Semiconductor Device

The transistor design with a controlled gate insulator composition and channel region energy gap addresses the issue of characteristic changes in oxide semiconductor transistors, ensuring stable threshold voltage and improved reliability.

JP7559147B2Active Publication Date: 2024-10-01SEMICON ENERGY LAB CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023102188
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2016-08-19
Filing Date
2023-06-22
Publication Date
2024-10-01
Estimated Expiration
2036-12-08

AI Technical Summary

Technical Problem

Existing transistors using oxide semiconductors face significant changes in characteristics, particularly in threshold voltage, due to defects at the interface between the semiconductor and gate insulator, leading to reliability issues.

Method used

A transistor design incorporating a gate insulator with a specific atomic ratio of indium, element M, and zinc, where the number of oxygen atoms exceeds silicon atoms, and a channel region with a controlled energy gap and defect levels, minimizing the interface defects and stabilizing the transistor characteristics.

Benefits of technology

The design provides a transistor with minimal changes in characteristics, enhancing reliability and reducing power consumption by maintaining stable threshold voltage, suitable for use in circuits and semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559147000008
    Figure 0007559147000008
  • Figure 0007559147000009
    Figure 0007559147000009
  • Figure 0007559147000010
    Figure 0007559147000010
Patent Text Reader

Abstract

To provide a transistor whose characteristics change little, and a circuit, a semiconductor device, a display device, and an electronic device in which characteristics of transistors change little.SOLUTION: A transistor 100A includes an oxide semiconductor 108 and a gate insulator 106. A channel region 108i overlapping with a conductor 104 is formed in the oxide semiconductor. The channel region has indium, an element M and zinc. The element M is selected from one or more of aluminum, gallium, yttrium, tin, boron, silicon, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, and magnesium. The gate insulator 106 includes silicon and oxygen with an atomic ratio of 1.5 or more to silicon, the carrier density in the channel region is 1×109 cm-3 or more and 5×1016 cm-3, and the energy gap of the channel region is 2.7 eV or more and 3.1 eV or less.SELECTED DRAWING: Figure 17
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to, for example, a semiconductor, a transistor, a circuit, and a semiconductor device. The present invention relates to, for example, a semiconductor, a transistor, a circuit, and a method for manufacturing a semiconductor device. Alternatively, the present invention relates to, for example, a display device, a light-emitting device, a lighting device, a power storage device, a storage device, a processor, Also, the present invention relates to a display device, a liquid crystal display device, a light emitting device, a storage device, an The present invention relates to a method for manufacturing a sub-device, a transistor, a circuit, a semiconductor device, a display device, and a liquid crystal display. The present invention relates to a display device, a light-emitting device, a storage device, and a method for driving electronic equipment.

[0002] Note that one embodiment of the present invention is not limited to the above technical fields. The technical field of one aspect of the present invention relates to an object, a method, or a manufacturing method. One aspect of the present invention is a process, machine, manufacture, or composition of matter. It concerns the science of matter.

[0003] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. This refers to devices in general. Display devices, light-emitting devices, lighting devices, electro-optical devices, semiconductor circuits, and electronic devices The vessel may include a semiconductor device. [Background technology]

[0004] A transistor including an oxide semiconductor has an extremely small leakage current in an off-state. For example, it is known that a transistor using an oxide semiconductor has a very high leakage current. A low-power CPU that utilizes the low power consumption characteristic of the chip has been disclosed (see Patent Document 1). .).

[0005] Silicon oxide may be used as the gate insulator for transistors. When silicon oxide is used as the material, the interface between the semiconductor and the gate insulator of the transistor The defect level of the gate insulator is E'center described in Non-Patent Document 1, and hy drogen-complexed oxygen vacancy A defect that bridges the gap between two silicon layers; hydrogen bridge defect), nonbridging oxy Defects such as non-gen hole center (NBOHC) are known.

[0006] In addition, Non-Patent Document 3 describes the use of X-ray photoelectron spectroscopy (XPS). SiO2 and InGaZnO4 were measured using a neutron spectroscopy. A method for estimating the Gee band diagram is described.

[0007] In addition, Non-Patent Document 4 describes the negative bias in PMOS transistors. Reliability test called NBTI (NBTI) The reaction diffusion (RD) model is used as a degradation model. It is mentioned about. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2012-257187 A [Non-patent literature]

[0009] [Non-Patent Document 1] Fabien Devynck et al., “Charge transition levels of carbon-, oxygen-, and hydrogen-related defects at the SiC / SiO2 interface through hybrid functionals”, Physical Review B, 2011, Vol. 84, p. 235320. [Non-Patent Document 2] Shuji Munekuni et al., “Various types of nonbridging oxygen hole center in high-purity silica glass”, Journal of Applied Physics, 1990, Vol. 68, No. 3, pp. 1212-1217. [Non-Patent Document 3] EA Douglas et al., “Measurement of SiO2 / InZnGaO4 heterojunction band offsets by x-ray photoelectron spectroscopy”, Applied Physics Letters, 2011, Vol. 98, p. 242110. [Non-Patent Document 4] MA Alam et al., “A comprehensive model of PMOS NBTI degradation”, MICROELETRONICS RELIABILITY, 2005, Vol. 45, pp. 71-81. Summary of the Invention [Problem to be solved by the invention]

[0010] An object of one embodiment of the present invention is to provide a transistor with little change in characteristics. Another aspect of the present invention is to provide a transistor with a small threshold voltage change. This is one of the topics.

[0011] A circuit according to one embodiment of the present invention includes a transistor. It is an object of the present invention to provide a circuit in which the characteristics of a transistor change little. One aspect of the present invention is to provide a circuit in which the change in threshold voltage of a transistor included in the circuit is small. One of the challenges we face is to:

[0012] Another embodiment of the present invention provides a semiconductor device in which the characteristics of a transistor change little. Another object of one embodiment of the present invention is to provide a method for reducing a change in characteristics of a transistor. Another object of the present invention is to provide a display device. An object of the present invention is to provide an electronic device with little change in characteristics.

[0013] Another object of one embodiment of the present invention is to provide a highly reliable semiconductor device. Another object of one embodiment of the present invention is to provide a highly reliable display device. Another object of one embodiment of the present invention is to provide a highly reliable electronic device.

[0014] Another object of one embodiment of the present invention is to provide a novel circuit. An object of one embodiment of the present invention is to provide a novel device. One of the objects of the present invention is to provide a novel electronic device.

[0015] Note that one embodiment of the present invention does not necessarily have to solve all of the above problems, but It is sufficient if the invention can solve at least one of the problems. In addition, the description of the problem above may be changed without prior notice. Problems other than these cannot be identified from the description in the specification, drawings, claims, etc. It is obvious that there are other problems than these from the description, drawings, claims, etc. It is possible to extract [Means for solving the problem]

[0016] One embodiment of the present invention is a transistor including an oxide semiconductor, a gate insulator, and a gate electrode. The oxide semiconductor has a channel region formed therein. The channel region is made of indium. The element M is aluminum, gallium, yttrium, Tin, boron, silicon, titanium, iron, nickel, germanium, zirconium, molyb Dense, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium The gate insulator comprises silicon and oxygen, and the gate insulator comprises In the channel region, the number of oxygen atoms is 1.5 times or more the number of silicon atoms. The rear density is 1×10 9 cm -3 5×10 or more 16 cm -3 of the channel region. The energy gap of the transistor is 2.7 eV or more and 3.1 eV or less. In the above structure, the gate insulator has a defect level, and the defect level and the conduction of the channel region are The difference in energy from the lower end of the conductive band is preferably 0.2 eV or more and 1.0 eV or less. .

[0017] In the above structure, the gate insulator is disposed on either the upper surface or the lower surface of the first region. The atomic ratios of indium, element M, and zinc are represented by x, y, and z, respectively. , x / (x+y+z) is greater than or equal to 0.33 and less than or equal to 0.7, and y / (x+y+z) is less than or equal to 0 It is preferable that the ratio be greater than .08 and less than 0.33.

[0018] Alternatively, one embodiment of the present invention is a semiconductor device including a first oxide semiconductor, a second oxide semiconductor, and a gate insulator. a first oxide semiconductor layer and a gate electrode; the second oxide semiconductor has a second region in contact with the first oxide semiconductor; The gate insulator has a region in contact with the second region, and the first region has a channel region formed therein. The first region and the second region have indium, an element M, and zinc, and the element M is , aluminum, gallium, yttrium, tin, boron, silicon, titanium, iron, nickel Kel, Germanium, Zirconium, Molybdenum, Lanthanum, Cerium, Neodymium, Hafnium The gate insulator is selected from one or more of sulphur, tantalum, tungsten and magnesium. The gate insulator has a thickness of 100 nm to 150 nm, and the number of oxygen atoms is equal to the number of silicon atoms. The carrier density of the first region is 1×10 9 cm -3 5×10 or more 16 cm -3 The energy gap of the first region is 2.7 eV or more and 3.1 eV or less. V or less, and the energy gap of the second region is smaller than the energy gap of the first region. This transistor is 0.15 eV to 2 eV larger than the above.

[0019] In the above structure, the number of atoms of indium, element M, and zinc contained in the first region is The ratios are represented by x1, y1 and z1, respectively, and x1 / (x1+y1+z1) is 0.33. 0.7 or less, and y1 / (x1+y1+z1) is 0.08 or more and 0.33 or less. It is preferable to satisfy.

[0020] In the above structure, the gate insulator has a trap level, and the trap level and the first The difference in energy between the conduction band minimum of region 1 and region 2 is 0.2 eV or more and 1.0 eV or less, The difference between the trap level and the energy of the bottom of the conduction band of the second region is -0.2 eV or more. It is preferable that it is 0.8 eV or less.

[0021] In the above configuration, the thickness of the second region is 1 nm or more and 20 nm or less. In the above structure, the channel length of the transistor is preferably 0.01 μm or more. 5 μm or less, and a voltage of 0.1 V or more between the drain and source of the transistor When a potential difference of 0V or less is applied, the threshold value is preferably -0.5V or more and 2V or less. In the above structure, the gate insulator has a thickness of 5 nm or more and 200 nm or less. It is preferred to have a certain region.

[0022] Another embodiment of the present invention is a circuit including any one of the above transistors. A voltage between -1V and 20V is applied between the source and gate electrodes of the transistor. This is a circuit.

[0023] Another embodiment of the present invention is a semiconductor device including any of the above circuits.

[0024] Another embodiment of the present invention is an electronic device including any of the above semiconductor devices.

[0025] Another embodiment of the present invention is a display device including any of the above electronic devices.

[0026] Another embodiment of the present invention is a display device including the circuit described above, The display device is a gate driver of the display device.

[0027] Another embodiment of the present invention is the display device described above, further comprising a touch sensor and a speaker. and an imaging device.

[0028] Another embodiment of the present invention is an electronic device including the above-described display device. Effect of the Invention

[0029] According to one embodiment of the present invention, a transistor whose characteristics change little can be provided. According to one embodiment of the present invention, a transistor with a small change in threshold voltage can be provided. do.

[0030] According to one embodiment of the present invention, the circuit includes a transistor. It is possible to provide a circuit in which the characteristics of a transistor change little when the transistor is turned on. According to an embodiment, a circuit having a transistor with a small change in threshold voltage is provided. can be done.

[0031] According to another embodiment of the present invention, a semiconductor device in which the characteristics of a transistor change little is provided. Furthermore, according to one embodiment of the present invention, a display device with little change in transistor characteristics can be obtained. In addition, according to one embodiment of the present invention, a device can be provided. It is possible to provide an electronic device with less

[0032] According to one embodiment of the present invention, a highly reliable semiconductor device can be provided. According to one embodiment of the present invention, a highly reliable display device can be provided. According to one embodiment, a highly reliable electronic device can be provided.

[0033] According to one embodiment of the present invention, a novel circuit can be provided. According to one aspect of the present invention, a novel device can be provided. An electronic device can be provided.

[0034] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have to have all of these effects. The above will become apparent from the description in the specification, drawings, claims, etc. It is possible to extract other effects from the descriptions in the claims, etc. [Brief description of the drawings]

[0035] [Figure 1] A transistor according to one embodiment of the present invention. [Diagram 2] Transistor Ids-Vgs characteristics. [Diagram 3] Transistor threshold voltage change over time. [Figure 4] The time it takes for a transistor's threshold voltage to change. [Diagram 5] 1A and 1B are diagrams showing band structures of an oxide semiconductor and a gate insulator. [Figure 6] Conduction band of oxide semiconductor and gate insulator. [Figure 7] Electron density in an oxide semiconductor and the conduction band of a gate insulator. [Figure 8] Defect levels in silicon oxide. [Figure 9] FIG. 1 is a diagram showing changes in the charge state of defects. [Figure 10] Diagram showing electron transitions. [Figure 11] 1A and 1B are diagrams showing band structures of an oxide semiconductor and a gate insulator. [Figure 12] FIG. [Figure 13] Transistor Ids-Vgs characteristics. [Figure 14] FIG. [Figure 15] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 16] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 17] FIG. 1 is a cross-sectional view of a transistor. [Figure 18] FIG. [Figure 19] 1A to 1C illustrate a method for manufacturing a transistor. [Figure 20] 1A to 1C illustrate a method for manufacturing a transistor. [Figure 21] 1A to 1C illustrate a method for manufacturing a transistor. [Figure 22] 1A and 1B are diagrams illustrating structural analyses of a CAAC-OS and a single crystal oxide semiconductor by XRD, and diagrams showing selected-area electron diffraction patterns of a CAAC-OS. [Figure 23] Cross-sectional TEM image and planar TEM image of CAAC-OS, and their image analysis images. [Figure 24] Electron diffraction pattern of nc-OS and cross-sectional TEM image of nc-OS. [Diagram 25] Cross-sectional TEM image of a-like OS. [Figure 26] FIG. 1 shows the change in the crystal part of an In-Ga-Zn oxide due to electron irradiation. [Figure 27] FIG. 2 is a diagram for explaining the range of atomic ratio of oxides according to the present invention. [Figure 28] A diagram explaining the InMZnO4 crystal. [Figure 29] FIG. 1 is a top view illustrating one embodiment of a display device. [Diagram 30] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Diagram 31] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Diagram 32] 1A and 1B are a block diagram and a circuit diagram illustrating a display device. [Diagram 33] FIG. 2 is a diagram illustrating a display module. [Diagram 34] 1A to 1C are diagrams illustrating electronic devices. [Diagram 35]1A and 1B are a circuit diagram and a cross-sectional view of a semiconductor device. [Diagram 36] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 37] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 38] Transistor Ids-Vgs characteristics. [Figure 39] FIG. 13 is a graph for explaining the relationship between stress time and threshold change. [Diagram 40] FIG. 4 is a diagram for explaining the relationship between stress temperature and threshold change. [Diagram 41] 1A and 1B are a top view and a cross-sectional view of a transistor. [Diagram 42] FIG. 1 is a cross-sectional view of a transistor. [Diagram 43] 1A and 1B are a top view and a cross-sectional view of a transistor. [Diagram 44] A diagram showing the model. [Diagram 45] Transistor Ids-Vgs characteristics. [Diagram 46] FIG. 13 is a graph for explaining the relationship between stress time and threshold change. [Figure 47] Calculated density of states of In-Ga-Zn oxide. [Figure 48] Calculated projected density of states of indium and gallium in In-Ga-Zn oxide. [Figure 49] Calculated projected density of states of zinc and oxygen in In-Ga-Zn oxide. [Figure 50] Temperature dependence of electron mobility in oxide semiconductors. [Figure 51] Evaluation results by X-ray diffraction. [Figure 52] XPS analysis results. [Diagram 53] XPS analysis results. [Figure 54] XPS analysis results. [Figure 55] SIMS analysis results. [Figure 56] Cross-sectional TEM observation results. [Figure 57] Planar TEM observation results. [Figure 58] Electron diffraction observation results. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] The present invention will be described in detail with reference to the drawings. The present invention is not limited to the description, and various modifications in form and details are possible. In addition, the present invention should not be construed as being limited to the description of the following embodiments. In explaining the configuration of the invention using the drawings, the same reference numerals are used It is used commonly across different drawings. Note that when referring to similar objects, the hatch pattern is used in the same way. In some cases, no particular symbol is given.

[0037] In the figures, the size, thickness of the film (layer), or area is exaggerated for clarity. There may be cases where this is the case.

[0038] In this specification, the terms "film" and "layer" are interchangeable. It is possible to do so.

[0039] Also, a voltage is a voltage between a certain potential and a reference potential (such as ground potential (GND) or source potential). Therefore, voltage can be replaced with electric potential. do.

[0040] The ordinal numbers 1 and 2 are used for convenience and do not indicate the order of processes or stacking. It does not indicate the layer order. Therefore, for example, "first" should not be changed to "second" or "third" In addition, the ordinal numbers described in this specification and the like can be appropriately replaced with the ordinal numbers. In some cases, the term may not match the ordinal number used to identify an aspect of the invention.

[0041] Even if a material is described as a "semiconductor," it may be considered an "insulator" if, for example, its electrical conductivity is sufficiently low. In addition, the boundary between "semiconductors" and "insulators" is unclear and cannot be clearly defined. In some cases, the distinction cannot be made precisely. Therefore, the term "semiconductor" as used herein means "insulator" Similarly, the term "insulator" used in this specification can be interpreted as "semiconductor." In some cases, this can be rephrased as "body."

[0042] In addition, even if a material is written as a "semiconductor," if the material has a sufficiently high electrical conductivity, it may be written as a "conductor." In addition, the boundary between "semiconductor" and "conductor" is unclear and not strictly defined. In some cases, the distinction may not be clear. Therefore, the term "semiconductor" as used herein means "conductor" or "electroconductor". Similarly, the term "conductor" used in this specification can be interpreted as "semiconductor In some cases, this can be rephrased as "body."

[0043] The impurities in a semiconductor are, for example, substances other than the main components that make up the semiconductor. Elements present at less than 0.1 atomic percent are considered impurities. The formation of DOS (Density of States) in the conductor and carrier migration In some cases, the mobility and crystallinity of the semiconductor may decrease. In the case of semiconductors, impurities that change the properties of the semiconductor include, for example, group 1 elements, These include Group 2 elements, Group 13 elements, Group 14 elements, Group 15 elements, and transition metals other than the main components. In particular, for example, hydrogen (also contained in water), lithium, sodium, silicon, boron, In the case of oxide semiconductors, for example, impurities such as hydrogen can cause In addition, when the semiconductor is silicon, the characteristics of the semiconductor Examples of impurities that change the value of the valence number include oxygen, Group 1 elements excluding hydrogen, Group 2 elements, and These include Group 3 elements and Group 15 elements.

[0044] Note that the channel length is, for example, the length of a semiconductor (or transistor) in a top view of a transistor. When the transistor is on, the gate electrode overlaps with the semiconductor (the part through which current flows). The source region or the channel region This refers to the distance between the drain (drain region or drain electrode) and the In the transistor, the channel length does not necessarily have the same value in all regions. The channel length of a transistor may not be determined to a single value. In the detailed description, the channel length is any one value or the maximum value in the region where the channel is formed. , the minimum or average value.

[0045] The channel width is the width of the semiconductor (or transistor) when it is in the on state. The area where the gate electrode overlaps with the electrode (the area where the current flows) forms a channel. This refers to the length of the part of the region where the source and drain face each other. In a transistor, the channel width does not necessarily have the same value in all regions. That is, The channel width of a transistor may not be determined to a single value. In the fine print, the channel width is any one value or the maximum value in the region where the channel is formed. , the minimum or average value.

[0046] Depending on the structure of the transistor, the channel in the region where the channel is actually formed may be The effective channel width is shown in the top view of the transistor. The channel width that is actually used (hereinafter referred to as the apparent channel width) may differ from the actual channel width. For example, In a transistor having a three-dimensional structure, the effective channel width is The channel width becomes larger than the apparent width shown in the figure, and the effect becomes non-negligible. For example, in transistors with a fine, three-dimensional structure, the lateral surface of the semiconductor In this case, the ratio of the channel region formed in the top view may be large. The effective channel width of the channel is actually formed rather than the apparent channel width shown. will be larger.

[0047] In a transistor having a three-dimensional structure, the effective channel width is For example, it may be difficult to estimate the effective channel width from the design value. In order for deposition to occur, it is necessary to assume that the shape of the semiconductor is known. It is difficult to accurately measure the effective channel width unless the exact channel conditions are known. .

[0048] Therefore, in this specification, in a top view of a transistor, a semiconductor and a gate electrode are not mutually connected. The apparent length of the source and drain facing each other in the overlapping region. The above channel width is called "Surrounded Channel Width (SCW)". In this specification, it is simply referred to as the channel width. In some cases, it may refer to the enclosed channel width or apparent channel width. In this specification, when the term "channel width" is used simply, it may refer to the effective channel width. In addition, the channel length, channel width, effective channel width, apparent channel width, and The width of the interstitial channel can be determined by acquiring a cross-sectional TEM image and analyzing the image. Thus, the value can be determined.

[0049] In addition, the field effect mobility of the transistor and the current value per channel width are calculated. In some cases, the effective channel width is calculated using the enclosed channel width. The value may differ from that calculated using the channel width.

[0050] In this specification, when it is stated that A has a shape protruding from B, this is a top view. Or in the cross-sectional view, at least one end of A is outside at least one end of B. Therefore, it is written that A has a shape that protrudes more than B. For example, in the top view, one end of A is on the outside of one end of B. This can be read as having the following.

[0051] In this specification, "parallel" means that two straight lines are arranged at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Parallel" refers to two lines that are arranged at an angle between -30° and 30°. Also, "perpendicular" means that two straight lines are arranged at an angle of 80° or more and 100° or less. Therefore, it also includes the case where the angle is between 85° and 95°. This refers to a state in which two straight lines are arranged at an angle of 60° or more and 120° or less.

[0052] In this specification, when the crystal is a trigonal or rhombohedral crystal, it is represented as a hexagonal crystal system. vinegar.

[0053] In addition, the following embodiments and examples can be combined as appropriate in this specification. In addition, when multiple configuration examples are shown in one embodiment or example, the configurations are mutually exclusive. The examples can be combined as appropriate.

[0054] (Embodiment 1) In this embodiment, a transistor or the like according to one embodiment of the present invention will be described.

[0055] The transistor of one embodiment of the present invention can be used in a circuit, a display element, or the like of one embodiment of the present invention. A semiconductor device according to one embodiment of the present invention includes the circuit, a display element, or the like. An electronic device according to one embodiment of the present invention includes the semiconductor device. The display device preferably includes the semiconductor device according to one embodiment of the present invention. It is preferable to do so.

[0056] The transistor of one embodiment of the present invention preferably includes an oxide semiconductor. The transistor of one embodiment preferably includes an oxide semiconductor in a channel region.

[0057] The oxide semiconductor included in the transistor preferably contains indium and zinc. The oxide semiconductor preferably contains an element M. The element M is aluminum, gallium, or the like. Other elements that can be used for M include lithium, yttrium, and tin. are boron, silicon, titanium, iron, nickel, germanium, zirconium, molybdenum Lanthanum, Cerium, Neodymium, Hafnium, Tantalum, Tungsten, Magnesium Examples include:

[0058] When the oxide semiconductor contains In, for example, the carrier mobility (electron mobility) is increased. In addition, when the oxide semiconductor contains Zn, the oxide semiconductor is easily crystallized. When a semiconductor has an element M that functions as a stabilizer, for example, an oxide semiconductor The energy gap becomes larger.

[0059] A circuit, a semiconductor device, a display device, and an electronic device according to one embodiment of the present invention include an oxide semiconductor. It is preferable that the transistor has a

[0060] In the transistor including an oxide semiconductor according to one embodiment of the present invention, the current value in an off state ( The off-state current (off-state current) of a transistor including an oxide semiconductor can be reduced. This allows data to be stored for a long period of time. Therefore, the power consumption of a circuit, a semiconductor device, a display device, an electronic device, etc. can be reduced. can be reduced.

[0061] The off-state current of a transistor having an oxide semiconductor in a channel region is, for example, 10 -21 A For example, if the channel width W is 1×10 6 μm and the channel length L is 10 μm. However, the voltage between the source and drain electrodes (drain voltage) is in the range of 1V to 10V. The off-state current is below the measurement limit of the semiconductor parameter analyzer, that is, 1×10 - 13 It is possible to obtain a characteristic of A or less.

[0062] For example, in a display device, the retention time of an electric signal such as an image signal can be extended, When the power is on, the write interval can be set longer. This reduces the frequency of refresh operations. In addition, the oxide semiconductor can be used as a semiconductor device. By using such a transistor, a high-definition display device can be realized in some cases. In addition, by using a transistor including an oxide semiconductor, the display quality of a display device can be improved. In this way, a transistor having an oxide semiconductor in a channel region can be used. The transistor has excellent characteristics.

[0063] When a transistor is applied to a circuit, the transistor Voltages are applied between the source and drain of the transistor, and between the source and gate of the transistor. Changes in characteristics can cause circuit malfunctions. Changes in transistor characteristics This can lead to high power consumption in the circuit. Also, changes in transistor characteristics As a result, the performance of a semiconductor device having a circuit, a display device, and an electronic device may be degraded. Therefore, it is preferable that the change in the characteristics of a transistor caused by the operation of a circuit is as small as possible.

[0064] The threshold voltage is one of the parameters for evaluating the characteristics of a transistor. In this specification, the threshold voltage refers to the gate voltage when a channel is formed. For example, the gate voltage (Vg) is plotted on the horizontal axis and the square root of the drain current Id on the vertical axis. The line obtained by extrapolating the tangent line with the maximum slope in the simulated curve (Vg-√Id characteristics) is The square root of the drain current (current between the gate and source) Ids is 0 (Id is 0A) The gate voltage (Vg) at the intersection of the channel Let L be the length and W be the channel width, and the value of Ids[A]×L[μm]÷W[μm] is 1×10 - 9 The Vgs at which [A] is reached is sometimes defined as the threshold voltage.

[0065] In order to reduce the variation in transistor characteristics due to circuit operation, the inventors In a transistor having an oxide semiconductor in a gate region, The relationship between the trap levels at the interface and in the gate insulator and the transistor threshold change As a result, it was found that the band offset of the oxide semiconductor can be changed They found that this can suppress fluctuations in transistor characteristics.

[0066] <An example of a stress test> First, the change in threshold voltage was evaluated before and after applying stress to the transistor. .

[0067] Hereafter, the voltage applied between the gate and source is called Vgs, and the voltage between the drain and source is called V The voltage is called Vds. The stresses are Vgs=V1[V] and Vds=0V. V1 and The evaluation was carried out under three conditions: 10 V, 30 V, and 40 V. The measurement temperature was 80 The three conditions were: 100°C, 100°C, and 125°C.

[0068] The transistor 100 shown in FIG. The transistor 100 includes an oxide semiconductor 108a and a source The conductor 112a functions as a gate electrode, the conductor 112b functions as a drain electrode, and the The conductor 104 functions as a gate electrode, and the insulators 106a and 106b function as gate insulators. and an insulator 106b.

[0069] The transistors to be stressed are made of silicon nitride with a thickness of 400 nm as the insulator 106a. A silicon oxide nitride film having a thickness of 50 nm was used as the insulator 106b. In the silicon oxynitride film, the atomic ratio of oxygen is higher than that of nitrogen.

[0070] The oxide semiconductor 108a was made of In-Ga-Zn oxide having a thickness of 35 nm. In-Ga-Zn oxide is a polycrystalline metal oxide target (In:Ga:Zn=1: The film was formed by sputtering using a 1:1 atomic ratio.

[0071] Here, as an example, the insulator 106a is a PEC made of silane, nitrogen, and ammonia. VD(Plasma Enhanced Chemical Vapor Deposit) The insulator 106b was formed by the deposition method using silane and dinitrogen monoxide. (Gas flow rates were 20sccm and 3000sccm, respectively), pressure was 40Pa, and The oxide semiconductor 108 was formed by a PECVD method at a power of 100 W. A metal oxide target (In:Ga:Zn=1:1:1 [atomic ratio]) was used to The temperature was set at 300°C, and argon and oxygen were used (gas flow rates were 20 sccm and 20 sccm, respectively). and 10 sccm), pressure was 0.4 Pa, and power was 100 W DC power source. The film was formed by the method.

[0072] In addition, tungsten is used as the conductor 104. In addition, the conductor 112a and the conductor Three metal layers were used for 112b. The metal layers were tungsten, aluminium, The layers are laminated in the order of lumi and titanium.

[0073] Ids-Vgs characteristics of a transistor with a channel length L of 6 μm and a channel width W of 50 μm This is shown in Figure 2.

[0074] In Fig. 3, the horizontal axis shows the stress application time and the vertical axis shows the threshold fluctuation (hereafter, This is a graph plotting the threshold voltage (hereinafter referred to as Vth) and the The Ids-Vgs characteristics were calculated at ds = 10 V. Here, Ids is the gate and source The current between the

[0075] The time when ΔVth becomes 1V is called Time to Fail (TTF). Figure 4 shows the absolute temperature of the measured temperature at Vgs=30V, with the TTF on the vertical axis. This is a graph plotting the inverse (1 / T) of

[0076] The data in Figure 4 is approximated by equation (1) to obtain the activation energy E a can be asked for In equation (1), A is a constant and k is the Boltzmann constant.

[0077]

number

[0078] Activation energy E at V1 of 10 V, 30 V, and 40 V a are 0.51 respectively. The calculated values ​​were 0.45 eV, 0.39 eV and 0.51 eV.

[0079] Next, the phenomenon that causes the threshold voltage shift was considered.

[0080] <Band structure 1> The energy gap energy was calculated from the XPS measurement by referring to the method described in Non-Patent Document 3. The valence band depth and conduction band depth were estimated. A polycrystalline metal oxide target (In:Ga: Zn=1:1:1 [atomic ratio]) was used to deposit In-Ga-Zn oxide by sputtering. A film of the compound was formed.

[0081] Figure 5 shows the valence and conduction bands of the oxide semiconductor and the gate insulator, respectively. Here, the gate insulator is shown in terms of the interface region with the oxide semiconductor and the bulk region. .

[0082] <Conduction band> Next, the electron affinity and ionization potential calculated from the actual measurements described in FIG. Using the model, the conduction band of the gate insulator and the oxide semiconductor when Vgs is changed is calculated. The calculation was performed using ATLAS manufactured by Silvaco. The work function of the gate electrode is set to 4 0.7 eV, and the electron affinity of the gate insulator and oxide semiconductor are 0.9 eV and 4.6 eV. The ionization potentials of the gate insulator and the oxide semiconductor were set to 9.5 eV and and 7.8 eV, and the energy gaps of the gate insulator and oxide semiconductor are 8.6 eV and The dielectric constants of the gate insulator and the oxide semiconductor were set to 4.1 and 3.2 eV. The number was set at 15.

[0083] The calculated conduction bands of the oxide semiconductor and the gate insulator are shown in Figure 6. The energy is shown with respect to the Fermi level. , 15V, 20V, 30V, 40V, 60V and 80V, the calculated values ​​are As shown in Figure 6, the conduction of the gate insulator at the interface with the oxide semiconductor is It can be seen that the band gradually becomes lower with respect to the Fermi level as Vgs increases. 6, the accumulation of carriers in the oxide semiconductor at the interface with the gate insulator, i.e., the electron density The results are shown in Figure 7.

[0084] In FIG. 7, the horizontal axis represents Vgs, and the vertical axis represents the oxide semiconductor and the The Fermi level of the gate insulator at the gate electrode is plotted as a white square. The electron density of the oxide semiconductor at the interface with the oxide insulator is plotted as a black square. .

[0085] <Transistor characteristic estimation> Next, we consider the Fermi effect of the gate insulator when changing the energy gap of the oxide semiconductor. The change in the level and the Ids-Vgs characteristics of the transistor are calculated. The ATLAS manufactured by Silvaco was used. The parameters used were as shown in Table 1.

[0086] [Table 1]

[0087] The energy gap was changed from 1.5 eV to 3.5 eV. Here, the electron affinity The energy gap between the two states is expressed as follows: Before bonding, the physical properties of the oxide semiconductor single layer are adjusted so that the valence bands are at the same position. The energy gap was 3.2 eV, and the donor density was 6.6 × 10 -9 [cm -3 The results are shown in Figure 11. In Figure 11, the Fermi level is located at 0 eV. .

[0088] Next, when Vgs is set to 30 V, the gate insulator at the interface with the oxide semiconductor The conduction band is shown in Figure 12. In Figure 12, the Fermi level is located at 0 eV.

[0089] Next, we consider the Ids- of a transistor when changing the energy gap of an oxide semiconductor. The Vgs characteristics are shown in Figure 13. The smaller the energy gap, the greater the Ids-Vgs characteristics. It can be seen that the threshold value is negatively shifted.

[0090] <Defect levels> As shown in Non-Patent Documents 1 and 2, E' center, hydrogen-complexed oxygen vacancy , NBOHC, etc. are known.

[0091] In this embodiment, the defect in amorphous silicon oxide is calculated by first-principles calculation. The transition levels of the recessive levels were calculated using the plane wave basis first-principles calculation software VASP (Vi The enna ab-initio simulation package was used. The hybrid functional used was HSE06, and the exchange-correlation term was GGA-PBE. The mixing ratio is 0.4, and the pseudopotential is PAW. Cutoff energy of the plane wave The energy was set to 800 eV. A model of amorphous silicon oxide was calculated. The molecular dynamics method was used as the method for the calculation, and the structure was optimized by the melt quench method. The parameters used are the number of atoms, 96, the pseudopotential of oxygen, O_h, and the The mesh size was 1x1x1 k-points (a 1x1x1 k-point mesh was used).

[0092] FIG. 8 shows the calculated transition levels of the defect levels in silicon oxide. , E'center, hydrogen-complexed oxygen vaca The defect levels corresponding to ncy(Si-H-Si) and NBOHC are E', E Si-H-Si and E NBOHC Here, the levels shown as (0 / -) in the figure are the charged The level indicated as (+ / 0) is when the charge state changes from neutral to negative, and the level indicated as (+ / 0) is when the charge state changes from positive to neutral, The Fermi energy changes as a function of the hydrogen-complex. Regarding the exhaled oxygen vacancy, the charge state changes from positive to neutral. The energy that Si-H-Si(+ / 0) This is expressed as:

[0093] As shown in Figure 4, at V1 = 30 V, the activation energy E a is calculated as 0.45 eV. As shown in Fig. 7, the Fermi level of the gate insulator at Vgs=30V was E fg From the conduction band to E fg The energy to the nucleus was estimated to be 3.65 eV. From Fig. 8, the defect level E Si-H-Si(+ / 0) Energy up to The energy is about 3.1 eV. These relationships are shown in the band diagram of Figure 10.

[0094] From the above, when the charge state changes from positive to neutral, the defect level E Si-H- Si The energy from to the conduction band is E fg and E a The energy difference between Therefore, the defect level E Si-H-Si(+ / 0) The corresponding reaction This suggests that this is one of the main factors behind the threshold shift. In the n-complexed oxygen vacancy, the charge state is positive or negative. The reaction when the defect changes from a neutral state to a neutral state, that is, when an electron is donated to the defect, is shown in the model of FIG. As shown in the figure.

[0095] By increasing the activation energy, the interface between the gate insulator and the oxide semiconductor and may result in less trapped charge in the gate insulator, which is preferred. To increase the activation energy, the distance between the channel region of the transistor and the defect level must be increased. The energy difference can be increased. For example, the activation energy can be increased by The energy at the bottom of the conduction band of a semiconductor can be lowered. For example, the electron affinity can be increased. Just do that.

[0096] In addition, the increase in ΔVth due to the charge being trapped in the traps in the gate insulator is In addition to the increase in the capacitance, the gate insulator is desorbed of easily diffusible elements, such as hydrogen. This generates fixed charges in the gate insulator and at the interface between the gate insulator and the oxide semiconductor. This may lead to an increase in ΔVth. For example, , etc. are possible reactions.

[0097] [ka]

[0098] [ka]

[0099] The generation of fixed charges in the gate insulator can be explained as follows. A reaction represented by at least one of formula (G1) and general formula (G2) occurs. This reaction breaks the bonds in H2O and SiOH, generating fixed charges and hydrogen. Hydrogen is an element that diffuses easily. The resulting hydrogen diffuses, and the reaction The balance of both sides of is lost. To restore the balance, the direction in which the fixed charge is generated (to the right) As a result, the fixed charge increases over time, causing the threshold voltage to fluctuate. Increase.

[0100] Here, ΔVth is expressed by the following formula (2) using α, β and stress time t. This can be done.

[0101]

number

[0102] Here, formula (2) is the reaction-diffusi on(RD)model, and α is the charge transport due to carrier trapping and reaction. Initial deterioration, i.e., due to the amount of initial reaction in general formula (G1) and general formula (G2) is a parameter that determines the diffusion coefficient, and β is a parameter that is due to diffusion.

[0103] α is thought to represent the ease of reaction. For example, a larger activation energy By making it difficult for traps to occur in the gate insulating film, α can be reduced. It is believed that the reaction represented by general formula (G1), general formula (G2), etc. can be suppressed. It is believed that by controlling this, α can be made small.

[0104] It is believed that β is due to diffusion and depends on, for example, the ease of diffusion of hydrogen.

[0105] Here, the RD model will be explained with reference to FIG. 44 and the following general formula (G3).

[0106] [ka]

[0107] FIG. 44(A) shows a case where a compound having elements A and B is used as a gate insulator and an oxide semiconductor. In this compound, element A and element B are bonded to each other. .

[0108] Figure 44(B) shows the initial reaction process. As shown in Figure 44(B), electrons (e - ) is given When the electron is released, the bond between element A and element B is broken (general formula (G3)). For example, this phenomenon is likely to occur when an electric field is applied to the gate insulating film and the oxide semiconductor. The ease of the initial reaction can be expressed by the parameter α.

[0109] Thereafter, as shown in FIG. 44(C), element B diffuses into the gate insulating film. The ease can be represented by the parameter β.

[0110] <Oxide semiconductor> The energy gap of an oxide semiconductor in a channel region of a transistor according to one embodiment of the present invention The gap is preferably 2.6 eV or more and 3.3 eV or less, and more preferably 2.7 eV or more and 3. It is preferably 1 eV or less, and more preferably 2.9 eV or more and 3.1 eV or less.

[0111] The oxide semiconductor included in the channel region of the transistor of one embodiment of the present invention is indium and and zinc. The oxide semiconductor preferably contains an element M. The atomic ratios of indium, element M, and zinc are represented as x, y, and z, respectively.

[0112] In addition, by increasing the atomic ratio of indium, the energy gap can be made smaller. In addition, by making the atomic ratio of element M smaller, the energy In some cases, the Gap can be made smaller. In addition, the atomic ratio of element M can be made smaller. This may result in a larger electron affinity.

[0113] It is preferable that x / (x+y+z) is 0.33 or more and less than 0.7. It is preferable that (x+y+z) is 0.08 or more and less than 0.33. is preferably gallium.

[0114] In addition, for example, by increasing the carrier density of the oxide semiconductor of one embodiment of the present invention, The oxide semiconductor in the channel region of the transistor according to one embodiment of the present invention The carrier density of the body is 1×10 5 cm -3 5×10 or more 17 cm -3 The following is preferred: 1 ×10 7 cm -3 More than 1×10 17 cm -3 Less than 1×10 is preferable. 9 cm -3 Below top 5×10 16 cm -3 More preferably, 1×10 10 cm -3 More than 1×10 16 cm -3 More preferably, 1×10 11 cm -3 More than 1×10 15 cm -3 The following is Even more preferred.

[0115] Here, the oxygen vacancy (V O When hydrogen bonds to the hydrogen atom (called The carrier density may increase.

[0116] If the carrier density increases too much, the Ids-Vgs characteristics of the transistor will be significantly negative. That is, the threshold value is shifted negatively. The negative shift is excessive. When this occurs, the transistor is likely to have normally-on characteristics. Normally-on characteristics are when the gate voltage Vg = 0V and the current (for example, the drain This refers to the characteristic that a current (Ids) flows between the diode and the source.

[0117] The hydrogen concentration in the oxide semiconductor in the channel region of the transistor of one embodiment of the present invention is preferably Preferably 2 x 10 20 atoms / cm 3 Less than or equal to 5×10 19 atoms / cm 3 Less than 1×10, more preferably 19 atoms / cm 3 The following is more preferable: is 5 x 10 18 atoms / cm 3 The following is the result.

[0118] <Transistor threshold voltage> As mentioned above, when the energy gap becomes too small and the carrier density becomes too high, If the degree increases too much, the threshold may be excessively negatively shifted.

[0119] For example, when the channel length of a transistor is 10 nm or more and 10,000 nm or less, A potential difference between the drain and source of the transistor is 0.1 V to 15 V. In this case, the threshold value is preferably −0.5 V or more and 2 V or less, more preferably −0.3 V or more It is less than 1V.

[0120] <Projected density of states> In the In-Ga-Zn oxide, the total density of states (TdS) f States) and the projected density of states (Pr ojected Density of States (PDOS) and The conditions used in the calculation are shown in Table 2.

[0121] [Table 2]

[0122] Figure 47 shows the total density of states of the In-Ga-Zn oxide. Fig. 48(B) shows the projection of gallium, Fig. 49(A) shows the projection of zinc, and Fig. 49(B) shows the projection of oxygen. The shape densities are shown respectively.

[0123] From Figures 48 and 49, the conduction band minimum The orbitals of all four elements contribute to the upper valence band (Vale It was found that the oxygen 2p orbital mainly contributes to the VBM. It is suggested.

[0124] (Embodiment 2) In this embodiment, a transistor according to one embodiment of the present invention will be described.

[0125] <Transistor structure example 1> An example of a structure of a transistor according to one embodiment of the present invention will be described below.

[0126] FIG. 1C is a top view of a transistor 100 which is a semiconductor device of one embodiment of the present invention. 1(A) and (B) are cross-sectional views taken along a dashed line X1-X2 shown in FIG. 1(A). , and a cross-sectional view taken along dashed line Y1-Y2.

[0127] In addition, in order to avoid complication, in FIG. 1C, the configuration of the transistor 100 is Some of the elements (such as an insulating film that functions as a gate insulator) are omitted in the figure. The direction of the dashed dotted line X1-X2 is called the channel length direction, and the direction of the dashed dotted line Y1-Y2 is called the channel width direction. In the top view of the transistor, the same reference numerals as those in FIG. As in (C), some of the components may be omitted in the illustration.

[0128] The transistor 100 includes a conductor 104 on a substrate 102 that functions as a gate electrode, and a An insulator 106a on the plate 102 and the conductor 104, and an insulator 106b on the insulator 106a. The oxide semiconductor 108a over the insulator 106b and the oxide semiconductor 108b electrically connected to the oxide semiconductor 108a are The conductor 112a serving as a source electrode is electrically connected to the oxide semiconductor 108a. and a conductor 112b serving as a drain electrode connected to the insulator 106a. The insulator 106b functions as a gate insulator for the transistor 100. On the transistor 100, more specifically, the conductors 112a and 112b and the oxide semiconductor 108a On top of this are provided insulators 114, 116, and 118. The insulator 118 functions as a protective insulating film for the transistor 100. may be referred to as a first protective insulating film, and insulator 116 may be referred to as a second protective insulating film.

[0129] Here, the transistor 100 functions as a gate electrode as shown in FIG. The oxide semiconductor 108a on the conductor 104 side and the oxide semiconductor 10 on the oxide semiconductor 108a 8b may have a two-layer structure in which oxide semiconductors are stacked.

[0130] The oxide semiconductor 108a described in Embodiment 1 is used as the oxide semiconductor 108a. can be done.

[0131] The oxide semiconductor 108a is In-M (wherein M is aluminum, gallium, or yttrium). In particular, the oxides of In-Zn-Zn can be used. As the semiconductor 108, it is preferable to use In-M-Zn oxide.

[0132] The oxide semiconductor 108a has a composition of In:M:Zn=4:α1(1.5≦α1≦2.5):α2 (2.5≦α2≦3.5) [atomic ratio], In:M:Zn=1:β1(0.8≦β1≦1.2):β2(0.8≦β2≦1.2 ) [atomic number ratio] is preferable.

[0133] The oxide semiconductor 108a has the above-mentioned atomic ratio, that is, the atomic ratio of In is greater than the atomic ratio of M. By making the composition rich in Cr, the conduction band of the oxide semiconductor can be made deeper with respect to the vacuum level. In addition, the field effect mobility (simply called mobility, or μ Specifically, the current of the transistor 100 can be increased by Field effect mobility is 10 cm 2 / Vs, and more preferably the electric field of the transistor 100 Effective mobility is 30cm 2 / Vs can be exceeded.

[0134] For example, the above-mentioned high field effect mobility transistor is used as a gate driver for generating a gate signal. A driver (especially a demux connected to the output terminal of a shift register of a gate driver) By using it in a semiconductor device or display device with a narrow frame (also called a narrow frame), Locations can be provided.

[0135] In addition, since the transistor 100 includes the oxide semiconductor 108b, The oxide semiconductor 108b is a semiconductor having a thickness of 100 nm and a thickness of 100 nm. Since the atomic ratio of In is smaller than that of oxide semiconductor 108a, the oxide semiconductor Therefore, the amount of light absorbed by the oxide semiconductor during light irradiation can be reduced. Therefore, the oxide semiconductor 108a and the oxide semiconductor 10 By forming a laminated structure with 8b, the resistance to negative bias light stress testing is increased. do.

[0136] The insulators 114 and 116 are regions containing oxygen in excess of the stoichiometric composition (oxygen In other words, the insulators 114 and 116 preferably have an oxygen excess region. The insulating film is capable of releasing oxygen. To achieve this, for example, oxygen is introduced into the insulators 114 and 116 after deposition to form an oxygen excess region. The oxygen introduction method includes ion implantation, ion doping, plasma immersion, etc. The insulators 114 and 116 may be formed by a method such as a ion implantation method or a plasma treatment. The released oxygen diffuses into the oxide semiconductor 108a and compensates for oxygen vacancies in the oxide semiconductor 108a. It can be filled.

[0137] In order to compensate for oxygen vacancies in the oxide semiconductor 108a, the oxide semiconductor 108b It is preferable to make the film thickness in the vicinity of the channel region of the oxide semiconductor 108b thinner. The film thickness in the vicinity of the channel region is preferably 1 nm or more and 20 nm or less, and more preferably is 3 nm or more and 10 nm or less.

[0138] In order to compensate for oxygen vacancies in the oxide semiconductor 108a, the oxide semiconductor 108b The oxide semiconductor 108b preferably has high oxygen permeability. This allows excess oxygen contained in the insulators 114 and 116 to be suitably transmitted into the oxide semiconductor 108a. It can be passed.

[0139] In this manner, in the semiconductor device of one embodiment of the present invention, oxide semiconductors have a stacked-layer structure, In addition, by using a structure in which excess oxygen is contained in the insulator in contact with the oxide semiconductor, In addition, in one embodiment of the present invention, a semiconductor device having the above structure can be provided. The temperature during the manufacturing process of the semiconductor device is low (typically less than 400° C. or 375° C. The temperature can be set to less than 340° C. and preferably to 360° C.

[0140] Other components included in the semiconductor device of this embodiment will be described in detail below. do.

[0141] <Substrate> There is no particular restriction on the material of the substrate 102, but it should be strong enough to withstand the subsequent heat treatment. For example, glass substrates, ceramic substrates, quartz substrates, and sa A fire substrate or the like may be used as the substrate 102. Also, a material such as silicon or silicon carbide may be used. Single crystal semiconductor substrates, polycrystalline semiconductor substrates, compound semiconductors such as silicon germanium, etc. It is also possible to use a substrate, an SOI substrate, or the like, on which a semiconductor element is provided. The substrate 102 may be a glass substrate. When using large area substrates such as 6th generation, 7th generation, 8th generation, 9th generation, and 10th generation, By using such a large-area substrate, a large display device can be manufactured. This is preferable because it is possible to reduce the manufacturing cost.

[0142] In addition, a flexible substrate is used as the substrate 102, and the transistor 10 is directly formed on the flexible substrate. Alternatively, a peeling layer may be provided between the substrate 102 and the transistor 100. The release layer is preferably removed from the substrate 102 after a semiconductor device is partially or entirely completed thereon. The transistor 100 can be separated and transferred to another substrate. It can also be transferred to substrates with poor thermal properties or flexible substrates.

[0143] <Conductors that function as gate electrodes, source electrodes, and drain electrodes> A conductor 104 that functions as a gate electrode and a conductor 112 that functions as a source electrode. The conductive material 112b serving as the drain electrode is made of chromium (Cr), copper (C u), aluminum (Al), gold (Au), silver (Ag), zinc (Zn), molybdenum (M o), Tantalum (Ta), Titanium (Ti), Tungsten (W), Manganese (Mn), Ni A metal element selected from nickel (Ni), iron (Fe), and cobalt (Co), or the above The alloys are made of metal elements or alloys combining the above metal elements. It can be formed.

[0144] The conductors 104, 112a, and 112b may have a single-layer structure or a laminated structure of two or more layers. For example, a single layer structure of an aluminum film containing silicon, titanium on an aluminum film, A two-layer structure in which a titanium film is laminated on a titanium nitride film, a two-layer structure in which a titanium film is laminated on a titanium nitride film, a titanium nitride film A two-layer structure in which a tungsten film is laminated on top of a tantalum nitride film or a tungsten nitride film A two-layer structure in which a tungsten film is laminated, a titanium film, and an aluminum film is laminated on the titanium film. There are three-layer structures, such as a titanium film on top of an aluminum film. Select from tantalum, tungsten, molybdenum, chromium, neodymium, and scandium. Alternatively, an alloy film or a nitride film made by combining one or more of these may be used.

[0145] The conductors 104, 112a, and 112b are made of indium tin oxide or tungsten oxide. Indium oxide containing tungsten oxide, indium zinc oxide containing tungsten oxide, titanium oxide Indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc oxide A conductive material having light transmitting properties, such as indium tin oxide doped with silicon oxide, is used. It is also possible.

[0146] The conductors 104, 112a, and 112b are made of a Cu-X alloy film (X is Mn, Ni, Cr, Fe, Co, Mo, Ta, or Ti) may be applied. This allows processing using a wet etching process, which reduces manufacturing costs. It becomes possible.

[0147] <Insulator that functions as a gate insulator> The insulators 106a and 106b functioning as the gate insulators of the transistor 100 include , Plasma Enhanced Chemical Vapor Deposition (PECVD) The oxide film is formed by the thermal vapor deposition (CVD) method, sputtering method, etc. Silicon film, silicon oxynitride film, silicon nitride oxide film, silicon nitride film, aluminum oxide film, hafnium oxide film, yttrium oxide film, zirconium oxide film, gallium oxide film, Tantalum oxide film, magnesium oxide film, lanthanum oxide film, cerium oxide film and neodymium oxide film The insulating layer may be made of one or more types of zinc film. Instead of the laminated structure of 106b, a single insulating film selected from the above-mentioned materials or three or more insulating films may be used. The insulating film may be used.

[0148] The insulator 106a also functions as a blocking film that suppresses the permeation of oxygen. For example, excess ZnO in the insulators 106b, 114, 116 and / or the oxide semiconductor 108 may be present. When oxygen is supplied, the insulator 106a can suppress the permeation of oxygen.

[0149] Note that the oxide semiconductor 108 functioning as a channel region of the transistor 100 The insulator 106b is preferably an oxide insulating film, and is preferably made of an oxide having a stoichiometric composition. It is more preferable that the insulator 1 has a region containing oxygen (an oxygen excess region). The insulator 106b is an insulating film capable of releasing oxygen. To provide the region, for example, the insulator 106b may be formed in an oxygen atmosphere. Alternatively, oxygen may be introduced into the insulator 106b after deposition to form an oxygen excess region. The implantation methods include ion implantation, ion doping, and plasma immersion ion implantation. A method such as a plasma treatment can be used.

[0150] Furthermore, when hafnium oxide is used as the insulator 106b, the following effects are obtained. Hafnium nitride has a higher dielectric constant than silicon oxide and silicon oxynitride. In comparison with the case where silicon oxide is used, the thickness of the insulator 106b can be made larger, so that the thickness of the insulator 106b can be made larger. This reduces the leakage current due to the transistor current. Furthermore, hafnium oxide, which has a crystalline structure, can be used to realize an amorphous It has a higher dielectric constant than hafnium oxide, which has a structure. Therefore, the off-current is small. To make a small transistor, it is preferable to use hafnium oxide having a crystalline structure. Examples of the crystal structure include monoclinic and cubic. An embodiment is not limited to these.

[0151] In this embodiment, a silicon nitride film is formed as the insulator 106a, and the insulator 10 A silicon oxide film is formed as 6b. The silicon nitride film is comparatively Because of its high dielectric constant and the large film thickness required to obtain the same capacitance as a silicon oxide film, The gate insulator of the transistor 100 is made of a silicon nitride film. Therefore, the decrease in the dielectric strength of the transistor 100 can be suppressed. Furthermore, the dielectric strength can be improved, and electrostatic breakdown of the transistor 100 can be suppressed. .

[0152] <Oxide semiconductor> The oxide semiconductor 108a and the oxide semiconductor 108b may be, for example, the indium oxide semiconductor shown above. For example, a material containing In, an element M, and zinc can be used. In the case of In-M-Zn oxide, the sputtering method used to deposit the In-M-Zn oxide film The atomic ratio of the metal elements in the target preferably satisfies In≧M and Zn≧M. The atomic ratio of metal elements in such a sputtering target is In:M:Zn=1:1. :1, In:M:Zn=1:1:1.2, In:M:Zn=2:1:3, In:M:Zn In:M:Zn=3:1:2, and In:M:Zn=4:2:4.1. In the case of In-M-Zn oxide, the sputtering target is polycrystalline In-M It is preferable to use a target containing In-M-Zn oxide. By using a target containing arsenic, the oxide semiconductor 108 having crystallinity can be easily formed. The atomic ratio of the oxide semiconductor 108 to be formed is determined by the above sputtering method as an error. This includes a ±40% variation in the atomic ratio of metal elements contained in the ring target. For example, a sputtering target with an atomic ratio of In:Ga:Zn=4:2:4. In the case of using the oxide semiconductor 108 having the structure shown in FIG. 1, the atomic ratio of In:Ga:Zn is 4: In some cases, the ratio may be around 2:3.

[0153] For example, the oxide semiconductor 108a may be the above-mentioned In:M:Zn=2:1:3, In: Sputtering targets such as M:Zn=3:1:2, In:M:Zn=4:2:4.1 The oxide semiconductor 108a is preferably formed using a composition containing In:M:Zn=4: It is preferable that the ratio of the number of atoms is α1 (1.5≦α1≦2.5):α2 (2.5≦α2≦3.5). I wish.

[0154] The oxide semiconductor 108b may be the above-mentioned In:M:Zn=1:1:1, In:M : It may be formed using a sputtering target such as Zn=1:1:1.2. Preferably the oxide semiconductor 108b has an atomic ratio of In:M:Zn = 1:β1 (0.8 ≤ β1 ≤ 1.2): β2 (0.8 ≤ β2 ≤ 1.2). Note that for the atomic ratio of the metal elements of the sputtering target used for the oxide semiconductor 108b, it is not necessary to satisfy In ≥ M and Zn ≥ M, and a composition satisfying In ≥ M and Zn < M may be used. Specifically, examples include In:M:Zn = 1:3:2, In:M:Zn = 1:3:4, In:M:Zn = 1:3:6, etc.

[0155] Also, by using an oxide semiconductor with a wide energy gap as the oxide semiconductor 108a and the oxide semiconductor 108b, the off-current of the transistor 100 can be reduced. Moreover, it is preferable that the energy gap of the oxide semiconductor 108b is larger than that of the oxide semiconductor 108a. The energy gap of the oxide semiconductor 108b is preferably 0.15 eV or more, or 0.5 eV or more, and 2 eV or less, or 1 eV or less larger than that of the oxide semiconductor 108a. It is preferable to use the following oxide semiconductor films.

[0156] Also, the thicknesses of the oxide semiconductor 108a and the oxide semiconductor 108b are each 3 nm or more and 200 nm or less, preferably 3 nm or more and 100 nm or less, more preferably 3 nm or more and 50 nm or less.

[0157] As the oxide semiconductor 108b, an oxide semiconductor film with a low carrier density is used. For example, the oxide semiconductor 108b preferably has a carrier density of less than 1×10 15 / cm 3 and more preferably less than 1×10 13 ​​​​​​​​​ / cm 3 less than 1×10 11 / cm 3 Less than, More preferably, 1×10 9 / cm 3 It is sufficient to set it to less than.

[0158] Note that the oxide semiconductors 108a and 108b each contain By using an oxide semiconductor film with a low defect level and a low density of defect states, it is possible to obtain better electrical characteristics. The impurities are preferably hydrogen, nitrogen, or aluminum. Examples include potassium metal and alkaline earth metals.

[0159] The oxide semiconductor film has a significantly small off-state current and a channel width W of 1×10 6 Channel in μm Even if the length L of the element is 10 μm, the voltage between the source and drain electrodes (drain voltage ) in the range of 1V to 10V, the off-state current is within the measurement limit of the semiconductor parameter analyzer. below the boundary, i.e. 1×10 -13 It is possible to obtain a characteristic of A or less.

[0160] In addition, the oxide semiconductor 108a has a portion with a lower hydrogen concentration than the oxide semiconductor 108b. The oxide semiconductor 108a may have a lower hydrogen concentration than the oxide semiconductor 108b. By having a portion free of such a defect, a highly reliable semiconductor device can be realized in some cases.

[0161] In addition, the oxide semiconductor 108a contains silicon or carbon, which is one of the Group 14 elements. When the oxide semiconductor 108a is filled with the fluorine atom, oxygen vacancies are increased in the oxide semiconductor 108a, causing the oxide semiconductor 108a to become n-type. Therefore, the concentrations of silicon and carbon in the oxide semiconductor 108a and the oxide semiconductor 108b are The concentration of silicon and carbon near the interface (obtained by SIMS analysis) was 2×10 18 atoms / cm 3 Less than or equal to 2×10 17 atoms / cm 3 The following applies.

[0162] In addition, in the oxide semiconductor 108a, an alkali metal or is the concentration of alkaline earth metals, 1×10 18 atoms / cm 3 Below, preferably 2 x 1 0 16 atoms / cm 3 Alkali metals and alkaline earth metals are oxide semiconductors. When it bonds with a conductor, it can generate carriers, which increases the off-state current of the transistor. For this reason, the alkali metal or alkaline earth metal of the oxide semiconductor 108a is It is preferable to reduce the concentration of the genus.

[0163] In addition, when the oxide semiconductor 108a contains nitrogen, electrons that serve as carriers are generated, and The carrier density increases and the n-type is easily formed. As a result, if the nitrogen content is too high, the oxide semiconductor A transistor using a conductor film may have an excessive negative shift. In the conductive film, it is preferable that the nitrogen content is reduced as much as possible. For example, SIMS analysis The nitrogen concentration obtained by the precipitation is 5×10 18 atoms / cm 3 The following is the result.

[0164] The oxide semiconductors 108a and 108b each have a non-single crystal structure. The non-single crystal structure may be, for example, a CAAC-OS (C Axis Aligned Array) structure, which will be described later. ed Crystalline Oxide Semiconductor), polycrystalline structure Among non-single crystal structures, the amorphous structure is the most defective. The defect level density is high in CAAC-OS, while the defect level density is the lowest in CAAC-OS.

[0165] <Band structure 2> In FIG. 14A, an oxide semiconductor 108a and an oxide The band structure in the case of using the semiconductor 108b is shown in FIG. The description of the electric conductor 104 is omitted.

[0166] FIG. 14A illustrates an insulator 106b, an oxide semiconductor 108a, an oxide semiconductor 108b, and a 1 is an example of a band structure in the thickness direction of a laminated structure having an insulating layer 114 and an insulating layer 114. For ease of understanding, the structure is shown as an insulator 106b, an oxide semiconductor 108a, and an oxide semiconductor 10 8b, and the energy level (Ec) of the conduction band minimum of the insulator 114.

[0167] In the band structure shown in FIG. 14(A), oxides are used as insulators 106b and 114. A silicon film is used as the oxide semiconductor 108a, and the atomic ratio of metal elements is In:Ga:Zn The oxide semiconductor film was formed using a metal oxide target having a ratio of 4:2:4.1. The compound semiconductor 108b is a gold compound semiconductor having an atomic ratio of In:Ga:Zn=1:1:1.2. FIG. 1 is a band diagram of a configuration using a metal oxide film formed using a metal oxide target.

[0168] As shown in FIG. 14A, in the oxide semiconductor 108a and the oxide semiconductor 108b, In other words, the energy level at the bottom of the conduction band changes smoothly. In order to have such a band structure, the oxide At the interface between the semiconductor 108a and the oxide semiconductor 108b, trap centers and recombination centers Assume that there are no impurities that would form such defect levels.

[0169] In order to form a continuous junction between the oxide semiconductor 108a and the oxide semiconductor 108b, Using a multi-chamber deposition system (sputtering system) equipped with a lock chamber, Each film can be laminated in succession without being exposed to the air. Each chamber is sealed to remove water and other impurities as much as possible. A high vacuum (5×10 -7 Pa~1×10 -4 It is preferable to evacuate the inside of the chamber to a temperature of about 10 Pa. Alternatively, a turbo molecular pump and a cold tra A combination of a gas pump and a gas pumping system is used to pump gas, especially gas containing carbon or hydrogen, into the chamber from the exhaust system. It is preferable to prevent backflow.

[0170] In the structure shown in FIG. 14A, the oxide semiconductor 108a serves as a well. In the transistor using the above stacked structure, a channel region is formed in the oxide semiconductor 108a. It is clear that this will be achieved.

[0171] When the oxide semiconductor 108b is not formed, the oxide semiconductor 108a has a defect state. On the other hand, by forming the above-described stacked structure, the defect states can be formed in the oxide semiconductor 1. Therefore, defect states can be separated from the oxide semiconductor 108a. Cut.

[0172] In addition, the defect level is at the bottom of the conduction band of the oxide semiconductor 108a that functions as a channel region. The electrons can accumulate in the defect levels, which can be farther from the vacuum level than the energy level (Ec). When electrons accumulate in the defect level, they become negative fixed charges, causing The threshold voltage of the transistor is shifted in the positive direction. The energy level (Ec) of the conduction band minimum of the semiconductor 108a is closer to the vacuum level. This structure makes it difficult for electrons to accumulate in the defect level, It is possible to increase the on-current of the transistor and also to increase the field effect mobility. This can be done.

[0173] In addition, in FIG. 14A, the oxide semiconductor 108b has a higher conductivity than the oxide semiconductor 108a. The energy level of the conduction band minimum is close to the vacuum level. The energy level of the conduction band minimum of the oxide semiconductor 108b is The difference is 0.15 eV or more, or 0.5 eV or more and 2 eV or less, or 1 eV or less. That is, the electron affinity of the oxide semiconductor 108b and the electron affinity of the oxide semiconductor 108a are The difference between the sum force is 0.15 eV or more, or 0.5 eV or more and 2 eV or less, or 1 e V or less.

[0174] With such a structure, the oxide semiconductor 108a serves as a main path for current, and The oxide semiconductor 108b functions as a channel region. The oxide semiconductor film 108a is made of one or more metal elements. Therefore, interface scattering occurs at the interface between the oxide semiconductor 108a and the oxide semiconductor 108b. Therefore, the movement of carriers is not hindered at the interface, and the transistor The field effect mobility of

[0175] In addition, the oxide semiconductor 108b is formed by using a SiO 2 film to prevent the oxide semiconductor 108b from functioning as part of the channel region. For this reason, a material having a sufficiently low electrical conductivity is used for the oxide semiconductor 108b. The electron affinity (the difference between the vacuum level and the energy level at the bottom of the conduction band) is higher than that of the oxide semiconductor 108a. The energy level of the conduction band minimum is smaller than that of the oxide semiconductor 108a. The material used has a band offset with respect to the drain voltage. In order to suppress the occurrence of a difference in threshold voltage depending on the magnitude of the voltage, an oxide semiconductor The energy level of the conduction band minimum of the oxide semiconductor 108b is lower than that of the oxide semiconductor 108a. It is preferable to use a material having a vacuum level closer to the Vcc level than the Vcc level. For example, the oxide semiconductor 108 The energy level of the conduction band minimum of oxide semiconductor 108a and oxide semiconductor 108c is The difference between the energy level of the fluorine-containing compound and the fluorine-containing compound is preferably 0.2 eV or more, more preferably 0.5 eV or more. stomach.

[0176] In FIG. 14B, the insulator 106b has an energy E 01 A field with a defect level located at The band diagram for the case is shown below. Energy E 01 and the bottom of the conduction band of the oxide semiconductor 108a. Energy E x Here, the energy E x E 01 is the conduction band of the oxide semiconductor 108a. It takes a positive value when the energy is higher than the lower limit of the energy range, i.e., closer to the vacuum level. -E x is preferably 0.01 eV or more and 1.2 eV or less, and more preferably 0.2 eV or more and 1.0 eV or less. More preferably, 0.3 eV or more and 0.8 eV or less are further preferable, and 0.5 eV or more and 0. More preferably, it is 8 eV or less.

[0177] When a silicon oxide film or a silicon oxynitride film is used as the insulator 106b, In this case, E 01 For example, the defect level shown in FIG. Si-H-Si(+ / 0) is approximately 3.1 eV from the conduction band of the insulator 106b and approximately 4.0 eV from the vacuum level. Therefore, the electron affinity of the oxide semiconductor 108a is greater than or equal to 4.01 eV and less than or equal to 5.2 eV. Preferably, the value is 4.2 eV or more and 5.0 eV or less, more preferably, 4.4 eV or more and 4.8 eV or less. V or less is more preferable, and 4.5 eV to 4.8 eV is even more preferable.

[0178] It is preferable that the oxide semiconductor 108b not have a spinel crystal structure. In the case where the oxide semiconductor 108b contains a spinel crystal structure, the spinel crystal structure At the interface between the structure and other regions, the constituent elements of the conductors 112a and 112b are the oxide semiconductor 1 In addition, when the oxide semiconductor 108b is a CAAC- In the case of OS, blocking of the constituent elements of the conductors 112a and 112b, for example, copper elements This is preferable as it increases the efficiency.

[0179] The thickness of the oxide semiconductor 108b is determined by determining whether the constituent elements of the conductors 112a and 112b are oxide semiconductors. The thickness of the insulating film 114 is thick enough to prevent the diffusion of oxygen from the insulating film 114 to the insulating film 108a. For example, the thickness of the oxide semiconductor 108a is set to be less than the thickness at which the supply of oxygen to the oxide semiconductor 108a is suppressed. When the thickness of the conductive layer 112a and 112b is 10 nm or more, the constituent elements of the conductive layers 112a and 112b are oxide semiconductors. The diffusion of the oxide semiconductor 108b into the conductor 108a can be suppressed. When the thickness is set to 100 nm or less, the insulators 114 and 116 can be effectively transferred to the oxide semiconductor 108a. Oxygen can be supplied.

[0180] <Insulator that functions as a protective insulating film for transistors> The insulators 114 and 116 have a function of supplying oxygen to the oxide semiconductor 108. The insulator 118 functions as a protective insulating film for the transistor 100. The insulators 114 and 116 contain oxygen. The insulator 114 is also permeable to oxygen. The insulator 114 is an insulating film. The insulator 114 is formed by oxidation when the insulator 116 is formed later. It also functions as a film for reducing damage to the compound semiconductor 108 .

[0181] The insulator 114 has a thickness of 5 nm or more and 150 nm or less, preferably 5 nm or more and 50 Silicon oxide, silicon oxynitride, etc., having a thickness of 1 nm or less can be used.

[0182] In addition, it is preferable that the insulator 114 has a small amount of defects. Typically, the insulator 114 has a small amount of defects as determined by ESR measurement. The spin density of the signal at g=2.001 originating from the silicon dangling bond is 3×10 17 spins / cm 3 This is because the insulator 114 is preferably If the defect density is high, oxygen will bind to the defects, and the oxygen in the insulator 114 will The amount of transmission of the light is reduced.

[0183] In the insulator 114, all of the oxygen that has entered the insulator 114 from the outside is absorbed in the insulator 114. Some oxygen does not move to the outside of the insulator 114 and remains in the insulator 114. At the same time, oxygen contained in the insulator 114 moves to the outside of the insulator 114, In some cases, oxygen transfer may occur in the body 114. When the oxide insulating film capable of forming the insulating film is formed, the insulating film 116 provided on the insulating film 114 is The desorbed oxygen can be transferred to the oxide semiconductor 108 through the insulator 114.

[0184] The insulator 114 can be formed using an oxide insulating film having a low density of nitrogen oxide levels. Note that the density of the nitrogen oxide level can be determined by the energy level at the upper end of the valence band of the oxide semiconductor film. Energy (E V_OS ) and the conduction band edge energy (E C_OS )and The oxide insulating film may be formed between the first and second insulating films. Silicon oxynitride film or aluminum oxynitride film that emits less nitrogen oxide is used. There can be.

[0185] In addition, the silicon oxynitride film, which emits a small amount of nitrogen oxide, is This membrane releases more ammonia than nitrogen oxides, and typically releases ammonia. The amount of molecules released is 1×10 18 molecule / cm 3 5×10 or more 19 molecule / cm 3 The following is the result. The amount of ammonia released is determined when the surface temperature of the membrane is 50°C or higher and 650°C or lower, preferably 50°C or lower. The amount released is determined by heat treatment at or above 550°C or below.

[0186] Nitrogen oxides (NO x , x is greater than 0 and less than or equal to 2, preferably greater than or equal to 1 and less than or equal to 2), typically NO or NO forms a level in the insulator 114. The nitroxide is located within the energy gap of the insulator 114 and the When the oxide semiconductor 108 is diffused to the interface, the level causes electrons to be transferred to the insulator 114. As a result, the trapped electrons may be transported between the insulator 114 and the oxide semiconductor. 108The threshold voltage of the transistor is shifted in the positive direction because it remains near the interface. Put away.

[0187] Nitrogen oxides also react with ammonia and oxygen during the heat treatment. The nitrogen oxide contained in the insulator 116 reacts with the ammonia contained in the insulator 116 during the heat treatment. Therefore, the nitrogen oxides contained in the insulator 114 are reduced. Electrons are less likely to be trapped at the interface between the oxide semiconductor 106 and the oxide semiconductor 108.

[0188] The insulator 114 is formed using an oxide insulating film having a low density of states due to nitrogen oxide. Note that the density of states caused by the nitrogen oxides can be determined by the valence electrons of the oxide semiconductor. The energy of the upper edge of the conduction band (Ev_os) and the energy of the lower edge of the conduction band of an oxide semiconductor (Ec By using the oxide insulating film, It is possible to reduce the shift in the threshold voltage of the transistor, and the fluctuation in the electrical characteristics of the transistor can be reduced.

[0189] Heat treatment in the manufacturing process of a transistor is typically performed at a temperature of less than 400° C. or less than 375° C. By the heat treatment at 300° C. or more (preferably, 340° C. or more and 360° C. or less), the insulator 114 is heated to 10 In the spectrum obtained by ESR measurement below 0 K, the g value is 2.037 or more and 2.03 a first signal with a g value of 0.9 or less, a second signal with a g value of 0.25 or more and 0.3 or less, and A third signal with a g value between 1.964 and 1.966 is observed. The split width of the null and the second signal, and the split width of the second signal and the third signal The split width is about 5 mT in the X-band ESR measurement. The g value is 2.037. The first signal has a g value of 2.039 or more, and the second signal has a g value of 2.001 or more, and The sum of the spin densities of the third signal with g values ​​between 1.964 and 1.966 The total is 1 x 10 18 spins / cm 3 is less than 1×10 17 spins / cm 3 More than 1×10 18 spins / cm 3 is less than.

[0190] In addition, the g value in the ESR spectrum below 100K is 2.037 to 2.039. The first signal has a g value of 2.001 to 2.003, and the second signal has a g value of 1 The third signal, between .964 and 1.966, is nitrogen oxide (NO x , x is greater than 0 Representative examples of nitrogen oxides are: Examples include nitrogen monoxide and nitrogen dioxide. That is, the g value is between 2.037 and 2.039. a first signal having a g value of 2.001 to 2.003, and a second signal having a g value of The lower the sum of the spin densities of the third signals between 1.964 and 1.966, the more acidic the signal is. This means that the nitride insulating film contains a small amount of nitrogen oxide.

[0191] The oxide insulating film has a nitrogen concentration of 6×10 20 atoms / cm 3 The following is the result.

[0192] The substrate temperature is between 220℃ and 350℃, and PEC using silane and nitrous oxide is used. By forming the oxide insulating film using a VD method, a dense and hard film can be formed. It can be formed.

[0193] The insulator 116 is an oxide insulating film containing more oxygen than the oxygen that satisfies the stoichiometric composition. The oxide insulating film containing more oxygen than the stoichiometric composition is formed using When heated, some of the oxygen is released. The oxygen content is greater than the stoichiometric composition. The oxide insulating film had a release of oxygen of 1.0×10 in terms of oxygen atoms as determined by TDS analysis. 1 9 atoms / cm 3 More than 3.0×10 20 atoms / cm 3 That's all. The oxide insulating film is a thin film. The surface temperature of the film during the TDS analysis was 100°C or less. The temperature range is preferably from 100° C. to 500° C. or from 100° C. to 700° C.

[0194] The insulator 116 has a thickness of 30 nm or more and 500 nm or less, preferably 50 nm or more. Silicon oxide, silicon oxynitride, etc., having a thickness of 400 nm or less can be used.

[0195] In addition, it is preferable that the insulator 116 has a small amount of defects. Typically, the insulator 116 has a small amount of defects as determined by ESR measurement. The spin density of the signal at g=2.001 originating from the silicon dangling bond is 1.5×10 18 spins / cm 3 Less than or even 1×10 18 spins / cm 3 It is preferable that the insulator 116 is an oxide semiconductor as compared with the insulator 114. Because it is farther away from the body 108 , it may have a higher defect density than the insulator 114 .

[0196] In addition, the insulators 114 and 116 can be made of insulating materials of the same kind. In some cases, the interface between the body 114 and the insulator 116 may not be clearly visible. In this embodiment, the interface between the insulator 114 and the insulator 116 is shown by a dashed line. In the embodiment, the two-layer structure of the insulator 114 and the insulator 116 has been described. For example, the insulator 114 or the insulator 116 may have a single-layer structure, without being limited thereto.

[0197] The insulator 118 is a blocking material for oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. By providing the insulator 118, oxygen from the oxide semiconductor 108 can be prevented from being generated. The diffusion of oxygen from the insulators 114 and 116 to the outside and the diffusion of oxide from the outside It is possible to prevent hydrogen, water, etc. from entering the semiconductor 108. The insulator 118 is, for example, For example, a nitride insulating film can be used. Examples of the nitride insulating film include silicon nitride, nitride, and the like. Silicon oxide, aluminum nitride, aluminum oxide nitride, etc. When a silicon oxynitride or silicon nitride film is used as the material 8, the diffusion of oxygen to the outside can be prevented. This is preferable because it can suppress the

[0198] It also has a blocking effect against oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. Instead of a nitride insulating film, an oxide insulating film having a blocking effect against oxygen, hydrogen, water, and the like is used. may be provided as the insulator 118. The insulating film may be aluminum oxide, aluminum oxynitride, gallium oxide, or oxynitride. Gallium, yttrium oxide, yttrium oxynitride, hafnium oxide, hafnium oxynitride As an oxide insulating film having a blocking effect against oxygen, hydrogen, water, and the like, is particularly preferably aluminum oxide, hafnium oxide, or yttrium oxide. .

[0199] The above-mentioned various films such as conductors, insulators, and oxide semiconductors can be formed by sputtering. It can be formed by the PECVD method, but other methods such as thermal CVD (Chemical CVD) are also possible. Chemical Vapor Deposition (ALD) method or Atomic Laser Deposition (ALD) method As an example of a thermal CVD method, MO CVD(Metal Organic Chemical Vapor Deposit) Examples include the ion method.

[0200] Thermal CVD is a film formation method that does not use plasma, so defects can occur due to plasma damage. This has the advantage that no additional steps are required.

[0201] In the thermal CVD method, the source gas and the oxidizing agent are fed into the chamber at the same time, and the chamber is heated to atmospheric pressure. Alternatively, a film is formed by reacting the reactants near or on the substrate under reduced pressure and depositing the reactants on the substrate. You may go.

[0202] In addition, in the ALD method, the pressure inside the chamber is set at atmospheric pressure or reduced pressure, and the source gas for the reaction is The gases may be introduced into the chamber in sequence, and the film may be formed by repeating the gas introduction sequence. For example, by switching between two or more switching valves (also called high-speed valves), The source gases are sequentially supplied to the chamber, and the first source gas is supplied to the chamber so as not to mix the source gases. Inert gas (argon, nitrogen, etc.) is introduced simultaneously with or after the feed gas. In addition, when an inert gas is introduced at the same time, the inert gas is The second source gas may be introduced simultaneously with the introduction of the inert gas. Also, instead of introducing an inert gas, the first source gas is discharged by evacuation. The first source gas is adsorbed on the surface of the substrate to form a first layer. The second layer is deposited on the first layer by reacting with the second source gas introduced later. This process is repeated several times while controlling the gas introduction sequence until a thin film of the desired thickness is formed. By doing so, a thin film with excellent step coverage can be formed. The thickness of the thin film depends on the order of gas introduction. The thickness can be precisely adjusted by changing the number of times the process is repeated. This is suitable for producing thin FETs.

[0203] Thermal CVD methods such as MOCVD can be used to deposit the conductors, insulators, oxide semiconductors, and metals described above. It is possible to form various films such as metal oxide films. For example, an In-Ga-ZnO film can be formed. In some cases, trimethylindium, trimethylgallium, and dimethylzinc are used. The chemical formula for trimethylindium is In(CH3)3. The chemical formula for zinc is Ga(CH3)3. The chemical formula for dimethylzinc is Zn(C H3)2. In addition, the combination is not limited to these, and instead of trimethylgallium, Triethylgallium (chemical formula Ga(C2H5)3) can also be used, and dimethylzinc Alternatively, diethylzinc (chemical formula Zn(C2H5)2) can be used.

[0204] For example, when forming a hafnium oxide film using a film forming apparatus that uses ALD, the solvent and liquids containing hafnium precursor compounds (hafnium alkoxides, tetrakisdimethylamine, etc.) The raw material gas is vaporized hafnium amide (TDMAH, etc.) and oxidized Two types of gases are used: tetrakisdimethylamide hafnium (TDA) and ozone (O3). The chemical formula for nium is Hf[N(CH3)2]4. Other materials include tetrahydrofuran. Examples include kis(ethylmethylamido)hafnium.

[0205] For example, when forming an aluminum oxide film using an ALD deposition system, A liquid containing a catalyst and an aluminum precursor compound (e.g., trimethylaluminum (TMA)) is added. Two types of gases are used: vaporized source gas and H2O as an oxidizing agent. The chemical formula for aluminum is Al(CH3)3. Other liquid materials include Tris( Dimethylamido)aluminum, triisobutylaluminum, aluminum tris(2 ,2,6,6-tetramethyl-3,5-heptanedionate).

[0206] For example, when forming a silicon oxide film using a deposition system that uses ALD, Chlorodisilane is adsorbed onto the surface to be coated, the chlorine contained in the adsorbed matter is removed, and the oxidizing gas (O 2. Nitrous oxide (NO) radicals are supplied to react with the adsorbed material.

[0207] For example, when forming a tungsten film using an ALD deposition system, WF6 The initial tungsten film was formed using B2H6 gas and WF6 gas, and then H2 gas. A tungsten film is formed using SiH4 gas instead of B2H6 gas. This is also fine.

[0208] For example, an oxide semiconductor film, such as In-Ga-ZnO, can be formed by a film formation apparatus using ALD. When forming a film, an In-O layer is formed using In(CH3)3 gas and O3 gas, Then, a Ga-O layer was formed using Ga(CH3)3 gas and O3 gas, and then Zn The Zn-O layer is formed using (CH3)2 gas and O3 gas. The order of these layers is The present invention is not limited to this example. In addition, In-Ga-O layers, In-Zn-O layers, A mixed compound layer such as Ga-Zn-O layer may be formed. It is also possible to use H2O gas obtained by bubbling water with an inert gas containing H It is preferable to use O3 gas. Also, instead of In(CH3)3 gas, In(C2H 5)3 gas may be used. Also, Ga(C2H5) 3 gas may be used. Also, Zn(CH3)2 gas may be used.

[0209] Next, a configuration example different from that of the transistor 100 shown in FIGS. 5(A)(B) will be used for the explanation. Note that if the function is the same as that described above, have the same hatch pattern and may not be specifically numbered.

[0210] FIG. 15A is a top view of a transistor 170 which is a semiconductor device of one embodiment of the present invention. FIG. 15B is a cross section taken along dashed line X1-X2 in FIG. 15(A) along dashed line Y1-Y2.

[0211] The transistor 170 includes a conductor 104 on the substrate 102 that serves as a first gate electrode. , an insulator 106a on the substrate 102 and the conductor 104, and an insulator 106a on the insulator 106a. 6b, the oxide semiconductor 108 on the insulator 106b, and the insulator 11 on the oxide semiconductor 108. 4, an insulator 116 on the insulator 114, and a source electrically connected to the oxide semiconductor 108. A conductor 112a serving as a drain electrode and a drain electrically connected to the oxide semiconductor 108 are The conductor 112b functions as an insulator electrode, the insulator 118 on the insulator 116, and the insulator 1 The insulator 118 has a conductor 120a thereon and the insulator 118 has a conductor 120b thereon. 4, 116, and 118 function as the second gate insulator of transistor 170. The conductor 120a is also provided through the openings 142c in the insulators 114, 116, and 118. The transistor 170 is electrically connected to the conductor 112b through The conductor 120a functions as, for example, a pixel electrode used in a display device. In the transistor 170, the conductor 120b is a second gate electrode (a back gate electrode). It functions as a

[0212] As shown in FIG. 15B, the conductor 120b is made of insulators 106a, 106b, and 11 In the openings 142a and 142b provided in the first gate electrodes 114, 116 and 118, Therefore, the conductor 120b and the conductor 104 are , the same potential is applied.

[0213] In this embodiment, openings 142a and 142b are provided, and the conductor 120b and Although the configuration in which the conductor 104 is connected has been illustrated, the present invention is not limited to this. For example, Only one of the openings, 142a or 142b, is formed, and the conductor 120b and A configuration in which the conductor 104 is connected, or a configuration in which the conductor 104 is not provided with the openings 142a and 142b, The conductor 120b and the conductor 104 may not be connected to each other. In the case where the conductor 104 is not connected, the conductor 120b and the conductor 104 are each connected to a different It is possible to apply a voltage to the

[0214] As shown in FIG. 15B, the oxide semiconductor 108 functions as a first gate electrode. The conductor 104 functions as a first gate electrode, and the conductor 120b functions as a second gate electrode. The second gate is sandwiched between two conductors that function as gate electrodes. The length in the channel length direction and the length in the channel width direction of the conductor 120b functioning as a gate electrode are The length of the oxide semiconductor 108 is larger than the length in the channel length direction and the length in the channel width direction. The oxide semiconductor 108 is generally a conductor with insulators 114, 116, and 118 interposed therebetween. The first gate electrode 120b is covered with the conductor 120b. The conductor 104 functioning as the gate electrode of the 16, 118 are connected through openings 142a, 142b. The side surface of the conductor 108 in the channel width direction is connected to the second gate via insulators 114, 116, and 118. It faces the conductor 120b which functions as a base electrode.

[0215] In other words, in the channel width direction of the transistor 170, The functional conductor 104 and the conductor 120b acting as the second gate electrode are the first gate. Insulators 106a, 106b function as a gate insulator and a second gate insulator. The first insulator 114, 116, and 118 are connected to each other through openings provided in the insulators 114, 116, and 118. Insulators 106a and 106b functioning as gate insulators and a second gate insulator The oxide semiconductor 108 is surrounded by functional insulators 114, 116, and 118 therebetween.

[0216] With such a structure, the oxide semiconductor 108 included in the transistor 170 A conductor 104 functions as a first gate electrode and a conductor 105 functions as a second gate electrode. The transistor 170 can be electrically surrounded by the electric field of the conductive body 120b. An oxide film is formed in which a channel region is formed by the electric field of the first gate electrode and the second gate electrode. The device structure of a transistor that electrically surrounds a semiconductor film is called surrounded cha. This can be called a nnel (s-channel) structure.

[0217] The transistor 170 has an s-channel structure and therefore functions as a gate electrode. The electric field for inducing a channel is effectively applied to the oxide semiconductor 10 by the conductor 104. 8, the current driving capability of the transistor 170 is improved, and a high on-state current can be obtained. It is also possible to obtain high on-current characteristics. The transistor 170 can be miniaturized. The conductor 104 functions as an electrode and the conductor 120b functions as a second gate electrode. Therefore, the enclosed structure can increase the mechanical strength of the transistor 170. do.

[0218] The other configuration of the transistor 170 is the same as that of the transistor 100 described above. It is similar and has the same effect.

[0219] Here, as shown in FIG. 15C, the transistor 170 includes an oxide semiconductor 108b. It is not necessary.

[0220] In addition, the transistor according to the present embodiment can be freely combined with each of the above structures. It is possible.

[0221] <Transistor structure example 2> The transistor 100 shown in FIGS. 16A, 16B, and 16C includes an insulating layer formed on a substrate 102. An insulator 101, an oxide semiconductor 108 on the insulator 101, and an insulator on the oxide semiconductor 108 106b, the conductor 104 on the insulator 106b, the insulator 101, the oxide semiconductor 108, and an insulator 122 over the conductor 104. The oxide semiconductor 108 has a conductor A channel region 108i overlapping with the insulator 104, and a source region 108s in contact with the insulator 122. 1, the drain region 108d is in contact with the insulator 122, and the channel region 108i is a layer 108_2, which is in contact with the upper surface of the layer 108_2 and has a side surface in the channel width direction of the layer 108_2. The layer 108_2 has a channel region 108i, and the layer 108_3 covers the channel region 108i. The insulator 106b can be the oxide semiconductor 108a described above. The transistor 100 also functions as an insulator 124 on the insulator 122. Through an opening 141a provided in the insulators 122 and 124, the source region 108s is electrically connected 1 through an opening 141b provided in the insulators 122 and 124. and a conductor 112b electrically connected to the drain region 108d. stomach.

[0222] Here, an oxide semiconductor functioning as an electrode may be used as the conductor 104. The oxide semiconductor functioning as an electrode has a function of supplying oxygen to the insulator 106b. The compound semiconductor has a function of supplying oxygen to the insulator 106b. By having the excess oxygen region in the insulator 110, The excess oxygen is supplied to the oxide semiconductor 108, more specifically, to the channel region 108i. Therefore, the oxygen vacancies in the channel region 108i can be compensated for by the excess oxygen. As a result, a highly reliable semiconductor device can be obtained.

[0223] In order to supply excess oxygen to the oxide semiconductor 108, Excess oxygen may be supplied to the insulator 101 formed below. However, if the insulator 101 The excess oxygen contained in the oxide semiconductor 108 is The source region 108s and the drain region 108d may also be provided with excess. When oxygen is supplied, the resistance in the source region 108s and the drain region 108d increases. There may be cases where this occurs.

[0224] On the other hand, in the case of a structure in which the insulator 110 formed above the oxide semiconductor 108 has excess oxygen, By doing so, it is possible to selectively supply excess oxygen only to the channel region 108i. Alternatively, the channel region 108i, the source region 108s, and the drain region 108 After supplying excess oxygen to the source region 108s and the drain region 108d, All you have to do is selectively increase the rear density.

[0225] The insulator 122 contains either nitrogen or hydrogen or both. By configuring 22 to have either nitrogen or hydrogen or both, an oxide semiconductor The oxide semiconductor serving as the gate electrode and the body 108 are provided with either nitrogen or hydrogen. Or both may be provided.

[0226] Note that the oxide semiconductor functioning as a gate electrode is formed by supplying oxygen to the insulator 106b. In other words, when either nitrogen or hydrogen or both are supplied from the insulator 122, the In other words, the oxide semiconductor that functions as a gate electrode has a high carrier density. It also functions as an oxide conductor (OC). The oxide semiconductor functioning as a gate electrode has a higher carrier density than the oxide semiconductor 108. Therefore, it can function as a gate electrode.

[0227] The oxide semiconductor 108 includes a source region 108s and a drain region 108d. The oxide semiconductor functioning as the gate electrode contains an element that forms oxygen vacancies. Representative examples of the element that forms the oxygen vacancy include hydrogen, boron, carbon, and the like. Examples of rare gas elements include nitrogen, nitrogen, fluorine, phosphorus, sulfur, chlorine, and rare gases. Examples include helium, neon, argon, krypton, and xenon.

[0228] When an impurity element is added to an oxide semiconductor, the metal element in the oxide semiconductor is bonded to oxygen. When an impurity element is added to an oxide semiconductor, oxygen vacancies are formed. The oxygen that was bonded to the metal element in the oxide semiconductor bonds with the impurity element, and the metal element is converted to oxygen. As a result, the carrier density in the oxide semiconductor decreases. increases, and the conductivity becomes higher.

[0229] In addition, in the transistor 100, the side end of the insulator 106b and the gate electrode In other words, it is preferable that the side edge of the oxide semiconductor that functions as a transistor is aligned. In the photodiode 100, the upper end of the insulator 106b and the oxide semiconductor serving as the gate electrode are For example, the oxide semiconductor that functions as the gate electrode is The above structure can be achieved by processing the insulator 106b as a mask.

[0230] As described above, in the semiconductor device of one embodiment of the present invention, the oxide semiconductor layer that becomes the channel region is An insulator that covers the side of the conductor and is formed above the channel region is provided with a gate electrode. Excess oxygen is contained by an oxide semiconductor that functions as a gate insulating film. Therefore, a semiconductor device with high reliability can be provided.

[0231] The side surface or the vicinity of the channel region 108i in the channel width (W) direction is processed. Damage in the junctions can easily lead to the formation of defects (e.g. oxygen vacancies) or the presence of impurities. Therefore, even if the channel region 108i is substantially intrinsic, When a stress such as an electric field is applied, the channel width ( The side surface or its vicinity in the W direction is activated and tends to become a low-resistance (n-type) region. When the side surface or the vicinity of the side surface of the channel region 108i in the channel width (W) direction is an n-type region, Since the n-type region serves as a path for carriers, a parasitic channel may be formed.

[0232] Therefore, in the semiconductor device according to one embodiment of the present invention, the channel region 108i has a stacked structure. The side surface of the channel region 108i in the channel width (W) direction is covered with one layer of the laminated structure. By adopting this configuration, defects on the side surface of the channel region 108i or in the vicinity thereof can be prevented. Alternatively, it is possible to reduce adhesion of impurities.

[0233] The layer 108_3 of the channel region 108i may be, for example, the oxide semiconductor 108b. It can be referred to.

[0234] The insulator 122 includes either nitrogen or hydrogen or both. By using a structure containing either nitrogen or hydrogen or both, the oxide semiconductor 10 8 can be supplied with either nitrogen or hydrogen or both.

[0235] The source region 108s and the drain region 108d of the oxide semiconductor 108 are Each of them may contain an element that forms an oxygen vacancy. Representative examples of these include hydrogen, boron, carbon, nitrogen, fluorine, phosphorus, sulfur, chlorine, and rare gases. Representative examples of rare gas elements include helium, neon, argon, and crypto Examples include fluorine, fluorine, and xenon.

[0236] When an impurity element is added to an oxide semiconductor, the metal element in the oxide semiconductor is bonded to oxygen. When an impurity element is added to an oxide semiconductor, oxygen vacancies are formed. The oxygen that was bonded to the metal element in the oxide semiconductor bonds with the impurity element, and the metal element is converted to oxygen. As a result, the carrier density in the oxide semiconductor decreases. increases, and the conductivity becomes higher.

[0237] On the other hand, the source region 108s and the drain region 108d are in contact with the insulator 122. The source region 108s and the drain region 108d are in contact with the insulator 122. 122 to the source region 108s and the drain region 108d. Since one or both of them are added, the carrier density is increased.

[0238] Note that in the oxide semiconductor 108, the channel region 108i, the source region 108s, and the The crystallinity of the oxide semiconductor 104 may differ between the drain region 108d and the oxide semiconductor 106. 8, the source region 108s and the drain region 108d are closer to the channel region 108i. This is because the source region 108s and the drain region 108 When an impurity element is added to the source region 108s and the drain region 108d, damage is caused to the source region 108s and the drain region 108d. This is because defects are introduced and the crystallinity is reduced.

[0239] The insulator 101 can be formed by sputtering, CVD, evaporation, pulsed laser deposition ( The insulating film 101 can be formed by appropriately using a photolaser laser deposition (PLD) method, a printing method, a coating method, or the like. For example, a single layer or a stack of oxide insulators or nitride insulators can be used. In order to improve the interface characteristics with the oxide semiconductor 108, At least a region in contact with the oxide semiconductor 108 is preferably formed of an oxide insulator. In addition, by using an oxide insulator that releases oxygen when heated as the insulator 101, By the heat treatment, oxygen contained in the insulator 101 can be transferred to the oxide semiconductor 108. As the insulator 101, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, etc. Silicon, silicon nitride, aluminum oxide, hafnium oxide, gallium oxide or Ga- Zn oxide or the like may be used, and the film may be provided as a single layer or a multilayer. The insulator 101 has a laminated structure of a silicon nitride film and a silicon oxynitride film. In this way, the insulator 101 has a laminated structure, with a silicon nitride film on the lower layer and By using a silicon oxynitride film as the oxide semiconductor 108, oxygen can be efficiently introduced into the oxide semiconductor 108. It is possible.

[0240] The thickness of the insulator 101 is 50 nm or more, or 100 nm or more and 3000 nm or less, or The thickness of the insulator 101 can be set to 200 nm or more and 1000 nm or less. In addition, the amount of oxygen released from the insulator 101 can be increased. The interface state at the interface with the conductor 108 and the channel region 108 of the oxide semiconductor 108 It is possible to reduce the oxygen vacancies contained in i.

[0241] The insulator 124 is formed by a single layer or a laminate of an oxide insulator or a nitride insulator. The insulator 118 may be, for example, silicon oxide, silicon oxynitride, or silicon nitride. Silicon oxide, silicon nitride, aluminum oxide, hafnium oxide, gallium oxide or G It is sufficient to use a-Zn oxide, and it can be provided as a single layer or a multilayer. The body 118 is preferably a film that functions as a barrier film against hydrogen, water, etc. from the outside. It is nice.

[0242] In addition, in FIG. 16B and FIG. 16C, the stacked structure of the channel region 108i is the layer 108 For example, the layer 108_2 and the layer 108_3 are arranged in a two-layer structure, but the present invention is not limited to this. A laminated structure as shown in (B) may also be used.

[0243] 17(A) and (B) are cross-sectional views of the transistor 100A. 16(A) , the top view of the transistor 100 is the same as that of the transistor 100 shown in FIG. FIG. 17(A) is a cross-sectional view taken along the dashed line X1-X2 in FIG. 16(A). FIG. 17B is a cross-sectional view taken along dashed line Y1-Y2 in FIG. 16A.

[0244] The oxide semiconductor 108 included in the transistor 100A has a channel overlapping with the conductor 104. A source region 108i in contact with the insulator 122, a source region 108s in contact with the insulator 122, and a The channel region 108i includes a layer 108_2 and a drain region 108d. A layer 108_2 is in contact with the upper surface of the layer 108_2 and covers the side surface of the layer 108_2 in the channel width direction. 3 and a layer 108_1 in contact with the lower surface of the layer 108_2.

[0245] In this way, the transistor 100A has the same oxide semiconductor as the transistor 100 shown above. The transistor 100A is different in configuration from the transistor 100A in other respects. It has a similar configuration to the transistor 100 and provides the same effects.

[0246] The layer 108_1 in the channel region 108i may be, for example, the oxide semiconductor 108b. It can be referred to.

[0247] <Band structure 3> The oxide semiconductor in the transistor 100A shown in FIG. The band structure of the insulator is shown in FIG.

[0248] FIG. 18(A) shows an insulator 101, a layer 108_1, a layer 108_2, a layer 108_3, and an insulator The band structure is shown in the thickness direction of the insulator 106. The conduction band minimums of the insulator 101, the layers 108_1, 108_2, 108_3, and the insulator 106 The energy level (Ec) of

[0249] In this embodiment, silicon oxide films are used as the insulators 101 and 106, and the layer 10 The atomic ratio of the metal elements is In:Ga:Zn=1:1:1.2. The number of atoms of a metal element in the layer 108_2 is set to 1.0. The oxide formed using a metal oxide target with a ratio of In:Ga:Zn=4:2:4.1 A compound semiconductor film is used as the layer 108_3, and the atomic ratio of metal elements is In:Ga:Zn=1:1. : An oxide semiconductor film formed using the metal oxide target of 1.2 is used.

[0250] As shown in FIG. 18A, in the layers 108_1, 108_2, and 108_3, In this case, the energy at the bottom of the conduction band has no barrier and changes smoothly. The band is also called a buried channel structure.

[0251] By adopting the structure shown in FIG. 18(A), the layer 108_2 becomes a well, and In a transistor 100A having a layer 108_1, a layer 108_2, and a layer 108_3, , it can be seen that a channel region is formed in layer 108_2.

[0252] Here, the transistor 100 has a layer 108_2 and a layer 108_3, and a layer 108_1. No. In this case, the energy of the conduction band minimum of the layer 108_2 is equal to the energy of the conduction band minimum of the layer 108_3. Since the energy of the first charge is lower than that of the second charge, a channel region is formed in the layer 108_2.

[0253] In FIG. 18B, the insulator 106 is 01 If the defect level is located at The band diagram of the energy E 01 The difference between the bottom edge of the conduction band of layer 108_1 and the bottom edge of the conduction band of layer 108_2 is the energy E y. Here, the energy Ey is E 01 is closer to the bottom of the conduction band of the layer 108_2. When the energy is high, i.e., closer to the vacuum level, it takes a positive value. The energy Ey is 0.01 Preferably, the range is from 0.2 eV to 1.0 eV, and more preferably from 0.4 eV to 1.2 eV. The energy E 01 and the conduction band of layer 108_3 The difference between the lower ends is the energy Ew. Here, in FIG. 18(C), the energy Ew is negative. An example having the above configuration is shown below.

[0254] The energy Ew is preferably -0.2 eV or more and less than 0.8 eV, and more preferably 0 eV or more and less than 0.7 eV. V is more preferable, and 0.1 eV or more and less than 0.5 eV is further preferable.

[0255] Here, when a silicon oxide film and a silicon oxynitride film are used as the insulator 106, E 01 For example, the defect level shown in FIG. Si-H-Si(+ / 0 ) is approximately 3.1 eV from the conduction band of the insulator 106b and approximately 4.0 eV from the vacuum level. Therefore, the electron affinity of the oxide semiconductor 108a is greater than or equal to 4.01 eV and less than or equal to 5.2 eV. is preferable, 4.2 eV or more and 5.0 eV or less is more preferable, 4.4 eV or more and 4.8 eV or less is more preferable. More preferably, the potential is 4.5 eV or more and 4.8 eV or less. The electron affinity of the semiconductor 108b is preferably 3.8 eV or more and less than 4.8 eV, and more preferably 4 eV or more. Less than 4.7 eV is more preferable, and 4.1 eV or more and less than 4.5 eV is even more preferable.

[0256] In the transistor 100, an impurity is present near the interface between the layer 108_3 and the insulator 106. Even if a defect level due to a defect is formed, the layer 108_3 is provided. Therefore, the layer 108_2 can be separated from the region where the defect level is formed. In the case of the sta 100A, the layer 108_1 and the insulator 101 are adjacent to the interface, and the layer 108_3 is adjacent to the interface. Even if a defect level due to impurities or defects is formed near the interface between the semiconductor substrate 104 and the insulator 106, By providing the layers 108_1 and 108_3, a defect level is formed together with the layer 108_2. Therefore, the transistor 100 and the transistor 1 00A has layer 108_3, which reduces the thickness of insulator 106 that functions as a gate insulator. The probability of carrier capture at defect levels can be reduced.

[0257] As shown in FIG. 41, the transistor 100 includes a layer 108_1 and a layer 108_3. It is not necessary to have one.

[0258] In addition, the conductor 104 may be a laminate of two or more layers of conductors. For example, as shown in FIG. As shown in FIG. 1, a two-layer stack of a conductor 104a and a conductor 104b may be used.

[0259] Here, an oxide semiconductor may be used as the conductor 104a. In that case, For example, 04b is a metal element, or an alloy containing two or more metal elements, or nitrogen. Nitrides of metal elements such as tantalum nitride and titanium nitride may be used. For example, two or more layers of metal elements, alloys, and nitrides of metal elements are laminated as 4b. Good too.

[0260] As shown in FIG. 42B, the end of the conductor 104a is connected to the end of the conductor 104b. Alternatively, as shown in FIG. 42(C), the end of the insulator 106 may be located on the outside. It may be located outside the end of the body 104a.

[0261] FIG. 43 illustrates an example of a transistor 100. FIG. 43A illustrates a transistor 100. FIG. 43(B) shows a cross-sectional view taken along the dashed line X1-X2 in FIG. 43(A), and FIG. FIG. 43(C) shows a cross-sectional view taken along the dashed line Y1-Y2 in FIG. 43(A). 41(A), the cross section shown in FIG. 41(B) has a conductor 105 that functions as a second gate electrode. In addition, the cross section shown in FIG. 43(C) is different from that shown in FIG. 41(B) in that the conductor 10 5, and the conductor 104 is embedded in the opening 143 of the insulator 106 and the insulator 101. The difference is that the conductor 105 is embedded in the layer 1 through the insulator 101 and comes into contact with the conductor 105. Facing 08_2.

[0262] <How to fabricate a transistor> Next, an example of a method for manufacturing the transistor 100 shown in FIG. 16 will be described with reference to FIGS. 19 to 21 are used to explain a method for manufacturing the transistor 100. 1 is a cross-sectional view in the channel length (L) direction and the channel width (W) direction.

[0263] First, an insulator 101 is formed on a substrate 102, and an oxide semiconductor film is formed on the insulator 101. After that, the oxide semiconductor film is processed into an island shape to form a layer 108_2 ( See Figure 19(A).

[0264] The insulator 101 can be formed by sputtering, CVD, evaporation, pulsed laser deposition ( The film can be formed by appropriately using a PLD method, a printing method, a coating method, or the like. In this example, a PECVD apparatus was used to deposit a silicon nitride film having a thickness of 400 nm as the insulator 101. Then, a silicon oxynitride film having a thickness of 50 nm is formed.

[0265] After the insulator 101 is formed, oxygen may be added to the insulator 101. The oxygen added to 1 can be oxygen radicals, oxygen atoms, oxygen atomic ions, or oxygen molecular ions. The doping method includes ion doping, ion implantation, plasma treatment, etc. In addition, a film for suppressing oxygen desorption is formed on the insulator 101, and then the Oxygen may be added to the insulator 101 by using the above method.

[0266] The above-mentioned oxygen desorption-suppressing film may be made of indium, zinc, gallium, tin, aluminum, or the like. Aluminum, chromium, tantalum, titanium, molybdenum, nickel, iron, cobalt, tungsten A metal element selected from the above, an alloy containing the above metal element, or a combination of the above metal elements. an alloy having the above-mentioned metal element, a metal nitride having the above-mentioned metal element, a metal oxide having the above-mentioned metal element, The insulating layer 11 is formed by using a conductive material such as a metal nitride oxide having the above-mentioned metal element. This can be done.

[0267] In addition, when oxygen is added in plasma treatment, the oxygen is excited by microwaves to produce high-density oxygen. By generating atomic plasma, the amount of oxygen added to the insulator 101 can be increased. .

[0268] The layer 108_2 can be formed by sputtering, coating, pulsed laser deposition, laser deposition, or the like. The layer 108_2 can be formed by an ablation method, a thermal CVD method, or the like. In the processing, a mask is formed over the oxide semiconductor film by a lithography process, and then the mask is The oxide semiconductor film can be partially etched using a printing method. The layer 108_2 may be formed directly on the insulator 101.

[0269] When an oxide semiconductor film is formed by a sputtering method, a power source for generating plasma The device may be an RF power supply device, an AC power supply device, a DC power supply device, or the like. In the case of forming an oxide semiconductor film, a sputtering gas is a rare gas (typically, argon). ), oxygen, rare gas, and mixed gas of oxygen are used as appropriate. Note that the mixed gas of rare gas and oxygen In this case, it is preferable to increase the gas ratio of oxygen to the rare gas.

[0270] Note that when the oxide semiconductor film is formed by, for example, a sputtering method, Temperature: 150℃ to 750℃, 150℃ to 450℃, or 200℃ By forming the oxide semiconductor film at a temperature of 350° C. or less, the crystallinity can be improved. Therefore, it is preferable.

[0271] In this embodiment, a sputtering device is used to deposit the layer 108_2. The sputtering target was In-Ga-Zn metal oxide (In:Ga:Zn=4:2 A 30-nm-thick oxide semiconductor film was formed using a SiO2 / SiO2 (atomic ratio: 4.1).

[0272] After the layer 108_2 is formed, heat treatment is performed to dehydrogenate or desorb the layer 108_2. The temperature of the heat treatment is typically 150° C. or higher and lower than the substrate distortion point, or is 250°C or higher and 450°C or lower, or 300°C or higher and 450°C or lower.

[0273] Heat treatment is carried out using rare gases such as helium, neon, argon, xenon, krypton, or It can be carried out in an inert gas atmosphere containing nitrogen. Alternatively, it can be heated in an inert gas atmosphere. After that, heating may be performed in an oxygen atmosphere. Note that hydrogen, water, etc. may be added to the inert atmosphere and oxygen atmosphere. It is preferable that the treatment time does not include the above-mentioned. The treatment time may be from 3 minutes to 24 hours.

[0274] The heat treatment can be performed using an electric furnace, an RTA device, or the like. Therefore, heat treatment can be performed at a temperature above the distortion point of the substrate for a short period of time. The processing time can be reduced.

[0275] The oxide semiconductor film is formed while being heated, or the oxide semiconductor film is formed and then subjected to heat treatment. By performing the process, the hydrogen concentration in the oxide semiconductor film obtained by secondary ion mass spectrometry can be Degrees 5×10 19 atoms / cm 3 or less, or 1×10 19 atoms / cm 3 below , 5×10 18 atoms / cm 3 or less, or 1×10 18 atoms / cm 3 below, or 5×10 17 atoms / cm 3 or less, or 1×10 16 atoms / cm 3 Below It can be below.

[0276] Note that in the step of forming the layer 108_2, an oxide semiconductor film having a stacked structure is formed. The oxide semiconductor film having the stacked structure is processed into an island shape to form a layer 108_1 and a layer 108_2. In this way, the transistor 100A described above can be formed.

[0277] Next, the insulator 101, the oxide semiconductor 107_3 which becomes the layer 108_3 on the layer 108_2, And an insulator 106_0 is formed (see FIG. 19B).

[0278] The oxide semiconductor 107_3 is formed to cover the side surfaces of the layer 108_2. The oxide semiconductor 107_3 is formed of the same material and by the same method as the layer 108_2 described above. It can be formed by the method.

[0279] In this embodiment, the oxide semiconductor 107_3 is formed by a sputtering apparatus. The sputtering target was In-Ga-Zn metal oxide (In:Ga:Zn=1 A 5-nm-thick oxide semiconductor film was formed using a SiO2 / SiO2 (atomic ratio: 1:1.2).

[0280] The insulator 106 is a silicon oxide film or a silicon oxynitride film, In this case, the source gas is a deposition gas containing silicon. It is preferable to use a reactive gas and an oxidizing gas. Representative examples of deposition gases containing silicon include Examples of oxidizing gases include silane, disilane, trisilane, and fluorinated silane. These include nitrous oxide, ozone, nitrous oxide, and nitrogen dioxide.

[0281] In addition, the flow rate of the oxidizing gas is set to 20 times the flow rate of the deposition gas as the insulator 106. The pressure in the treatment chamber should be less than 100 times, or between 40 and 80 times. By using the PECVD method with a pressure of 50 Pa or less, it is possible to fabricate an oxynitride silicon nitride film with a small amount of defects. A silicon film can be formed.

[0282] The insulator 106 is a substrate placed in a vacuum-evacuated processing chamber of a PECVD apparatus. The plate is kept at 280°C or more and 400°C or less, and raw material gas is introduced into the treatment chamber to The pressure is set to 20 Pa or more and 250 Pa or less, and more preferably, 100 Pa or more and 250 Pa or less. Depending on the conditions for supplying high frequency power to the electrode provided in the processing chamber, the insulator 106 A dense silicon oxide film or silicon oxynitride film can be formed.

[0283] Alternatively, the insulator 106 may be formed using a microwave PECVD method. Microwaves refer to the frequency range from 300MHz to 300GHz. The electron energy is low. In addition, when using a microwave PECVD device, The proportion of the power used to generate plasma, i.e., ionize molecules, out of the power supplied. The ratio of power used to accelerate electrons is low. This allows the generation of high-density plasma, which is highly effective in preventing the deposition of the film on the surface and deposits. The insulator 106 can be formed with less Z-type damage and fewer defects.

[0284] The insulator 106 can also be formed by a CVD method using an organic silane gas. The organic silane gas is ethyl silicate (TEOS: chemical formula Si(OC2H5)4), Tetramethylsilane (TMS: chemical formula Si(CH3)4), tetramethylcyclotetrasilane Octamethylcyclotetrasiloxane (TMCTS), Octamethylcyclotetrasiloxane (OMCTS), Hexa Methyldisilazane (HMDS), triethoxysilane (SiH(OC2H5)3), tri Silicon-containing compounds such as dimethylaminosilane (SiH(N(CH3)2)3) are used. By using the CVD method with organic silane gas, it is possible to obtain insulating films with high coating properties. A body 106 can be formed.

[0285] In this embodiment, a PECVD apparatus is used to form the insulator 106, and an oxide film having a thickness of 100 nm is formed. A silicon nitride film is formed.

[0286] Next, the conductor 104_0 is formed on the insulator 106. In the case where an oxide semiconductor film is used, the conductor 104_0 is formed. Oxygen is added to the insulator 106 from 0 (see FIG. 19C).

[0287] The conductor 104_0 can be formed by a sputtering method or the like.

[0288] When an oxide semiconductor film is used as the conductor 104_0, the conductor is formed in an atmosphere containing oxygen gas. It is preferable to form the conductor 104_0 in an atmosphere containing oxygen gas during formation. In this case, oxygen can be suitably added to the insulator 106. The oxygen added to the insulator 106 is shown by an arrow. The same material as that of the layer 108_2 described above can be used for the layer 108_2.

[0289] Next, a mask 140 is formed at a desired position on the conductor 104_0 by a lithography process. (See FIG. 19(D)).

[0290] Next, etching is performed from above the mask 140 to form a conductor 104_0 and an insulator 104_1. After processing the oxide semiconductor 107_3, the mask 140 is removed, and an island-like The conductor 104, the island-shaped insulator 106, and the island-shaped layer 108_3 are formed (FIG. 20). (See (A)).

[0291] When the layer 108_3 is formed, a part of the surface of the layer 108_2 is exposed. The region where a part of the surface of the _2 is exposed will later be a source region 108s and a drain region 108 The result is d.

[0292] In this embodiment, the processing of the conductor 104_0, the insulator 106, and the layer 108_3 The etching is performed by using a dry etching method.

[0293] In addition, when the conductor 104, the insulator 106, and the layer 108_3 are processed, the conductor 104 In some cases, the thickness of the layer 108_2 in the region where the conductor 104 and the The insulator 106 and the insulator in the region where the layer 108_2 does not overlap when processing the layer 108_3 The thickness of the film 101 may become thin.

[0294] Next, an impurity element 145 is added from above the insulator 101, the layer 108_2, and the conductor 104. (See FIG. 20(B)).

[0295] The impurity element 145 can be added by ion doping, ion implantation, plasma In the case of plasma treatment, the plasma is heated in a gas atmosphere containing the impurity element to be added. Impurity elements can be added by generating a plasma and performing a plasma treatment. The plasma generating device may be a dry etching device, an ashing device, A PECVD apparatus, a high density PECVD apparatus, or the like can be used.

[0296] The source gas for the impurity element 145 is B2H6, PH3, CH4, N2, NH3 , AlH3, AlCl3, SiH4, Si2H6, F2, HF, H2 and one or more of the rare gases Alternatively, B2H6, P diluted with a rare gas (e.g., argon) can be used. One or more of H3, N2, NH3, AlH3, AlCl3, F2, HF, and H2 may be used. B2H6, PH3, N2, NH3, AlH3, AlCl diluted with rare gases 3, F2, HF, and H2 are used to inject impurity elements 145 into the layer 108_2 and the conductor Adding it to 104 will remove rare gases, hydrogen, boron, carbon, nitrogen, fluorine, phosphorus, sulfur, and One or more of fluorine and chlorine may be added to the layer 108_2 and the conductor 104.

[0297] Or, the impurity element 145 is added as a source gas, and then B2H6, PH3 , CH4, N2, NH3, AlH3, AlCl3, SiH4, Si2H6, F2, HF, One or more of H2 and H2 may be added to the layer 108_2 and the conductor 104 as source gases.

[0298] Or, the impurity element 145 is B2H6, PH3, CH4, N2, NH3, AlH3, Add one or more of AlCl3, SiH4, Si2H6, F2, HF, and H2 as source gas. After the addition, a rare gas may be added to the layer 108_2 and the conductor 104 as a source gas.

[0299] The addition of the impurity element 145 is controlled by appropriately setting implantation conditions such as acceleration voltage and dose amount. For example, when argon is added by ion implantation, the acceleration voltage is set to 10 kV or more. 00kV or less, dose amount is 1×10 13 ions / cm 2 More than 1×10 16 ions / c m 2 For example, 1×10 14 ions / cm 2 Also, When phosphorus ions are added by the on-implantation method, the acceleration voltage is 30 kV and the dose is 1×10 13 ions / cm 2 5×10 or more 16 ions / cm 2 For example, 1×1 0 15 ions / cm 2 This can be done as follows.

[0300] In this embodiment, the mask 140 is removed, and then the impurity element 145 is added. However, the present invention is not limited to this. For example, the mask 140 may be left in place. The impurity element 145 may be added in this state.

[0301] In this embodiment, the impurity element 145 is doped using a doping device. Argon is added to the layer 108_2. However, this is not limited to this, and for example, impurity element 1 The step of adding 45 may be omitted.

[0302] Next, the insulator 122 is formed over the insulator 101, the layer 108_2, and the conductor 104. By forming the insulator 122, the layer 108_2 in contact with the insulator 122 is provided with a source The layer 108 that is not in contact with the insulator 122 becomes the drain region 108s and the drain region 108d. The layer 108_2 and the layer 108_3 form a channel region 108i. The oxide semiconductor 108 is formed (see FIG. 20C).

[0303] In this manner, the oxide semiconductor 108 has a channel region 108i overlapping with the conductor 104. , a source region 108s in contact with the insulator 122, and a drain region 10 8d, and the channel region 108i is in contact with the layer 108_2 and the upper surface of the layer 108_2. and a layer 108_3 covering the side surface of the layer 108_2 in the channel width direction. .

[0304] The insulator 122 can be formed by selecting the above-mentioned materials. In this embodiment, a 100 nm thick nitride silicon film is deposited as the insulator 122 using a PECVD apparatus. Form a recombinant membrane.

[0305] By using a silicon nitride film as the insulator 122, the conductor 1 04, hydrogen in the silicon nitride film enters the source region 108s and the drain region 108d. The carrier density of the conductor 104, the source region 108s, and the drain region 108d is It can be improved.

[0306] Next, the insulator 124 is formed over the insulator 122 (see FIG. 20D).

[0307] The insulator 124 can be formed by selecting the above-mentioned material. In this example, a PECVD apparatus was used to deposit a silicon oxynitride layer having a thickness of 300 nm as the insulator 124. Form a cone film.

[0308] Next, a mask is formed by lithography at a desired position of the insulator 124, and then the insulator 124 and a portion of the insulator 122 are etched to form an opening that reaches the source region 108s. An opening 141a and an opening 141b reaching the drain region 108d are formed (FIG. 21 (See (A)).

[0309] The method for etching the insulator 124 and the insulator 122 is a wet etching method. and / or dry etching can be appropriately used. The insulator 124 and the insulator 122 are processed by dry etching.

[0310] Next, the conductor 112 is formed on the insulator 124 so as to cover the openings 141a and 141b. (See FIG. 21(B)).

[0311] For the conductor 112, a material that can be used for the conductors 112a and 112b is selected. In this embodiment, the conductor 112 can be formed by sputtering. The titanium film with a thickness of 50 nm, the aluminum film with a thickness of 400 nm, and the aluminum film with a thickness of 100 A titanium film having a thickness of nm is formed.

[0312] Next, a mask is formed at a desired position on the conductor 112 by a lithography process, and then A part of the conductor 112 is etched to form the conductors 112a and 112b (FIG. 21(C)).

[0313] The conductor 112 may be processed by wet etching and / or dry etching. In this embodiment, a dry etching method is used to remove the conductor 112 is processed to form conductors 112a and 112b.

[0314] Through the above steps, the transistor 100 illustrated in FIG. 16 can be manufactured.

[0315] Note that the films (insulators, oxide semiconductors, conductors, etc.) or layers constituting the transistor 100 The methods include sputtering, chemical vapor deposition (CVD), vacuum deposition, and pulsed laser deposition ( It can be formed by using the PLD (proton-layer deposition) method or the ALD (atomic layer deposition) method. The film can be formed by a sputtering method, a plasma chemical deposition method, or a printing method. A typical example is a PECVD method, but a thermal CVD method may also be used. An example of such a method is metal-organic chemical vapor deposition (MOCVD).

[0316] In the thermal CVD method, the pressure in the chamber is set to atmospheric pressure or reduced pressure, and the source gas and the oxidizing agent are simultaneously The reaction is carried out in the chamber near or on the substrate, where it is deposited on the substrate to form a film. As described above, the thermal CVD method is a film formation method that does not generate plasma. This has the advantage that defects are not generated due to damage.

[0317] In addition, in the ALD method, the pressure inside the chamber is set at atmospheric pressure or reduced pressure, and the source gas for the reaction is The film is formed by repeatedly introducing the gas into the chamber and reacting it. A reactive gas (such as argon or nitrogen) may be introduced as a carrier gas. For example, two types of At least one type of source gas may be supplied to the chamber in sequence. In order to avoid this, after the reaction of the first raw material gas, an inert gas is introduced, and then the second raw material gas is introduced. Alternatively, instead of introducing an inert gas, the first source gas is discharged by evacuation. After that, the second source gas may be introduced. The first source gas is adsorbed and reacted with the surface of the substrate. The first layer is formed, and the second source gas introduced later is adsorbed and reacted with the first layer. The order of gas introduction is controlled to obtain a thin film of the desired thickness. By repeating the process several times up to 1000 nm, a thin film with excellent step coverage can be formed. The thickness can be adjusted by changing the number of times the gas introduction sequence is repeated, allowing precise film thickness adjustment. This makes it possible to fabricate miniaturized FETs.

[0318] Thermal CVD methods such as MOCVD can be used to deposit the above-mentioned conductors, insulators, oxide semiconductors, etc. For example, when forming an In-Ga-Zn-O film, the trimer In(CH3)3, trimethylgallium (Ga(CH3)3), and Dimethyl zinc (Zn(CH3)2) is used. Triethylgallium (chemical formula Ga(C2H5)3) can also be used instead of triethylgallium. Diethylzinc (chemical formula Zn(C2H5)2) can also be used instead of dimethylzinc. can.

[0319] For example, when forming a hafnium oxide film using a film forming apparatus that uses ALD, the solvent and liquids containing hafnium precursor compounds (hafnium alkoxides, tetrakisdimethyl Amidohafnium (TDMAH, Hf[N(CH3)2]4) and tetrakis(ethylmethy The raw material gas is vaporized and used as an oxidizer. Two types of gases are used:

[0320] For example, when forming an aluminum oxide film using an ALD deposition system, A liquid containing a catalyst and an aluminum precursor compound (trimethylaluminum (TMA, Al(C) Two types of gases are used: vaporized H3)3) and H2O as an oxidizing agent. Other liquid materials include tris(dimethylamido)aluminum and triisobutylaluminum. Aluminum tris(2,2,6,6-tetramethyl-3,5-heptanedionato) Examples include:

[0321] For example, when forming a silicon oxide film using a deposition system that uses ALD, Chlorodisilane is adsorbed on the surface to be coated, and the radicals of oxidizing gases (O2, nitrous oxide) are The adsorbate is reacted with the adsorbate.

[0322] For example, when forming a tungsten film using an ALD deposition system, WF6 The initial tungsten film was formed using B2H6 gas and WF6 gas, and then H2 gas. A tungsten film is formed using the gas. Note that SiH4 gas is used instead of B2H6 gas. It's fine.

[0323] For example, an oxide semiconductor film, such as In-Ga-Zn- When forming an O film, an In-O layer is formed using In(CH3)3 gas and O3 gas. Then, a Ga-O layer is formed using Ga(CH3)3 gas and O3 gas, and then The Zn-O layer is formed using Zn(CH3)2 gas and O3 gas. The order is not limited to this example. In addition, In-Ga-O layers and In-Zn- It is also possible to form a mixed compound layer such as an O layer or a Ga-Zn-O layer. H2O gas obtained by bubbling water with an inert gas such as Ar may be used. It is preferable to use O3 gas, which does not cause oxidation.

[0324] (Embodiment 3) In this embodiment, an oxide semiconductor of one embodiment of the present invention will be described.

[0325] <Structure of oxide semiconductor> The structure of an oxide semiconductor will be described below.

[0326] Oxide semiconductors can be divided into single-crystal oxide semiconductors and other non-single-crystal oxide semiconductors. As a non-single-crystal oxide semiconductor, CAAC-OS (c-axis-aligned d crystalline oxide semiconductor), polycrystalline oxide Nanocrystalline oxide semiconductor, nc-OS (nanocrystalline oxide semiconducting ductor), pseudo-amorphous oxide semiconductor (a-like OS: amorphous- amorphous oxide semiconductors, etc. be.

[0327] From another point of view, the oxide semiconductor is classified into an amorphous oxide semiconductor and a crystalline oxide semiconductor. Crystalline oxide semiconductors are classified into single crystal oxide semiconductors, CAAC -OS, polycrystalline oxide semiconductors, and nc-OS.

[0328] Amorphous structures are generally isotropic and have no inhomogeneous structure, and are characterized by the arrangement of atoms in a metastable state. The positions are not fixed, the bond angles are flexible, and there is short-range order but no long-range order. It is said that there is no such thing.

[0329] That is, a stable oxide semiconductor is transformed into a completely amorphous s) It cannot be called an oxide semiconductor. Also, it is not isotropic (for example, it has a periodic structure in a small area). An oxide semiconductor having an Al structure cannot be called a completely amorphous oxide semiconductor. ike OS is not isotropic, but has an unstable structure with voids. In terms of instability, the a-like OS is physically similar to an amorphous oxide semiconductor. stomach.

[0330] <caac-os> First, let me explain about CAAC-OS.

[0331] CAAC-OS is an oxide that has multiple crystal parts (also called pellets) aligned along the c-axis. It is a type of semiconductor.

[0332] CAAC-OS was analyzed by X-ray diffraction (XRD). For example, InGaZnO4, which is classified into the space group R-3m, The structure of CAAC-OS with crystals was analyzed by the out-of-plane method. As shown in FIG. 22(A), a peak appears at a diffraction angle (2θ) of about 31°. The peak is attributed to the (009) plane of the InGaZnO4 crystal, so In this case, the crystal has a c-axis orientation, and the c-axis is the surface on which the CAAC-OS film is to be formed (also called the surface on which the film is to be formed). It can be confirmed that the direction is perpendicular to the surface of the crystal, or perpendicular to the surface of the crystal. In addition to the peaks around 2θ of 36°, a peak may also appear around 2θ of 36°. The nearby peak is due to a crystal structure classified into the space group Fd-3m. It is preferred that the C-OS does not exhibit such a peak.

[0333] On the other hand, in-plane X-ray irradiation is performed on the CAAC-OS in a direction parallel to the surface on which the X-ray is to be formed. When structural analysis was performed using the ane method, a peak appeared at 2θ of approximately 56°. This peak is It is attributed to the (110) plane of the InGaZnO4 crystal. And, 2θ is fixed at around 56°. Then, the sample is rotated around the normal vector of the sample surface as an axis (φ axis) while analyzing (φ scan). Even if this is done, no clear peak appears as shown in FIG. 22(B). On the other hand, single crystal InGa When 2θ is fixed at around 56° and φ is scanned for ZnO4, the results shown in Figure 22(C) As shown in the figure, six peaks attributable to crystal planes equivalent to the (110) plane are observed. XRD structural analysis revealed that the orientation of the a-axis and b-axis of CAAC-OS is irregular. It can be confirmed that:

[0334] Next, we will explain the CAAC-OS analyzed by electron diffraction. For CAAC-OS with ZnO4 crystals, the process was parallel to the CAAC-OS surface. When an electron beam with a probe diameter of 300 nm is incident, a diffraction pattern ( This is also called a selected area electron diffraction pattern.) may appear. This diffraction pattern includes I The spots are due to the (009) plane of the nGaZnO4 crystal. Diffraction also confirmed that the pellets contained in the CAAC-OS have a c-axis orientation and that the c-axis is the unformed On the other hand, for the same sample, the sample surface is The diffraction pattern when an electron beam with a probe diameter of 300 nm was incident perpendicularly to the ) is shown. From FIG. 22(E), a ring-shaped diffraction pattern is confirmed. Electron diffraction using an electron beam with a diameter of 300 nm also revealed that the PEG-1000 nanometers in the CAAC-OS It can be seen that the a-axis and b-axis of the slits have no orientation. The first ring is due to the (010) and (100) planes of the InGaZnO4 crystal. The second ring in Fig. 22(E) is thought to be due to the (110) plane. It is thought that.

[0335] In addition, a transmission electron microscope (TEM) Combined analysis of bright-field images and diffraction patterns of CAAC-OS using a microscope. When observing the image (also called a high-resolution TEM image), multiple pellets can be confirmed. On the other hand, even in high-resolution TEM images, the boundaries between pellets, i.e., grain boundaries (grain boundaries), are not clearly visible. (also called underly.) may not be clearly identified. It can be said that C-OS is less susceptible to the decrease in electron mobility caused by grain boundaries.

[0336] Figure 23(A) shows a high-resolution cross-section of CAAC-OS observed from a direction approximately parallel to the sample surface. The TEM image is shown. A spherical aberration correction (SCA) was used for high-resolution TEM imaging. The spherical aberration corrector function was used. A high-resolution TEM image is specifically called a Cs-corrected high-resolution TEM image. For example, an atomic resolution analytical electron microscope JEM-ARM200F manufactured by JEOL Ltd. Therefore, it can be observed.

[0337] From FIG. 23(A), a pellet, which is an area where metal atoms are arranged in layers, can be confirmed. The size of each pellet can be 1 nm or more, or 3 nm or more. Therefore, the pellets are called nanocrystals (nc). CAAC-OS can also be used as a C-Axis Aligned Navigator (CANC). The pellets can also be called oxide semiconductors with no crystals. It reflects the unevenness of the surface on which the C-OS is formed or the top surface, and the unevenness of the surface on which the CAAC-OS is formed or It is parallel to the top surface.

[0338] In addition, Fig. 23(B) and Fig. 23(C) show CAA images observed from a direction approximately perpendicular to the sample surface. Cs-corrected high-resolution TEM images of the C-OS surface. 23(B) and 23(C), respectively. First, the method of processing is explained. Then, the FFT image is obtained by Fourier Transform (FFT) processing. In the acquired FFT image, the origin is used as the reference point, and the -1 From 5.0 nm -1 The range between Next, the masked FFT image is transformed by inverse fast Fourier transform (IFFT : Inverse Fast Fourier Transform) processing is used to The image obtained in this way is called an FFT filtered image. The filtered image is an image in which periodic components are extracted from a Cs-corrected high-resolution TEM image. This indicates a child array.

[0339] In FIG. 23(D), the area where the lattice arrangement is disturbed is indicated by a dashed line. The area indicated by the dashed line is the connection between the pellets. The broken line shows the hexagonal shape, so we can see that the pellet is hexagonal. The shape of the let is not limited to a regular hexagon, and is often a non-regular hexagon.

[0340] In FIG. 23(E), a grid is formed between an area with a uniform lattice arrangement and an area with a different uniform lattice arrangement. The dotted lines indicate the changes in the orientation of the child array, and the dashed lines indicate the changes in the orientation of the lattice array. Even in the vicinity of the dotted line, no clear crystal grain boundaries can be confirmed. When you connect the surrounding lattice points with the center at the center, you can see the shape of a distorted hexagon, pentagon, or / and heptagon. In other words, the formation of grain boundaries is suppressed by distorting the lattice arrangement. This is because the atomic arrangement of CAAC-OS is not dense in the ab-plane direction. The substitution of metal elements changes the bond distance between atoms, allowing distortion to be tolerated. This is thought to be because

[0341] As described above, the CAAC-OS has a c-axis orientation and is Multiple pellets (nanocrystals) are connected to form a distorted crystal structure. AAC-OS, CAA crystal(c-axis-aligned abp It can also be called an oxide semiconductor having lane-anchored crystals. Cut.

[0342] CAAC-OS is a highly crystalline oxide semiconductor. The crystallinity of oxide semiconductors is determined by the presence of impurities. CAAC-OS is designed to prevent impurities and defects from causing degradation. It can also be said to be an oxide semiconductor with few defects (such as oxygen vacancies).

[0343] The impurities are elements other than the main components of the oxide semiconductor, such as hydrogen, carbon, silicon, and transition metals. For example, metal elements such as silicon have a higher acidity than metal elements that constitute oxide semiconductors. Elements with strong bonds to oxygen remove oxygen from the oxide semiconductor, which changes the atomic arrangement of the oxide semiconductor. In addition, heavy metals such as iron and nickel, argon, Carbon dioxide and other molecules have a large atomic radius (or molecular radius), so the atomic arrangement of oxide semiconductors This disrupts the structure and reduces the crystallinity.

[0344] When an oxide semiconductor has impurities or defects, its characteristics may change due to light, heat, etc. For example, impurities contained in oxide semiconductors can act as carrier traps or For example, oxygen vacancies in oxide semiconductors can act as carrier traps. In some cases, the ZnO traps hydrogen and becomes a carrier generation source.

[0345] CAAC-OS, which has few impurities and oxygen vacancies, is an oxide semiconductor with low carrier density. CAAC-OS has low impurity concentration and low defect level density. In other words, it has stable characteristics. It can be said that the oxide semiconductor has a

[0346] <nc-os> Next, we will explain nc-OS.

[0347] The following describes the case where nc-OS is analyzed by XRD. However, when structural analysis was performed using the out-of-plane method, no peaks indicating orientation appeared. That is, the crystals of the nc-OS do not have any orientation.

[0348] For example, an nc-OS having InGaZnO4 crystals was sliced ​​to a thickness of 34 nm. When an electron beam with a probe diameter of 50 nm is incident parallel to the surface to be formed on the region of m, the result shown in Fig. 2 A ring-shaped diffraction pattern (nanobeam electron diffraction pattern) as shown in FIG. 4(A) was observed. In addition, the diffraction pattern when an electron beam with a probe diameter of 1 nm is incident on the same sample ( The nanobeam electron diffraction pattern is shown in Figure 24(B). Therefore, the nc-OS has a probe diameter of 50 nm. No order was observed when an electron beam with a probe diameter of 1 nm was incident. When light is incident on it, order is confirmed.

[0349] In addition, when an electron beam with a probe diameter of 1 nm is incident on an area with a thickness of less than 10 nm, As shown in FIG. 24(C), an electron diffraction pattern was observed in which the spots were arranged in a substantially regular hexagonal shape. Therefore, it is considered that the nc-OS is ordered in the range of thickness less than 10 nm. It can be seen that the crystals are highly ordered. Therefore, there are some areas where no regular electron diffraction pattern is observed.

[0350] FIG. 24(D) shows the Cs-corrected height of the cross section of the nc-OS observed from a direction approximately parallel to the surface on which the film was formed. The nc-OS is shown in the high-resolution TEM image as the area indicated by the auxiliary lines. How to identify the crystals and the areas where no clear crystals can be identified The crystal parts in the nc-OS have a size of 1 nm to 10 nm. In particular, the size of the crystals is often between 1 nm and 3 nm. An oxide semiconductor having a size of 10 nm or more and 100 nm or less is called a microcrystalline oxide semiconductor (microcrystalline oxide semiconductor). It is sometimes called ocrystalline oxide semiconductor. For example, in the case of nc-OS, the grain boundaries cannot be clearly identified in high-resolution TEM images. It is possible that the nanocrystals originate from the same source as the pellets in CAAC-OS. Therefore, below, the crystalline part of the nc-OS may be called a pellet.

[0351] In this way, the nc-OS can be used in microscopic regions (e.g., regions of 1 nm to 10 nm, particularly The atomic arrangement has periodicity in the region of 1 nm to 3 nm. In the case of the Cr-Al-Al-Fe-Al-Fe-O-Pb-Al-Zn ... Therefore, depending on the analytical method, nc-OS may be classified as a-like OS or amorphous OS. In some cases, it may be difficult to distinguish them from solid oxide semiconductors.

[0352] In addition, since the crystal orientation between the pellets (nanocrystals) is not regular, nc-OS is , oxidation with RANC (Random Aligned nanocrystals) Semiconductors or NANC (Non-Aligned nanocrystals) In other words, the oxide semiconductor has a conductivity of 1000.

[0353] The nc-OS is an oxide semiconductor with higher order than an amorphous oxide semiconductor. The nc-OS has a lower density of defect states than the a-like OS and amorphous oxide semiconductors. However, the crystal orientation of nc-OS is not regular among different pellets. Therefore, the nc-OS may have a higher density of defect states than the CAAC-OS.

[0354] <a-like OS> The a-like OS is an oxide semiconductor that has a structure between the nc-OS and the amorphous oxide semiconductor. It is a semiconductor.

[0355] FIG. 25 shows a high-resolution cross-sectional TEM image of the a-like OS. is a high-resolution cross-sectional TEM image of the a-like OS at the start of electron irradiation. B) is 4.3 x 10 8 e - / nm 2 Electrons (e - ) A-like OS after irradiation High-resolution cross-sectional TEM images. Figures 25(A) and 25(B) show that a-like O It can be seen that striped bright regions extending in the vertical direction are observed in S from the start of electron irradiation. It can also be seen that the shape of the bright regions changes after electron irradiation. It is suspected to be a density region.

[0356] Because of the porosity, the a-like OS has an unstable structure. e OS has an unstable structure compared with CAAC-OS and nc-OS. This shows the change in structure due to electron irradiation.

[0357] As samples, a-like OS, nc-OS and CAAC-OS are prepared. Both samples are In-Ga-Zn oxides.

[0358] First, high-resolution cross-sectional TEM images of each sample are obtained. All of the materials have crystalline parts.

[0359] The unit cell of the InGaZnO4 crystal has three In-O layers and a Ga-Zn It is known that the structure has a total of nine layers, six of which are -O layers, stacked in layers in the c-axis direction. The distance between these adjacent layers is the lattice spacing (also called the d value) of the (009) plane. The value is about the same, and is calculated to be 0.29 nm from crystal structure analysis. In the following, the area where the lattice spacing is 0.28 nm or more and 0.30 nm or less is called InGaZ. The lattice fringes correspond to the ab plane of the InGaZnO4 crystal. do.

[0360] Figure 26 shows an example of the average size of the crystal parts (22 to 30 places) of each sample. The length of the lattice fringes is the size of the crystal part. e. The crystal part of the OS grows larger according to the cumulative dose of electrons used in obtaining the TEM image. As can be seen from Fig. 26, in the early stages of TEM observation, the size of the particles is about 1.2 nm. The part of the crystal that grew up (also called the initial nucleus) absorbs electrons (e - ) cumulative exposure of 4.2 × 10 8 e - / nm 2 It can be seen that the size of the crystals grows to about 1.9 nm in the n For c-OS and CAAC-OS, the cumulative electron irradiation dose was 4.2 × 10 8 e - / nm 2 It can be seen that there is no change in the size of the crystals within the range of 100 to 150 mm. Therefore, the size of the crystalline parts of nc-OS and CAAC-OS is constant regardless of the cumulative dose of electron irradiation. , and 1.3 nm and 1.8 nm, respectively. The Hitachi transmission electron microscope H-9000NAR was used for the TEM observations. The conditions were an acceleration voltage of 300 kV and a current density of 6.7 × 10 5 e - / (nm 2 ·s), irradiation area The diameter of the region was set to 230 nm.

[0361] Thus, in a-like OS, the growth of crystals can be observed by electron irradiation. On the other hand, in the case of nc-OS and CAAC-OS, the growth of the crystals due to electron irradiation is almost nonexistent. That is, a-like OS is not seen in comparison with nc-OS and CAAC-OS. , it is clear that this is an unstable structure.

[0362] In addition, because of the porosity, a-like OS is more difficult to treat than nc-OS and CAAC-OS. Specifically, the density of the a-like OS is The density of the nc-OS and the CAA The density of C-OS is 92.3% or more but less than 100% of the density of a single crystal of the same composition. It is difficult to form a film of an oxide semiconductor having a crystal density of less than 78%.

[0363] For example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, The density of single crystal InGaZnO4 with a rhombohedral crystal structure is 6.357 g / cm 3 That is it. For example, in an oxide semiconductor that satisfies the atomic ratio of In:Ga:Zn=1:1:1, The density of a-like OS is 5.0g / cm 3 More than 5.9g / cm 3 Less than For example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, , the density of nc-OS and the density of CAAC-OS are 5.9 g / cm 3 More than 6.3g / cm 3 is less than.

[0364] If single crystals of the same composition are not available, single crystals of different compositions may be combined in any ratio. By combining these, it is possible to estimate the density equivalent to a single crystal of a desired composition. The density of a single crystal of a desired composition is calculated based on the ratio of the single crystals of different compositions. However, the density can be estimated by using as few types of single crystals as possible. A combined estimate is preferred.

[0365] As described above, oxide semiconductors have various structures and each structure has various characteristics. The oxide semiconductor may be, for example, an amorphous oxide semiconductor, an a-like OS, or an nc-OS. The film may be a laminated film having two or more of the CAAC-OS and CAAC-OS.

[0366] The atomic ratio of an oxide containing indium, the element M, and zinc will be described below.

[0367] First, using Figs. 27(A), 27(B), and 27(C), indium, element The range of the atomic ratio of M and zinc will be described. Note that FIG. 27 shows the range of the atomic ratio of oxygen. This is not stated.

[0368] In FIG. 27(A), FIG. 27(B), and FIG. 27(C), the dashed lines indicate In:M:Zn = (1+α):(1-α):1 atomic ratio (-1≦α≦1), In:M:Z The line where the atomic ratio of n=(1+α):(1-α):2 is In:M:Zn=(1+α) The line where the atomic ratio is In:M:Zn=(1+α):(1-α):3. The line with the atomic ratio of 4 and the atomic ratio of In:M:Zn=(1+α):(1-α):5 Represents a line that is a numerical ratio.

[0369] The dashed line indicates the atomic ratio of In:M:Zn=1:1:β (β≧0). The line where the atomic ratio of In:M:Zn=1:2:β is shown, and the line where the atomic ratio of In:M:Zn=1:3:β is shown. The line where the atomic ratio is In:M:Zn=1:4:β, the line where the atomic ratio is In:M: The line showing the atomic ratio of Zn=2:1:β and the line showing the atomic ratio of In:M:Zn=5:1:β This represents the line where

[0370] In FIG. 27(A) and FIG. 27(B), indium contained in the oxide of one embodiment of the present invention is shown. , element M, and zinc.

[0371] As an example, FIG. 28 shows the crystal structure of InMZnO4, where In:M:Zn=1:1:1. Figure 28 shows the crystal structure of InMZnO4 when observed from a direction parallel to the b axis. The layer having M, Zn, and oxygen shown in FIG. The metal element in the layer (layer) represents element M or zinc. In this case, the ratio of element M to zinc is The combination of elements M and zinc is equal. Substitution is possible between the elements M and zinc, and the arrangement is random.

[0372] InMZnO4 has a layered crystal structure (also called a layered structure), as shown in Figure 28. The layer containing indium, indium, and oxygen (hereinafter referred to as the In layer) is 1, while the (M,Zn) layer is 2. It becomes.

[0373] Indium and element M can be substituted for each other. Therefore, the elements of the (M, Zn) layer The element M can be replaced with indium and expressed as an (In, M, Zn) layer. In that case, In It has a layered structure with one layer and two (In, M, Zn) layers.

[0374] In the oxide with the atomic ratio of In:M:Zn=1:1:2, the In layer is 1, and the (M,Z n) It has a layered structure with three layers. In other words, [Zn] is large compared to [In] and [M]. As the temperature increases, when the oxide crystallizes, the ratio of the (M, Zn) layer to the In layer increases.

[0375] However, in the oxide, when the number of In layers is 1 and the number of (M, Zn) layers is not an integer, There may be multiple types of layered structures where the number of In layers is 1 and the number of (M, Zn) layers is an integer. For example, For example, when In:M:Zn=1:1:1.5, there is 1 In layer and 1 (M,Zn) layer. The layer structure is a mixture of a layer structure in which the number of (M,Zn) layers is 2 and a layer structure in which the number of (M,Zn) layers is 3. There are cases.

[0376] For example, when forming an oxide film using a sputtering device, the ratio of the number of atoms in the target is different. In particular, depending on the substrate temperature during film formation, the [Z In some cases, the [Zn] of the film may be smaller than the [n].

[0377] In addition, multiple phases may coexist in an oxide (two-phase coexistence, three-phase coexistence, etc.). For example, At atomic ratios close to the In:M:Zn=0:2:1 atomic ratio, spinel-type crystals are formed. In:M:Zn=1:0:0, two phases, a crystalline structure and a layered crystalline structure, tend to coexist. At atomic ratios close to the atomic ratio shown in Fig. 1, the bixbyite-type crystal structure and the layered crystal structure are When multiple phases coexist in an oxide, the two phases tend to coexist between different crystal structures. In some cases, grain boundaries may be formed.

[0378] In addition, by increasing the indium content, the carrier mobility (electron mobility) of the oxide This is mainly due to the fact that in the oxides containing indium, element M and zinc, The s orbital of the heavy metal contributes to carrier conduction, and by increasing the indium content, This results in a larger overlapping area of ​​s orbitals, making oxides with a high indium content. This is because the carrier mobility is higher in comparison with oxides having a lower indium content.

[0379] On the other hand, when the content of indium and zinc in the oxide is low, the carrier mobility is low. Therefore, the atomic ratio of In:M:Zn=0:1:0 and its neighboring values ​​are In the case of a ratio of the number of atoms (eg, region C shown in FIG. 27C), the insulating property is high.

[0380] When the oxide of one embodiment of the present invention is used for a channel region of a transistor, for example, In the region of FIG. 27(A), the carrier mobility is high and the layer structure with few grain boundaries is easily formed. The atomic ratio is shown in region A.

[0381] In addition, in the region B shown in FIG. 27(B), In:M:Zn=4:2:3 to 4.1, The neighboring values ​​are shown. For example, the atomic ratio of In:M:Zn=5:3:4 The oxides having the atomic ratio shown in region B are particularly highly crystalline and have good carrier It is an excellent oxide with high electron mobility.

[0382] The condition for an oxide to form a layered structure is not uniquely determined by the atomic ratio. The difficulty of forming a layered structure varies depending on the atomic ratio. However, depending on the formation conditions, a layered structure may or may not be formed. The illustrated region is a region showing an atomic ratio in which the oxide has a layered structure, and is represented by Region A to Region B. The bounds of C are not strict.

[0383] Next, the case where the oxide has a two-layer structure or a three-layer structure will be described. Consider the case where three layers of oxide S1, oxide S2, and oxide S3 are stacked in order. For example, it is preferable to use an oxide having an atomic ratio shown in region A of FIG. 27(A) for 2. It is more preferable to use an oxide having an atomic ratio shown in region B of FIG. For example, the material S1 and the oxide S3 are shown in FIG. 27(C) as region C where the insulating property is increased. The oxide having the atomic ratio of In:M:Zn is used. = 0:1:0 or a value close to that. The oxide semiconductor 108a and the layer 108_2 included in the channel region 108i shown in the embodiment In addition, the oxide S2 can be used as the oxide semiconductor 10 shown in the above embodiment. 8b, and the layer 108_1 and the layer 108_3 of the channel region 108i are, for example, It is preferable that the atomic ratio is as shown in region C.

[0384] (Embodiment 4) In this embodiment, a display device including the transistor described in the above embodiment will be An example will be described below with reference to FIGS.

[0385] FIG. 29 is a top view showing an example of a display device. The display device 700 shown in FIG. A pixel portion 702 provided on a substrate 701 and a source driver 703 provided on the first substrate 701 are A pixel portion 702, a source driver circuit portion 704, a gate driver circuit portion 706, and a a sealant 712 arranged to surround the gate driver circuit section 704 and the gate driver circuit section 706; and a second substrate 705 disposed opposite to the first substrate 701. The first substrate 701 and the second substrate 705 are sealed with a sealant 712. That is, the pixel section 702, the source driver circuit section 704, and the gate driver circuit section 706 are The first substrate 701, the sealant 712, and the second substrate 705 are used for sealing. Although not shown in FIG. 29, a display element is provided between the first substrate 701 and the second substrate 705. can be done.

[0386] The display device 700 is surrounded by a sealant 712 on the first substrate 701. A pixel section 702, a source driver circuit section 704, and a gate driver circuit section 705 are arranged in a region different from the region. and an FPC terminal portion 708 (FPC: Flexible Printed Circuit portion 706) electrically connected to the In addition, the FPC terminal portion 708 is provided with The FPC 716 is connected to the pixel section 702 and the source driver circuit Various signals are supplied to the pixel section 704 and the gate driver circuit section 706. 02, a source driver circuit section 704, a gate driver circuit section 706, and an FPC terminal section 7 08 are connected to signal lines 710. Various signals are supplied by the FPC 716. 7, are connected to a pixel section 702, a source driver circuit section 704, a gate driver circuit section 705, and the like via a signal line 710. The wiring is provided to a driver circuit portion 706 and an FPC terminal portion 708.

[0387] The display device 700 may include a plurality of gate driver circuits 706. The device 700 includes a source driver circuit section 704 and a gate driver circuit section 706. Although an example in which the pixel portion 702 is formed on the same first substrate 701 is shown, the present invention is not limited to this configuration. For example, only the gate driver circuit section 706 may be formed on the first substrate 701. Alternatively, only the source driver circuit portion 704 may be formed on the first substrate 701. In this case, the substrate on which the source driver circuit or the gate driver circuit is formed (for example, A driving circuit board formed of a monocrystalline semiconductor film or a polycrystalline semiconductor film is mounted on a first substrate 701. The method of connecting the separately formed drive circuit board is not particularly limited. Instead, we use COG (Chip On Glass) method, wire bonding method, etc. can be used.

[0388] The display device 700 also includes a pixel portion 702, a source driver circuit portion 704, and a gate The driver circuit portion 706 includes a plurality of transistors. For example, a transistor having a gate driver circuit section may be used. The transistor has a voltage between the source and gate of -40V or more and 40V or less, more preferably A voltage of −5 V or more and 30 V or less, more preferably −1 V or more and 20 V or less, is applied to the terminals.

[0389] The display device 700 can also include various elements, such as: Liquid crystal elements, EL (electroluminescence) elements (EL elements containing organic and inorganic materials, Organic EL elements, inorganic EL elements), LEDs (white LEDs, red LEDs, green LEDs, blue LEDs ED, etc.), transistors (transistors that emit light according to the current), electron emitters, electron Ink, electrophoretic element, grating light valve (GLV), plasma display Using panels (PDP) and MEMS (Micro-Electro-Mechanical Systems) Display element, Digital Micromirror Device (DMD), DMS (Digital Micromirror Device) Shutter), MIRASOL (registered trademark), IMOD (Interferometric Modulation modulation element, shutter-type MEMS display element, optical interference-type MEMS display element, electrowetting element, piezoelectric ceramic display, carbon nanotube The display element may be a light-emitting diode or a light-emitting diode. The display medium has a contrast, brightness, reflectance, transmittance, etc. that change depending on the action of the light. An example of a display device using an EL element is an EL display. An example of a display device using emission elements is a field emission display (FE D) or SED type flat panel display (SED: Surface-conductio n Electron-emitter Display) and others. An example of such a display device is a liquid crystal display (transmissive liquid crystal display, semi-transmissive liquid crystal display, etc.). Display, reflective LCD display, direct-view LCD display, projection LCD display An example of a display device using electronic ink or electrophoretic elements is the electronic Paper, etc. In addition, semi-transmissive LCD displays and reflective LCD displays have been realized. In this case, a part or the whole of the pixel electrode is arranged to function as a reflective electrode. For example, a part or the whole of the pixel electrode may be made of aluminum, silver, etc. In this case, a memory circuit such as an SRAM may be provided under the reflective electrode. This makes it possible to further reduce power consumption.

[0390] The display method of the display device 700 may be a progressive method or an interlace method. In addition, the color elements controlled by pixels when displaying in color are R It is not limited to the three colors GB (R stands for red, G stands for green, B stands for blue). For example, It may be composed of four pixels: a pixel, a pixel, and a pixel of white (W). As in the column, two colors of RGB form one color element, and different two colors are generated depending on the color element. You can also select colors to configure the color. Or, you can select one or more colors such as yellow, cyan, and magenta for RGB. The size of the display area may be different for each dot of the color element. However, the disclosed invention is not limited to color display devices, and may be used in monochrome display devices. The present invention can also be applied to display devices.

[0391] In addition, the backlight (organic EL element, inorganic EL element, LED, fluorescent lamp, etc.) is white light ( In order to display full color on a display device, a colored layer (also called a color filter) is used. The colored layer may be, for example, red (R), green (G), blue (B) , yellow (Y), etc. can be used in appropriate combination. The color reproducibility can be improved compared to when no color layer is used. By disposing a region having a colored layer and a region not having a colored layer, The white light in the region may be directly used for display. This reduces the decrease in brightness caused by the colored layer during bright display, reducing power consumption by 20%. However, it may be possible to reduce the amount of light emitted by organic EL elements and inorganic EL elements by about 30%. When using elements to display full color, R, G, B, Y, and white (W) are It is also possible to emit light from an element having a luminescent color. By using a self-luminous element, it is possible to use a colored layer. In some cases, power consumption can be reduced even further than when the

[0392] In this embodiment, a liquid crystal element and an EL element are used as display elements. 30 and 31. Note that FIG. 30 shows the state of the circuit shown in FIG. FIG. 31 is a cross-sectional view of the liquid crystal display device shown in FIG. 29 is a cross-sectional view taken along the dashed line QR shown in FIG. 29, and shows a configuration in which an EL element is used as a display element. It is.

[0393] First, the common parts shown in FIG. 30 and FIG. 31 will be explained, and then the different parts will be explained. This will be explained below.

[0394] <Explanation of common parts of display device> The display device 700 shown in FIG. 30 and FIG. 31 includes a wiring portion 711 and a pixel portion 702. The display panel 700 includes a source driver circuit section 704 and an FPC terminal section 708. The line portion 711 includes a signal line 710. The pixel portion 702 includes a transistor 750 and The source driver circuit portion 704 includes a transistor 752. Yes.

[0395] The transistors 750 and 752 may be the transistors shown above. can.

[0396] The transistor used in this embodiment is made of a highly purified oxide film in which the formation of oxygen vacancies is suppressed. The transistor has a semiconductor film. Therefore, the retention time of electric signals such as image signals can be extended, and the power supply When the write interval is on, it is possible to set it longer. This reduces the frequency of refresh operations. This has the effect of reducing power consumption.

[0397] In addition, the transistor used in this embodiment has a relatively high field-effect mobility. For example, a transistor capable of such high speed operation can be used for a liquid crystal display. By using this in a display device, the switching transistor in the pixel section and the driver circuit section In other words, the driver transistor can be formed on the same substrate as the driver circuit. Therefore, it is not necessary to use a semiconductor device formed from a silicon wafer or the like. The number of components can be reduced. By using a register, a high quality image can be provided.

[0398] The capacitor 790 has a structure having a dielectric between a pair of electrodes. One electrode of the transistor 790 is a conductive film that functions as a gate electrode of the transistor 750. The other electrode of the capacitor 790 is formed using a conductive film formed in the same process as that of the transistor. A conductive film is used to function as the source electrode and the drain electrode of the transistor 750. The dielectric sandwiched between the electrodes functions as the gate insulating film of the transistor 750. An insulating film is used.

[0399] 30 and 31, a transistor 750, a transistor 752, and a capacitor Over the quantum dot element 790, insulating films 764, 766, and 768, an oxide semiconductor film 767, and a planarizing An insulating film 770 is provided.

[0400] The insulating films 764, 766, and 768 are the same as the insulators 114 shown in the previous embodiment. , 116, 118 can be formed by the same material and manufacturing method. The oxide semiconductor film 767 can be formed using a material similar to that of the oxide semiconductor 108 in the above embodiment. The planarization insulating film 770 can be formed by a method using a polyimide film. Resin, acrylic resin, polyimide amide resin, benzocyclobutene resin, polyamide resin Heat-resistant organic materials such as epoxy resins can be used. The planarization insulating film 770 may be formed by stacking a plurality of insulating films formed in the above manner. The planarization insulating film 770 may not be provided.

[0401] The signal line 710 is connected to the source and drain electrodes of the transistors 750 and 752. The signal line 710 is formed in the same process as the conductive film that functions as the transistor 75. 0, 752, a conductive film formed in a process different from the source electrode and drain electrode, e.g., The signal line 710 may be a conductive film that functions as a conductive electrode. When this material is used, there is little signal delay caused by wiring resistance, making it possible to display images on a large screen. do.

[0402] The FPC terminal portion 708 includes a connection electrode 760, an anisotropic conductive film 780, and an FPC 71. 6. The connection electrode 760 is connected to the source and drain electrodes of the transistors 750 and 752. The connection electrode 760 is formed in the same process as the conductive film that functions as the drain electrode. The terminal of the PC 716 is electrically connected via an anisotropic conductive film 780 .

[0403] The first substrate 701 and the second substrate 705 may be, for example, a glass substrate. In addition, the first substrate 701 and the second substrate 705 may be flexible substrates. The flexible substrate may be, for example, a plastic substrate. do.

[0404] In addition, a structure 778 is provided between the first substrate 701 and the second substrate 705. The structure 778 is a columnar spacer obtained by selectively etching an insulating film. A device for controlling the distance (cell gap) between the first substrate 701 and the second substrate 705 is provided. In addition, a spherical spacer may be used as the structure 778. In this embodiment, the structure 778 is provided on the first substrate 701 side. However, the present invention is not limited to this. For example, a structure 778 may be provided on the second substrate 705 side. Alternatively, the structures 778 may be provided on both the first substrate 701 and the second substrate 705. .

[0405] In addition, on the second substrate 705 side, a light-shielding film 738 functioning as a black matrix and A colored film 736 that functions as a color filter, a light-shielding film 738 that is in contact with the colored film 736, and An insulating film 734 is provided.

[0406] <Example of the configuration of a display device using a liquid crystal element as a display element> The display device 700 shown in FIG. 30 includes a liquid crystal element 775. The liquid crystal element 775 includes a conductive film The conductive film 774 is a second substrate 705. The display device 700 shown in FIG. The alignment state of the liquid crystal layer 776 changes depending on the voltage applied to the conductive film 772 and the conductive film 774. By controlling the light transmission or non-transmission, an image can be displayed.

[0407] The conductive film 772 serves as a source electrode and a drain electrode of the transistor 750. The conductive film 772 is connected to a conductive film that functions as a pixel electrode. The conductive film 772 functions as a reflective electrode, that is, one of the electrodes of the display element. The display device 700 shown in FIG. The liquid crystal display device 730 is a so-called reflective color liquid crystal display device, which reflects the light and displays it through the colored film 736.

[0408] The conductive film 772 may be a conductive film that transmits visible light or a conductive film that reflects visible light. A conductive film having a reflectivity can be used. For example, a material containing one of the elements indium (In), zinc (Zn), and tin (Sn) As a conductive film that is reflective in visible light, for example, aluminum In this embodiment, the conductive film 772 may be formed of A conductive film that is reflective in visible light is used.

[0409] In addition, when a conductive film that is reflective to visible light is used as the conductive film 772, the conductive film The film may have a laminated structure. For example, an aluminum film having a thickness of 100 nm is formed on the lower layer, A 30 nm thick silver alloy film (e.g., an alloy film containing silver, palladium, and copper) is formed on the upper layer. The above-mentioned structure provides the following excellent effects.

[0410] (1) The adhesiveness between the base film and the conductive film 772 can be improved. (2) By using a chemical solution, It is possible to etch the aluminum film and the silver alloy film at the same time. (3) Conductivity The cross-sectional shape of the membrane 772 can be made to have a good shape (for example, a tapered shape). (3) The reason is that the etching rate of the aluminum film by the chemical solution is slower than that of the silver alloy film. Or, when the lower aluminum film is exposed after etching the upper silver alloy film, the silver alloy The electrons are drawn from aluminum, which is a metal that is less noble than the membrane, in other words, has a high ionization tendency. Therefore, etching of the silver alloy film is suppressed and etching of the underlying aluminum film progresses. This is because the journey will be faster.

[0411] In the display device 700 shown in FIG. 30, the planarization insulating film 770 of the pixel section 702 The unevenness is formed in a part of the insulating film 770 by, for example, forming an organic resin film or the like. The reflecting current can be formed by forming a reflecting current on the surface of the organic resin film and providing the reflecting current on the surface of the organic resin film. The conductive film 772, which functions as an electrode, is formed along the above-mentioned unevenness. When light enters the conductive film 772, the light can be diffusely reflected on the surface of the conductive film 772. This makes it possible to improve visibility.

[0412] The display device 700 shown in FIG. 30 is a reflective color liquid crystal display device. However, the present invention is not limited to this. For example, the conductive film 772 may be a conductive film that transmits visible light. A transmissive color liquid crystal display device may be formed by using the above-mentioned. In this case, the unevenness provided in the planarization insulating film 770 does not necessarily have to be provided.

[0413] Although not shown in FIG. 30, the conductive films 772 and 774 on the side in contact with the liquid crystal layer 776 In addition, although not shown in FIG. Optical members (optical substrates) such as optical members, phase difference members, and anti-reflection members may be provided as appropriate. For example, circularly polarized light produced by a polarizing substrate and a retardation substrate may be used. Crites, sidelights, etc. may also be used.

[0414] When liquid crystal elements are used as display elements, thermotropic liquid crystal, low molecular weight liquid crystal, high molecular weight liquid crystal, For example, a liquid crystal, a polymer-dispersed liquid crystal, a ferroelectric liquid crystal, an antiferroelectric liquid crystal, etc. can be used. Depending on the conditions, the liquid crystal material can have a cholesteric phase, a smectic phase, a cubic phase, or a chiral phase. It shows nematic phase, isotropic phase, etc.

[0415] In addition, when the in-plane switching method is adopted, liquid crystal that exhibits a blue phase without using an alignment film may be used. The blue phase is one of the liquid crystal phases. When the temperature of a cholesteric liquid crystal is increased, the cholesteric The blue phase appears just before the transition from the black phase to the isotropic phase. In order to improve the temperature range, a liquid crystal composition containing a chiral agent of several weight percent or more is used. The liquid crystal composition containing the liquid crystal exhibiting the blue phase and the chiral agent is used in the liquid crystal layer. The liquid crystal composition containing the liquid crystal exhibiting the blue phase and the chiral agent has a short wavelength and is optically isotropic. The composition does not require alignment treatment and has low viewing angle dependency. Also, no alignment film is required. This eliminates the need for rubbing, preventing electrostatic damage caused by rubbing. This can prevent the liquid crystal display device from being damaged or broken during the manufacturing process.

[0416] In addition, when liquid crystal elements are used as display elements, TN (Twisted Nematic) ) mode, IPS (In-Plane-Switching) mode, FFS (Frin ge Field Switching) mode, ASM (Axially Symme tric aligned Micro-cell) mode, OCB(Optical Compensated Birefringence mode, FLC (Ferrero lectric Liquid Crystal) mode, AFLC (AntiFerr Electrochemical Liquid Crystal (ECC) mode can be used. .

[0417] In addition, normally black type liquid crystal display devices, for example, those using a vertical alignment (VA) mode The vertical alignment mode may be a transmission type liquid crystal display device. For example, MVA (Multi-Domain Vertical Alignment) ) mode, PVA (Patterned Vertical Alignment) mode mode, ASV mode, etc. can be used.

[0418] <Display device using light-emitting elements as display elements> The display device 700 shown in FIG. 31 includes a light-emitting element 782. The light-emitting element 782 includes a conductive film The display device 700 shown in FIG. The EL layer 786 of the light element 782 emits light, thereby displaying an image. do.

[0419] The conductive film 784 serves as a source electrode and a drain electrode of the transistor 750. The conductive film 784 is connected to a conductive film that functions as a pixel electrode. The conductive film 784 functions as an electrode, that is, one of the electrodes of the display element. In the above, a conductive film that transmits light or a conductive film that reflects visible light can be used. Examples of conductive films that are transparent to visible light include indium (In), zinc (Zn), and ZnO. It is recommended to use a material containing one of the following elements: Zn (Zn) or tin (Sn). The reflective conductive film may be made of a material containing aluminum or silver. stomach.

[0420] In addition, in the display device 700 shown in FIG. An insulating film 730 is provided. The insulating film 730 covers a part of the conductive film 784. 782 has a top emission structure. Therefore, the conductive film 788 has a light transmitting property, and It transmits the light emitted by the L layer 786. In this embodiment, the top emission The structure is exemplified, but is not limited to this. For example, a bottom emission structure in which light is emitted to both the conductive film 784 and the conductive film 788; It can also be applied to al-emission structures.

[0421] A colored film 736 is provided at a position overlapping the light emitting element 782, and a colored film 736 is provided at a position overlapping the insulating film 730. A light-shielding film 738 is provided at the position where the light-shielding film 738 is to be formed, the wiring portion 711, and the source driver circuit portion 704. The colored film 736 and the light-shielding film 738 are covered with an insulating film 734. In addition, the space between the light emitting element 782 and the insulating film 734 is filled with a sealing film 732. In the display device 700 shown in FIG. 1, a configuration in which a colored film 736 is provided is illustrated. For example, when the EL layer 786 is formed by coloring, The film 736 may not be provided.

[0422] The structure described in this embodiment may be used in appropriate combination with structures described in other embodiments. can be done.

[0423] (Embodiment 5) In this embodiment, a display device including a semiconductor device of one embodiment of the present invention will be described with reference to FIG. This will be used to explain.

[0424] The display device shown in FIG. 32(A) has a region having pixels of a display element (hereinafter, referred to as a pixel portion 502). ) and a circuit section ( hereinafter referred to as a drive circuit section 504) and a circuit having a function of protecting the element (hereinafter referred to as a protection circuit 50 6) and a terminal portion 507. Note that the protection circuit 506 is not provided. This is also fine.

[0425] A part or the whole of the driver circuit portion 504 is formed on the same substrate as the pixel portion 502. This makes it possible to reduce the number of parts and terminals. When a part or the whole of the pixel portion 502 is not formed on the same substrate, the driving circuit A part or the whole of the path portion 504 is COG or TAB (Tape Automated Band). It can be implemented by using the onding.

[0426] The pixel section 502 is arranged in X rows (X is a natural number of 2 or more) and Y columns (Y is a natural number of 2 or more). The display device has a circuit for driving a plurality of display elements (hereinafter, referred to as pixel circuit 501), The path section 504 is a circuit (hereinafter, a gate driver) that outputs a signal (scanning signal) for selecting a pixel. 504a) to provide a signal (data signal) for driving the display element of the pixel. The pixel circuit 504 includes a driver circuit such as a circuit (hereinafter, referred to as a source driver 504b).

[0427] The gate driver 504a includes a shift register and the like. A signal for driving the shift register is input via a terminal unit 507, and a signal is output. For example, a start pulse signal, a clock signal, etc. are input to the gate driver 504a. The gate driver 504a outputs a pulse signal. The gate has a function of controlling the potential of the scanning lines GL_1 to GL_X. A plurality of drivers 504a are provided, and the scanning lines GL_1 to Alternatively, the gate driver 504a may control the GL_X by dividing it. However, the gate driver 50 has a function of supplying 4a may also provide another signal.

[0428] The source driver 504b includes a shift register and the like. Through the terminal section 507, a signal for driving the shift register as well as a source of a data signal are input. The source driver 504b outputs a pixel circuit based on the image signal. The source driver 504b has a function of generating a data signal to be written to the source driver 501. A data signal is generated according to a pulse signal obtained by inputting a start pulse, a clock signal, etc. The source driver 504b has a function of controlling the output of a data signal. The data lines DL_1 to DL_Y are connected to the data line 101 through the data line 102. Alternatively, the source driver 504b may have a function of supplying an initialization signal. However, the present invention is not limited to this, and the source driver 504b may also supply other signals. It is possible.

[0429] The source driver 504b is configured using, for example, a plurality of analog switches. The source driver 504b sequentially turns on a number of analog switches, The image signal can be time-division-multiplexed and output as a data signal. Also, a shift register, etc. This may be used to configure the source driver 504b.

[0430] Each of the plurality of pixel circuits 501 is connected to one of the plurality of scanning lines GL to which a scanning signal is applied. A pulse signal is inputted through the data line DL, and a data signal is given through one of the data lines DL. A data signal is input to each of the pixel circuits 501. 504a controls writing and holding of data of the data signal. For example, The second pixel circuit 501 is connected to a gate driver GL_m (where m is a natural number equal to or smaller than X) via a scanning line GL_m. A pulse signal is input from 504a, and the data line DL_n ( A data signal is input from the source driver 504b via a source driver 504c (n is a natural number equal to or smaller than Y).

[0431] The protection circuit 506 shown in FIG. 32(A) is, for example, a gate driver 504a and a pixel circuit 5 01. Alternatively, the protection circuit 506 is connected to the scanning line GL, which is the wiring between the source driver The data line DL is connected between the driver 504b and the pixel circuit 501. The protection circuit 506 can be connected to a wiring between the gate driver 504a and the terminal unit 507. Alternatively, the protection circuit 506 may be a wiring between the source driver 504b and the terminal unit 507. The terminal unit 507 can be connected to a power supply and a power supply line from an external circuit to the display device. This refers to the part provided with terminals for inputting control signals and image signals.

[0432] When a potential outside a certain range is applied to the wiring to which the protection circuit 506 is connected, the protection circuit This is a circuit that brings one wire into electrical continuity with another wire.

[0433] As shown in FIG. 32A, a protection circuit 50 is provided in each of a pixel section 502 and a driver circuit section 504. 6, ESD (Electro Static Discharge: This can improve the resistance of the display device to overcurrent caused by electrostatic discharge (ESD) and the like. However, the configuration of the protection circuit 506 is not limited to this. For example, A configuration in which a protection circuit 506 is connected, or a protection circuit 506 is connected to the source driver 504b Alternatively, a protection circuit 506 may be connected to the terminal portion 507. It can also be done like this.

[0434] In FIG. 32A, the gate driver 504a and the source driver 504b Therefore, although an example in which the driver circuit portion 504 is formed is shown, the present invention is not limited to this configuration. For example, only the gate driver 504a is formed, and a source driver circuit is formed separately. A substrate (for example, a drive circuit substrate formed of a single crystal semiconductor film or a polycrystalline semiconductor film) is It may also be configured to be equipped with

[0435] In addition, the pixel circuits 501 shown in FIG. 32(A) may have a configuration shown in FIG. 32(B), for example. It can be said that:

[0436] The pixel circuit 501 shown in FIG. 32B includes a liquid crystal element 570, a transistor 550, and a capacitor. The transistor 550 may be any of the transistors described in the previous embodiment. can be applied.

[0437] The potential of one of the pair of electrodes of the liquid crystal element 570 is appropriately set according to the specifications of the pixel circuit 501. The alignment state of the liquid crystal element 570 is set by the written data. A common potential is applied to one of a pair of electrodes of the liquid crystal element 570 in each of the pixel circuits 501. A common potential may be applied to the pair of liquid crystal elements 570 of the pixel circuits 501 in each row. A different potential may be applied to one of the electrodes.

[0438] For example, the display device including the liquid crystal element 570 can be driven in a TN mode, an STN mode, or the like. Mode, VA mode, ASM (Axially Symmetric Aligned M icro-cell mode, OCB (Optically Compensated Birefringence mode, FLC (Ferroelectric Liquid id Crystal) mode, AFLC (AntiFerroelectric Li quid Crystal) mode, MVA mode, PVA (Patterned Ve Vertical Alignment mode, IPS mode, FFS mode, or TBA (Transverse Bend Alignment) mode, etc. may also be used. In addition to the above-mentioned driving method, the display device can be driven by an ECB (Electric Carrier Bipolar Transistor) or the like. Ally Controlled Birefringence mode, PDLC(P Oligomeric Dispersed Liquid Crystal (PNLC) mode (Polymer Network Liquid Crystal) mode, guest hole However, there are various types of liquid crystal elements and their driving methods, and they are not limited to these. A variety of different types of sensors can be used.

[0439] In the pixel circuit 501 in the mth row and the nth column, One of the electrodes is electrically connected to the data line DL_n, and the other is a pair of electrodes of the liquid crystal element 570. The gate electrode of the transistor 550 is electrically connected to the other of the scan lines G The transistor 550 is electrically connected to the data signal writing terminal L_m. It has the function of controlling.

[0440] One of a pair of electrodes of the capacitor 560 is connected to a wiring to which a potential is supplied (hereinafter, a potential supply line VL ) and the other is electrically connected to the other of the pair of electrodes of the liquid crystal element 570. The value of the potential of the potential supply line VL is set appropriately according to the specifications of the pixel circuit 501. The capacitor 560 functions as a storage capacitor for storing written data.

[0441] For example, in a display device having the pixel circuit 501 shown in FIG. The pixel circuits 501 in each row are sequentially selected by a gate driver 504a shown in FIG. 550 is turned on to write data of the data signal.

[0442] In the pixel circuit 501 in which data has been written, the transistor 550 is turned off. By repeating this process row by row, an image can be displayed.

[0443] In addition, the pixel circuits 501 shown in FIG. 32(A) may have a configuration shown in FIG. It can be said that:

[0444] The pixel circuit 501 shown in FIG. 32C includes transistors 552 and 554 and a capacitance element. The transistor 552 and the transistor 554 include a light-emitting element 562 and a light-emitting element 568. The transistor described in the above embodiment can be used for either or both of the above. .

[0445] A data signal is applied to one of the source and drain electrodes of the transistor 552. The transistor 55 is electrically connected to a wiring (hereinafter, referred to as a signal line DL_n). The gate electrode of 2 is electrically connected to the wiring (hereinafter referred to as the scanning line GL_m) to which the gate signal is applied. are connected to the network.

[0446] The transistor 552 has a function of controlling writing of data signals.

[0447] One of a pair of electrodes of the capacitor 562 is connected to a wiring to which a potential is applied (hereinafter, a potential supply line VL _a), and the other is electrically connected to the source electrode and drain electrode of the transistor 552. The second electrode is electrically connected to the other of the first and second electrodes.

[0448] The capacitor 562 functions as a storage capacitor for storing written data.

[0449] One of the source electrode and the drain electrode of the transistor 554 is connected to the potential supply line VL_a. In addition, the gate electrode of the transistor 554 is electrically connected to the It is electrically connected to the other of the source electrode and the drain electrode.

[0450] One of the anode and the cathode of the light-emitting element 568 is electrically connected to the potential supply line VL_b. The other one is electrically connected to the other of the source electrode and drain electrode of the transistor 554. will be done.

[0451] The light-emitting element 568 may be, for example, an organic electroluminescence element (also called an organic EL element). However, the light-emitting element 568 is not limited to this. Alternatively, an inorganic EL element made of an inorganic material may be used.

[0452] A high power supply potential VDD is applied to one of the potential supply lines VL_a and VL_b. and the other is supplied with a low power supply potential VSS.

[0453] In a display device having the pixel circuit 501 shown in FIG. 32C, for example, The pixel circuits 501 in each row are sequentially selected by the gate driver 504a, and the transistors 552 are turned on. The data signal is written by turning it on.

[0454] In the pixel circuit 501 to which the data has been written, the transistor 552 is turned off. Furthermore, the transistor 554 is in a holding state in response to the potential of the written data signal. The amount of current flowing between the source electrode and the drain electrode is controlled, and the light emitting element 568 is The light is emitted with a brightness that corresponds to the flow rate. By performing this process row by row, an image can be displayed.

[0455] The structure described in this embodiment may be used in appropriate combination with structures described in other embodiments. can be done.

[0456] (Embodiment 6) In this embodiment, a display module and an electronic device each including a semiconductor device according to one embodiment of the present invention will be described. This will be described with reference to FIG. 33 and FIG.

[0457] The display module 8000 shown in FIG. 33 includes an upper cover 8001 and a lower cover 8002. Between them, there is a touch panel 8004 connected to the FPC 8003 as a touch sensor. In addition, the display panel 8006, the backlight 8007, and the It has a frame 8009, a printed circuit board 8010, and a battery 8011.

[0458] The semiconductor device of one embodiment of the present invention can be used for the display panel 8006, for example.

[0459] The upper cover 8001 and the lower cover 8002 are connected to the touch panel 8004 and the display panel The shape and dimensions can be changed as appropriate to match the size of 8006.

[0460] The touch panel 8004 is a resistive or capacitive touch panel. The display panel 8006 can be used by overlapping it with the opposing substrate (sealing substrate). It is also possible to provide the display panel 8 with a touch panel function. It is also possible to provide an optical sensor in each pixel of the display panel 006 to make it into an optical touch panel.

[0461] The backlight 8007 has a light source 8008. In FIG. In the above example, the light source 8008 is disposed on the light source 8007, but the present invention is not limited to this example. For example, a light source 8008 is arranged at the end of a backlight 8007, and a light diffusion plate is further used. In addition, when a self-luminous light-emitting element such as an organic EL element is used, or when a reflective In the case of a flat panel or the like, the backlight 8007 need not be provided.

[0462] The frame 8009 protects the display panel 8006 and also supports the movement of the printed circuit board 8010. It also functions as an electromagnetic shield to block electromagnetic waves generated by the operation of the frame. The frame 8009 may also function as a heat sink.

[0463] The printed circuit board 8010 includes a power supply circuit, a signal circuit for outputting a video signal, and a clock signal. The power supply circuit is provided with a signal processing circuit. Alternatively, the power source may be a battery 8011 provided separately. , this can be omitted when using a commercial power source.

[0464] In addition, the display module 8000 includes components such as a polarizing plate, a retardation plate, and a prism sheet. It may be added.

[0465] 34(A) to 34(G) are diagrams showing electronic devices. These electronic devices are housed in a housing. A body 9000, a display unit 9001, a speaker 9003, and operation keys 9005 (power switch, etc.) includes an operation switch), a connection terminal 9006, a sensor 9007 (force, displacement, position, speed, Acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical substances, sound, time, hardness, electricity Measures field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, odor, or infrared rays The device may have a built-in microphone 9008, etc.

[0466] The electronic devices illustrated in FIGS. 34A to 34G can have various functions. For example, the function to display various information (still images, videos, text images, etc.) on the display, Panel function, calendar, date or time display function, various software ( A function to control processing by a program, wireless communication function, and various functions using wireless communication function Functions for connecting to computer networks, transmitting various data using wireless communication functions, or receiving the program or data recorded on the recording medium, and displaying the program or data. The display unit may have a function to display the information on the display unit. The functions that the electronic device shown in the figure can have are not limited to these, and the electronic device may have a variety of functions. Although not shown in FIG. 34(A) to FIG. 34(G), the electronic device may include The electronic device may have a plurality of display units. It is preferable to provide the electronic device with a camera or the like, and to provide a function of taking still images, a function of taking videos, a function of taking pictures, and a function of taking pictures. The function to save the captured image to a recording medium (external or built-in to the camera), and to display the captured image The display unit 10 may have a function of displaying the information on the display unit 10 in the display unit 10 .

[0467] The imaging device includes a circuit using a transistor having an oxide semiconductor in a channel region, By using the transistor in a circuit of an imaging device, for example, a high-speed In imaging at 300 nm, it is possible to obtain excellent images with little distortion.

[0468] The electronic devices shown in FIGS. 34A to 34G will be described in detail below.

[0469] FIG. 34A is a perspective view showing a portable information terminal 9100. The display unit 9001 has flexibility. The display unit 9001 can be incorporated along the screen. The device is equipped with a touch sensor, and can be operated by touching the screen with a finger or a stylus. By touching the icon displayed on the display 9001, the application can be started. can.

[0470] FIG. 34B is a perspective view showing a portable information terminal 9101. For example, the device has one or more functions selected from a telephone, a notebook, an information viewing device, etc. Specifically, the mobile information terminal 9101 can be used as a smartphone. Although the speaker 9003, the connection terminal 9006, the sensor 9007, etc. are omitted in the figure, It can be installed in the same position as the mobile information terminal 9100 shown in FIG. The information terminal 9101 can display text and image information on multiple surfaces. For example, Three operation buttons 9050 (also called operation icons or simply icons) are displayed on the display unit 900. The information 9051 shown in the dashed rectangle can be displayed on one side of the display unit 90. 01. An example of the information 9051 is an e-mail Displays to notify you of incoming calls, SNS (social networking services), etc. , subject of email or SNS, sender name of email or SNS, date and time, time, Battery level, antenna reception strength, etc. Or, information 9051 is displayed. Instead of the information 9051, an operation button 9050 or the like may be displayed at that position.

[0471] FIG. 34C is a perspective view showing a portable information terminal 9102. , and has a function of displaying information on three or more faces of the display unit 9001. An example is shown in which information 9053 and information 9054 are displayed on different sides. The user of the portable information terminal 9102 holds the portable information terminal 9102 in the breast pocket of the clothes. In this state, the display (information 9053 in this case) can be confirmed. The telephone number or name of the caller is displayed on the mobile information terminal 9102 so that it can be observed from above. The user can read the display without taking the mobile information terminal 9102 out of his pocket. You can check the number and decide whether to answer the call or not.

[0472] 34(D) is a perspective view showing a wristwatch-type portable information terminal 9200. The 9200 is used for mobile phone calls, e-mail, document browsing and writing, music playback, and Internet communications. It is possible to execute various applications such as computer games. The display unit 9001 has a curved display surface, and displays information along the curved display surface. In addition, the portable information terminal 9200 can perform short-distance wireless communication according to a communication standard. For example, by communicating with a wireless headset, The mobile information terminal 9200 also has a connection terminal 9006. It has a connector and can directly exchange data with other information terminals. Charging can also be performed via the connection terminal 9006. Power may also be supplied wirelessly without going through 6.

[0473] 34(E), (F), and (G) are perspective views showing a foldable portable information terminal 9201. FIG. 34(E) is a perspective view of the portable information terminal 9201 in an unfolded state. (F) shows the mobile information terminal 9201 being changed from one of the unfolded and folded states to the other. FIG. 34(G) is a perspective view of the portable information terminal 9201 in a folded state. The portable information terminal 9201 is highly portable when folded and is unfolded. When the display is turned on, the seamless, wide display area provides excellent visibility of the display. The display unit 9001 of the display device 9001 is made up of three housings 9000 connected by hinges 9055. The two housings 9000 are supported by the hinge 9055. The portable information terminal 9201 can be reversibly transformed from an unfolded state to a folded state. For example, the portable information terminal 9201 can be bent with a radius of curvature of 1 mm or more and 150 mm or less. It can be done.

[0474] The electronic device described in this embodiment has a display unit for displaying some information. However, the semiconductor device of one embodiment of the present invention is an electronic device that does not have a display portion. The present invention can also be applied to the display unit of the electronic device described in this embodiment. In the case of a display device, the display device may be flexible and capable of displaying information along a curved display surface, or may be folded. Although a foldable display unit has been exemplified, the present invention is not limited to this. A display may be provided on the surface.

[0475] The structure described in this embodiment may be used in appropriate combination with structures described in other embodiments. can be done.

[0476] (Embodiment 7) In this embodiment, a semiconductor device according to one embodiment of the present invention will be described.

[0477] [Semiconductor Devices] FIG. 35A shows an example of a circuit included in the semiconductor device 10. 35A shows an example of a cross-sectional view of a semiconductor device 10 having the circuit shown in FIG.

[0478] The semiconductor device 10 shown in FIG. 35B includes five layers, ie, layers 627 to 631. Layer 627 includes transistor 493, transistor 494, etc. Layer 629 includes transistors 490, etc. The layer 631 includes the capacitor elements C1, etc.

[0479] <layer 627> Layer 627 includes substrate 400 and transistors 493 and 494 on substrate 400. etc., an insulator 464 over transistors 493 etc., and plugs such as plug 541. The plugs 541 and the like are, for example, gate electrodes, source electrodes, or drain electrodes of the transistors 493 and the like. The transistor 493 and the transistor 494 are connected to the electrode. do.

[0480] The insulator 464 may be, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, or nitrogen. Silicon nitride, aluminum oxide, aluminum oxynitride, aluminum nitride oxide, aluminum nitride Aluminum or the like may be used.

[0481] The insulator 464 is silicon carbonitride. Silicon oxycarbide, silicon oxycarbide, etc. In addition, USG (Undoped Silicate Glass), BPS G(Boron Phosphorus Silicate Glass), BSG(B orosilicate glass) can be used. USG, BPSG, etc. The film may be formed by atmospheric pressure CVD. For example, HSQ (hydrogen silsesquioxane) may be used. Here, it is preferable that the insulator 464 contains hydrogen. When the insulator 464 contains hydrogen, the substrate 400 has fewer defects and is more stable. The characteristics of the transistor 493 may be improved.

[0482] The insulator 464 may be a single layer or a laminate of multiple materials. As shown in FIG. 1, the insulating layer 464 may have two layers, an insulator 464a and an insulator 464b. Here, silicon nitride is used for the insulator 464a, and USG is used for the insulator 464b.

[0483] The layer 627 is a peripheral circuit of the semiconductor device 10 according to one embodiment of the present invention, for example, a semiconductor device having a semiconductor layer 627. A transformer for constructing circuits such as a sense amplifier circuit, a driver circuit, a main amplifier, and an input / output circuit. In addition, the layer 629 is preferably provided with a transistor having an oxide semiconductor. The memory cell of one embodiment of the present invention is preferably provided in layer 629. The peripheral circuits of the semiconductor device 10 are provided on the layer 627, and the layer 629 is laminated thereon. By providing transistor 490 in layer 629, the area of ​​semiconductor device 10 can be reduced. can be done.

[0484] <layer 628> Layer 628 includes an insulator 581, an insulator 584 on insulator 581, and an insulator 584 on insulator 584. The insulating member 571 and the insulating member 585 on the insulating member 571 are also provided. The conductor 511 and the like are connected to the insulator 584, the insulator 571, and the insulator 5 and a conductor 513 formed to fill the opening of the insulating film 85. It is preferably configured to be embedded in the body 581 .

[0485] The layer 628 also preferably includes a conductor 126. The conductor 126 is made of an insulator 5. The conductor 126 is preferably formed so as to be embedded in the transistor 4. It is preferable that the second gate electrode of the first insulating film 90 be formed of the first insulating film 90 .

[0486] For the insulator 581, the description of the insulator 464 can be referred to. For example, as shown in FIG. 35B, the insulator 581 is Alternatively, the insulator 581 may be formed as two layers, that is, an insulator 581a and an insulator 581b on the insulator 581a. 1a and insulator 581b refer to the descriptions of insulator 464a and insulator 464b, respectively. It is possible.

[0487] The insulators 584 and 585 may be made of the material described for the insulator 464. The insulators 584 and 585 may be single layers or may be stacked layers of multiple materials. They may also be used in layers.

[0488] The conductor 511, the conductor 513, the conductor 126, etc. may be made of a metal material, an alloy material, or a gold material. Conductive materials such as metal oxide materials can be used. For example, aluminum, titanium, Chromium, nickel, copper, yttrium, zirconium, niobium, molybdenum, silver, tantalum The metals, such as tungsten, or alloys containing these as the main components are used in a single layer or laminated structure. It can be used as a layer structure. Tungsten nitride, molybdenum nitride, titanium nitride Metal nitrides such as niobium and the like can be used.

[0489] In the semiconductor device according to one embodiment of the present invention, the conductor 511 and the conductor The conductor 513, the conductor 126, etc. may have a laminated structure of two or more layers.

[0490] As an example, copper can be used as the top layer of the conductor. Copper has low resistance and is It is preferable to use copper as a conductor for wiring and other purposes. On the other hand, copper is prone to diffusion and is prone to be transferred to semiconductor elements. Diffusion can degrade the characteristics of semiconductor devices. It is preferable to use a material with low copper permeability for the lower layer of the conductor or plug. The layer preferably has low permeability to hydrogen and oxygen. The material may be tantalum, tantalum nitride, titanium nitride, etc. The layer may be tungsten.

[0491] As an example of the insulator 581a, silicon nitride formed by a CVD method can be used. It is preferable to use a film from which the amount of hydrogen desorbed is small as the insulator 581a. For example, thermal desorption spectrometry (TDS) is used. The hydrogen in the insulator 581a can be analyzed by using a method such as electron spectroscopy. The amount of desorption was calculated as hydrogen atoms in the range of 50℃ to 500℃ by TDS analysis. The amount of desorption is, for example, 5 × 10 20 atoms / cm 3 Less than or equal to 1×10 20 ato ms / cm 3 Alternatively, the amount of desorption of the insulator 581a converted into hydrogen atoms is equal to or less than the absolute value. For example, 5 × 10 per area of ​​the velum 15 atoms / cm 2 Less than or equal to 1×10 1 5 atoms / cm 2 The insulator 581b has a higher dielectric constant than the insulator 581a. A low rate is preferred.

[0492] The insulator 571 is preferably formed using an insulating material that has low impurity permeability. For example, it is preferable that the insulator 571 has low oxygen permeability. It is preferable that the insulator 571 has low hydrogen permeability. Also, for example, the insulator 571 has low water permeability. is preferred.

[0493] The insulator 571 may be, for example, aluminum oxide, hafnium oxide, tantalum oxide, or Zirconium, lead zirconate titanate (PZT), strontium titanate (SrTiO 3) Or (Ba,Sr)TiO3 (BST), silicon nitride, etc. are deposited as a single layer or These insulating films can be laminated. Niobium oxide, niobium oxide, silicon oxide, titanium oxide, tungsten oxide, yttrium oxide Gallium oxide may be added to the insulating film. Alternatively, these insulating films may be nitrided to form oxynitride films. Silicon oxide, silicon oxynitride or silicon nitride may be laminated on the insulating film. In particular, aluminum oxide has excellent barrier properties against water and hydrogen. The insulator 571 may be, for example, silicon carbide, silicon carbonitride, or carbon oxide. Silicon carbide or the like may also be used.

[0494] The insulator 571 is made by laminating a layer of a material with low water and hydrogen permeability with a layer containing another insulating material. For example, a layer containing silicon oxide or silicon oxynitride, a layer containing metal oxide, etc. may be laminated and used.

[0495] For example, the semiconductor device 10 has an insulator 571, so that the conductor 513, the conductor The elements contained in the insulator 126, etc. are in the insulator 571 and the layers thereunder (insulator 584, insulator 58 1, layer 627, etc.) can be suppressed.

[0496] <layer 629> Layer 629 includes transistors such as transistor 490 and plugs 544 and 54 The plugs, such as plug 544 and plug 544b, are made of conductive material. 513, a gate electrode, a source electrode or a drain electrode of the transistor 490, etc. Connect.

[0497] The transistor 490 includes the oxide semiconductor 108. The oxide semiconductor 108 includes an oxide semiconductor 108h, an oxide semiconductor 108j, and an oxide semiconductor The transistor 490 is formed of three layers, an oxide semiconductor 108h, The oxide semiconductor 108j on the oxide semiconductor 108h and the conductor 1 12a and the conductor 112b, the top surface and the side surface of the oxide semiconductor 108j, and the conductor 11 an oxide semiconductor 108k in contact with the upper surface of the conductor 112b and the upper surface of the oxide semiconductor 108k and a conductor 104 on the insulator 106. 04 is an insulator 112a provided on the region between the conductor 112a and the conductor 112b (the region where they are spaced apart). It is preferable that the semiconductor device 10 shown in FIG. It has an insulator 591 on the conductor 104 and an insulator 408 on the insulator 591 .

[0498] The oxide semiconductor 108j is formed using, for example, the oxide semiconductor 108a described in Embodiment 1. It is possible.

[0499] For example, the layer 108_1 described in the first embodiment may be formed as the oxide semiconductor 108h. For example, the layer 108_3 described in the first embodiment can be used for the body 108k. Cut.

[0500] Conductor 112a and conductor 112b are the source or drain electrodes of transistor 490. The conductor 104 preferably serves as an in-electrode of the transistor 490. In the transistor 490, the conductor 104 is a first Preferably, the gate electrode, conductor 126, functions as a second gate electrode.

[0501] The transistor 490 of one embodiment of the present invention includes a first insulating film between the oxide semiconductor 108 and the conductor 126. The transistor 490 shown in FIG. An insulator 402b is disposed between the semiconductor 108 and the conductor 126, and an insulator 571a is disposed on the insulator 402b. , and insulator 402 on insulator 571a.

[0502] The insulator 402 and the insulator 402b may refer to the description of the insulator 584, for example. The semiconductor device 10 may not have the insulator 402b. For example, silicon oxide and silicon oxynitride (where silicon oxynitride is a material with a low nitrogen content) The insulator 402b may be, for example, For example, silicon oxide may be used.

[0503] For the insulator 571a, for example, the description of the insulator 571 can be referred to.

[0504] The insulator 571a preferably functions as a charge trapping layer. By trapping charge, the threshold voltage of transistor 490 can be controlled. In this specification, the threshold value is, for example, the gate voltage when a channel is formed. For example, the threshold voltage is expressed as the gate voltage (Vg) on ​​the horizontal axis and the square root of the drain current Id on the vertical axis. If we extrapolate the tangent line with the maximum slope in the curve (Vg-√Id characteristics) plotted on the axis, The gate voltage ( Vg).

[0505] Here, the transistor 490 is a conductive layer overlapping the oxide semiconductor 108 with the insulator 106 interposed therebetween. The insulator 104 and the oxide semiconductor 108 and an overlapping conductor 126.

[0506] As shown in the above embodiment, the conductor 126 of the transistor 490 and the By providing a potential difference between the source of the transistor 490 and the insulator 571a, the insulator 40 2 and insulator 402b to trap electric charges, and data is In addition, among the insulator 571a, the insulator 402, and the insulator 402b, two in contact with each other are stored. Charge may be trapped at the interface between the two insulators.

[0507] The charge trapping layer can be made of an insulator, a semiconductor, or a conductor. Silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, hafnium oxide Aluminum, aluminum oxide, tantalum oxide, aluminum silicate, etc. can be used. Semiconductors include polycrystalline silicon, microcrystalline silicon, amorphous silicon, and oxide semiconductors. The conductive material may be tantalum, tungsten, titanium, molybdenum, etc. The material may be selected from the group consisting of tungsten, molybdenum, aluminum, copper, and molybdenum-tungsten alloys. Tantalum nitride, tungsten nitride, titanium nitride, etc., which have the function of being difficult to transmit oxygen. They may be appropriately combined to form a multi-layer film.

[0508] The charge trapping layer preferably contains, for example, oxygen and a metal. In the layer, the proportion of metals detected by EDX analysis is 20 atomic % or more and 50 atomic % or less. The oxygen ratio is preferably 30 atomic % or more and 70 atomic % or less. The following metals are preferred: hafnium, aluminum, tantalum, tungsten, Molybdenum, etc.

[0509] Alternatively, the charge trapping layer preferably comprises silicon nitride. In the above, the nitrogen ratio is preferably 45 atomic % or more and less than 60 atomic %. The recon ratio is preferably greater than or equal to 40 atomic % and less than 55 atomic %.

[0510] The insulator 571a is formed by stacking a layer that easily captures charges and a layer that is difficult for impurities to pass through. For example, hafnium oxide may be formed as a layer that easily captures electric charges. Aluminum oxide may be laminated on the surface of the glass to make it more impermeable to impurities. Alternatively, hafnium oxide may be formed on aluminum oxide. In addition to aluminum oxide, silicon oxide may be used to form a three-layer stack. The order of lamination of the layers does not matter.

[0511] Here, since the semiconductor device 10 has the insulators 571 and 571a, the layer 62 It is possible to prevent hydrogen, water, etc. contained in the semiconductor 7 from diffusing into the transistor 490, etc. Since the body device 10 has the insulator 408, impurities from above the insulator 408, e.g. For example, the diffusion of hydrogen and water can be suppressed. In the case where a conductor is provided, the diffusion of hydrogen into the oxide semiconductor can be suppressed, thereby improving the transistor. This may prevent deterioration of characteristics.

[0512] The conductor 112a and the conductor 112b are made of the material shown in the conductor 511, for example. The conductors 112a and 112b can be made of, for example, tungsten. If the material is made of a material that easily bonds with oxygen, such as titanium, an oxide of the material will be formed. As a result, the conductors 112a and 112b are in contact with the oxide semiconductor 108 and Oxygen vacancies in the oxide semiconductor 108 may increase in the region surrounding the oxide semiconductor 108 and the oxygen vacancies in the region surrounding the oxide semiconductor 108. When hydrogen bonds to the vacancies, the carrier density in the area increases, and the resistivity decreases. The conductor 112a and the conductor 112b may be formed as a stacked film.

[0513] The material shown in the insulator 571 can be used as the insulator 408. During the deposition of the insulating film 8, excess oxygen is supplied to the interface between the insulating film 408 and the underlying film and to the vicinity thereof. It is preferable that

[0514] In addition, the insulators 571, 571a and 408 are made of a material having low oxygen permeability. By using the material, oxygen is prevented from diffusing outward from the transistor 490 etc. (for example, the insulating layer In this way, it is possible to suppress diffusion of the ions into layers below the insulator 571 or above the insulator 408. Therefore, there are cases where oxygen can be efficiently supplied to the transistor 490. When the transistor 490 or the like has an oxide semiconductor, oxygen can be easily supplied to the oxide semiconductor. This may improve the characteristics of the transistor.

[0515] <layer 630> Layer 630 includes insulator 592, conductors such as conductor 514, and plugs such as plug 545. , The plugs 545, etc. connect with conductors such as conductor 514.

[0516] <layer 631> The layer 631 includes a capacitor C1. The capacitor C1 includes a conductor 516 and a conductor 517. and an insulator 572. The insulator 572 is sandwiched between the conductor 516 and the conductor 517. Layer 631 also includes an insulator 594 and a plug 547 on conductor 517. It is preferable that the plug 547 is formed so as to be embedded in the insulator 593. Also, the layer 631 has a conductive layer that is connected to a plug (not shown) that the layer 630 has. It is preferable that the insulator 516b has a plug 547b on the conductor 516b. For 72, the description of insulator 571 can be referred to.

[0517] Layer 631 may also include a wiring layer that connects to plug 547 and plug 547b. In the example shown in FIG. 35B, the wiring layer includes the conductor 54 connected to the plug 547 and the plug 547b. 18, etc., plug 548 on conductor 518, insulator 595, and conductor on plug 548. 519 and an insulator 599 on the conductor 519. The plug 548 is embedded in the insulator 595. It is preferable that the insulator 599 is formed so as to be embedded in the conductor 519. It has an opening.

[0518] The deposition methods for insulators, conductors and semiconductors are sputtering, CVD (thermal deposition) and VD method, MOCVD method, PECVD method, etc.), MBE method, ALD method, or PLD method In particular, the insulator can be formed by a CVD method, preferably a plasma CVD method. It is preferable to form the film by plasma, since it is possible to improve the covering property. In order to reduce damage caused by the deposition, the thermal CVD method, the MOCVD method, or the ALD method is preferable.

[0519] <Transistor 493 and Transistor 494> The transistor 493 and the transistor 494 will be described below.

[0520] The transistor 493 includes a channel formation region 407, an insulator 462 on a substrate 400, and A conductor 454 on an insulator 462, an insulator 470 in contact with the side of the conductor 454, and a substrate 4 00, which is a region 476 that does not overlap with the conductor 454 and the insulator 470; The region 474 is a region overlapping the insulator 470. The region 476 is a low resistance layer. 493, which preferably functions as a source or drain region of the transistor 493. Additionally, region 474 preferably functions as an LDD (lightly doped drain) region. stomach.

[0521] The transistor 493 may be either a p-channel type or an n-channel type. An appropriate transistor may be used depending on the driving method. Transistor 494 is, for example, a transistor of the opposite polarity to transistor 493 .

[0522] The substrate 400 preferably comprises a semiconductor, such as a silicon-based semiconductor, and is preferably a single crystal It is preferable to have silicon. Alternatively, Ge (germanium), SiGe (silicon Germanium), GaAs (gallium arsenide), GaAlAs (gallium aluminum arsenide) ) or the like. Also, a configuration using silicon having a distortion in the crystal lattice may be used. Alternatively, the transistor 493 can be a HEMT ( High Electron Mobility Transistor) .

[0523] Region 476 may be doped with an element that provides n-type conductivity, such as phosphorus, or a p-type conductive element, such as boron. It is preferable that the material contains an element that imparts electrical conductivity.

[0524] The conductor 454 is an element that provides n-type conductivity, such as phosphorus, or a p-type element, such as boron. Semiconductor materials such as silicon that contain elements that give them electrical conductivity, metal materials, alloy materials, or gold Conductive materials such as metal oxide materials can be used. In particular, It is preferable to use a high melting point material such as tungsten or molybdenum, and particularly tungsten. It is preferable to use:

[0525] The transistor 493 and the transistor 494 shown in FIG. 35B are formed by trench isolation. (STI: Shallow Trench Isolation) and other methods are used to separate elements. Specifically, an oxide film is formed in a trench in the substrate 400 by etching or the like. After embedding an insulating material containing silicon dioxide, etc., the insulating material is partially etched. In the case where the transistor is isolated by the element isolation region 460 formed by removing the The following example shows a case where

[0526] In addition, in the convex portion of the substrate 400 existing in the region other than the trench, the region 476 and the region 47 4 and a channel forming region 407 are provided on the channel forming region 407. An insulator 462 covering the channel forming region 407 and a semiconductor layer 404 sandwiching the insulator 462 between the channel forming region 407 and the semiconductor layer 404 are formed. A conductor 454 is provided that overlaps area 407 .

[0527] The transistor 493 and the transistor 494 do not need to have a protruding portion on the substrate 400. For example, the transistor 493 and the transistor 494 are made of SOI (Silicon Insulator). Alternatively, the insulating layer 14 may be formed using a (on-insulator) substrate.

[0528] <Transistor 490> A top view of the transistor 490 shown in FIG. 35 is shown in FIG. The cross-sectional view corresponding to the dashed line E1-E2 and the dashed line E3-E4 shown in FIG. 36(B) is vinegar.

[0529] As shown in FIG. 36B, the oxide semiconductor 108j is electrically charged by the electric field of the conductor 104. (The electric field of a conductor can electrically surround the semiconductor.) The structure of the transistor is called the surrounded channel (s-channel) structure. Therefore, in the case where a channel is formed in the entire oxide semiconductor 108j (bulk), In the s-channel structure, a large current flows between the source and drain of the transistor. It is possible to increase the current (on-state current) when the transistor is conductive.

[0530] Because of the high on-current, the s-channel structure is suitable for miniaturized transistors. Since the transistor can be miniaturized, the structure is suitable for devices having the transistor. It is possible to make highly integrated and highly dense devices. For example, The channel length is preferably 40 nm or less, more preferably 30 nm or less, and even more preferably The transistor preferably has a channel width of 40 nm or less. m or less, more preferably 30 nm or less, and further preferably 20 nm or less.

[0531] FIG. 37 shows a structure of a transistor 490 different from that shown in FIG. 37(A) and the dashed line E1-E2 and the dashed line E3 A cross-sectional view corresponding to -E4 is shown in FIG. 37(B). In FIG. 37(B), the insulator 106 is The conductor 104 is laminated on the oxide semiconductor 108k. The oxide semiconductor 108k is formed so as to fill the opening covered by the insulator 106. And insulator 106 is formed on the side of the opening of insulator 591 .

[0532] <Circuit operation> The operation of the circuit shown in FIG. 35(A) will be described. The circuit shown in FIG. The gate potential of the transistor 494 can be maintained, as shown below. It is possible to write, retain, and read information.

[0533] The writing and holding of information will be described. First, the potential of the terminal WL is set to 0V by the transistor The transistor 490 is set to a potential at which the transistor 490 is in a conducting state, and the transistor 490 is in a conducting state. The potential of the terminal BL is connected to the gate of the transistor 494 and one of the electrodes of the capacitor C1. That is, the gate of the transistor 494 is provided to a node FN that electrically connects Then, a certain charge is applied (write). Here, two different potential levels are applied. Either a low-level charge or a high-level charge is applied. After that, the potential of the terminal WL is set to a potential at which the transistor 490 is turned off. This causes charge to be retained (held) at node FN.

[0534] By using an oxide semiconductor for the semiconductor layer of the transistor 490, the off-state current can be reduced extremely. Since the capacitance can be made extremely small, the charge on the node FN is retained for a long period of time.

[0535] Next, the reading of information will be explained. A state in which a predetermined potential (constant potential) is applied to the terminal BL Then, when an appropriate potential (read potential) is applied to the terminal CL, the terminal SL is held at the node FN. The potential depends on the amount of charge transferred. If the transistor 494 is an n-channel type, When a high-level charge is applied to the gate of transistor 494, Threshold voltage V th_H A low level charge is applied to the gate of transistor 494. The apparent threshold voltage V th_L This is because the temperature is lower than that of the The threshold voltage on the terminal C required to make the transistor 494 "conductive" is Therefore, the potential of the terminal CL is V th_H and V th_L Between By setting the potential of the node FN to V0, the charge applied to the node FN can be determined. When a high-level charge is applied to node FN, When the potential is V0 (>V th_H ), transistor 494 is "on". If a low-level charge is applied to node FN, the potential of terminal CL becomes V0 (< V th_L ), transistor 494 remains in a "non-conducting state." By determining the potential of the terminal SL, the data stored in the node FN can be read out. can.

[0536] When memory cells are arranged in an array, the information of a desired memory cell is read out. In order not to read information from other memory cells, For example, in a memory cell from which information is not read, the transistor is turned on regardless of the charge applied to the node FN. The potential at which transistor 494 is in a "non-conducting state," i.e., V th_H Lower potential may be applied to terminal CL so that only the information in a desired memory cell can be read out. Alternatively, in a memory cell from which information is not read, the charge applied to the node FN First, the potential at which transistor 494 is "conducting", i.e., V th_L Higher voltage By applying a potential to the terminal CL, it is possible to read out only the information of the desired memory cell. .

[0537] The above-described semiconductor device is a transistor using an oxide semiconductor and having an extremely small off-state current. By applying the memory, it is possible to retain the memory contents for a long period of time. Refresh operations are no longer necessary or can be performed very infrequently. Therefore, a semiconductor device with low power consumption can be realized. Even if there is no potential (but it is preferable that the potential is fixed), It is possible to retain the stored contents.

[0538] In addition, the semiconductor device does not require a high voltage to write information, so there is no risk of element deterioration. For example, unlike conventional non-volatile memory, the flow of electrons to the floating gate is Since there is no injection or extraction of electrons from the floating gate, there is no degradation of the insulator. That is, the semiconductor device according to one embodiment of the present invention does not have the same problem as the conventional nonvolatile memory. There is no limit to the number of times that memory can be rewritten, which is a problem with memory, and the reliability of the semiconductor has been dramatically improved. Furthermore, information can be written by turning on or off the transistor. This enables high speed operation. EXAMPLES

[0539] In this embodiment, a transistor having a structure shown in FIG. 15C (hereinafter referred to as transistor d A sample having the above properties was prepared and its characteristics were evaluated.

[0540] <Making a transistor> Two samples, Sample A-1 and Sample A-2, were fabricated. Fabrication of the transistors in each sample The method for preparing sample A-2 is the same as that for preparing sample A-1. Explanation of the points will be omitted and only the different points will be explained.

[0541] First, a tungsten film having a thickness of 100 nm is formed on a glass substrate as a conductive film to be the conductor 104. After that, a mask was formed and the conductor 104 was formed by etching.

[0542] Next, a silicon nitride film having a thickness of 400 nm was formed as the insulator 106a. The CP film was formed using the PECVD method, and the deposition gases were silane, nitrogen, and ammonia. Then, a silicon oxynitride film having a thickness of 50 nm was formed as the insulator 106b. The silicon oxynitride film was formed by the PECVD method under a pressure of 40 Pa and an RF power of 1. The power was 100 W, the substrate temperature was 350°C, and the gas flow rates of silane and nitrous oxide were 20 The flow rate was set to 3000sccm and 3000sccm.

[0543] Next, an oxide semiconductor film to be the oxide semiconductor 108a was formed. A 50-nm-thick In was deposited by sputtering using a polycrystalline metal oxide target. The sample A-1 was formed with an In:Ga:Zn=4:2:4.1 [original The target was a 1000 nm target with a 1000 nm atomic ratio of 1.0 to 1.5 nm, and oxygen and argon were used as gases. The ratio of oxygen to the sum of gas flow rates is 30%, AC power is 2.5kW, and pressure is 0. The pressure was 6 Pa and the substrate temperature was 170° C. Sample A-2 was In:Ga:Zn=1:1:1 A target with an atomic ratio of .2 was used, and oxygen and argon were used as gases. The ratio of oxygen to the sum of the gas flows of argon and argon is 50%, the AC power is 2.5 kW, and the pressure is The pressure was 0.6 Pa and the substrate temperature was 170°C.

[0544] Next, the substrate was heat-treated at 450°C for 1 hour in a nitrogen atmosphere, and then in an oxygen atmosphere. Heat treatment was carried out at 450°C for 1 hour.

[0545] Next, a tungsten carbide film having a thickness of 50 nm was formed as a conductive film to be the conductors 112a and 112b. Then, 400 nm of ZnO, 400 nm of aluminum, and 100 nm of titanium were deposited in that order. Then, the conductors 112a and 112b were formed by etching. The sample was treated with a 1:100 diluted solution of 5% phosphoric acid for 15 seconds.

[0546] Next, silicon oxynitride is formed to a thickness of 40 nm by the PECVD method as the insulator 114. The pressure was 200 Pa, the RF power was 100 W, and the substrate temperature was 220°C. The gas flow rates of the nitrogen oxide and nitrous oxide were set to 50 sccm and 2000 sccm, respectively. After that, a silicon oxynitride film having a thickness of 400 nm is formed as the insulator 116 by the PECVD method. The pressure was 200 Pa, the power was 1500 W, and the substrate temperature was 220°C. The gas flow rates of nitrous oxide were set to 160 sccm and 4000 sccm, respectively.

[0547] Next, a first heat treatment was performed at 350° C. for 1 hour in a nitrogen atmosphere. nm thick indium tin oxide film (hereinafter, ITSO film) is formed by sputtering. The film was formed from a target of In2O3:SnO2:SiO2 = 85:10:5 [wt %]. The deposition gases used were argon and oxygen.

[0548] Next, an oxygen addition process was performed on the insulator 116 through the ITSO film. The ashing equipment was used, the substrate temperature was set to 40° C., and oxygen gas was used at a flow rate of 250 sccm. was introduced into the chamber, the pressure was set to 15 Pa, and a bias was applied to the substrate side. RF power of 4500 W was applied between the parallel plate electrodes installed in the ashing device for 120 sec. I supplied it.

[0549] Next, the ITSO film was removed to expose the insulator 116. As the etching method, wet etching was used.

[0550] Next, a silicon nitride film having a thickness of 100 nm is formed as the insulator 118 by using the PECVD method. The deposition gases used were silane, nitrogen, and ammonia, and the substrate temperature was 350°C. did.

[0551] Next, an opening 142c reaching the conductor 112b and an opening 142b reaching the conductor 104 are formed. The openings 142a, 142b, and 142c were formed by dry etching. The film was formed using a mixing apparatus.

[0552] Next, a conductive film is formed on the insulator 118 so as to cover the openings 142a, 142b, and 142c. The conductive film was processed to form the conductors 120a and 120b. In the transistor structure shown in FIG. 1, the conductor 120b is not provided. 120b is a 100 nm thick ITSO film formed using a sputtering device. The composition of the target used for the ITSO film was the same as that of the ITSO film shown above. It was decided.

[0553] Next, a second heat treatment was performed at 250° C. in a nitrogen gas atmosphere. It was set to one hour.

[0554] Through the above steps, samples A-1 and A-2 having transistors were manufactured.

[0555] <Transistor evaluation> Next, the transistors of the fabricated samples A-1 and A-2 were subjected to a temperature The temperature was 60°C, Vgs=30V, and stress was applied for 1 hour. A transistor with a panel width W of 50 μm was evaluated. Figure 38 shows the results before and after 100 seconds of stress. Ids- after 500 seconds, 1500 seconds, 2000 seconds, and 1 hour (3600 seconds) The Ids-Vgs characteristics are measured under two conditions: Vds is 0.1V and 10V. Here, Vgs was applied to the conductor 104 of the transistor s. For the transistor d, the conductor 104 and the conductor 120b are set to the same potential, and the conductor 104 And Vgs was applied to conductor 120b.

[0556] FIG. 38A shows the Ids-Vds characteristics of a transistor d included in the sample A-1. FIG. 38B shows the Ids-Vds characteristics of the transistor s of the sample A-2. The change in threshold voltage (ΔVth) after one hour was 0 .17V for transistor d, and 0.18V for transistor d. The voltages were 0.79 V for transistor s and 1.26 V for transistor d. The reason for this is that the sample A-1 had better properties than the sample A-2. The oxide semiconductor 108a used in Sample A-1 has a lower conduction band minimum. It is speculated that the energy gap of a is smaller, etc. EXAMPLES

[0557] In this example, a transistor having the structure shown in FIG. 15C is manufactured, and its characteristics are evaluated. It was worth it.

[0558] <Making a transistor> Two samples, sample B-1 and B-2, were fabricated. Fabrication of the transistors in each sample The method for preparing sample B-2 is the same as that for preparing sample B-1. Explanation of the points will be omitted and only the different points will be explained.

[0559] First, a tungsten film having a thickness of 100 nm is formed on a glass substrate as a conductive film to be the conductor 104. After that, a mask was formed and the conductor 104 was formed by etching.

[0560] Next, a silicon nitride film having a thickness of 400 nm was formed as the insulator 106a. The CP film was formed using the PECVD method, and the deposition gases were silane, nitrogen, and ammonia. Then, a silicon oxynitride film having a thickness of 50 nm was formed as the insulator 106b. The silicon oxynitride film was formed by the PECVD method under a pressure of 40 Pa and an RF power of 1. The power was 100 W, the substrate temperature was 350°C, and the gas flow rates of silane and nitrous oxide were 20 The flow rate was set to 3000sccm and 3000sccm.

[0561] Next, an oxide semiconductor film to be the oxide semiconductor 108a was formed. A 25-nm-thick In was deposited by sputtering using a polycrystalline metal oxide target. The sample B-1 was made of In:Ga:Zn=4:2:4.1 [original The target was a 1000 nm target with a 1000 nm atomic ratio of 1.0 to 1.5 nm, and oxygen and argon were used as gases. The ratio of oxygen to the sum of gas flow rates is 30%, AC power is 2.5kW, and pressure is 0. The pressure was 6 Pa and the substrate temperature was 170° C. Sample B-2 was In:Ga:Zn=1:1:1 A target with an atomic ratio of 0.2 was used, and oxygen and argon were used as gases. The ratio of oxygen to the sum of the gas flows of argon and argon is 50%, the AC power is 2.5 kW, and the pressure is The pressure was 0.6 Pa and the substrate temperature was 170°C.

[0562] Next, the substrate was heat-treated at 450°C for 1 hour in a nitrogen atmosphere, and then in an oxygen atmosphere. Heat treatment was carried out at 450°C for 1 hour.

[0563] Next, a tungsten carbide film having a thickness of 50 nm was formed as a conductive film to be the conductors 112a and 112b. Then, 400 nm of ZnO, 400 nm of aluminum, and 100 nm of titanium were deposited in that order. Then, the conductors 112a and 112b were formed by etching. The sample was treated with a 1:100 diluted solution of 5% phosphoric acid for 15 seconds.

[0564] Next, a silicon oxynitride film was formed as the insulator 114 by the PECVD method. The conditions were 0 Pa, RF power 100 W, and substrate temperature 220°C. Silane and dinitrogen monoxide were The gas flow rates were set to 50 sccm and 2000 sccm, respectively. A silicon oxynitride film was formed by the PECVD method using a pressure of 200 Pa and a power of 150 The power was 100 W, the substrate temperature was 220°C, and the gas flow rates of silane and nitrous oxide were 160 The flow rate was set to 4000sccm and 4000sccm.

[0565] Next, a first heat treatment was performed at 350° C. for 1 hour in a nitrogen atmosphere. The ITSO film was deposited by sputtering. The deposition gas was argon and oxygen. Used.

[0566] Next, an oxygen addition process was performed on the insulator 116 through the ITSO film. The ashing equipment was used, the substrate temperature was set to 40° C., and oxygen gas was used at a flow rate of 250 sccm. was introduced into the chamber, the pressure was set to 15 Pa, and a bias was applied to the substrate side. RF power of 4500 W was applied between the parallel plate electrodes installed in the ashing device for 120 sec. I supplied it.

[0567] Next, the ITSO film was removed to expose the insulator 116. As the etching method, wet etching was used.

[0568] Next, a silicon nitride film having a thickness of 100 nm is formed as the insulator 118 by using the PECVD method. The deposition gases used were silane, nitrogen, and ammonia, and the substrate temperature was 350°C. did.

[0569] Next, an opening 142c reaching the conductor 112b and an opening 142b reaching the conductor 104 are formed. The openings 142a, 142b, and 142c were formed by dry etching. The film was formed using a mixing apparatus.

[0570] Next, a conductive film is formed on the insulator 118 so as to cover the openings 142a, 142b, and 142c. The conductive film was processed to form the conductors 120a and 120b. 120b is a 100 nm thick ITSO film formed using a sputtering device. The composition of the target used for the ITSO film was the same as that of the ITSO film shown above. It was decided.

[0571] Next, a second heat treatment was performed at 250° C. in a nitrogen gas atmosphere. It was set to one hour.

[0572] Through the above steps, samples B-1 and B-2 having transistors were manufactured.

[0573] <Transistor evaluation> Next, regarding the transistors d of the fabricated samples B-1 and B-2, The transistor d was subjected to stress of Vgs=30V for 1 hour. 04 and the conductor 120b are set to the same potential, and Vgs is applied to the conductor 104 and the conductor 120b. The measurement temperatures were 40°C, 60°C, 70°C, 80°C, 100°C and 110°C. (70°C and 110°C were only for sample B-1).

[0574] A transistor with a channel length L of 6 μm and a channel width W of 50 μm was evaluated. Before, 100 seconds later, 500 seconds later, 1500 seconds later, 2000 seconds later, and 1 hour later (3600 sec), the Ids-Vgs characteristics were measured at Vds of 0.1 V and 10 V. The threshold voltage was calculated from the characteristics at 40°C before the stress was applied. The threshold value was 0.8 V for sample B-1 and 1.0 V for sample B-2. The threshold value is Ids[A]×L[μm]÷W[μm]=1×10 -9 [A]Vg It was calculated as s.

[0575] In samples B-1 and B-2, the relationship between stress time and the change in threshold voltage (ΔVth) The relationship is shown in Figure 39 (A) and (B), respectively. The horizontal axis represents 1000 / T, and the vertical axis represents The time when ΔVth becomes 1 V is plotted in FIG. (B) shows the results for samples B-1 and B-2. Based on these results, the formula (1 ) to calculate the activation energy E a The activation energy E a In sample B-1, The activation energy was 0.53 eV for sample B-1 and 0.45 eV for sample B-2. It is considered that the capture of carriers into the defect level of the insulator 106a is suppressed. The lower end of the conduction band of the oxide semiconductor 108a is lower. It is assumed that the activation energy becomes larger when the gap is smaller, etc. . EXAMPLES

[0576] In this example, a transistor having the structure shown in FIG. 43 was fabricated and its characteristics were evaluated. .

[0577] <Making a transistor> Two samples, C-1 and C-2, were fabricated. The method for preparing sample C-2 is the same as that for preparing sample C-1. Explanation of the points will be omitted and only the different points will be explained.

[0578] First, a conductor 105 was formed on a glass substrate. In the sample C-1, the conductor 10 A tungsten film with a thickness of 100 nm was formed as the conductive film for 5. Then, a mask was formed. Then, the conductor 105 was formed by etching. As the conductive film, a titanium film with a thickness of 10 nm was formed, and then a copper film with a thickness of 100 nm was formed on the titanium film. Thereafter, a mask was formed and the conductor 105 was formed by etching.

[0579] Next, as the insulator 101, a silicon nitride film having a thickness of 400 nm and an oxide film having a thickness of 50 nm are A laminated film with a silicon nitride film was used. First, the silicon nitride film was formed using the PECVD method. The deposition gases used were silane, nitrogen, and ammonia. The silicon film was formed by the PECVD method under the conditions of pressure 40 Pa, RF power 100 W, and substrate temperature 0. The temperature was set to 350° C., and the gas flow rates of silane and nitrous oxide were 20 sccm and 20 sccm, respectively. The flow rate was set to 3000sccm.

[0580] Next, an oxide semiconductor film to be the layer 108_2 was formed. Using the metal oxide target, In-Ga-Zn oxide was formed by sputtering. Sample C-1 was deposited using a target with an atomic ratio of In:Ga:Zn=4:2:4.1. The oxygen and argon gases were used, and the oxygen and argon gas flow rates were compared. The ratio of elements was set to 10%, the AC power was set to 2.5 kW, the pressure was set to 0.6 Pa, and the substrate temperature was set to The temperature was set to 130° C., and an In-Ga-Zn oxide film with a thickness of 40 nm was formed. A target of Ga:Zn=1:1:1.2 [atomic ratio] was used, and oxygen and Argon is used, and the ratio of oxygen to the sum of oxygen and argon gas flow rates is set to 50%, and AC The power was 2.5 kW, the pressure was 0.6 Pa, the substrate temperature was 170° C., and the thickness was 40 nm. An In-Ga-Zn oxide film was formed.

[0581] Next, a three-layer silicon oxynitride film is formed as the insulator 106 by the PECVD method. The first layer was deposited at a pressure of 200 Pa, an RF power of 100 W, and a substrate temperature of 350°C. The gas flow rates of silane and nitrous oxide were set at 20 sccm and 3000 sccm, respectively. The second layer was formed with a pressure of 200 Pa and RF The power was 1500 W, the substrate temperature was 220° C., and the gas flow rates of silane and nitrous oxide were At 160sccm and 4000sccm, respectively, silicon oxynitride was deposited at 100nm. The third layer was formed using the same conditions as the first layer, and a silicon oxynitride film was deposited to a thickness of 20 nm.

[0582] Next, a heat treatment was performed in a nitrogen atmosphere at 350° C. for 1 hour.

[0583] Next, the conductor 104 was formed. First, In-Ga-Zn Then, an In-Ga-Zn oxide film was formed at 100 nm. Then, the In-Ga-Zn oxide and the insulator 106 were The mask was used to process the material into a land shape. Argon and nitrogen were used as gases, and the reduced pressure atmosphere was used. Then, a silicon nitride film was formed as the insulator 122. Next, a silicon oxynitride film is formed as the insulator 124, and In is Hydrogen was supplied to the -Ga-Zn oxide to form the conductor 104. The silicon film was fabricated using the PECVD method under the conditions of pressure 100 Pa, RF power 1000 W, and substrate temperature. The temperature was 220° C., and the gas flow rates of silane, nitrogen, and ammonia were 50 sccm and 50 The silicon oxynitride film was deposited at 100 nm with a flow rate of 00 sccm and 100 sccm. Using the PECVD method, the pressure was 200 Pa, the RF power was 1500 W, and the substrate temperature was 220°C. The gas flow rates of silane and nitrous oxide were 160 sccm and 4000 sccm, respectively. The thickness was 300 nm.

[0584] After that, for sample C-1, a 300 nm thick silicon oxynitride film was formed by PECVD. A SiO2 film was formed, and then heat treatment was performed at 350° C. for 1 hour in a nitrogen atmosphere.

[0585] Next, for the samples C-1 and C-2, the insulators 122 and 124 were subjected to an opening The opening 141a and the like are provided, and then the conductors 112a and 112b are formed. Then, a 1.5 μm acrylic resin film was formed, and then heat-treated at 250° C. for 1 hour in a nitrogen atmosphere. The theory was carried out.

[0586] By the above steps, the transistors having the structure shown in FIG. 43 were fabricated as Sample C-1 and Sample It was formed in C-2.

[0587] <Transistor evaluation> Next, the transistors of the fabricated samples C-1 and C-2 were subjected to a temperature The temperature was 60°C, Vgs=30V, and stress was applied for 1 hour. A transistor with a panel width W of 50 μm was evaluated. Figure 45 shows the results before and after 100 seconds of stress. Ids- after 500 seconds, 1500 seconds, 2000 seconds, and 1 hour (3600 seconds) The Vgs characteristics are shown in Fig. 45(A) for the transistor of sample C-1 and in Fig. 45(B) for the transistor of sample C-2. The results of the test are shown below. The Ids-Vgs characteristics for sample C-1 are as follows: Vds is 0. The two conditions were 1 V and 10 V, and for sample C-2, Vds was 0.1 V and 5 V. Here, the conductor 104 and the conductor 105 are set to the same potential, and the conductors 104 and Vgs was applied to the conductor 105. The change in threshold voltage (ΔVth) after one hour was 0.79V for the transistor of sample C-1, and 4.23V for the transistor of sample C-2 It was V.

[0588] FIG. 46 shows a plot of stress application time on the horizontal axis and ΔVth on the vertical axis. Here, the results obtained in FIG. 46 are approximated by the formula (2) shown in the first embodiment, and α and β In sample C-1, α was 0.04, β was 0.35, and in sample C-2, α was 0.61 and beta was 0.26.

[0589] The results showed that α was small in sample C-1. The reason for this is that sample C-2 and In comparison, the bottom edge of the conduction band of the layer 108_2 used in the sample C-1 is lower. It is speculated that the energy gap is smaller. EXAMPLES

[0590] Example 1 In this example, evaluation results of temperature dependence of hole mobility in an oxide semiconductor are described.

[0591] <Sample preparation> A sample for evaluation was prepared. First, a silicon nitride film was formed to a thickness of 100 nm on a glass substrate. Silicon oxynitride was deposited on the substrate at 150 nm. Silicon oxynitride was formed by mixing silane gas and suboxide. The film was formed by the PECVD method using nitrogen gas.

[0592] Next, a tungsten film is formed and patterned to function as the first gate electrode. The hole mobility was measured after the formation of the conductor 104. Then, silicon oxynitride was deposited by PECVD as the insulator 106b. The silicon oxynitride film was deposited at 200 nm using the following conditions: silane and nitrous oxide. The gas flow rates were set to 20sccm and 3000sccm, respectively, and the substrate temperature was set to 350°C. The power was 100 W and the pressure was 40 Pa.

[0593] Next, the oxide semiconductor 108a was formed. The oxide semiconductor 108a was formed by sputtering. A 100 nm In-Ga-Zn oxide film was formed using the ring method. The In-Ga-Zn oxide was used with a numerical ratio of In:Ga:Zn=1:1:1. The deposition conditions were The gas used was argon and oxygen, with the ratio of oxygen to the total gas being 10%. The pressure was controlled to 0.7 Pa, the substrate temperature was 100°C, and a DC power supply was applied with an output of 5 kW. .

[0594] Next, heat treatment was performed in a nitrogen atmosphere at 350°C for 1 hour, followed by heating in oxygen gas at 350°C. Heat treatment was carried out at ℃ for 1 hour.

[0595] Next, 50 nm of tungsten, 400 nm of aluminum, and 100 nm of titanium are applied. Then, electrodes such as a conductor 112a and a conductor 112b were formed by patterning.

[0596] Next, heat treatment was performed in an oxygen atmosphere at 300°C for 1 hour. A silicon oxide film was formed to a thickness of 400 nm by a deposition method.

[0597] Next, the sample was heat-treated in an oxygen atmosphere at 350°C for 1 hour. Heat treatment was carried out at 250° C. for 1 hour.

[0598] By the above steps, a sample for measuring the Hall effect was prepared.

[0599] <Sample evaluation> The Hall effect of the prepared sample was measured to evaluate the Hall mobility. Hall effect measurements were performed using the ResiTest8300 series manufactured by Toyo Corporation. went.

[0600] The temperature dependence of the electron Hall mobility obtained by Hall effect measurement is shown in Figure 50. The vertical axis shows the measurement temperature, and the vertical axis shows the Hall mobility. The Hall mobility tends to increase with temperature. However, in In-Ga-Zn oxide, the effect of phonon scattering on the electron transport is not dominant. This suggests that EXAMPLES

[0601] The composition, impurity concentration, and crystallinity of an oxide semiconductor are changed by irradiating the oxide semiconductor with a laser. Below is an example of this:

[0602] The sample evaluated was a metal oxide film on a quartz substrate with a composition of In:Ga:Zn=1:1: Sample A was deposited to a thickness of 35 nm using a target of In-Ga-Zn oxide with an atomic ratio of 1. Then, the sample was irradiated with laser light.

[0603] The sample A was prepared by sputtering a Zn-In alloy with an atomic ratio of In:Ga:Zn=1:1. The sputtering gas was 30 sccm of argon and 15 s ccm of oxygen was supplied to the processing chamber of the sputtering device, and the pressure in the processing chamber was set to 0.4 Pa. The In-Ga-Zn oxide film was deposited by controlling the supply of 0.5 kW of DC power. The substrate temperature during deposition was room temperature (25° C.).

[0604] For laser processing, a XeCl excimer laser (Lambda STEEL2000 ) was used, the laser wavelength was λ = 308 nm, and the pulse width was 25 nsec (full width at half maximum). The linearly shaped laser beam was then irradiated at room temperature (25°C) with N2 spraying. The substrate was scanned in the direction perpendicular to the long axis of the laser beam. The width of the linear beam was approximately 320 μm. The laser beam was irradiated to the same location at 1 mm / sec with 30 Hz oscillation. The number of shots was about 10. The laser energy density was 200 mJ / s without irradiation. cm 2 , 290mJ / cm 2 , 392 mJ / cm 2 , and 445 mJ / cm 2 It was decided.

[0605] The crystallinity of the samples was evaluated by the out-of-plane method using XRD.

[0606] Figure 50 shows the laser energy density of the XRD pattern by the out-of-plane method. Indicates dependency.

[0607] As shown in Figure 51, sample A has a laser energy density of 290 mJ / cm 2 The above 2θ is 31° A peak near the 445 mJ / cm 2 So, 39 2mJ / cm 2 The peak near 31° tends to be weaker than that near 36°. The sting has almost disappeared.

[0608] X-ray Photoelectron Spectroscopy (XPS) The specimens were measured by ion spectroscopy. The composition ratios of gallium, zinc, oxygen, and silicon were determined.

[0609] The results of the XPS analysis are shown in Figs. 52 to 54. In Figs. 52 to 54, the horizontal axis indicates the spat The vertical axis represents time (min) and the vertical axis represents composition ratio (atomic %). Indium in (A), gallium in (B), zinc in (A), oxygen in (B), and silicon in (B). The results of each are shown below.

[0610] 445mJ / cm 2 For example, the film surface tends to change more slowly. The substrate may be rougher than the metal oxide. It is also possible that this is occurring.

[0611] Next, sample A was analyzed in the depth direction by SIMS.

[0612] Figure 55 shows the results for no irradiation, 290 mJ / cm 2 , 392 mJ / cm 2 , and 445mJ / cm 2 The depth profile of silicon concentration was evaluated by SIMS under each condition. vinegar.

[0613] The silicon concentration is 392 mJ / cm 2 So 1×10 20 atoms / cm 3 That's it, 44 5mJ / cm 2 So 1×10 21 atoms / cm 3 The results were as follows: No irradiation and 2 90mJ / cm 2 In the region, the silicon concentration is approximately 1×10 19 a toms / cm 3 It was found that this could be reduced to the following:

[0614] The samples were characterized by TEM observation and electron diffraction.

[0615] Figure 56 shows the results of cross-sectional TEM. The H-90 manufactured by Hitachi High-Technologies was used for the observation. 00NAR was used. Figure 56 (A), (B), (C) and (D) show the results of laser irradiation, respectively. No radiation, laser energy density is 290mJ / cm 2 , 392 mJ / cm 2 , and 44 5mJ / cm 2 As the laser energy density increases, lattice fringes become visible. This suggests that the laser irradiation caused crystallization. However, at 445 mJ / cm 2 In , 392 mJ / cm as suggested by the XRD results. 2 The lattice pattern is weaker compared to A trend is observed.

[0616] Next, the results of planar TEM are shown in Figure 57. Figure 57(A), (B), (C) and (D) are without laser irradiation and with a laser energy density of 290 mJ / cm 2 , 392mJ / cm 2 , and 445 mJ / cm 2 As the laser energy density increases, Crystal grains are clearly observed, suggesting crystallization due to laser irradiation. 45mJ / cm 2 In the case of As per the chart, 392 mJ / cm 2 In comparison with the above, the crystal grains are not clearly observed.

[0617] In Figure 58, the laser energy density is 392 mJ / cm 2 In the case of The results of electron beam diffraction on the surface are shown. The electron beam diameter was set to about 1 nmφ. In terms of thickness, there was a correspondence with JCPDS card No. 38-1114. In the region (2) near the center, several bright spots arranged in a ring shape were observed, and nc (nano It is suggested that the crystal structure is (crystal). [Explanation of symbols]

[0618] 10 Semiconductor device 100 Transistors 100A Transistor 101 Insulators 102 Substrate 104 Conductors 104_0 Conductor 104a Conductor 104b Conductor 105 Conductors 106 Insulators 106a Insulator 106b Insulators 107_3 Oxide semiconductors 108 Oxide Semiconductor 108_1 layer 108_2 layers 108_3 layers 108a Oxide Semiconductor 108b Oxide semiconductor 108d Drain region 108h Oxide Semiconductor 108i Channel Area 108j Oxide semiconductor 108k Oxide Semiconductor 108s Source Area 110 Insulator 112 Conductors 112a Conductor 112b Conductor 114 Insulators 116 Insulators 117 Oxide Semiconductor Film 118 Insulators 120a Conductor 120b Conductor 122 Insulator 124 Insulators 126 Conductors 141a opening 141b opening 142a opening 142b opening 142c opening 143 Opening 170 Transistors 400 Substrates 402 Insulator 402b Insulator 407 Channel formation region 408 Insulator 454 Conductors 460 Element isolation area 462 Insulator 464 Insulator 464a Insulators 464b Insulators 470 Insulator 474 area 476 area 490 Transistors 493 Transistor 494 Transistors 501 Pixel circuit 502 Pixel section 504 Drive circuit section 504a Gate Driver 504b source driver 506 Protection circuit 507 Terminal section 511 Conductors 513 Conductors 514 Conductors 516 Conductors 516b Conductor 517 Conductors 518 Conductor 519 Conductors 541 Plug 544 Plug 544b Plug 545 Plug 547 Plug 547b Plug 548 Plug 550 Transistor 552 Transistor 554 Transistor 560 Capacitive element 562 Capacitive element 568 Light-emitting element 570 Liquid crystal element 571 Insulators 571a Insulator 572 Insulators 581 Insulators 581a Insulator 581b Insulator 584 Insulators 585 Insulator 591 Insulators 591b Insulator 592 Insulators 593 Insulators 594 Insulators 599 Insulators 627 layers 628 layers 629 layers 630 layers 631 layers 700 Display device 701 Substrate 702 Pixel section 704 Source driver circuit section 705 Substrate 706 Gate driver circuit section 708 FPC terminal section 710 Signal Line 711 Wiring section 712 Sealing material 716 FPC 730 Insulating film 732 Sealing film 734 Insulating film 736 Colored film 738 Light-shielding film 750 Transistors 752 Transistor 760 Connection electrode 764 Insulating film 766 Insulating Film 767 Oxide Semiconductor Film 768 Insulating Film 770 Planarizing Insulating Film 772 Conductive Film 774 Conductive Film 775 Liquid crystal elements 776 Liquid crystal layer 778 Structure 780 Anisotropic Conductive Film 782 Light emitting element 784 Conductive Film 786 EL layer 788 Conductive Film 790 Capacitive element 8000 Display Module 8001 Top cover 8002 Lower cover 8003 FPC 8004 Touch Panel 8005 FPC 8006 Display Panel 8007 Backlight 8008 light source 8009 Frame 8010 Printed Circuit Board 8011 Battery 9000 Chassis 9001 Display section 9003 Speaker 9005 Operation key 9006 Connection terminal 9007 Sensor 9008 Microphone 9050 Operation button 9051 Information 9052 Information 9053 Information 9054 Information 9055 Hinge 9100 Mobile Information Terminal 9101 Portable information terminal 9102 Portable information terminal 9200 Mobile Information Terminal 9201 Mobile information terminals

Claims

[Claim 1] a first conductor on the substrate; a first insulator on the first conductor; and a first oxide semiconductor on the first insulator; a second oxide semiconductor on the first oxide semiconductor; a second conductor and a third conductor electrically connected to the second oxide semiconductor; a second insulator on the second conductor and on the third conductor; a fourth conductor and a fifth conductor on the second insulator, the first conductor functions as a first gate electrode; the second conductor functions as one of a source electrode or a drain electrode; the third conductor functions as the other of the source electrode and the drain electrode; the fourth conductor functions as a second gate electrode; the fifth conductor functions as a pixel electrode; the fifth conductor is electrically connected to the third conductor through a first opening provided in the second insulator; In a cross-sectional view of the transistor in a channel width direction, the second insulator has a region in contact with a top surface of the second oxide semiconductor, a region in contact with a side surface of the second oxide semiconductor, and a region in contact with a side surface of the first oxide semiconductor; the fourth conductor is electrically connected to the first conductor through a second opening and a third opening provided in the first insulator and the second insulator, the first oxide semiconductor has a carrier density of 1×10 9 cm −3 or more and 5×10 16 cm −3 or less; The energy gap of the first oxide semiconductor is 2.7 eV or more and 3.1 eV or less; a hydrogen concentration in the first oxide semiconductor is 2×10 20 atoms / cm 3 or less; the first oxide semiconductor has an alkali metal or alkaline earth metal concentration of 1×10 18 atoms / cm 3 or less; the first oxide semiconductor has a nitrogen concentration of 5×10 18 atoms / cm 3 or less; The energy gap of the second oxide semiconductor is larger than the energy gap of the first oxide semiconductor by 0.15 eV to 2 eV, The second oxide semiconductor has a carrier density of less than 1×10 9 cm −3 .

Citation Information

Patent Citations

  • Semiconductor device and method for manufacturing the same

    JP2011135063A

  • Semiconductor integrated circuit

    JP2012257187A

  • Display device

    JP2015015459A

  • Semiconductor device, method of manufacturing semiconductor device, and display device

    JP2015128152A

  • Semiconductor device

    JP2015195327A