Wireless communication device and method for manufacturing same

The wireless communication device addresses high manufacturing costs and environmental sensitivity issues by using a two-layer antenna structure with matching materials for electrodes and antennas, ensuring cost-effectiveness and durability.

JP7559563B2Active Publication Date: 2024-10-02TORAY INDUSTRIES INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021004710
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-01-28
Filing Date
2021-01-15
Publication Date
2024-10-02
Estimated Expiration
2041-01-15

AI Technical Summary

Technical Problem

Existing methods for manufacturing RFID tags, such as etching metal foils and using photosensitive conductive pastes, result in high costs and are sensitive to environmental changes, leading to peeling and characteristic deterioration due to material expansion and contraction.

Method used

A wireless communication device with a two-layer antenna structure where the materials for the upper and lower antennas are the same as the materials for the upper and lower electrodes, respectively, allowing for easy impedance matching and reducing manufacturing costs while minimizing peeling and characteristic deterioration due to environmental changes.

Benefits of technology

The solution enables low-cost manufacturing with improved antenna size, flexibility, and reduced peeling, while maintaining consistent performance across varying environmental conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559563000002
    Figure 0007559563000002
  • Figure 0007559563000003
    Figure 0007559563000003
  • Figure 0007559563000004
    Figure 0007559563000004
Patent Text Reader

Abstract

To provide a wireless communication device that is low in manufacturing cost, allows antenna size to be miniaturized, and has suppressed peeling and characteristic deterioration due to environmental changes.SOLUTION: A wireless communication device includes: a circuit unit 102 on a substrate; and a plurality of antennas 101 connected to the circuit unit. The circuit unit includes elements (FET 104) each having an upper electrode (source electrode 5 or drain electrode 6) and a lower electrode (gate electrode 2). The antennas include an upper layer antenna 12 and a lower layer antenna 11. A material that makes up the upper layer antenna is the same as a material that makes up the upper electrode, and a material that makes up the lower layer antenna is the same as a material that makes up the lower electrode.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wireless communication device and a method for manufacturing the same. [Background technology]

[0002] In recent years, the development of technology for constructing field effect transistors (hereinafter referred to as FETs) using semiconductor layers formed on insulating substrates has been progressing. FETs are widely used in electronic devices such as ICs and switching elements for image display devices. In particular, wireless communication systems using RFID (Radio Frequency IDentification) technology as contactless tags having circuits composed of FETs have been attracting attention in recent years.

[0003] An RFID tag has an IC chip with a circuit made of semiconductor elements, and an antenna for wireless communication with a reader / writer. The antenna installed inside the tag receives the carrier wave transmitted from the reader / writer, and the driver circuit inside the IC chip operates.

[0004] RFID tags are expected to be used for a variety of purposes, including logistics management, product management, and shoplifting prevention, and are already being introduced in some areas, such as in IC cards for transportation cards and product tags.

[0005] RFID tags are expected to be used in a wide variety of products, and so there is a demand for lower costs. To this end, there are plans to move away from manufacturing processes that use vacuum and high temperatures and instead manufacture them on flexible substrates using coating and printing technology to reduce costs.

[0006] Methods for forming antennas for RFID include etching a metal foil attached to a substrate such as a plastic film using a resist layer formed on the metal foil as a mask (see, for example, Patent Document 1). Another method involves applying a photosensitive conductive paste to a substrate such as a plastic film, and then photolithographically processing the pattern corresponding to the antenna and the pattern corresponding to the electrodes of the circuit section (see, for example, Patent Document 2). [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2012-8857 A [Patent Document 2] International Publication No. 2017 / 030070 Summary of the Invention [Problem to be solved by the invention]

[0008] The method of etching metal foil described in Patent Document 1 allows for the formation of patterns of about several hundred microns, but has the problem of high manufacturing costs. The method of photolithographically processing an antenna pattern and a partial electrode pattern of a circuit section using a photosensitive conductive paste described in Patent Document 2 has the problem that, compared to a method of mounting an IC on an antenna pattern, the distortion caused by material expansion and contraction due to environmental changes such as temperature and humidity is likely to differ between the antenna section and the circuit section, which makes it more likely for material peeling and deterioration of the characteristics of the wireless communication device to occur.

[0009] The present invention has been made in view of the above-mentioned problems, and has an object to provide a wireless communication device that can be manufactured at low cost, has a small antenna size, and is suppressed from peeling off or from deteriorating in characteristics due to environmental changes. [Means for solving the problem]

[0010] In order to solve the above problems, a wireless communication device according to the present invention comprises: On the board, A circuit unit; an antenna connected to the circuit unit; Equipped with the circuit section includes an element having an upper electrode and a lower electrode, The antenna has an upper layer antenna and a lower layer antenna, the material constituting the upper layer antenna is the same as the material constituting the upper electrode; The material constituting the lower layer antenna is the same as the material constituting the lower electrode. It is a wireless communication device. Effect of the Invention

[0011] According to the present invention, it is possible to provide an antenna which can be manufactured at low cost, which allows easy adjustment of impedance matching between the antenna and a circuit section, and which allows the formation of complex shapes and fine patterns. [Brief description of the drawings]

[0012] [Figure 1] 1 is a schematic diagram illustrating an example of a configuration of a wireless communication device according to an embodiment of the present invention. [Diagram 2] 2 is a schematic cross-sectional view of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. FIG. [Diagram 3] 2 is a schematic cross-sectional view of an antenna unit of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. [Figure 4] 2 is a schematic cross-sectional view of an antenna unit of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. [Diagram 5] 2 is a schematic cross-sectional view of an antenna unit of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. [Figure 6]2 is a schematic cross-sectional view of an antenna unit of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. [Figure 7] 2 is a schematic cross-sectional view of an antenna unit of the wireless communication device according to the first embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. [Figure 8] 2 is a schematic cross-sectional view of a wireless communication device according to a second embodiment of the present invention taken along line II' within an area surrounded by a dashed line in the wireless communication device shown in FIG. 1. FIG. [Figure 9] 3A to 3C are partial enlarged schematic views showing an example of a method for manufacturing the wireless communication device according to the first embodiment of the present invention. [Figure 10] 3A to 3C are partial enlarged schematic views showing an example of a method for manufacturing the wireless communication device according to the first embodiment of the present invention. [Figure 11] 1 is a schematic plan view illustrating a configuration of a ring oscillator included in a wireless communication device according to a first embodiment of the present invention. [Figure 12] FIG. 1 is a schematic perspective view showing a state in which bending resistance of a wireless communication device is evaluated. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, embodiments of a wireless communication device and a manufacturing method thereof according to the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to these embodiments, and various modifications are possible within the scope of the invention as long as the object of the invention can be achieved and the gist of the invention is not deviated from.

[0014] <Wireless communication device> A wireless communication device according to an embodiment of the present invention is a wireless communication device comprising a circuit unit and an antenna connected to the circuit unit on a substrate, the circuit unit having an element having an upper electrode and a lower electrode, the antenna having an upper layer antenna and a lower layer antenna, the material constituting the upper layer antenna being the same as the material constituting the upper electrode, and the material constituting the lower layer antenna being the same as the material constituting the lower electrode.

[0015] This wireless communication device is a device that operates using wireless radio waves received by an antenna. Examples of wireless communication devices include, but are not limited to, (1) a power supply device that supplies energy contactlessly without using a wired connection with an adapter, (2) a device that performs electrical communication by partially modulating a carrier wave used for sensing, and (3) a device that exchanges information by receiving a carrier wave transmitted from an antenna mounted on a reader / writer. A more specific example of (3) is an RFID (Radio Frequency IDentification) tag, which is a contactless tag such as a product tag, an anti-shoplifting tag, various tickets, and smart cards.

[0016] The specific operation of a wireless communication device will be described using an RFID tag as an example. For example, when an antenna in an RFID tag receives a wireless signal transmitted from an antenna mounted on a reader / writer, the wireless signal is converted to a direct current by a rectifier circuit in the circuit section of the RFID tag, causing the RFID tag to become electrically charged. Next, the electrically charged RFID tag receives a command from the wireless signal and performs an operation according to the command. After that, a response to the command is transmitted as a wireless signal from the antenna in the RFID tag to the antenna of the reader / writer. The operation according to the command is executed by a demodulation circuit, a control circuit, a modulation circuit, etc.

[0017] In a wireless communication device according to an embodiment of the present invention, an element having an upper electrode and a lower electrode that is included in a circuit section is an element that constitutes an element required for a circuit configuration according to the above-mentioned application, such as a capacitor, a field effect transistor, or a rectifying element that constitutes the circuit section.

[0018] In the following embodiments, the present invention will be described in detail using examples in which the elements are field effect transistors (FETs), but the present invention is not limited to these embodiments.

[0019] (Embodiment 1) 1 and 2 are schematic diagrams showing the configuration of a wireless communication device according to a first embodiment of the present invention. As shown in Fig. 1, the wireless communication device according to the first embodiment of the present invention includes, on a substrate 1, an antenna 101, a circuit section 102, and a connection wiring 103 between the circuit section and the antenna.

[0020] Fig. 2 is a cross-sectional view taken along line I-I' within the area enclosed by the dashed line in Fig. 1, and shows an example of the configuration of an antenna constituting the wireless communication device shown in Fig. 1 and a FET included in the circuit unit. For the sake of simplicity, Fig. 2 shows only two FETs 104 included in the circuit unit, but the circuit unit 102 in this embodiment includes as many FETs of similar configuration as are required to configure the above-mentioned demodulation circuit, operation control logic circuit, modulation circuit, etc. The circuit unit 102 also includes connection wiring that connects these circuits.

[0021] In the wireless communication device according to the first embodiment, an antenna 101 and a FET 104 are formed on a substrate 1. In FIG. 2, there are two FETs 104, and on the substrate 1, the FETs 104 have a source electrode 5 and a drain electrode 6 corresponding to an upper electrode, a gate insulating layer 3, and a gate electrode 2 corresponding to a lower electrode. The gate electrode 2 is electrically insulated from the source electrode 5 and the drain electrode 6 by the gate insulating layer 3. The FET 104 further has a semiconductor layer 4 between the source electrode 5 and the drain electrode 6. In the first embodiment, the gate insulating layer 3 is shared between the two FETs 104, but may be provided independently in each FET 104.

[0022] The structure of the FET 104 illustrated in FIG. 2 is a so-called bottom gate structure in which a gate electrode is disposed below (on the substrate side of) a semiconductor layer, and a source electrode and a drain electrode are disposed on the same plane as the semiconductor layer.

[0023] Antenna 101 has a two-layer structure, and is composed of upper layer antenna 12 and lower layer antenna 11. The two-layer structure of the antenna expands the variety of methods for adjusting the impedance matching between the antenna and the circuit section. Specifically, the above adjustment can be achieved not only by the area and thickness of the antenna, but also by the combination of materials for the upper layer antenna and the lower layer antenna. This is effective in reducing the size and thickness of the antenna.

[0024] Moreover, the material constituting the upper layer antenna 12 is the same as the material constituting the source electrode 5 and the drain electrode 6, and the material constituting the lower layer antenna 11 is the same as the material constituting the gate electrode 2. This makes it possible to reduce the manufacturing cost of the wireless communication device.

[0025] Furthermore, by using the same material for the antenna and the electrode layer of the FET in the circuit unit, material expansion and contraction caused by environmental changes such as temperature and humidity can be made uniform between the antenna and the circuit unit (in this embodiment 1, the upper layer antenna, source electrode 5, and drain electrode 6, as well as the lower layer antenna 11 and gate electrode 2), thereby preventing the antenna and electrode layer from peeling off and the characteristics of the wireless communication device from deteriorating due to environmental changes.

[0026] The material constituting the antenna and the material constituting the electrode are the same means that the element contained in the antenna with the highest molar ratio is the same as the element contained in the electrode with the highest molar ratio. The types and content ratios of the elements contained in the antenna and the electrode can be identified by elemental analysis using X-ray photoelectron spectroscopy (XPS).

[0027] In Fig. 2, the upper layer antenna 12 and the lower layer antenna 11 are overlapped with the same shape without any misalignment, but the antenna 101 of the wireless communication device according to the first embodiment is not limited to this. Figs. 3 to 7 show variations in the way the upper layer antenna 12 and the lower layer antenna 11 overlap with each other using cross-sectional views similar to Fig. 2. Note that in these figures, the circuit unit 102 is omitted for simplification.

[0028] As shown in Fig. 3, the upper layer antenna 12 and the lower layer antenna 11 may overlap with a misalignment. Also, as shown in Fig. 4, there may be a partial area where the upper layer antenna 12 and the lower layer antenna 11 do not overlap. Also, as shown in Fig. 5 and Fig. 6, the lower layer antenna 11 and the upper layer antenna 12 may be different in size and overlap. Furthermore, as shown in Fig. 7, part of the upper layer antenna 12 may overlap so as to cover part or all of the lower layer antenna 11.

[0029] The overlapping manner of the upper layer antenna 12 and the lower layer antenna 11 of the antenna 101 of the wireless communication device of this embodiment 1 is not limited to the above, and various overlapping manners can be adopted as long as the object of the invention can be achieved and the gist of the invention is not deviated from.

[0030] There are no particular limitations on the material used for the substrate 1, as long as at least the surface on which the electrodes are disposed is insulating. For example, inorganic materials such as glass, sapphire, alumina sintered body, silicon wafer, and the like, and those whose surfaces are coated with an oxide film; Resins such as polyimide (PI) resins, polyester resins, polyamide resins, epoxy resins, polyamideimide resins, polyetherimide resins, polyetherketone resins, polysulfone resins, polyphenylene sulfide (PPS) resins, and cycloolefin resins; Substrates containing the following are preferably used, but are not limited to these.

[0031] Among these, it is preferable that the film contains at least one resin selected from polyethylene terephthalate (PET), polyethylene naphthalate, PPS, polyphenylene sulfone, cycloolefin polymer, polyamide, or PI, and a PET film is preferable from the viewpoint of low cost.

[0032] From the viewpoint of adhesion between the substrate and the lower electrode or wiring, polysulfone resin substrates and PPS resin substrates are also preferred, presumably because metal atoms in the lower electrode or wiring strongly interact with sulfur atoms contained in these resins.

[0033] The thickness of the substrate is preferably 25 μm or more and 100 μm or less, in order to provide durability and appropriate flexibility.

[0034] In the present invention, a primer layer may be formed on the substrate, which can improve the flatness of the substrate and the adhesion of the lower electrode.

[0035] The material used for the primer layer is not particularly limited, but specifically, acrylic resin, epoxy resin, novolac resin, phenolic resin, polyimide precursor resin, polyimide resin, polysiloxane resin, fluorine-based resin, polyvinyl acetal resin, etc. can be used.

[0036] The primer layer may be a single layer or multiple layers. In addition, one layer may be formed from multiple resin materials, or multiple resin materials may be laminated.

[0037] There is no particular restriction on the material used for antenna 101, and any material containing a usable conductive component may be used. By constructing upper layer antenna 12 and lower layer antenna 11 from different materials, impedance matching between the antenna and the circuit section can be adjusted without changing the area or thickness of the antenna, which has a significant effect on miniaturizing the antenna size and thinning it.

[0038] Examples of the conductive component include conductive metal oxides such as tin oxide, indium oxide, and indium tin oxide (ITO). Other examples include metals such as platinum, gold, silver, copper, iron, tin, zinc, aluminum, indium, chromium, lithium, sodium, potassium, cesium, calcium, magnesium, palladium, molybdenum, amorphous silicon, and polysilicon, alloys of a plurality of metals selected from these, and inorganic conductive substances such as copper iodide and copper sulfide. Other examples include polythiophene, polypyrrole, polyaniline, a complex of polyethylenedioxythiophene and polystyrenesulfonic acid, and conductive polymers whose conductivity is improved by doping with iodine or the like. Other examples include carbon materials and materials containing an organic component and a conductive component. These conductive components may be used alone, or a plurality of materials may be stacked or mixed for use.

[0039] At least one of the upper layer antenna 12 and the lower layer antenna 11 preferably contains a conductive component and an organic component. This increases the flexibility of the antenna, and improves adhesion to the substrate even when bent, resulting in good electrical connection. The organic component is not particularly limited, but may include monomers, oligomers or polymers, photopolymerization initiators, plasticizers, leveling agents, surfactants, silane coupling agents, defoamers, pigments, etc. From the viewpoint of improving the bending resistance of the electrode, oligomers or polymers are preferred.

[0040] It is more preferable that one of the upper layer antenna 12 and the lower layer antenna 11 contains a conductive component and an organic component, and the other antenna contains a metal component, which makes it easier to obtain an antenna with excellent conductivity and stability.

[0041] The conductive component used in the present invention is preferably silver. By using silver as the conductive component, a conductive film and a conductive pattern having excellent conductivity and stability can be easily obtained.

[0042] The organic component used in the present invention is not particularly limited, and examples thereof include monomers, oligomers or polymers, photopolymerization initiators, plasticizers, leveling agents, surfactants, silane coupling agents, defoamers, pigments, etc., and from the viewpoint of improving bending resistance, oligomers or polymers are preferred.

[0043] The oligomer or polymer is not particularly limited, and examples thereof include acrylic resin, epoxy resin, novolac resin, phenol resin, polyimide precursor, polyimide, etc. Among them, acrylic resin is preferable from the viewpoint of crack resistance when bent. This is presumably because the glass transition temperature of acrylic resin is 100°C or less, and it softens when the conductive film is thermally cured, which enhances the bonding between the conductive particles.

[0044] The acrylic resin is a resin containing at least a structure derived from an acrylic monomer in the repeating unit. Specific examples of the acrylic monomer include all compounds having a carbon-carbon double bond, but are preferably methyl acrylate, acrylic acid, 2-ethylhexyl acrylate, ethyl methacrylate, n-butyl acrylate, i-butyl acrylate, i-propane acrylate, glycidyl acrylate, N-methoxymethylacrylamide, N-ethoxymethylacrylamide, Nn-butoxymethylacrylamide, N-isobutoxymethylacrylamide, butoxytriethylene glycol acrylate, dicyclopentanyl acrylate, dicyclopentenyl acrylate, 2-hydroxyethyl acrylate, isobornyl acrylate, 2-hydroxypropyl acrylate, isodexyl acrylate, isooctyl acrylate, lauryl acrylate, 2-methoxyethyl ... Examples of the acrylate monomer include acrylic monomers such as ethyl acrylate, methoxyethylene glycol acrylate, methoxydiethylene glycol acrylate, octafluoropentyl acrylate, phenoxyethyl acrylate, stearyl acrylate, trifluoroethyl acrylate, acrylamide, aminoethyl acrylate, phenyl acrylate, 1-naphthyl acrylate, 2-naphthyl acrylate, thiophenol acrylate, and benzyl mercaptan acrylate, as well as methacrylates of these acrylates, styrene, p-methylstyrene, o-methylstyrene, m-methylstyrene, α-methylstyrene, chloromethylstyrene, and hydroxymethylstyrene, as well as γ-methacryloxypropyltrimethoxysilane and 1-vinyl-2-pyrrolidone.

[0045] These acrylic monomers may be used alone or in combination of two or more.

[0046] Examples of the metal component used in the present invention include gold, silver, copper, nickel, tin, bismuth, lead, zinc, palladium, platinum, aluminum, tungsten, molybdenum, etc. Among them, it is preferable to contain at least one element selected from the group consisting of gold, silver, copper, nickel, tin, bismuth, lead, zinc, palladium, platinum, and aluminum.

[0047] The metal component used in the present invention is more preferably copper. By using copper as the metal component, an antenna having excellent conductivity and stability can be easily obtained, and the adhesion between the antenna layer containing the metal component and the antenna layer containing the conductive component and the organic component described above can be improved.

[0048] In addition, the thickness of the lower layer antenna 11 is preferably equal to the thickness of the lower electrode of the FET 104. This allows the lower layer antenna and the lower electrode to be formed more easily and at a lower cost than when the thicknesses of the two are different. In addition, the thicknesses of the lower layer antenna and the lower electrode are preferably each 1 μm or less, and more preferably both 1 μm or less. This makes it easier to prevent leakage current between the upper electrode and the lower electrode even when the gate insulating layer is thin, and improves the FET characteristics, thereby improving the operational stability of the wireless communication device.

[0049] In addition, it is preferable that the upper layer antenna 12 contains a conductive component and an organic component, and the thickness of the upper layer antenna 12 is three or more times thicker than the thickness of the lower layer antenna 11. This improves the adhesion between the upper layer antenna and the lower layer antenna, and improves the bending resistance of the wireless communication device. In addition, when a large number of the wireless communication devices are manufactured on a long substrate by the RtoR method, the following advantages are obtained. In the manufacturing method by the RtoR method, bending and rubbing occur in the long film during the manufacturing process of the wireless communication device and when storing the long film on which a large number of wireless communication devices are formed after manufacturing. These can cause peeling and chipping of the wireless communication device on the film, but by adopting a configuration in which the upper layer antenna 12 contains a conductive component and an organic component and the thickness of the upper layer antenna 12 is three or more times thicker than the thickness of the lower layer antenna 11, such peeling and chipping can be suppressed.

[0050] The thicknesses of the upper layer antenna, lower layer antenna, and lower electrode can be calculated by observing the cross-section of a wireless communication device using a scanning electron microscope (SEM) or transmission electron microscope (TEM), and averaging the thickness measurements taken at any five points on each of the upper layer antenna, lower layer antenna, and lower electrode.

[0051] In addition, it is preferable that the area of ​​the overlapping portion between the upper layer antenna and the lower layer antenna is 50% or more of the overall projected area of ​​the antenna from above. The area of ​​the overlapping portion between the upper layer antenna and the lower layer antenna means the area of ​​the portion where the upper layer antenna is directly laminated on the lower layer antenna. By having the area of ​​the overlapping portion be 50% or more of the overall projected area of ​​the antenna from above, it is possible to improve the adhesion between the upper layer antenna and the lower layer antenna while easily adjusting the impedance matching between the circuit section and the antenna.

[0052] Whether the upper layer antenna is directly laminated onto the lower layer antenna can be confirmed by observing the cross section of the wireless communication device with a scanning electron microscope (SEM), a transmission electron microscope (TEM), etc. In addition, the overlapping area of ​​the upper layer antenna and the lower layer antenna can be calculated by peeling the wireless communication device from the substrate as necessary and observing it from the front and back sides.

[0053] There are no particular restrictions on the material used for connection portion 103, and any material containing a usable conductive component may be used; however, using the same material as that used to construct upper layer antenna 12 and / or lower layer antenna 11 allows for reducing the number of types of material while avoiding insufficient strength or peeling due to bonding between dissimilar metals.

[0054] The FET 104 will be described in detail later.

[0055] The wireless communication device described in the first embodiment of the present invention can be used for applications such as contactlessly supplying energy to an LED to light it up by connecting an LED to the circuit section. Also, by connecting a sensor to the circuit section, the device can be used for applications such as contactlessly modulating a carrier wave in response to sensor detection and communicating the signal as an electrical signal. Also, by providing a memory element to the circuit section, the device can be used for applications such as contactlessly transmitting and receiving unique information as a signal via a reader / writer.

[0056] (Embodiment 2) 8 is a schematic diagram showing the configuration of a wireless communication device according to embodiment 2 of the present invention, illustrating another example of the configuration of the FET included in the antenna and circuit unit constituting the wireless communication device shown in FIG.

[0057] As in Fig. 2 shown in the first embodiment, this embodiment will be described by taking as an example a cross-sectional view of an example of the configuration of an antenna constituting a wireless communication device and a FET included in a circuit unit along line I-I' within the area surrounded by a dashed line in Fig. 1. For the sake of simplicity, two FETs 204 included in the circuit unit are shown in Fig. 8, but the circuit unit 102 in this embodiment includes as many FETs of similar configuration as are necessary to configure the above-mentioned demodulation circuit, operation control logic circuit, modulation circuit, etc. The circuit unit 102 also includes connection wiring that connects these circuits.

[0058] In the wireless communication device according to the second embodiment, an antenna 101 and a FET 204 are formed on a substrate 1. In FIG. 8, there are two FETs 104, and on the substrate 1, they have a source electrode 5 and a drain electrode 6 corresponding to a lower electrode, a gate insulating layer 3, and a gate electrode 2 corresponding to an upper electrode. The gate electrode 2 is electrically insulated from the source electrode 5 and the drain electrode 6 by the gate insulating layer 3. The FET 104 further has a semiconductor layer 4 between the source electrode 5 and the drain electrode 6. In the second embodiment, the gate insulating layer 3 is shared between the two FETs 104, but may be provided independently in each FET 104.

[0059] The structure of the FET 104 illustrated in FIG. 8 is a so-called top gate structure in which the gate electrode is disposed above the semiconductor layer (opposite the substrate), and the source electrode and drain electrode are disposed on the same plane as the semiconductor layer.

[0060] Thus, except that the FET 204 has a top-gate structure, the wireless communication device according to the second embodiment is similar to the wireless communication device according to the first embodiment described above.

[0061] <Field-effect transistor> Next, a field effect transistor (FET) suitable for use in each of the above-mentioned embodiments of the present invention will be described in detail, focusing on the partial views of the first and second embodiments as representative examples.

[0062] (Lower and upper electrodes) The material used for the lower electrode and the upper electrode may be any material that contains a conductive component.

[0063] The width and thickness of the upper and lower electrodes, and the distance between the electrodes are arbitrary. Specifically, in the case of a gate electrode, the width of the electrode is preferably 5 μm or more and 1 mm or less. By setting the width of the gate electrode within this range, it becomes easier to control the overlap with the source and drain electrodes and the FET characteristics by controlling the channel length. The distance between the source and drain electrodes is preferably 1 μm or more and 500 μm or less.

[0064] Furthermore, the width and thickness of the wiring are also arbitrary. Specifically, the thickness of the wiring is preferably 0.01 μm or more and 100 μm or less. The width of the wiring is preferably 5 μm or more and 500 μm or less. However, these dimensions are not limited to the above.

[0065] (Gate insulation layer) The material used for the gate insulating layer is not particularly limited, but may be inorganic materials such as silicon oxide and alumina; organic polymer materials such as polyimide, polyvinyl alcohol, polyvinyl chloride, polyethylene terephthalate, polyvinylidene fluoride, polysiloxane, and polyvinylphenol; or a mixture of inorganic material powder and organic material. Among them, it is preferable to include an organic compound containing a bond between a silicon atom and a carbon atom. In addition, it is more preferable to include a metal compound containing a bond between a metal atom and an oxygen atom.

[0066] The gate insulating layer may be a single layer or multiple layers. In addition, one layer may be formed from multiple insulating materials, or multiple insulating materials may be stacked to form multiple insulating layers.

[0067] (Semiconductor layer) The material used for the semiconductor layer is not particularly limited as long as it exhibits semiconductivity, and a material with high carrier mobility is preferably used. In addition, a material that can be applied by a low-cost and simple coating process is preferable, and preferred examples include organic semiconductors and carbon materials.

[0068] Examples of the organic semiconductor that can be used include known organic semiconductors such as pentacene, polythiophenes, compounds containing a thiophene unit in the main chain, polypyrroles, poly(p-phenylenevinylenes), polyanilines, polyacetylenes, polydiacetylenes, polycarbazoles, polyfurans, polyheteroaryls having a nitrogen-containing aromatic ring as a constituent unit, condensed polycyclic aromatic compounds, heteroaromatic compounds, aromatic amine derivatives, biscarbazole derivatives, pyrazoline derivatives, stilbene compounds, hydrazone compounds, metal phthalocyanines such as copper phthalocyanine, metal porphyrins such as copper porphyrin, distyrylbenzene derivatives, aminostyryl derivatives, aromatic acetylene derivatives, condensed ring tetracarboxylic acid diimides, and organic dyes, and two or more of these may be used.

[0069] Examples of carbon materials include carbon nanotubes (hereafter referred to as CNTs), graphene, and fullerenes. When applied to the roll-to-roll method, CNTs are preferred because they can be formed at low temperatures of 200°C or less, are highly suitable for coating processes, and, unlike organic semiconductors, do not require crystallization and can achieve high mobility due to the network structure between CNTs, making it easy to maintain high mobility even if the sheet substrate expands and contracts due to external factors such as heat or tension.

[0070] As the CNT, any of the following may be used: single-walled CNT in which one carbon film (graphene sheet) is wound in a cylindrical shape; double-walled CNT in which two graphene sheets are wound concentrically; and multi-walled CNT in which multiple graphene sheets are wound concentrically. Two or more of these may be used. From the viewpoint of exhibiting semiconductor properties, it is preferable to use single-walled CNT, and it is more preferable that the single-walled CNT contains 90% by weight or more of semiconducting single-walled CNT. It is even more preferable that the single-walled CNT contains 95% by weight or more of semiconducting single-walled CNT.

[0071] Furthermore, CNTs having a conjugated polymer attached to at least a portion of the surface (hereinafter referred to as a CNT composite) are particularly preferred because they have excellent dispersion stability in solution and can provide high mobility. Here, the conjugated polymer refers to a compound whose repeating unit has a conjugated structure and has a degree of polymerization of 2 or more. Furthermore, by using a solution in which CNTs are uniformly dispersed, a film in which CNTs are uniformly dispersed can be formed by a coating method such as an inkjet method.

[0072] The state where a conjugated polymer is attached to at least a part of the surface of a CNT means that the conjugated polymer covers a part or the entire surface of the CNT. It is speculated that the reason why a conjugated polymer can cover a CNT is because the π-electron clouds derived from each conjugated structure overlap and interact with each other. Whether a CNT is covered with a conjugated polymer can be determined by checking whether the reflected color of the covered CNT approaches that of the conjugated polymer from that of the uncovered CNT. The presence of the deposit and the mass ratio of the deposit to the CNT can be quantitatively identified by elemental analysis such as X-ray photoelectron spectroscopy (XPS).

[0073] The conjugated polymer to be attached to the CNT can be used regardless of its molecular weight, molecular weight distribution, or structure. In view of ease of attachment to the CNT, the conjugated polymer preferably has a weight average molecular weight of 1000 or more.

[0074] Methods for attaching a conjugated polymer to CNT include (I) a method of adding CNT to a molten conjugated polymer and mixing it, (II) a method of dissolving a conjugated polymer in a solvent, adding CNT to the solution, and mixing it, (III) a method of adding a conjugated polymer to a solution in which CNT has been preliminarily dispersed in a solvent using ultrasonic waves or the like, and (IV) a method of putting a conjugated polymer and CNT in a solvent, and mixing the mixture by irradiating ultrasonic waves, etc. In the present invention, a combination of multiple methods may be used.

[0075] In the present invention, the length of the CNT is preferably shorter than the distance (channel length) between the source electrode and the drain electrode. The average length of the CNT depends on the channel length, but is preferably 2 μm or less. Since commercially available CNTs generally have a distribution in length and may contain CNTs longer than the channel length, it is preferable to add a process of shortening the CNT to be shorter than the channel length. For example, a method of cutting the CNT into short fibers by acid treatment with nitric acid, sulfuric acid, or the like, ultrasonic treatment, or freeze-pulverization is effective. In addition, it is more preferable to use separation by a filter in order to improve purity.

[0076] Furthermore, the diameter of the CNT is not particularly limited, but is preferably from 1 nm to 100 nm, and more preferably 50 nm or less.

[0077] Examples of the conjugated polymer that coats the CNT include polythiophene polymers, polypyrrole polymers, polyaniline polymers, polyacetylene polymers, poly-p-phenylene polymers, poly-p-phenylenevinylene polymers, and thiophene-heteroarylene polymers having thiophene units and heteroaryl units in the repeating units, and two or more of these may be used. The above polymers may be those in which a single monomer unit is arranged, those in which different monomer units are block copolymerized, those in which random copolymerization is performed, and those in which graft polymerization is performed.

[0078] The semiconductor layer may be a mixture of a CNT composite and an organic semiconductor. By uniformly dispersing the CNT composite in the organic semiconductor, it is possible to achieve high mobility while maintaining the properties of the organic semiconductor itself.

[0079] The semiconductor layer may further include an insulating material, such as the insulating material composition of the present invention, or a polymer material such as poly(methyl methacrylate), polycarbonate, or polyethylene terephthalate, but is not limited to these.

[0080] The semiconductor layer may be a single layer or multiple layers. The thickness of the semiconductor layer is preferably 1 nm to 200 nm, more preferably 100 nm or less. By setting the thickness within this range, it becomes easy to form a uniform thin film, and furthermore, it is possible to suppress the source-drain current that cannot be controlled by the gate voltage, and to increase the on-off ratio of the FET. The thickness can be measured by an atomic force microscope, ellipsometry, etc.

[0081] An orientation layer can be provided between the gate insulating layer and the semiconductor layer. For the orientation layer, known materials such as silane compounds, titanium compounds, organic acids, and heteroorganic acids can be used, and organic silane compounds are particularly preferred.

[0082] In the present invention, a second insulating layer may be formed on the semiconductor layer on the opposite side to the gate insulating layer, thereby protecting the semiconductor layer from the external environment such as oxygen and moisture.

[0083] The material used for the second insulating layer is not particularly limited, but specific examples include inorganic materials such as silicon oxide and alumina, polymer materials such as polyimide and its derivatives, polyvinyl alcohol, polyvinyl chloride, polyethylene terephthalate, polyvinylidene fluoride, polysiloxane and its derivatives, polyvinylphenol and its derivatives, and the like, or mixtures of inorganic material powders and polymer materials, and mixtures of organic low molecular weight materials and polymer materials.

[0084] The formed FET can control the current flowing between the source and drain electrodes by changing the gate voltage. The mobility, which is an index of the performance of the FET, can be calculated using the following formula (a).

[0085] μ=(δId / δVg)L·D / (W·εr·ε·Vsd) (a) where Id is the source-drain current, Vsd is the source-drain voltage, Vg is the gate voltage, D is the thickness of the gate insulating layer, L is the channel length, W is the channel width, εr is the relative dielectric constant of the gate insulating layer, and ε is the dielectric constant of vacuum (8.85×10 -12 F / m).

[0086] The above-mentioned FET has high mobility and is an FET in which the relative positions of the gate electrode, source electrode and drain electrode are controlled with high precision.

[0087] <Method of manufacturing wireless communication device> A method for manufacturing a wireless communication device according to the present invention will be described in detail, focusing on the method for manufacturing a wireless communication device according to the first embodiment as a representative example. The method for manufacturing a wireless communication device according to the present invention is for manufacturing the wireless communication device according to the above-mentioned embodiment. The method for manufacturing the wireless communication device according to the above-mentioned embodiment includes the steps of: (A) forming a lower electrode of a field effect transistor and a lower antenna on a substrate simultaneously or successively; (B) simultaneously or successively forming an upper electrode of the field effect transistor and an upper layer antenna on the substrate; This makes it possible to reduce the number of types of materials and steps.

[0088] Fig. 9 is a perspective view of the area surrounded by the dashed line in Fig. 1, and shows an example of the configuration of an antenna and a FET included in the circuit unit constituting the wireless communication device shown in Fig. 1. For the sake of simplicity, Fig. 9 shows two FETs included in the circuit unit, but the circuit unit 102 in this embodiment includes as many FETs of similar configuration as are necessary to configure the above-mentioned demodulation circuit, operation control logic circuit, modulation circuit, etc. The circuit unit 102 also includes connection wiring that connects these circuits.

[0089] First, as shown in Fig. 9(a), the gate electrode 2 and the lower layer antenna 11, which correspond to the lower electrode, are formed on the substrate 1 simultaneously or successively. "Simultaneously" means that the gate electrode 2 and the lower layer antenna 11 are formed at the same time. "Successively" means that one of the gate electrode 2 or the lower layer antenna 11 is formed first, and then the other is formed before the step of forming the next gate insulating layer. Among these, it is preferable to form the gate electrode 2 and the lower layer antenna 11 at the same time.

[0090] Methods for forming the gate electrode and the lower layer antenna include methods using known techniques such as vacuum deposition, electron beam, sputtering, plating, CVD, ion plating coating, inkjet, and printing, and methods in which a paste containing an organic component and conductive particles is applied onto an insulating substrate by known techniques such as blade coating, slit die coating, screen printing, bar coater, casting, print transfer, and immersion and pulling, and then dried using an oven, a hot plate, infrared rays, or the like, to form the gate electrode and the lower layer antenna. However, there are no particular limitations on the methods as long as they can provide electrical conductivity.

[0091] The lower electrode and the lower antenna may be patterned in a desired shape by using a known photolithography method or the like to pattern the electrode thin film prepared by the above method, or the electrode and wiring material may be patterned through a mask of a desired shape during vacuum deposition or sputtering. Alternatively, the pattern may be directly formed using an inkjet or printing method.

[0092] For example, a metal film is formed on the entire surface of a PET substrate by sputtering or vacuum deposition, and a pattern is formed by photolithography using a photoresist through a photomask on which the lower antenna and lower electrode are designed.

[0093] Alternatively, a photosensitive conductive paste is applied onto a PET substrate and directly patterned by photolithography using a photomask on which the lower antenna and lower electrode are designed.

[0094] However, among these methods, the method of processing a metal film formed by sputtering or vacuum deposition into a pattern corresponding to the lower electrode and lower layer antenna is preferable. By using these methods, it is possible to form a lower electrode and lower layer antenna with high flatness and uniform thickness and pattern shape, thereby reducing the leakage rate of the FET and the variation in FET characteristics.

[0095] 9(b), a gate insulating layer 3 is formed on the gate electrode 2. Methods for forming the gate insulating layer include known techniques such as vacuum deposition, electron beam, sputtering, plating, CVD, ion plating coating, inkjet, printing, spin coating, blade coating, slit die coating, bar coater, casting, printing transfer, and immersion and pulling up, but are not limited to these.

[0096] Next, as shown in FIG. 9(c), a solution containing CNT is applied onto the gate insulating layer 3 to form the semiconductor layer 4. As a method for forming the semiconductor layer 4, a coating method is preferably used from the viewpoints of manufacturing cost and suitability for large areas. Examples of the coating method include known coating methods such as spin coating, blade coating, slit die coating, screen printing, bar coating, mold coating, print transfer, immersion and pulling, and inkjet coating. Among them, any one selected from the group consisting of the inkjet method, dispenser method, and spray method is preferable. Furthermore, from the viewpoint of the efficiency of using raw materials, the inkjet method is more preferable. From these coating methods, an appropriate one can be selected according to the coating film properties to be obtained, such as coating film thickness control and orientation control.

[0097] The formed coating film may be subjected to an annealing treatment in air, under reduced pressure, or in an inert gas atmosphere (nitrogen or argon atmosphere).

[0098] Next, as shown in FIG. 9(d), a source electrode 5 and a drain electrode 6 corresponding to the upper electrodes are formed on the gate insulating layer 3 and the semiconductor layer 4. In addition, an upper layer antenna 12 is formed on the lower layer antenna 11. These are formed simultaneously or successively. "Simultaneously" means that the source electrode 5, the drain electrode 6, and the upper layer antenna 12 are formed at the same time. "Successively" means that either the source electrode 5 and the drain electrode 6 or the upper layer antenna 12 is formed first, and then the other is formed. Among these, it is preferable to form the source electrode 5, the drain electrode 6, and the upper layer antenna 12 at the same time.

[0099] These forming methods include methods using known techniques such as vacuum deposition, electron beam, sputtering, plating, CVD, ion plating coating, inkjet, and printing, and methods in which a paste containing organic components and conductive particles is applied to an insulating substrate by known techniques such as spin coating, blade coating, slit die coating, screen printing, bar coater, casting, printing transfer, and immersion and pulling, and then dried using an oven, hot plate, infrared, or the like, but are not particularly limited as long as they can be conductive. As a method for forming the upper electrode and upper layer antenna in a pattern, the electrode thin film produced by the above method may be patterned into a desired shape by known photolithography, or the electrode and wiring material may be patterned through a mask of a desired shape during deposition or sputtering. In addition, a pattern may be formed directly using an inkjet or printing method.

[0100] Among these methods, it is preferable to apply a photosensitive conductive paste and form a pattern by photolithography.

[0101] The method for simultaneously forming the upper layer antenna and the upper electrode using the photosensitive conductive paste preferably includes (B-1) a film forming step of forming a coating film on a substrate using a photosensitive conductive paste containing conductive particles and a photosensitive organic component, and (B-2) a step of patterning the coating film by a photolithography method. More specifically, the method preferably includes a step of applying the photosensitive conductive paste on a substrate to form a coating film, a step of exposing the coating film, and a step of developing the exposed coating film, and further includes a step of curing the coating film to simultaneously develop the conductivity of the patterns corresponding to the upper layer antenna and the upper electrode.

[0102] In the process of applying a photosensitive conductive paste onto a substrate to form a coating film, there are a method of applying a region required to form a pattern corresponding to the upper layer antenna and the upper electrode in an exposure process and a development process, a method of applying a pattern film corresponding to the upper layer antenna and a region required to form a pattern corresponding to the upper electrode in an exposure process and a development process, etc. In addition, a part or the whole of the coating film may be coated in layers to increase the thickness.

[0103] Even if a pattern corresponding to the upper layer antenna is formed by the process of applying a photosensitive conductive paste onto a substrate, it is possible to improve the film strength and conductivity by further exposing and developing the upper layer antenna pattern.

[0104] In addition, to align the lower and upper electrodes of the TFT, a photosensitive conductive paste is used, and a self-alignment photolithography method is used in which the lower electrode is used as a mask to expose the substrate from the back side where the photosensitive conductive paste is applied, making it possible to form the upper electrode pattern with high alignment precision.

[0105] The photosensitive conductive paste contains at least conductive particles and a photosensitive organic component. The conductive paste is produced by mixing the necessary materials and then using a dispersing machine or kneading machine such as a three-roller mill, a ball mill, or a planetary ball mill.

[0106] (Conductive particles) Examples of the conductive particles contained in the conductive paste used in the present invention include gold, silver, copper, nickel, tin, bismuth, lead, zinc, palladium, platinum, aluminum, tungsten, molybdenum, carbon, etc. Among them, conductive particles containing at least one element selected from the group consisting of gold, silver, copper, nickel, tin, bismuth, lead, zinc, palladium, platinum, aluminum, and carbon are preferred.

[0107] In the conductive component used in the present invention, the conductive component is preferably silver particles. When the conductive component is silver particles, a conductive film or conductive pattern having excellent conductivity and stability can be easily obtained. Preferably, silver particles are used.

[0108] (Photosensitive organic component) The photosensitive organic component preferably contains a monomer, oligomer, or polymer having a polymerizable unsaturated group in the molecule, such as an ethylenically unsaturated group such as a vinyl group, an allyl group, an acrylate group, or a methacrylate group, or an acrylamide group.

[0109] (Photopolymerization initiator / sensitizer) In order to photocure the photosensitive organic component by photoreaction, the conductive paste preferably contains a photopolymerization initiator. Examples of the photopolymerization initiator include a photoradical polymerization initiator and a photocationic polymerization initiator, and may be appropriately selected depending on the light used in the exposure step.

[0110] In addition, by using a sensitizer together with the photopolymerization initiator in the conductive paste, the sensitivity can be improved and the wavelength range effective for the reaction can be expanded.

[0111] (solvent) The photosensitive conductive paste preferably contains an organic solvent from the viewpoints of adjusting the viscosity and improving the surface smoothness of the coating film. The viscosity of the conductive paste (measured at 3 rpm with a Brookfield viscometer) is preferably 10 to 100 Pa·s, more preferably 10 to 50 Pa·s, from the viewpoints of preventing poor coating caused by the settling of conductive particles, preventing dripping, and improving coverage.

[0112] Examples of organic solvents include methyl ethyl ketone, dioxane, acetone, cyclohexanone, cyclopentanone, isobutyl alcohol, isopropyl alcohol, tetrahydrofuran, γ-butyrolactone, bromobenzene, chlorobenzene, dibromobenzene, dichlorobenzene, bromobenzoic acid, chlorobenzoic acid, diethylene glycol monoethyl ether acetate, diethylene glycol monobutyl ether, diethylene glycol monobutyl ether acetate, 2-methyl-2,4-pentanediol, 3-methyl-1,5-pentanediol, 2-ethyl-1,3-hexanediol, terpineol, 3-methyl-3-methoxybutanol, texanol, benzyl alcohol, dipropylene glycol monoethyl ether, tripropylene glycol monomethyl ether, and propylene glycol monomethyl ether acetate.

[0113] (Other Ingredients) The conductive paste may contain additives such as organic or inorganic pigments, glass powder, fillers, plasticizers, leveling agents such as special vinyl polymers or special acrylic polymers, surfactants, silane coupling agents, defoamers, or antioxidants.

[0114] According to the manufacturing method of the wireless communication device described above, the circuit section includes a field effect transistor having a bottom gate structure, and the formation of the gate electrode and the lower layer antenna included in the field effect transistor, and the formation of the source electrode, drain electrode and upper layer antenna are performed simultaneously or consecutively, respectively, thereby reducing the number of processes compared to the case where the electrodes and wiring are manufactured in separate processes.

[0115] Furthermore, since the circuit portion and the antenna are patterned by photolithography, the accuracy of aligning the circuit portion and the antenna can be improved compared to a method in which the circuit portion and the antenna are formed separately and then bonded together.

[0116] The above-described method for manufacturing a wireless communication device can be applied to both the case of manufacturing a wireless communication device on a single substrate and the case of manufacturing a plurality of wireless communication devices on a long substrate by the RtoR method. EXAMPLES

[0117] The present invention will be described in more detail below with reference to examples, although the present invention is not limited to the following examples.

[0118] (Preparation of photosensitive paste) Synthesis example 1; Compound P1 (photosensitive organic component) Copolymerization ratio (by mass): ethyl acrylate (hereinafter, "EA") / 2-ethylhexyl methacrylate (hereinafter, "2-EHMA") / styrene (hereinafter, "St") / glycidyl methacrylate (hereinafter, "GMA") / acrylic acid (hereinafter, "AA") = 20 / 40 / 20 / 5 / 15.

[0119] In a reaction vessel in a nitrogen atmosphere, 150 g of diethylene glycol monoethyl ether acetate (hereinafter, "DMEA") was charged, and the temperature was raised to 80°C using an oil bath. A mixture consisting of 20 g of EA, 40 g of 2-EHMA, 20 g of St, 15 g of AA, 0.8 g of 2,2'-azobisisobutyronitrile, and 10 g of DMEA was added dropwise over 1 hour. After the dropwise addition was completed, the polymerization reaction was carried out for another 6 hours. Then, 1 g of hydroquinone monomethyl ether was added to stop the polymerization reaction. Subsequently, a mixture consisting of 5 g of GMA, 1 g of triethylbenzylammonium chloride, and 10 g of DMEA was added dropwise over 0.5 hours. After the dropwise addition was completed, the addition reaction was carried out for another 2 hours. The obtained reaction solution was purified with methanol to remove unreacted impurities, and further dried in vacuum for 24 hours to obtain compound P1.

[0120] Synthesis example 2; Compound P2 (photosensitive organic component) Copolymerization ratio (by mass): bifunctional epoxy acrylate monomer (Epoxy Ester 3002A; manufactured by Kyoeisha Chemical Co., Ltd.) / bifunctional epoxy acrylate monomer (Epoxy Ester 70PA; manufactured by Kyoeisha Chemical Co., Ltd.) / GMA / St / AA=20 / 40 / 5 / 20 / 15.

[0121] In a reaction vessel in a nitrogen atmosphere, 150 g of diethylene glycol monoethyl ether acetate (hereinafter, "DMEA") was charged, and the temperature was raised to 80°C using an oil bath. A mixture consisting of 20 g of epoxy ester 3002A, 40 g of epoxy ester 70PA, 20 g of St, 15 g of AA, 0.8 g of 2,2'-azobisisobutyronitrile, and 10 g of DMEA was added dropwise over 1 hour. After the dropwise addition was completed, the polymerization reaction was carried out for another 6 hours. Then, 1 g of hydroquinone monomethyl ether was added to stop the polymerization reaction. Subsequently, a mixture consisting of 5 g of GMA, 1 g of triethylbenzylammonium chloride, and 10 g of DMEA was added dropwise over 0.5 hours. After the dropwise addition was completed, the addition reaction was carried out for another 2 hours. The obtained reaction solution was purified with methanol to remove unreacted impurities, and further dried in vacuum for 24 hours to obtain compound P2.

[0122] Synthesis Example 3; Compound P3 (photosensitive organic component) Compound P2 urethane modified compound 100g of DMEA was charged into a reaction vessel in a nitrogen atmosphere, and the temperature was raised to 80°C using an oil bath. A mixture consisting of 10g of photosensitive component P2, 3.5g of n-hexyl isocyanate, and 10g of DMEA was added dropwise to the reaction vessel over a period of 1 hour. After the addition was completed, the reaction was continued for another 3 hours. The resulting reaction solution was purified with methanol to remove unreacted impurities, and then vacuum dried for 24 hours to obtain compound P3 having a urethane bond.

[0123] Preparation Example 1: Photosensitive Paste A In a 100 ml clean bottle, 16 g of the compound P1 obtained above, 4 g of compound P3, 2 g of light acrylate BP-4EA (Kyoeisha Chemical Co., Ltd.), 4 g of photopolymerization initiator OXE-01 (BASF Japan Ltd.), 0.6 g of acid generator SI-110 (Sanshin Chemical Industry Co., Ltd.), and 10 g of γ-butyrolactone (Mitsubishi Gas Chemical Co., Ltd.) were added and mixed with a rotation-revolution vacuum mixer "Awatori Rentaro" (registered trademark) (ARE-310; Thinky Co., Ltd.) to obtain 34.6 g of photosensitive resin solution 1 (solid content 78.5% by mass). 8.0 g of the obtained photosensitive resin solution 1 was mixed with 42.0 g of Ag particles having an average particle size of 0.06 μm, and kneaded using a three-roller "EXAKT M-50" (trade name, EXAKT Co., Ltd.) to obtain 50 g of photosensitive paste A.

[0124] Preparation example 2: Photosensitive paste B Into a clean bottle were placed 25.0 g of a solution of alkali-soluble resin 1 (40% by mass), 1.5 g of Irgacure (registered trademark) OXE02 (oxime ester compound; manufactured by BASF) as a photopolymerization initiator, 5.5 g of Light Acrylate (registered trademark) PE-4A (manufactured by Kyoeisha Chemical Co., Ltd.), and 2.0 g of DISPERBYK (registered trademark) 140 (manufactured by BYK Japan KK) (amine value: 146 mg KOH / g) as a dispersant, and mixed using a planetary centrifugal mixer "Awatori Rentaro" (registered trademark) (ARE-310; manufactured by Thinky Corporation) to obtain a photosensitive resin solution 2.

[0125] 8.0 g of the obtained photosensitive resin solution 2 was mixed with 42.0 g of Ag particles having an average particle diameter of 0.06 μm, and DMEA was added so that the solid content ratio was 80 mass %. The mixture was then kneaded using a three-roller “EXAKT M-50” (product name, manufactured by EXAKT) to obtain a conductive paste B.

[0126] Preparation example 3: Photosensitive paste C Photosensitive paste C was obtained in the same manner as in Preparation Example 2, except that Ag particles having an average particle size of 0.30 μm were used.

[0127] Preparation example 4: Photosensitive paste D Photosensitive paste C was obtained in the same manner as in Preparation Example 2, except that Ag particles having an average particle size of 0.50 μm were used.

[0128] (Preparation of semiconductor solution) In preparing the semiconductor solution, first, 1.0 mg of CNT (CNI, single-walled CNT, purity 95%) was added to a chloroform solution (10 ml) containing 2.0 mg of P3HT (Aldrich, poly(3-hexylthiophene)), and the mixture was ultrasonically stirred for 4 hours at 20% output using an ultrasonic homogenizer (Tokyo Rikakikai, VCX-500) while cooling on ice. This resulted in CNT dispersion A11 (CNT composite concentration in solvent: 0.96 g / l).

[0129] Next, the CNT dispersion A11 was filtered using a membrane filter (pore size 10 μm, diameter 25 mm, Millipore Omnipore Membrane) to remove CNT composites with a length of 10 μm or more. 5 ml of o-DCB (Wako Pure Chemical Industries, Ltd.) was added to the filtrate obtained in this way, and then the low boiling point solvent chloroform was distilled off using a rotary evaporator, thereby replacing the solvent with o-DCB to obtain CNT dispersion B11. 3 ml of o-DCB was added to CNT dispersion B11 (1 ml), thereby obtaining semiconductor solution A (CNT composite concentration relative to the solvent is 0.03 g / l).

[0130] (Example of gate insulating layer fabrication) 13.12g (0.05 mol) of 3-trimethoxysilylpropyl succinic anhydride (SucSi), 93.73g (0.40 mol) of 3-acryloxypropyltrimethoxysilane (AcrSi) and 109.06g (0.55 mol) of phenyltrimethoxysilane (PheSi) were dissolved in 215.91g of propylene glycol monomethyl ether acetate (PGMEA, boiling point 146°C), and 54.90g of water and 0.864g of phosphoric acid were added thereto while stirring. The resulting solution was heated at a bath temperature of 105°C for 2 hours, the internal temperature was raised to 90°C, and the components mainly consisting of by-produced methanol were distilled out. Next, the solution was heated at a bath temperature of 130°C for 2 hours, the internal temperature was raised to 118°C, and the components mainly consisting of water and methanol were distilled out, and then cooled to room temperature to obtain a polysiloxane solution A with a solid content concentration of 26.0 mass%. 10 g of the obtained polysiloxane solution A was weighed out, and 1.04 g of DPHA (trade name "KAYARAD", manufactured by Nippon Kayaku Co., Ltd.; dipentaerythritol hexaacrylate), 0.15 g of OXE-01 (trade name "Irgacure", manufactured by BASF Ltd.) and 4.60 g of PGMEA were mixed and stirred at room temperature for 2 hours to obtain gate insulating layer solution A (solid content concentration 24 mass%). The content of DPHA in the gate insulating layer material solution A was 40 parts by mass relative to 60 parts by mass of polysiloxane. The content of OXE-01 in the gate insulating layer solution A was 3.5 parts by mass relative to 60 parts by mass of polysiloxane.

[0131] (Example of creating a second insulating layer) 2.5 g of polymethyl methacrylate (manufactured by Fuji Film Wako Pure Chemical Industries, Ltd.) was dissolved in 7.5 g of N,N-dimethylformamide to prepare polymer solution A. Next, 1 g of N,N,N',N'-tetramethyl-1,4-phenylenediamine (manufactured by Tokyo Chemical Industry Co., Ltd.) was dissolved in 9.0 g of N,N-dimethylformamide to prepare compound solution A. 0.30 g of compound solution A was added to 0.68 g of polymer solution A to obtain second insulating layer solution A.

[0132] Example 1 In Example 1, a wireless communication device according to the first embodiment of the present invention (see FIG. 1) was fabricated in which the circuit section had a ring oscillator formed by combining field effect transistors with a bottom gate-top contact structure.

[0133] In fabricating the semiconductor device of this Example 1, as exemplified in the above-described embodiment 1, after forming FETs, a second insulating layer is formed on some of the FETs to form an inverter including a p-type FET and an n-type FET, and a ring oscillator, which is an oscillation circuit, is fabricated using this inverter.

[0134] Fig. 11 is a schematic plan view showing the configuration of the ring oscillator in the present embodiment 1. This ring oscillator 27 is configured by connecting 21 stages of inverters 26 in series. In Fig. 11, in order to simply show the configuration of the ring oscillator 27, the inverters 26 that are configured in a repeated manner among the 21 inverters 26 are omitted from the illustration. Also, the multiple sets of FETs that configure each of these inverters 26 are connected by wiring (not shown).

[0135] A specific method for fabricating a wireless communication device will be described with reference to FIG. 10. First, copper was vacuum-deposited over the entire surface of a PET film substrate 1 (width 35 mm, length 120 mm, film thickness 50 μm) by resistance heating. A photoresist (product name "LC100-10cP", manufactured by Rohm and Haas Co., Ltd.) was printed over the entire surface by slit coating, and then heated and dried in a hot air drying oven at 100°C for 4 minutes. The fabricated photoresist film was exposed to light at an exposure dose of 40 mJ / cm through a photomask on which a gate electrode 2 and a lower layer antenna 11 were designed. 2(converted to a wavelength of 365 nm) and subjected to full line exposure. The gate electrode width designed on the photomask was set to 50 μm. After exposure, the substrate was developed with a 2.38 wt % tetramethylammonium hydroxide aqueous solution for 30 seconds, and then washed with water for 1 minute. Then, the substrate was etched with mixed acid (product name SEA-5, manufactured by Kanto Chemical Co., Ltd.) for 30 seconds, and then washed with water for 30 seconds. The substrate was immersed in a photoresist stripping solution (product name AZ Remover 100, manufactured by Merck Performance Materials Co., Ltd.) for 2 minutes to remove the resist, washed with water for 30 seconds, and then water droplets were removed with an air knife. Then, the substrate was heated and dried in a hot air drying oven at 80° C. for 60 seconds to form the lower antenna 11 and the gate electrode 2 (FIG. 10(a)).

[0136] Thereafter, the gate insulating layer solution A, which would become the gate insulating layer, was printed by spin coating and then heated and dried in a hot air drying oven at 100° C. for 2 minutes. The gate insulating layer solution A was printed again on the dried film by spin coating and then heated and dried in a hot air drying oven at 100° C. for 2 minutes. The produced gate insulating layer film was exposed to light through a photomask at an exposure dose of 80 mJ / cm2. 2 (converted to a wavelength of 365 nm) was used for the entire exposure. After the exposure, the film was developed with a 2.38% by weight aqueous solution of tetramethylammonium hydroxide for 30 seconds, and then washed with water for 1 minute to expose the electrodes in the contact holes from the gate insulating layer. After that, the film was heat-treated in an IR drying furnace in a nitrogen atmosphere at 150° C. for 20 minutes to form a gate insulating layer 3 with a thickness of 1.5 μm.

[0137] On the substrate on which the gate insulating layer was formed as described above, 100 pL of semiconductor solution A was applied by the inkjet method onto each of the gate insulating layers positioned on the projection of the gate electrode, and a heat treatment was performed in an IR drying furnace under a nitrogen gas flow at 150°C for 30 minutes to form a semiconductor layer 4 (Figure 10(c)).

[0138] Next, photosensitive paste A was applied by screen printing onto the PET film substrate on which the gate insulating layer was formed, and pre-baked in a hot air drying oven at 100°C for 4 minutes. After that, the photosensitive paste A was exposed to light at a dose of 80 mJ / cm through a photomask on which the source electrode 5, the drain electrode 6, and the upper layer antenna 12 were designed to completely overlap with the lower layer antenna 11. 2 (converted to a wavelength of 365 nm) was used for the entire line exposure. After exposure, the substrate was developed with a 0.5% Na2CO3 solution for 30 seconds, washed with ultrapure water for 60 seconds, and then cured in an IR drying furnace at 150°C for 10 minutes. This resulted in the formation of a source electrode 5, a drain electrode 6, and an upper layer antenna 12 (Figure 10(d)). The width of the source electrode and the drain electrode was 1000 μm, and the distance between these electrodes was 20 μm. The formed upper layer antenna 12 and lower layer antenna 11 were observed from the front and back sides of the substrate 1, respectively, and it was confirmed that the overlapping area of ​​the upper layer antenna and the lower layer antenna was 100%.

[0139] Next, 5 μL of the second insulating layer solution A was dropped onto a part of the semiconductor layer 4 on the PET film substrate on which the semiconductor layer was formed, by a drop casting method so as to cover the semiconductor layer 4. After that, the resultant was heat-treated at 110° C. for 30 minutes under a nitrogen gas flow, to form a second insulating layer 7 (FIG. 10(e)). The thickness of the second insulating layer X was 20 μm.

[0140] For the obtained wireless communication device, with a power supply voltage of 5.0 V applied to the ring oscillator circuit, an oscilloscope (DSOX6002A, manufactured by Keysight Technology) was connected to the output of the ring oscillator circuit to observe the waveform and confirm the oscillation operation of the ring oscillator circuit.

[0141] The obtained wireless communication device was evaluated as described in the following sections [1] to [3]. The results of [1] to [3] are shown in Table 1.

[0142] [1] Film thickness measurement The cross section was observed using a scanning electron microscope (SEM), and the thicknesses of the gate electrode, the lower layer antenna, and the upper layer antenna were measured at five arbitrary positions, and the average values ​​were calculated.

[0143] [2] Evaluation of bending resistance The following description will be given with reference to Fig. 12. For a wireless communication device 30, a metal cylinder 29 with a diameter of 30 mm was fixed to the center of the surface on which the antenna was formed, and the sample was placed along the cylinder with an embrace angle of 0° (when the sample was in a flat state) (see Fig. 12(A)), and then bent within a range where the embrace angle with respect to the cylinder was 180° (when the sample was folded back around the cylinder) (see Fig. 12(B)). The bending resistance was evaluated by observing the antenna, the connection between the antenna and the circuit, and the ring oscillator in the circuit with an optical microscope before and after the bending operation to check for peeling and disconnection, and using the following criteria. A (Good): No peeling or breakage is observed even after 300 bending operations. B (Acceptable): No peeling or breakage is observed even after 100 repeated bending operations. C (Fail): After less than 100 repeated bending cycles, peeling and breakage were observed.

[0144] [3] Evaluation of FET characteristics (current value) Five p-type FETs were extracted from the ring oscillator circuit, and the source-drain current (Id)-source-drain voltage (Vsd) characteristics were measured when the gate voltage (Vg) was changed. The measurements were performed in air using a Semiconductor Characterization System Model 4200-SCS (Keithley Instruments, Inc.). The average value of Id at Vsd=-5V when Vg=-5V was changed from +5V to -5V was measured.

[0145] Example 2 In Example 2, a wireless communication device was fabricated in the same manner as in Example 1, except that the thickness of copper vacuum-deposited over the entire surface by a resistance heating method was changed when forming a gate electrode and a lower layer antenna. For the obtained wireless communication device, an oscilloscope (DSOX6002A, manufactured by Keysight Technology) was connected to the output of the ring oscillator circuit while a power supply voltage of 5.0 V was applied to the ring oscillator circuit, and the waveform was observed to confirm the oscillation operation of the ring oscillator circuit.

[0146] Moreover, the obtained wireless communication device was evaluated in the same manner as in [1] to [3] of Example 1. The evaluation results are shown in Table 1.

[0147] (Examples 3 to 5) In Examples 3 to 5, the source electrode, drain electrode, and upper layer antenna were formed by using the photosensitive paste shown in Table 1 instead of the photosensitive paste A, and the devices were fabricated in the same manner as in Example 2. With respect to the obtained wireless communication device, an oscilloscope (DSOX6002A, manufactured by Keysight Technology Corp.) was connected to the output of the ring oscillator circuit while a power supply voltage of 5.0 V was applied to the ring oscillator circuit, and the waveform was observed to confirm the oscillation operation of the ring oscillator circuit.

[0148] Moreover, the obtained wireless communication device was evaluated in the same manner as in [1] to [3] of Example 1. The evaluation results are shown in Table 1.

[0149] [Table 1] [Explanation of symbols]

[0150] 1 Board 2. Gate electrode 3 Gate insulation layer 4 Semiconductor layer 5. Source Electrode 6 Drain electrode 7 Second insulating layer 11 Lower Antenna 12 Upper Antenna 25 Semiconductor Devices 26 Inverter 27 Ring Oscillator 29 Metal Cylinder 30 Wireless communication devices 101 Antenna 102 Circuit section 103 Connection Wiring 104 FET 105 p-type FET 106 n-type FET

Claims

1. On the board, A circuit unit; an antenna connected to the circuit unit; Equipped with the circuit portion includes an element having an upper electrode and a lower electrode, The antenna includes an upper layer antenna and a lower layer antenna, the material constituting the upper layer antenna is the same as the material constituting the upper electrode; the material constituting the lower layer antenna is the same as the material constituting the lower electrode; At least one of the upper layer antenna and the lower layer antenna comprises a conductive component and an organic component. Wireless communication devices.

2. The wireless communication device of claim 1 , wherein the element is a field effect transistor.

3. 3. The wireless communication device of claim 1, wherein one of the top layer antenna or the bottom layer antenna comprises a conductive component and an organic component, and the other comprises a metallic component.

4. 4. The wireless communication device according to claim 1, wherein the lower layer antenna and the lower electrode have the same thickness.

5. The wireless communication device of claim 4 , wherein the thickness of the lower layer antenna and the lower electrode is 1 μm or less.

6. 6. The wireless communication device according to claim 1, wherein the upper layer antenna includes a conductive component and an organic component, and the thickness of the upper layer antenna is at least three times greater than the thickness of the lower layer antenna.

7. 7. The wireless communication device according to claim 1, wherein an area of ​​an overlap between the upper layer antenna and the lower layer antenna is 50% or more of an area of ​​the entire antenna projected from above.

8. 8. The wireless communication device according to claim 1, wherein the element is a field effect transistor, the field effect transistor includes a semiconductor layer, and the semiconductor layer contains carbon nanotubes.

9. 9. The wireless communication device according to claim 1, wherein the element is a field effect transistor, the upper electrode is a source electrode and a drain electrode, and the lower electrode is a gate electrode.

10. 9. The wireless communication device according to claim 1, wherein the element is a field effect transistor, the upper electrode is a gate electrode, and the lower electrode is a source electrode and a drain electrode.

11. The wireless communication device according to claim 1, wherein the antenna transmits and receives signals to and from a transceiver in a non-contact manner.

12. A method for manufacturing a wireless communication device according to any one of claims 1 to 11, comprising the steps of: (A) simultaneously or consecutively forming a lower electrode and a lower layer antenna of an element on a substrate; (B) simultaneously or successively forming an upper electrode and an upper layer antenna of the element on the substrate; A method for manufacturing a wireless communication device comprising:

13. The method for manufacturing a wireless communication device according to claim 12, wherein the step of (B) simultaneously or successively forming the upper electrode and the upper layer antenna of the element on the substrate includes: (B-1) a film formation step of forming a coating film on the substrate using a photosensitive conductive paste containing conductive particles and a photosensitive organic component; and (B-2) a step of patterning the coating film by a photolithography method.

Citation Information

Patent Citations

  • Integrated inductor structure and its manufacture

    JP1997162354A

  • Semiconductor device and method for manufacturing same

    JP2007043115A

  • Semiconductor device, and method for manufacturing same

    JP2008112988A

  • Antenna circuit configuring body for IC card / tag, and method for manufacturing the same

    JP2012008857A

  • Semiconductor device, display module and electronic apparatus

    JP2013236093A