Magnetic Parts

The magnetic component with a resin hollow container and colorimetric properties addresses the challenge of determining deterioration in high-temperature environments, ensuring reliable performance and efficient manufacturing.

JP7567064B2Active Publication Date: 2024-10-15NITERRA MATERIALS CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023549383
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-09-27
Filing Date
2022-07-01
Publication Date
2024-10-15
Estimated Expiration
2042-07-01

AI Technical Summary

Technical Problem

Existing magnetic components used in noise suppression elements for switching power supplies face challenges in determining the degree of deterioration when used in high-temperature environments, as their magnetic properties degrade over time without visible external changes.

Method used

A magnetic component design featuring a resin hollow container with a donut-shaped magnetic core, where the resin exhibits specific colorimetric properties that change with temperature exposure, allowing for visual assessment of deterioration through JIS Z8721 color standards, and a lid formation method using bent extensions to secure the core without adhesives.

Benefits of technology

Enables easy determination of magnetic property degradation by color change and enhances manufacturing efficiency with reduced material waste and improved heat resistance, ensuring reliable performance in high-temperature conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567064000004
    Figure 0007567064000004
  • Figure 0007567064000005
    Figure 0007567064000005
  • Figure 0007567064000006
    Figure 0007567064000006
Patent Text Reader

Abstract

A magnetic component 8 of an embodiment has a hollow container 1 made of resin in which a doughnut-shaped magnetic core 5 is housed, wherein the resin of which the hollow container 1 is formed exhibits a white to gray color having a chromatic value C of 0 (achromatic) to 2 inclusive, and a lightness V of 8 or more as defined by JIS Z8721: "Colour specification − Specification according to their three attributes". Further, the hollow container 1 has a structure comprising an inner wall portion 2 formed so as to create a hollow portion 4, an outer wall portion 3 formed so as to surround the inner wall portion 2, and a bottom portion 6 provided at one end of each of the inner wall portion 2 and the outer wall portion 3 so as to close a space between the inner wall portion 2 and the outer wall portion 3, wherein the doughnut-shaped magnetic core 5 is housed in the space between the inner wall portion 2 and the outer wall portion 3.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The embodiments relate to a magnetic component. [Background technology]

[0002] Noise from switching power supplies installed in electronic devices is regulated by classes, as typified by the FCC (Federal Communications Commission, USA). Noise in power supplies is generated by a variety of causes, but it is mainly generated around semiconductor elements that turn large amounts of power on and off. High-frequency components in particular travel through the air as radiated noise, causing various electronic devices to malfunction. For this reason, regulatory values ​​are set for each frequency band. In switching power supplies, noise countermeasures are implemented for semiconductor elements, mainly MOS-FETs and diodes. Typical examples of noise countermeasures for MOS-FETs and diodes include noise countermeasures using CR snubbers and ferrite beads.

[0003] Noise countermeasures are selected based on the balance between effectiveness, cost, and installation space. When performance is a consideration, Co-based amorphous materials are the mainstream noise countermeasures. Co-based amorphous materials have excellent magnetic properties, making them more effective at reducing noise than ferrite beads. Also, instead of Co-based amorphous materials, magnetic ribbons made from Fe-based amorphous or Fe-based magnetic alloys with microcrystalline crystals may be used.

[0004] Amorphous and even microcrystalline magnetic alloys generally exhibit electrical conductivity, so when using leads or windings, they must be housed in an insulating resin case or must be provided with an exterior insulation such as an epoxy coating. Magnetic components made by winding a thin metal strip, unlike press-molded products such as ferrite, tend to have shape variations, so epoxy coating can result in dimensional variations. Also, when winding thick wires of about φ1 to φ2 mm around magnetic components, insulating resin cases are generally used to withstand the stress.

[0005] When a noise suppression element is incorporated into an electric circuit such as a power supply, it may be used in a high-temperature environment for a long period of time due to heat generation within the circuit. In this case, the magnetic properties of the noise suppression element deteriorate, reducing its noise suppression effect. However, since the current noise suppression element does not show any visible changes in appearance, it is not possible to determine how high the temperature or the length of time it has been used. This makes it difficult to determine the degree of product degradation. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Patent No. 5175843 Summary of the Invention [Problem to be solved by the invention]

[0007] For example, Japanese Patent No. 5175843 (Patent Document 1) uses a hollow container made of insulating resin such as PBT (polybutylene terephthalate), PET (polyethylene terephthalate), or LCP (liquid crystal polymer). The hollow container made of insulating resin in Patent Document 1 had excellent strength. Therefore, it was not damaged even when a lead or the like was inserted. On the other hand, there was little change in the appearance of the magnetic component even after long-term use as a noise suppression element. Therefore, even if the doughnut-shaped magnetic core housed inside had deteriorated, it was not possible to tell from its appearance. The problem to be solved by the present invention is to provide a magnetic component that allows easy determination of the degree of deterioration when used for a long period of time in a high-temperature environment. [Means for solving the problem]

[0008] In order to solve the above problems, a magnetic component according to an embodiment has a resin hollow container that houses a doughnut-shaped magnetic core, and the resin forming the hollow container exhibits a white to gray color, with a chroma C of 0 (achromatic) to 2 and a brightness V of 8 or greater, as defined in JIS Z8721 "Method of displaying color - Display by three attributes." This hollow container has an inner wall formed to create a hollow space, an outer wall formed to surround the inner wall, and a bottom provided at one end of the inner wall and the outer wall to seal the gap between the inner wall and the outer wall, and the doughnut-shaped magnetic core is housed between the inner wall and the outer wall. [Brief explanation of the drawings]

[0009] [Figure 1] FIG. 1 is a perspective view showing a hollow container for a magnetic component according to a first embodiment. [Figure 2] 1 is a cross-sectional view showing the configuration of a magnetic component according to a first embodiment. [Figure 3] FIG. 10 is a cross-sectional view showing the structure of the magnetic component according to the second embodiment before the lid portion is folded. [Figure 4] FIG. 10 is a cross-sectional view showing the structure of the magnetic component according to the second embodiment after the lid portion is bent. [Figure 5] FIG. 10 is a perspective view showing the configuration of an insertion-lead magnetic component according to a third embodiment. [Figure 6] FIG. 10 is a perspective view showing the rectangular parallelepiped hollow container according to the fourth embodiment before the lid portion is folded. [Figure 7] FIG. 10 is a perspective view showing the rectangular parallelepiped hollow container according to the fourth embodiment after the lid portion is folded. [Figure 8] FIG. 10 is a perspective view showing the configuration of a rectangular lead insertion type magnetic component according to a fifth embodiment. [Figure 9] FIG. 10 is a perspective view showing the configuration of a wound-lead magnetic component according to a fifth embodiment. DETAILED DESCRIPTION OF THE INVENTION

[0010] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Fig. 1 is a perspective view showing a hollow container 1 for a magnetic component 8 according to one embodiment of the present invention. A hollow container 1 shown in FIG. 1 houses a conductive doughnut-shaped magnetic core 5 between its inner wall 2 and outer wall 3 to form a magnetic component 8. The doughnut-shaped magnetic core 5 is not particularly limited, and may be any soft magnetic material having a hollow shape. Ferrite, permalloy, amorphous magnetic alloy, and Fe-based magnetic alloy having microcrystals are applicable as the soft magnetic material constituting the doughnut-shaped magnetic core 5. Various forms of the doughnut-shaped magnetic core 5 can be used, such as a wound or laminated body of a soft magnetic alloy ribbon, a sintered body of soft magnetic alloy powder, or a soft magnetic alloy powder solidified with a resin. A doughnut-shaped magnetic core is a soft magnetic material having a hollow shape, and a doughnut-shaped magnetic core housed in a hollow container is a magnetic component.

[0011] The soft magnetic material constituting the doughnut-shaped magnetic core 5 is preferably a Co-based amorphous magnetic alloy, an Fe-based amorphous magnetic alloy, a microcrystalline Fe-based magnetic alloy, or the like. These alloys are suitable as constituent materials of the doughnut-shaped magnetic core 5 because they are easy to obtain as magnetic alloy ribbons with a thickness of 30 μm or less. The doughnut-shaped magnetic core 5 can be easily produced by winding or laminating the magnetic alloy ribbon.

[0012] The amorphous alloy constituting the doughnut-shaped magnetic core 5 preferably has a composition represented by the following formula (1). General formula:(T 1-a M a ) 100-b X b ···(1) (In the formula, T represents at least one element selected from Fe and Co, M represents at least one element selected from Ti, V, Cr, Mn, Ni, Cu, Zr, Nb, Mo, Ta and W, X represents at least one element selected from B, Si, C and P, and a and b are numbers that satisfy the conditions 0≦a≦0.5 and 10≦b≦35 at %.)

[0013] The composition ratio of the element T is adjusted according to the required magnetic properties such as magnetic flux density and core loss. When the element T contains a large amount of Fe, an Fe-based amorphous magnetic alloy is obtained. When the element T contains a large amount of Co, a Co-based amorphous magnetic alloy is obtained. The element M is an element added for thermal stability, corrosion resistance, and control of crystallization temperature. The element M is more preferably at least one selected from Cr, Mn, Zr, Nb, and Mo. If the content of the element M is too high, the amount of the element T decreases relatively, resulting in a deterioration in the magnetic properties of the amorphous magnetic alloy ribbon. Therefore, the value a, which indicates the content of the element M, is set to 0.5 or less. In practical terms, it is preferably set to 0.01 or more.

[0014] Element X is an essential element for obtaining an amorphous alloy. In particular, B (boron) is an element that is effective in amorphizing a magnetic alloy. Si is an element that promotes the formation of an amorphous phase or is effective in raising the crystallization temperature. If the amount of element X added is too large, a decrease in magnetic permeability and brittleness occur. If the amount of element X added is too small, it becomes difficult to amorphize the magnetic alloy. For these reasons, the content b of element X is preferably in the range of 10≦b≦35 at%.

[0015] Furthermore, it is preferable to use a Co-based amorphous alloy ribbon having excellent saturable characteristics as the magnetic alloy ribbon constituting the doughnut-shaped magnetic core 5. By using a Co-based amorphous alloy ribbon, it is possible to improve the magnetic characteristics of the doughnut-shaped magnetic core 5. It is preferable that the Co-based amorphous alloy ribbon has a composition represented by the following formula (2). General formula:Co a Fe b M c Si d B e ···(2) (wherein a+b+c+d+e=100 at%, 3≦b≦7 at%, 0.5≦c≦3 at%, 9≦d≦18 at%, and 7≦e≦16 at%).

[0016] In formula (2), the element M is preferably at least one selected from Nb, Cr, W, Mo, and Ta. By including such an element M as an essential component, the heat resistance of the Co-based amorphous alloy ribbon is improved. By improving the heat resistance of the Co-based amorphous alloy ribbon, it is possible to suppress deterioration of the magnetic properties of the doughnut-shaped magnetic core 5 due to the drying process described below. The element M is more preferably Nb. Nb particularly contributes to improving the heat resistance of the Co-based amorphous alloy ribbon.

[0017] The amorphous alloy ribbon used as the magnetic alloy ribbon is preferably produced by applying a liquid quenching method. Specifically, an alloy material adjusted to a predetermined composition ratio is melted and cooled to a temperature of 1000°C. 5 An amorphous alloy ribbon is obtained by quenching at a cooling rate of °C / second or more. The amorphous alloy produced by the liquid quenching method has the shape of a ribbon. The thickness of the amorphous alloy ribbon is preferably 30 μm or less, and more preferably 8 to 20 μm. By controlling the thickness of the magnetic thin body, it is possible to obtain a low-loss magnetic core.

[0018] The Fe-based magnetic alloy having microcrystals preferably has a composition represented by the following formula (3). General formula: FeaCubMcSidBe...(3) (In the formula, M represents at least one element selected from the group consisting of Group 4a elements, Group 5a elements, Group 6a elements, Mn, Ni, Co, and Al in the periodic table, and a+b+c+d+e=100 at%, 0.01≦b≦4 at%, 0.01≦c≦10 at%, 10≦d≦25 at%, 3≦e≦12 at%, and 17≦d+e≦30 at%.) The elements in groups 4a, 5a, and 6a of the periodic table are based on the Japanese periodic table.

[0019] In the composition of formula (3), Cu is an element that is effective in increasing corrosion resistance, preventing coarsening of crystal grains, and improving soft magnetic properties such as core loss and magnetic permeability. Element M is effective in making crystal grains uniform, reducing magnetostriction and magnetic anisotropy, and improving magnetic properties against temperature changes. A magnetic alloy having microcrystals preferably has microcrystals in which crystal grains with a grain size of 5 to 30 nm account for 50% or more, preferably 90% or more, of the alloy by area.

[0020] An Fe-based magnetic alloy ribbon having microcrystals is produced, for example, as follows. First, an amorphous alloy ribbon having the alloy composition of formula (3) is produced by a liquid quenching method, and then the amorphous alloy ribbon is heat-treated at −50 to +120° C. relative to the crystallization temperature for 1 minute to 5 hours to precipitate microcrystals. Alternatively, the quenching temperature when producing the alloy ribbon by the liquid quenching method is controlled to directly precipitate microcrystals. The thickness of the magnetic alloy ribbon is preferably 30 μm or less, similar to that of the amorphous alloy ribbon, and more preferably 8 to 20 μm.

[0021] A wound body is produced by winding the magnetic alloy ribbon as described above. Alternatively, a laminate is produced by stacking the magnetic alloy ribbons. The number of windings and the number of stacks are appropriately set depending on the required magnetic properties. If necessary, an insulating layer may be provided on the surface of the magnetic alloy ribbon. The wound body is produced by winding the magnetic alloy ribbon so that a hollow portion is formed in the center. By winding the magnetic alloy ribbon, a magnetic core having a hollow portion in the center, i.e., a doughnut-shaped magnetic core 5 (see FIG. 2), can be obtained.

[0022] The laminate is made by laminating magnetic alloy ribbons so that a hollow portion is formed in the center. For example, the magnetic alloy ribbon is cut to a predetermined length to prepare a magnetic alloy ribbon, and a hole is drilled in the center of the magnetic alloy ribbon. By laminating such magnetic alloy flakes, a magnetic core having a hollow portion in the center is formed. In other words, a doughnut-shaped magnetic core 5 can be obtained.

[0023] The doughnut-shaped magnetic core 5 is housed in a hollow container 1. The hollow container 1 has a cylindrical inner wall 2 formed to provide a hollow space 4 inside, and an outer wall 3 arranged to surround the inner wall 2. A bottom is provided at one end of the cylindrical inner wall 2 and the outer wall 3 to close the space between them. The other ends of the cylindrical inner wall 2 and the outer wall 3 are open, forming open portions. The doughnut-shaped magnetic core 5 is housed between the cylindrical inner wall 2 and the outer wall 3 by being inserted through the open portion.

[0024] The hollow container 1 is preferably made of an insulating material, and the thickness of each part is preferably in the range of 0.05 to 1 mm, more preferably in the range of 0.1 to 0.5 mm. The hollow container 1 is preferably integrally formed by molding or the like. The cylindrical inner wall 2, outer wall 3, and bottom 6 (see FIG. 2) are preferably integrally formed.

[0025] The magnetic component 8 shown in Figure 2 obtained as described above may be used in a high-temperature environment for a long period of time due to heat generation within the circuit, such as when incorporated as a noise suppression element in an electrical circuit such as a power supply. In such cases, the magnetic properties of the noise suppression element tend to deteriorate, reducing the noise suppression effect. Therefore, knowing the usage time in a high-temperature environment can help determine the deterioration of the magnetic properties of the magnetic component. Meanwhile, the hollow resin container 1 of the magnetic component 8 is also exposed to a high-temperature environment, which can cause discoloration of the resin.

[0026] The resin used for the hollow container 1 can be colored, and various colors such as blue and black can be used. However, these colors only slightly discolor the resin even when used in a high-temperature environment. Therefore, the deterioration of the magnetic properties of magnetic parts cannot be determined from the appearance. By using a color with a saturation C of 0 (achromatic) to 2 and a brightness V of 8 to 10 in accordance with JIS Z8721 "Color Display Method - Display by Three Attributes," it becomes easy to determine the degree of discoloration of the resin over time in a high-temperature environment, and it becomes easy to determine the deterioration of the magnetic properties of magnetic parts from the appearance.

[0027] The degree of discoloration is easily determined when the initial color of the resin has a saturation C of 0 or more and a brightness V of 8 or more and 10 or less. To make it even easier to determine the degree of discoloration, the initial color of the resin preferably has a saturation C of 1 or less and a brightness V of 9 or more.

[0028] Furthermore, the resin material is formed from insulating resins such as PET (polyethylene terephthalate) and LCP (liquid crystal polymer), but in order to easily determine the degree of discoloration, it is more preferable to use PA (polyamide) resin, which has a large degree of discoloration.

[0029] The magnetic component 8 of the first embodiment is produced by inserting a doughnut-shaped magnetic core 5 into the opening of the hollow container 1, storing it in the hollow container 1, and then attaching a lid. If the doughnut-shaped magnetic core 5 is not fixed inside the hollow container 1 and moves within the container, it is fixed with an adhesive or the like. As shown in FIG. 2, the lid 10 is inserted into the opening of the hollow container 1 and fixed therein. An adhesive is used for this fixation. In addition to using an adhesive to fix the lid 10, a lid-retaining protrusion may be provided on the hollow container 1 side to prevent the lid from coming off after it has been inserted therein.

[0030] Instead of using the lid 10, an adhesive can be poured into the lid, which also serves to secure the doughnut-shaped magnetic core 5. Examples of adhesives that can be used include acrylic-modified silicone resin adhesives, epoxy resin adhesives, and phenolic resin adhesives. Furthermore, before pouring the adhesive, the leads can be passed through the hollow portion, and the lid can be formed with the adhesive while the lead portions are secured. It is preferable that the adhesive portion penetrate into the gap between the doughnut-shaped magnetic core 5 and the hollow container 1, and into the gap between the hollow container 1 and the lead portions, from the open side of the hollow container 1, by an average of 5% to 50% of the thickness of the doughnut-shaped magnetic core 5.

[0031] Furthermore, the outer wall 3 or the inner wall 2 of the hollow container 1 may have an extension in the height direction beyond the inserted doughnut-shaped magnetic core 5, and at least one of them may be bent to form a lid. As shown in Figure 3, the hollow container 1 of the magnetic component 8 of the second embodiment has an extension portion in which the inner wall portion 2 and the outer wall portion 3 exceed the height of the doughnut-shaped magnetic core 5 when the doughnut-shaped magnetic core 5 is stored through the open portion 7.

[0032] 4, the extensions 2a and 3a are subjected to a folding process described below to form folded portions 9a and 9b, which serve as the lid of the magnetic component 8. At this time, the lid can be formed on either the inner wall or the outer wall by lengthening the extension 2a and bringing the folded portion 9a into close contact with the extension 3a of the outer wall, or conversely, by lengthening the extension 3a and bringing the folded portion 9b into close contact with the extension 2b of the inner wall. When bending the extensions 2a, 3a of the inner wall 2 and the outer wall 3 to form the bent portions 9a, 9b, it is preferable to use a method in which a heated metal head or the like is pressed against the extensions 2a, 3a to bend them, which improves the mass productivity of the magnetic component 8. Therefore, it is preferable that the hollow container 1 has properties that allow it to be bent at a predetermined temperature without cracking. The wall thickness t of the hollow container 1 is not particularly limited, but is preferably in the range of 0.1 to 0.5 mm, taking into account processability and strength. If the wall thickness is less than 0.1 mm, the strength of the hollow container 1 decreases, and further, the circulation of the resin during molding in a mold becomes poor, requiring molding at high temperatures. If the wall thickness of the hollow container 1 exceeds 0.5 mm, the strength increases, but the volume becomes larger than necessary, making it impossible to miniaturize the hollow container 1. In this case, there is a risk that the magnetic component 8 cannot be inserted into the leads of a semiconductor element, etc. It is preferable that the thickness of the hollow container 1, including the inner wall 2, outer wall 3, and bottom 6, is all uniform and within the range of 0.1 to 0.5 mm.

[0033] 4, the magnetic component 8 according to the second embodiment has a first bent portion 9a formed by bending the extension 2a of the inner wall portion 2 toward the outer wall portion 3, and a second bent portion 9b formed by bending the extension 3a of the outer wall portion 3 toward the inner wall portion 2. The first and second bent portions 9a, 9b are formed to cover the open portion 7 of the hollow container 1, and essentially function as a lid portion 9 of the hollow container 1. Because the lid portion 9 has the first and second bent portions 9a, 9b, the doughnut-shaped magnetic core 5 does not fall out of the hollow container 1.

[0034] The magnetic component 8 shown in Fig. 4 includes a lid portion 9 formed by bending the extension portion 2a of the inner wall portion 2 and the extension portion 3a of the outer wall portion 3 so that the first bent portion 9a is located below the second bent portion 9b (more inward than the second bent portion 9b). The configuration of the lid portion 9 is not limited to this. The lid portion 9 may also be formed by bending the extension portion 2a of the inner wall portion 2 and the extension portion 3a of the outer wall portion 3 so that the second bent portion 9b is located below the first bent portion 9a (more inward than the first bent portion 9a).

[0035] In the magnetic component 8 according to the second embodiment, the first bent portion 9a and the second bent portion 9b preferably intersect. The magnetic component 8 has an intersection 11 where the first bent portion 9a and the second bent portion 9b intersect. Providing the intersection 11 eliminates gaps, improving the functionality of the lid portion 9. This more reliably prevents problems such as the doughnut-shaped magnetic core 5 falling off. This eliminates the need for adhesive fixation, allowing for weight reduction and preventing problems caused by adhesive overflow. The simplified manufacturing process also enables a shorter lead time.

[0036] The magnetic component 8 of the second embodiment described above is fabricated, for example, as follows: First, a hollow container 1 made of resin and having an extension 2a of an inner wall 2 and an extension 3a of an outer wall 3 is prepared, and a doughnut-shaped magnetic core 5 is placed inside the hollow container 1.

[0037] Next, a heated metal head is pressed against the extension 2a of the inner wall 2 and the extension 3a of the outer wall 3, thereby bending the extension 2a of the inner wall 2 toward the outer wall 3 to form a first bent portion 9a, and bending the extension 3a of the outer wall 3 toward the inner wall 2 to form a second bent portion 9b. In this way, the open portion of the hollow container 1 is covered with the lid 9 having the first bent portion 9a and the second bent portion 9b.

[0038] By using a heated metal head, the extensions 2a and 3a of the inner wall 2 and outer wall 3 can be bent smoothly. The metal head is preferably heated to a temperature in the range of 20% lower than the melting point (Mp (°C)) of the resin constituting the hollow container 1 (Mp - 0.2Mp = 0.8Mp (°C)) or higher and up to the melting point (Mp (°C)). The heating temperature of the metal head is more preferably 15% lower than the melting point (Mp (°C)) of the resin (Mp (°C)) (0.85Mp (°C)) or higher and 5% lower than the melting point (Mp (°C)) (0.95Mp (°C)). The specific heating temperature varies depending on the constituent material of the hollow container 1, but is preferably in the range of 100 to 300°C, and more preferably in the range of 160 to 240°C.

[0039] If the heating temperature of the metal head is less than 0.8 Mp (°C), the extensions 2a, 3a of the inner wall 2 and the outer wall 3 cannot be bent properly. If the heating temperature of the metal head exceeds Mp (°C), the resin forming the hollow container 1 may be altered and melt. In this case, the shape of the bent portions 9a, 9b cannot be maintained, the doughnut-shaped magnetic core 5 is exposed, and its function as an insulating exterior is impaired. Furthermore, if the temperature of the metal head is too high, it may have an adverse effect on the doughnut-shaped magnetic core 5. For example, if an amorphous alloy ribbon is used as the constituent material of the doughnut-shaped magnetic core 5, the coercive force and squareness ratio characteristics may be deteriorated due to heat.

[0040] As a third embodiment, a lead insertion type magnetic component 12 in which a lead wire 13 is disposed in a hollow portion at the center of the magnetic component 8 of the second embodiment is shown in Figure 5. The lead wire 13 does not need to be straight, and may be bent to fit the mounting form on the board. [Example]

[0041] Next, a magnetic component according to an embodiment will be described. As a method for determining discoloration of the magnetic part of the examples, it is also effective to determine the whiteness by the ISO whiteness measurement method (JIS P8148). In Example 1, a magnetic component sample was formed by winding an amorphous ribbon containing Co as the main component into a doughnut shape and inserting it into a white hollow container 1 made of polyamide resin. The magnetic component sample was heated at 120°C for 1000 hours, and the ISO whiteness and compressive strength were measured at room temperature (25°C) after each elapsed time. The compressive strength was measured by applying an excessive load to the magnetic component and measuring the load at which it broke. In Example 2, a magnetic component sample having the same configuration as Example 1 was heated at 140°C for 1000 hours, and the whiteness and compressive strength were measured at room temperature (25°C) after each elapsed time. Furthermore, in Comparative Example 1, the hollow container was made of a commonly used white PBT resin. The hollow container was heated at 140°C for 1000 hours, and the whiteness and compressive strength were measured at room temperature (25°C) after each elapsed time. Furthermore, a blue PBT resin was used as Comparative Example 2 and similar measurements were carried out. The results are shown in Table 1. Change delta (%): Lower limit: Whiteness (N) Min - Whiteness (0H) Max Upper limit: Whiteness (N) Max - Whiteness (0H) Min N is the elapsed time (however, the difference in change is ≦0) Let's say.

[0042] As a result, it can be seen that the ISO whiteness fluctuates over time at temperatures above 120°C, where the device's characteristics are thought to deteriorate. At 120°C, the initial ISO whiteness (0 hours) is 85-90%, but after 1000 hours the ISO whiteness falls to less than 20%, a difference in ISO whiteness percentage of more than 60%. From this, by measuring the ISO whiteness of the insulating case, it is possible to estimate how long the device has been exposed to such high temperatures. By obtaining the correlation between this variation in whiteness and the characteristic variation of the element, it is possible to determine the timing for replacing the element based on the ISO whiteness. On the other hand, discoloration hardly occurred in Comparative Example 1, and discoloration was hardly visible in Comparative Example 2, and the results showed that neither was suitable for determining the elapsed time based on discoloration.

[0043] [Table 1]

[0044] In Examples 1 and 2, the variation in ISO whiteness (JIS P8148) was used as an index, but the variation in hue, lightness, and saturation according to JIS Z8721 "Color display method - display by three attributes" or the variation in the tristimulus value Y and chromaticity coordinates x and y shown as the standard may also be used. Furthermore, the color display method according to the XYZ system shown in JIS Z8701 and the L color display method according to JIS Z8729, which is converted from the numerical values ​​of the XYZ system, may also be used. * a * b * Color space and L * u * v * It is also possible to evaluate the change in values ​​of a color system or the like and use this as an index.

[0045] Also, if you prepare a color sample, you can compare the color of the product with that to determine the elapsed time. Furthermore, if there is a large change in color, you can make a visual judgment, so you can visually determine when to replace magnetic parts when they have reached their limit of use.

[0046] As Example 3 of the second embodiment, a donut-shaped magnetic core 5 was prepared by winding a 3 mm wide Fe-based amorphous metal ribbon containing 1 at% Cu into a ring shape, forming it into a shape with an outer diameter of φ3 mm and an inner diameter of φ2 mm, and then heat-treating it to fine crystallize it. The material of the hollow resin container 1 to house the donut-shaped magnetic core 5 was DuPont's Zytel polyamide resin. It was injection molded into a shape with an opening, as shown in Figure 1 . After inserting the donut-shaped magnetic core 5 into the hollow resin container 1, a metal head heated to 0.9°C × the melting point of the resin was pressed against the extension 2 a of the inner wall 2 and the extension 3 a of the outer wall 3 to bend the extension 2 a of the inner wall 2 toward the outer wall 3 and close the extension 3 a of the outer wall 3 toward the inner wall 2, thereby obtaining the magnetic component 8 shown in Figure 4 .

[0047] In Example 4 of the fourth embodiment, as shown in Fig. 6, the hollow container 1 housing the doughnut-shaped magnetic core 5 was made of the same material as in Example 3, and its outermost shape was a rectangular parallelepiped. A ring-shaped groove was provided where the doughnut-shaped magnetic core 5 was housed, and the inner wall 2 and outer wall 3 had extensions. A rectangular hollow portion 4 was formed in the center of the hollow container 1 for inserting a rectangular lead. After the doughnut-shaped magnetic core 5 was inserted into the hollow container 1, the extension portion 2a of the inner wall and the extension portion 3a of the outer wall were bent in the same manner as in Example 3, thereby obtaining the magnetic component 8 shown in Fig. 7.

[0048] As Example 5 of the fifth embodiment, a flat rectangular lead 15 was inserted into the structure of Example 4 shown in FIG. 7, and a bent portion of the lead was provided as a soldering terminal during mounting, thereby preparing a surface-mounted magnetic component 14 shown in FIG. 8. As Comparative Example 3, a hollow container 1 in Example 3 was prepared in which the resin material was a PBT material (Duranex made of polyplastics). As Comparative Example 4, a hollow container made of a liquid crystal resin (Civelas, manufactured by Toray Industries, Inc.) was used instead of the resin material in Example 3.

[0049] 500 pieces were produced for each of the examples and comparative examples, and their appearances were compared. Pieces with problems in the insulating exterior, such as cracks or chips, were considered defective, and the yield was compared. The yield was calculated as (number of good pieces / number produced (500) x 100) [%].

[0050] [Table 2]

[0051] In this evaluation, no cracks or chips were observed in Comparative Example 3. In Comparative Example 4, many chips and cracks occurred on the folded side of the inner diameter side. Furthermore, the components were left in an atmosphere at 260°C for 10 minutes, which is similar to the reflow conditions, and the appearance was similarly compared.

[0052] [Table 3]

[0053] The PBT resin of Comparative Example 3 was deformed due to melted dripping and the like.

[0054] In this way, by using polyamide resin as the material for the hollow resin container 1 used in the magnetic component 8, which has a structure in which both or one of the extension 2a of the inner wall 2 and the extension 3a of the outer wall 3 are folded to form the lid 9, heat resistance at reflow temperatures is maintained, eliminating defects such as deformation, which was an issue with PBT resin. It was also found that the issue of cracks and fractures caused by stresses that occur when the extension 2a of the inner wall 2 or the extension 3a of the outer wall 3 are folded by thermal caulking, which was an issue with liquid crystal resin, which has weak weld strength, is eliminated.

[0055] As a result, in the magnetic component 5 in which the outermost shape of the container is a rectangular parallelepiped, rectangular leads 15 are passed through the central hollow portion 4, and bent portions are provided to serve as solder terminals, as in Example 5, the container does not deform and can withstand the reflow temperature, making it possible to mount by reflow soldering using an automatic mounting machine. Also, in this case, rectangular leads 15 are provided with solder terminals on the outside of hollow container 1 in Figure 8, but it is also possible to bend them toward hollow container 1 and form solder terminals on the lower part of one surface that will become the bottom surface of the rectangular parallelepiped.

[0056] Furthermore, even if the connecting portions of the surfaces of the rectangular parallelepiped in the outermost shape of the container are chamfered with C or R, it is sufficient as long as mechanical stability is ensured during pick-up for transport during automatic mounting and during soldering. Furthermore, as long as no problems occur during transport during mounting, the surfaces other than those used for pick-up and soldering are not limited to being flat. Furthermore, as shown in FIG. 9, the doughnut-shaped magnetic component 8 can also be used as a wound-lead magnetic component 16 according to the fifth embodiment, in which a lead wire 17 is wound around the doughnut-shaped magnetic component 8.

[0057] Although several embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be embodied in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included within the scope and spirit of the invention, and are also included in the scope of the invention and its equivalents as defined in the claims. [Explanation of symbols]

[0058] 1. Hollow container 2. Inner wall 2a...Inner wall extension 3...Outer wall 3a...exterior wall extension 4...Hollow part 5. Doughnut-shaped core 6...Bottom 7...open area 8 Magnetic parts 9...Lid part 9a...Bending part 1 9b...Bending part 2 10...Lid part 11 Intersection 12 Lead insertion type magnetic components 13 Lead 14. Inserted rectangular lead magnetic components 15 ···Flat rectangular lead 16 Lead-wound magnetic components 17 ···Wound lead

Claims

1. An inner wall portion formed to form a hollow portion; An outer wall portion formed so as to surround the inner wall portion; a doughnut-shaped magnetic core is housed in a hollow resin container having a bottom provided at one end of the inner wall portion and the outer wall portion so as to close a gap between the inner wall portion and the outer wall portion, The color of the resin forming the hollow container has a hue having a chroma C of 0 (achromatic color) or more and 2 or less and a brightness V of 8 or more as defined in JIS Z8721 "Color display method-Display by three attributes." Magnetic parts.

2. The color of the resin forming the hollow container has a hue with the brightness V of 9 or more. The magnetic component according to claim 1 .

3. The color of the resin forming the hollow container has a hue whose saturation C is 1 or less. The magnetic component according to claim 1 or 2.

4. The hollow container is made of a polyamide resin. The magnetic component according to claim 1 .

5. The difference in the percentage change in the ISO whiteness after being left at a high temperature of 120° C. for 1000 hours is reduced by 60% or more with respect to the initial ISO whiteness percentage determined by the ISO whiteness measurement method (JIS P8148). The magnetic component according to claim 1 .

6. The hollow container has a structure in which at least one of the outer wall portion and the inner wall portion at the end opposite to the bottom portion is folded to form a lid portion. The magnetic component according to claim 1 .

7. The doughnut-shaped core is a core in which a magnetic ribbon is wound. The magnetic component according to claim 1 .

8. The compressive strength of the magnetic part at room temperature (25°C) is 50N or more. The magnetic component according to claim 1 .

9. A lead is inserted into the hollow portion. The magnetic component according to claim 1 .

10. A lead is inserted into the hollow portion and wound around the inner wall side and the outer wall side of the magnetic component alternately. The magnetic component according to claim 1 .

11. A lead having a rectangular cross section is inserted into the hollow portion. The magnetic component according to claim 1 .

12. The magnetic component is a noise suppression element; The magnetic component according to claim 1 .

Citation Information

Patent Citations

  • Kapuserudoryokugensochi

    JP1976075843A

  • Molded electric device

    JP1994295823A

  • Magnetic component with leads and noise reducing circuit using the same

    JP2000091142A

  • Electric box, and manufacturing method of electric box

    JP2009115737A

  • Inductance element and switching power supply using the same

    JP2013225689A