Semiconductor device and semiconductor package
The semiconductor device addresses on-resistance by locally thinning the drain region through recess formation, maintaining substrate integrity for easy handling and reducing manufacturing challenges.
Patent Information
- Application Number
- JP2021008604
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-01-22
- Publication Date
- 2024-09-26
- Estimated Expiration
- 2041-01-22
AI Technical Summary
Existing semiconductor devices face challenges in reducing on-resistance while maintaining ease of handling during the manufacturing process, as thinning the drain region leads to poor handling due to reduced substrate thickness.
A semiconductor device with a recessed portion on the second surface of the substrate reduces the thickness of the drain region locally, maintaining overall substrate thickness in non-recessed areas for handling, and incorporates a gate trench and insulating film to reduce on-resistance.
The solution effectively reduces on-resistance by up to 20% while ensuring ease of handling and preventing cracking during manufacturing processes.
Smart Images

Figure 0007556798000005 
Figure 0007556798000030 
Figure 0007556798000022
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a semiconductor device and a semiconductor package. [Background technology]
[0002] The semiconductor device described in U.S. Pat. No. 5,998,833 (Patent Document 1) has a semiconductor substrate, a gate insulating film, and a gate. The semiconductor substrate has a first surface and a second surface. The second surface is the surface opposite to the first surface. The semiconductor substrate has a source region located in the first surface, a drain region located in the second surface, a drift region in contact with the first surface side of the drain region, and a base region including a channel region sandwiched between the source region and the drift region.
[0003] A gate trench is formed in the first surface. A bottom wall of the gate trench is located within the drift region. A channel region is exposed from a side wall of the gate trench. A gate insulating film is formed on the side wall and bottom wall of the gate trench. A gate is disposed within the gate trench so as to face the channel region with the gate insulating film interposed therebetween. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] U.S. Pat. No. 5,998,833 Summary of the Invention [Problem to be solved by the invention]
[0005] In the semiconductor device described in Patent Document 1, a possible measure to reduce the on-resistance is to thin the drain region by polishing the semiconductor substrate from the second surface side. However, in this case, the entire semiconductor substrate becomes thin, which impairs the handleability in the manufacturing process.
[0006] The present disclosure provides a semiconductor device capable of reducing the on-resistance while maintaining ease of handling during the manufacturing process. [Means for solving the problem]
[0007] A semiconductor device according to one embodiment includes a semiconductor substrate having a first surface and a second surface opposite to the first surface, a gate insulating film formed on the first surface, a gate formed on the first surface via the gate insulating film, a source region formed on the first surface side of the semiconductor substrate, a body region formed in contact with the source region and including a channel region, a drain region formed on the second surface side of the semiconductor substrate, and a drift region formed in contact with the second surface side of the body region and the first surface side of the drain region. The gate faces the channel region with the gate insulating film interposed therebetween. At least one recess recessed toward the first surface is formed in the second surface of the semiconductor substrate. Effect of the Invention
[0008] According to the semiconductor device of the embodiment, the on-resistance can be reduced while maintaining ease of handling during the manufacturing process. [Brief description of the drawings]
[0009] [Figure 1] FIG. 2 is a plan view of the semiconductor device DEV1. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3 is an enlarged view of region III in FIG. 2. [Figure 4] FIG. 2 is a cross-sectional view taken along line IV-IV in FIG. [Diagram 5] 1A to 1C are process diagrams showing a manufacturing method of the semiconductor device DEV1. [Figure 6] 1 is a cross-sectional view of the semiconductor device DEV1 in a preparation step S1. [Figure 7] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in the epitaxial growth step S2. [Figure 8]11 is a cross-sectional view of the semiconductor device DEV1 in a first ion implantation step S3. FIG. [Figure 9] FIG. 11 is a cross-sectional view of the semiconductor device DEV2 in a second ion implantation step S4. [Figure 10] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in a trench forming step S5. [Figure 11] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in a gate insulating film forming step S6. [Figure 12] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in a gate formation step S7. [Figure 13] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in an interlayer insulating film forming step S8. [Figure 14] 11 is a cross-sectional view of the semiconductor device DEV1 in a substrate polishing step S10. FIG. [Figure 15] FIG. 11 is a cross-sectional view of the semiconductor device DEV1 in a recess forming step S11. [Figure 16] 11 is a cross-sectional view of the semiconductor device DEV1 in a first electrode formation step S12. FIG. [Figure 17] 11 is a cross-sectional view of the semiconductor device DEV1 in a second electrode formation step S13. FIG. [Figure 18] 11 is a cross-sectional view of a semiconductor device DEV1 according to a first modified example. [Figure 19] FIG. 11 is a cross-sectional view of a semiconductor device DEV1 according to a second modified example. [Figure 20] FIG. 11 is a cross-sectional view of a semiconductor device DEV1 according to a third modified example. [Figure 21] FIG. 2 is a bottom view of the semiconductor device DEV2. [Figure 22] 22 is a cross-sectional view taken along line XXII-XXII in FIG. 21. [Figure 23] FIG. 13 is a bottom view of the semiconductor device DEV2 according to the first modification. [Figure 24] FIG. 11 is a bottom view of the semiconductor device DEV2 according to Modification 2. [Diagram 25] FIG. 13 is a bottom view of the semiconductor device DEV2 according to Modification 3. [Figure 26] FIG. 13 is a bottom view of the semiconductor device DEV3. [Figure 27] FIG. 27 is a cross-sectional view taken along line XXVII-XXVII in FIG. 26. [Figure 28] FIG. 13 is a cross-sectional view of the semiconductor device DEV4. [Figure 29] 1 is a cross-sectional view of a semiconductor package PKG1. [Diagram 30] FIG. 2 is a cross-sectional view of a semiconductor package PKG2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The details of the embodiment will be described with reference to the drawings. In the following drawings, the same or corresponding parts are given the same reference numerals, and the overlapping description will be repeated.
[0011] (First embodiment) The semiconductor device according to the first embodiment (hereinafter referred to as "semiconductor device DEV1") will be described below.
[0012] <Configuration of semiconductor device DEV1> Fig. 1 is a plan view of the semiconductor device DEV1. Fig. 2 is a cross-sectional view taken along II-II in Fig. 1. Fig. 3 is an enlarged view of region III in Fig. 2. Fig. 4 is a cross-sectional view taken along IV-IV in Fig. 1. As shown in Figs. 1 to 4, the semiconductor device DEV1 has a semiconductor substrate SUB, a gate insulating film GI, a gate GA, an interlayer insulating film ILD, a source electrode EL1, a gate electrode EL2, and a drain electrode EL3.
[0013] The semiconductor substrate SUB has a first surface FS and a second surface SS. The first surface FS and the second surface SS are end surfaces in the thickness direction of the semiconductor substrate SUB. The second surface SS is the opposite surface to the first surface FS.
[0014] The semiconductor substrate SUB has an outer periphery region R1 and a cell region R2 in a plan view (when viewed from a direction perpendicular to the first surface FS and the second surface SS). The outer periphery region R1 is a portion located on the periphery of the semiconductor substrate SUB in a plan view. The cell region R2 is located inside the outer periphery region R1 in a plan view. The cell region R2 is a portion in which a cell structure of a MOSFET (Metal Oxide Field Effect Transistor) is formed.
[0015] In the cell region R2, the semiconductor substrate SUB has a source region SR, a drain region DRA, a drift region DRI, and a body region BR. The source region SR, the drain region DRA, and the drift region DRI have a first conductivity type. The body region BR has a second conductivity type. The second conductivity type is the opposite conductivity type to the first conductivity type. For example, when the first conductivity type is n-type, the second conductivity type is p-type. The impurity concentration in the source region SR and the drain region DRA is higher than the impurity concentration in the drift region DRI.
[0016] The source region SR is located on the first surface FS. The drain region DRA is located on the second surface SS. The drift region DRI is formed on the drain region DRA. That is, the drift region DRI is in contact with the first surface FS side of the drain region DRA. The body region BR is sandwiched between the source region SR and the drift region DRI.
[0017] In the cell region R2, a gate trench GTR is formed in the first surface FS. The gate trench GTR extends toward the second surface SS. The bottom wall of the gate trench GTR is located in the drift region DRI. The source region SR, the body region BR, and the drift region DRI are exposed from the sidewall of the gate trench GTR. The portion of the body region BR exposed from the gate trench GTR is defined as a channel region CH.
[0018] In the cell region R2, a recess RP is formed in the second surface SS. In the recess RP, the second surface SS is recessed toward the first surface FS. As shown in Fig. 3, a part of the recess RP may be formed in the second surface SS located outside the cell region R2. However, the recess RP is not formed in the second surface SS located in the outer peripheral region R1.
[0019] The semiconductor substrate SUB is made of, for example, single crystal silicon. The first surface FS and the second surface SS are made of single crystal silicon. <100> The sidewall of the recess RP is preferably perpendicular to the direction of the first surface SS. The sidewall of the recess RP forms an angle θ with the second surface SS. The angle θ is preferably 50° or more and 60° or less. <111> It is preferable that the direction of the crystal grains is perpendicular to the direction of the crystal grains. <100> Direction and <111> The angle between the direction is approximately 55°, and more specifically, 54.7°.
[0020] The thickness of the drift region DRI is defined as thickness T1. The thickness of the drain region DRA in the portion where the recess RP is formed is defined as thickness T2. The thickness of the drain region DRA in the portion where the recess RP is not formed (i.e., the peripheral region R1) is defined as thickness T3. Thickness T2 is smaller than thickness T3. That is, the semiconductor substrate SUB has a sufficient thickness in the peripheral region R1.
[0021] The gate insulating film GI is disposed on the sidewall and bottom wall of the gate trench GTR. The gate insulating film GI is formed of, for example, silicon oxide. The gate GA is disposed in the gate trench GTR. The gate insulating film GI is interposed between the gate GA and the sidewall and bottom wall of the gate trench GTR. That is, the gate GA faces the channel region CH while being insulated by the gate insulating film GI. The gate GA is formed of, for example, polysilicon.
[0022] The interlayer insulating film ILD is disposed on the first surface FS. The interlayer insulating film ILD is made of, for example, silicon oxide.
[0023] The source electrode EL1 and the gate electrode EL2 are disposed on the interlayer insulating film ILD. The source region SR and the gate GA are electrically connected to the source electrode EL1 and the gate electrode EL2, respectively, by contact plugs (not shown) formed in the interlayer insulating film ILD. The source electrode EL1 is disposed so as to overlap with the cell region R2. The gate electrode EL2 is disposed so as not to overlap with the cell region R2. The drain electrode EL3 is formed on the second surface SS. The source electrode EL1, the gate electrode EL2, and the drain electrode EL3 are formed of, for example, aluminum.
[0024] <Manufacturing Method of Semiconductor Device DEV1> 5 is a process diagram showing a method for manufacturing the semiconductor device DEV1. As shown in FIG. 5, the method for manufacturing the semiconductor device DEV1 includes a preparation step S1, an epitaxial growth step S2, a first ion implantation step S3, a second ion implantation step S4, a trench formation step S5, a gate insulating film formation step S6, a gate formation step S7, an interlayer insulating film formation step S8, and a contact plug formation step S9. The method for manufacturing the semiconductor device DEV1 further includes a substrate polishing step S10, a recess formation step S11, a first electrode formation step S12, a second electrode formation step S13, and a singulation step S14. The first ion implantation step S3 and the second ion implantation step S4 may be performed after the trench formation step S5, the gate insulating film formation step S6, and the gate formation step S7.
[0025] In the preparation step S1, a semiconductor substrate SUB is prepared. Fig. 6 is a cross-sectional view of the semiconductor device DEV1 in the preparation step S1. As shown in Fig. 6, the semiconductor substrate SUB prepared in the preparation step S1 has only a drain region DRA.
[0026] In the epitaxial growth step S2, an epitaxial layer EPI is formed. Fig. 7 is a cross-sectional view of the semiconductor device DEV1 in the epitaxial growth step S2. As shown in Fig. 7, the epitaxial layer EPI is formed on the drain region DRA. The epitaxial layer EPI has a first conductivity type. The epitaxial layer EPI is formed, for example, by a CVD (Chemical Vapor Deposition) method.
[0027] Fig. 8 is a cross-sectional view of the semiconductor device DEV1 in the first ion implantation step S3. As shown in Fig. 8, in the first ion implantation step S3, a body region BR is formed. Fig. 9 is a cross-sectional view of the semiconductor device DEV2 in the second ion implantation step S4. As shown in Fig. 9, in the second ion implantation step S4, a source region SR is formed. The body region BR and the source region SR are formed by ion implantation. A portion of the epitaxial layer EPI in which the body region BR and the source region SR are not formed becomes a drift region DRI.
[0028] Fig. 10 is a cross-sectional view of the semiconductor device DEV1 in a trench forming step S5. As shown in Fig. 10, in the trench forming step S5, a gate trench GTR is formed. The gate trench GTR is formed by dry etching such as RIE (Reactive Ion Etching). Fig. 11 is a cross-sectional view of the semiconductor device DEV1 in a gate insulating film forming step S6. As shown in Fig. 11, in the gate insulating film forming step S6, a gate insulating film GI is formed. The gate insulating film GI is formed by thermal oxidation, for example.
[0029] 12 is a cross-sectional view of the semiconductor device DEV1 in the gate formation step S7. As shown in FIG. 12, in the gate formation step S7, the gate GA is formed. In forming the gate GA, first, a material constituting the gate GA is embedded in the gate trench GTR. Second, the material constituting the gate GA protruding from the gate trench GTR is removed by etch-back, CMP (Chemical Mechanical Polishing), or the like.
[0030] Fig. 13 is a cross-sectional view of the semiconductor device DEV1 in the interlayer insulating film forming step S8. As shown in Fig. 13, in the interlayer insulating film forming step S8, the interlayer insulating film ILD is formed. The interlayer insulating film ILD is formed by, for example, a CVD method.
[0031] In the contact plug formation step S9, a contact plug is formed. In the formation of the contact plug, first, a contact hole is formed in the interlayer insulating film ILD. The contact hole penetrates the interlayer insulating film ILD in the thickness direction. The contact hole is formed by dry etching such as RIE. Second, a material constituting the contact plug is embedded in the contact hole by a CVD method. Third, the material constituting the contact plug protruding from the contact hole is removed by etch-back, CMP, or the like.
[0032] 14 is a cross-sectional view of the semiconductor device DEV1 in the substrate polishing step S10. As shown in FIG. 14, in the substrate polishing step S10, the second surface SS side of the semiconductor substrate SUB is polished. As a result, the thickness of the drain region DRA becomes a thickness T3.
[0033] Fig. 15 is a cross-sectional view of the semiconductor device DEV1 in the recess forming step S11. As shown in Fig. 15, in the recess forming step S11, a recess RP is formed. In forming the recess RP, first, a mask is formed on the second surface SS. The mask is formed, for example, by forming a silicon oxide film on the second surface SS by CVD or the like and patterning the formed silicon oxide film.
[0034] Secondly, the semiconductor substrate SUB is etched through the openings in the mask to form recesses RP. This etching is preferably performed by wet etching using tetramethylammonium hydroxide (TMAH). When wet etching using TMAH is performed on single crystal silicon, the etching speed varies significantly depending on the crystal orientation. Therefore, when the second surface SS is a single crystal silicon, <100> When the direction is perpendicular to the direction of the recess RP, the side wall of the recess RP is <111> The surface perpendicular to the direction is exposed, and the angle θ is 50° or more and 60° or less.
[0035] As a result of performing the recess forming step S11, the drain region DRA becomes thinner in the portion where the recess RP is formed, and the thickness of the drain region DRA becomes thickness T2 from thickness T3. That is, as a result of performing the recess forming step S11, the thickness of the drain region DRA becomes thinner in the position where the recess RP is formed than in the position where the recess RP is not formed (i.e., the outer circumferential region R1).
[0036] Fig. 16 is a cross-sectional view of the semiconductor device DEV1 in the first electrode forming step S12. As shown in Fig. 16, in the first electrode forming step S12, a source electrode EL1 and a gate electrode EL2 are formed.
[0037] In forming the source electrode EL1 and the gate electrode EL2, first, a material constituting the source electrode EL1 (gate electrode EL2) is deposited on the interlayer insulating film ILD by sputtering, etc. Second, the deposited material constituting the source electrode EL1 (gate electrode EL2) is patterned to form the source electrode EL1 and the gate electrode EL2.
[0038] Fig. 17 is a cross-sectional view of the semiconductor device DEV1 in the second electrode forming step S13. As shown in Fig. 17, in the second electrode forming step S13, a drain electrode EL3 is formed. The drain electrode EL3 is formed by, for example, a sputtering method, a plating method, or the like. In the singulation step S14, the semiconductor device DEV1 is singulated. This singulation is performed using, for example, a dicing blade. In this manner, the semiconductor device DEV1 having the structure shown in Figs. 1 to 4 is manufactured.
[0039] <Effects of semiconductor device DEV1> In the semiconductor device DEV1, the thickness of the drain region DRA is thin in the portion where the recess RP is formed, and therefore the on-resistance is reduced. For example, if the thickness of the drift region DRI is 5 μm, the resistivity of the drift region DRI is 0.12 Ω·cm, and the resistivity of the drain region DRA is 0.8 mΩ·cm, and the thickness of the drain region DRA is thinned from 150 μm to 5 μm by forming the recess RP, the on-resistance can be reduced by about 20 percent (when the thickness of the drain region DRA is 150 μm, the on-resistance is 0.12 Ω·cm×5 μm+0.8 mΩ·cm×150 μm≈7.2 mΩ·mm 2 When the thickness of the drain region DRA is reduced to 5 μm, the on-resistance is 0.12 Ω cm × 5 μm + 0.8 mΩ × 5 μm ≒ 6.0 mΩ mm 2 (It becomes.)
[0040] On the other hand, in the portion where the recess RP is not formed, that is, in the outer circumferential region R1, the thickness of the drain region DRA is maintained, and therefore handling properties in the manufacturing process are maintained.
[0041] That is, if the thickness of the recess RP is also thin in the outer peripheral region R1, it is difficult to cut the semiconductor substrate SUB using a dicing blade in the singulation step S14, but in the semiconductor device DEV1, the thickness of the drain region DRA is maintained in the outer peripheral region R1, so that the semiconductor substrate SUB can be cut using a dicing blade. In this way, with the semiconductor device DEV1, it is possible to maintain the handleability in the manufacturing process while reducing the on-resistance.
[0042] The second surface SS is made of single crystal silicon. <100> When the angle θ is perpendicular to the direction, the angle θ can be set to 50° or more and 60° or less by wet etching the recess RP using TMAH. That is, in this case, a tapered recess RP can be formed. As a result, when the drain electrode EL3 is formed, it is possible to suppress the drain electrode EL3 from becoming locally thin (the drain electrode EL3 from being discontinuous).
[0043] <Variation 1> Fig. 18 is a cross-sectional view of a semiconductor device DEV1 according to Modification 1. As shown in Fig. 18, a gate trench GTR may not be formed in the semiconductor substrate SUB. That is, the semiconductor device DEV1 may be a planar gate MOSFET instead of a trench gate MOSFET. Note that in Modification 1, a gate insulating film GI is disposed on the channel region CH exposed to the first surface FS, and a gate GA is disposed on the gate insulating film GI.
[0044] Fig. 19 is a cross-sectional view of a semiconductor device DEV1 according to a second modification. As shown in Fig. 19, the semiconductor substrate SUB may have a pillar region PR. The pillar region PR extends from the body region BR toward the second surface SS. The conductivity type of the pillar region PR is the second conductivity type (p-type). That is, the semiconductor device DEV1 may be a MOSFET having a superjunction structure. In this case, the impurity concentration of the drift region DRI is set relatively high, and therefore, the effect of reducing the on-resistance due to the drain region DRA being thin at the position where the recess RP is formed becomes relatively large.
[0045] The first surface FS and the second surface SS are made of single crystal silicon. <110> 20 is a cross-sectional view of a semiconductor device DEV1 according to Modification 3. In this case, as shown in FIG. 20, the angle θ becomes approximately 90° by performing wet etching of the recess RP using TMAH.
[0046] Second embodiment A semiconductor device according to a second embodiment (hereinafter referred to as "semiconductor device DEV2") will be described below. Here, differences from the semiconductor device DEV1 will be mainly described, and overlapping descriptions will not be repeated.
[0047] <Configuration of semiconductor device DEV2> Fig. 21 is a bottom view of the semiconductor device DEV2. Fig. 22 is a cross-sectional view taken along line XXII-XXII of Fig. 21. As shown in Figs. 21 and 22, the semiconductor device DEV2 has a semiconductor substrate SUB, a gate insulating film GI, a gate GA, an interlayer insulating film ILD, a source electrode EL1, a gate electrode EL2, and a drain electrode EL3. In the cell region R2, a recess RP is formed in the second surface SS. In these respects, the configuration of the semiconductor device DEV2 is common to the configuration of the semiconductor device DEV1.
[0048] In the semiconductor device DEV2, the number of recesses RP is multiple. In the semiconductor device DEV2, the multiple recesses RP are arranged in a lattice shape in a plan view. This lattice shape is, for example, a square lattice arrangement. In these respects, the configuration of the semiconductor device DEV2 differs from the configuration of the semiconductor device DEV1. Note that the recesses RP have, for example, a rectangular shape in a plan view.
[0049] The pitch between two adjacent recesses RP is defined as pitch P. The minimum distance between the side walls of the recesses RP facing each other is defined as width W. The pitch P is preferably larger than the width W. The value obtained by dividing the width W by the pitch P is preferably 0.1 or more and 0.4 or less. The recesses RP are preferably formed at a position that does not overlap with the gate electrode EL2 in a planar view. Note that the gate electrode EL2 is located at a position that does not overlap with the cell region in a planar view.
[0050] <Effects of semiconductor device DEV2> Wire bonding may be performed on the source electrode EL1 and the gate electrode EL2. Since one relatively large recess RP is formed in the semiconductor device DEV1, a load that bends the semiconductor substrate SUB may be applied during the wire bonding, which may result in cracking of the semiconductor substrate SUB.
[0051] On the other hand, in the semiconductor device DEV2, a plurality of relatively small recesses RP are formed in a lattice pattern, and the second surface SS between the recesses RP can support the load applied during wire bonding. Therefore, the semiconductor device DEV2 can prevent the semiconductor substrate SUB from cracking due to the load applied during wire bonding.
[0052] When the value obtained by dividing the width W by the pitch P is 0.1 or more and 0.4 or less, the on-resistance caused by the formation of the recesses RP can be reduced, while ensuring strength against the load during wire bonding.
[0053] When the recess RP is disposed at a position where it does not overlap with the gate electrode EL2 in a plan view, it is possible to suppress the semiconductor substrate SUB from cracking due to the load applied when wire bonding is performed on the gate electrode EL2. Since the gate electrode EL2 is disposed at a position where it does not overlap with the cell region R2 in a plan view, the on-resistance hardly increases even if the recess RP is not formed at a position where it overlaps with the gate electrode EL2 in a plan view.
[0054] <Variation 1> Fig. 23 is a bottom view of the semiconductor device DEV2 according to Modification 1. As shown in Fig. 23, the recesses RP do not have to be arranged in a square lattice pattern. The recesses RP may be arranged in a staggered pattern, for example.
[0055] Fig. 24 is a bottom view of the semiconductor device DEV2 according to Modification 2. Fig. 25 is a bottom view of the semiconductor device DEV2 according to Modification 3. As shown in Fig. 24 and Fig. 25, the planar shape of the recess RP does not have to be rectangular. As shown in Fig. 24, the planar shape of the recess RP may be a polygonal shape other than a rectangular shape, and as shown in Fig. 25, the planar shape of the recess RP may be a circular (or elliptical) shape.
[0056] Third embodiment A semiconductor device according to a third embodiment (hereinafter referred to as "semiconductor device DEV3") will be described below. Here, differences from the semiconductor device DEV1 will be mainly described, and overlapping descriptions will not be repeated.
[0057] <Configuration of semiconductor device DEV3> Fig. 26 is a bottom view of the semiconductor device DEV3. Fig. 27 is a cross-sectional view taken along line XXVII-XXVII of Fig. 26. As shown in Fig. 26 and Fig. 27, the semiconductor device DEV3 has a semiconductor substrate SUB, a gate insulating film GI, a gate GA, an interlayer insulating film ILD, a source electrode EL1, a gate electrode EL2, and a drain electrode EL3. In these respects, the configuration of the semiconductor device DEV3 is common to the configuration of the semiconductor device DEV1.
[0058] In the semiconductor device DEV3, a plurality of trenches TR are formed as the recesses RP. In this respect, the configuration of the semiconductor device DEV3 is different from the configuration of the semiconductor device DEV1.
[0059] The trenches TR extend along a first direction DR1 in plan view. The trenches TR are spaced apart from one another in a second direction DR2. The second direction DR2 is a direction perpendicular to the first direction DR1. The trenches TR are preferably formed at positions not overlapping the gate electrode EL2 in plan view.
[0060] The extension direction of the gate trench GTR is preferably along the first direction DR1 in a plan view. That is, the extension direction of the gate trench GTR is preferably parallel to the extension direction of the trench TR. However, the extension direction of the gate trench GTR may be along the second direction DR2.
[0061] <Effects of semiconductor device DEV3> In the semiconductor device DEV3, since a plurality of grooves TR are formed, the second surface SS between the grooves TR can support the load applied during wire bonding. Therefore, the semiconductor device DEV3 can prevent the semiconductor substrate SUB from cracking due to the load applied during wire bonding. When the extension direction of the grooves TR is aligned with the extension direction of the gate trench GTR, the on-resistance can be further reduced.
[0062] (Fourth embodiment) A semiconductor device according to the fourth embodiment (hereinafter referred to as "semiconductor device DEV4") will be described below. Here, differences from the semiconductor device DEV1 will be mainly described, and overlapping descriptions will not be repeated.
[0063] <Configuration of semiconductor device DEV4> Fig. 28 is a cross-sectional view of the semiconductor device DEV4. As shown in Fig. 28, the semiconductor device DEV3 has a semiconductor substrate SUB, a gate insulating film GI, a gate GA, an interlayer insulating film ILD, a source electrode EL1, a gate electrode EL2, and a drain electrode EL3. In the cell region R2, a recess RP is formed in the second surface SS. In these respects, the configuration of the semiconductor device DEV3 is common to the configuration of the semiconductor device DEV1.
[0064] The semiconductor device DEV4 further includes a conductor CB. In this respect, the configuration of the semiconductor device DEV4 differs from that of the semiconductor device DEV1. The conductor CB is embedded in the recess RP. The conductor CB is formed of, for example, a sintered body of silver particles. However, the conductor CB is not limited to this.
[0065] <Effects of semiconductor device DEV4> In the semiconductor device DEV3, since the conductor CB is embedded in the recess RP, the load applied during wire bonding is also supported by the conductor CB. Therefore, according to the semiconductor device DEV4, it is possible to prevent the semiconductor substrate SUB from cracking due to the load applied during wire bonding.
[0066] Fifth embodiment A semiconductor package according to the fifth embodiment (hereinafter referred to as "semiconductor package PKG1") will be described below.
[0067] <Configuration of semiconductor package PKG1> Fig. 29 is a cross-sectional view of a semiconductor package PKG1. As shown in Fig. 29, the semiconductor package PKG1 has a semiconductor device DEV1 and a lead frame LF. The lead frame LF has a die pad DP. The die pad DP has a protrusion PP. The lead frame LF is formed of, for example, copper, a copper alloy, or the like.
[0068] The semiconductor device DEV1 is disposed so that the second surface SS faces the lead frame LF (die pad DP). As a result, the protrusion PP is inserted into the recess RP. Although not shown, the drain electrode EL3 and the lead frame LF (die pad DP) are connected by, for example, solder. The source electrode EL1 and the gate electrode EL2 are connected to a bonding wire BW.
[0069] <Effects of semiconductor package PKG1> In the semiconductor package PKG1, the load applied when wire bonding the bonding wire BW to the source electrode EL1 and the gate electrode EL2 is also supported by the protrusion PP, thereby preventing the semiconductor substrate SUB from cracking due to the load applied during wire bonding.
[0070] Sixth embodiment A semiconductor package according to the sixth embodiment (hereinafter referred to as "semiconductor package PKG2") will be described below.
[0071] <Configuration of semiconductor package PKG2> Fig. 30 is a cross-sectional view of a semiconductor package PKG2. As shown in Fig. 30, the semiconductor package PKG1 has a semiconductor device DEV1 and a lead frame LF. The lead frame LF has a die pad DP. The die pad DP is divided into a first portion DP1 and a second portion DP2.
[0072] The semiconductor device DEV1 is arranged such that the first surface FS faces the lead frame LF (die pad DP). The source electrode EL1 and the gate electrode EL2 are connected to the first portion DP1 and the second portion DP2, respectively. The connection between the source electrode EL1 and the first portion DP1 and the connection between the gate electrode EL2 and the second portion DP2 are made by, for example, solder (not shown). The bonding wire BW is connected to a portion of the drain electrode EL3 located on the bottom wall of the recess RP.
[0073] <Effects of semiconductor package PKG2> In the semiconductor package PKG2, since wire bonding is not performed on the source electrode EL1 and the gate electrode EL2, it is possible to prevent the semiconductor substrate SUB from cracking due to the load during wire bonding.
[0074] The invention made by the inventor has been specifically described above based on an embodiment, but it goes without saying that the present invention is not limited to the above embodiment and can be modified in various ways without departing from the gist of the invention. [Explanation of symbols]
[0075] BR body region, BW bonding wire, CB conductor, DEV1, DEV2, DEV3, DEV4 semiconductor device, DP die pad, DP1 first part, DP2 second part, DR1 first direction, DR2 second direction, DRA drain region, DRI drift region, EL1 source electrode, EL2 gate electrode, EL3 drain electrode, EPI epitaxial layer, FS first surface, GA gate, GI gate insulating film, GTR gate trench, III region, ILD interlayer insulating film, LF lead frame, P pitch, PKG1, PKG2 semiconductor package, PP protrusion, PR pillar region, R1 outer periphery region, R2 cell region, RP recess, S1 preparation step, S2 epitaxial growth step, S3 first ion implantation step, S4 second ion implantation step, S5 trench formation step, S6 gate insulating film formation step, S7 gate formation step, S8 Interlayer insulating film forming step, S9 contact plug forming step, S10 substrate polishing step, S11 recess forming step, S12 first electrode forming step, S13 second electrode forming step, S14 singulation step, SR source region, SS second surface, SUB semiconductor substrate, T1 thickness, T2 thickness, T3 thickness, TR trench, W width.
Claims
1. a semiconductor substrate having a first surface and a second surface opposite the first surface; a gate insulating film formed on the first surface; a gate formed on the first surface via the gate insulating film; a source region formed on the first surface side of the semiconductor substrate; a body region formed in contact with the source region and including a channel region; a drain region formed on the second surface side of the semiconductor substrate; a drift region formed in contact with the second surface side of the body region and the first surface side of the drain region, the gate faces the channel region with the gate insulating film interposed therebetween; the semiconductor substrate has at least one recess formed in the second surface that is recessed toward the first surface; the at least one recessed portion is a plurality of recessed portions arranged in a lattice pattern in a plan view, a gate electrode formed on the first surface and electrically connected to the gate; The semiconductor device, wherein the plurality of recesses are located at positions not overlapping with the gate electrode in a plan view.
2. A semiconductor substrate having a first surface and a second surface opposite the first surface; a gate insulating film formed on the first surface; a gate formed on the first surface via the gate insulating film; a source region formed on the first surface side of the semiconductor substrate; a body region formed in contact with the source region and including a channel region; a drain region formed on the second surface side of the semiconductor substrate; a drift region formed in contact with the second surface side of the body region and the first surface side of the drain region, the gate faces the channel region with the gate insulating film interposed therebetween; the semiconductor substrate has at least one recess formed in the second surface that is recessed toward the first surface; the at least one recess is a plurality of grooves extending along a first direction and spaced apart from one another in a second direction intersecting the first direction; a gate electrode formed on the first surface and electrically connected to the gate; The semiconductor device, wherein the plurality of trenches are positioned so as not to overlap the gate electrode in a plan view.
Citation Information
Patent Citations
Semiconductor integrated circuit device
JP1994302727A
Semiconductor element and its manufacturing method
JP2002016266A
Method for manufacturing semiconductor device
JP2005294773A
Semiconductor device and manufacturing method of the same
JP2013016580A
Semiconductor device and method of manufacturing semiconductor device
JP2013201413A