Semiconductor Device

The use of a dual gate structure with specific metal oxide compositions in oxide semiconductor transistors addresses mobility and reliability issues, resulting in high-resolution displays with reduced power consumption.

JP7560512B2Active Publication Date: 2024-10-02SEMICON ENERGY LAB CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2022118918
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2017-05-19
Filing Date
2022-07-26
Publication Date
2024-10-02
Estimated Expiration
2037-09-07

AI Technical Summary

Technical Problem

Oxide semiconductor transistors face issues with high field-effect mobility and normally-on characteristics due to oxygen vacancies, which affect electrical characteristics and reliability, especially in high-resolution display devices requiring fast operation and low power consumption.

Method used

A transistor design incorporating a metal oxide film with a dual gate structure and specific metal oxide compositions, including In, M, and Zn, is used to suppress fluctuations in electrical characteristics and improve reliability, while maintaining high field-effect mobility.

Benefits of technology

The design enhances the reliability and electrical stability of transistors, enabling high-resolution displays with reduced power consumption and improved display quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560512000007
    Figure 0007560512000007
  • Figure 0007560512000008
    Figure 0007560512000008
  • Figure 0007560512000009
    Figure 0007560512000009
Patent Text Reader

Abstract

A novel display device is provided. The device has a pixel section and a drive circuit for driving the pixel section, and the drive circuit is a dual gate driver. The pixel portion has a first transistor having a gate structure, and the pixel portion has a second transistor having a single gate structure. The display device has a pixel electrode electrically connected to the first transistor and the second transistor. The first transistor and the second transistor each have a first metal oxide layer having a channel function. The metal oxide film has a first region and a second region, and the first region The first region has In or Zn and oxygen, and the second region has In or element M and oxygen. The first region and the second region are dispersed or distributed in a mosaic pattern.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention relates to a display device and an electronic device.

[0002] Note that one embodiment of the present invention is not limited to the above technical fields. The technical field of one aspect of the present invention relates to an article, a method, or a manufacturing method. is a process, machine, manufacture, or composition of matter. In particular, one embodiment of the present invention relates to a semiconductor device, a display device, a light-emitting device, a power storage device, The present invention relates to a storage device, a driving method thereof, or a manufacturing method thereof.

[0003] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. Refers to devices in general. Semiconductor elements such as transistors, semiconductor circuits, computing devices, memory The device is one aspect of a semiconductor device. Optical devices, power generation devices (including thin-film solar cells, organic thin-film solar cells, etc.), and electronic devices The device may include a semiconductor device. [Background technology]

[0004] Oxide semiconductors have been attracting attention as semiconductor materials that can be used for transistors. A plurality of oxide semiconductor layers are stacked, and an oxide semiconductor layer that serves as a channel is formed among the plurality of oxide semiconductor layers. The compound semiconductor layer contains indium and gallium, and the ratio of indium to the ratio of gallium is By making it larger than A semiconductor device with improved thermal conductivity has been disclosed (see Patent Document 1).

[0005] In addition, oxide semiconductor transistors are being used in liquid crystal displays and organic electroluminescence (EL) displays. The technology is attracting attention for its use in display devices such as oxide semiconductor displays. The off-state current of a transistor is very small. This is used to Reduce refresh frequency and power consumption of LCD and OLED displays The technology is disclosed in Patent Documents 2 and 3. The driving method for reducing the power consumption of the display device described above is called IDS (idling stop) driving. It is called movement. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2014-7399 A [Patent Document 2] JP 2011-141522 A [Patent Document 3] JP 2011-141524 A Summary of the Invention [Problem to be solved by the invention]

[0007] As a transistor using an oxide semiconductor film for a channel region, the field-effect mobility is high. However, increasing the field effect mobility of a transistor However, there is a problem that the characteristics of the normally-on transistor tend to become normally-on characteristics. This means that a channel exists and current flows through the transistor even when no voltage is applied to the gate electrode. It is a state in which one becomes disoriented.

[0008] In addition, in a transistor using an oxide semiconductor film for a channel region, The oxygen vacancies formed in the semiconductor layer are problematic because they affect the transistor characteristics. For example, When oxygen vacancies are formed in the oxide semiconductor film, hydrogen is bonded to the oxygen vacancies to supply carriers. When a carrier supply source is generated in the oxide semiconductor film, This causes a change in the electrical characteristics of the transistor, typically a shift in the threshold voltage.

[0009] For example, when there are too many oxygen vacancies in the oxide semiconductor film, the threshold voltage of the transistor is increased. Therefore, the oxide semiconductor film is shifted to the negative side, resulting in a normally-on characteristic. In particular, in the channel region, there is little oxygen vacancy or the device has normally-on characteristics. It is preferable that the amount of oxygen deficiency is not so large as to cause the formation of a void.

[0010] In addition, when forming a plurality of different circuits on an insulating surface to manufacture a display device, For example, when the pixel portion and the driver circuit are formed on the same substrate, the transistor used in the pixel portion is In order to meet the demands of driver circuits, excellent switching characteristics, such as a large on-off ratio, are required. The transistors used in televisions are required to operate at high speeds. It is also called "4K resolution," "4K2K," or "4K.") Super Hi-Vision (also called "8K resolution", "8K4K", "8K", etc.) The more the display device is used, the shorter the time it takes to write the display image. It is preferable that the transistor has a high operating speed.

[0011] In view of the above problems, one embodiment of the present invention is a transistor including a metal oxide film. One of the objectives is to improve the field effect mobility and the reliability. One embodiment of the present invention is a transistor including a metal oxide film, which is capable of suppressing a change in electrical characteristics. Another object of the present invention is to provide a semiconductor device having a high reliability and high reliability. One of the objects of the present invention is to provide a high-resolution display device having excellent display quality. An object of one embodiment of the present invention is to provide a display device with reduced power consumption. An object of one embodiment of the present invention is to provide a novel display device. An object of one embodiment of the present invention is to provide a novel electronic device.

[0012] The above description of the problem does not preclude the existence of other problems. The embodiment does not necessarily have to solve all of these problems. Problems other than those mentioned above may be solved by the specification. The above problems are obvious from the description of the specification, etc., and problems other than those mentioned above cannot be extracted from the description of the specification, etc. It is possible to issue it. [Means for solving the problem]

[0013] One embodiment of the present invention includes a pixel portion and a driver circuit for driving the pixel portion. a pixel portion electrically connected to the second transistor and The first transistor has a pixel electrode connected to a first gate electrode and a second gate electrode. a first gate electrode and a second gate electrode, and the first gate electrode and the second gate electrode are provided between the first gate electrode and the second gate electrode, and the second gate electrode ... function as a channel. and a first metal oxide film having an electrode, The second transistor is electrically connected to the second metal oxide film having a channel function. The pixel electrode is formed of a third metal oxide film, and the third metal oxide film is formed of a second metal oxide film. A first metal oxide film, a second metal oxide film, and a second metal oxide film having a region in which hydrogen concentration is higher than that of the first metal oxide film. The first and third metal oxide films each have a first region and a second region, and the first region is I the first region has In or an element M and oxygen; The first region and the second region are display devices that are dispersed or distributed in a mosaic pattern.

[0014] Note that an insulating film is provided over the first metal oxide film and the second transistor. The second metal oxide film has an opening on the second transistor and is disposed on the gate insulating film. one of the first gate electrode and the second gate electrode and the third metal oxide film The third metal oxide film is provided on the insulating film, and the third metal oxide film is formed on the second transistor in the opening of the insulating film. The resistor may be electrically connected to the

[0015] Alternatively, a first insulating film and a second insulating film are formed on the first metal oxide film and the second transistor. The first insulating film and the second insulating film are respectively formed on the second transistor. The second metal oxide film is provided on the gate insulating film, and the first metal oxide film is provided on the gate insulating film. One of the gate electrode and the second gate electrode is provided on the first insulating film, and the third metal oxide The third metal oxide film is provided on the first insulating film and the second insulating film. The insulating film may be electrically connected to the second transistor through the opening thereof.

[0016] Alternatively, the first insulating film may include an inorganic insulating film, and the second insulating film may include an organic resin film. good.

[0017] Alternatively, the second transistor has a third gate electrode and a gate insulating film, The first metal oxide film and the third metal oxide film may be provided on a gate insulating film.

[0018] One embodiment of the present invention includes a pixel portion and a driver circuit for driving the pixel portion. a pixel portion electrically connected to the second transistor and a pixel electrode connected to the second transistor, and a first insulating film and a second insulating film are formed on the second transistor. The first insulating film and the second insulating film are laminated in this order, The first transistor has a first gate electrode and a second gate electrode. a first gate electrode and a second gate electrode, and the second gate electrode is provided between the first gate electrode and the second gate electrode, and the second gate electrode has a function of a channel. and a first metal oxide film that is electrically connected to the first gate electrode and the second gate electrode. The second transistor has a second metal oxide film having a channel function. One of the first gate electrode and the second gate electrode is provided on the first insulating film, and the pixel electrode is The electrode is provided on the second insulating film, and the pixel electrode is provided on the first insulating film and the second insulating film. In the opening, the first metal oxide film and the second transistor are electrically connected to each other. The metal oxide film of the second metal oxide film has a first region and a second region, and the first region is made of In or Zn. and oxygen, the second region having In or an element M and oxygen, the first region and The second area is a display device that is dispersed or distributed in a mosaic pattern.

[0019] The first insulating film may include an inorganic insulating film, and the second insulating film may include an organic resin film. stomach.

[0020] The hydrogen concentration of the third metal oxide film is 1×10 20 atoms / cm 3 That's all. This is also fine.

[0021] The first metal oxide film, the second metal oxide film, and the third metal oxide film are each The In content is 40% or more and 50% or less of the total number of In, M, and Zn atoms. and a region in which the M content is 5% or more and 30% or less.

[0022] The first metal oxide film, the second metal oxide film, and the third metal oxide film are each When the ratio of the numbers of In, M, and Zn atoms is In:M:Zn=4:x:y, x is 1.5 or less. The upper limit is 2.5 or less, and y may be 2 or more and 4 or less.

[0023] The first metal oxide film, the second metal oxide film, and the third metal oxide film are each When the ratio of the numbers of In, M, and Zn atoms is In:M:Zn=5:x:y, x is 0.5 or less. The upper limit may be 1.5 or less, and y may be 5 or more and 7 or less.

[0024] The element M is gallium, aluminum, silicon, boron, yttrium, tin, Copper, vanadium, beryllium, titanium, iron, nickel, germanium, zirconium, molybdenum Lithium, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, and The metal may be any one or more selected from magnesium.

[0025] The first transistor has a dual gate structure, and the second transistor has a A single gate structure may also be used.

[0026] Another embodiment of the present invention is a display device including a display device having any of the above structures and a touch sensor. Another embodiment of the present invention is a display module having any of the above structures. Or an electronic device having the above display module, a receiving device, an operation key, or a battery. It is a vessel. Effect of the Invention

[0027] According to one embodiment of the present invention, in a transistor having a metal oxide film, the field effect mobility Also, according to one embodiment of the present invention, In a transistor having a metal oxide film, the change in electrical characteristics is suppressed and reliability is improved. According to one embodiment of the present invention, a high resolution display having excellent display quality can be obtained. According to one embodiment of the present invention, a display device having reduced power consumption can be provided. According to one embodiment of the present invention, a novel display device can be provided. According to one embodiment of the present invention, a novel electronic device can be provided. This can be done.

[0028] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have to have all of these effects. The above will become apparent from the description in the specification, drawings, claims, etc. It is possible to extract other effects from the descriptions in the claims, etc. [Brief description of the drawings]

[0029] [Figure 1] FIG. 1 is a cross-sectional view illustrating a display device. [Diagram 2] FIG. [Diagram 3] Conceptual diagram of the structure of metal oxides. [Figure 4] FIG. 1 is a cross-sectional view illustrating a display device. [Diagram 5] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 6] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 7] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 8] FIG. 1 is a cross-sectional view illustrating a display device. [Figure 9] FIG. [Figure 10] FIG. 1 is a cross-sectional view illustrating a display device. [Figure 11] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 12] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 13] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Figure 14] 1A and 1B are a top view and a cross-sectional view illustrating a transistor. [Figure 15] 1A and 1B are a top view and a cross-sectional view illustrating a transistor. [Figure 16] 1 is a conceptual diagram showing the diffusion path of oxygen or excess oxygen diffusing into a metal oxide film. [Figure 17] 1A and 1B are a top view and a cross-sectional view illustrating a transistor. [Figure 18] FIG. 4 is a diagram for explaining the measurement results of the XRD spectrum of a sample. [Figure 19] 1A to 1C are diagrams illustrating a TEM image and an electron beam diffraction pattern of a sample. [Figure 20] FIG. 1 is a diagram illustrating EDX mapping of a sample. [Figure 21] 1A to 1C are diagrams illustrating a manufacturing process of a display device using a lateral electric field mode liquid crystal element. [Figure 22] FIG. 1 is a top view illustrating one embodiment of a display device. [Figure 23] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Figure 24] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Diagram 25] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Figure 26] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Figure 27] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Figure 28] FIG. 1 is a cross-sectional view showing one embodiment of a display device. [Figure 29] 1A and 1B are a block diagram and a circuit diagram illustrating a display device. [Diagram 30] FIG. 1 is a block diagram showing an example of the configuration of a controller IC. [Diagram 31] FIG. [Diagram 32] FIG. 2 is a diagram showing an example of the configuration of a frame memory. [Diagram 33] FIG. 2 is a block diagram showing an example of the configuration of a register. [Diagram 34] FIG. 4 is a circuit diagram showing an example of the configuration of a register. [Diagram 35] FIG. 2 is a diagram illustrating a display module. [Diagram 36] 1A to 1C are diagrams illustrating electronic devices. [Figure 37] 1A to 1C are diagrams illustrating electronic devices. [Figure 38] FIG. 1 is a block diagram showing an example of the configuration of a broadcasting system. [Figure 39] FIG. 1 is a block diagram showing an example of the configuration of a broadcasting system. [Diagram 40] FIG. 1 is a schematic diagram showing data transmission in a broadcasting system. [Diagram 41] FIG. 2 is a diagram showing an example of the configuration of a receiving device. [Diagram 42] FIG. [Diagram 43] FIG. 4 is a diagram showing a drivable range of a display according to an embodiment. [Diagram 44] FIG. 13 is a graph showing Id-Vg characteristics of a transistor in the embodiment. [Diagram 45] 5A to 5C are diagrams for explaining changes in transistor characteristics in the embodiment. [Figure 46] FIG. [Figure 47] 13A to 13C are diagrams illustrating the results of a GBT test on a transistor according to an embodiment. [Figure 48] 5A to 5C are diagrams for explaining changes in transistor characteristics in the embodiment. [Figure 49] FIG. [Figure 50] FIG. [Figure 51] FIG. [Figure 52] 4 is a timing chart according to an embodiment. [Figure 53] FIG. 13 is a diagram illustrating the relationship between mobility and writing time in the embodiment. [Figure 54] FIG. 13 is a graph showing Id-Vg characteristics of a transistor in the embodiment. [Figure 55] 13A to 13C are diagrams illustrating the results of a GBT test on a transistor according to an embodiment. [Figure 56] 5A to 5C are diagrams for explaining changes in transistor characteristics in the embodiment. [Figure 57] 5A to 5C are diagrams for explaining changes in transistor characteristics in the embodiment. [Figure 58] 4 shows ESR analysis results according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] Hereinafter, the embodiments will be described with reference to the drawings. The present invention may be embodied in various different forms without departing from its spirit and scope. It will be readily understood by those skilled in the art that various modifications and changes may be made to the embodiments and details of the present invention. However, the present invention should not be construed as being limited to the description of the following embodiments.

[0031] Also, in the drawings, the size, layer thickness, or area are exaggerated for clarity. Therefore, the drawings are not necessarily limited to the scale. and are not limited to the shapes or values ​​shown in the drawings.

[0032] In addition, the ordinal numbers "first," "second," and "third" used in this specification refer to the components of the It should be noted that this is added to avoid confusion and is not intended to limit the numbers.

[0033] In addition, in this specification, the words "above" and "below" indicating the position of the components are used. The positional relationship is used for convenience in describing the drawings. The relationship changes depending on the direction in which each component is depicted. The above words and phrases are not limited to those used above, but can be rephrased appropriately depending on the situation.

[0034] In this specification, a transistor includes a gate, a drain, and a source. The drain terminal is a diode that has at least three terminals. Between the drain region or drain electrode and the source (source terminal, source region or source electrode) A current flows between the source and drain through the channel region. In this specification and the like, the channel region refers to a region through which a current mainly flows. This refers to the area in which the flow occurs as

[0035] In addition, the functions of the source and drain may differ depending on whether transistors of different polarities are used or the circuit In operation, when the direction of the current changes, the positions may be reversed. In the specification, the terms source and drain may be used interchangeably. do.

[0036] In addition, in this specification, "electrically connected" means "something that has some kind of electrical effect." This includes cases where the device is connected via a "device having some electrical function." "of" is not subject to any particular restrictions as long as it enables the transmission and reception of electrical signals between connected objects. For example, "something that has an electrical effect" includes electrodes, wiring, and transistors. These devices have various functions such as switching elements, resistor elements, inductors, capacitors, etc. This includes elements such as:

[0037] In addition, in this specification, "parallel" means that two straight lines are at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Perpendicular" means that two straight lines are arranged at an angle of 80° or more and 100° or less. Therefore, this also includes cases where the angle is between 85° and 95°.

[0038] In addition, in this specification and the like, the terms "film" and "layer" are interchangeable. For example, the term "conductive layer" can be changed to the term "conductive film." Alternatively, for example, the term "insulating film" may be changed to "insulating layer." It may be possible to change the term to:

[0039] In this specification and the like, unless otherwise specified, the off-state current refers to the current that occurs when a transistor is off. This refers to the drain current when the device is in a non-conducting state (also called a cut-off state). Unless otherwise specified, for n-channel transistors, V is the voltage between the gate and source When gs is lower than the threshold voltage Vth, the gate and This refers to a state in which the voltage Vgs between the n-channel transistors is higher than the threshold voltage Vth. The off-state current of a transistor is the voltage between the gate and source, Vgs, that is, the threshold voltage, Vt This may refer to the drain current when it is lower than h.

[0040] The off-state current of a transistor may depend on Vgs. The off-state current is I or less if there exists a Vgs value at which the off-state current of the transistor is I or less. The off-state current of a transistor is the current that flows through it in the off-state at a given Vgs. , an off-state at Vgs within a given range or a sufficiently reduced off-current is obtained. In some cases, it may refer to the off-state current at Vgs.

[0041] As an example, when the threshold voltage Vth is 0.5V and Vgs is 0.5V, The current is 1×10 -9 A, and the drain current at Vgs of 0.1 V is 1×10 -1 3 A, and the drain current at Vgs -0.5 V is 1×10 -19 A and Vg The drain current at s = -0.8 V is 1 × 10 -22 A n-channel transistor The drain current of the transistor is as follows when Vgs is -0.5V: , or 1×10 when Vgs is in the range of -0.5V to -0.8V -19 A or below Therefore, the off-state current of the transistor is 1×10 -19 There are cases where it is said to be A or lower. The drain current of the transistor is 1×10 -22 A or less Vgs exists. Therefore, the off-state current of the transistor is 1×10 -22 It may be said that it is below A.

[0042] In this specification, the off-state current of a transistor having a channel width W is expressed as It is sometimes expressed as the current value that flows per watt. Also, for a given channel width (for example, 1 μm), In the latter case, the unit of the off-state current is current / length. It may be expressed in units with an element (e.g., A / μm).

[0043] The off-state current of a transistor may depend on temperature. Unless otherwise specified, the operating temperature is room temperature, 60°C, 85°C, 95°C, or 125°C. Or, the reliability of a semiconductor device including the transistor may be guaranteed. The temperature at which the transistor is certified, or the temperature at which a semiconductor device or the like that contains the transistor is used (e.g. For example, the off-state current at any one of temperatures from 5° C. to 35° C. The off-state current of the transistor is I or less at room temperature, 60°C, 85°C, 95°C, 125°C, The temperature at which the reliability of a semiconductor device including the transistor is guaranteed, or The temperature at which the semiconductor device containing the transistor is used (for example, any one of 5°C to 35°C) (temperature), there exists a value of Vgs at which the off-state current of the transistor is equal to or less than I. There are cases where it is pointed out.

[0044] The off-state current of a transistor may depend on the voltage Vds between the drain and source In this specification, unless otherwise specified, the off-state current is measured when Vds is 0.1 V, 0.8 V, 1V, 1.2V, 1.8V, 2.5V, 3V, 3.3V, 10V, 12V, 16V, or In some cases, it indicates the off-state current at 20 V. In other cases, it indicates the off-state current at 20 V. Vds that guarantees the reliability of semiconductor devices, or semiconductor devices including the transistor The term may also refer to the off-state current at Vds used in the transistor off-state. The current is equal to or less than I when Vds is 0.1V, 0.8V, 1V, 1.2V, 1.8V, 2.5V, 3V, 3.3V, 10V, 12V, 16V, 20V, transistors included Vds that guarantees the reliability of the semiconductor device in which the transistor is used, or Vds used in semiconductor devices, etc., where the off-state current of the transistor is I or less This may refer to the existence of a gs value.

[0045] In the above description of the off-state current, the drain may be read as the source. The current may also refer to the current through the source when the transistor is in the off state.

[0046] In this specification and the like, the term "leak current" may be used to mean the same thing as the "off current." In this specification, the off-state current refers to, for example, the current flowing when a transistor is in an off state. , may refer to the current flowing between the source and drain.

[0047] In this specification, the threshold voltage of a transistor is the threshold voltage of a transistor. This refers to the gate voltage (Vg) when a gate is formed. Specifically, it refers to the threshold voltage of a transistor. Voltage is plotted on the horizontal axis as gate voltage (Vg) and on the vertical axis as the square root of drain current (Id). The line obtained by extrapolating the tangent line with the maximum slope in the simulated curve (Vg-√Id characteristics) is , the gate voltage (Vg Alternatively, the threshold voltage of a transistor can be expressed as the channel length L and the The channel width is W, and the value of Id[A]×L[μm] / W[μm] is 1×10 -9 [A] Sometimes it refers to the gate voltage (Vg) applied to the device.

[0048] In addition, even when the term "semiconductor" is used in this specification, for example, If the electrical conductivity is low enough, the material may have the properties of an insulator. The boundary between "insulators" and "insulators" is unclear, and it may not be possible to strictly distinguish them. In some cases, the term "semiconductor" in the above can be replaced with "insulator." In some cases, the term "insulator" in the specification can be replaced with "semiconductor." In some cases, the term "insulator" in this specification can be rephrased as "semi-insulator." .

[0049] In addition, even when the term "semiconductor" is used in this specification, for example, If the electrical conductivity is high enough, it may have the properties of a "conductor". The boundary between the term "conductor" and the term "electrical conductor" is unclear, and it may not be possible to strictly distinguish between them. In some cases, the term "semiconductor" in the above can be replaced with "conductor." The term "conductor" in the specification etc. may be replaced with "semiconductor" in some cases.

[0050] In this specification, the term "impurities in a semiconductor" refers to anything other than the main component that constitutes the semiconductor film. For example, an element with a concentration of less than 0.1 atomic percent is an impurity. This causes the formation of DOS (Density of States) in the semiconductor and the In some cases, the rear mobility and crystallinity of the semiconductor may decrease. In the case of an oxide semiconductor, impurities that change the characteristics of the semiconductor include, for example, Group 1 Elements, Group 2 elements, Group 13 elements, Group 14 elements, Group 15 elements, transition metals other than the main component In particular, hydrogen (which is also contained in water), lithium, sodium, silicon, and boron In the case of oxide semiconductors, for example, impurities such as hydrogen can cause Therefore, oxygen vacancies may be formed. In addition, when the semiconductor contains silicon, Impurities that change the characteristics include, for example, oxygen, Group 1 elements excluding hydrogen, Group 2 elements, These include Group 13 elements and Group 15 elements.

[0051] In this specification, the term "metal oxide" refers to a metal in a broad sense. Metal oxides are oxide insulators and oxide conductors (including transparent oxide conductors). ), oxide semiconductor (also called oxide semiconductor or simply OS) For example, when a metal oxide is used in the active layer of a transistor, the metal Oxides are sometimes called oxide semiconductors. In other words, metal oxides have amplifying and rectifying properties. and switching action, the metal oxide is Metal oxide semiconductor, abbreviated as OS. In addition, when describing OS FET, it is possible to use a metal oxide or an oxide semiconductor. In other words, it is a transistor having a conductor.

[0052] In the present specification and the like, metal oxides having nitrogen are also referred to as metal oxides. Metal oxides containing nitrogen are also called metal oxynitrides (MEs). It may also be called tal oxynitride.

[0053] (Embodiment 1) In this embodiment, a display device and a manufacturing method thereof according to one embodiment of the present invention will be described with reference to FIGS. This will be explained with reference to 16.

[0054] <1-1. Display device configuration example 1> FIG. 2 illustrates a transistor included in a driver circuit and a display portion of a display device according to one embodiment of the present invention. FIG. 2A is a top view of a transistor 100A included in a driver circuit. FIG. 2B is a top view of a transistor 200A included in a pixel portion. 1) corresponds to a cross-sectional view taken along the dashed line X1-X2 in FIG. 2(A), and FIG. (A-2) corresponds to a cross-sectional view of the cut surface between the dashed line Y1-Y2 shown in FIG. FIG. 1(B-1) is a cross-sectional view taken along the dashed line X3-X4 in FIG. 2(B). FIG. 1(B-2) corresponds to a cross section taken along the dashed line Y3-Y4 in FIG. 2(B). In FIG. 2, in order to avoid complication, the transistor 1 is Eliminate some of the components of 00A and 200A (such as the insulating film that functions as a gate insulating film) In each transistor, the directions of the dashed lines X1-X2 and X3- The X4 direction is the channel length direction, the dashed dotted line Y1-Y2 direction, and the Y3-Y4 direction are the channel width direction. Note that in the top view of a transistor, As with FIG. 2, some of the components may be omitted in the illustration.

[0055] As shown in FIG. 1(A-1) and FIG. 1(A-2), the driving circuit includes a transistor 100A. Yes.

[0056] The transistor 100A includes a conductive film 104 on a substrate 102 and a semiconductor device including the substrate 102 and the conductive film 10 4, an insulating film 106 on the insulating film 106, and a metal oxide film 108 on the metal oxide film 108. The conductive film 112a is on the metal oxide film 108, and the conductive film 112b is on the metal oxide film 108. Specifically, the metal oxide film 108, the conductive film 112a, and the conductive film 112b are formed on the transistor 100A. On 12b, an insulating film 114, an insulating film 116 on the insulating film 114, and an insulating film 116 on the insulating film 116 are provided. A marginal membrane 118 is formed.

[0057] The insulating films 106, 114, and 116 have an opening 142a. , and is electrically connected to the conductive film 104 through the opening 142a.

[0058] The transistor 100A is a so-called channel etch type transistor. It is a rugate structure.

[0059] As shown in FIG. 1B-1 and FIG. 1B-2, the pixel portion includes a transistor 20 0A, a conductive film 220a having a function as a pixel electrode, a conductive film 220b having a function as a capacitance wiring 13, and a capacitive element 250a.

[0060] The transistor 200A includes a conductive film 204 on the substrate 102 and a conductive film 20 4, a metal oxide film 208 on the insulating film 106, and The conductive film 212a is on the metal oxide film 208, and the conductive film 212b is on the metal oxide film 208. Specifically, the metal oxide film 208, the conductive film 212a, and the conductive film 212b are formed on the transistor 200A. On 12b, an insulating film 114, an insulating film 116 on the insulating film 114, and an insulating film 116 on the insulating film 116 are provided. A marginal membrane 118 is formed.

[0061] The insulating films 114 and 116 have an opening 242a. The conductive film 220a is electrically connected to the conductive film 212b through the opening 242a. In addition, a conductive film 213 having a function as a capacitance wiring is formed on the insulating film 106. The conductive film 213 is formed at the same time as the conductive films 112a, 112b, 212a, and 212b. The conductive film 213, the insulating film 114, and the insulating film 204 may be formed at the same time. The capacitor 250a is formed by the conductive film 220a and the insulating film 116.

[0062] The transistor 200A is a so-called channel etch type transistor. It is a rugate structure.

[0063] In addition, the conductive film 120a included in the transistor 100A and the conductive film 120b having a function as a pixel electrode The conductive film 220a is formed in the same process. The conductive films 120a and 220a are preferably made of an oxide conductive film (OC) as described below. By using the insulating film, oxygen can be added to the insulating films 114 and 116. The oxygen added to the metal oxide films 108 and 208 moves to the metal oxide films 14 and 116. It is possible to compensate for the oxygen vacancies in the transistors 108 and 208. It is possible to improve the reliability of the currents of 0 A and 200 A. The same materials as those listed for the conductive films 104, 112a, 112b, 204, 212a, and 212b are used. The same materials may be used.

[0064] The insulating film 106 serves as a first gate insulating film for the transistors 100A and 200A. The insulating films 114 and 116 function as a second gate insulating film of the transistor 100A. The insulating film 118 functions as a protective insulating film for the transistors 100A and 200A. In the transistor 100A, the conductive film 104 serves as a first gate electrode. The conductive film 112a functions as a source electrode, and the conductive film The drain electrode 112b functions as a drain electrode. The conductive film 120a functions as a second gate electrode. At 0A, the conductive film 204 functions as a gate electrode, and the conductive film 212a functions as a solenoid. The conductive film 212b functions as a source electrode, and the conductive film 212b functions as a drain electrode.

[0065] In the transistor 100A, as shown in FIG. is electrically connected to the conductive film 104 through the opening 142a.

[0066] As shown in FIG. 1(A-2), the metal oxide film 108 is a conductive film 104 and a conductive The gate electrode is sandwiched between two conductive films having the function of a gate electrode. The length of the conductive film 120a in the channel length direction and the width of the conductive film 120a in the channel width direction are The length is the length of the metal oxide film 108 in the channel length direction and the channel width of the metal oxide film 108. The metal oxide film 108 is entirely formed of insulating films 114 and 11 6 and is covered with a conductive film 120a.

[0067] In other words, the conductive film 104 and the conductive film 120a are provided on the insulating films 106, 114, and 116. The metal oxide film 108 is connected to the opening 104 and is located outside the side edge of the metal oxide film 108. It has an area.

[0068] With such a configuration, the metal oxide film 108 included in the transistor 100A The conductive film 104 and the conductive film 120a can electrically surround the conductive film 104 and the conductive film 120a. As in the transistor 100A, the electric field of the first gate electrode and the second gate electrode The device structure of the transistor that electrically surrounds the metal oxide film on which the panel region is formed is called Su. This can be called a rounded channel (S-channel) structure.

[0069] Since the transistor 100A has an S-channel structure, the first gate electrode The conductive film 104 having the function effectively generates an electric field to induce a channel. Therefore, the current driving capability of the transistor 100A can be This improves the on-state current characteristics, making it possible to obtain high on-state current characteristics. This allows the transistor 100A to be miniaturized. In the photodiode 100A, the metal oxide film 108 is a conductive film 104 having a function of a first gate electrode. and has a structure surrounded by a conductive film 120a having a function of a second gate electrode. , the mechanical strength of the transistor 100A can be increased.

[0070] In the transistor 100A, the metal oxide film 108 is formed by disposing the metal oxide film 108 on the insulating film 106. The metal oxide film 108_1 and the metal oxide film 108_2 on the metal oxide film 108_1 are provided. In the transistor 200A, the metal oxide film 208 is formed on the metal oxide film 106. A metal oxide film 208_1 and a metal oxide film 208_2 on the metal oxide film 208_1 are provided. The metal oxide films 108_1, 108_2, 208_1, and 208_2 are For example, the metal oxide films 108_1, 108_2, 208_1, and 20 8_2 are each independently In and M (M is gallium, aluminum, silicon, ho Uranium, yttrium, tin, copper, vanadium, beryllium, titanium, iron, nickel, gel Manium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum It is preferable that the alloy contains at least one of these metals, i.e., niobium, tungsten, or magnesium, and Zn.

[0071] In addition, the metal oxide films 108_1, 108_2, 208_1, and 208_2 are each independently In particular, it is preferable to have a region in which the atomic ratio of In is greater than the atomic ratio of M. As an example, In, M, and Zn in the metal oxide films 108_1, 108_2, 208_1, and 208_2 It is preferable that the atomic ratio is about In:M:Zn=4:2:3. When In is 4, M is 1.5 or more and 2.5 or less, and Zn is 2 or more and 4 or less. or In, M, and It is preferable that the ratio of the number of Zn atoms is about In:M:Zn=5:1:6. The metal oxide films 108_1, 108_2, 208_1, and 208_2 are made to have approximately the same composition. This allows the same sputtering target to be used for both, reducing manufacturing costs. In addition, when using the same sputtering target, Metal oxide films 108_1, 108_2, 208_1, and 208_2 are successively formed in a vacuum. Therefore, the interface between the metal oxide film 108_1 and the metal oxide film 108_2 can be formed. Impurities are taken in the interfaces between the metal oxide film 208_1 and the metal oxide film 208_2. This can prevent the data from being captured.

[0072] In addition, the metal oxide films 108_1, 108_2, 208_1, and 208_2 are each Metal oxide with CAC (Cloud-Aligned Composite) structure The metal oxide will be described with reference to FIG.

[0073] A conceptual diagram of a metal oxide having a CAC structure is shown in FIG. When the metal oxide, which is one embodiment of the present invention, has a semiconductor function, it is called CAC-MO (Metal Oxide Semiconductor) or CAC-OS(Oxide Sem Define the term "electronic conductor."

[0074] CAC-MO or CAC-OS is, for example, a compound that constitutes a metal oxide as shown in FIG. The uneven distribution of the elements forms regions 001 and 002, each of which is the main component of the element. In other words, the metal oxides that make up the metal oxides are mixed together and formed or dispersed in a mosaic pattern. The element has a size of 0.5 nm to 10 nm, preferably 1 nm to 2 nm, or In the following, in the case of metal oxides, One or more metal elements are unevenly distributed, and the region having the metal element is 0.5 nm or more. Mixtures with sizes of 10 nm or less, preferably 1 nm to 2 nm or less, or in the vicinity thereof. This state is also called mosaic or patchy.

[0075] In addition, CAC-MO or CAC-OS refers to the conductive function of some materials and the Some of the material has insulating properties, while the material as a whole has semiconductor properties. When AC-MO or CAC-OS is used for the channel of a transistor, the conductive function is the function of allowing the flow of electrons (or holes) that act as carriers, and the insulating function is the function of allowing the carriers The function of preventing the flow of electrons is to prevent the flow of electrons. By applying this function to the CAC- It can be given to MO or CAC-OS. By separating the functions of each, the functions of both can be maximized.

[0076] In the present specification and the like, CAC-MO or CAC-OS refers to a conductive region and an insulating region. For example, one of the regions 001 and 002 shown in FIG. 3 is a conductive region. The conductive region may have the above-mentioned conductive function and may be an insulating region. The conductive region has the insulating function described above. Conductive regions and insulating regions may be separated at the nanoparticle level. The conductive regions may be unevenly distributed in the material. They may be observed connected in a woody form.

[0077] In addition, CAC-MO and CAC-OS are characterized by their different band gap components. For example, CAC-MO or CAC-OS may be configured as A component having a wide gap and a component having a narrow gap due to a conductive region, In this configuration, when the carrier flows, a component having a narrow gap In addition, the narrow gap component is smaller than the wide gap component. It acts complementarily to the component with a narrow gap and acts in conjunction with the component with a wide gap. Carriers also flow to the components that have the CAC-MO or CAC-OS When used in the channel region of a transistor, a high current flows when the transistor is in the on state. It is possible to obtain a large driving force, that is, a large on-current, and a high field effect mobility.

[0078] CAC-MO and CAC-OS are matrix composites. mposite, or metal matrix composite For more information on CAC-MO or CAC-OS, see This will be described in detail in the second embodiment.

[0079] The metal oxide films 108_1, 108_2, 208_1, and 208_2 are each independently The atomic ratio of In is greater than the atomic ratio of M, and the CAC structure is also provided. The field effect mobility of the transistors 100A and 200A can be increased. Specifically, The field effect mobility of transistors 100A and 200A is 40cm 2 / Vs, more favorable Length: 50cm 2 / Vs, more preferably 100 cm 2 / Vs can be exceeded It becomes Noh.

[0080] In addition, the transistor 100A, which has an S-Channel structure, has a high field-effect mobility. Since the driving capability is high, the transistor 100A is used as a driving circuit, typically a gate signal generator. By using this in a gate driver that configures the display device, a display device with a narrow frame width (also called a narrow frame) can be provided. In addition, the transistor 100A can be connected to a signal line of the display device. The source driver (especially the output terminal of the shift register of the source driver) supplies By using it as a demultiplexer connected to the terminal, the number of wires connected to the display device can be reduced. It is possible to provide a display device that is easy to use.

[0081] Also, transistors 100A and 200A are transistors with channel etch structures. Therefore, the number of manufacturing steps is smaller than that of a transistor using low-temperature polysilicon. In addition, since the transistors 100A and 200A use a metal oxide film as the channel, Unlike transistors using low-temperature polysilicon, the laser crystallization process is not required. Therefore, even in the case of a display device using a large-area substrate, the manufacturing cost can be reduced. In addition, there are ultra-high definition ("4K resolution", "4K2K", "4K"), High resolution such as super high definition ("8K resolution", "8K4K", "8K") In addition, in large display devices, field effect transistors such as transistors 100A and 200A By using highly efficient transistors in the driver circuits and display area, writing can be done in a short time. This is preferable because it is possible to reduce display defects.

[0082] <1-2. Components of the display device> Next, components included in the display device of this embodiment will be described in detail.

[0083] [substrate] There is no particular restriction on the material of the substrate 102, but it should be strong enough to withstand the subsequent heat treatment. For example, glass substrates, ceramic substrates, quartz substrates, and sa A fire substrate or the like may be used as the substrate 102. Also, a material such as silicon or silicon carbide may be used. Single crystal semiconductor substrates, polycrystalline semiconductor substrates, compound semiconductors such as silicon germanium, etc. It is also possible to use a substrate, an SOI substrate, or the like, on which a semiconductor element is provided. The substrate 102 may be a glass substrate. If you have 6th generation (1500mm x 1850mm), 7th generation (1870mm x 220 0mm), 8th generation (2200mm x 2400mm), 9th generation (2400mm x 280 By using large-area substrates such as 10th generation (2950mm x 3400mm), Larger display devices can be manufactured.

[0084] In addition, a flexible substrate is used as the substrate 102, and the transistor 10 is directly formed on the flexible substrate. Alternatively, the substrate 102 and the transistors 100A and 200A may be formed. A release layer may be provided between A and B. The release layer is used to form a semiconductor device that is partially or completely completed on the surface. After that, it can be separated from the substrate 102 and used for transfer to another substrate. Therefore, the transistors 100A and 200A can be mounted on substrates with poor heat resistance or flexible substrates.

[0085] [Conductive film] Conductive films 104, 204, 120a functioning as gate electrodes, and conductive films 112a and 212a having a function of a drain electrode. The metals are chromium (Cr), copper (Cu), aluminum (Al), gold (Au), and silver (Ag). , Zinc (Zn), Molybdenum (Mo), Tantalum (Ta), Titanium (Ti), Tungste Choose from tungsten (W), manganese (Mn), nickel (Ni), iron (Fe), and cobalt (Co). The metallic elements mentioned above, or alloys containing the metallic elements mentioned above, or combinations of the metallic elements mentioned above Each of them can be formed using a combined alloy or the like.

[0086] In addition, the conductive films 104, 112a, 112b, 120a, 204, 212a, and 212b Indium-tin oxide (In-Sn oxide), indium-tungsten oxide and oxides having indium, tungsten and zinc (In-W oxides). oxides containing indium and titanium (In-Ti oxides) ), oxides of indium, titanium and tin (In-Ti-Sn oxides), indium and zinc (In-Zn oxide), and oxide having indium, tin and silicon oxides (In-Sn-Si oxides), oxides containing indium, gallium and zinc (In Metal oxides such as Zn-Ga-Zn oxide can be used. A material conductor or an oxide semiconductor can also be used.

[0087] Here, the oxide conductor will be described. In this specification, the oxide conductor is referred to as OC The oxide conductor may be, for example, When oxygen vacancies are formed in a metal oxide and hydrogen is added to the oxygen vacancies, donors are generated near the conduction band. As a result, the metal oxide becomes conductive and becomes a conductor. The metal oxide that is electrically conductive can be called an oxide conductor. Since the energy gap is large, the oxide conductor is transparent to visible light. A metal oxide has a donor level near the conduction band. The effect of absorption due to the - level is small, and the transparency to visible light is comparable to that of oxide semiconductors. do.

[0088] The oxide conductor is a metal oxide having a function as a channel. One example is an oxide semiconductor. It has a higher hydrogen concentration than the human body, typically 8×10 19 atoms / cm 3 The above, preferably 1×10 20atoms / cm 3 More than 5×10 20 atoms / cm 3 End It is.

[0089] An oxide conductor has defects and contains impurities, and thus has electrical conductivity. The resistivity of a conductive film having a conductor is 1×10 -3 Ωcm or more 1×10 4 Less than Ωcm, even better Preferably, the resistivity is 1×10 -3 Ωcm or more 1×10 -1 It is less than Ωcm.

[0090] The electrical conductivity of a conductive film having an oxide conductor is typically 1×10 -2 S / m or more1 ×10 5 S / m or less, or 1×10 3 S / m or more 1×10 5 It is preferable that the value is less than S / m.

[0091] In addition, the oxide conductor contains impurities and defects. The conductive film is a film in which defects are generated by adding a rare gas. The film is exposed to ultraviolet light and has defects.

[0092] In addition, it is preferable to use a metal oxide having a CAC structure as the oxide conductor.

[0093] In addition, the conductive films 104, 112a, 112b, 120a, 204, 212a, and 212b Cu-X alloy film (X is Mn, Ni, Cr, Fe, Co, Mo, Ta, or Ti) By using a Cu-X alloy film, it is possible to process it by a wet etching process. This allows the manufacturing cost to be reduced. , the conductive films 104, 112a, 112b, 120a, 204, 212a, and 212b are Cu- By forming the wiring using an X alloy film, it is possible to reduce wiring delay. In producing such a display device, it is preferable to use a Cu-X alloy film as wiring.

[0094] In addition, the conductive films 112a, 112b, 212a, and 212b contain, among the above-mentioned metal elements, , in particular any one selected from copper, titanium, tungsten, tantalum, and molybdenum. It is preferable to have one or more conductive films 112a, 112b, 212a, 212b, and 212c. A tantalum nitride film is preferably used as 12b. The tantalum nitride film has a conductive property. and has a high barrier property against copper or hydrogen. Furthermore, since hydrogen is released from the metal oxide film 108, 208 little, the conductive layer It is most suitable to use the conductive film in the vicinity of the metal oxide film 108, 208. In addition, when a copper film is used as the conductive films 112a, 112b, 212a, and 212b, This is preferable because it is possible to reduce the resistance of the conductive films 112a, 112b, 212a, and 212b. It is appropriate.

[0095] In addition, the conductive films 112a, 112b, 212a, and 212b are formed by electroless plating. Materials that can be formed by the electroless plating method include, for example, Cu, One or more selected from Ni, Al, Au, Sn, Co, Ag, and Pd In particular, when Cu or Ag is used, the resistance of the conductive film is reduced. This is preferable because it is possible to

[0096] [Insulating film that functions as a gate insulating film] An insulating film 106 that functions as a gate insulating film for the transistors 100A and 200A; The plasma enhanced chemical vapor deposition (PECVD) Oxidation is performed by the (chemical vapor deposition) method, sputtering method, etc. Silicon film, silicon oxynitride film, silicon oxynitride film, silicon nitride film, aluminum oxide hafnium oxide film, yttrium oxide film, zirconium oxide film, gallium oxide film , tantalum oxide film, magnesium oxide film, lanthanum oxide film, cerium oxide film and neodymium oxide film The insulating layer may be formed of one or more layers of a zirconia film. A laminated structure of three or more layers may also be used.

[0097] Also, a metal oxide film having a function as a channel region of the transistors 100A and 200A is formed. The insulating film 106 in contact with the insulating films 108 and 208 is preferably an oxide insulating film. It is more preferable to have a region (excess oxygen region) containing oxygen in excess of the stoichiometric composition. In other words, the insulating film 106 is an insulating film capable of releasing oxygen. To provide an excess oxygen region in the insulating film 106, for example, the insulating film 106 is formed in an oxygen atmosphere. Alternatively, the insulating film 106 after deposition may be heat-treated in an oxygen atmosphere.

[0098] Furthermore, when hafnium oxide is used as the insulating film 106, the following effects are obtained. Hafnium has a higher dielectric constant than silicon oxide and silicon oxynitride. Compared to the case where silicon oxide is used, the thickness of the insulating film 106 can be made larger, so that the tunnel This reduces the leakage current caused by the current. Furthermore, hafnium oxide, which has a crystalline structure, can be used to realize an amorphous structure. It has a higher relative dielectric constant than hafnium oxide, which has a low off-current. To form a transistor, it is preferable to use hafnium oxide having a crystalline structure. Examples of the crystal structure include monoclinic and cubic. The types are not limited to these.

[0099] However, the present invention is not limited to the above configuration. Alternatively, a nitride insulating film may be used. As an example of such a configuration, a silicon nitride film may be used. The surface of the silicon nitride film is subjected to oxygen plasma treatment or the like to form a silicon nitride film. The surface of the silicon nitride film is oxidized. When silicon nitride film is subjected to a thermal treatment, the surface of the silicon nitride film may be oxidized at the atomic level. Therefore, even if a cross section of a transistor is observed, the oxide film may not be observed. That is, when the cross section of the transistor is observed, the silicon nitride film and the metal oxide film are In addition, oxygen plasma treatment is a process in which oxygen gas is used The plasma is generated in an atmosphere containing oxygen, ozone, and other gases. This refers to gases that contain oxygen, such as nitrous oxide and nitrous oxide.

[0100] In addition, the silicon nitride film has a higher dielectric constant than the silicon oxide film. Since a large film thickness is required to obtain the same capacitance as that of a gate insulating film of a transistor, In addition, the insulating film 106 can be made thick by including a silicon nitride film. By suppressing the decrease in the dielectric strength of the transistor and improving the dielectric strength, Destruction can be suppressed.

[0101] In this embodiment, the insulating film 106 is a film made of a silicon nitride film and a silicon oxide film. A laminated film is formed.

[0102] [Metal oxide film] The metal oxide films 108 and 208 may be made of the materials listed above.

[0103] When the metal oxide film 108, 208 is an In-M-Zn oxide, The atomic ratio of the metal elements in the sputtering target used for film formation satisfies In>M. It is preferable that the atomic ratio of the metal elements in such a sputtering target is , In:M:Zn=2:1:3, In:M:Zn=3:1:2, In:M:Zn=4:2 :4.1, In:M:Zn=5:1:6, In:M:Zn=5:1:7, In:M:Zn = 5:1:8, In:M:Zn = 6:1:6, In:M:Zn = 5:2:5, etc. do.

[0104] In addition, when the metal oxide films 108 and 208 are made of In-M-Zn oxide, the The target used for the ion implantation was a polycrystalline In-M-Zn oxide target. It is preferable to use a target containing polycrystalline In-M-Zn oxide. In addition, the metal oxide film 108, 208 having the above structure can be easily formed. The atomic ratio of the films 108 and 208 is determined by the ratio of the metal elements contained in the sputtering target. The atomic ratio can vary by ±40%. For example, the metal oxide films 108 and 208 The composition of the sputtering target used is In:Ga:Zn=4:2:4.1 [atomic ratio] In this case, the composition of the metal oxide film 108, 208 to be formed is In:Ga:Zn=4:2. :3 [atomic ratio] may be close to

[0105] The metal oxide films 108 and 208 have an energy gap of 2 eV or more, preferably In this way, the energy gap of the oxide semiconductor is wide. As a result, the off-state current of the transistors 100A and 200A can be reduced.

[0106] In addition, it is preferable that the metal oxide films 108 and 208 have a non-single crystal structure. For example, CAAC-OS (C Axis Aligned Crystal Line Oxide Semiconductor, polycrystalline structure, microcrystalline structure, Among non-single crystal structures, the amorphous structure has the highest defect level density, C AAC-OS has the lowest defect state density.

[0107] In addition, the metal oxide films 108_1, 108_2, 208_1, and 208_2 are each independently In other words, even if there is a region in which the atomic ratio of In is greater than the atomic ratio of M, the metal oxide film 108 When the crystallinity of each of _1, 108_2, 208_1, and 208_2 is high, the field effect transfer The degree may be lower.

[0108] Therefore, the metal oxide film 108_1 has a region with lower crystallinity than the metal oxide film 108_2. In addition, the metal oxide film 208_1 may have a higher crystallinity than the metal oxide film 208_2. The metal oxide films 108_1, 108_2, and 208_1 may have regions with low conductivity. The crystallinity of 208_2 can be measured by, for example, X-ray diffraction (XRD: X-Ray Diffraction Analysis using a transmission electron microscope (TEM) or The analysis was carried out using a ssion electron microscope. Cut.

[0109] When the metal oxide films 108_1 and 208_1 have a region with low crystallinity, the following excellent It has an effect.

[0110] First, oxygen vacancies that can be formed in the metal oxide film 108 will be described.

[0111] The oxygen vacancies formed in the metal oxide film 108 are problematic because they affect the transistor characteristics. For example, when oxygen vacancies are formed in the metal oxide film 108, hydrogen is introduced into the oxygen vacancies. The carrier supply source is generated in the metal oxide film 108. The fluctuation of the electrical characteristics of the transistor 100A having the metal oxide film 108, typically Therefore, in the metal oxide film 108, oxygen vacancies occur. The less the better.

[0112] Therefore, in one embodiment of the present invention, the insulating film in the vicinity of the metal oxide film 108, specifically, The insulating films 114 and 116 formed above the metal oxide film 108 contain excess oxygen. Oxygen or excess oxygen is transferred from the insulating films 114 and 116 to the metal oxide film 108. By this, it becomes possible to reduce oxygen vacancies in the metal oxide film.

[0113] Here, using FIG. 16(A) and (B), oxygen or peroxide diffusing into the metal oxide film 108 is The route of excess oxygen will be described. FIG. 16(A) and (B) show the route of excess oxygen diffusing into the metal oxide film 108. FIG. 16(A) is a conceptual diagram showing the diffusion path of oxygen or excess oxygen in the channel length direction. FIG. 16(B) is a conceptual diagram of the channel width direction. The metal oxide film 108 will be used for the description, but the metal oxide film 208 may also be used for the metal oxide film 108. Oxygen diffuses in the same manner.

[0114] The oxygen or excess oxygen contained in the insulating films 114 and 116 is introduced from above, i.e., from the metal oxide. The electrons pass through the metal oxide film 108_2 and diffuse into the metal oxide film 108_1 (see FIG. 16(A) and (B)). Shown is Route 1).

[0115] Alternatively, the oxygen or excess oxygen contained in the insulating films 114 and 116 may be converted into oxygen from the metal oxide film 108. _1 and the metal oxide film 108_2 diffuse into the metal oxide film 108 from each side thereof. (Route 2 shown in Figure 16(B)).

[0116] For example, in the case of Route 1 shown in FIG. 16(A)(B), the metal oxide film 108_2 High crystallinity may hinder the diffusion of oxygen or excess oxygen. In the case of Route 2 shown in B), the metal oxide film 108_1 and the metal oxide film 108_ 2. From each side, oxygen or the like is introduced into the metal oxide film 108_1 and the metal oxide film 108_2. or excess oxygen can diffuse away.

[0117] In the case of Route 2 shown in FIG. 16B, the metal oxide film 108_1 is a metal oxide. When the oxide film 108_1 has a region with lower crystallinity than the oxide film 108_2, the region serves as a diffusion path for excess oxygen. As a result, the metal oxide film 108_2, which has higher crystallinity than the metal oxide film 108_1, also contains excess oxygen. Although not shown in FIGS. 16(A) and 16(B), an insulating film is also used. If 106 contains oxygen or excess oxygen, oxygen may enter the metal oxide film 108 from the insulating film 106. Oxygen or excess oxygen can diffuse out.

[0118] In this way, a laminated structure of metal oxide films with different crystallinity is formed, and the region with low crystallinity is treated with excess acid. By using an elemental diffusion path, a highly reliable transistor can be provided.

[0119] When the metal oxide film 108 is made of only a metal oxide film having low crystallinity, The channel side, that is, the region corresponding to the metal oxide film 108_2, is doped with impurities (e.g., hydrogen or Reliability may decrease due to adhesion of dirt, moisture, etc. or contamination by impurities. .

[0120] Impurities such as hydrogen or moisture that are mixed into the metal oxide film 108 affect the transistor characteristics. Therefore, in the metal oxide film 108, hydrogen or water The fewer impurities such as fluorine, the more preferable.

[0121] Therefore, by increasing the crystallinity of the metal oxide film on the upper layer of the metal oxide film 108, In particular, the metal oxide film 108_2 can suppress impurities that may be mixed into the metal oxide film 108_2. By increasing the crystallinity of the conductive films 112a and 112b, damage caused during processing can be suppressed. The surface of the metal oxide film 108, i.e., the surface of the metal oxide film 108_2, can be The conductive films 112a and 112b are exposed to an etchant or etching gas when processing the conductive films 112a and 112b. However, when the metal oxide film 108_2 has a region with high crystallinity, the region with low crystallinity The metal oxide film 108_1 has a higher etching resistance than the metal oxide film 108_2. The film 108_2 functions as an etching stopper.

[0122] The metal oxide film 108 is made of a metal oxide having a low impurity concentration and a low defect level density. By using the film, a transistor having excellent electrical characteristics can be manufactured, which is preferable. Here, high purity refers to low impurity concentration and low defect level density (low oxygen vacancies). The metal oxide film is called intrinsic or substantially high-purity intrinsic. In the present specification, the term "water and hydrogen" refers to the removal of water and hydrogen from a metal oxide film. The reduction or removal of the metal oxide film may be referred to as dehydration or dehydrogenation. Adding oxygen to an oxide insulating film may be referred to as oxygen addition. The state in which the mixture is mixed with water and has an excess of oxygen compared to the stoichiometric composition is sometimes referred to as an overoxygenated state.

[0123] High-purity intrinsic or substantially high-purity intrinsic metal oxide films have fewer carrier generation sources Therefore, the carrier density can be reduced. The transistors formed have electrical characteristics in which the threshold voltage is negative (normally on and Also, high purity intrinsic or substantially high purity intrinsic metals are rarely used. Since the oxide film has a low defect state density, the trap state density may also be low. High-purity intrinsic or substantially high-purity intrinsic metal oxide films have significantly lower off-state currents, Channel width is 1×10 6 Even if the device has a channel length L of 10 μm, the source electrode and When the voltage between the drain electrodes (drain voltage) is in the range of 1V to 10V, the off-state current is Below the measurement limit of the semiconductor parameter analyzer, i.e. 1×10 -13 Characteristics below A can be obtained.

[0124] The metal oxide film 108_1 has a region with lower crystallinity than the metal oxide film 108_2. By having such a structure, the carrier density may be increased.

[0125] In addition, when the carrier density of the metal oxide film 108_1 becomes high, the metal oxide film 108_1 The Fermi level may be relatively high with respect to the conduction band of the metal oxide. The lower end of the conduction band of the metal oxide film 108_1 becomes lower, and the lower end of the conduction band of the metal oxide film 108_2 and the gate The energy difference between the trap level that can be formed in the insulating film (the insulating film 106 in this example) and the When the energy difference becomes large, a transistor may occur in the gate insulating film. This may reduce the charge that is transferred to the transistor, and may reduce the variation in the threshold voltage of the transistor. In addition, when the carrier density of the metal oxide film 108_1 becomes high, the metal oxide film 108 The field effect mobility of the ZnO can be improved.

[0126] [Insulating film 1 that functions as a protective insulating film] The insulating films 114 and 116 function as protective insulating films for the transistors 100A and 200A. The insulating films 114 and 116 supply oxygen to the metal oxide films 108 and 208. That is, the insulating films 114 and 116 contain oxygen. Reference numeral 4 denotes an insulating film that can transmit oxygen. Note that the insulating film 114 is a film that is formed later. Also serves as a film for reducing damage to the metal oxide films 108 and 208 when forming the insulating film 116. It works.

[0127] The insulating film 114 has a thickness of 5 nm to 150 nm, preferably 5 nm to 50 nm. A silicon oxide film, a silicon oxynitride film, or the like having a thickness of 1 nm or less can be used.

[0128] In addition, it is preferable that the insulating film 114 has a small amount of defects. Typically, the insulating film 114 has a small amount of defects as determined by ESR measurement. The spin density of the signal at g=2.001 originating from the silicon dangling bond is 3×10 17 spins / cm 3 It is preferable that the insulating film 114 is If the defect density is high, oxygen will bind to the defects, and the oxygen permeability of the insulating film 114 will decrease. will decrease.

[0129] In the insulating film 114, all of the oxygen that has entered the insulating film 114 from the outside is Some oxygen does not move to the outside of the insulating film 114 and remains in the insulating film 114. At the same time, oxygen contained in the insulating film 114 moves to the outside of the insulating film 114, In some cases, oxygen may move through the film 114. When the oxide insulating film capable of forming the insulating film 116 is formed over the insulating film 114, The desorbed oxygen can be transferred to the metal oxide films 108 and 208 via the insulating film 114. can.

[0130] The insulating film 114 is formed using an oxide insulating film having a low density of states caused by nitrogen oxides. The density of states caused by the nitrogen oxides can be calculated by the valence charge of the metal oxide film. The upper edge of the electron band (Ev_os) and the lower edge of the conduction band (E c_os) may be formed during the above oxide insulating film. Silicon oxynitride film with low nitrogen oxide emission or aluminum oxynitride film with low nitrogen oxide emission A rubber film or the like can be used.

[0131] In addition, the silicon oxynitride film, which emits a small amount of nitrogen oxide, was analyzed by thermal desorption spectrometry (TD S: Thermal Desorption Spectroscopy This is a membrane that releases more ammonia than elemental oxide, and is typically The amount is 1×10 18 molecule / cm 3 5×10 or more 19 molecule / cm 3 The following is the case. The amount of NiA released is determined when the surface temperature of the film is 50°C or higher and 650°C or lower, preferably 50°C or higher and 550°C or lower. The amount released is determined by heating at or below ℃.

[0132] Nitrogen oxides (NO x , x is greater than 0 and less than or equal to 2, preferably greater than or equal to 1 and less than or equal to 2), In this case, NO2 or NO forms a level in the insulating film 114. The oxides of nitrogen are located within the energy gap of the insulating film 108, 208. When the metal oxide film 108 and the metal oxide film 208 diffuse to the interface between the insulating film 114 and the metal oxide film 108, 208, the level As a result, the trapped electrons may be trapped in the insulating film 11. 4 and the metal oxide film 108, 208. This shifts the value in the positive direction.

[0133] Nitrogen oxide reacts with ammonia and oxygen during heat treatment. The nitrogen oxide contained in the insulating film 116 reacts with ammonia contained in the insulating film 116 during the heat treatment. Therefore, the amount of nitrogen oxide contained in the insulating film 114 is reduced. Electrons are less likely to be trapped at the interfaces between the metal oxide films 108 and 208 .

[0134] By using the oxide insulating film as the insulating film 114, the threshold voltage of the transistor It is possible to reduce the shift in the electrical characteristics of the transistor. can.

[0135] The oxide insulating film was also analyzed by secondary ion mass spectrometry (SIMS). The nitrogen concentration measured by ion mass spectrometry is 6×10 20 a toms / cm 3 The following is the result.

[0136] The substrate temperature is between 220℃ and 350℃, and PEC using silane and nitrous oxide is used. By forming the oxide insulating film by the VD method, a dense and hard film can be obtained. It can be formed.

[0137] The insulating film 116 is an oxide insulating film containing more oxygen than the oxygen required for the stoichiometric composition. When the oxide insulating film is heated, some of the oxygen is released. The amount of oxygen released from the oxide insulating film is 1.0×10 19 atoms / cm 3 That's all good Preferably 3.0 x 10 20 atoms / cm 3 The above region is also included. The amount of release is determined when the heat treatment temperature in TDS is 50°C or higher and 650°C or lower, or when the heat treatment temperature is 50°C or higher and 650°C or lower. The total amount of oxygen released is below 550℃. The amount of oxygen released is calculated based on the oxygen content in TDS. This is the total amount converted into atoms.

[0138] The insulating film 116 has a thickness of 30 nm to 500 nm, preferably 50 nm or more. A silicon oxide film, a silicon oxynitride film, or the like having a thickness of 400 nm or less can be used.

[0139] In addition, it is preferable that the insulating film 116 has a small amount of defects. The spin density of the signal at g=2.001 originating from the silicon dangling bond is 1.5×10 18 spins / cm 3 Less than or even 1×10 18 spins / cm 3 Note that the insulating film 116 is preferably made of a metal oxide or less than the insulating film 114. Since it is separated from the films 108 and 208 , it may have a higher defect density than the insulating film 114 .

[0140] In addition, the insulating films 114 and 116 can be made of the same material, so that the insulating films In some cases, the interface between the film 114 and the insulating film 116 cannot be clearly seen. In this embodiment, the interface between the insulating film 114 and the insulating film 116 is shown by a dashed line. In the embodiment, the two-layer structure of the insulating film 114 and the insulating film 116 has been described. For example, the insulating film 114 may have a single layer structure or a laminated structure of three or more layers. Good too.

[0141] [Insulating film 2 that functions as a protective insulating film] The insulating film 118 functions as a protective insulating film for the transistors 100A and 200A.

[0142] The insulating film 118 contains either hydrogen or nitrogen, or both. The insulating film 118 contains nitrogen and silicon. The insulating film 118 contains oxygen, hydrogen, water, and alkali. The insulating film 118 has a function of blocking metals, alkaline earth metals, etc. As a result, oxygen diffuses from the metal oxide films 108 and 208 to the outside, and the insulating films 114 and 116 The oxygen contained in the metal oxide film 108, 208 diffuses to the outside, and hydrogen, water, etc. This can prevent the intrusion of

[0143] The insulating film 118 may be, for example, a nitride insulating film. Examples of the thin film include silicon nitride film, silicon oxynitride film, aluminum nitride film, and aluminum oxynitride film. Examples include tungsten films.

[0144] The various films such as the conductive film, insulating film, metal oxide film, and metal film described above include: It can be formed by sputtering or PECVD, but other methods, such as thermal It may be formed by a CVD (Chemical Vapor Deposition) method. As an example of thermal CVD, MOCVD (Metal Organic Chemical Vapor Deposition) is Vapor Deposition method or ALD (Atomic Layer Deposition) method Deposition method.

[0145] Thermal CVD is a film formation method that does not use plasma, so defects can occur due to plasma damage. The thermal CVD method has the advantage that the source gas is not generated in a chamber. The pressure in the chamber is then set to atmospheric pressure or reduced pressure, and a film is deposited on the substrate. .

[0146] In the ALD method, the source gas is sent into the chamber and the chamber is kept at atmospheric pressure or The pressure may be reduced and a film may be deposited on the substrate.

[0147] <1-3. Display device configuration example 2> Next, a display device having a different laminated structure of a protective insulating film will be described with reference to FIG.

[0148] FIG. 4(A-1) is a cross-sectional view taken along the dashed line X1-X2 in FIG. 2(A). FIG. 4(A-2) is a cross-sectional view taken along the dashed line Y1-Y2 in FIG. 2(A). FIG. 4(B-1) corresponds to a cross-sectional view taken along the dashed line X3-X4 in FIG. 2(B). FIG. 4(B-2) corresponds to a cross-sectional view of the cross section, and FIG. 4(B-2) is a cross-sectional view of the cross section between the dashed line Y3-Y4 shown in FIG. This corresponds to a cross-sectional view of a cut surface in a

[0149] In the display device shown in FIG. 4, an insulating film 114 is provided over a transistor 200A provided in a pixel portion. The insulating film 116 is provided with an insulating film 119 having a function as a planarizing film. The insulating film 114, the insulating film 116, and the insulating film 119 have an opening 242b. A conductive film 220a having a function as a pixel electrode is formed on the insulating film 119. The insulating film 220a is electrically connected to the conductive film 212b in the opening 242b. An insulating film 118 is provided on the insulating film 119 and the conductive film 220a. 10, and a portion of the conductive film 220a may be exposed in the opening.

[0150] The insulating film 119 is formed using an organic material that functions as a planarizing insulating film. The film 119 is formed by spin coating or printing using an organic material such as polyimide resin or acrylic resin. In addition to the above organic materials, low dielectric constant materials can be used. A material having a high dielectric constant (low-k material) can be used. A planarizing insulating film may be formed by stacking a plurality of insulating films. It is preferable to use an organic resin having light-transmitting properties, typically polyimide. By using an organic resin having light-transmitting properties as the substrate 119, the display device can be a transmissive liquid crystal display device. In this case, the transmittance of light from the backlight can be increased.

[0151] In the display device shown in FIG. 4, the driving circuit includes an insulating film 1 having a function as a planarizing film. Therefore, by using an oxide conductive film as the conductive film 120a, Oxygen can be added to the insulating films 114 and 116. The oxygen migrates to the metal oxide film 108 and compensates for the oxygen vacancies in the metal oxide film 108. This makes it possible to improve the reliability of the transistor 100A.

[0152] On the other hand, in the display device shown in FIG. 4, in the pixel portion, an insulating film having a function as a planarizing film is used. A conductive film 119 having a function as a pixel electrode is formed on the insulating film 116. The conductive film 220a is formed on the insulating film 119. Since the conductive film 220a has a high flatness, the display device In the case of a liquid crystal display device, it is possible to reduce alignment defects in the liquid crystal layer. The distance between the conductive film 204 and the conductive film 220a, which have both functions, and the conductive film 220b, which have both functions as a signal line, The insulating film 119 can widen the distance between the conductive film 212a and the conductive film 220a. This makes it possible to reduce wiring delay.

[0153] <1-4. Display device configuration example 3> Next, regarding display devices with different shapes of conductive films functioning as pixel electrodes, FIG. This will be explained with reference to FIG.

[0154] FIG. 9 illustrates a transistor included in a driver circuit and a display unit in a display device according to one embodiment of the present invention. 9A is a top view of a transistor 100A included in a driver circuit. 9(B) is a top view of a transistor 200B included in a pixel portion. A-1) corresponds to a cross-sectional view taken along the dashed line X1-X2 in FIG. 9(A), FIG. 8(A-2) corresponds to a cross-sectional view taken along the dashed line Y1-Y2 in FIG. 9(A). FIG. 8(B-1) is a cross-sectional view taken along the dashed line X3-X4 in FIG. 9(B). FIG. 8(B-2) corresponds to a cross-sectional view taken along the dashed line Y3-Y4 shown in FIG. 9(B). It corresponds to a cross-sectional view of a surface.

[0155] As shown in FIG. 8(A-1) and FIG. 8(A-2), the driving circuit includes a transistor 100A. Yes.

[0156] As shown in FIG. 8B-1 and FIG. 8B-2, the pixel portion includes a transistor 200. B includes a conductive film 210 functioning as a pixel electrode and a capacitor element 250.

[0157] The transistor 200B has a pixel capacitance of 1.0 V compared to the transistor 200A shown in FIGS. The transistor 200B is different in the connection with the conductive film having the function as an electrode. Between the conductive film 212b and the conductive film 210 having a function as a pixel electrode, Connected.

[0158] The conductive film 210 is the metal oxide film 108 of the transistor 100A and the metal oxide film 108 of the transistor 200B. The conductive film 210 is formed simultaneously with the metal oxide film 208. The conductive film 210 is made up of island-shaped conductive films 210_1 and 210_2. The conductive film 210_1 is a metal oxide film 108. _1, 208_1, and the conductive film 210_2 is formed at the same time as the metal oxide films 108_2, 2 Formed at the same time as 08_2.

[0159] In FIG. 8(B-1), the insulating film 118 has an opening 211. 1, the conductive film 210 is exposed. Also, as shown in FIG. 10(B-1), 118 may cover the conductive film 210. For example, when the display device is a liquid crystal display device, It is preferable that the insulating film 118 is not provided on the conductive film 210 having a function as an electrode. However, depending on the voltage applied to the liquid crystal layer, the insulating film 118 may be provided. stomach.

[0160] The conductive film 210 is preferably an oxide conductive film (OC). In comparison with the metal oxide films 108 and 208 included in 200A and 200B, the conductive film 210 is The element concentration is high.

[0161] <1-5. Modified Transistors> Next, modified examples of the transistor that can be used in this embodiment will be described. FIG. 14A is a top view of a transistor 100C, and FIG. 14B is a top view of a transistor 100C shown in FIG. 4(A) is a cross-sectional view taken along the dashed line X1-X2 in FIG. 14(C). 14(A) corresponds to a cross-sectional view taken along the dashed line Y1-Y2 in FIG. Here, a modified example of the transistor 100A will be described as the transistor 100C. The configuration of the transistor 100C can be appropriately applied to the transistors 200A and 200B. do.

[0162] The transistor 100C has the conductive films 112a and 112b of the transistor 100A. 12b is a three-layer laminated structure.

[0163] The conductive film 112a of the transistor 100C includes a conductive film 112a_1 and a conductive film 11 A conductive film 112a_2 on the conductive film 2a_1 and a conductive film 112a_3 on the conductive film 112a_2 are The conductive film 112b included in the transistor 100C is a conductive film 112b_1. , a conductive film 112b_2 on the conductive film 112b_1, and a conductive film 112 on the conductive film 112b_2 b_3 and

[0164] For example, the conductive film 112a_1, the conductive film 112b_1, the conductive film 112a_3, and the conductive film 112b_3 includes titanium, tungsten, tantalum, molybdenum, indium, and gallium. It is preferable that the metal oxide contains one or more selected from the group consisting of lithium, tin, and zinc. The conductive film 112a_2 and the conductive film 112b_2 are made of copper, aluminum, or silver. It is preferable that the ink composition has one or more selected from the following:

[0165] More specifically, the conductive film 112a_1, the conductive film 112b_1, the conductive film 112a_3, and and the conductive film 112b_3 is made of In-Sn oxide or In-Zn oxide. Copper can be used for the conductive film 112a_2 and the conductive film 112b_2.

[0166] With the above-mentioned configuration, the wiring resistance of the conductive films 112a and 112b is reduced, and the metal oxide This is preferable because it can suppress the diffusion of copper into the conductive film 108. The contact resistance between the conductive film 112b and a conductive film in contact with the conductive film 112b can be reduced. In addition, when the above configuration is applied to the transistor 200A of the pixel portion, This is preferable because it is possible to reduce the contact resistance between the conductive film 212b and the conductive film 220a. The other configurations of the transistor 100C are the same as those of the transistor 100A described above. and has the same effect.

[0167] FIG. 15A shows a transistor 1 which can be used in this embodiment. 15(B) is a top view of 00D, and FIG. 15(B) is a top view of the 00D between the dashed line X1-X2 shown in FIG. FIG. 15(C) corresponds to a cross-sectional view of the cut surface in the cross section taken along the dashed line Y1-Y2 in FIG. 15(A). This corresponds to a cross-sectional view of the cut surface between the two.

[0168] The transistor 100D has the same structure as the transistor 100A except for the conductive films 112a and 1 The transistor 100D has a three-layer structure. The transistor 100C differs from the transistor 100 in the shape of the conductive films 112a and 112b.

[0169] The conductive film 112a of the transistor 100D includes a conductive film 112a_1 and a conductive film 11 A conductive film 112a_2 on the conductive film 2a_1 and a conductive film 112a_3 on the conductive film 112a_2 are The conductive film 112b included in the transistor 100D is a conductive film 112b_1. , a conductive film 112b_2 on the conductive film 112b_1, and a conductive film 112 on the conductive film 112b_2 b_3. _3, the conductive film 112b_1, the conductive film 112b_2, and the conductive film 112b_3 are The materials shown in the following can be used.

[0170] In addition, the end of the conductive film 112a_1 is located outside the end of the conductive film 112a_2. The conductive film 112a_3 covers the upper surface and side surfaces of the conductive film 112a_2 and has a conductive The conductive film 112b_1 has an area in contact with the conductive film 112a_1. The conductive film 112b_3 has an area located outside the end of the conductive film 11 It covers the upper surface and side surfaces of 2b_2 and has a region in contact with the conductive film 112b_1.

[0171] With the above-mentioned configuration, the wiring resistance of the conductive films 112a and 112b is reduced, and the metal oxide This is preferable because it can suppress the diffusion of copper into the semiconductor film 108. It has been found that the structure shown in transistor 100D is more effective at suppressing copper diffusion than that of transistor 100C. In addition, with the above structure, the conductive film 112b and the conductive film 112b This is preferable because it is possible to reduce the contact resistance with the conductive film formed on the transistor 10. The other configurations of OD are similar to those of the transistors shown above, and provide similar effects.

[0172] The transistors 100A, 100C, 200A, and 200B are formed using six photomasks. On the other hand, the transistor 100D is fabricated using the conductive films 112a and 112 In order to form b, two photomasks are used, so seven photomasks are used. It is produced by

[0173] FIG. 17A shows a transistor 1 which can be used in this embodiment. 17(B) is a top view of 00E, and FIG. 17(B) is a top view of the 00E between the dashed line X1-X2 shown in FIG. FIG. 17(C) corresponds to a cross-sectional view of the cut surface in the state shown in FIG. 17(A) along the dashed line Y1-Y2. This corresponds to a cross-sectional view of the cut surface between the two.

[0174] The transistor 100E shown in FIG. 17 has the insulating film 118 The stacking order of the conductive film 120a and the insulating film 116 in the transistor 100E is different. The insulating film 118 is provided. The conductive film 120a is provided on the insulating film 118. In the opening 142 a of the film 114 , the insulating film 116 , and the insulating film 118 , the conductive film 104 and the The conductive film 120a is electrically connected to the conductive film 120b.

[0175] In addition, the transistor according to the present embodiment is a transistor having the above structure, which is independently It is possible to combine them freely.

[0176] <1-6. Display device manufacturing method 1> Next, a method for manufacturing the transistors 100A and 200A included in the display device of one embodiment of the present invention will be described. The method will be described with reference to FIGS.

[0177] 5 to 7 are cross-sectional views illustrating a method for manufacturing a display device. 1A-1 to 1A-3 are cross-sectional views of a transistor 100A in the channel length direction. 1A to 1C are cross-sectional views of the transistor 200A in the channel length direction. do.

[0178] First, a conductive film is formed on the substrate 102, and the conductive film is then subjected to a lithography process and an etching process. The process is carried out to form a conductive film having a function as the first gate electrode of the transistor 100A. The conductive film 204 having the function of the gate electrode of the transistor 200A is formed on the film 104. Next, an insulating film 106 having a function as a first gate insulating film is formed on the conductive film 104. (See FIG. 5(A-1) and FIG. 5(B-1)).

[0179] In this embodiment, a glass substrate is used as the substrate 102, and a conductive film 104 or 204 is A titanium film having a thickness of 50 nm and a copper film having a thickness of 200 nm were deposited by sputtering. The insulating film 106 is a silicon nitride film having a thickness of 400 nm and a silicon nitride film having a thickness of 50 A silicon oxynitride film having a thickness of nm is formed by PECVD.

[0180] The silicon nitride film includes a first silicon nitride film, a second silicon nitride film, and a third silicon nitride film. The silicon nitride film 3 is a three-layer laminate structure. An example of the three-layer laminate structure is as follows: It can be formed as follows.

[0181] The first silicon nitride film is formed by, for example, silane at a flow rate of 200 sccm, PECVD was performed using nitrogen at a flow rate of 100 sccm and ammonia gas at a flow rate of 100 sccm as source gas. The pressure in the reaction chamber was controlled at 100 Pa, and a high-frequency wave of 27.12 MHz was generated. A power of 2000 W may be supplied using a microwave power source to form the film to a thickness of 50 nm. stomach.

[0182] For the second silicon nitride film, silane at a flow rate of 200 sccm, The nitrogen gas and the ammonia gas with a flow rate of 2000sccm were used as raw material gases in the PECVD equipment. The pressure in the reaction chamber was controlled to 100 Pa, and a 27.12 MHz high-frequency power supply was used. A power of 2000 W may be supplied using the above method to form a film having a thickness of 300 nm.

[0183] The third silicon nitride film was prepared by using silane at a flow rate of 200 sccm and 5000 sccm. The pressure in the reaction chamber was kept at 100 The thickness was measured by controlling the temperature to 50 Pa and supplying 2000 W of power using a 27.12 MHz high frequency power source. It is sufficient to form it so that the thickness is 50 nm.

[0184] The first silicon nitride film, the second silicon nitride film, and the third silicon nitride film The substrate temperature during formation can be 350° C. or less.

[0185] By forming the silicon nitride film into the above-mentioned three-layer laminated structure, for example, the conductive film 104 can be made to contain copper. When a conductive film including the conductive material is used, the following effects are obtained.

[0186] The first silicon nitride film can suppress the diffusion of copper from the conductive films 104 and 204. The second silicon nitride film has a function of releasing hydrogen and a function as a gate insulating film. The third silicon nitride film can improve the breakdown voltage of the insulating film. Hydrogen release from the silicon nitride film is small, and hydrogen released from the second silicon nitride film is diffused. can be suppressed.

[0187] Next, a metal oxide film 108_1_0 and a metal oxide film 108_2_ 0 (see Figure 5(A-2) and Figure 5(B-2)).

[0188] 5A-1 and 5B-1 show a metal oxide film 108_1 formed on the insulating film 106. 1 is a schematic cross-sectional view of the inside of a film forming apparatus when forming a metal oxide film 108_0 and a metal oxide film 108_2_0. In Fig. 5(A-1) and Fig. 5(B-1), a sputtering device is used as the film forming device. A target 191 is installed inside the sputtering device, and a The plasma 192 that is formed is shown diagrammatically.

[0189] In addition, in FIG. 5(A-1) and FIG. 5(B-1), oxygen or The excess oxygen is represented by a dashed arrow. For example, in the metal oxide film 108_1_0, When oxygen gas is used in the deposition, oxygen can be suitably added to the insulating film 106 .

[0190] First, a metal oxide film 108_1_0 is formed on the insulating film 106. The thickness of _1_0 is 1 nm or more and 25 nm or less, preferably 5 nm or more and 20 nm or less. The metal oxide film 108_1_0 is formed by absorbing an inert gas (typically, Ar gas). The metal oxide film 10 is formed by using either or both of a metal oxide gas and an oxygen gas. The ratio of oxygen gas in the total deposition gas when forming 8_1_0 (hereinafter referred to as the oxygen flow ratio) The content of the oxidizing agent (referred to as "oxidizing agent") is 0% or more and less than 30%, and preferably 5% or more and 15% or less.

[0191] By forming the metal oxide film 108_1_0 at the oxygen flow rate ratio in the above range, the metal oxide film The crystallinity of the metal oxide film 108_1_0 can be made lower than that of the metal oxide film 108_2_0.

[0192] Subsequently, a metal oxide film 108_2_0 is formed on the metal oxide film 108_1_0. When forming the metal oxide film 108_2_0, plasma is generated in an atmosphere containing oxygen gas. At that time, the metal oxide film 108_2_0 is formed on the metal oxide film 108_2_0. Oxygen is added to the metal oxide film 108_1_0. The flow rate ratio of the primary gas is 30% or more and 100% or less, preferably 50% or more and 100% or less, and more preferably 50% or more and 100% or less. More preferably, it is 70% or more and 100% or less.

[0193] The thickness of the metal oxide film 108_2_0 is preferably 20 nm or more and 100 nm or less. Preferably, the thickness is 20 nm or more and 50 nm or less.

[0194] As described above, the conditions for forming the metal oxide film 108_2_0 are as follows: It is preferable to increase the oxygen flow rate of the metal oxide film 108_1_0. It is preferable that the metal oxide film 108_1_0 is formed at a lower oxygen partial pressure than that of the metal oxide film 108_2_0.

[0195] In addition, the substrate when the metal oxide film 108_1_0 and the metal oxide film 108_2_0 are formed The temperature is from room temperature (25°C) to 200°C, preferably from room temperature to 130°C. By setting the substrate temperature in the above range, it is possible to form a large-area glass substrate (for example, This is particularly suitable for use with 8th to 10th generation glass substrates. The substrate temperature during the deposition of the metal oxide film 108_1_0 and the metal oxide film 108_2_0 is room temperature. By this, it is possible to suppress bending or distortion of the substrate. In the case where it is desired to improve the crystallinity of the metal oxide film 108_2_0, the substrate Higher temperatures are preferred.

[0196] The metal oxide film 108_1_0 and the metal oxide film 108_2_0 are successively formed in a vacuum. This is more preferable because it prevents impurities from being introduced into the interfaces.

[0197] In addition, the sputtering gas must be highly purified. The oxygen gas and argon gas used in the present invention have a dew point of -40°C or less, preferably -80°C or less, and Preferably, the gas is purified to a temperature of -100°C or lower, more preferably -120°C or lower. By using this, it is possible to prevent moisture and the like from being taken into the metal oxide film as much as possible.

[0198] In addition, when forming a metal oxide film by sputtering, The chamber is cryo-treated to remove as much water as possible, which is an impurity for the metal oxide film. A high vacuum (5×10 -7 Pa to 1×1 0 -4 It is preferable to evacuate the gas to a pressure of about 10 Pa. Gas molecules equivalent to HO in the chamber (gas molecules equivalent to m / z=18) The partial pressure is 1×10 -4 Pa or less, and 5×10 -5 Pa or less is preferred.

[0199] In this embodiment, the conditions for forming the metal oxide film 108_1_0 are In-Ga-Z Using an n-metal oxide target (In:Ga:Zn=4:2:4.1 [atomic ratio]), The metal oxide film 108_1_0 is formed by a sputtering method. The temperature was set to room temperature, and the deposition gas was argon gas with a flow rate of 180 sccm and argon gas with a flow rate of 20 sccm. Use oxygen gas (oxygen flow rate ratio 10%).

[0200] The metal oxide film 108_2_0 was formed under the following conditions: In-Ga-Zn metal oxide Using a target (In:Ga:Zn=4:2:4.1 [atomic ratio]), sputtering was performed. The metal oxide film 108_2_0 is formed by a bonding method. The substrate temperature during the formation of the metal oxide film 108_2_0 is set to room temperature. As a deposition gas, oxygen gas with a flow rate of 200 sccm is used (oxygen flow rate ratio 100%).

[0201] In addition, oxygen during the formation of the metal oxide film 108_1_0 and the metal oxide film 108_2_0 By changing the flow rate ratio, it is possible to form laminated films having different crystallinity.

[0202] Although the manufacturing method using the sputtering method has been described here, the present invention is not limited to this. First, pulsed laser deposition (PLD), plasma enhanced chemical vapor deposition (PECVD), and thermal CV D (Chemical Vapor Deposition) method, ALD (Atomic Alternatively, a thermal CVD method, a vacuum deposition method, etc. may be used. An example of this is MOCVD (Metal Organic Chemical Vapor Deposition). r Deposition method is one example.

[0203] Next, the metal oxide film 108_1_0 and the metal oxide film 108_2_0 are formed into a desired shape. By processing, the island-shaped metal oxide film 108_1 and the island-shaped metal oxide film 108_2, In addition, an island-shaped metal oxide film 208_1 and an island-shaped metal oxide film 208_2 are formed. In this embodiment, the metal oxide film 108_1 and the metal oxide film 108_2 Thus, island-shaped metal oxide films 108 are formed (see FIG. 5(A-3)). The film 208_1 and the metal oxide film 208_2 constitute an island-shaped metal oxide film 208. (See Figure 5(B-3)).

[0204] After the metal oxide film 108 and the metal oxide film 208 are formed, the metal oxide film 108 The metal oxide film 208 may be subjected to oxygen plasma treatment. It is possible to add oxygen to the surfaces of the metal oxide film 108 and the metal oxide film 208. In particular, the oxygen vacancies in the metal oxide film 208 and the metal oxide film 208 can be reduced. Reducing the oxygen vacancies on the side surfaces of the film 108 and the metal oxide film 208 improves the transistor performance. This is preferable because it is possible to suppress the occurrence of leakage current in the capacitor.

[0205] After the metal oxide films 108 and 208 are formed, a heat treatment (hereinafter, a first heat treatment) is performed. The first heat treatment is preferably performed to remove the oxide contained in the metal oxide films 108 and 208. It is possible to reduce hydrogen, water, etc. contained in the fuel. The treatment may be performed before processing the metal oxide films 108_1_0 and 108_2_0 into islands. The first heat treatment is one of the purification treatments for a metal oxide film.

[0206] The first heat treatment is performed at a temperature of, for example, 150° C. or higher and lower than the distortion point of the substrate, preferably 200° C. °C or higher and 450 °C or lower, and more preferably 250 °C or higher and 350 °C or lower.

[0207] The first heat treatment can be performed using an electric furnace, an RTA device, or the like. By using this, it is possible to perform heat treatment at a temperature above the distortion point of the substrate for a short period of time. Therefore, the heating time can be shortened. Dry air (water content is 20 ppm or less, preferably 1 ppm or less, preferably 10 ppm The reaction may be carried out under an atmosphere of air (air (B) or less) or a rare gas (argon, helium, etc.). It is preferable that the nitrogen, oxygen, ultra-dry air, or rare gas does not contain hydrogen, water, etc. In addition, after heat treatment in a nitrogen or rare gas atmosphere, it is heated in an oxygen or ultra-dry air atmosphere. As a result, hydrogen, water, etc. contained in the metal oxide film are released, and the metal Oxygen can be supplied to the oxide film. As a result, oxygen deficiency in the metal oxide film is eliminated. Losses can be reduced.

[0208] Next, a conductive film is formed over the insulating film 106 and the metal oxide films 108 and 208. The conductive film is processed into a desired shape to form the conductive film 112a, the conductive film 112b, and the conductive film 2. 12a, a conductive film 212b, and a conductive film 213 are formed.

[0209] In this embodiment, the conductive film 112a, the conductive film 112b, the conductive film 212a, and the conductive film 2 12b, and a conductive film 213 made of a titanium film having a thickness of 30 nm and a copper film having a thickness of 200 nm. A 10 nm thick titanium film and a 10 nm thick titanium film are then formed in this order by sputtering.

[0210] Note that in this embodiment mode, the conductive film is processed using a wet etching apparatus. However, the method for processing the conductive film is not limited to this, and may be, for example, a dry etching apparatus. may also be used.

[0211] After the conductive films 112a, 112b, 212a, 212b, and 213 are formed, a metal oxide The surfaces (baths) of the metal oxide films 108, 208 (more specifically, the metal oxide films 108_2, 208_2) The cleaning method may be, for example, cleaning the side of the substrate (the side of the substrate) with a chemical solution such as phosphoric acid. By performing cleaning using a chemical solution such as phosphoric acid, the metal oxide film 10 Impurities (e.g., conductive films 112a, 112b, 21 The cleaning can be performed to remove elements contained in the SiO2 layer, such as elements contained in SiO2, SiO2, and SiO2. It is not necessary to perform this, and in some cases, cleaning may not be required.

[0212] Also, a step of forming conductive films 112a, 112b, 212a, 212b, and 213; In either or both of the above cleaning steps, the conductive film of the metal oxide film 108, 208 The exposed areas of 112a, 112b, 212a, 212b may be thinned.

[0213] In addition, the regions exposed from the conductive films 112a, 112b, 212a, and 212b, i.e., The metal oxide films 108_2 and 208_2 are preferably metal oxide films with enhanced crystallinity. A metal oxide film with high crystallinity is preferable because it is free of impurities, particularly the conductive films 112a, 112b, and 212. The constituent elements used in 212a and 212b are unlikely to diffuse into the film. It is possible to fabricate high-performance transistors.

[0214] In addition, in FIG. 5(A-3) and FIG. 5(B-3), the conductive films 112a, 112b, and 212 a, 212b, i.e., the surfaces of the metal oxide films 108, 208 exposed from the metal oxide films 1 Although the above embodiment has been described with respect to a case where a recess is formed on the surface of 08_2 and 208_2, the present invention is not limited to this. The metal oxide film 108 exposed from the conductive films 112a, 112b, 212a, and 212b is , 208 may not have any recesses.

[0215] Next, the metal oxide films 108 and 208 and the conductive films 112a, 112b, 212a, and 21 An insulating film 114 and an insulating film 116 are formed on the insulating film 2b and the insulating film 213 (FIG. 6(A-1), FIG. 6( See B-1)).

[0216] After the insulating film 114 is formed, the insulating film 116 is successively formed without exposing it to the air. After the insulating film 114 is formed, it is preferable to adjust the flow rate, pressure, and temperature of the source gas without exposing the insulating film 114 to the air. By adjusting one or more of the frequency power and the substrate temperature, the insulating film 116 is continuously formed. The concentration of impurities derived from atmospheric components can be reduced at the interface between the insulating film 114 and the insulating film 116. can.

[0217] For example, a silicon oxynitride film is formed as the insulating film 114 by using a PECVD method. In this case, the source gas may be a deposition gas containing silicon and an oxidizing gas. Representative examples of deposition gases containing silicon include silane, disilane, etc. Examples of oxidizing gases include nitrous oxide, nitrous oxide, and trisilane. In addition, the flow rate of the oxidizing gas is set to 20 times or more than 50 times the flow rate of the deposition gas. 0 times or less, preferably 40 times or more and 100 times or less.

[0218] In this embodiment, the insulating film 114 is formed by heating the substrate 102 at a temperature of 220° C. The source gases were silane at a flow rate of 50 sccm and dinitrogen monoxide at a flow rate of 2000 sccm. The pressure in the treatment chamber was set to 20 Pa, and the high frequency power supplied to the parallel plate electrodes was set to 13.56 M. Hz, 100W (power density is 1.6×10 -2 W / cm 2 ) PECVD method A silicon oxynitride film is formed using this.

[0219] The insulating film 116 is formed by depositing a substrate in a vacuum-evacuated processing chamber of a PECVD apparatus. The temperature is kept at 180°C or higher and 350°C or lower, and the raw material gas is introduced into the treatment chamber to increase the pressure in the treatment chamber. is set to 100 Pa or more and 250 Pa or less, and more preferably set to 100 Pa or more and 200 Pa or less. 0.17 W / cm2 at the electrode installed in the treatment chamber 2 More than 0.5W / cm 2 Below are some more Preferably 0.25W / cm 2 More than 0.35W / cm 2 The following high frequency power supply conditions are met: In this way, a silicon oxide film or a silicon oxynitride film is formed.

[0220] The conditions for forming the insulating film 116 are as follows: high frequency power density in a reaction chamber with the above pressure; By supplying power, the efficiency of decomposition of the source gas in the plasma increases, and the number of oxygen radicals increases. As the oxidation of the source gas progresses, the oxygen content in the insulating film 116 becomes lower than the stoichiometric composition. On the other hand, in the film formed at the above substrate temperature, the bonding strength between silicon and oxygen is Since the oxygen in the film is weak, some of the oxygen in the film is released by the heat treatment in the subsequent process. An oxide that contains more oxygen than satisfies the theoretical composition and loses some of the oxygen when heated. An insulating film can be formed.

[0221] In the process of forming the insulating film 116, the insulating film 114 is formed on the metal oxide films 108 and 208. Therefore, while reducing damage to the metal oxide films 108 and 208, The insulating film 116 can be formed using high-frequency power with a high power density.

[0222] In the deposition conditions for the insulating film 116, a deposition gas containing silicon is mixed with an oxidizing gas. By increasing the flow rate of the gas, it is possible to reduce the amount of defects in the insulating film 116. In the first place, ESR measurements revealed that the g value was 2.001, which is due to the dangling bonds of silicon. The spin density of the signal is 6×10 17 spins / cm 3 Less than 3 x 10 17 spins / cm 3 Less than or equal to 1.5×10 17 spins / cm 3 The following is a missing It is possible to form an oxide insulating film with few pits. As a result, the transistor 100A, The reliability of 200A can be improved.

[0223] After the insulating films 114 and 116 are formed, heat treatment (hereinafter referred to as second heat treatment) is performed. The nitrogen oxide contained in the insulating films 114 and 116 is preferably removed by the second heat treatment. Alternatively, the second heat treatment can reduce the amount of oxides in the insulating films 114 and 116. A part of the oxygen contained in the metal oxide film 108, 208 is transferred to the metal oxide film 108, 208. It is possible to reduce the oxygen vacancies contained in 08.

[0224] The temperature of the second heat treatment is typically less than 400° C., preferably less than 375° C., and The second heat treatment is preferably performed at a temperature of 150° C. or higher and 350° C. or lower. Dry air (water content is 20 ppm or less, preferably 1 ppm or less, preferably 10 ppb The reaction may be carried out under an atmosphere of air (see below) or a rare gas (argon, helium, etc.). It is preferable that the nitrogen, oxygen, ultra-dry air, or rare gas does not contain hydrogen, water, or the like. The heat treatment can be performed using an electric furnace, RTA, or the like.

[0225] Next, openings 142a, 242a are formed in desired regions of the insulating films 114, 116.

[0226] In this embodiment, the openings 142a and 242a are formed using a dry etching device. The opening 142a reaches the conductive film 104, and the opening 242a reaches the conductive film 2. Reach 12b.

[0227] Next, a conductive film 120 is formed on the insulating film 116 (FIGS. 6(A-2) and 6(B-2)). reference).

[0228] 6A-1 and 6B-1 show a process for forming a conductive film 120 on an insulating film 116. 6(A-1) and 6(B-1) are schematic cross-sectional views of the inside of a film forming apparatus when a film is formed. A sputtering device was used as the device, and a target was placed inside the sputtering device. 1, a target 193 and a plasma 194 formed below the target 193 are shown. It is being done.

[0229] First, when forming the conductive film 120, plasma is discharged in an atmosphere containing oxygen gas. At this time, oxygen is added to the insulating film 116, which is the surface on which the conductive film 120 is to be formed. When forming the conductive film 120, in addition to oxygen gas, an inert gas (e.g., helium gas, Argon gas, xenon gas, etc.) may be mixed.

[0230] The oxygen gas may be contained at least when the conductive film 120 is formed. The ratio of oxygen gas in the entire deposition gas when forming the film 120 is greater than 0%. 100% or less, preferably 10% to 100%, more preferably 30% to 100%. % or less.

[0231] In addition, in FIG. 6A and FIG. 6B, the oxygen added to the insulating film 116 The excess oxygen is represented diagrammatically by dashed arrows.

[0232] In this embodiment, an In-Ga-Zn metal oxide target (In:Ga:Zn=4: 2:4.1 [atomic ratio], the conductive film 120 is formed by sputtering. Alternatively, sputtering was performed using an ITO target and 100% oxygen gas as the deposition gas. The conductive film 120 may be formed by a ring method.

[0233] Note that in this embodiment, oxygen is added to the insulating film 116 when the conductive film 120 is formed. However, the present invention is not limited to this. For example, after the conductive film 120 is formed, Oxygen may be added to the insulating film 116.

[0234] As a method for adding oxygen to the insulating film 116, for example, indium, tin, and silicon An oxide (In-Sn-Si oxide, also called ITSO) target (InO 3: SnO2: SiO2 = 85: 10: 5 [wt %]) was used to form a 5 nm thick ITSO In this case, the thickness of the ITSO film is 1 nm or more and 20 nm or less. Alternatively, when the thickness is set to 2 nm or more and 10 nm or less, oxygen can be suitably transmitted and oxygen release can be suppressed. Then, oxygen is added to the insulating film 116 by passing it through an ITSO film. The method of adding the element includes ion doping, ion implantation, plasma treatment, etc. In addition, when oxygen is added, a bias voltage is applied to the substrate side to effectively The insulating film 116 can be applied with a bias voltage of, for example, asyn The power density of the bias voltage applied to the substrate side of the ashing device was set to 1 W / cm. m 2 More than 5W / cm 2 The substrate temperature when oxygen is added is as follows: The insulating film 1 is formed by heating the insulating film 1 at a temperature of from room temperature to 300° C., preferably from 100° C. to 250° C. Oxygen can be efficiently added to 16.

[0235] Next, the conductive film 120 is processed into a desired shape to form the conductive films 120a_1, 220a_ 1 (see FIG. 7(A-1) and FIG. 7(B-1)).

[0236] In this embodiment, a wet etching device is used to process the conductive film 120. The conductive films 120a_1 and 220a_1 are formed.

[0237] Next, the insulating film 118 is formed on the insulating film 116 and the conductive films 120a_1 and 220a_1. (See FIG. 7(A-2) and FIG. 7(B-2)).

[0238] The insulating film 118 contains either hydrogen or nitrogen, or both. For example, a silicon nitride film is preferably used as the insulating film 118. For example, it can be formed by using a sputtering method or a PECVD method. When the insulating film 118 is formed by the PECVD method, the substrate temperature is set to less than 400° C., preferably less than 375° C. The temperature is preferably less than 180° C. and more preferably 350° C. or higher. In this case, it is preferable to set the substrate temperature in the above-mentioned range since a dense film can be formed. By setting the substrate temperature in the above range when forming the insulating film 118, the insulating films 114 and 1 The oxygen or excess oxygen in the metal oxide film 108, 208 can be transferred to the metal oxide film 108, 208. become.

[0239] In addition, when a silicon nitride film is formed as the insulating film 118 by the PECVD method, silicon It is preferable to use a deposition gas containing nitrile, nitrogen, and ammonia as the source gas. By using a small amount of ammonia compared to hydrogen, ammonia dissociates in the plasma and becomes active. The active species are generated by bonding with silicon and hydrogen contained in the silicon-containing deposition gas. This breaks the triple bond between silicon and nitrogen. As a result, the bond between silicon and nitrogen is promoted, It is possible to form a dense silicon nitride film with few silicon and hydrogen bonds and few defects. On the other hand, if the amount of ammonia relative to nitrogen is large, the deposition gas containing silicon and the nitrogen The decomposition of the silicon does not proceed, silicon and hydrogen bonds remain, and defects increase and the material becomes rough. For these reasons, the source gas is not suitable for ammonia. It is preferable that the flow rate ratio of nitrogen to oxygen is 5 times or more and 50 times or less, and more preferably 10 times or more and 50 times or less.

[0240] In this embodiment, the insulating film 118 is formed by depositing silane, nitrogen, etc., using a PECVD apparatus. A silicon nitride film with a thickness of 50 nm is formed using nitrogen and ammonia as source gases. The flow rates were 50 sccm for silane, 5000 sccm for nitrogen, and 100 for ammonia. The pressure in the processing chamber was 100 Pa, the substrate temperature was 350°C, and the flow rate was 27.12 MWh. A high-frequency power supply of 1000 W is supplied to the parallel plate electrodes. The device has an electrode surface area of ​​6000 cm 2 The parallel plate type PECVD equipment is The force can be converted to power per unit area (power density) of 1.7 x 10 -1 W / cm 2 is .

[0241] The conductive films 120a_1 and 220a_1 are made of In-Ga-Zn metal oxide target. When a conductive film is formed using a ZnO solution (In:Ga:Zn=4:2:4.1 [atomic ratio]) By forming the insulating film 118, either hydrogen or nitrogen contained in the insulating film 118 is removed. Or, both may penetrate into the conductive films 120a_1 and 220a_1. In this case, Oxygen deficiency and either hydrogen or nitrogen in the conductive films 120a_1 and 220a_1, or By bonding the two together, the resistance of the conductive films 120a_1 and 220a_1 is reduced. As a result, the conductive films 120a and 220a having reduced resistance can be formed. The reduced conductive film is an oxide conductive film. Either one or both of the elements move to the conductive film 120a, 220a, thereby forming the conductive film 12 The hydrogen concentration and / or nitrogen concentration of the metal oxide films 108, 200a and 220a are Higher than 8.

[0242] After the insulating film 118 is formed, the insulating film 118 is heated by the same heat treatment as the first heat treatment and the second heat treatment described above. A heat treatment (hereinafter referred to as a third heat treatment) may be performed.

[0243] By performing the third heat treatment, oxygen in the insulating film 116 is converted into oxygen from the metal oxide films 108 and 2 The oxygen migrates into the metal oxide films 108 and 208 and compensates for the oxygen vacancies in the metal oxide films 108 and 208 .

[0244] Through the above steps, the display device shown in FIG. 1 can be manufactured.

[0245] <1-7. Display device manufacturing method 2> A method for manufacturing the display device shown in FIG. 4 will be described. The display device shown in FIG. As in the display device, the insulating film 116 is formed. Next, the insulating film 119 is formed in the pixel portion. After a photosensitive resin is applied onto the insulating film 116, exposure and development are performed to form an insulating film 119. Alternatively, a non-photosensitive resin may be applied onto the insulating film 116 and then baked. Next, a resist mask is formed, and the non-photosensitive resin that has been baked using the resist mask is etched. By etching, the insulating film 119 can be formed.

[0246] Next, a conductive film 120 is formed over the insulating film 116 and the insulating film 119 in the same manner as in the display device shown in FIG. When the conductive film 120a_1 is formed, the insulating film 11 Oxygen can be added to the insulating film 116 and the insulating film 114 of the transistor 100. The metal oxide film 108 of the transistor 200A and the metal oxide film 208 of the transistor 200B are reduced in oxygen vacancies. It is possible to reduce

[0247] Next, on the insulating film 116, the insulating film 119, the conductive film 120a_1, and the conductive film 220a_1, An insulating film 118 is formed on the insulating film 118. Note that if either hydrogen or nitrogen is contained in the insulating film 118, Or, both may penetrate into the conductive films 120a_1 and 220a_1. In this case, Oxygen deficiency and either hydrogen or nitrogen in the conductive films 120a_1 and 220a_1, or By bonding the two together, the resistance of the conductive films 120a_1 and 220a_1 is reduced. As a result, the conductive films 120a and 220a can be formed with reduced resistance. Either or both of hydrogen and nitrogen contained in 118 are transferred to the conductive films 120a and 220a. By the movement, the hydrogen concentration and / or the nitrogen concentration of the conductive films 120a and 220a , higher than the metal oxide films 108 and 208.

[0248] After that, a part of the insulating film 118 that overlaps with the conductive film 220a may be etched. .

[0249] Through the above steps, the display device shown in FIG. 4 can be manufactured.

[0250] <1-8. Display device manufacturing method 3> A method for manufacturing the display device shown in FIG. 8 will be described. First, a conductive film is formed on a substrate 102. The conductive film is then processed by a lithography process and an etching process to form a transistor 10. The conductive film 104 functions as a first gate electrode of the transistor 200A. A conductive film 204 having a function as a gate electrode and a capacitance wiring 205 are formed. An insulating film 106 having a function as a first gate insulating film is formed on the conductive film 104. Then, metal oxide films 108, 208, and 209 are formed on the insulating film 106 (FIG. 11(A-1) 11B-1). Note that the metal oxide film 209_1 and the metal oxide film 209_ 2 constitutes an island-shaped metal oxide film 209.

[0251] After the metal oxide films 108, 208, and 209 are formed, a first heat treatment is performed. Good too.

[0252] Next, the conductive film 112a and the conductive film 112b are formed over the metal oxide film 108. A conductive film 212a is formed on the metal oxide film 208, and a conductive film 212 is formed on the metal oxide films 208 and 209. b is formed (see FIG. 11(A-2) and FIG. 11(B-2)).

[0253] Next, the metal oxide films 108, 208, and 209 and the conductive films 112a, 112b, and 212 An insulating film 114 and an insulating film 116 are formed on the insulating films 212a and 212b (FIG. 12(A-1), FIG. 1 2(B-1)). Note that the insulating film 114 and the insulating film 116 have an opening 117. In the opening 117, the metal oxide film 209 is exposed.

[0254] Next, a conductive film 120a is formed on the insulating film 116. Next, the insulating film 114 and the insulating film 11 6. Forming an insulating film 118 on the conductive film 120a, the conductive film 212b, and the metal oxide film 209 (see FIG. 12A-2 and FIG. 12B-2). Note that hydrogen and Either or both of the nitrogen atoms may penetrate into the metal oxide film 209. In this case, oxygen vacancies in the metal oxide film 209 are bonded to either hydrogen or nitrogen or both. This reduces the resistance of the metal oxide film, resulting in the conductive film 210. The conductive film 210 is composed of the insulating film 118 and the conductive film 210_2. Either or both of the hydrogen and nitrogen contained therein are transferred to the conductive film 210, so that the conductive film The hydrogen concentration and / or nitrogen concentration of the film 210 is higher than that of the metal oxide films 108, 208. expensive.

[0255] After that, the insulating film 118 may be etched in a portion that overlaps with the conductive film 210 ( See Figures 13(A-1) and 13(B-1).

[0256] Through the above steps, the display device shown in FIG. 8 can be manufactured.

[0257] By the steps shown in FIG. 12(A-2) and FIG. 12(B-2), the display device shown in FIG. can be produced.

[0258] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0259] (Embodiment 2) In this embodiment, a metal oxide film of one aspect of the present invention will be described with reference to FIGS. 18 to 20. This will be described with reference to FIGS. 18 to 20.

[0260] <Configuration of CAC-OS> Hereinafter, the details of the metal oxide having a CAC structure that can be used in the transistor disclosed in one aspect of the present invention will be described. Here, the metal oxide having a CAC structure will be described using CAC-OS as a representative example. will be described using CAC-OS as a representative example.

[0261] That is, as shown in FIG. 3, for example, in CAC-OS, the elements constituting the metal oxide are unevenly distributed to form regions 001 and 002 mainly composed of each element, and each region is mixed and formed or dispersed in a mosaic pattern. That is, the elements constituting the metal oxide are unevenly distributed in a size of 0.5 nm or more and 10 nm or less, preferably 0.5 nm or more and 3 nm or less, or in the vicinity thereof This is one configuration of the material.

[0262] The region where a specific element is unevenly distributed has its physical properties determined by the properties of the element. For example a region where an element that tends to be an insulator among the elements constituting the metal oxide is unevenly distributed becomes a dielectric region. On the other hand, a region where an element that tends to be a conductor among the elements constituting the metal oxide is unevenly distributed becomes a conductor region. Further, by mixing the conductor region and the dielectric region in a mosaic pattern, the material functions as a semiconductor.

[0263] That is, the metal oxide in one aspect of the present invention is a matrix composite or a metal matrix composite in which materials having different physical properties are mixed. It is a kind of material.

[0264] Note that the oxide semiconductor preferably contains at least indium. In addition to these, it is preferable that the element M (M is gallium, aluminum, etc.) is contained. Minium, silicon, boron, yttrium, copper, vanadium, beryllium, titanium, iron , nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium , hafnium, tantalum, tungsten, magnesium, or The present invention may include a plurality of types of the above-mentioned compounds.

[0265] For example, CAC-OS in In-Ga-Zn oxide (In- The Ga-Zn oxide may be specifically referred to as CAC-IGZO. (hereinafter referred to as InO X1 (X1 is a real number greater than 0.) or Indium Zinc Oxide (hereinafter, In X2 Zinc Y2 O Z2 (X2, Y2, and Z2 are real numbers greater than 0) ) and gallium oxide (GaO X3 (X3 is a real number greater than 0) ), or gallium zinc oxide (Ga X4 Zinc Y4 O Z4 (X4, Y4, and Z1 and Z2 are real numbers greater than 0.) The material is separated into a mosaic pattern. The mosaic-like InO X1 , or In X2 Zinc Y2 O Z2 is uniformly distributed in the film. This is a configuration (hereinafter also referred to as a cloud-like configuration).

[0266] In other words, CAC-OS is X3 The region where In is the main component andX2 Zinc Y2 O Z2 , or InO X1 A composite oxide semiconductor having a structure in which a region in which In this specification, for example, the number of In atoms relative to the element M in the first region is The ratio of the number of atoms of In to the element M in the first region is greater than the atomic ratio of In to the element M in the second region. It is assumed that the concentration of In is higher than that of the second region.

[0267] Note that IGZO is a common name and refers to a compound made of In, Ga, Zn, and O. A typical example is InGaO3(ZnO). m1 (m1 is a natural number), or In ( 1+x0) Ga (1-x0) O3(ZnO) m0 (-1≦x0≦1, m0 is an arbitrary number) Examples of the crystalline compounds include those which are

[0268] The crystalline compound has a single crystal structure, a polycrystalline structure, or a CAAC structure. The CAAC structure is a structure in which multiple IGZO nanocrystals have a c-axis orientation and are aligned on the ab plane. In the case of ZnO, the crystal structure is non-oriented and connected.

[0269] On the other hand, CAC-OS refers to the material composition of an oxide semiconductor. In a material composition containing Ga, Zn, and O, a nanoparticle-like region in which Ga is the main component is In some areas, nanoparticle regions mainly composed of In were observed, and mosaic-like regions were observed. Therefore, in CAC-OS, the crystal structure is It is an element of this.

[0270] Note that CAC-OS does not include a laminated structure of two or more types of films with different compositions. . For example, a structure composed of two layers, a film mainly composed of In and a film mainly composed of Ga, is not included.

[0271] Note that GaO X3 in the region where it is the main component and In X2 Zn Y2 O Z2 , or InO X1 in the region where it is the main component may not have a clear boundary.

[0272] Note that when one or more selected from aluminum, silicon, boron, yttrium, copper, barium, sodium, beryllium, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, or magnesium etc. are included, CAC-OS has a structure in which nano-particle-like regions mainly composed of the element are observed in part and nano-particle-like regions mainly composed of In are observed in part, and they are randomly dispersed in a mosaic pattern.

[0273] <Analysis of CAC-OS> Subsequently, the results of measurements of the oxide semiconductor formed on the substrate using various measurement methods will be described.

[0274] ≪Configuration and Fabrication Method of Samples≫ Hereinafter, nine samples according to one aspect of the present invention will be described. Each sample is fabricated under different conditions of the substrate temperature and the oxygen gas flow ratio when forming the oxide semiconductor. Note that the sample has a structure including a substrate and an oxide semiconductor on the substrate.

[0275] The preparation method of each sample will be described.

[0276] First, a glass substrate is used as the substrate. Then, the glass is A 100 nm-thick In-Ga-Zn oxide is formed as an oxide semiconductor on a silicon substrate. The deposition conditions were a pressure of 0.6 Pa in the chamber and an oxide target. (In:Ga:Zn=4:2:4.1 [atomic ratio]) was used. An AC power of 2500 W is supplied to an oxide target placed in the chamber.

[0277] As a condition for forming an oxide film, the substrate temperature is set to a temperature at which the substrate is not intentionally heated (hereinafter (also called room temperature or RT), 130°C, or 170°C. The flow rate ratio of oxygen gas to the mixed gas of the raw material (hereinafter referred to as the oxygen gas flow rate ratio) is set to 10%. , 30%, or 100%, resulting in nine samples.

[0278] <Analysis by X-ray diffraction> In this section, X-ray diffraction (XRD) was performed on nine samples. The results of the measurement are described below. The XRD device used was a Bruker product. D8 ADVANCE was used. The conditions were θ / In 2θ scan, the scanning range is 15 deg. to 50 deg., and the step width is 0.02d. For example, the scanning speed was 3.0 deg. / min.

[0279] Figure 18 shows the results of measuring the XRD spectrum using the out-of-plane method. In addition, in Fig. 18, the upper row shows the measurement results for a sample where the substrate temperature during film formation was 170°C. The middle row shows the measurement results for a sample with a substrate temperature of 130°C during film formation, and the lower row shows the film formation The left column shows the results of measurements taken with the substrate temperature at RT. The center column shows the results of measurements taken with the gas flow rate ratio at 10%. The right column shows the results for the sample with a 30% oxygen gas flow rate, and the right column shows the results for the sample with a 100% oxygen gas flow rate. The measurement results are shown below.

[0280] The XRD spectrum shown in FIG. 18 shows that the increase in the substrate temperature during film formation or the decrease in the amount of acid during film formation By increasing the ratio of the atomic gas flow rate, the peak intensity around 2θ=31° becomes higher. The peak near 2θ=31° indicates that the c-axis is oriented in the direction approximately perpendicular to the surface on which the film is formed or the upper surface. The c-axis aligned crystal of IGZO compound (CAAC) It is also called line-IGZO.

[0281] In addition, the XRD spectrum shown in FIG. 18 shows that the substrate temperature during film formation was low or the oxygen gas The smaller the flow rate ratio, the less clear the peak. Alternatively, the sample with a small oxygen gas flow rate ratio had ab-plane and c-axis orientations in the measurement area. It is clear that it cannot be seen.

[0282] Analysis by electron microscope In this section, the samples were prepared at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. ,HAADF(High-Angle Annular Dark Field)-ST EM(Scanning Transmission Electron Micros) The results of the observation and analysis using HAADF-ST are described below. Images obtained by EM are also called TEM images.

[0283] Planar images obtained by HAADF-STEM (hereinafter also referred to as planar TEM images), and The results of image analysis of the cross-sectional images (hereinafter also referred to as cross-sectional TEM images) will be described. The TEM images were observed using a spherical aberration correction function. The image was taken using an atomic resolution analytical electron microscope JEM-ARM200F manufactured by JEOL Ltd. The specimen was irradiated with an electron beam having an accelerating voltage of 200 kV and a beam diameter of approximately 0.1 nmφ.

[0284] FIG. 19(A) shows a sample prepared at a substrate temperature of RT during film formation and an oxygen gas flow rate of 10%. FIG. 19(B) shows the relationship between the substrate temperature RT and the oxygen gas flow rate during film formation. This is a cross-sectional TEM image of a sample prepared with a 10% concentration ratio.

[0285] <Analysis of electron diffraction patterns> In this section, the samples were prepared at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. By irradiating the electron beam with a probe diameter of 1 nm (also called nano-beam electron beam), The results of the obtained X-ray diffraction patterns will now be described.

[0286] As shown in FIG. 19(A), the substrate temperature during film formation was RT, and the oxygen gas flow rate ratio was 10%. In the planar TEM image of the sample, black spots a1, a2, a3, a4, and a5 are The electron beam diffraction pattern shown in FIG. 5 is observed. While irradiating the area, move the area from the 0 second position to the 35 second position at a constant speed. The results of black point a1 are shown in Fig. 19(C), the results of black point a2 are shown in Fig. 19(D), and the results of black point a3 are shown in Fig. 19(E). ), the results for black point a4 are shown in FIG. 19(F), and the results for black point a5 are shown in FIG. 19(G).

[0287] From Fig. 19(C), Fig. 19(D), Fig. 19(E), Fig. 19(F), and Fig. 19(G), A bright area can be observed in a circular (ring-like) pattern. Several spots can be observed.

[0288] In addition, as shown in FIG. 19(B), when the substrate temperature RT during film formation and the oxygen gas flow rate ratio were 10%, In the cross-sectional TEM image of the prepared sample, black spots b1, b2, b3, b4, and Observe the electron diffraction pattern indicated by black spot b5. The results of black spot b1 are shown in Figure 19(H), and black spot b The results of black point b2 are shown in Fig. 19(I), the results of black point b3 are shown in Fig. 19(J), and the results of black point b4 are shown in Fig. 19(K). ), and the results for black point b5 are shown in Figure 19(L).

[0289] From Fig. 19(H), Fig. 19(I), Fig. 19(J), Fig. 19(K), and Fig. 19(L), A ring-shaped area of ​​high brightness can be observed. Also, multiple spots can be observed in the ring-shaped area. can.

[0290] For example, for a CAAC-OS having an InGaZnO4 crystal, When an electron beam with a probe diameter of 300 nm is incident on the row, the (00 9) The diffraction pattern includes spots due to the CAAC-OS It has been found that the film has a c-axis orientation, and the c-axis is oriented in a direction substantially perpendicular to the surface on which the film is formed or the upper surface. On the other hand, an electron beam with a probe diameter of 300 nm is incident perpendicularly to the surface of the same sample. In other words, the CAAC-OS has a ring-shaped diffraction pattern along the a-axis and b-axis. It can be seen that the axis has no orientation.

[0291] In addition, a nanocrystalline oxide semiconductor nc-OS) with a large probe diameter When electron diffraction is performed using an electron beam (e.g., 50 nm or larger), a halo pattern is observed. A diffraction pattern is observed. In addition, a small probe diameter electron beam (e.g. When nanobeam electron diffraction is performed using a material with a diameter of less than 50 nm, bright spots are observed. In addition, when nanobeam electron diffraction was performed on the nc-OS, a circular (ring-shaped) In some cases, a bright area is observed. In addition, multiple bright spots are observed in a ring-shaped area. It may be measured.

[0292] Electron beam diffraction patterns of the sample prepared at the substrate temperature RT and oxygen gas flow rate of 10% during film formation. The turn has a ring-shaped area of ​​high brightness and multiple bright points in the ring area. The sample was fabricated at a substrate temperature of RT and an oxygen gas flow rate of 10%. The turns become nc-OS, and have no orientation in the planar and cross-sectional directions.

[0293] From the above, oxide semiconductors formed at low substrate temperatures or with a small oxygen gas flow rate are The oxide semiconductor film has a structure that is clearly different from that of an amorphous oxide semiconductor film and that of a single crystal oxide semiconductor film. It can be assumed that the substance has the following properties.

[0294] ≪Elemental analysis≫ In this article, we will discuss energy dispersive X-ray spectroscopy (EDX). EDX mapping was obtained and evaluated using vective X-ray spectroscopy. By evaluating the film formation temperature, the film was formed at a substrate temperature of RT and an oxygen gas flow rate of 10%. The results of elemental analysis of the sample are described below. Note that the EDX measurement was performed using an elemental analyzer and The energy dispersive X-ray analyzer JED-2300T manufactured by JEOL Ltd. is used. A Si drift detector is used to detect the X-rays emitted from the sample.

[0295] In EDX measurement, each point in the analysis area of ​​the sample is irradiated with an electron beam, The energy and frequency of the characteristic X-rays of the sample are measured, and the EDX spectrum corresponding to each point is obtained. In this embodiment, the peaks in the EDX spectrum at each point are determined as electron transitions to the L shell of the In atom. electron transition to the K shell of Ga atom, electron transition to the K shell of Zn atom, and electron transition to the K shell of O atom The ratio of each atom at each point is calculated. By performing EDX analysis on the target area, an EDX map showing the distribution of the ratio of each atom is obtained. It is possible.

[0296] FIG. 20 shows the results of the sample fabricated at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. FIG. 20(A) shows the EDX mapping of Ga atoms ( The ratio of Ga atoms to the total atoms is in the range of 1.18 to 18.64 [atomic%]. FIG. 20(B) shows the EDX mapping of In atoms (the ratio of In atoms to the total atoms). The ratio is in the range of 9.28 to 33.74 [atomic%]. C) EDX mapping of Zn atoms (ratio of Zn atoms to total atoms is 6.69 to 2. 4.99 [atomic%] range.) Also, Fig. 20(A) and Fig. 20(B) ), and FIG. 20(C) are fabricated at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. The EDX mapping shows the same area in the cross section of the sample. The more the measured element, the brighter the light, and the less the measured element, the darker the light. The EDX mapping shown in Figure 20 was taken at a magnification of 7.2 million times. be.

[0297] In the EDX mapping shown in FIG. 20(A), FIG. 20(B), and FIG. 20(C), The relative distribution of light and dark can be seen. The substrate temperature during film formation is RT, and the oxygen gas flow rate is 10%. In the prepared sample, it can be seen that each atom exists with its own distribution. The areas surrounded by solid lines and the areas surrounded by dashed lines shown in Figures 20(A), 20(B), and 20(C) Focus on.

[0298] In FIG. 20(A), the area enclosed by the solid line contains many relatively dark areas, and the area enclosed by the dashed line contains many relatively dark areas. In FIG. 20B, the area surrounded by the solid line contains many relatively bright areas. The area surrounded by the dashed line contains many relatively bright areas, while the area surrounded by the dashed line contains many relatively dark areas.

[0299] In other words, the area surrounded by the solid line is the area with a relatively large amount of In atoms, and the area surrounded by the dashed line is the area with a relatively large amount of In atoms. This is a region with relatively few atoms. In FIG. 20(C), the area surrounded by the solid line The right side is a relatively bright area, and the left side is a relatively dark area. The range is In X2 Zinc Y2 O Z2 , or InO X1 This is an area where the main components are:

[0300] The area surrounded by the solid line is the area with relatively few Ga atoms, and the area surrounded by the dashed line is the area with relatively few Ga atoms. In Figure 20(C), the upper left area in the area enclosed by the dashed line is The upper right area is a relatively bright area, and the lower right area is a relatively dark area. The area enclosed by the dashed line is GaO X3 , or Ga X4 Zinc Y4 O Z4 Areas where the main components are It is.

[0301] In addition, from Fig. 20(A), Fig. 20(B), and Fig. 20(C), the distribution of In atoms is The atoms are relatively uniformly distributed, and the InO X1 The region where is the main component is In X2 Zinc Y2 O Z2 It appears that the layers are connected to each other through the regions where In this way, X2 Zinc Y2 O Z2 , or InO X1 The area where is the main component is It is formed in a loud, spreading shape.

[0302] Thus, GaO X3 The main components are In X2 Zinc Y2 O Z2 ,or InO X1 In-Ga-Z The n-oxide can be referred to as CAC-OS.

[0303] The crystal structure of CAC-OS is an nc structure. The c-structure is IGZO including single crystal, polycrystal, and CAAC structures in the electron diffraction pattern. In addition to the bright spots caused by In addition to several bright spots, a ring-shaped area of ​​high brightness appears, indicating crystallization. The structure is defined.

[0304] In addition, from FIG. 20(A), FIG. 20(B), and FIG. 20(C), GaO X3 The main components are and In X2 Zinc Y2 O Z2 , or InO X1 The size of the area where is the principal component The size of the defects observed is 0.5 nm to 10 nm, or 1 nm to 3 nm. Preferably, in the EDX mapping, the diameter of the region in which each element is the main component is 1 nm or more. The thickness should be 2 nm or less.

[0305] From the above, it can be seen that CAC-OS has a structure different from that of IGZO compounds in which metal elements are uniformly distributed. and has properties different from those of IGZO compounds. X3 N The regions where In is the main component and X2 Zinc Y2 O Z2 , or InO X1 The area where is the main component The structure is such that the regions having each element as a main component are in a mosaic pattern.

[0306] Here, In X2 Zinc Y2 O Z2 , or InO X1 The area where GaO is the main component X This is a region with high conductivity compared to the region where In 3 is the main component. X2 Zinc Y2 O Z2 , or InO X1 The carriers flow through the area where the main component is oxygen. Therefore, the conductivity of In is expressed as a semiconductor. X2Zinc Y2 O Z2 , or InO X1 The region where the main component is a metal is distributed in a cloud-like shape in the oxide semiconductor, which results in a high electric field efficiency. As a result, a high mobility (μ) can be achieved.

[0307] On the other hand, GaO X3 The region where the main components are In X2 Zinc Y2 O Z2 , or InO X1 This region has higher insulating properties than the region where GaO is the main component. X3 etc. By distributing the region in which the main component is Switching operation can be achieved.

[0308] Therefore, when CAC-OS is used in a semiconductor device, GaO X3 Insulation and , In X2 Zinc Y2 O Z2 , or InO X1 The conductivity caused by the This results in a high on-state current (I on ) and high field-effect mobility (μ) can.

[0309] In addition, semiconductor devices using CAC-OS have high reliability. It is ideal for a variety of semiconductor devices including displays.

[0310] <Transistors with metal oxide films> Next, the case where the metal oxide film is used for a transistor will be described.

[0311] By using the above metal oxide film in a transistor, the carrier mobility is high and In this way, a transistor with high switching characteristics can be realized. A transistor can be realized.

[0312] In addition, a metal oxide film having a low carrier density is preferably used for the transistor. For example, a metal oxide film has a carrier density of 8×10 11 / cm 3 Less than 1x1 0 11 / cm 3 less than 1×10 10 / cm 3 Less than 1 x 10 -9 / cm 3 That should be enough.

[0313] In the case of lowering the carrier density of the metal oxide film, the impurity concentration in the metal oxide film In this specification and the like, the impurity concentration is low and the defect level density is low. A low density of recessed levels is called high purity intrinsic or substantially high purity intrinsic. Metal oxide films that are essentially high-purity intrinsic have a low carrier density because they have few carrier sources. In addition, the high purity intrinsic or substantially high purity intrinsic metal oxide can be used. Because the film has a low density of defect states, it may also have a low density of trap states.

[0314] In addition, the time it takes for the charges trapped in the trap levels of the metal oxide film to disappear is Therefore, the trap level density is high. In a transistor in which a channel region is formed in a thin oxide semiconductor, the electrical characteristics may become unstable. There is a match.

[0315] Therefore, in order to stabilize the electrical characteristics of the transistor, the impurity concentration in the metal oxide film In order to reduce the impurity concentration in the metal oxide film, It is preferable to reduce the impurity concentration in the adjacent film. These include alkali metals, alkaline earth metals, iron, nickel, silicon, etc.

[0316] Here, the influence of each impurity in the metal oxide film will be described.

[0317] When a metal oxide film contains silicon or carbon, which is one of the group 14 elements, oxidation occurs. Defect levels are formed in oxide semiconductors. The concentration of silicon and carbon near the interface with the oxide semiconductor (obtained by SIMS) The concentration of 18 atoms / cm 3 Less than or equal to 2×10 17 atoms / cm 3 The following applies.

[0318] In addition, when an alkali metal or an alkaline earth metal is contained in the metal oxide film, the defect level is increased. Therefore, alkali metals or alkaline earth metals A transistor using a metal oxide film containing such a metal oxide tends to have normally-on characteristics. Therefore, it is possible to reduce the concentration of alkali metals or alkaline earth metals in the metal oxide film. Specifically, the alkali metal or The concentration of alkaline earth metals is 1×10 18 atoms / cm 3 Less than or equal to 2×10 16 atoms / cm 3 The following applies.

[0319] In addition, when nitrogen is contained in a metal oxide film, electrons that act as carriers are generated, and the carriers The nitrogen density increases and it becomes easier to make the oxide semiconductor n-type. Therefore, the transistor used in the oxide semiconductor In this case, it is preferable that the nitrogen content is reduced as much as possible. For example, the nitrogen content in the oxide semiconductor is The concentration is 5×10 19 atoms / cm 3 Less than 5 x 10 18 atoms / cm 3 Less than or equal to 1×10 18 atoms / cm 3 Below, More preferably 5×10 17 atoms / cm 3 The following applies.

[0320] In addition, hydrogen contained in the metal oxide film reacts with oxygen that bonds with metal atoms to form water. Therefore, oxygen deficiency (V o ) may be formed. o ) hydrogen enters, In some cases, electrons that act as carriers are generated. In other cases, some of the hydrogen atoms bond with metal atoms. It can combine with other elements to produce electrons, which act as carriers. Therefore, hydrogen is included. A transistor using an oxide semiconductor tends to be normally on. It is preferable that the hydrogen content in the oxide semiconductor is reduced as much as possible. The hydrogen concentration obtained by SIMS in the body is 1×10 20 atoms / cm 3 less than , preferably 1 x 10 19 atoms / cm 3 less than 5×10 18 ato ms / cm 3less than 1×10 18 atoms / cm 3 Less than.

[0321] In addition, oxygen vacancies (V o ) is achieved by introducing oxygen into a metal oxide film. In other words, the oxygen vacancies (V o ) is supplemented with oxygen By this, oxygen vacancies (V o ) disappears. Therefore, oxygen is diffused into the metal oxide film. This reduces the oxygen deficiency (V o ) and improve reliability.

[0322] As a method for introducing oxygen into a metal oxide film, for example, It is possible to provide an oxide that contains more oxygen than the stoichiometric composition. In the oxide, there is a region where oxygen is present in excess of the stoichiometric composition (hereinafter referred to as the excess oxygen region). In particular, a metal oxide film is preferably used for the transistor. In this case, an oxide having an excess oxygen region is provided in the undercoat film near the transistor or in the interlayer film. This reduces oxygen vacancies in the transistor, thereby improving the reliability.

[0323] By using a metal oxide film with sufficiently reduced impurities in the channel formation region of a transistor, This makes it possible to impart stable electrical characteristics.

[0324] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0325] (Embodiment 3) In this embodiment, a display element of a lateral electric field mode (also called a horizontal electric field mode) is used. A display device using a liquid crystal element will be described with reference to FIG.

[0326] FIG. 21 is a flow diagram for explaining the manufacturing process of a display device using a lateral electric field mode liquid crystal element. In FIG. 21, oxide semiconductor (particularly, CAC-OS), low-temperature polysilicon (LTPS (Low Temperature Poly-Silicon)), or When hydrogenated amorphous silicon (a-Si:H) is used for the transistor channel 1 shows an example of a manufacturing process for each of the above.

[0327] <3-1.CAC-OS> The use of CAC-OS in a transistor will be described. A gate electrode (GE) is formed at the position (SP). When processing the gate electrode, one mask is used.

[0328] Next, a gate insulating film (GI) is formed on the gate electrode using a PECVD device. Then, a sputtering device is used to form a silicon sulator on the gate insulating film. An oxide semiconductor (OS) film is formed as an active layer. The oxide semiconductor film is processed into islands. Use one mask when

[0329] Next, a part of the gate insulating film is processed to form an opening that reaches the gate electrode. When forming the opening, one mask is used.

[0330] Next, a conductive film is formed over the gate insulating film and the oxide semiconductor film by using a sputtering apparatus. The conductive film is then processed to form source and drain electrodes (S / D electrodes). In addition, one mask is used when forming the source electrode and the drain electrode.

[0331] Next, a PECVD apparatus is used to form a pas- on the oxide semiconductor film, the source electrode, and the drain electrode. An oxidization film is formed.

[0332] Next, a part of the passivation film is processed to form openings that reach the source and drain electrodes. When forming the opening, one mask is used.

[0333] Next, a film is placed on the passivation film so as to cover the opening formed in the passivation film. A conductive film is formed using a sputtering device, and the conductive film is processed to form a common electrode. When forming the common electrode, one mask is used.

[0334] Next, an insulating film is formed on the passivation film and the common electrode using a PECVD device. Then, a part of the insulating film is opened to form openings reaching the source electrode and the drain electrode. When forming the insulating film (when forming an opening in a part of the insulating film), a mask Use one.

[0335] Next, a conductive film is formed on the insulating film using a sputtering apparatus, and the conductive film is processed. The pixel electrodes are formed by this process. Note that one mask is used to form the pixel electrodes.

[0336] By the above steps, a liquid crystal display device of the in-plane switching mode can be manufactured. When the OS is used, the number of masks required for a lateral electric field mode liquid crystal display device is eight.

[0337] <3-2.LTPS> The case where LTPS is used for a transistor will be described. First, a sputtering device is A light-shielding film is formed using a mask.

[0338] Next, a base insulating film is formed on the light-shielding film using a PECVD device. Using a PECVD device, Si is formed on the film to become the active layer. In order to anneal the material, excimer laser annealing (ELA: Excimer Laser Annealing) is used. After the ELA process, the active layer Si is annealed by crystallizing silicon ( p-Si: poly-Silicon). To perform ELA on a large area, a large In addition, linear irregularities peculiar to ELA may occur.

[0339] Next, the p-Si is processed to form islands. Note that when processing the p-Si into islands, a mask is used. Use one.

[0340] Next, a gate insulating film (GI) is formed on the p-Si using a PECVD device. After that, a gate electrode (GE) is formed on the gate insulating film using a sputtering device. In addition, when forming a gate electrode, one mask is used. Additionally, a part of the gate insulating film is also removed.

[0341] Next, ion doping (ID:Ion Doping) is performed to form an n+ region in the p-Si. The impurity is implanted using a masking device. Next, to form an n-region in the p-Si, an ion doping device is used. When forming the n-region, the impurity is implanted on the entire surface without using a mask. Next, an ion doping device is used to form a p+ region in the p-Si. The impurity is implanted using a mask. do.

[0342] Next, thermal activation is performed. For the thermal activation, an annealing furnace, an RTA device, etc. may be used. stomach.

[0343] Next, an interlayer insulating film is formed on the p-Si and the gate electrode using a PECVD apparatus. Then, the interlayer insulating film and a part of the gate insulating film are processed to form n+ and p+ regions. An opening is formed so as to reach the substrate 1. When forming the opening, one mask is used.

[0344] Next, a conductive film is formed on the interlayer insulating film in which the opening is formed, using a sputtering device. The conductive film is then processed to form source and drain electrodes (S / D electrodes). It should be noted that one mask is used when forming the source electrode and the drain electrode.

[0345] Next, a planarizing insulating film is formed on the source electrode and the drain electrode using a coater device. As the planarizing insulating film, for example, an organic resin film or the like may be used. When forming, one mask is used.

[0346] Next, a conductive film is formed over the planarizing insulating film by using a sputtering apparatus. The common electrode is formed by processing the mask. Use.

[0347] Next, an insulating film is formed on the common electrode using a PECVD apparatus. The insulating film is then partially opened to form openings reaching the source electrode and the drain electrode. When forming an opening in a part of the insulating film, one mask is used.

[0348] Next, a conductive film is formed on the insulating film using a sputtering apparatus, and the conductive film is processed. The pixel electrodes are formed by this process. Note that one mask is used to form the pixel electrodes.

[0349] Through the above steps, a liquid crystal display device of the lateral electric field mode can be manufactured. When using this, the number of masks required for a lateral electric field mode liquid crystal display device is 11.

[0350] <3-3. a-Si:H> The case of using a-Si:H for a transistor will be explained. First, the sputtering equipment The gate electrode (GE) is formed using a mask. Use one.

[0351] Next, a gate insulating film (GI) is formed on the gate electrode using a PECVD apparatus. After that, a silicon (Si) film that will become the active layer is formed on the gate insulating film using a PECVD device. When processing the silicon film into islands, a mask is used.

[0352] Next, a part of the gate insulating film is processed to form an opening that reaches the gate electrode. When forming the opening, one mask is used.

[0353] Next, a conductive film is formed on the gate insulating film by using a sputtering apparatus. The capacitor electrodes are formed by processing the silicon substrate. Use one piece.

[0354] Next, a conductive film is formed on the gate insulating film and the silicon film using a sputtering device. The conductive film is processed to form source and drain electrodes (S / D electrodes). In addition, one mask is used when forming the source electrode and the drain electrode.

[0355] Next, a conductive film is formed on the source electrode and the drain electrode by using a sputtering device. The conductive film is processed to form a common electrode. , use one mask.

[0356] Next, an insulating film is formed on the common electrode using a PECVD apparatus. The insulating film is then opened to form openings that reach the source and drain electrodes. When forming the insulating film (when forming an opening in a part of the insulating film), one mask is used.

[0357] Next, a conductive film is formed on the insulating film using a sputtering apparatus, and the conductive film is processed. The pixel electrodes are formed by this process. Note that one mask is used to form the pixel electrodes.

[0358] By the above process, a liquid crystal display device of the horizontal electric field mode can be manufactured. When using :H, the number of masks required for a lateral electric field mode liquid crystal display device is eight.

[0359] In each flow shown for CAC-OS, LTPS, and a-Si:H, The electrode formation, the insulating film formation on the common electrode, and the pixel electrode formation are performed on the liquid crystal display of the horizontal electric field mode. Due to the process caused by the display device, the liquid crystal element is in the vertical electric field mode (e.g. VA mode, etc.). In the case of a liquid crystal display device or an organic EL element is used as a display element, , may be different processes.

[0360] As shown in FIG. 21, a CAC- By using OS, the manufacturing process can be simplified compared to LTPS. The transistors using AC-OS have the same mask as the transistors using a-Si:H. It can be fabricated in large quantities and has higher mobility than transistors using s-Si:H. Therefore, by using a transistor using CAC-OS, a driver circuit (gate It is possible to implement part or all of the driver (driver, source driver, etc.) in the same way.

[0361] The characteristics of each process are shown in Table 1.

[0362] [Table 1]

[0363] As shown in Table 1, by using CAC-OS, it is possible to fabricate with the same number of masks as a-Si:H. It can be fabricated and has better electrical properties (field effect mobility (also simply called mobility)) than a-Si:H. Therefore, by using CAC-OS, the display quality As shown in Table 1, CAC-OS can achieve high quality display devices. Compared to LTPS, the maximum process temperature is lower, and device and plant costs are also lower. Therefore, it is possible to realize a display device with reduced manufacturing costs.

[0364] Note that a transistor using an oxide semiconductor, such as CAC-OS, is similar to a transistor using silicon. Compared to the transistors used in the past, 1. off-state current is low, 2. there is no short channel effect, and 3. High voltage resistance; and 4. Little change in temperature characteristics. In addition, a transistor using an oxide semiconductor has a higher efficiency than a transistor using silicon. It has the same switching speed and frequency characteristics (also called frequency characteristics) as a transistor. Therefore, high-speed operation is possible. A display device having such a capacitor can achieve high display quality and high reliability.

[0365] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0366] (Embodiment 4) In this embodiment, a display device including the transistor described in the above embodiment will be An example will be described below with reference to FIGS.

[0367] 22 is a top view showing an example of a display device. The display device 700 shown in FIG. A pixel portion 702 is provided on the first substrate 701, and a source driver is provided on the first substrate 701. A pixel portion 702, a source driver circuit portion 704, a gate driver circuit portion 706, A sealant 712 is disposed so as to surround the path portion 704 and the gate driver circuit portion 706. and a second substrate 705 disposed so as to face the first substrate 701. The first substrate 701 and the second substrate 705 are bonded together with a sealant 712 . That is, the pixel section 702, the source driver circuit section 704, and the gate driver circuit section 70 6 is sealed by a first substrate 701 , a sealant 712 and a second substrate 705 . Although not shown in FIG. 22, a display element is provided between the first substrate 701 and the second substrate 705. will be established.

[0368] The display device 700 is surrounded by a sealant 712 on the first substrate 701. A pixel section 702, a source driver circuit section 704, and a gate driver circuit section 705 are arranged in a region different from the region. and a flexible printed circuit (FPC) terminal section 708 (FPC: Flex Also, an FPC terminal portion 708 is provided. An FPC 716 is connected to the pixel section 702 and the source driver circuit. Various signals are supplied to the path section 704 and the gate driver circuit section 706. 702, a source driver circuit section 704, a gate driver circuit section 706, and an FPC terminal section Signal lines 710 are connected to the terminals 708. Various signals are supplied by the FPC 716. The signals are transmitted through a signal line 710 to a pixel section 702, a source driver circuit section 704, a gate driver A driver circuit portion 706 and an FPC terminal portion 708 are provided.

[0369] The display device 700 may include a plurality of gate driver circuits 706. The device 700 includes a source driver circuit section 704 and a gate driver circuit section 706. Although an example in which the pixel portion 702 is formed on the same first substrate 701 is shown, the present invention is not limited to this configuration. For example, only the gate driver circuit section 706 may be formed on the first substrate 701. Alternatively, only the source driver circuit portion 704 may be formed on the first substrate 701. In this case, the substrate on which the source driver circuit or the gate driver circuit is formed (for example, A driving circuit board formed of a monocrystalline semiconductor film or a polycrystalline semiconductor film is formed on a first substrate 701. The method of connecting the separately formed drive circuit board is not particularly limited. Instead, we use COG (Chip On Glass) method, wire bonding method, etc. can be used.

[0370] The display device 700 also includes a pixel portion 702, a source driver circuit portion 704, and a gate The driver circuit section 706 includes a plurality of transistors.

[0371] The display device 700 can also include various elements, such as: For example, electroluminescence (EL) elements (EL elements including organic and inorganic materials, organic EL elements, inorganic EL elements, LEDs, etc.), light-emitting transistor elements (light-emitting elements that emit light according to electric current) transistors, electron emission elements, liquid crystal elements, electronic ink elements, electrophoretic elements, Rowetting element, plasma display panel (PDP), MEMS (microelectromechanical systems) Electro-mechanical systems) displays (e.g., grating light bars) GLV, Digital Micromirror Device (DMD), Digital Microsha (DMS) elements), and piezoelectric ceramic displays.

[0372] An example of a display device using an EL element is an EL display. An example of a display device using emission elements is a field emission display (FE D) or SED type flat panel display (SED: Surface-conductive LCDs are used in LCD displays. An example of a display device that has been used is a liquid crystal display (transmissive liquid crystal display, semi-transmissive liquid crystal display, etc.). LCD, reflective LCD, direct-view LCD, projection LCD Examples of display devices using electronic ink elements or electrophoretic elements include Examples of such displays include electronic paper. Semi-transmissive LCD displays and reflective LCD displays are also available. In order to realize the above-mentioned, a part or the whole of the pixel electrode has a function as a reflective electrode. For example, a part or the whole of the pixel electrode may be made of aluminum, silver, etc. In this case, a memory such as an SRAM may be provided under the reflective electrode. It is also possible to provide a circuit, which can further reduce power consumption. .

[0373] The display method of the display device 700 may be a progressive method or an interlace method. In addition, the color elements controlled by pixels when displaying in color are R It is not limited to the three colors GB (R stands for red, G stands for green, B stands for blue). For example, It may be composed of four pixels: a pixel, a pixel, and a pixel of white (W). As in the column, two colors of RGB form one color element, and different two colors are generated depending on the color element. You can also select colors to configure the color. Or, you can select one or more colors such as yellow, cyan, and magenta for RGB. The size of the display area may be different for each dot of the color element. However, the disclosed invention is not limited to color display devices, and may be used in monochrome display devices. The present invention can also be applied to display devices.

[0374] Also, white light is emitted from the backlight (organic EL element, inorganic EL element, LED, fluorescent lamp, etc.) In order to display full color using (W), a colored layer (also called a color filter) is The colored layer may be, for example, red (R), green (G), blue (B), or red (C). ), yellow (Y), etc. can be used in appropriate combination. In this case, the color reproducibility can be improved compared to when no color layer is used. By disposing a region having a color layer and a region not having a color layer, The white light in the region may be directly used for display. By placing the colored layer over the entire display, the decrease in brightness caused by the colored layer can be reduced during bright display, and power consumption can be reduced by 2. However, in some cases, the emission of light from organic EL elements and inorganic EL elements can be reduced by about 10 to 30%. When using optical elements to display full color, R, G, B, Y, and W are each emitted in different colors. By using a self-luminous element, it is possible to obtain a light emission from a colored layer. In some cases, power consumption can be reduced even further.

[0375] In addition, the colorization method involves passing a portion of the white light through a color filter. In addition to the color filter method, which converts the light into red, green, and blue by filtering the light, A method that uses each color of light (three-color method), or converts part of the blue light into red or green A method for achieving this (color conversion method, quantum dot method) may be applied.

[0376] In this embodiment, a liquid crystal element and an EL element are used as display elements. 23 to 28. Note that FIG. 23 to FIG. 25 and FIG. 27 are the same as FIG. 22. 1 is a cross-sectional view taken along dashed line QR shown in FIG. 1, and shows a configuration in which a liquid crystal element is used as a display element. 26 and 28 are cross-sectional views taken along the dashed line QR shown in FIG. The device is configured using an EL element.

[0377] First, the common parts shown in FIGS. 23 to 28 will be explained, and then the different parts will be explained. This will be explained below.

[0378] <4-1. Explanation of common parts of display device> A display device 700 shown in FIGS. 23 to 28 includes a wiring portion 711 and a pixel portion 702. The display panel 700 includes a source driver circuit section 704 and an FPC terminal section 708. The line portion 711 includes a signal line 710. The pixel portion 702 includes a transistor 750 and The source driver circuit portion 704 includes a transistor It has 752.

[0379] Transistor 750 and transistor 752 are similar to transistor 100D shown above. However, the transistor 750 does not have a second gate electrode. The transistor 750 and the transistor 752 may have the same configuration as those described in the above embodiment. Other transistors may also be used.

[0380] The transistor used in this embodiment is a metal oxide semiconductor having a high purity and in which the formation of oxygen vacancies is suppressed. The off-state current of the transistor can be reduced. This allows the retention time of electrical signals such as the EEPROM to be extended, and the write interval can be extended when the power is on. This allows the frequency of refresh operations to be reduced, resulting in reduced power consumption. This has the effect of suppressing the above.

[0381] In addition, the transistor used in this embodiment has a relatively high field-effect mobility. For example, a transistor capable of such high speed operation can be used for a liquid crystal display. By using this in a display device, the switching transistor in the pixel section and the driver circuit section In other words, the driver transistor can be formed on the same substrate as the driver circuit. Therefore, it is not necessary to use a semiconductor device formed from a silicon wafer or the like. The number of components can be reduced. By using a register, a high quality image can be provided.

[0382] 23 to 28, the transistor 750 and the A transistor having the same structure as the transistor 752 included in the source driver circuit portion 704 is used. The configuration used is illustrated above, but is not limited to this. For example, A transistor different from that in the driver circuit section 704 may be used. 02 is a staggered transistor, and the source driver circuit portion 704 is In the pixel portion 702, an inverted staggered transistor is used. A reverse staggered transistor is used, and a staggered transistor is provided in the source driver circuit section 704. The source driver circuit section 704 may be configured as a gate driver. It may also be read as a driver circuit section.

[0383] The signal line 710 is connected to the source and drain electrodes of the transistors 750 and 752. The signal line 710 is formed through the same process as the conductive film having the function of the signal line 710. When materials containing copper are used, signal delays caused by wiring resistance are reduced, and the display is easier to see on a large screen. It becomes possible to show

[0384] The FPC terminal portion 708 includes a connection electrode 760, an anisotropic conductive film 780, and an FPC 71. 6. The connection electrode 760 is connected to the source and drain electrodes of the transistors 750 and 752. The connection electrode 7 is formed in the same process as the conductive film that functions as the drain electrode. 60 is electrically connected to a terminal of the FPC 716 via an anisotropic conductive film 780. .

[0385] The first substrate 701 and the second substrate 705 may be, for example, a glass substrate. In addition, the first substrate 701 and the second substrate 705 may be flexible substrates. The flexible substrate may be, for example, a plastic substrate. do.

[0386] In addition, a structure 778 is provided between the first substrate 701 and the second substrate 705. The structure 778 is a columnar spacer obtained by selectively etching an insulating film. A device for controlling the distance (cell gap) between the first substrate 701 and the second substrate 705 is provided. In addition, a spherical spacer may be used as the structure 778.

[0387] In addition, on the second substrate 705 side, a light-shielding film 73 having a function as a black matrix is ​​provided. 8, a colored film 736 having a function as a color filter, a light-shielding film 738 and a colored film 7 An insulating film 734 is provided in contact with 36 .

[0388] <4-2. Configuration examples of display devices using liquid crystal elements> The display device 700 shown in FIG. 23 includes a liquid crystal element 775. The liquid crystal element 775 includes a conductive film The conductive film 774 is a second substrate 705. The display device 700 shown in FIG. The alignment state of the liquid crystal layer 776 changes depending on the voltage applied to the conductive film 772 and the conductive film 774. The light transmission or non-transmission can be controlled to display images.

[0389] The conductive film 772 serves as a source electrode and a drain electrode of the transistor 750. The conductive film 772 is electrically connected to a conductive film having the functions of the transistor 750. A pixel electrode formed on the gate insulating film, i.e., a function as one electrode of a display element. The conductive film 772 also functions as a reflective electrode. 00 uses external light, reflects the light on the conductive film 772, and displays the light through the colored film 736. It is a reflective color liquid crystal display device.

[0390] The conductive film 772 may be a conductive film that transmits visible light or a conductive film that reflects visible light. A conductive film having a reflectivity can be used. For example, a material containing one of the elements indium (In), zinc (Zn), and tin (Sn) As a conductive film that is reflective in visible light, for example, aluminum In this embodiment, the conductive film 772 may be formed of A conductive film that is reflective in visible light is used.

[0391] As shown in FIG. 24, in the pixel portion 702, an insulating film having a function as a planarizing film is An insulating film 770 may be formed. A conductive film 772 may be formed over the insulating film 770. In addition, an insulating film 735 having an opening is formed over the conductive film 772 .

[0392] The display device 700 shown in FIGS. 23 and 24 is a reflective color liquid crystal display device. However, the present invention is not limited to this. For example, the conductive film 772 may be a light-transmitting film that transmits visible light. By using a certain conductive film, a transmissive color liquid crystal display device may be formed. A so-called semi-transmissive type is a combination of a color liquid crystal display device of the type 1 and a transmissive color liquid crystal display device. The display device may be a color liquid crystal display device.

[0393] An example of a transmissive color liquid crystal display device is shown in FIG. 25. FIG. 25 shows the same as that shown in FIG. This is a cross-sectional view taken along the dashed line QR, and shows a configuration in which liquid crystal elements are used as display elements. In addition, the display device 700 shown in FIG. 25 uses a horizontal electric field method (for example, F This is an example of a configuration using FS (Fringe Field Switching) mode. In the case of the structure shown in FIG. 25, an insulating film is formed on a conductive film 772 having a function as a pixel electrode. A conductive film 774 is provided over the insulating film 773. The insulating film 773 is formed on the conductive layer 4. The conductive layer 4 functions as a common electrode. The alignment state of the liquid crystal layer 776 is controlled by the electric field generated between the conductive film 772 and the conductive film 774. It is possible.

[0394] Although not shown in FIGS. 23 to 25, the conductive film 772 or the conductive film 774 An alignment film is provided on either one or both of the surfaces of the liquid crystal layer 776. 23 to 25, a polarizing member, a phase difference member, a reflecting member, etc. Optical members (optical substrates) such as a polarizing substrate and a positioning member may be provided as appropriate. Circularly polarized light produced by a retardation substrate may be used. Either may be used.

[0395] When liquid crystal elements are used as display elements, thermotropic liquid crystal, low molecular weight liquid crystal, high molecular weight liquid crystal, For example, a liquid crystal, a polymer-dispersed liquid crystal, a ferroelectric liquid crystal, an antiferroelectric liquid crystal, etc. can be used. Depending on the conditions, the liquid crystal material can have a cholesteric phase, a smectic phase, a cubic phase, or a chiral phase. It shows nematic phase, isotropic phase, etc.

[0396] In addition, when the in-plane switching method is adopted, liquid crystal that exhibits a blue phase without using an alignment film may be used. The blue phase is one of the liquid crystal phases. When the temperature of a cholesteric liquid crystal is increased, the cholesteric The blue phase appears just before the transition from the black phase to the isotropic phase. In order to improve the temperature range, a liquid crystal composition containing a chiral agent of several weight percent or more is used. The liquid crystal composition containing the liquid crystal exhibiting the blue phase and the chiral agent is used in the liquid crystal layer. Since the liquid crystal display has a short rotational angle and is optically isotropic, no alignment treatment is required. Since the rubbing process is unnecessary, electrostatic damage caused by the rubbing process is prevented. This can prevent the occurrence of defects or damage to the liquid crystal display device during the manufacturing process. Furthermore, liquid crystal materials exhibiting a blue phase have little viewing angle dependency.

[0397] In addition, when liquid crystal elements are used as display elements, TN (Twisted Nematic) ) mode, IPS (In-Plane-Switching) mode, FFS mode, A SM(Axially Symmetrically aligned Micro-cell) mode, OCB (Optical Compensated Birefringenc e) mode, FLC (Ferroelectric Liquid Crystal) mode AFLC (AntiFerroelectric Liquid Crystal) ) mode can be used.

[0398] In addition, normally black type liquid crystal display devices, for example, those using a vertical alignment (VA) mode The vertical alignment mode may be a transmission type liquid crystal display device. For example, MVA (Multi-Domain Vertical Alignment) ) mode, PVA (Patterned Vertical Alignment) mode mode, ASV mode, etc. can be used.

[0399] <4-3. Display devices using light-emitting elements> The display device 700 shown in FIG. 26 includes a light-emitting element 782. The light-emitting element 782 is a conductive film The display device 700 shown in FIG. The EL layer 786 of the light element 782 emits light, thereby displaying an image. The EL layer 786 includes an organic compound or an inorganic compound such as quantum dots.

[0400] Examples of materials that can be used for the organic compound include fluorescent materials and phosphorescent materials. In addition, materials that can be used for quantum dots include colloidal quantum dots. materials, alloy type quantum dot materials, core-shell type quantum dot materials, core type quantum dot materials, In addition, the elements of the 12th and 16th families, the 13th and 15th families, or the 14th and 16th families Materials containing the element group may also be used. Cadmium (Cd), selenium (Se), Zinc (Zn), Sulfur (S), Phosphorus (P), Indium (In), Tellurium (Te), Lead (P b) Quantum containing elements such as gallium (Ga), arsenic (As), and aluminum (Al). Dot material may also be used.

[0401] In addition, in the display device 700 shown in FIG. 26, an insulating film 730 is provided over the transistor 750. The insulating film 730 covers part of the conductive film 772. Therefore, the conductive film 788 has a light-transmitting property, and the EL layer 786 emits light. In this embodiment, the top emission structure is, for example, For example, a bottom emitter that emits light to the conductive film 772 side is shown. and a dual emission structure in which light is emitted to both the conductive film 772 and the conductive film 788. It can also be applied to structures.

[0402] A colored film 736 is provided at a position overlapping the light emitting element 782, and a colored film 736 is provided at a position overlapping the insulating film 730. A light-shielding film 738 is provided at the position where the light-shielding film 738 is to be formed, the wiring portion 711, and the source driver circuit portion 704. The colored film 736 and the light-shielding film 738 are covered with an insulating film 734 in the same manner as in FIG. The space between the light emitting element 782 and the colored film 736 may be filled with a sealing film 732. In the display device 700 shown in FIG. 26, the colored film 736 is provided. However, the present invention is not limited to this. For example, the EL layer 786 may be formed by coloring. In some cases, the colored film 736 may not be provided.

[0403] The insulating film 730 may be made of polyimide resin, acrylic resin, polyimide amide resin, or benzophenone. Heat-resistant organic materials such as cyclobutene resin, polyamide resin, and epoxy resin are used. In addition, by stacking multiple insulating films made of these materials, it is possible to obtain an insulating A membrane 730 may be formed.

[0404] <4-4. Example of a configuration in which an input / output device is provided on a display device> Moreover, the display device 700 shown in FIG. 25 and FIG. 26 may be provided with an input / output device. An example of the force device is a touch panel.

[0405] FIG. 27 shows a configuration in which a touch panel 791 is provided on the display device 700 shown in FIG. FIG. 28 shows a configuration in which a touch panel 791 is provided on the display device 700 shown in FIG.

[0406] FIG. 27 is a cross-sectional view of a configuration in which a touch panel 791 is provided on the display device 700 shown in FIG. FIG. 28 is a cross-sectional view of a configuration in which a touch panel 791 is provided on the display device 700 shown in FIG. be.

[0407] First, the touch panel 791 shown in FIGS. 27 and 28 will be described below.

[0408] The touch panel 791 shown in FIG. 27 and FIG. 28 is made of a second substrate 705 and a colored film 736. The touch panel 791 is a so-called in-cell type touch panel that is provided between a colored film It may be formed on the second substrate 705 before forming 736 .

[0409] The touch panel 791 includes a light-shielding film 738, an insulating film 792, an electrode 793, and an electrode 794, an insulating film 795, an electrode 796, and an insulating film 797. When a detection object such as a stylus approaches, a change in capacitance between electrode 793 and electrode 794 occurs. It is possible to detect the change.

[0410] 27 and 28, an electrode 793 and The electrode 796 is formed by passing through an opening in the insulating film 795. The electrode 794 is electrically connected to the two electrodes 793 that sandwich the electrode 794 via the electrodes 793. 28, a configuration in which the region where the electrode 796 is provided is provided in the pixel portion 702 is illustrated. However, the present invention is not limited to this. For example, the light emitting diode 704 may be formed in the source driver circuit section 704.

[0411] The electrodes 793 and 794 are provided in a region overlapping with the light-shielding film 738. As shown in FIG. 1, the electrode 793 is preferably provided so as not to overlap with the liquid crystal element 775. In addition, as shown in FIG. 28, the electrode 793 is provided so as not to overlap the light emitting element 782. In other words, the electrode 793 overlaps with the light-emitting element 782 and the liquid crystal element 775. In other words, the electrode 793 has a mesh shape. By this configuration, the electrode 793 does not block the light emitted by the light emitting element 782. Alternatively, the electrode 793 may be configured so as not to block light passing through the liquid crystal element 775. Therefore, the reduction in brightness due to the placement of the touch panel 791 is extremely small. Since the number of pixels is small, a display device with high visibility and reduced power consumption can be realized. Pole 794 may be of a similar configuration.

[0412] In addition, since the electrodes 793 and 794 do not overlap with the light-emitting element 782, The electrode 794 may be made of a metal material having a low transmittance of visible light. Since the electrodes 793 and 794 do not overlap with the liquid crystal element 775, In addition, a metal material having a low transmittance of visible light can be used.

[0413] Therefore, compared with electrodes using oxide materials with high visible light transmittance, the electrodes 793 and The resistance of the electrode 794 can be reduced, improving the sensor sensitivity of the touch panel. It is possible.

[0414] For example, the electrodes 793, 794, and 796 may be made of conductive nanowires. The nanowires have an average diameter of 1 nm to 100 nm, preferably 5 nm to 50 nm. The size of the nanoparticles may be 5 nm or less, and more preferably 5 nm or more and 25 nm or less. The wires are metal nanowires such as Ag nanowires, Cu nanowires, or Al nanowires. For example, electrodes 793 and 794 may be used. When Ag nanowires are used for either 94 or 796, or for all of them, the The light transmittance is to be 89% or more, and the sheet resistance is to be 40Ω / □ or more and 100Ω / □ or less. can.

[0415] 27 and 28 show an example of the configuration of an in-cell type touch panel. However, the present invention is not limited to this. For example, a so-called on-cell type transistor formed on the display device 700 may be used. A so-called out-cell type touch panel that is attached to the display device 700. It is also possible to use the following.

[0416] In this manner, the display device according to one embodiment of the present invention can be used in combination with various types of touch panels. It can be used.

[0417] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0418] (Embodiment 5) In this embodiment, a display device of one embodiment of the present invention will be described with reference to FIGS.

[0419] <Circuit configuration of display device> The display device shown in FIG. 29A has a region having pixels of a display element (hereinafter, referred to as a pixel portion 502). ) and a circuit section ( hereinafter referred to as a drive circuit section 504) and a circuit having a function of protecting the element (hereinafter referred to as a protection circuit 50 6) and a terminal portion 507. Note that the protection circuit 506 is not provided. This is also fine.

[0420] A part or the whole of the driver circuit portion 504 is formed on the same substrate as the pixel portion 502. This makes it possible to reduce the number of parts and terminals. When a part or the whole of the pixel portion 502 is not formed on the same substrate, the driving circuit A part or the whole of the path portion 504 is COG or TAB (Tape Automated Band). It can be implemented by using the onding.

[0421] The pixel section 502 is arranged in X rows (X is a natural number of 2 or more) and Y columns (Y is a natural number of 2 or more). The display device has a circuit for driving a plurality of display elements (hereinafter, referred to as pixel circuit 501), The path section 504 is a circuit (hereinafter, a gate driver) that outputs a signal (scanning signal) for selecting a pixel. 504a) to provide a signal (data signal) for driving the display element of the pixel. The pixel circuit 504 includes a driver circuit such as a circuit (hereinafter, referred to as a source driver 504b).

[0422] The gate driver 504a includes a shift register and the like. A signal for driving the shift register is input via a terminal unit 507, and a signal is output. For example, a start pulse signal, a clock signal, etc. are input to the gate driver 504a. The gate driver 504a outputs a pulse signal. The gate has a function of controlling the potential of the scanning lines GL_1 to GL_X. A plurality of drivers 504a are provided, and the scanning lines GL_1 to Alternatively, the gate driver 504a may control the GL_X by dividing it. However, the gate driver 50 has a function of supplying 4a may also provide another signal.

[0423] The source driver 504b includes a shift register and the like. Through the terminal section 507, a signal for driving the shift register as well as a source of a data signal are input. The source driver 504b outputs a pixel circuit based on the image signal. The source driver 504b has a function of generating a data signal to be written to the source driver 501. A data signal is generated according to a pulse signal obtained by inputting a start pulse, a clock signal, etc. The source driver 504b has a function of controlling the output of a data signal. The data lines DL_1 to DL_Y are connected to the data line 101 through the data line 102. Alternatively, the source driver 504b may have a function of supplying an initialization signal. However, the present invention is not limited to this, and the source driver 504b may also supply other signals. It is possible.

[0424] The source driver 504b is configured using, for example, a plurality of analog switches. The source driver 504b sequentially turns on a number of analog switches, The image signal can be time-division-divided and output as a data signal. Also, a shift register, etc. This may be used to configure the source driver 504b.

[0425] Each of the plurality of pixel circuits 501 is connected to one of the plurality of scanning lines GL to which a scanning signal is applied. A pulse signal is inputted through the data line DL, and a data signal is given through one of the data lines DL. A data signal is input to each of the pixel circuits 501. 504a controls writing and holding of data of the data signal. For example, The second pixel circuit 501 is connected to a gate driver GL_m (where m is a natural number equal to or smaller than X) via a scanning line GL_m. A pulse signal is input from 504a, and the data line DL_n ( A data signal is input from the source driver 504b via a source driver 504c (n is a natural number equal to or smaller than Y).

[0426] The protection circuit 506 shown in FIG. 29(A) is, for example, a gate driver 504a and a pixel circuit 5 01. Alternatively, the protection circuit 506 is connected to the scanning line GL, which is the wiring between the source driver The data line DL is connected between the driver 504b and the pixel circuit 501. The protection circuit 506 can be connected to a wiring between the gate driver 504a and the terminal unit 507. Alternatively, the protection circuit 506 may be a wiring between the source driver 504b and the terminal unit 507. The terminal unit 507 can be connected to a power supply and a power supply line from an external circuit to the display device. This refers to the part provided with terminals for inputting control signals and image signals.

[0427] When a potential outside a certain range is applied to the wiring to which the protection circuit 506 is connected, the protection circuit This is a circuit that brings one wire into electrical continuity with another wire.

[0428] As shown in FIG. 29A, a protection circuit 50 is provided in each of a pixel section 502 and a driver circuit section 504. 6, ESD (Electro Static Discharge: This can improve the resistance of the display device to overcurrent caused by electrostatic discharge (ESD) and the like. However, the configuration of the protection circuit 506 is not limited to this. For example, A configuration in which a protection circuit 506 is connected, or a protection circuit 506 is connected to the source driver 504b Alternatively, a protection circuit 506 may be connected to the terminal portion 507. It can also be written as:

[0429] In FIG. 29(A), the gate driver 504a and the source driver 504b Therefore, although an example in which the driver circuit portion 504 is formed is shown, the present invention is not limited to this configuration. For example, only the gate driver 504a is formed, and a source driver circuit is formed separately. A substrate (for example, a drive circuit substrate formed of a single crystal semiconductor film or a polycrystalline semiconductor film) is It may also be configured to be equipped with

[0430] In addition, the pixel circuits 501 shown in FIG. 29(A) may have a configuration shown in FIG. 29(B), for example. It can be said that:

[0431] The pixel circuit 501 shown in FIG. 29B includes a liquid crystal element 570, a transistor 550, and a capacitor. The transistor 550 may be any of the transistors described in the previous embodiment. can be applied.

[0432] The potential of one of the pair of electrodes of the liquid crystal element 570 is appropriately set according to the specifications of the pixel circuit 501. The alignment state of the liquid crystal element 570 is set by the written data. A common potential is applied to one of a pair of electrodes of the liquid crystal element 570 in each of the pixel circuits 501. A common potential may be applied to the pair of liquid crystal elements 570 of the pixel circuits 501 in each row. A different potential may be applied to one of the electrodes.

[0433] For example, the display device including the liquid crystal element 570 can be driven in a TN mode, an STN mode, or the like. mode, VA mode, ASM mode, OCB mode, FLC mode, AFLC mode, MV A mode, PVA mode, IPS mode, FFS mode, or TBA (Transve A 3D bend alignment mode may also be used. In addition to the above-mentioned driving method, ECB (Electrically Controlled Bias Circuit) is also available. trolled birefringence mode, PDLC (Polymer D ispersed Liquid Crystal mode, PNLC (Polymer Network Liquid Crystal) mode, guest host mode, etc. However, the present invention is not limited to this, and various liquid crystal elements and driving methods thereof may be used. It is possible.

[0434] In the pixel circuit 501 in the mth row and the nth column, One of the electrodes is electrically connected to the data line DL_n, and the other is a pair of electrodes of the liquid crystal element 570. The gate electrode of the transistor 550 is electrically connected to the other of the electrodes of the scan line G. The transistor 550 is electrically connected to the data signal writing terminal L_m. It has the function of controlling.

[0435] One of a pair of electrodes of the capacitor 560 is connected to a wiring to which a potential is supplied (hereinafter, a potential supply line VL ) and the other is electrically connected to the other of the pair of electrodes of the liquid crystal element 570. The value of the potential of the potential supply line VL is set appropriately according to the specifications of the pixel circuit 501. The capacitor 560 functions as a storage capacitor for storing written data.

[0436] For example, in a display device having the pixel circuit 501 shown in FIG. The pixel circuits 501 in each row are sequentially selected by a gate driver 504a shown in FIG. 550 is turned on to write data of the data signal.

[0437] In the pixel circuit 501 in which data has been written, the transistor 550 is turned off. By repeating this process row by row, an image can be displayed.

[0438] In addition, the pixel circuits 501 shown in FIG. 29(A) may be, for example, a configuration shown in FIG. 29(C). It can be said that:

[0439] The pixel circuit 501 shown in FIG. 29C includes transistors 552 and 554 and a capacitance element. The transistor 552 and the transistor 554 The transistor described in the above embodiment can be used for either or both of the above. .

[0440] A data signal is applied to one of the source and drain electrodes of the transistor 552. The transistor 55 is electrically connected to a wiring (hereinafter, referred to as a signal line DL_n). The gate electrode of 2 is electrically connected to the wiring to which the gate signal is given (hereinafter, referred to as the scanning line GL_m). are connected to the network.

[0441] The transistor 552 has a function of controlling writing of data signals.

[0442] One of a pair of electrodes of the capacitor 562 is connected to a wiring to which a potential is applied (hereinafter, a potential supply line VL _a), and the other is electrically connected to the source electrode and drain electrode of the transistor 552. The second electrode is electrically connected to the other of the first and second electrodes.

[0443] The capacitor 562 functions as a storage capacitor for storing written data.

[0444] One of the source electrode and the drain electrode of the transistor 554 is connected to the potential supply line VL_a. In addition, the gate electrode of the transistor 554 is electrically connected to the It is electrically connected to the other of the source electrode and the drain electrode.

[0445] One of the anode and the cathode of the light-emitting element 572 is electrically connected to the potential supply line VL_b. The other one is electrically connected to the other of the source electrode and drain electrode of the transistor 554. will be done.

[0446] The light-emitting element 572 may be, for example, an organic electroluminescence element (also called an organic EL element). However, the light-emitting element 572 is not limited to this. Alternatively, an inorganic EL element made of an inorganic material may be used.

[0447] A high power supply potential VDD is applied to one of the potential supply lines VL_a and VL_b. and the other is supplied with a low power supply potential VSS.

[0448] In a display device having the pixel circuit 501 shown in FIG. 29(C), for example, The pixel circuits 501 in each row are sequentially selected by the gate driver 504a, and the transistors 552 are turned on. The data signal is written by turning it on.

[0449] In the pixel circuit 501 to which the data has been written, the transistor 552 is turned off. Furthermore, the transistor 554 is in a holding state in response to the potential of the written data signal. The amount of current flowing between the source electrode and the drain electrode is controlled, and the light emitting element 572 The light is emitted with a brightness that corresponds to the flow rate. By performing this process row by row, an image can be displayed.

[0450] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0451] (Embodiment 6) FIG. 30 is a block diagram showing a configuration example of a display device 800. The display device 800 is Unit 810, touch sensor unit 820, controller IC 815, host 840 In addition, the display device 800 may include a light sensor 843 and an open / close sensor 844 as necessary. The display unit 810 may include a pixel portion 502, a gate driver 504a, and a The switch 504 has a switch driver 504b.

[0452] <<Controller IC>> In FIG. 30, a controller IC 815 includes an interface 850, a frame memory 851, decoder 852, sensor controller 853, controller 854, clock generator A synthesis circuit 855, an image processing unit 860, a memory 870, a timing controller 873, a register The touch sensor controller 875 and the touch sensor controller 884.

[0453] Communication between the controller IC 815 and the host 840 occurs through an interface 850. Image data, various control signals, etc. are sent from the host 840 to the controller IC 815. Also, the touch sensor controller 884 receives the signal from the controller IC 815. The acquired touch position and other information are sent to the host 840. Each circuit of the display device 800 is determined according to the specifications of the host 840 and the display device 800. They are selected and discarded as appropriate.

[0454] The frame memory 851 stores image data input to the controller IC 815. When compressed image data is sent from the host 840, the frame The memory 851 is capable of storing compressed image data. The decoder 852 is , a circuit for expanding compressed image data. In this case, the decoder 852 does not perform any processing. 51 and the interface 850.

[0455] The image processing unit 860 has a function of performing various image processing on image data. For example, The image processing unit 860 includes a gamma correction circuit 861, a light adjustment circuit 862, and a color adjustment circuit 863. .

[0456] In addition, the display device 800 may be configured to use a display element that allows a current to flow, such as an organic EL or LED. When a display element that emits light at different wavelengths is used, the image processing unit 860 may include a correction circuit 864. In this case, the source driver 504b is a circuit for detecting the current flowing through the display element. The correction circuit 864 is preferably provided with The luminance of the display element is adjusted based on the signal.

[0457] The image data processed by the image processing unit 860 is transmitted to the source driver 5 via the memory 870. The image data is output to the memory 870. The source driver 504b processes the input image data and outputs the source The number of source drivers 504b is not limited, and the number of the source drivers 504b is not limited. Depending on the number of pixels in 2, only as many as necessary may be provided.

[0458] The timing controller 873 controls the source driver 504b, the touch sensor controller The driver 884 has the function of generating a timing signal used by the gate driver 504a.

[0459] The touch sensor controller 884 controls the drive circuit of the touch sensor unit 820. The signal including the touch information read from the touch sensor unit 820 is The touch sensor controller 884 processes the touch sensor data and transmits the data to the host 88 via the interface 850. The host 840 generates image data reflecting the touch information and transmits it to the controller 840. The controller IC 815 outputs the touch information to the image data. It is also possible to configure it to reflect the information.

[0460] The clock generation circuit 855 generates the clock signal used by the controller IC 815. The controller 854 communicates with the host 840 via the interface 850. It processes various control signals sent from the controller and controls various circuits in the controller IC815. The controller 854 also controls the power supply to various circuits in the controller IC 815. It has the function of controlling the power supply. It temporarily cuts off the power supply to unused circuits. This is called power gating. Note that the power supply lines are omitted in Figure 30. .

[0461] Register 875 stores data used in the operation of controller IC 815. The data stored in the register 875 includes the image data used by the image processor 860 to perform correction processing. Parameter, the parameters used by the timing controller 873 to generate waveforms of various timing signals The register 875 is a scan chain consisting of multiple registers. It has a register.

[0462] The sensor controller 853 is electrically connected to the optical sensor 843. 843 detects the light 845 and generates a detection signal. A control signal is generated based on the signal. The control signal generated by the sensor controller 853 is For example, it is output to the controller 854.

[0463] In response to the brightness of the light 845 measured using the light sensor 843 and the sensor controller 853, In other words, the brightness of the light 845 can be adjusted by the image processor 860. In dark environments, the pixel brightness is reduced to reduce glare and power consumption. In addition, in an environment where the brightness of the light 845 is bright, the brightness of the pixel can be increased. By reducing the brightness, it is possible to obtain a display quality with excellent visibility. The brightness may be adjusted based on the brightness setting. Here, this adjustment is called dimming or dimming process. The circuit that executes this process is called a dimming circuit.

[0464] In addition, the optical sensor 843 and the sensor controller 853 are provided with a function for measuring the color tone of the light 845. For example, in a reddish environment at dusk, In this case, the eyes of the user of the display device 800 undergo color adaptation, and the reddish color is perceived as white. In this case, the display of the display device 800 appears bluish white. By emphasizing the R (red) component, the color tone can be corrected. This is called color or color-matching processing, and the circuit that executes this processing is called a color-matching circuit.

[0465] The image processing unit 860 may include an RGB-RGBW conversion circuit or the like depending on the specifications of the display device 800. , and other processing circuits. A circuit that converts (red, green, blue, white) image data into RGBW (red, green, blue, white) image data. That is, when the display device 800 has pixels of four colors, RGBW, By displaying the W (white) component using W (white) pixels, it is possible to reduce power consumption. In addition, when the display device 800 has pixels of four colors, RGBY (red, green, blue, yellow), For example, an RGB-RGBY conversion circuit can be used.

[0466] <parameters> Image correction processes such as gamma correction, brightness adjustment, and color adjustment are used to correct the output for the input image data X. This corresponds to the process of creating the correct data Y. The parameters used by the image processing unit 860 are This is a parameter for converting data X into corrected data Y.

[0467] There are two methods for setting parameters: the table method and the function approximation method. In the table method, the correction data Yn is used as a parameter to create a table for image data Xn. In the table method, the register that stores the parameters corresponding to the table is On the other hand, it requires a large number of images, but the degree of freedom of correction is high. When the correction data Y for the A configuration using a1, a2, b2, etc. is effective. Here, the line A method of approximating the shape of a function is shown, but a method of approximating the shape of a function using a nonlinear function is also possible. Although the degree of freedom of correction is low, the number of registers that store the parameters that define the function is small. Done.

[0468] The parameters used by the timing controller 873 are, for example, as shown in FIG. In this way, the generated signal of the timing controller 873 is set to “L” (or The parameter Ra (or Rb) indicates the timing when the reference signal This indicates how many clock cycles the timing at which the signal becomes "L" (or "H") is doing.

[0469] The parameters for the correction can be stored in the register 875. Other parameters that can be stored in the register 875 include the brightness and color tone of the display device 800. , Energy saving settings (time until the display is dimmed or turned off), Touch sensor The sensitivity of the controller 884.

[0470] <Power gating> If there is no change in the image data sent from the host 840, the controller 854 It is possible to power-gate some of the circuits in the controller IC815. Specifically, For example, the circuits in the area 890 (frame memory 851, decoder 852, image processing unit 86 0, memory 870, timing controller 873, and register 875) are temporarily stopped. The host 840 sends a control signal to the controller 820 indicating that the image data is unchanged. When the control signal is detected by the controller 854, the power A gating configuration is possible.

[0471] Even if there is no change in the image data, for example, by incorporating a timer function in the controller 854, By doing so, the power supply to the circuit in the area 890 is resumed based on the time measured by the timer. The timing of the determination may be determined.

[0472] The power gating is performed not only on the circuit in the region 890 but also on the source driver 50 This may also be done for 4b.

[0473] In the configuration of FIG. 30, the source driver 504b is included in the controller IC 815. That is, the source driver 504b and the controller IC 815 may be integrated in the same It may be formed on a chip.

[0474] A specific example of the circuit configuration of the frame memory 851 and the register 875 will now be described.

[0475] <Frame Memory 851> FIG. 32A shows an example of the configuration of the frame memory 851. The frame memory 851 is The peripheral circuit 908 includes a sense amplifier 902, a cell array 903, and a peripheral circuit 908. The image sensor includes an amplifier circuit 904 , a driver 905 , a main amplifier 906 , and an input / output circuit 907 .

[0476] The control unit 902 has a function of controlling the frame memory 851. For example, the control unit 90 2 controls a driver 905 , a main amplifier 906 , and an input / output circuit 907 .

[0477] A plurality of wirings WL and CSEL are electrically connected to the driver 905. 905 generates signals to be output to a plurality of wirings WL and CSEL.

[0478] The cell array 903 includes a plurality of memory cells 909. The memory cells 909 are connected to the wiring W L, LBL (or LBLB), and BGL are electrically connected. In the example of FIG. 32(A), the lines LBL and LBLB are local bit lines. The cell array 903 is configured in a folded bit line manner, but can be configured in an open bit line manner. It is also possible.

[0479] FIG. 32B shows a configuration example of the memory cell 909. The memory cell 909 is a transistor. The memory cell 909 includes a DRAM (dynamic random access memory) The circuit configuration is similar to that of a memory cell in a random access memory (RANDOM ACCESS MEMORY). The transistor NW1 has a back gate. The port is electrically connected to the wiring BGL. The wiring BGL receives the voltage Vbg_w1. Be encouraged.

[0480] The transistor NW1 has a semiconductor layer in which the channel is formed, which is a type of metal oxide. A transistor using an organic semiconductor (also called an OS transistor). Since the off-state current of an OS transistor is extremely small, the memory cell 909 is composed of an OS transistor. This prevents charge from leaking from the capacitive element CS1, so frame memory 8 This reduces the frequency of the refresh operation of the frame 51. The memory 851 is capable of holding image data for a long period of time. By making the voltage Vcc negative, the threshold voltage of the transistor NW1 can be shifted to the positive potential side. Therefore, the retention time of the memory cell 909 can be extended.

[0481] Here, the off-state current is the current between the source and drain when the transistor is in the off state. When a transistor is an n-channel type, for example, the threshold voltage is If the voltage of the gate relative to the source is negative, the source The current that flows between the source and drain can be called the off-state current. For example, the off-current per 1 μm of channel width is 100 zA (z; zepto, 10 -21 ) or less. Since the smaller the off-state current, the better, this normalized It is preferable that the off-state current is 10 zA / μm or less, or 1 zA / μm or less. 10yA / μm(y; Yocto, 10 -24 ) or less is more preferable.

[0482] The transistor NW1 of each of the memory cells 909 in the cell array 903 is an OS transistor. Since the transistors are the same, the transistors in the other circuits are fabricated on silicon wafers, for example. This allows the cell array 903 to be a sense amplifier. The frame memory 851 can be stacked on the flip-chip circuit 904. This reduces the size of the controller IC 815.

[0483] The cell array 903 is stacked on a sense amplifier circuit 904. The sense amplifier circuit 904 has a plurality of sense amplifiers SA. The sense amplifiers SA are connected to adjacent wirings L BL, LBLB (local bit line pair), wiring GBL, GBLB (global bit line pair) ) are electrically connected to a plurality of wirings CSEL. The sense amplifier SA is connected to the wirings LBL and It has the function of amplifying the potential difference with the wiring LBLB.

[0484] In the sense amplifier circuit 904, one wiring GBL is provided for four wirings LBL. 1 wire GBLB is provided for 4 wires LBLB, but the sense amplifier circuit The configuration of the path 904 is not limited to the example configuration of FIG.

[0485] The main amplifier 906 is connected to the sense amplifier circuit 904 and the input / output circuit 907. The main amplifier 906 has a function of amplifying the potential difference between the wiring GBL and the wiring GBLB. The main amplifier 906 may be omitted.

[0486] The input / output circuit 907 supplies a potential corresponding to write data to the wirings GBL and GBLB, or or a function of outputting to the main amplifier 906, the potential of the wiring GBL and the wiring GBLB, or The output potential of the amplifier 906 is read out and output as data to the outside. The CSEL signal controls the sense amplifier SA to read data and the sense amplifier SA to write data. Therefore, the input / output circuit 907 can select the sense amplifier SA. Since no selection circuit such as the above is required, the circuit configuration can be simplified and the occupied area can be reduced. Cut.

[0487] <Register 875> 33 is a block diagram showing an example of the configuration of the register 875. The register 875 is The scan chain includes a register unit 875A and a register unit 875B. The register section 875A includes a plurality of registers 930. A scan chain register is configured. The register unit 875B includes a plurality of registers. It has 931.

[0488] The register 930 is a non-volatile register that does not lose data even when the power supply is cut off. In order to make the register 930 nonvolatile, the register 930 is It is equipped with a holding circuit that uses a transistor.

[0489] On the other hand, the register 931 is a volatile register. There are no restrictions, and any circuit capable of storing data can be used. The image processing unit 860 and the timing controller 87 3 accesses the register section 875B and retrieves data from the corresponding register 931 Alternatively, the image processing unit 860 and the timing controller 873 may include a register unit 87 The processing contents are controlled according to the data supplied from 5B.

[0490] When updating the data stored in the register 875, the scan chain register The data in the scan chain register unit 875A is changed. After rewriting the data in the registers 930 of the scan chain register unit 875A, The data is loaded into each register 931 of the register section 875B all at once.

[0491] As a result, the image processing unit 860, the timing controller 873, etc. are updated collectively. Various processes can be performed using the updated data. This allows the controller IC815 to operate stably. By providing the image processing unit 860 and the timing Even while the scanning controller 873 is in operation, the data in the scan chain register section 875A is It can be updated.

[0492] When the power gating of the controller IC 815 is executed, the register 930 stores: The data is saved in the holding circuit before the power supply is cut off. After the power is restored, the register The data in 930 is restored (loaded) to the register 931 to resume normal operation. The data stored in register 930 and the data stored in register 931 are consistent. If not, the data in register 931 is saved in register 930 and then the register It is preferable to store the data in the holding circuit of the register 930. For example, update data is being inserted into the scan chain register unit 875A.

[0493] FIG. 34 shows an example of the circuit configuration of the register 930 and the register 931. Two stages of registers 930 in the can chain register section 875A, and these registers 930 The register 930 corresponds to the signal Scan In. is input, and the signal Scan Out is output.

[0494] The register 930 includes a holding circuit 947, a selector 948, and a flip-flop circuit 949. The selector 948 and the flip-flop circuit 949 form a scan flip-flop circuit. A selector 948 receives the signal SAVE1.

[0495] The signals SAVE2 and LOAD2 are input to the holding circuit 947. The holding circuit 947 The transistors T1 to T6 and the capacitive elements C4 and C6 are included. The transistors T1 and T2 are The transistors T1 and T2 are transistors N of the memory cell 909. Similar to W1 (see FIG. 32B), an OS transistor with a back gate may be used. .

[0496] The transistors T1, T3, T4 and the capacitor C4 form a three-transistor gain selector. Similarly, a three-transistor circuit is formed by transistors T2, T5, T6 and a capacitance element C6. A transistor type gain cell is constructed. Two gain cells form a flip-flop. The circuit 949 stores the complementary data held by the transistors T1 and T2. Since the data is stored in the memory, the holding circuit 947 can hold data for a long time even when the power supply is cut off. In the resistor 930, transistors other than the transistors T1 and T2 may be used. The transistors can be made of silicon.

[0497] The holding circuit 947 outputs the phase held by the flip-flop circuit 949 in response to the signal SAVE2. The complementary data is stored, and the held data is transferred to the flip-flop circuit according to the signal LOAD2. Load to 949.

[0498] The input terminal of the flip-flop circuit 949 is electrically connected to the output terminal of the selector 948. The data output terminal is electrically connected to an input terminal of a register 931. The flip-flop circuit 949 includes inverters 950 to 955, an analog switch 957, The conductive state of the analog switches 957 and 958 is determined by the scan clock (S The flip-flop circuit 949 is controlled by a signal called the can Clock. The circuit configuration is not limited to that of FIG. 34, and various flip-flop circuits 949 can be applied. Cut.

[0499] The output terminal of the register 931 is electrically connected to one of the two input terminals of the selector 948. The other end is electrically connected to the output terminal of the previous stage flip-flop circuit 949. The input terminal of the first stage selector 948 of the scan chain register unit 875A is , data is input from outside the register 875.

[0500] The register 931 includes inverters 961 to 963, a clocked inverter 964, and an analog The register 931 has a log switch 965 and a buffer 966. The data of the flip-flop circuit 949 is loaded by the transistor of the register 931. The capacitor can be made of a Si transistor.

[0501] <<Example of operation>> An example of the operation of the controller IC 815 and the register 875 for the display device 800 is as follows: The following will be described separately for the time before shipment, when the electronic device having the display device 800 is started up, and during normal operation. .

[0502] <Before shipping> Before shipment, parameters related to the specifications of the display device 800 are stored in the register 875. These parameters include, for example, the number of pixels, the number of touch sensors, the timing control, etc. These include parameters used by the 873 to generate waveforms for various timing signals. If the unit 860 includes a correction circuit 864, the correction data is also registered as a parameter. These parameters are stored in the register 875. In addition to the register 875, a dedicated ROM is also used. It may be provided and stored.

[0503] <Startup> When the electronic device having the display device 800 is started, the user setting sent from the host 840 The parameters such as the display are stored in the register 875. brightness and color, touch sensor sensitivity, energy saving settings (dimming the display or turning off the There are also gamma correction curves and tables. When data is stored in the register 875, the controller 854 scans the data into the register 875. A clock signal and data corresponding to the parameter in synchronization with the scan clock signal is sent.

[0504] <Normal operation> Normal operation includes a state where a video is being displayed, a state where a still image is being displayed and IDS operation is possible. The state where a moving image or the like is displayed is divided into a display state, a display state, and a non-display state. The timing controller 873 and the like are in operation, but the data in the register 875 is changed. Since this is performed for the scan chain register unit 875A, After the data change in the scan chain register unit 875A is completed, The data in the chain register unit 875A is loaded into the register unit 875B all at once. Then, the data change of the register 875 is completed. Switch to the corresponding action.

[0505] When a still image is being displayed and IDS driving is possible, the register 875 is, for example, Like other circuits in 0, it can be power-gated. Before the scan, the signal is input to the register 930 of the scan chain register unit 875A. In response to signal SAVE2, the complementary data held by the flip-flop circuit 949 is transferred to the hold circuit 94 Work is underway to store it in 7.

[0506] When returning from power gating, the holding circuit 947 holds the load in accordance with the signal LOAD2. The data stored in the flip-flop circuit 949 is loaded into the flip-flop circuit 949 in response to the signal LOAD1. The data of the flip-flop circuit 949 is loaded into the register 931. The data in register 875 is valid in the same state as before power gating. Even if the host 840 is in the loading state, a parameter change request for the register 875 can be If so, release the power gating of register 875 and change the parameters. can be done.

[0507] In the non-display state, for example, the circuitry in area 890 (including register 875) In this case, the host 840 may also be shut down. Since the frame memory 851 and the register 875 are non-volatile, power gating is not required. When returning from power gating, the display before power gating (static) is displayed without waiting for the host 840 to return. It is possible to perform still images.

[0508] For example, when the display device 800 is applied to the display unit of a folding information terminal, In response to a signal from the terminal 844, the information terminal is folded and the display surface of the display device 800 is used. When the absence of the sensor is detected, in addition to the circuitry in area 890, a sensor controller 853, And the touch sensor controller 884 etc. can be power gated.

[0509] When the information terminal is folded, depending on the host 840 standard, the host 840 may stop Even if the information terminal is deployed again while the host 840 is stopped, the frame The system memory 851 and the register 875 are non-volatile, so that image data from the host 840 can be Before various control signals are sent, the image data in the frame memory 851 is displayed. can be done.

[0510] In this manner, the register 875 includes a scan chain register section 875A and a register section 87 5B, and by changing data in the scan chain register unit 875A, Smoothly without affecting the image processing unit 860 and the timing controller 873. In addition, each register of the scan chain register unit 875A can be changed. The starter 930 has a holding circuit 947, which smoothly switches between the power gating state and the power gating state. This can be done easily.

[0511] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments.

[0512] (Embodiment 7) In this embodiment, a display module and an electronic device including a display device according to one embodiment of the present invention will be described. This will be described with reference to FIGS.

[0513] <7-1. Display module> FIG. 35 is a schematic cross-sectional view of a display module 7000 with an optical touch sensor. The display module 7000 shown in FIG. 35 includes an upper cover 7001 and a lower cover 7002. Between them, a display panel 7006 connected to the FPC, a backlight (not shown), a frame The housing 7009 has a printed circuit board 7010 and a battery 7011.

[0514] The display device of one embodiment of the present invention can be used for the display panel 7006, for example.

[0515] The upper cover 7001 and the lower cover 7002 are adapted to the size of the display panel 7006. The shape and dimensions can be changed appropriately.

[0516] Although not shown, the backlight has a light source. A light source may be disposed at the end of the backlight, and a light diffusion plate may be further used. In addition, when using a self-luminous light-emitting element such as an organic EL element, or a reflective panel In such cases, a configuration without a backlight may be used.

[0517] The frame 7009 protects the display panel 7006 and also supports the movement of the printed circuit board 7010. It also functions as an electromagnetic shield to block electromagnetic waves generated by the operation of the frame. The frame 7009 may also function as a heat sink.

[0518] The printed circuit board 7010 includes a power supply circuit, a signal circuit for outputting a video signal, and a clock signal. The power supply circuit is provided with a signal processing circuit. Alternatively, the power source may be a battery 7011 provided separately. , this can be omitted when using a commercial power source.

[0519] In addition, the display module 7000 includes components such as a polarizing plate, a retardation plate, and a prism sheet. It may be added.

[0520] The display module 7000 includes a light emitting section 7015 and a receiving section 7016 provided on a printed circuit board 7010. The optical unit 7016 is surrounded by an upper cover 7001 and a lower cover 7002. The region has a pair of light guiding portions (light guiding portion 7017a, light guiding portion 7017b).

[0521] The upper cover 7001 and the lower cover 7002 can be made of, for example, plastic. In addition, the upper cover 7001 and the lower cover 7002 are each thin (for example, 0. Therefore, it is possible to make the display module 7000 extremely In addition, the upper cover 7001 and the lower cover 7002 can be made lighter by using less material. Since it is possible to fabricate 002, the fabrication cost can be reduced.

[0522] The display panel 7006 is connected to a printed circuit board 7010 and a battery via a frame 7009. The display panel 7006 and the frame 7009 are disposed so as to overlap with the light guide unit 7011. 7017a and fixed to the light guiding portion 7017b.

[0523] Light 7018 emitted from the light emitting portion 7015 is guided to the display panel 70 by the light guiding portion 7017a. 7017b and reaches the light receiving part 7016. When the light 7018 is blocked by a detection object such as a stylus, a touch operation is detected. It is possible.

[0524] A plurality of light emitting units 7015 are provided, for example, along two adjacent sides of the display panel 7006. A plurality of light receiving sections 7016 are provided at positions facing the light emitting sections 7015. It is possible to obtain information on the position where the touch operation was performed.

[0525] The light emitting unit 7015 may be a light source such as an LED element. 7015, a light that emits infrared rays that are invisible to the user and harmless to the user It is preferred to use a source.

[0526] The light receiving section 7016 is a photoelectric element that receives the light emitted by the light emitting section 7015 and converts it into an electrical signal. Preferably, a photodiode capable of receiving infrared rays can be used. can.

[0527] The light guiding portion 7017a and the light guiding portion 7017b are made of a material that transmits at least the light 7018. By using the light guiding portion 7017a and the light guiding portion 7017b, The light receiving unit 7015 and the light receiving section 7016 can be disposed below the display panel 7006. This can prevent the touch sensor from malfunctioning due to the light receiving portion 7016 being reached. It is preferable to use a resin that absorbs infrared rays and transmits infrared rays. This prevents false touch sensor detection. This allows for more effective suppression of movement.

[0528] In addition, although FIG. 35 shows a display module having an optical touch sensor, it is also possible to use a resistor as appropriate. A capacitive or electrostatic touch panel may be superimposed on the display panel 7006. In addition, the opposing substrate (sealing substrate) of the display panel 7006 is provided with a touch panel function. It is also possible to provide an optical sensor in each pixel of the display panel 7006, It is also possible to use a touch panel.

[0529] <7-2.Electronic equipment 1> Next, examples of electronic devices are shown in FIGS.

[0530] FIG. 36(A) shows the appearance of the camera 8000 with the viewfinder 8100 attached. This is a diagram.

[0531] The camera 8000 includes a housing 8001, a display unit 8002, an operation button 8003, and a shutter. The camera 8000 has a button 8004 and the like. The camera 8000 also has a detachable lens 8006. It is attached.

[0532] In this example, a camera 8000 is used, and a lens 8006 is detached from a housing 8001 and replaced. However, the lens 8006 and the housing may be integrated together.

[0533] The camera 8000 can capture an image by pressing the shutter button 8004. The display unit 8002 also functions as a touch panel. It is also possible to capture an image by doing so.

[0534] The housing 8001 of the camera 8000 has a mount having electrodes, and a finder 810 In addition to 0, strobe devices etc. can also be connected.

[0535] The finder 8100 includes a housing 8101, a display unit 8102, a button 8103, and the like. .

[0536] The housing 8101 has a mount that engages with the mount of the camera 8000, The mount can be attached to the camera 8000. The mount also includes an electrode The image received from the camera 8000 through the electrode is displayed on the display unit 8102. It is possible to do so.

[0537] The button 8103 functions as a power button. The 8102 display can be switched on and off.

[0538] The display unit 8002 of the camera 8000 and the display unit 8102 of the viewfinder 8100 are The display device according to one embodiment of the present invention can be applied.

[0539] In FIG. 36(A), the camera 8000 and the finder 8100 are treated as separate electronic devices. These are configured to be removable, but the camera 8000 has a housing 8001 equipped with a display device. The camera may have a built-in viewfinder that can be used to capture images.

[0540] FIG. 36B is a diagram showing the external appearance of the head mounted display 8200.

[0541] The head mounted display 8200 includes a mounting part 8201, a lens 8202, and a main body 82 8203, a display unit 8204, a cable 8205, etc. It has a built-in 8206 battery.

[0542] A cable 8205 supplies power from a battery 8206 to the main body 8203. 03 is equipped with a wireless receiver and the like, and image information such as image data received is displayed on a display unit 8204. In addition, the camera installed in the main body 8203 can record the movement of the user's eyeballs and eyelids. The system captures the user's gaze and calculates the coordinates of the user's gaze based on that information. It can be used as an input means.

[0543] Furthermore, the mounting unit 8201 may be provided with a plurality of electrodes at positions that come into contact with the user. The main body 8203 detects the current flowing through the electrodes in response to the movement of the user's eyeball, The device may have a function of recognizing the user's viewpoint. Also, the device may have a function of detecting the current flowing through the electrode. By doing so, the mounting unit 820 may have a function of monitoring the pulse of the user. The sensor 1 may have various sensors such as a temperature sensor, a pressure sensor, and an acceleration sensor. The device may have a function of displaying the user's biological information on the display unit 8204. The image displayed on the display unit 8204 is changed according to the movement of the part. Good too.

[0544] The display device of one embodiment of the present invention can be applied to the display portion 8204.

[0545] 36(C), (D), and (E) are diagrams showing the appearance of the head mounted display 8300. The head mounted display 8300 includes a housing 8301, a display unit 8302, and a backlight. The optical element has a band-shaped fixture 8304 and a pair of lenses 8305.

[0546] A user can view the display on the display unit 8302 through the lens 8305 . It is preferable to arrange the display portion 8302 in a curved manner. By placing the device in the position shown in FIG. Although the configuration in which one display unit 8302 is provided has been illustrated, the present invention is not limited to this. For example, Two display units 8302 may be provided. In this case, one display unit is provided for each eye of the user. If the display unit is arranged in such a way that a 3D display using parallax is possible, do.

[0547] Note that the display device of one embodiment of the present invention can be applied to the display portion 8302. Since the display device of one embodiment of the present invention has extremely high definition, the lens 8305 as shown in FIG. Even if the image is enlarged using a 3D effect, the pixels will not be visible to the user, resulting in a more realistic image. can be displayed.

[0548] <7-3.Electronic equipment 2> Next, an example of an electronic device different from the electronic devices shown in FIG. 36(A) to FIG. 36(E) will be described. 7(A) to 37(G).

[0549] The electronic device shown in FIG. 37A to FIG. 37G includes a housing 9000, a display portion 9001, a switch A speaker 9003, an operation key 9005 (including a power switch or an operation switch), and a connection Terminal 9006, sensor 9007 (force, displacement, position, speed, acceleration, angular velocity, rotation speed, distance , light, liquid, magnetism, temperature, chemicals, sound, time, hardness, electric field, current, voltage, power, radiation , flow, humidity, gradient, vibration, odor or infrared measurement capabilities), micro 9008, etc.

[0550] The electronic devices shown in FIGS. 37A to 37G have various functions. Function to display various information (still images, videos, text images, etc.) on the display unit, touch panel function , calendar, date or time display functions, various software (programs) A function for controlling processing by wireless communication, a function for controlling various computers by using wireless communication, Functions for connecting to a network and transmitting or receiving various data using wireless communication functions A function to read out a program or data recorded on a recording medium and display it on the display unit. The electronic devices shown in FIGS. The functions that can be possessed by the can be not limited to these, and can have various functions. Although not shown in FIG. 37(A) to FIG. 37(G), the electronic device may have a plurality of display units. The electronic device may be provided with a camera or the like to capture still images. , the function to shoot videos, and save the captured images to a recording medium (external or built-in to the camera) The camera may have a function of capturing an image on a display unit, a function of displaying a captured image on a display unit, etc.

[0551] Next, a broadcasting system using electronic equipment will be described. The transmitting system will now be described.

[0552] <7-4. Broadcasting System> FIG. 38 is a block diagram showing a typical configuration example of a broadcasting system. 1500 includes a camera 1510, a transmitting device 1511, and an electronic device system 1501. The equipment system 1501 includes a receiving device 1512 and a display device 1513. The transmitter 1511 includes an image sensor 1520 and an image processor 1521. The signal processing unit 1520 includes an encoder 1522 and a modulator 1523 .

[0553] The receiving device 1512 and the display device 1513 are included in the electronic device system 1501. Antenna, demodulator, decoder, logic circuit, image processor, and display unit Specifically, as an example, the receiving device 1512 is configured by an antenna , a demodulator, a decoder, and a logic circuit, and the display device 1513 is an image processing device. , and a display unit. The receiving device 1512 also includes a decoder and a logic circuit. The display device 1513 may have a decoder and a logic circuit. good.

[0554] If the camera 1510 is capable of capturing 8K video, the image sensor 1520 For example, each pixel has one red (R) sub-pixel, When the image sensor 15 has two green (G) sub-pixels and one blue (B) sub-pixel, 20 requires at least 7680 x 4320 x 4 [R, G + G, B] pixels, Also, for a 4K camera, the number of pixels of the image sensor 1520 is at least 384. For a 2K camera, the number of pixels must be at least 1920x1080x4 pixels are required.

[0555] The image sensor 1520 generates unprocessed raw data 1540. 521 performs image processing (noise removal, interpolation, etc.) on the raw data 1540 to create a video The video data 1541 is output to the transmitting device 1511.

[0556] The transmitting device 1511 processes the video data 1541 and outputs a broadcast signal 1541 that is compatible with the broadcast band. The encoder 1522 generates the video data 543 (broadcast signals are sometimes called carrier waves). The encoder 1522 processes the image data 1541 and generates the encoded data 1542. A process of encoding the data 1541, and adding broadcast control data (e.g. authentication data) to the video data 1541. Processing to add extra data, encryption processing, scrambling processing (for spectrum spreading) (data sorting processing, etc.)

[0557] The modulator 1523 performs IQ modulation (quadrature amplitude modulation) on the encoded data 1542, A broadcast signal 1543 is generated and output. The broadcast signal 1543 is composed of an I (in-phase) component and a Q (in-phase) component. A TV broadcasting station acquires video data 1541, and is responsible for providing broadcast signals 1543.

[0558] The broadcast signal 1543 is received by a receiving device 1512 included in the electronic device system 1501. do.

[0559] FIG. 39 shows a broadcast system 1500A having an alternative electronic equipment system.

[0560] The broadcasting system 1500A includes a camera 1510, a transmitting device 1511, and an electronic device system 1 501A, and an image generating device 1530. The electronic equipment system 1501A includes a receiving device 1 512, and a display device 1513. The camera 1510 has an image sensor 1520, an image processor, The transmitting device 1511 includes an encoder 1522A, an encoder 1523B, and an encoder 1524. 22B, and a modulator 1523.

[0561] The receiving device 1512 and the display device 1513 are included in the electronic device system 1501A. The antenna, demodulator, decoder, image processor, and display unit Specifically, as an example, the receiving device 1512 is configured with an antenna and a demodulator. and a decoder, and the display device 1513 includes an image processing device and a display unit In addition, the receiving device 1512 does not have a decoder, and the display device 1513 has a decoder. It may also be configured to include a coder.

[0562] A camera 1510, an image sensor 1520 included in the camera 1510, and an image processing device The image processing device 1521 is a device for processing image data. The video data 1541A is output to the transmitting device 1511.

[0563] The image generating device 1530 generates text to be added to the image data generated by the image processing device 1521. It is a device that generates image data such as characters, figures, and patterns. The data is sent to the transmitting device 1511 as video data 1541B.

[0564] The transmitting device 1511 processes the video data 1541A and the video data 1541B and broadcasts them. A broadcast signal 1543 that matches the transmission band is generated (a broadcast signal is sometimes called a carrier wave). Encoder 1522A processes video data 1541A to generate encoded data 1542A. Also, the encoder 1522B processes the video data 1541B to generate the encoded data 1541B. The encoder 1522A and the encoder 1522B generate the video data 142B. A process of encoding the image data 1541A and the image data 1541B, A process of adding broadcast control data (for example, data for authentication) to the image data 1541B and the image data 1541C. Processing, encryption, scrambling (data sorting for spectrum spreading), etc. Do the following.

[0565] The broadcasting system 1500A broadcasts the video data 1541A and the video data 1541B. As shown in FIG. 38, the broadcasting system 1500 is configured to perform processing using one encoder. Good too.

[0566] The encoded data 1542A and the encoded data 1542B are sent to the modulator 1523. The modulator 1523 IQ modulates the encoded data 1542A and the encoded data 1542B. By this, a broadcast signal 1543 is generated and output. The broadcast signal 1543 is an I component and a Q component. A TV broadcasting station acquires video data 1541 and transmits it. Responsible for supplying No. 1543.

[0567] The broadcast signal 1543 is received by a receiving device 1512 included in the electronic device system 1501A. can be.

[0568] FIG. 40 shows a schematic diagram of data transmission in a broadcasting system. The radio waves (broadcast signals) transmitted from 61 are received by television receivers (TV) 156 in each home. The TV 1560 includes a receiving device 1512 and a display device. The artificial satellite 1562 may be, for example, a CS satellite or a BS satellite. Examples of the antenna 1564 include a BS·110°CS antenna, a CS antenna, The antenna 1565 may be, for example, a UHF (Ultra High Frequency) h Frequency antennas and the like.

[0569] Radio waves 1566A and 1566B are broadcast signals for satellite broadcasting. When it receives the radio wave 1566A, it transmits the radio wave 1566B to the ground. The radio wave 1566B is received by the antenna 1564, and the satellite TV broadcast is viewed on the TV 1560. Alternatively, radio wave 1566B can be received by the antenna of another broadcasting station and broadcast. The signal is then processed by the receiving device in the transmitting station into a signal that can be transmitted over the optical fiber cable. The broadcast signal is transmitted to the input unit of the TV 1560 in each home using a radio wave 1567A. 1567B is a broadcast signal for terrestrial broadcasting. 7A is amplified and radio waves 1567B are transmitted. At each home, radio waves 1565 are transmitted through antennas 1565. By receiving 67B, you can watch terrestrial TV broadcasts on TV1560.

[0570] In addition, the video distribution system of this embodiment is not limited to a system for TV broadcasting. In addition, the video data to be distributed may be either video data or still image data. .

[0571] FIG. 41 shows an example of a receiving device. A TV 1560 receives a broadcast signal from a receiving device. The receiving device 157 can receive the signal and display it on the TV 1560. 1 is provided on the outside of the TV 1560. ), antennas 1564, 1565 and TV 1560 are connected to radio 1572 and radio 15 In this case, data is transmitted and received via the wireless device 1572. The wireless device 1573 also has a function of a receiving device. 73 may be built in (see FIG. 41(C)).

[0572] The receiving device can be made portable. The receiving device 15 shown in FIG. 74 has a connector portion 1575. Electronic devices such as computers, smartphones, mobile phones, tablet devices, etc. If the TV has a terminal that can be connected to the 1575, you can watch satellite and terrestrial broadcasts using these. It becomes possible to do so.

[0573] In the broadcasting system 1500 of FIG. 38, a semiconductor device is applied to the encoder 1522. It is also possible to combine dedicated ICs and processors (e.g., GPU, CPU, etc.) By combining the above, the encoder 1522 can be configured. It is also possible to integrate the above-mentioned functions on a single dedicated IC chip.

[0574] This embodiment may be any of the other embodiments, at least some of which are described herein, or It can be implemented in appropriate combination with other embodiments. EXAMPLES

[0575] In this example, a transistor including a metal oxide of one embodiment of the present invention is used. This verified that a large, high-resolution display module could operate.

[0576] [About 8K displays] The international standard for 8K displays is Recommendation ITU- R BT.2020-2. In this standard, the resolution is 7680 horizontally and 7680 vertically. Resolution 4320, driving method is progressive, frame frequency is up to 120H It is said to be z.

[0577] Figure 42(A) shows a block diagram of an ideal display module. The configuration shown in (A) is for one pixel area formed on a substrate. A source driver and a pair of gate drivers The pair of gate drivers also controls the transistors of the pixels. The so-called G-type transistors are formed in the same process and mounted on the display module. It is preferable that the substrate is formed by the Gate On Array (GOA) method. The IC that functions as the source driver is based on the COG (Chip On Glass) method. It is preferably mounted on a board.

[0578] The transistors required to drive such high-resolution display modules are extremely In particular, when display panels become large, amorphous In transistors with low field effect mobility using semiconductors such as fast silicon, During the reset period, the image may not be rewritten in time, making it impossible to operate.

[0579] Therefore, when a transistor using amorphous silicon is used, as shown in FIG. As shown in the figure, the pixel area is divided into four parts, and each part is equipped with a source driver and a gate driver. This type of configuration allows four pixel sections to be rewritten simultaneously. By using a transistor with low field effect mobility, the image quality during a frame period is improved. In addition, since the field effect mobility of the transistor is low, If it is difficult to implement the gate driver using the GOA method, Therefore, the IC that functions as the gate driver can be implemented in the same way as the source driver. preferable.

[0580] However, in the configuration shown in FIG. 42(B), the source driver, gate driver, etc. Increased costs due to an increase in ICs and associated materials, and a decrease in aperture ratio due to an increase in the number of wiring The mounting of ICs increases the frame area, and a separate circuit is required to synchronize the divided pixels. The boundary between the divided pixels is visible, resulting in poor visibility. There are also concerns about image processing to divide the input image data into four parts. This raises concerns that a high-speed, large-scale image processing circuit will be required.

[0581] [About the validation model] In the following, a transistor using a metal oxide according to one embodiment of the present invention and an alumina transistor for comparison will be described. Large 8K LCD display modules can be operated with rufus silicon. It was verified that this was the case.

[0582] The specifications of the LCD module used in the verification are as follows. The pixel size is 65 inch, effective pixel count 7680×RGB(H)×4320(V), pixel size 187 The size is 187.5μm×187.5μm, the liquid crystal mode is VA mode, and the number of gradations is 12bit. The data voltage of the source driver IC is set to 3.5V to 14.5V, and one horizontal period is set to 1.92μ The driving method was dot inversion driving. The clock frequency of the gate driver was set to 260 The frequency was set to 1.16 kHz and the voltage was set to -6.0 V to 22.0 V. The common potential of the liquid crystal element was set to 9. The voltage was set to .0V.

[0583] In addition, each sub-pixel has one transistor and one capacitor. The transistor used is a channel-etched type single-gate transistor. The channel length was set to 4 μm and the channel width to 8 μm. The transistor has a channel-etched dual-gate structure (S-channel structure). The transistor has a channel length of 4 μm and a channel width of 4000 μm. The semiconductor layer of each of the transistors is formed of a metal oxide (CAC-OS ) was used.

[0584] For comparison, the semiconductor layer of the above transistor is made of hydrogenated amorphous silicon (a- The case where a Si:H film was applied was also examined.

[0585] [verification] The verification was carried out by measuring the time it takes for the potential of the gate line to completely fall (gate fall time) and the source The time it takes for the source line potential to reach 95% of the maximum input voltage (source line charging time) The total time was estimated. The verification results are shown below.

[0586] [Table 2]

[0587] When using CAC-OS, the total gate fall time and source line charge time is 1.91μ s, which is shorter than one horizontal period of 1.92 μs when driven at 120 Hz. This result shows that it is possible to build a gate driver. In this case, the frame width on the gate driver side is estimated to be 3.85 mm. It was also found that it is possible to realize a display module with an extremely narrow frame.

[0588] On the other hand, when hydrogenated amorphous silicon is used, the gate fall time is one horizontal period. It was found that it was not possible to incorporate a gate driver because the In this calculation, the loads of the gate line and source line are assumed to be equal. When using silicon, the size of the transistors arranged in the pixels is large, so The load will be greater than this.

[0589] Next, we compared the results for the cases using CAC-OS and hydrogenated amorphous silicon. , the panel size (pixel size) that can incorporate a gate driver, The relationship with frame frequency was verified.

[0590] The verification results are shown in Figure 43. In Figure 43, the vertical axis is panel size and the horizontal axis is frame rate. By applying CAC-OS, it is possible to achieve a maximum gate drive of 70 inches. A display with a built-in driver, 8K resolution, 120Hz frame rate, and 12-bit gradation It was confirmed that the panel could be realized.

[0591] As described above, by using the metal oxide of one embodiment of the present invention, it is possible to obtain a large-sized display with high resolution. The feasibility of the spray module was demonstrated. EXAMPLES

[0592] In this example, a transistor according to one embodiment of the present invention was manufactured. The -Vg characteristics were measured and reliability was evaluated.

[0593] [Making a transistor] First, a transistor corresponding to the transistor 100E described above is fabricated. The electrical characteristics of the transistors were evaluated. In this example, the following samples A1 and A2 were prepared. Made.

[0594] Note that Sample A1 and Sample A2 are samples in which transistors are formed. The channel length L is 3 μm and the channel width W is 50 μm.

[0595] [Preparation method of samples A1 and A2] First, a tungsten film with a thickness of 100 nm was deposited on a glass substrate using a sputtering device. The conductive film was then processed by photolithography to form a first gate electrode. A conductive film 104 having a function as an electrode was formed.

[0596] Next, four insulating films are laminated on the substrate and the conductive film 104 to form a first gate insulating film. The insulating film 106 having a function was formed. The insulating film 106 was formed by plasma enhanced chemical vapor deposition (PEC) The insulating film 106 was formed in a vacuum in a thickness of 50 nm from the bottom. silicon nitride film having a thickness of 300 nm, silicon nitride film having a thickness of 50 nm, A silicon oxynitride film having a thickness of 50 nm was used for each.

[0597] Next, two layers of metal oxide films (a first metal oxide film and a second metal oxide film) are formed on the insulating film 106. Next, the stacked metal oxide films were processed into islands to form metal An oxide film 108 was formed.

[0598] Here, the conditions for forming the metal oxide films of Sample A1 and Sample A2 were made different.

[0599] [Formation of metal oxide film on sample A1] The first metal oxide film of the sample A1 was an In-Ga-Zn film having a thickness of 20 nm, and the second The metal oxide film used was an In-Ga-Zn film with a thickness of 25 nm.

[0600] The first metal oxide film was formed by argon gas at a flow rate of 180 sccm at a substrate temperature of 130°C. The gas and oxygen gas at a flow rate of 20 sccm were introduced into the chamber of the sputtering device, and the pressure was increased. A metal oxide target having indium, gallium, and zinc at a pressure of 0.6 Pa (In:Ga:Zn=4:2:4.1 [atomic ratio]) was applied with 2.5 kW AC power. The ratio of oxygen in the entire deposition gas is referred to as the "oxygen flow rate ratio." The oxygen flow rate ratio during deposition of the first metal oxide film is 10%.

[0601] The second metal oxide film is formed by sputtering under the film forming conditions for the first metal oxide film. Specifically, the introduction of argon gas into the chamber was stopped, and The formation was achieved by introducing oxygen gas at a flow rate of 200sccm into the chamber of the sputtering device. The oxygen flow rate ratio during the formation of the second metal oxide film was 100%.

[0602] [Formation of metal oxide film on sample A2] The first metal oxide film of the sample A2 was an In-Ga-Zn film with a thickness of 20 nm, and the second The metal oxide film used was an In-Ga-Zn film with a thickness of 25 nm.

[0603] The first metal oxide film was formed by argon gas at a flow rate of 140 sccm and a substrate temperature of 170°C. The gas and oxygen gas at a flow rate of 60 sccm were introduced into the chamber of the sputtering device, and the pressure was increased. A metal oxide target having indium, gallium, and zinc at a pressure of 0.6 Pa (In:Ga:Zn=4:2:4.1 [atomic ratio]) was applied with 2.5 kW AC power. The oxygen flow rate during the formation of the first metal oxide film was 30%. do.

[0604] The second metal oxide film was formed by argon gas at a flow rate of 100 sccm at a substrate temperature of 170°C. The gas and oxygen gas at a flow rate of 100 sccm were introduced into the chamber of the sputtering device. The pressure was set to 0.6 Pa, and a metal oxide target having indium, gallium, and zinc was used. A 2.5kW AC power was applied to the In:Ga:Zn alloy (In:Ga:Zn=1:1:1.2 [atomic ratio]). The oxygen flow rate during the deposition of the second metal oxide film was 50%. be.

[0605] Through the above steps, the metal oxide films 108 of Samples A1 and A2 were formed.

[0606] Next, a heat treatment was performed. The heat treatment was performed at a heating temperature of 350° C. in a nitrogen atmosphere for 1 After the heat treatment for 1 hour, the resultant was subjected to a heat treatment for 1 hour in a mixed gas atmosphere of nitrogen and oxygen.

[0607] Next, a conductive film is formed over the insulating film 106 and the metal oxide film 108, and the conductive film is processed. The conductive films 112a and 112b were formed by this. A first titanium film with a thickness of 200 nm and a copper film with a thickness of 200 nm were formed in this order using a sputtering device. Next, the copper film was etched by photolithography, and then a first 50 nm thick film was formed. The titanium film 2 was formed using a sputtering device. The first titanium film and the second titanium film are then etched to form the conductive films 112a and 112b. Formed.

[0608] Next, the exposed surface (back channel side) of the metal oxide film 108 is washed with phosphoric acid. Purified.

[0609] Next, an insulating film is formed on the insulating film 106, the metal oxide film 108, and the conductive films 112a and 112b. A film 114 was formed, and an insulating film 116 was formed on the insulating film 114. 116 is formed continuously in a vacuum using a plasma enhanced chemical vapor deposition (PECVD) device. The insulating film 114 was a silicon oxynitride film having a thickness of 30 nm, and the insulating film 116 was a silicon oxynitride film having a thickness of 400 nm. The silicon oxynitride films used were each 1 nm thick.

[0610] Next, a heat treatment was performed. The heat treatment was performed at a heating temperature of 350° C. in a nitrogen atmosphere for 1 A heat treatment was carried out for 1 hour.

[0611] Next, a conductive film was formed over the insulating film 116. The conductive film was formed by using a sputtering apparatus. An ITSO film with a thickness of 6 nm was formed.

[0612] Next, oxygen is passed through the conductive film by a plasma treatment method to add oxygen to the insulating film 116. As the plasma treatment method, plasma was discharged in an atmosphere containing oxygen gas.

[0613] Next, the conductive film was etched.

[0614] Next, an insulating film 118 was formed on the insulating film 116. The insulating film 118 was formed by plasma chemical vapor deposition. A silicon nitride film having a thickness of 100 nm was formed using a PECVD apparatus.

[0615] Next, openings were formed in desired areas of the insulating film. The etching method was used.

[0616] Next, a conductive film is formed to fill the opening, and the conductive film is processed into an island shape. Then, a conductive film 120a having a function as a second gate electrode was formed. For this purpose, a 100 nm thick ITSO film was formed using a sputtering device.

[0617] Next, an insulating film was formed on the insulating film 118 and the conductive film 120a. An acrylic photosensitive resin with a thickness of 1.5 μm was used.

[0618] In this manner, samples A1 and A2 were prepared.

[0619] [Transistor Id-Vg characteristics] Next, the Id-Vg characteristics of the transistors of Sample A1 and Sample A2 prepared above were measured. The Id-Vg characteristics of the transistor were measured under the following conditions: A voltage applied to the conductive film having the function (hereinafter also referred to as a gate voltage (Vg)) and a second The voltage applied to the conductive film that functions as a gate electrode (hereinafter referred to as the back gate voltage (Vb g) was applied from -15V to +20V in steps of 0.25V. The voltage applied to the conductive film that functions as the source electrode (hereinafter referred to as the source voltage (Vs)) The voltage applied to the conductive film functioning as the drain electrode is set to 0 V (comm). The voltage (hereinafter also referred to as drain voltage (Vd)) was set to 0.1V and 20V.

[0620] 44(A) and (B) show the Id-Vg characteristic results of sample A1 and sample A2, respectively. In FIG. 44(A) and (B), the first vertical axis represents Id(A) and the second vertical axis represents the electric field effect transfer degree(μFE(cm 2 / Vs) and the horizontal axis represents Vg (V). The mobility is a value measured at Vd of 20V.

[0621] [Field effect mobility] Here, the field effect mobility will be described. As an index of the current driving power of a transistor, Field-effect mobility is used. The on-region of a transistor is divided into a linear region and a saturation region. From the characteristics of each region, the drain current is calculated based on the gradual channel approximation. The field effect mobility of a transistor can be calculated based on the analytical expression for the current. When necessary, linear mobility and saturation mobility, respectively. The saturation mobility is expressed by the following formula: 1).

[0622]

number

[0623] In this specification, the curve calculated from the formula (1) is called a mobility curve. 4 shows the mobility curve of the saturation mobility estimated from the Id-Vg characteristics based on equation (1). is doing.

[0624] As shown in Figure 44(A) and (B), the field effect mobility is high under all conditions. It is clear that a transistor with excellent switching characteristics has been fabricated.

[0625] [Gate bias thermal stress test] Next, the results of the stress test on sample A1 are shown in FIG. A bias stress test (GBT test) was used. The GBT test is a type of accelerated test, and Changes in transistor characteristics that occur over a period of use can be evaluated in a short period of time. In this GBT test, the substrate on which the transistor is formed is kept at 60°C. Apply 0V to the source and drain of the transistor, and 30V or -30V to the gate. This state was maintained for 3600 seconds. At this time, a test was performed to apply a positive voltage to the gate. S, the test to apply negative voltage is written as NBTS. Also, 10000lx white LED A voltage of 30V or -30V is applied to the gate while irradiating light. At this time, a test in which a positive voltage was applied to the gate was performed on the PBITS, and a test in which a negative voltage was applied was performed on the PBITS. The exam that will be added is referred to as NBITS.

[0626] The results of the GBT test are shown in Figure 47. In Figure 47, the variation in threshold voltage (ΔVth) is It can be seen that the results are good, at less than ±1V. Good results were obtained in the GBT test. The reason for this is that the transistor included in the sample A1 has a metal oxide film 108. Since the CAC-OS and CAAC-OS films are stacked, a buried channel is formed. The interface between the metal oxide film 108 and the insulating film 114 in the back channel is It can be inferred that the effects of defects and damage have been mitigated.

[0627] [Reliability rating 1] Next, the reliability of the samples A1 and A2 prepared above was evaluated.

[0628] Reliability evaluation is performed by repeatedly applying a pulse voltage to the transistor. was driven and the rate of change in on-current was evaluated.

[0629] The test conditions were as follows: a constant potential of -8 V was applied to the source electrode; The high-level voltage is 20 V, the low-level voltage is 20 V, and the drain electrode is 20 V. A pulse voltage with a filter voltage of -8 V was applied. The pulse voltage was 20 V for a period of 20%, - The 8V period is 80% (i.e., the duty ratio is 20%), and the frequency is about 17.1kH. The name was z.

[0630] In addition, after applying a pulse voltage for a certain period of time, the on-state current of the transistor was measured. The current measurement conditions were a gate voltage (Vg) and a back gate voltage (Vbg) of 15 V. The source voltage (Vs) was set to 0V (comm), and the drain voltage (Vd) was set to 5V. The measurement sampling period was set to 7.5 msec (duty ratio 7.5%).

[0631] The size of the transistors used in the evaluation was the channel length for both Sample A1 and Sample A2. The channel width is 1000 μm.

[0632] FIG. 45(A) shows the on-state currents of samples A1 and A2 estimated from the measured Id-Vg characteristics. In FIG. 45(A), the horizontal axis is time, and the vertical axis is the rate of change of the on-current. is the rate of

[0633] FIG. 45B shows the time it takes for the on-current to change by 50%. For sample A1, it was about 4.2 hours, and for sample A2, it was about 55.5 hours.

[0634] The above results indicate that the transistor including the metal oxide of one embodiment of the present invention has high reliability. It was confirmed that it was a transistor.

[0635] [Reliability rating 2] Next, the reliability evaluation was performed by changing the test conditions. The reliability of three transistors fabricated under the same conditions as in Example 1 was evaluated. The three transistors have channel lengths of 3 μm, 4 μm, and 6 μm, respectively, and channel widths of In reliability evaluation 1 and reliability evaluation 2, the measured samples Since the reliability evaluation results are slightly different,

[0636] The test conditions were as follows: a constant potential of -9 V was applied to the source electrode; The high-level voltage is 20 V, the low-level voltage is 20 V, and the drain electrode is 20 V. A pulse voltage of -9 V was applied. The pulse voltage was 20 V for a period of 20%, - The period of 9V was set to 80% (i.e., the duty ratio was 20%).

[0637] In addition, after applying a pulse voltage for a certain period of time, the on-state current of the transistor was measured. The current measurement conditions were: gate voltage (Vg) and back gate voltage (Vbg) were 15V The source voltage (Vs) is 0V (comm) and the drain voltage (Vd) is 5V. The measurement sampling period was set to 7.5 msec (duty ratio 7.5%).

[0638] The measurement results are shown in Figure 48. Figure 48(A) shows the measurement results in a semi-logarithmic graph, and Figure 48( FIG. 48(A) and FIG. 48(B) show the measurement results in a double logarithmic graph. The vertical axis indicates the measurement time, and the vertical axis indicates the rate of change of the on-current in the reliability evaluation. Therefore, it is expected that the on-current will decrease to 70% due to degradation after about 125,000 seconds. From the above results, the transistor including the metal oxide of one embodiment of the present invention has high reliability. It was confirmed that it was a transistor.

[0639] [Making a transistor] Next, a transistor corresponding to the transistor 100A described above is fabricated. The electrical characteristics of the transistors were evaluated. In this example, the following samples A3 and A4 were prepared. However, the conductive film 120a and the insulating film 120b in the transistors of Sample A3 and Sample A4 were The stacking order of 118 is different from that of transistor 100A.

[0640] Samples A3 and A4 are samples in which transistors are formed. The channel length L is 2 μm, and the channel width W is 50 μm.

[0641] [Preparation method of samples A3 and A4] First, a tungsten film with a thickness of 100 nm was deposited on a glass substrate using a sputtering device. The conductive film was then processed by photolithography to form a first gate electrode. A conductive film 104 having a function as an electrode was formed.

[0642] Next, different insulating films 106 were formed in the samples A3 and A4.

[0643] In the sample A3, four insulating films were laminated on the substrate and the conductive film 104 to form a first gate insulating film. The insulating film 106 of the sample A3 was formed by PECVD. The insulating film 106 of the sample A3 was formed continuously in a vacuum using a 50 mm thick film forming apparatus. nm thick silicon nitride film, 300 nm thick silicon nitride film, 50 nm thick silicon nitride film A silicon oxynitride film having a thickness of 50 nm and a silicon nitride film having a thickness of 50 nm were used.

[0644] In the sample A4, three insulating films were laminated on the substrate and the conductive film 104 to form a first gate insulating film. The insulating film 106 of the sample A4 was formed by PECVD. The insulating film 106 of the sample A4 was formed continuously in a vacuum using a 50 mm thick film forming apparatus. nm thick silicon nitride film, 300 nm thick silicon nitride film, 50 nm thick silicon nitride film In the sample A4, the surface of the insulating film 106 was The resultant was subjected to oxygen plasma treatment.

[0645] Next, two layers of metal oxide films (a first metal oxide film and a second metal oxide film) are formed on the insulating film 106. Next, the stacked metal oxide films were processed into islands to form metal An oxide film 108 was formed.

[0646] The first metal oxide film is a 10 nm thick In-Ga-Zn film, and the second metal oxide film is a 10 nm thick In-Ga-Zn film. The film used was an In-Ga-Zn film with a thickness of 25 nm.

[0647] The first metal oxide film was formed by argon gas at a flow rate of 180 sccm at a substrate temperature of 130°C. The gas and oxygen gas at a flow rate of 20 sccm were introduced into the chamber of the sputtering device, and the pressure was increased. A metal oxide target having indium, gallium, and zinc at a pressure of 0.6 Pa (In:Ga:Zn=4:2:4.1 [atomic ratio]) was applied with 2.5 kW AC power. The oxygen flow rate ratio during the formation of the first metal oxide film was 10%.

[0648] The second metal oxide film is formed by sputtering under the film forming conditions for the first metal oxide film. Specifically, the introduction of argon gas into the chamber was stopped, and The formation was achieved by introducing oxygen gas at a flow rate of 200sccm into the chamber of the sputtering device. The oxygen flow rate ratio during the formation of the second metal oxide film was 100%.

[0649] Next, a heat treatment was performed. The heat treatment was performed at a heating temperature of 350° C. in a nitrogen atmosphere for 1 After the heat treatment for 1 hour, the resultant was subjected to a heat treatment for 1 hour in a mixed gas atmosphere of nitrogen and oxygen.

[0650] Next, a conductive film is formed over the insulating film 106 and the metal oxide film 108, and the conductive film is processed. The conductive films 112a and 112b were formed by this. nm thick tungsten film, 400 nm thick aluminum film, and 100 nm thick titanium film. The films were then formed in sequence using a sputtering device. The conductive film was etched to form conductive films 112a and 112b.

[0651] Next, the exposed surface (back channel side) of the metal oxide film 108 is washed with phosphoric acid. Purified.

[0652] Next, an insulating film is formed on the insulating film 106, the metal oxide film 108, and the conductive films 112a and 112b. A film 114 was formed, and an insulating film 116 was formed on the insulating film 114. The insulating film 116 was formed continuously in a vacuum using a PECVD apparatus. The insulating film 116 is a silicon oxynitride film having a thickness of 400 nm. were used, respectively.

[0653] Next, a heat treatment was performed. The heat treatment was performed at a heating temperature of 350° C. in a nitrogen atmosphere for 1 A heat treatment was carried out for 1 hour.

[0654] Next, a conductive film was formed over the insulating film 116. The conductive film was formed by using a sputtering apparatus. An ITSO film with a thickness of 6 nm was formed.

[0655] Next, oxygen is passed through the conductive film by a plasma treatment method to add oxygen to the insulating film 116. As the plasma treatment method, plasma was discharged in an atmosphere containing oxygen gas.

[0656] Next, the conductive film was etched.

[0657] Next, an insulating film 118 was formed on the insulating film 116. A silicon nitride film having a thickness of 100 nm was formed using this apparatus.

[0658] Next, openings were formed in desired areas of the insulating film. The etching method was used.

[0659] Next, a conductive film is formed to fill the opening, and the conductive film is processed into an island shape. Then, a conductive film 120a having a function as a second gate electrode was formed. As the layer a, an ITSO film having a thickness of 100 nm was formed using a sputtering apparatus.

[0660] Next, an insulating film was formed on the insulating film 118 and the conductive film 120a. A 1.5 μm acrylic photosensitive resin was used.

[0661] In this manner, samples A3 and A4 were prepared.

[0662] [Transistor Id-Vg characteristics] Next, the Id-Vg of ten transistors each of Sample A3 and Sample A4 fabricated as above was measured. The Id-Vg characteristics of the transistor were measured under the following conditions: Vg and V bg was applied from -15V to +15V in steps of 0.25V. Vs was set to 0V. (comm), and Vd was set to 0.1V and 20V.

[0663] FIG. 54(A) shows the Id-Vg characteristics of ten transistors of sample A3. ) shows the Id-Vg characteristics of ten transistors of sample A4. The horizontal axis represents Vg. The vertical axis in Figures 54(A) and (B) represents the logarithmic drain current (Id). The profile group 331 in FIG. 54(A) is for sample A when Vd is 0.1 V. The Id-Vg characteristics of the transistors in profile group 33 in FIG. FIG. 5 shows the Id-Vg characteristics of the transistor of sample A3 when Vd is 20 V. The profile group 341 in FIG. 4(B) is the profile of the transistor of sample A4 when Vd is 0.1 V. The profile group 342 in FIG. 54(B) shows the Id-Vg characteristics. 4 shows the Id-Vg characteristics of the transistor of sample A4 at 100 V.

[0664] As shown in FIGS. 54A and 54B, the transistors of Sample A3 and Sample A4 It can be seen that both have low off-state current and small individual variation. Both the transistor of sample A1 and the transistor of sample A4 have good electrical characteristics. It can be seen that.

[0665] [Gate bias thermal stress test] Next, the GBT test was carried out on the transistors of sample A3 and sample A4. The channel length L of each transistor is 3 μm, and the channel width W is 50 μm. Here, for the GBT test, the substrate on which the transistor is formed is Hold at 0°C, apply 0V to the source and drain of the transistor, and 30V or -30V to the gate. A voltage of 0.01V was applied to the gate and this state was maintained for 3600 seconds. The test that applies a negative voltage is called PBTS, and the test that applies a negative voltage is called NBTS. A voltage of 30V or -30V was applied to the gate while irradiating the device with white LED light of 1x. The state was maintained for 3600 seconds. At this time, a test in which a positive voltage was applied to the gate was performed as PBIT. S, the test in which a negative voltage is applied is denoted as NBITS.

[0666] The results of the GBT test are shown in Figure 55. The variation in threshold voltage of the transistor of sample A3 (ΔV th) is 0.49V for PBTS, 0.04V for NBTS, 0.06V for PBITS, and N The BITS voltage was -0.50 V. The ΔVth of the transistor of sample A4 was 0 V at PBTS. .74V, 0.05V on NBTS, 0.11V on PBITS, -1.96V on NBITS In both the transistors of sample A3 and sample A4, the GBT test The change in Vth was less than 2 V. It was found that both the sensor and the data have good reliability.

[0667] Generally, a transistor uses a hydrogenated amorphous silicon layer as a semiconductor layer in which a channel is formed. In the a-Si:H transistor, a silicon nitride layer is used as the gate insulating layer. According to one aspect of the present invention, silicon nitride is used for the gate insulating layer of the OS transistor. That is, a-Si:H transistor production line can be converted to OS transistor. When converting to a JIS production line, no major equipment changes are required. Relatively easy conversion of Si:H transistor production lines to OS transistor production lines This can be achieved. EXAMPLES

[0668] In this example, we will discuss a display module for verifying operation of an 8K display. The transistor constituting the display module is the same as that of the present invention. A transistor including the metal oxide of one embodiment can be used.

[0669] The 2K or 4K display module has an operating environment that assumes an 8K display. By applying a load equivalent to 8K to the pixel section, operation verification assuming an 8K display was performed. It is possible to fabricate a display module for the

[0670] FIG. 46(A) shows a block diagram of a display module for operational verification. The configuration shown in A) has one source driver for one pixel unit 601 formed on a substrate. The pair of gate drivers 605 includes: It is formed in the same process as the transistors in the pixels and is mounted on the display module. It is preferable that the array is formed by a so-called gate on array method. Moreover, the source driver 603 is preferably mounted on the substrate by a COG method or the like.

[0671] Also, on the substrate, there is provided a terminal portion 607 for connecting to the FPC, and a gate driver 6 605, a wiring 611 connected to the gate driver 605, The wiring 609 is connected to the gate driver 603. The wiring 611 functions as a gate wiring. The line 613 functions as a signal line.

[0672] The pixel section 601 is made up of a plurality of regions 601_1, 601_2, 601_3, 601_4, Between the region 601_1 and the region 601_2, between the region 601_1 and the region 601_3 , between the region 601_2 and the region 601_4, between the region 601_3 and the region 601_4, a pair A load 602 is provided on each of the wirings between the gate drivers 605. The wiring load is a resistor element, a capacitor element, etc. that are provided on the wiring.

[0673] By providing a load 602 appropriately in the pixel section 601 and the driver circuit, It is possible to reproduce different behaviors for each region of the module.

[0674] For example, the region 601_1, the source driver 603, and the gate driver 605 Therefore, in the region 601_1, the signal line and the gate The distortion of the waveform of the signal in each wiring is small, and in the pixel portion 601, the signal is written to the pixel. The conditions for inclusion are the most lenient.

[0675] No load is provided between the region 601_2 and the source driver 603, but the region 60 A load 602 is provided between the gate driver 605 and the gate driver 605. In 601_2, the distortion of the signal waveform of the signal line is small, but the distortion of the signal waveform of the gate wiring is small. The dullness is large.

[0676] A load is provided between the area 601_3 and the source driver 603. There is no load between the region 601_3 and the gate driver 605. In _3, the distortion of the signal waveform of the signal line is large, but the distortion of the signal waveform of the gate wiring is small. small.

[0677] Negative connections are provided between the region 601_4 and the source driver 603 and the gate driver 605. Therefore, in the region 601_4, the signal lines and the gate wiring The waveform of the signal is significantly deformed, and the conditions for writing signals to the pixels in the pixel section 601 are Both are tough.

[0678] FIG. 46(B) is a block diagram of an actual 8K display module. The pixel 623 is provided in the element portion 621. The pixel 623 corresponds to the load 60 in FIG. 46(A) corresponds to the region 601_1 of the pixel section 621 of FIG. The region 601_2 in FIG. 46(A) corresponds to the pixel portion 621 in FIG. The region 601_3 in FIG. 46(A) corresponds to the pixel portion 6 in FIG. The area 601_4 in FIG. 46(A) corresponds to the area 621_3 in FIG. 46(B). This corresponds to the region 621_4 of the element part 621.

[0679] As shown in FIG. 46(A), a load 602 is provided in a pixel section 601, so that a single display In the play module, it is possible to verify pixel writing operations under four conditions. In addition, the source driver and gate driver are capable of driving a load equivalent to an 8K display. It is possible to verify the operation of the above. The module can be used to verify the operation of an 8K display module. EXAMPLES

[0680] In this embodiment, a large 8K liquid crystal display device is realized by using a transistor according to one embodiment of the present invention. To examine the possibilities, we performed a simulation and will now explain the results.

[0681] [Verification model] The specifications of the liquid crystal display device examined are shown in Table 3. The screen size of the liquid crystal display device was 65 inches. The pixel configuration is a striped arrangement of three sub-pixels for RGB. The pixel circuit contains a CAC-OS transistor. The transistor is assumed to have a channel etch structure with a film. The gate driver is built-in. The source driver is an external IC. When operating at a frame frequency of 120Hz The time required to write a video signal in the above was confirmed by simulation.

[0682] [Table 3]

[0683] Figure 49 shows a schematic diagram of the liquid crystal display device under consideration. It is desirable to have a structure that can minimize the time constant within the element domain. The gate selection signals are input from both sides of the gate line. By using this configuration, compared to when gate drivers are placed on only one side of the pixel area, This reduces the time constant of the gate line by a factor of four, shortening the charge and discharge time of the gate line. In order to maximize the period available for writing video signals, Two rows of gate lines are connected to a buffer, which selects two rows of gate lines at the same time and transmits two rows of video signals. This allows the gate driver shift register stages to be written simultaneously. The number of steps can be reduced from the usual 4320 to half, 2160, and one horizontal selection period can be reduced to 1. It can be lengthened from 92μs to 3.83μs.

[0684] FIG. 50 shows a circuit diagram of a pixel included in a liquid crystal display device. It has three sub-pixels corresponding to red (R), green (G), and blue (B). Each of the transistors M1, M2, M3, M4, M5, M6, M7, M8, M9, M10, M11, M12, M13, M14, M15, M16, M17, M18, M19, M20, M21, M22, M23, M24, M25, M36, M37, M48, M50, M51, M52, M61, M72 The transistor M1, which functions as a Either the drain or the drain is connected to the source line SL. The liquid crystal display 1 is provided between the other of the source or drain of the liquid crystal display 1 and the common potential line CsCOM. The crystal element LC is connected to the other of the source or drain of the transistor M1 and the common potential line TCOM The structure of one subpixel is the simplest, 1Tr + 1C / cel. l, but in order to write video signals for two rows at the same time, two sources are connected to the pixels in one column. In the odd-numbered rows, one source line is provided. In the even-numbered pixels, the source line (e.g., SL11) is connected to the transistor M1, and the other source line A line (eg, SL12) is connected to transistor M1.

[0685] Here, a block diagram of the configuration used in the simulation is shown in FIG. For the gate driver transistor, the actual measurement value of the transistor with CAC-OS film The model parameters were extracted based on the above. A behavior model was used for the source driver. In addition, the parasitic capacitance of the gate line and source line in the pixel area and the parasitic capacitance of the CLK line of the gate driver An RC load model was used for the components. The boundary element method was used to extract the parasitic capacitance and resistance. The pixel with the largest RC load in the pixel area requires the maximum time required for writing the video signal. The time was calculated.

[0686] Figure 52 shows a timing chart for the write operation to the pixels. Writing to a transistor in the previous row is performed after turning off the transistor M1 in the previous row. The time required to write to the pixel (c) is the time from when the CLK signal is input to the gate driver. From this, the time required for transistor M1 to turn off ((a) gate line fall time) and , the time from when a video signal is input until the potential in the pixel actually reaches the potential of the video signal (b) Source line rise time) and (c) Gate line fall time. The source line rise time is the period from when the source line reaches 75% of the target amplitude to when the source line reaches 95% of the target potential. The time required to write to the pixel was calculated from the total time. The time (c) required to write to the If this is the case, it can be determined that the liquid crystal display device is operable.

[0687] [Calculation result] Table 4 shows the extraction results of the parasitic resistance and parasitic capacitance of the gate line, source line, and gate driver CLK line. The results of extracting the pixel capacitance are also shown. Using these extraction results, the transient solution is Analysis was performed.

[0688] [Table 4]

[0689] Table 5 shows the calculation results of the gate line fall time and source line rise time by transient analysis. show.

[0690] [Table 5]

[0691] The total time of the gate line fall time and the source line rise time is 3 If the time is shorter than 0.83μs, it indicates that operation is possible. The time required for loading (3.51μs) is shorter than one horizontal selection period (3.83μs). It was confirmed that the liquid crystal display device was able to operate.

[0692] Next, Figure 53 shows the relationship between the field effect mobility of a transistor and the time required to write to a pixel. The vertical axis shows the time required to write to a pixel, and the horizontal axis shows the CAC- The field-effect mobility of a transistor with an OS film is set to 1. It is clear that the lower the field effect mobility, the longer it takes to write to a pixel. In addition, when the parameter of the field effect mobility is reduced to less than about 0.75, the image The time required for writing data becomes longer than one horizontal selection period, and the liquid crystal display device cannot be operated. The result was that it was not possible to do this.

[0693] By using transistors with CAC-OS film, it is possible to achieve a high resolution of 8K and Even large display panels of up to 120 inches can be driven at a high frame frequency of 120Hz. It was confirmed that: EXAMPLES

[0694] In this example, a transistor of one embodiment of the present invention was manufactured and its reliability was evaluated.

[0695] [Making a transistor] First, a transistor corresponding to the transistor 100A described above was fabricated. In this example, the following sample B was fabricated. The stacking order of the conductive film 120a and the insulating film 118 is different from that of the transistor 100A.

[0696] Sample B is a sample in which a transistor is formed, and the channel length L is 4 μm and the channel width W is 1000 μm.

[0697] [Preparation method of sample B] First, a tungsten film with a thickness of 100 nm was deposited on a glass substrate using a sputtering device. The conductive film was then processed by photolithography to form a first gate electrode. A conductive film 104 having a function as an electrode was formed.

[0698] Next, four insulating films are laminated on the substrate and the conductive film 104 to form a first gate insulating film. The insulating film 106 having a function was formed. The insulating film 106 was formed by plasma enha...

Claims

1. a pixel portion including a first transistor and a capacitor element electrically connected to the first transistor; a circuit provided outside the pixel portion and having a second transistor; the first transistor has a gate electrode and a first metal oxide film overlapping the gate electrode and having a first channel region; the capacitance element has a second metal oxide film having a function as a capacitance electrode; the second transistor includes a third metal oxide film having a second channel region, a first conductive layer provided above the second channel region and overlapping the second channel region, and a second conductive layer provided below the second channel region and overlapping the second channel region; the second conductive layer is electrically connected to the first conductive layer; the first to third metal oxide films are provided in contact with an upper surface of the same insulating film, the insulating film has a region that functions as a gate insulating film and a region that functions as a dielectric film of the capacitance element, Each of the first to third metal oxide films has a first region having indium oxide or indium zinc oxide and a second region having gallium oxide or gallium zinc oxide, The semiconductor device, wherein the first region and the second region are dispersed or distributed in a mosaic pattern.

2. a pixel portion including a first transistor and a capacitor element electrically connected to the first transistor; a circuit provided outside the pixel portion and having a second transistor; the first transistor has a gate electrode and a first metal oxide film overlapping the gate electrode and having a first channel region; the capacitance element has a second metal oxide film having a function as a capacitance electrode; the second transistor includes a third metal oxide film having a second channel region, a first conductive layer provided above the second channel region and overlapping the second channel region, and a second conductive layer provided below the second channel region and overlapping the second channel region; the second conductive layer is electrically connected to the first conductive layer; the first to third metal oxide films are provided in contact with an upper surface of the same insulating film, the insulating film has a region that functions as a gate insulating film and a region that functions as a dielectric film of the capacitance element, the second metal oxide film has a region having a higher hydrogen concentration than the first metal oxide film and the third metal oxide film; Each of the first to third metal oxide films has a first region having indium oxide or indium zinc oxide and a second region having gallium oxide or gallium zinc oxide, The semiconductor device, wherein the first region and the second region are dispersed or distributed in a mosaic pattern.

3. a pixel portion including a first transistor and a capacitor element electrically connected to the first transistor; a circuit provided outside the pixel portion and having a second transistor; the first transistor has a gate electrode and a first metal oxide film overlapping the gate electrode and having a first channel region; the capacitance element has a second metal oxide film having a function as a capacitance electrode; the second transistor includes a third metal oxide film having a second channel region, a first conductive layer provided above the second channel region and overlapping the second channel region, and a second conductive layer provided below the second channel region and overlapping the second channel region; the second conductive layer is electrically connected to the first conductive layer; the first to third metal oxide films are provided in contact with an upper surface of the same insulating film, the insulating film has a region that functions as a gate insulating film and a region that functions as a dielectric film of the capacitance element, In a cross-sectional view in a channel length direction of the first transistor, a length of the second metal oxide film is greater than a length of the first metal oxide film, Each of the first to third metal oxide films has a first region having indium oxide or indium zinc oxide and a second region having gallium oxide or gallium zinc oxide, The semiconductor device, wherein the first region and the second region are dispersed or distributed in a mosaic pattern.

4. a pixel portion including a first transistor and a capacitor element electrically connected to the first transistor; a circuit provided outside the pixel portion and having a second transistor; the first transistor has a gate electrode and a first metal oxide film overlapping the gate electrode and having a first channel region; the capacitance element has a second metal oxide film having a function as a capacitance electrode; the second transistor includes a third metal oxide film having a second channel region, a first conductive layer provided above the second channel region and overlapping the second channel region, and a second conductive layer provided below the second channel region and overlapping the second channel region; the second conductive layer is electrically connected to the first conductive layer; the first to third metal oxide films are provided in contact with an upper surface of the same insulating film, the insulating film has a region that functions as a gate insulating film and a region that functions as a dielectric film of the capacitance element, In a cross-sectional view in a channel length direction of the first transistor, a length of the second metal oxide film is greater than a length of the first metal oxide film, the second metal oxide film has a region having a higher hydrogen concentration than the first metal oxide film and the third metal oxide film; Each of the first to third metal oxide films has a first region having indium oxide or indium zinc oxide and a second region having gallium oxide or gallium zinc oxide, The semiconductor device, wherein the first region and the second region are dispersed or distributed in a mosaic pattern.

Citation Information

Patent Citations

  • Oxide semiconductor film and semiconductor device

    JP2011100979A

  • Liquid crystal display device and electronic device including the liquid crystal display device

    JP2011141522A

  • Display device and electronic device including the same

    JP2011141524A

  • Stable amorphous metal oxide semiconductors

    JP2012502486A

  • Semiconductor device

    JP2014007399A