Tube with insertion port and method for manufacturing tube with insertion port

Cold tandem welding with two materials efficiently forms protrusions on pipe bodies, addressing time and quality issues in existing welding methods, ensuring precise and robust construction.

JP7565713B2Active Publication Date: 2024-10-11KURIMOTO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020105893
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-19
Publication Date
2024-10-11
Estimated Expiration
2040-06-19

AI Technical Summary

Technical Problem

Existing methods for forming protrusions on the outer periphery of insertion openings in pipe bodies are time-consuming, require significant effort, and often result in poor quality due to welding challenges, leading to material waste or breakage.

Method used

A method using cold tandem welding with two welding materials, where a first welding material forms a molten part on the outer surface, followed by a second welding material to create a protrusion with controlled penetration depth, enhancing precision and efficiency.

Benefits of technology

The method allows for easy and precise formation of protrusions with improved weld quality, reducing time and material waste while maintaining structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007565713000001
    Figure 0007565713000001
  • Figure 0007565713000002
    Figure 0007565713000002
  • Figure 0007565713000003
    Figure 0007565713000003
Patent Text Reader

Abstract

To easily and accurately form a protrusion on the outer periphery of an insertion port by welding.SOLUTION: In a method of manufacturing a pipe body P having an insertion port 1 at one end in a pipe axis direction provided with a protrusion 10 protruding outward in a radial direction, first and second welding materials 21 and 22 are used; a melting zone W is formed on an outer surface 1a of the insertion port 1 by an arc generated by energizing the first welding material 21; and the second welding material 22 is applied to the melting zone W in an unenergized state before the hardening of the melting zone W so that the protrusion 10 can be formed by weld overlaying.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a tube having an insertion port and a method for manufacturing a tube having an insertion port. [Background technology]

[0002] Conventionally, there are pipes used to transport various fluids, and their joints have an expansion and contraction function and a separation prevention function. This type of joint structure is also called an earthquake-resistant pipe joint. For example, as shown in FIG. 5, a protrusion 10 provided on the outer periphery of an insertion port 1 of a pipe P engages with a lock ring 4 fitted into an inner peripheral groove of a socket 2 of another opposing pipe P to exert a disengagement prevention function. In addition, the protrusion 10 of the insertion port 1 moves a predetermined distance (corresponding to sections A and B in the figure) between the inner back end surface 3 of the socket 2 and the lock ring 4, thereby enabling expansion and contraction in the pipe axial direction. In addition, a rubber ring 5 is provided between the insertion port 1 and the socket 2, thereby ensuring liquid-tightness between the outer surface 1a of the insertion port 1 and the inner surface 2a of the socket 2. For example, a pipe P having an insertion port 1 is described in Patent Document 1.

[0003] The projection on the outer periphery of the insertion port is generally formed by fitting a metal ring around the outer periphery of the tube and fixing the ring to the outer surface of the tube by welding, etc. A method of forming the projection on the insertion port by welding a ring to the outer surface of the tube is described, for example, in Patent Document 2. Also, a method of forming the projection on the insertion port by depositing weld metal is described, for example, in Patent Document 3. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2012-77788 A [Patent Document 2] Japanese Patent Application Publication No. 9-122910 [Patent Document 3] Patent No. 6082087 Summary of the Invention [Problem to be solved by the invention]

[0005] However, the method of forming a protrusion by welding a ring as in Patent Document 2 has the problem that fitting the ring is time-consuming and requires a lot of time for the welding work and the processing before and after the welding. Also, the method of forming a protrusion by depositing weld metal as in Patent Document 3 has the problem that the welding takes a lot of time because the amount of welded beads is large. Also, in the case of a method involving welding, it is difficult to maintain the quality of the welded part, and poor construction may cause excessive penetration into the tube body, which is the base material, resulting in wasting material and making the tube body more susceptible to breakage.

[0006] SUMMARY OF THE PRESENTING EMBODIMENT An object of the present invention is to easily and accurately form a protrusion on the outer periphery of the insertion port by welding. [Means for solving the problem]

[0007] In order to solve the above problems, the present invention employs a method for manufacturing a tube having a protrusion protruding radially outward from an insertion port at one end in the tube axial direction, in which a first welding material and a second welding material are used, an arc is generated by passing an electric current through the first welding material to form a molten portion on the outer surface of the insertion port, and before the molten portion hardens, the second welding material is applied to the molten portion without passing an electric current through it, thereby forming the protrusion by weld build-up.

[0008] In this case, a configuration can be adopted in which a penetration portion in which the weld metal from the first welding material and the second welding material is fused with the base material of the insertion port is formed at a depth from the outer surface of the insertion port to a depth of 10% or more and less than 80% of the thickness of the base material of the insertion port.

[0009] In addition, in order to solve the above problems, the present invention employs a tube body having a protrusion protruding radially outward at an insertion port at one end in the axial direction, the protrusion being made of weld metal and protruding radially outward beyond the outer surface of the insertion port, and a penetration portion located on the inner diameter side of the protrusion and in which the base material of the insertion port and the weld metal are fused, the penetration portion extending from the outer surface of the insertion port to a depth of 10% or more but less than 80% of the thickness of the base material of the insertion port. Effect of the Invention

[0010] According to the present invention, the projection on the outer periphery of the insertion port can be easily and accurately formed by welding. [Brief description of the drawings]

[0011] [Figure 1] FIG. 1 is a cross-sectional view showing an embodiment of the present invention. [Diagram 2] Cross-sectional view showing the relative positions of the base material and the welding equipment during welding [Diagram 3] FIG. 1 is a perspective view showing the positional relationship between the base material and the welding device during welding. [Figure 4] FIG. 2 is a cross-sectional view showing a modification of FIG. 1; [Diagram 5] Vertical cross section of joint DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] One embodiment of the present invention will be described with reference to Figures 1 to 4. This embodiment relates to a tube P having a protrusion 10 protruding radially outward from an insertion port 1 at one end in the tube axial direction, and a manufacturing method for the tube P. The main configuration of the tube P is as shown in Figure 5 used in the explanation of the conventional example, so the explanation will be omitted and the following explanation will focus on the configuration of the protrusion 10 of the insertion port 1, which is a feature of the present invention.

[0013] The pipe body P has an insertion port 1 at one end in the pipe axis direction and a socket 2 at the other end in the pipe axis direction, and the insertion port 1 has a protrusion 10 that protrudes radially outward from the outer surface 1a of the insertion port 1 continuously around the entire circumference of the pipe axis (see FIG. 5). This protrusion 10 is composed of a weld buildup formed from a weld metal. That is, a weld buildup (weld bead) is formed on the metallic base material that constitutes the insertion port 1, and the portion formed by the weld metal becomes the protrusion 10. Here, although it is said that the protrusion 10 is composed of a weld metal, this does not exclude the case where the material that constitutes the protrusion 10 includes the base material of the insertion port 1 melted into the weld metal.

[0014] 1 and 4, the inner diameter side of the protrusion 10 has a penetration portion 11 which penetrates to a depth t1 on the inner diameter side from the outer surface 1a of the insertion port 1 and fuses the base material of the insertion port 1 with the weld metal. The maximum depth t1 of the penetration portion 11 reaches a depth from the outer surface 1a of the insertion port 1 that is 10% to 80% of the thickness t0 of the base material of the insertion port 1.

[0015] The tube P before the protrusion 10 of the insertion port 1 is formed is manufactured by centrifugal casting. In centrifugal casting, a cylindrical mold is placed on rollers that rotate by a driving force, and while rotating the mold around its axis, molten metal is poured into the mold and the molten metal is hardened to form the tube P. The mold is provided with a dam to prevent the poured molten metal from leaking out. After hardening, the tube P is pulled out of the mold. The material of the tube P is adjusted by a specified heat treatment or the like, and then the protrusion 10 of the insertion port 1 is processed.

[0016] 2 and 3 show a welding device 20 for processing the projection 10. This welding device 20 is a device for performing cold tandem welding, and includes an arc welding torch 23 for supplying a first welding material 21 for arc welding in an energized state, and a welding material supply device 24 for supplying a second welding material 22 in a non-energized state. The arc welding torch 23 and the welding material supply device 24 are connected by a connecting member 25 and maintained at a predetermined distance. This predetermined distance can be increased or decreased by adjustment.

[0017] The arc welding torch 23 uses a delivery device 28 to deliver the first welding material 21 to a welding position a on the outer surface 1a of the insertion port 1, which is the base material. The first welding material 21 functions as an electrode for passing a current, and a welding current supplied from a power source 27 is passed through the first welding material 21 to generate an arc between the first welding material 21 and the base material. As the first welding material 21, a known welding wire, for example, FeNi φ0.8 to 1.6 mm, can be used. In addition, as the first welding material 21, various materials such as a known solid wire, flux wire, various welding rods, and strip electrodes can be used. In this embodiment, a welding wire is used as the first welding material 21, and is hereinafter referred to as the first welding wire 21.

[0018] The welding material supply device 24 uses a delivery device 26 to deliver the second welding material 22 toward the welding position b on the outer surface of the insertion port 1, which is the base material, without passing current through it. As the second welding material 22, for example, FeNi φ0.8 to 1.6 mm can be used. In addition, as the second welding material 22, various materials such as well-known solid wire, flux wire, various welding rods, and strip electrodes can be used. In this embodiment, a welding wire is used as the second welding material 22, and will be referred to as the second welding wire 22 hereinafter.

[0019] Next, a method for manufacturing the pipe P according to this embodiment, in particular a method for forming the protrusion 10 of the insertion port 1, will be described.

[0020] 3, the tube P is held by a gripping device H and can rotate around the tube axis as indicated by an arrow R in the figure. This rotation of the tube P causes the arc welding torch 23 and the welding material supply device 24, which are connected by a connecting member 25, to move relatively along the tube circumference with respect to the insertion port 1 of the tube P, which is the base material. During this relative movement, it is desirable that the welding material supply device 24 be disposed forward of the arc welding torch 23 along the rotation direction R of the tube P. In other words, it is desirable that the position a of the first welding wire 21 be forward of the position b of the second welding wire 22 with respect to the moving direction of the welding point on the outer surface 1a of the insertion port 1 (the direction opposite to the rotation direction R of the tube P).

[0021] In this manner, the first welding wire 21 and the second welding wire 22 are used, and the first welding wire 21 is energized to generate an arc to form a molten portion W on the outer surface 1a of the insertion port 1 as shown in Fig. 2, and before the molten portion W hardens, the second welding wire 22 is applied to the molten portion W in a non-energized state. As a result, a protrusion 10 that protrudes toward the outer diameter side is formed on the outer surface 1a of the insertion port 1 by a weld buildup (weld bead). At this time, the second welding wire 22 is in a non-energized state, but is heated by being applied to the molten portion W generated by the arc of the first welding wire 21, and the metal of the second welding wire 22 melts and is supplied to the molten portion W as a weld metal.

[0022] At the same time, the penetration portion 11, in which the weld metal of the first welding wire 21 and the second welding wire 22 are fused with the base metal of the insertion port 1, is formed at a depth of 10% or more and less than 80% of the thickness t0 of the base metal of the insertion port 1 from the outer surface 1a of the insertion port 1. Here, it is more preferable that the ratio of the maximum depth t1 of the penetration portion 11 to the thickness t0 of the base metal is 20% or more and less than 60%. If this depth ratio is too low, the strength of the protrusion 10 may be insufficient due to insufficient penetration, and if this depth ratio is too large, the base metal may be penetrated. The inventors have discovered that the above-mentioned cold tandem welding method is optimal for setting such a depth ratio.

[0023] That is, by using cold tandem welding when forming the protrusion 10 of the insertion port 1 by weld build-up, the amount of weld metal supplied per unit time increases, and the amount of melting per unit time (welding speed) can be increased. Also, by adding a non-current-carrying second welding wire 22 to the fusion zone W, the molten pool of the metal material in the fusion zone W can be cooled, making it possible to reduce the penetration depth and prevent the weld metal from dripping. Due to these effects, it is possible to obtain the desired bead shape of the protrusion 10 at the same speed as with the conventional welding method using a ring.

[0024] As shown by the chain line in Fig. 1, the completed shape of the protrusion 10 has a flat cylindrical portion 10d in the center, and a tapered surface 10c on the tip 1b side of the insertion port 1 on the right side of the figure that gradually reduces in diameter toward the tip 1b. Also, a step portion 10b is formed between the rear end side and the outer surface 1a of the insertion port 1. As a result, the cross section of the protrusion 10 is trapezoidal in any cross section passing through the tube axis.

[0025] The shape of the protrusion 10 immediately after welding, as shown by the solid line in Fig. 1, is a cross-sectional shape having a bead surface 12 that is slightly larger than the finished shape of the protrusion 10, so this is cut to form the finished shape. In Fig. 1, the tip 10a of the protrusion 10 coincides with the tip 1b of the insertion port 1, so the pipe P is cut along the line indicated by the symbol S in the figure, but this cutting can be performed according to the positional relationship between the tip 10a of the protrusion 10 and the tip 1b of the insertion port 1, and is not an essential step. The shaping of the protrusion 10 into the finished shape can be performed by a combination of a high-frequency grinder and lathe processing.

[0026] In FIG. 1, the shape of the protrusion 10 immediately after welding is a shape having two peaks 12a, 12b on the bead surface 12 due to two-layer welding in which the protrusion 10 is completed during two revolutions around the tube axis. Similarly, the penetration portion 11 also has two valleys 11a, 11b whose penetration depth is slightly deeper than the surroundings. By performing such two-layer welding or three or more layers of welding, the protrusion 10 can be formed more easily and with higher accuracy. However, as shown in FIG. 4, it is also possible to perform one-layer welding in which the protrusion 10 is completed during one revolution around the tube axis. In the case of one-layer welding, the shape of the protrusion 10 immediately after welding is a shape having one peak 12a on the bead surface 12 and one valley 11a whose penetration depth is slightly deeper than the surroundings in the penetration portion 11.

[0027] In the experiment, FeNi φ1.6 mm was used as the first welding wire 21 and the second welding wire 22, and the rotation speed on the circumferential surface of the tube P with a tube thickness of 6 mm was 25 mm / s, the supply amount of the first welding wire 21 was 900 cm / min, and the supply amount of the second welding wire 22 was 500 cm / min, so that the amount of weld metal was 160 g in the entire protrusion 10 in two-layer welding, and a ratio of the penetration depth to the tube thickness of about 33% was ensured, and good results were obtained. In addition, in one-layer welding, FeNi φ1.6 mm was also used, and the rotation speed on the circumferential surface of the tube P was 12.5 mm / s, the supply amount of the first welding wire 21 was 900 cm / min, and the supply amount of the second welding wire 22 was 600 cm / min, so that the amount of weld metal was 170 g in the entire protrusion 10, and a ratio of the penetration depth to the tube thickness of about 60% was ensured, and good results were obtained. In this regard, in the conventional method of forming the protrusion 10 using a ring, when FeNi φ1.2 mm was used, the amount of weld metal for the entire protrusion 10 was 59 g when the rotation speed on the circumferential surface of the tube P was 25 mm / s and the supply rate of the welding wire was 920 cm / min. That is, it can be understood that the use of cold tandem welding in this invention realizes an increase in the amount of melting (welding speed) per unit time.

[0028] In this embodiment, the tube P before the projection 10 of the insertion port 1 is formed is manufactured by centrifugal casting, but the manufacturing method of the tube P before the projection 10 is formed may be other than centrifugal casting, for example, a pouring casting method in which molten metal is poured into a mold by gravity and solidified. Also, this invention can be applied to various tubes P as long as the insertion port 1 for forming the projection 10 is made of metal compatible with welding. [Explanation of symbols]

[0029] 1 Insertion port 1a External surface 10 Protrusion 11 Welding section 20 Welding equipment 21 First welding material (first welding wire) 22 Second welding material (second welding wire) P body

Claims

1. A method for manufacturing a tube (P) having a protrusion (10) protruding radially outward from an insertion port (1) at one end in the tube axial direction, comprising the steps of: The method for manufacturing a tube includes using a first welding material (21) and a second welding material (22), forming a molten portion (W) on an outer surface (1a) of the insertion hole (1) by an arc generated by passing an electric current through the first welding material (21), and applying the second welding material (22) to the molten portion (W) without passing an electric current through it before the molten portion (W) hardens, thereby forming the protrusion (10) by weld build-up.

2. The method for manufacturing a tube body according to claim 1, wherein a penetration portion (11) formed by fusing the weld metal of the first welding material (21) and the second welding material (22) with the base material of the insertion port (1) is formed at a depth from the outer surface (1a) of the insertion port (1) that is 10% or more and less than 80% of the wall thickness (t0) of the base material of the insertion port (1).

3. A tube body (P) manufactured by centrifugal casting, the tube body (P) having a protrusion (10) protruding radially outward from an insertion port (1) at one end in the tube axial direction, a protrusion (10) made of weld metal provided in the insertion port (1) and protruding radially outward from an outer surface (1a) of the insertion port (1); a penetration portion (11) located on the inner diameter side of the protrusion (10) and in which the base material of the insertion port (1) and the weld metal are fused together, The penetration portion (11) extends from the outer surface (1a) of the insertion port (1) to a depth of 10% or more and less than 80% of the wall thickness (t0) of the base material of the insertion port (1); The protrusion (10) is a pipe having a cylindrical portion (10d) formed on its outer surface so as to exert a function of preventing the earthquake-resistant pipe joint from coming loose.

Citation Information

Patent Citations

  • Drive circuit of brushless DC motor

    JP1985082087A

  • Filter wire type magnetic control MIG welding method

    JP1987124077A

  • Method for forming projection at insert port of tube

    JP1997122910A

  • Automatic arc welding equipment

    JP1997150265A

  • Production of spiral steel tube

    JP1998156534A