Coil parts

The coil component design addresses stress and material cost issues by employing smaller first via conductors for parallel connections and larger second via conductors for series connections, ensuring efficient and cost-effective electrical performance.

JP7559727B2Active Publication Date: 2024-10-02MURATA MFG CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2021159269
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-09-29
Publication Date
2024-10-02
Estimated Expiration
2041-09-29

AI Technical Summary

Technical Problem

The increasing stress between insulating layers and coil conductors due to stacking multiple sheets leads to cracks, and the use of more conductive material in through holes increases material costs.

Method used

A coil component design with smaller first via conductors connecting coil conductor layers in parallel and larger second via conductors in series, reducing the amount of conductive material used while maintaining good electrical characteristics.

Benefits of technology

Reduces conductive material usage while achieving desired coil characteristics by using smaller first via conductors for parallel connections and larger second via conductors for series connections, minimizing stress and material costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559727000002
    Figure 0007559727000002
  • Figure 0007559727000003
    Figure 0007559727000003
  • Figure 0007559727000004
    Figure 0007559727000004
Patent Text Reader

Abstract

To provide a coil component capable of obtaining good coil characteristics by reducing the amount of a conductive material used to connect a coil conductor.SOLUTION: A coil component 1 includes a laminate having a plurality of insulating layers I and coil conductor layers M laminated in a lamination direction and having a first via conductor FV and a second via conductor SV electrically connecting the coil conductor layers M to each other, the first via conductor FV is smaller than the second via conductor SV.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a coil component. [Background technology]

[0002] Due to the recent trend toward higher currents in electronic devices, coil components are being required to have a higher rated current. For example, Patent Documents 1 to 3 disclose coil components in which multiple sheets (e.g., two sheets) on which coil conductors are formed are stacked and connected in parallel via through holes, and the parallel connections are then connected in series. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2008-053368 A [Patent Document 2] Japanese Patent Application Publication No. 8-130115 [Patent Document 3] Japanese Utility Model Application Publication No. 5-57817 Summary of the Invention [Problem to be solved by the invention]

[0004] As more sheets with coil conductors are stacked together to obtain the desired coil characteristics, the stress between the insulating layer and the coil conductor increases, which can lead to cracks. Also, more conductive material is required to be supplied to the through holes that electrically connect the coil conductors. As a result of using more conductive material, the material cost increases.

[0005] Therefore, a main object of the present disclosure is to provide a coil component that reduces the amount of conductive material used to connect coil conductors and provides good coil characteristics. [Means for solving the problem]

[0006] The coil component of the present disclosure comprises: A coil component comprising a laminate in which insulating layers and coil conductor layers are laminated in a lamination direction, the laminate having first via conductors and second via conductors that electrically connect the coil conductor layers to each other, The first via conductor is smaller than the second via conductor. Effect of the Invention

[0007] According to the coil component of the present disclosure, the amount of conductive material used in the first via conductors and the second via conductors that electrically connect the coil conductor layers to each other can be reduced, thereby obtaining good coil characteristics. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a perspective view of a coil component according to the present disclosure. [Diagram 2] FIG. 2 is an exploded perspective view of a laminate of the coil component according to the first embodiment. [Diagram 3] FIG. 3 is a plan view of each lamination member constituting a laminate in the coil device according to the first embodiment. [Figure 4] 4 is a cross-sectional view taken along line IV-IV in FIG. 2. FIG. [Diagram 5] FIG. 5 is an enlarged cross-sectional view of the dashed line portion of FIG. [Figure 6] Figure 6(a) is a schematic cross-sectional view showing the insulating layer preparation process, Figure 6(b) is a schematic cross-sectional view showing the process of preparing a resin paste for forming a gap, Figure 6(c) is a schematic cross-sectional view showing the coil conductor layer preparation process, Figure 6(d) is a schematic cross-sectional view showing the process of arranging an insulating material around the coil conductor layer, and Figure 6(e) is a schematic cross-sectional view showing the laminate preparation process. [Figure 7] FIG. 7(a) is a plan view of laminated members constituting the laminate, and FIG. 7(b) is a cross-sectional view taken along line bb in FIG. 7(a). [Figure 8] FIG. 8(a) is a plan view of laminated members constituting the laminate, and FIG. 8(b) is a cross-sectional view taken along line bb in FIG. 8(a). [Figure 9]FIG. 9 is a plan view of each lamination member constituting a laminate in a coil device according to the second embodiment. [Figure 10] FIG. 10 is a cross-sectional view of a coil component according to the second embodiment. [Figure 11] FIG. 11 is a plan view of each lamination member constituting a laminate in a coil device according to the third embodiment. [Figure 12] FIG. 12 is a cross-sectional view of a coil component according to the third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] The coil components of the present disclosure will be described in detail below. Although the description will be given with reference to the drawings as necessary, the contents shown in the drawings are merely shown in a schematic and illustrative manner for understanding the present disclosure, and the appearance and dimensional ratios may differ from the actual product. Note that the configuration of the coil components described here is merely an example for understanding the invention, and does not limit the invention.

[0010] As shown in Fig. 1, the coil component 1 includes a laminate S and an external electrode E. The laminate S has a substantially rectangular parallelepiped shape and may have a built-in coil. The external electrodes E are electrically connected to the coil, extend in the lamination direction, and may be provided on side surfaces of the laminate S that face each other. Hereinafter, first to third embodiments of the coil component of the present disclosure will be described.

[0011] [Coil component according to the first embodiment] The coil component 1 of the present disclosure includes a laminate S in which insulating layers I and coil conductor layers M are laminated in a stacking direction, and which has first via conductors FV and second via conductors SV that electrically connect the coil conductor layers M to each other.

[0012] First, a description will be given of the plurality of laminated members sb1 to sb16 constituting the laminated body S. Note that, as an example, the number of laminated members will be described as 16, but the number is not limited to this.

[0013] The outermost lamination members sb1 and sb16 cover the coil conductor layer M described later and may include an insulating layer I. The insulating layer I may be preferably made of a magnetic material, more preferably sintered ferrite. The insulating layer I may contain at least Fe, Zn, Cu, and Ni as main components. For example, Fe is Fe 2 O 3 The insulating layer I may contain 40.0 mol % or more and 49.5 mol % or less in terms of Zn, 2 mol % or more and 35 mol % or less in terms of ZnO, 6 mol % or more and 13 mol % or less in terms of CuO, and 10 mol % or more and 45 mol % or less in terms of NiO. The insulating layer I may further contain additives such as Co, Bi, Sn, or Mn, or impurities that are unavoidable in the manufacturing process.

[0014] The lamination members sb2 to sb15 arranged on the inner side of the outermost lamination members sb1, sb16 may include the insulating layer I, the coil conductor layer M, and the via conductors V described above.

[0015] The conductive material constituting the coil conductor layer M is not particularly limited, and examples thereof include Au, Ag, Cu, Pd, and Ni. Ag or Cu is preferable, and Ag is more preferable. The conductive material may be one type or two or more types. The coil conductor layer M is configured in a shape such as a U-shape in which the ends are not connected to each other (i.e., the coil conductor layer is not closed), and the coil conductor layer M may be formed on the insulating layer I.

[0016] The thickness of the coil conductor layer M is determined by the rated current to be passed through the coil component. When a large current is passed through the coil conductor layer M, the thickness of the coil conductor layer M is preferably 20 μm or more and 100 μm or less. By increasing the thickness of the coil conductor layer M, the resistance value of the coil component becomes smaller. Here, if the thickness of the coil conductor layer M is increased, the amount of protrusion of the coil conductor layer M from the surface of the insulating layer I increases, and distortion may occur when manufacturing the laminate S by stacking the laminate members sb1 to sb16. In order to reduce this distortion, an insulating material Im may be disposed around the coil conductor layer M to reduce the amount of protrusion of the coil conductor layer M (see FIG. 7(b) and FIG. 8(b)). Note that if the thickness of the coil conductor layer M is relatively thin and distortion is small when manufacturing the laminate S, it is not necessary to form the insulating material Im around the coil conductor layer M.

[0017] From the viewpoint of manufacturing, it is preferable that the via conductor V is made of the same material as the coil conductor layer M, but a material different from that of the coil conductor layer M may be used. The via conductor V may include a first via conductor FV and a second via conductor SV that electrically connect the coil conductor layers M to each other. The first via conductor FV may be smaller than the second via conductor SV. In other words, the amount of conductive material used in the second via conductor SV may be less than the amount of conductive material used in the first via conductor FV. In other words, the phrase "the first via conductor FV is smaller than the second via conductor SV" in this specification refers to a relationship of size based on the volume of the via conductor. Therefore, since the first via conductor FV is smaller than the second via conductor SV, the coil component 1 of the present disclosure can reduce the amount of conductive material used in the via conductor compared to the coil component 1 in which the coil conductor layers M are electrically connected to each other only by the second via conductor SV.

[0018] In addition, any of the laminate members sb1 to sb16 may have a void A between the coil conductor layer M and the insulating layer I. The void A functions as a so-called stress relaxation space. That is, when the temperature of the laminate S is lowered to room temperature after firing, stress is applied between the coil conductor layer M and the insulating layer I due to the difference in linear expansion coefficient between the coil conductor layer M and the insulating layer I. This stress can be relaxed by the void A. The thickness of the void A is preferably 1 μm or more. By making the thickness of the void A 1 μm or more, internal stress can be further relaxed and the occurrence of cracks can be effectively suppressed.

[0019] Next, the laminate S formed by laminating the above-described laminate members sb1 to sb16 will be described.

[0020] In the laminate S of the coil component 1 of the present disclosure, the coil conductor layers M adjacent to each other in the stacking direction may be electrically connected in parallel using the first via conductor FV (see FIG. 2 and FIG. 3). Here, the term "parallel connection" in this specification refers to a configuration in which both ends of the coil conductor layer M are electrically connected to the coil conductor layer adjacent to each other in the stacking direction. As an example, as shown in FIG. 2 and FIG. 3, the second laminate member sb2 from the top and the third laminate member sb3 from the top in the stacking direction are electrically connected to each other at one end of the coil conductor layer M through the external electrode E, and the other end is electrically connected to each other through the first via conductor FV. As another example, the fourth laminate member sb4 and the fifth laminate member sb5 from the top in the stacking direction are electrically connected to each other at both ends of the coil conductor layer M through the first via conductor FV. Note that, although the illustrated example shows a mode in which two adjacent laminate members are connected in parallel, three or more laminate members may be connected in parallel.

[0021] In the laminate S of the coil component 1 of the present disclosure, the coil conductor layers M adjacent to each other in the stacking direction may be electrically connected in series using the second via conductor SV (see Figs. 2 and 3). Here, the term "series connection" as used herein refers to a configuration in which one of both ends of the coil conductor layer M is electrically connected to the coil conductor layer adjacent to the stacking direction. As an example, as shown in Figs. 2 and 3, the third laminate member sb3 from the top and the fourth laminate member sb4 from the top in the stacking direction are electrically connected to each other at one end of the coil conductor layer M through the second via conductor SV, but the other ends of the coil conductor layers M are not electrically connected to each other. The same can be said for the fifth laminate member sb5 from the top and the sixth laminate member sb6 from the top in the stacking direction, etc.

[0022] When the coil component 1 of the present disclosure is used for large current applications, the coil conductor layers M are connected in parallel, allowing the same current to flow as when the coil conductor layer M is made thicker. The parallel-connected coils are electrically connected in series to obtain desired coil characteristics. Here, the current flowing through the first via conductor FV used for the parallel connection is smaller than the current flowing through the second via conductor SV used for the series connection. Therefore, even if the first via conductor FV is made smaller than the second via conductor SV, the effect on the electrical characteristics of the coil component is low. Therefore, even if the amount of conductive material used in the via conductors is reduced, the coil component can have good electrical characteristics.

[0023] In a preferred embodiment of the coil component 1, the coil conductor layers M connected by the first via conductor FV may have the same shape, and the coil conductor layers M connected by the second via conductor SV may have different shapes. As an example, as shown in Fig. 2 and Fig. 3, the coil conductor layers M of the second laminate member sb2 and the coil conductor layers M of the third laminate member sb3 connected by the first via conductor FV have the same shape, and the coil conductor layers M of the third laminate member sb3 and the coil conductor layers M of the fourth laminate member sb4 connected by the second via conductor SV have different shapes. Here, "same shape" in this specification means that the coil conductor layers M are substantially overlapped with each other when viewed from the stacking direction, and "different shapes" means that the coil conductor layers M are substantially not overlapped with each other when viewed from the stacking direction. In the coil component disclosed herein, coil conductor layers M of the same shape are electrically connected to each other by a first via conductor FV, and coil conductor layers M of different shapes are electrically connected to each other by a second via conductor SV, thereby reducing the amount of conductive material used in the via conductors and resulting in a coil component with good electrical characteristics.

[0024] In a preferred embodiment of the coil component 1, adjacent coil conductor layers M located on the outermost sides of the laminate S may each be provided with a lead-out portion Md electrically connected to an external electrode E (see FIG. 2). According to the configuration of the lead-out portion Md of the present disclosure, the external electrode E is electrically connected by the lead-out portions Md provided on the adjacent coil conductor layers, so that even if one of the lead-out portions Md has a defect, the electrical connection can be ensured by the other lead-out portion Md.

[0025] Furthermore, with regard to the above-mentioned lead-out portions Md, the coil conductor layers M provided with the lead-out portions Md may be electrically connected to each other by the first via conductors FV. According to this configuration, the coil conductor layers M provided with the lead-out portions Md are connected in parallel by the lead-out portions Md together with the external electrodes E. Therefore, since the coil conductor layers M are connected to each other using the first via conductors FV that use a small amount of conductive material, the amount of conductive material used can be reduced, resulting in a coil component that can obtain good electrical characteristics.

[0026] Next, a preferred embodiment of the first via conductors FV and the second via conductors SV will be described.

[0027] As a preferred via conductor, the first via conductor FV and the second via conductor SV may be arranged on the same straight line. By arranging the via conductors in this manner, the coil conductor layers M can be electrically connected to each other in a simple manner without going through complicated processes.

[0028] As a preferred shape of the via conductors, the first via conductor FV and the second via conductor SV may have a tapered shape that widens in the stacking direction in a cross-sectional view (see Figs. 4 and 5). By making the via conductors have a tapered shape, it is possible to easily supply the conductive material from the wider side.

[0029] In addition, the narrowest width dimension of the first via conductor in a cross-sectional view may be 0.5 to less than 0.75 times the narrowest width dimension of the second via conductor. The basis for this value will be described in the examples below.

[0030] [Manufacturing method of coil component according to first embodiment] Next, a description will be given of a manufacturing method for the coil component of the first embodiment. The manufacturing method for the coil component includes an insulating layer forming step, a via conductor forming step, a coil conductor layer forming step, and a laminate forming step.

[0031] -Insulating layer fabrication process (see Figure 6(a))- First, Fe is used as a raw material. 2 O 3 ZnO, CuO, and NiO are weighed out to obtain the above-mentioned specified composition. The raw materials are placed in a ball mill together with pure water and PSZ (partially stabilized zirconia) balls, and wet mixed and ground for 4 to 8 hours. After evaporating and drying the water, the mixture is calcined at a temperature of 700°C to 800°C for 2 to 5 hours to produce a calcined product (calcined powder).

[0032] The calcined product is placed in a ball mill together with PSZ media, and then mixed with a polyvinyl butyral-based organic binder, an organic solvent such as ethanol or toluene, and a plasticizer. The product is then formed into a sheet with a thickness of 20 μm to 30 μm using a doctor blade method or the like, and punched into a rectangular shape to produce the sheet-shaped insulating layer I.

[0033] - Via conductor manufacturing process - A laser is irradiated to a predetermined portion of the prepared sheet-like insulating layer I to form through-holes. When the through-holes are formed by laser irradiation, the shape of the through-holes may be tapered, with the laser irradiated surface being wider and narrower. The formation of the through-holes is not limited to laser irradiation, and other processing techniques capable of forming through-holes may be used. The through-holes formed include a through-hole for forming the second via conductor SV and a through-hole for forming the first via conductor FV that is smaller than the second via conductor SV.

[0034] Although not an essential step in the manufacturing method of the coil component, after the via conductor fabrication step, a resin paste P for forming a void may be optionally prepared and printed on the insulating layer I (see FIG. 6(b)). As an example, the resin paste P for forming a void may be prepared by dissolving a resin that disappears during firing (e.g., acrylic resin, etc.) in a solvent (isophorone, etc.). Note that in order to prevent the void A from being exposed from the outer surface of the laminate S, the resin paste P for forming a void is not formed at the position of the lead-out portion Md that connects to the external electrode E.

[0035] - Coil conductor layer fabrication process (see Figure 6 (c)) - First, a conductive material is prepared. Examples of the conductive material include Au, Ag, Cu, Pd, and / or Ni, and preferably Ag or Cu, and more preferably Ag. A predetermined amount of conductive material powder is weighed out, and mixed with a predetermined amount of a solvent (e.g., eugenol), a resin (e.g., ethyl cellulose), and a dispersant in a planetary mixer or the like, and then dispersed in a three-roll mill or the like to prepare a conductive paste.

[0036] A conductive paste is printed on the insulating layer I so as to form a predetermined shape of the coil conductor layer M. In the manufacturing method shown in Fig. 6(c), the coil conductor layer M is formed so as to cover the void-forming resin paste P. In other words, it is preferable that the area of ​​the coil conductor layer M is larger than the area of ​​the void-forming resin paste P in a plan view. Note that the method of forming the conductive paste is not limited to printing, and may be coating or the like.

[0037] Here, although it is not an essential step in the manufacturing method of the coil component, since distortion occurs during lamination when the coil conductor layer M is thick, a step of disposing an insulating material Im around the coil conductor layer M to improve the distortion may be optionally performed (see FIG. 6(d)). This insulating material Im can be produced by kneading a raw material obtained by pulverizing a ferrite raw material (calcined product) of a predetermined composition to a predetermined particle size with a ketone solvent, a resin such as polyvinyl acetal, and a plasticizer such as an alkyd-based plasticizer using a planetary mixer or the like, and then dispersing the mixture using a three-roll mill or the like. The produced insulating material Im may be printed to cover the periphery of the coil conductor layer M. Note that this step may be omitted if the thickness of the coil conductor layer M is thin enough that distortion during lamination is small.

[0038] -Laminate manufacturing process (Figure 6(e))- The laminated members sb1 to sb16 produced by the above procedure are laminated in a predetermined order (see, for example, Figs. 2 and 3) and thermocompressed to produce a laminated block. After the laminated block is divided into individual pieces, it is fired in a firing furnace at a temperature of 900°C to 920°C for 2 hours to 4 hours. If the void-forming resin paste P is applied here, the void-forming resin paste P disappears during firing, and voids A are formed. After that, as an optional step, the fired laminate is placed in a rotary barrel machine to R-chamfer the corners.

[0039] A conductive paste for forming the external electrodes E is applied to the laminate S produced as described above, and the laminate is baked under conditions of 800°C to 820°C to form base electrodes, after which a Ni film and a Sn film are successively formed by electrolytic plating. In this way, the desired coil component 1 can be manufactured.

[0040] [Coil component according to the second embodiment] Next, a coil component according to a second embodiment will be described with reference to Fig. 9 and Fig. 10. Note that descriptions that overlap with the above description will be omitted as appropriate.

[0041] In the coil component of the first embodiment, adjacent coil conductor layers M are connected in parallel, but in the coil component of the second embodiment, the coil component may include portions that are not connected in parallel from the viewpoint of the rated current flowing through the coil component. In other words, the coil component 1 of the second embodiment may include portions in the laminate S that are electrically connected in series continuously in the stacking direction.

[0042] 9, for example, adjacent laminate members sb3 and sb4 are connected in series, and adjacent laminate members sb4 and sb5 are also connected in series. Note that, in this embodiment as well, the via conductor electrically connected in series may be the second via conductor SV, and the via conductor electrically connected in parallel may be the first via conductor FV.

[0043] According to this configuration, the coil component can be appropriately designed so that a predetermined rated current flows.

[0044] [Coil component according to the third embodiment] Next, a coil component according to a third embodiment will be described with reference to Fig. 11 and Fig. 12. Note that descriptions that overlap with the above description will be omitted as appropriate.

[0045] In the coil component of the first embodiment, each of the adjacent coil conductor layers M located on the outermost side of the laminate S is provided with an extraction portion Md electrically connected to an external electrode E, whereas in the coil component of the third embodiment, at least two extraction electrode layers D electrically connected to the external electrodes E may be provided adjacent to each other on the outer side of the stacking direction of the coil conductor layers M.

[0046] The lead electrode layer D may be formed in a non-bent shape, not in a bent shape to form a coil. In other words, the lead electrode layer D may be a wiring layer that serves to electrically connect the adjacent coil conductor layer M to the external electrode E.

[0047] As a preferred embodiment of the extraction electrode layer D, two extraction electrode layers D may be provided adjacent to each other. With this configuration, even if one of the extraction electrode layers D has a defect, the other extraction electrode layer D can ensure electrical connection.

[0048] According to the coil component of the third embodiment, since the external electrodes E are electrically connected by the extraction electrode layers D different from the coil conductor layers M, the degree of freedom in the layout (position, size, etc.) of the extraction electrode layers D can be improved.

[0049] In a preferred embodiment of the lead electrode layers D, the lead electrode layers D may be electrically connected to each other by the first via conductors FV. That is, the lead electrode layers D are connected in parallel to each other together with the external electrodes E by the first via conductors FV. Therefore, since the lead electrode layers D are connected using the first via conductors FV, ​​which use a small amount of conductive material, the amount of conductive material used can be reduced, and a coil component with good electrical characteristics can be obtained.

[0050] The lead electrode layer D and the coil conductor layer M may be electrically connected by the second via conductor SV. That is, the lead electrode layer D and the coil conductor layer M may be connected in series. With this configuration, it is possible to obtain desired coil characteristics as a coil component. EXAMPLES

[0051] A demonstration test was conducted on the "coil component" according to the present disclosure. Specifically, a 1.5-turn coil component was fabricated by connecting in series two coil conductor layers, each of which had a coil conductor with a thickness of 12 μm and a width of 110 μm connected in parallel (that is, a coil component in which the laminate members sb1 to sb3 and the laminate members sb14 to sb16 were connected in series for the coil component shown in FIG. 2 and FIG. 3). Here, the sizes of the first via conductor FV and the second via conductor SV were set to the narrowest width dimension as shown in [Table 1]. In addition, the ratio of the first via conductor FV and the second via conductor SV based on the width dimension was set to the same as [Table 1]. Then, the DC resistance of each of the fabricated coil components was measured. The measurement results of the DC resistance are shown in Table 1.

[0052] [Table 1]

[0053] The width dimension of the via conductors was evaluated by FIB processing the cross section where the first via conductor and the second via conductor were exposed using a focused ion beam processing device (SMI3050R, SII NanoTechnology Inc.), and observing the cross section with an SEM to calculate the narrowest width dimension of the first via conductor and the second via conductor.

[0054] The DC resistance was measured using a digital resistance meter 755611 manufactured by Yokogawa Electric Corporation at a measurement current value of 10 mA.

[0055] In addition, the presence or absence of cracks in the via conductors was confirmed by the above-mentioned SEM observation to see whether or not cracks occurred in the first via conductors or the second via conductors when 100 samples of each type were manufactured.

[0056] According to [Table 1] above, the DC resistance of the coil components increased by less than 5% in Samples No. 2 and No. 3, and good coil characteristics were obtained. Also, in Samples No. 1 and No. 2, the first via conductor FV and the second via conductor SV were large, so the stress between the coil conductor layer M and the insulating layer I increased, causing cracks and the like. Therefore, based on the above demonstration experiment, it was found that it is preferable that the narrowest width dimension of the first via conductor is 0.5 times or more and less than 0.75 times the narrowest width dimension of the second via conductor.

[0057] It should be noted that the embodiments disclosed herein are illustrative in all respects and are not intended to be limiting. Therefore, the technical scope of the present disclosure is not interpreted solely by the above-described embodiments, but is defined based on the claims. The technical scope of the present disclosure also includes all modifications within the scope and meaning equivalent to the claims. [Industrial Applicability]

[0058] The laminated coil component according to the present disclosure can be used in a wide variety of applications, such as as an inductor. [Explanation of symbols]

[0059] Coil parts 1 External electrode E Laminated body S Laminated materials sb1~sb16 Insulation Layer I Insulating material Im Coil conductor layer M Drawer part Md Extraction electrode layer D Via conductor V First via conductor FV Second via conductor SV Air gap A Resin paste for forming voids P

Claims

1. A coil component comprising a laminate in which a plurality of insulating layers and coil conductor layers are laminated in a lamination direction, the laminate having first via conductors and second via conductors that electrically connect the coil conductor layers to each other, the first via conductor is smaller than the second via conductor; In a cross-sectional view, a width dimension of the first via conductor at its narrowest is 0.5 times or more and less than 0.75 times a width dimension of the second via conductor at its narrowest, the first via conductor is a via conductor that electrically connects coil conductor layers adjacent to each other in the stacking direction in parallel, The second via conductor is a via conductor that electrically connects coil conductor layers adjacent to each other in the stacking direction in series. Coil parts.

2. the coil conductor layers connected to each other by the first via conductor have the same shape; The coil component according to claim 1 , wherein the coil conductor layers connected by the second via conductor have different shapes.

3. The coil component according to claim 1 , wherein the first via conductor and the second via conductor are arranged on the same straight line.

4. The coil component according to claim 1 , wherein the first via conductor and the second via conductor have a tapered shape that widens in the stacking direction in a cross-sectional view.

5. The coil component according to any one of claims 1 to 4, wherein adjacent coil conductor layers located on the outermost sides of the laminate are each provided with a lead portion electrically connected to an external electrode.

6. The coil component according to claim 5 , wherein the coil conductor layers provided with the lead-out portions are electrically connected to each other by the first via conductors.

7. The coil component according to any one of claims 1 to 4, wherein at least two extraction electrode layers electrically connected to external electrodes are provided adjacent to each other on the outside of the coil conductor layer.

8. The coil component according to claim 7 , wherein the lead electrode layers are electrically connected to each other by the first via conductors.

9. The coil component according to claim 7 , wherein the extraction electrode layer and the coil conductor layer are electrically connected to each other by the second via conductor.

10. The coil component according to any one of claims 1 to 9, further comprising a gap between the coil conductor layer and the insulating layer.

Citation Information

Patent Citations

  • Multilayer chip inductor

    JP1993057817U

  • Electronic chip component

    JP1996130115A

  • Laminated inductor

    JP1999097244A

  • Laminated electronic component

    JP2001044038A

  • Laminated ceramic electronic component

    JP2005167098A