The reaction time is, for example, 1 hour to 100 hours, preferably 2 hours to 48 hours.
[0038] <Organic solvent> Specific examples of the organic solvent contained in the resist underlayer film of the present application include ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, methyl cellosolve acetate, ethyl cellosolve acetate, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, propylene glycol, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, propylene glycol propyl ether acetate, toluene, xylene, methyl ethyl ketone, cyclopentanone, cyclohexanone, 2- Examples of the solvent include ethyl hydroxypropionate, ethyl 2-hydroxy-2-methylpropionate, ethyl ethoxyacetate, ethyl hydroxyacetate, methyl 2-hydroxy-3-methylbutanoate, methyl 3-methoxypropionate, ethyl 3-methoxypropionate, ethyl 3-ethoxypropionate, methyl 3-ethoxypropionate, methyl pyruvate, ethyl pyruvate, ethyl acetate, butyl acetate, ethyl lactate, and butyl lactate, and the most preferred is a mixed solvent of propylene glycol monomethyl ether and propylene glycol monomethyl ether acetate.
[0039] <Crosslinking acid catalyst> The resist underlayer film forming composition of the present application may further contain a crosslinking acid catalyst. The crosslinking acid catalyst is a thermal acid generator, and specific examples thereof include sulfonic acid compounds and carboxylic acid compounds such as p-toluenesulfonic acid, trifluoromethanesulfonic acid, pyridinium p-toluenesulfonate, salicylic acid, camphorsulfonic acid, 5-sulfosalicylic acid, 4-chlorobenzenesulfonic acid, 4-hydroxybenzenesulfonic acid, benzenedisulfonic acid, 1-naphthalenesulfonic acid, p-phenolsulfonic acid pyridinium salt, citric acid, benzoic acid, and hydroxybenzoic acid.
[0040] The resist underlayer film forming composition of the present application may contain a crosslinking agent. The crosslinking agent is a nitrogen-containing compound having at least two crosslinking-forming substituents (e.g., methylol group, methoxymethyl group, butoxymethyl group), and specific examples thereof include hexamethoxymethylmelamine, tetramethoxymethylbenzoguanamine, 1,3,4,6-tetrakis(methoxymethyl)glycoluril, 1,3,4,6-tetrakis(butoxymethyl)glycoluril, 1,3,4,6-tetrakis(hydroxymethyl)glycoluril, 1,3-bis(hydroxymethyl)urea, 1,1,3,3-tetrakis(butoxymethyl)urea, and 1,1,3,3-tetrakis(methoxymethyl)urea.
[0041] <Resist Underlayer Film> The resist underlayer film according to the present invention can be produced by applying the above-mentioned resist underlayer film-forming composition onto a semiconductor substrate and baking it. Examples of semiconductor substrates to which the resist underlayer film forming composition of the present invention can be applied include silicon wafers, germanium wafers, and wafers of compound semiconductors such as gallium arsenide, indium phosphide, gallium nitride, indium nitride, and aluminum nitride. When using a semiconductor substrate having an inorganic film formed on its surface, the inorganic film is formed by, for example, ALD (atomic layer deposition), CVD (chemical vapor deposition), reactive sputtering, ion plating, vacuum deposition, or spin-coating (spin-on glass: SOG). Examples of the inorganic film include polysilicon film, silicon oxide film, silicon nitride film, BPSG (Boro-Phospho Silicate Glass) film, titanium nitride film, titanium nitride oxide film, tungsten film, gallium nitride film, and gallium arsenide film. The resist underlayer film forming composition of the present invention is applied onto such a semiconductor substrate by a suitable application method such as a spinner or coater. Then, the composition is baked using a heating means such as a hot plate to form a resist underlayer film. The baking conditions are appropriately selected from a baking temperature of 100°C to 400°C and a baking time of 0.3 minutes to 60 minutes. The baking temperature is preferably 120°C to 350°C, the baking time is 0.5 minutes to 30 minutes, and more preferably, the baking temperature is 150°C to 300°C, and the baking time is 0.8 minutes to 10 minutes. The thickness of the resist underlayer film formed is, for example, 0.001 μm (1 nm) to 10 μm, preferably 0.002 μm (2 nm) to 1 μm, more preferably 0.005 μm (5 nm) to 0.5 μm (500 nm). If the baking temperature is lower than the above range, crosslinking may be insufficient. On the other hand, if the baking temperature is higher than the above range, the resist underlayer film may be decomposed by heat.
[0042] <Method for manufacturing a patterned substrate and a semiconductor device> The manufacturing method of the patterned substrate includes the following steps. Usually, a photoresist layer is formed on a resist underlayer film. The photoresist formed by coating and baking on the resist underlayer film by a method known per se is not particularly limited as long as it is sensitive to the light used for exposure. Either a negative photoresist or a positive photoresist can be used. There are positive photoresists consisting of a novolac resin and a 1,2-naphthoquinone diazide sulfonic acid ester, chemically amplified photoresists consisting of a binder having a group that decomposes with an acid to increase the alkaline dissolution rate and a photoacid generator, chemically amplified photoresists consisting of a low molecular compound that decomposes with an acid to increase the alkaline dissolution rate of the photoresist, an alkali-soluble binder, and a photoacid generator, chemically amplified photoresists consisting of a binder having a group that decomposes with an acid to increase the alkaline dissolution rate, a low molecular compound that decomposes with an acid to increase the alkaline dissolution rate of the photoresist, and a photoacid generator, and resists containing metal elements. Examples of such photoresists include V146G (trade name) manufactured by JSR Corporation, APEX-E (trade name) manufactured by Shipley & Sons, PAR710 (trade name) manufactured by Sumitomo Chemical Co., Ltd., and AR2772 and SEPR430 (trade names) manufactured by Shin-Etsu Chemical Co., Ltd. Further examples of such photoresists include fluorine atom-containing polymer photoresists as described in Proc. SPIE, Vol. 3999, 330-334 (2000), Proc. SPIE, Vol. 3999, 357-364 (2000), and Proc. SPIE, Vol. 3999, 365-374 (2000). Exposure is performed through a mask (reticle) for forming a predetermined pattern, and for example, i-rays, KrF excimer laser, ArF excimer laser, EUV (extreme ultraviolet) or EB (electron beam) is used. An alkaline developer is used for development, and the development temperature is appropriately selected from 5°C to 50°C and the development time is appropriately selected from 10 seconds to 300 seconds. As the alkaline developer, for example, aqueous solutions of alkalis such as inorganic alkalis such as sodium hydroxide, potassium hydroxide, sodium carbonate, sodium silicate, sodium metasilicate, and ammonia water, primary amines such as ethylamine and n-propylamine, secondary amines such as diethylamine and di-n-butylamine, tertiary amines such as triethylamine and methyldiethylamine, alcohol amines such as dimethylethanolamine and triethanolamine, quaternary ammonium salts such as tetramethylammonium hydroxide, tetraethylammonium hydroxide, and choline, cyclic amines such as pyrrole and piperidine, etc. can be used. Furthermore, an appropriate amount of alcohols such as isopropyl alcohol and surfactants such as nonionic surfactants can be added to the aqueous solutions of the above alkalis. Among these, the preferred developer is a quaternary ammonium salt, more preferably tetramethylammonium hydroxide and choline. Furthermore, a surfactant or the like can be added to these developers. Instead of an alkaline developer, a method can be used in which development is carried out with an organic solvent such as butyl acetate, and the part of the photoresist where the alkaline dissolution rate is not improved is developed. Through the above steps, a substrate having the resist patterned thereon can be manufactured. Next, the resist underlayer film is dry etched using the formed resist pattern as a mask. In this case, if the inorganic film is formed on the surface of the semiconductor substrate used, the surface of the inorganic film is exposed, and if the inorganic film is not formed on the surface of the semiconductor substrate used, the surface of the semiconductor substrate is exposed. Thereafter, the substrate is processed by a method known per se (e.g., dry etching method) to manufacture a semiconductor device. EXAMPLES
[0043] The present invention will be described in detail below with reference to synthesis examples and working examples, but the present invention is not limited to the following descriptions in any way.
[0044] The weight average molecular weights shown in Synthesis Examples 1 to 7 below in this specification are the results of measurement by gel permeation chromatography (hereinafter abbreviated as GPC in this specification). A GPC device manufactured by Tosoh Corporation was used for the measurement, and the measurement conditions are as follows. The dispersity shown in Synthesis Examples below in this specification is calculated from the measured weight average molecular weight and number average molecular weight. GPC column: Shodex (registered trademark) Asahipak (registered trademark) (Showa Denko K.K.) Column temperature: 40℃ Solvent: Tetrahydrofuran (THF) Flow rate: 0.6ml / min Standard sample: Polystyrene (manufactured by Tosoh Corporation) Detector: RI detector (Tosoh Corporation, RI-8020)
[0045] <Synthesis Example 1> 7.50 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 4.61 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.34 g of 3-hydroxybenzoic acid (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.60 g of ethyl triphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 62.30 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 2591 and a dispersity of 1.41 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulas (1a) and (2a), and has a structure represented by the following formula (4a) at its terminal. [ka]
[0046] <Synthesis Example 2> 7.50 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 4.61 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.48 g of 3,4-dihydroxybenzoic acid (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.60 g of ethyl triphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 63.01 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 2950 and a dispersity of 1.46 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulae (1a) and (2a), and also has a structure represented by the following formula (3a) at its terminal. [ka]
[0047] <Synthesis Example 3> 5.40 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 3.32 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.30 g of 1-hydroxy-2-naphthoic acid (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.43 g of ethyl triphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 46.74 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 2386 and a dispersity of 2.21 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulae (1a) and (2a), and also has a structure represented by the following formula (5a) at its terminal. [ka]
[0048] <Synthesis Example 4> 9.00 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 5.53 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.96 g of gallic acid (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.71 g of ethyl triphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 47.99 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 3402 and a dispersity of 2.23 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulas (1a) and (2a), and has a structure represented by the following formula (6a) at its terminal. [ka]
[0049] <Synthesis Example 5> 9.00 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 5.53 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.91 g of piperonyl alcohol (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.71 g of ethyl triphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 47.80 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 3186 and a dispersity of 2.57 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulas (1a) and (2a), and has a structure represented by the following formula (7a) at its terminal. [ka]
[0050] <Comparative Synthesis Example 1> 9.00 g of diglycidyl dimethylhydantoin (manufactured by Shikoku Kasei Co., Ltd.), 5.53 g of monoallyl diglycidyl isocyanuric acid (manufactured by Shikoku Kasei Co., Ltd.), 1.91 g of 4-(Methylsulfonyl)benzoic Acid (manufactured by Tokyo Kasei Kogyo Co., Ltd.), and 0.71 g of ethyltriphenylphosphonium bromide (manufactured by ACROSS Co., Ltd.) were added to 47.80 g of propylene glycol monomethyl ether and dissolved. After replacing the reaction vessel with nitrogen, the reaction was carried out at 135°C for 4 hours to obtain a polymer solution. The polymer solution did not become cloudy even when cooled to room temperature, and the solubility in propylene glycol monomethyl ether was good. When GPC analysis was performed, the polymer in the obtained solution had a weight average molecular weight of 2600 and a dispersity of 2.13 in terms of standard polystyrene. The polymer obtained in this synthesis example has structural units represented by the following formulae (1a) and (2a), and also has a structure represented by the following formula (8a) at its terminal. [ka]
[0051] <Example 1> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Synthesis Example 1 above was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd.) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter having a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0052] <Example 2> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Synthesis Example 2 above was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd., product name: POWDERLINK [registered trademark] 1174) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter with a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0053] <Example 3> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Synthesis Example 3 above was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd.) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter having a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0054] <Example 4> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Synthesis Example 4 above was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd.) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter with a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0055] <Example 5> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Synthesis Example 5 above was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd.) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter with a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0056] <Comparative Example 1> 0.21 g of the polymer solution containing 0.031 g of the polymer obtained in Comparative Synthesis Example 1 was mixed with 0.0077 g of tetramethoxymethylglycoluril (manufactured by Nippon Cytec Industries Co., Ltd.) and 0.0012 g of p-phenolsulfonic acid pyridinium salt (manufactured by Tokyo Chemical Industry Co., Ltd.), and 47.81 g of propylene glycol monomethyl ether and 2.00 g of propylene glycol monomethyl ether acetate were added and dissolved. The mixture was then filtered using a polyethylene microfilter with a pore size of 0.05 μm to obtain a resist underlayer film forming composition for lithography.
[0057] [Photoresist solvent elution test] The resist underlayer film forming compositions of Examples 1 to 5 and Comparative Example 1 were each applied onto a silicon wafer, which was a semiconductor substrate, by a spinner. The silicon wafer was placed on a hot plate and baked at 215° C. for 1 minute to form a resist underlayer film (film thickness 5 nm). These resist underlayer films were immersed in ethyl lactate and propylene glycol monomethyl ether, which are solvents used in photoresists, and it was confirmed that they were insoluble in these solvents.
[0058] [Formation of resist pattern by KrF exposure] DUV-30J (anti-reflective film manufactured by Nissan Chemical Industries, Ltd.) was applied as an anti-reflective film onto a silicon wafer using a spinner. The silicon wafer was baked on a hot plate at 205° C. for 60 seconds to obtain a film having a thickness of 18 nm. The resist underlayer film forming compositions of Examples 1 to 5 and Comparative Example 1 were applied onto the film using a spinner. The silicon wafer was baked on a hot plate at 215° C. for 60 seconds to obtain a resist underlayer film having a thickness of 5 nm. A positive resist solution for KrF excimer laser was spin-coated onto the resist underlayer film, and heated at 110° C. for 60 seconds to form a KrF resist film. The resist film was exposed under specified conditions using a KrF excimer laser exposure device (manufactured by Nikon Corporation, NSR S205C). After exposure, the film was baked at 110°C for 60 seconds (PEB), cooled to room temperature on a cooling plate, developed with butyl acetate, and rinsed with butyl acetate to form a resist pattern with 170 nm lines and 340 nm pitch. A scanning electron microscope (CG4100, manufactured by Hitachi High-Technologies Corporation) was used to measure the length of the resist pattern. In forming the resist pattern, the exposure dose at which 170 nm lines / 340 nm pitch (line and space (L / S=1 / 1) were formed was defined as the optimum exposure dose. Evaluation was performed based on whether 170 nm lines and spaces (L / S) could be formed, the size of the line width roughness (LWR) of the line pattern formed by observation from above, and the minimum pre-collapse dimension, which is the smallest line width at which the resist pattern does not collapse. Table 1 shows the evaluation results. The case where lines and spaces were formed was rated as "good." Regarding LWR, the magnitude of variation in the line width of the formed line pattern was shown in nm. Since a smaller LWR value is more preferable, Examples 1 to 5 showed better LWR than Comparative Example 1.
[0059] [Table 1]
[0060] [EUV Exposure Test] A resist underlayer film was formed on a silicon wafer by spin-coating the resist underlayer film forming composition of Example 1, Example 2, and Comparative Example 1 of the present invention, and heating at 215°C for 1 minute. An EUV resist solution was spin-coated on the resist underlayer film, heated, and exposed under the condition of NA = 0.33 Dipole using an EUV exposure device (manufactured by ASML, NXE3300B). After exposure, PEB (post-exposure baking) was performed, cooled to room temperature on a cooling plate, developed and rinsed, and a resist pattern was formed on the silicon wafer. The evaluation shows whether or not a 16 nm line and space (L / S) can be formed. In addition, the exposure amount at which a 16 nm line / 32 nm pitch (line and space (L / S = 1 / 1) was formed was defined as the optimal exposure amount, and the exposure amount (EOP) at that time is shown. Examples 1 and 2 showed improved sensitivity compared to Comparative Example 1.
[0061] [Table 2] [Industrial Applicability]
[0062] The resist underlayer film forming composition according to the present invention can provide a composition for forming a resist underlayer film capable of forming a desired resist pattern, and a method for forming a resist pattern using the resist underlayer film forming composition.
Claims
1. A resist underlayer film forming composition comprising a polymer having a structural unit represented by the following formula (3) and having a structure represented by the following formula (2) at an end of the polymer chain, a crosslinking acid catalyst, and an organic solvent. 【Chemistry 1】 (In the above formula (2), X is a divalent organic group, A is an aryl group having 6 to 40 carbon atoms, and R 2 and R 3 are each independently a hydrogen atom, a halogen atom, an optionally substituted alkyl group having 1 to 10 carbon atoms, or an optionally substituted aryl group having 6 to 40 carbon atoms, and n3 is an integer of 1 to 12. 【Chemistry 2】 In formula (3), A 1 , A 2 , A 3 , A 4 , A 5 and A 6 represent a hydrogen atom, and Y 1 represents a group represented by formula (6): 【Chemistry 3】 (In formula (6), R 6 represents an alkenyl group having 3 to 6 carbon atoms), and Q represents a group represented by formula (9): 【Chemistry 4】 (In formula (9), Y 2 is a group represented by formula (4): 【Chemistry 5】 (In formula (4), R 4 and R 5 each independently represent a hydrogen atom, a methyl group, or an ethyl group.)
2. The resist underlayer film forming composition according to claim 1 , wherein in the formula (2), X is an ester bond or an ether bond.
3. 2. The resist underlayer film forming composition according to claim 1, wherein in said formula (2), A is a group derived from benzene, naphthalene or anthracene.
4. In the formula (2), R 2 and R 3 The resist underlayer film forming composition according to claim 1 , wherein is a hydrogen atom.
5. 2. The resist underlayer film forming composition according to claim 1, wherein in formula (2), n3 is an integer of 1 to 6.
6. The resist underlayer film forming composition according to claim 1, wherein the polymer having a structural unit represented by the formula (3) is a polymer having a compound represented by the formula (10) and a compound represented by the formula (11) as comonomers. 【Chemistry 5】 (In formulas (10) and (11), A 1 , A 2 , A 3 , A 4 , A 5 , A 6 , Y 1 and Q have the same meanings as defined in claim 1 ).
7. The resist underlayer film forming composition according to claim 1, wherein the polymer having a structural unit represented by the formula (3) is a polymer having a compound represented by the formula (12) and a compound represented by the formula (13) as comonomers. 【Chemistry 6】 (wherein A 1 , A 2 , A 3 , A 4 , A 5 , A 6 , Y 1 and Q have the same meanings as defined in claim 1 ).
8. A resist underlayer film forming composition according to claim 1, further comprising a crosslinking agent.
9. A resist underlayer film, which is a fired product of a coating film comprising the resist underlayer film forming composition according to any one of claims 1 to 8.
10. A method for manufacturing a patterned substrate, comprising the steps of: applying a resist underlayer film forming composition described in any one of claims 1 to 8 onto a semiconductor substrate and baking the composition to form a resist underlayer film; applying a resist onto the resist underlayer film and baking the composition to form a resist film; exposing the resist underlayer film and the semiconductor substrate coated with the resist; and developing and patterning the resist film after exposure.
11. A process for forming a resist underlayer film on a semiconductor substrate, the resist underlayer film being composed of the resist underlayer film forming composition according to any one of claims 1 to 8; forming a resist film on the resist underlayer film; forming a resist pattern by irradiating the resist film with light or an electron beam and then developing it; forming a patterned resist underlayer film by etching the resist underlayer film through the formed resist pattern; processing a semiconductor substrate using the patterned resist underlayer film; A method for manufacturing a semiconductor device, comprising:
Citation Information
Patent Citations
Antireflection film for semiconductor containing condensation type polymer
WO2005098542A1
Resist underlayer film forming composition containing polymer which contains nitrogen-containing ring compound
WO2015019961A1
Resist underlayer film-forming composition and method for forming resist pattern using same
WO2015046149A1
Resist underlayer film forming composition and method for forming resist pattern in which same is used
WO2015163195A1