Multilayer ceramic electronic components and their mounting substrates

The multilayer ceramic capacitor design with L-shaped external electrodes and a thicker lower cover part addresses acoustic noise issues by reducing solder height and vibration transmission, improving reliability and capacitance.

JP7567146B2Active Publication Date: 2024-10-16SAMSUNG ELECTRO MECHANICS CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021106720
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2016-06-21
Filing Date
2021-06-28
Publication Date
2024-10-16
Estimated Expiration
2037-01-06

AI Technical Summary

Technical Problem

The miniaturization of multilayer ceramic electronic components has led to increased acoustic noise due to piezoelectric vibrations, which are transmitted to the printed circuit board, causing discomfort and noise interference.

Method used

A multilayer ceramic capacitor design with L-shaped external electrodes formed on both end faces and a thicker lower cover part, along with insulating layers, to reduce acoustic noise by minimizing solder height and vibration transmission.

Benefits of technology

The design effectively reduces acoustic noise by minimizing solder height and vibration transmission, enhancing reliability and board mounting efficiency while maintaining high capacitance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567146000002
    Figure 0007567146000002
  • Figure 0007567146000003
    Figure 0007567146000003
  • Figure 0007567146000004
    Figure 0007567146000004
Patent Text Reader

Abstract

To provide a multilayer ceramic electronic component and a mounting board thereof.SOLUTION: The present invention provides a multilayer ceramic electronic component including: a ceramic body including a plurality of dielectric layers: an active part including a plurality of first and second internal electrodes disposed in the ceramic body to be alternately exposed to respective end surfaces of the ceramic body, with each dielectric layer interposed therebetween; an upper cover part formed above the active part; a lower cover part formed below the active part and having a thickness greater than that of the upper cover part; and first and second external electrodes electrically connected to the first and second internal electrodes, respectively. The first and second external electrodes include first and second electrode layers, respectively. The first and second electrode layers are disposed on both side surfaces forming both end surfaces of the ceramic body in a length direction, respectively, and the lower surface of the ceramic body, but are not disposed on the upper surface of the ceramic body.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a multilayer ceramic capacitor, a mounting substrate thereof, and a manufacturing method thereof. [Background technology]

[0002] 2. Description of the Related Art Recently, with the trend towards miniaturization of electronic products, there is a demand for miniaturization and high capacity of multilayer ceramic electronic components used in such electronic products.

[0003] Therefore, various methods have been attempted to reduce the thickness and number of layers of the dielectric layers and internal electrodes, and in recent years, multilayer ceramic electronic components have been manufactured in which the thickness of the dielectric layers is reduced and the number of layers is increased.

[0004] Since the dielectric layers have piezoelectricity and electrostriction, when a DC or AC voltage is applied to the multilayer ceramic electronic component, a piezoelectric phenomenon occurs between the internal electrodes, which may cause vibration.

[0005] Such vibrations are transmitted via the external electrodes and solder of the multilayer ceramic electronic component to the printed circuit board on which the multilayer ceramic electronic component is mounted, causing the entire printed circuit board to become an acoustically reflective surface, generating vibration noise that is perceived as noise.

[0006] The vibration noise may be in the audible frequency range of 20 to 20,000 Hz, which is unpleasant to humans, and such vibration noise that is unpleasant to humans is called acoustic noise.

[0007] In recent electronic devices, due to the noise reduction of components, the acoustic noise generated by such multilayer ceramic electronic components can become more noticeable, making research into effective reduction of the acoustic noise generated by multilayer ceramic electronic components necessary.

[0008] Patent Document 1 listed below discloses a multilayer ceramic capacitor, but does not disclose a structure in which a lower cover part is formed thicker than an upper cover part in order to reduce acoustic noise, or a structure in which external electrodes include an insulating layer. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] Korean Patent Publication No. 2007-0089629 Summary of the Invention [Problem to be solved by the invention]

[0010] The present invention relates to a multilayer ceramic capacitor, a mounting substrate thereof, and a manufacturing method thereof. [Means for solving the problem]

[0011] An embodiment of the present invention provides a multilayer ceramic electronic component including: a ceramic body including a plurality of dielectric layers; an active portion including a plurality of first and second internal electrodes stacked in the ceramic body with the dielectric layers sandwiched therebetween and arranged to be alternately exposed at both end faces opposing each other in a longitudinal direction of the ceramic body; an upper cover portion formed on an upper portion of the active portion; a lower cover portion formed under the active portion and having a thickness greater than that of the upper cover portion; and first and second external electrodes electrically connected to the first and second internal electrodes, wherein the first and second external electrodes are first and second electrode layers arranged on both end faces and a lower surface opposing each other in a longitudinal direction of the ceramic body but not on an upper surface.

[0012] Another embodiment of the present invention provides a mounting substrate for a ceramic electronic component, the mounting substrate including a printed circuit board having electrode pads on an upper portion thereof, a multilayer ceramic electronic component according to the embodiment of the present invention installed on the electrode pads, and solder connecting the electrode pads and the multilayer ceramic electronic component, the solder being disposed on both end faces facing a mounting surface of the ceramic body in a longitudinal direction. Effect of the Invention

[0013] According to one embodiment of the present invention, since the external electrode has an L-shape, no separate marking is required to distinguish the upper and lower surfaces, and there is no problem of reduced reliability, such as cracks, which may occur due to a method of making the upper and lower parts of the body different colors for separate marking.

[0014] According to one embodiment of the present invention, the external electrodes are L-shaped and are formed only on both opposing end faces in the longitudinal direction of the ceramic body and on the bottom surface, which is the mounting surface. This makes it possible to realize a structure in which the solder creeps up only on one side of the body, thereby achieving the effect of reducing acoustic noise.

[0015] According to one embodiment of the present invention, the lower cover part is thicker than the upper cover part and is formed on the upper parts of the external electrodes arranged on both end surfaces facing each other in the longitudinal direction of the ceramic body. An insulating layer is formed from the upper corners of the ceramic body in the thickness direction to an upper region when the lower cover part is divided into three equal parts in the thickness direction. This reduces the height of the solder formed on the external electrodes when the multilayer ceramic electronic component is mounted on a printed circuit board, thereby reducing the transmission of vibration generated from the multilayer ceramic electronic component to the printed circuit board via the external electrodes and solder, thereby reducing acoustic noise. [Brief description of the drawings]

[0016] [Figure 1] 1 is a schematic cutaway perspective view of a multilayer ceramic capacitor according to an embodiment of the present invention; [Diagram 2]2 is a cross-sectional view of the capacitor structure shown in FIG. 1 taken along line II'. [Diagram 3] FIG. 3 is an enlarged view of area “A” in FIG. [Figure 4] 2 is a cross-sectional view showing a multilayer ceramic capacitor shown in FIG. 1 cut in the longitudinal direction for explaining the dimensional relationship between components included in the multilayer ceramic capacitor. FIG. [Diagram 5] 2 is a perspective view showing a state in which the multilayer ceramic capacitor in FIG. 1 is mounted on a printed circuit board, with a part of the multilayer ceramic capacitor being cut away. FIG. [Figure 6] 6 is a cross-sectional view showing the multilayer ceramic capacitor and the printed circuit board in FIG. 5 cut in the longitudinal direction. [Figure 7] 6 is a cross-sectional view illustrating a state in which the multilayer ceramic capacitor in FIG. 5 is deformed when a voltage is applied to the multilayer ceramic capacitor mounted on a printed circuit board. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, preferred embodiments of the present invention will be described with reference to the accompanying drawings. However, the embodiments of the present invention can be modified into various other forms, and the scope of the present invention is not limited to the embodiments described below. Furthermore, the embodiments of the present invention are provided to more completely explain the present invention to those having average knowledge in the art. Therefore, the shapes and sizes of elements in the drawings may be exaggerated for clearer explanation.

[0018] In the following description of a multilayer ceramic electronic component according to an embodiment of the present invention, a multilayer ceramic capacitor will be particularly described, but the present invention is not limited thereto.

[0019] Multilayer Ceramic Capacitor FIG. 1 is a schematic perspective view of a multilayer ceramic capacitor according to an embodiment of the present invention, and FIG. 2 is a cross-sectional view of the capacitor structure shown in FIG. 1 taken along line II'.

[0020] 1 and 2, the multilayer ceramic capacitor 100 according to this embodiment includes a ceramic body 110, an active part 115 including a plurality of first and second internal electrodes 121 and 122, upper and lower cover parts 112 and 113, and first and second external electrodes 131 and 132 electrically connected to the first and second internal electrodes 121 and 122, respectively.

[0021] The ceramic body 110 is formed by stacking a plurality of dielectric layers 111 and then firing them, and the shape, dimensions and number of the dielectric layers 111 of the ceramic body 110 are not limited to those shown in this embodiment.

[0022] In addition, the multiple dielectric layers 111 forming the ceramic body 110 are in a sintered state, and the boundaries between adjacent dielectric layers 111 can be integrated to such an extent that they cannot be confirmed without the use of a scanning electron microscope (SEM).

[0023] The ceramic body 110 may have a hexahedral shape. To clearly explain the embodiment of the present invention, the directions of the hexahedron are defined as L, W, and T shown in FIG. 1, which respectively indicate the length direction, width direction, and thickness direction.

[0024] In addition, in this embodiment, the thickness direction end faces that face each other in the stacking direction of the dielectric layers 111 of the ceramic body 110 are defined as the upper face and the lower face, the length direction end faces that connect the upper face and the lower face and face each other are defined as the first and second length direction side faces, and the width direction end faces that face each other are defined as the first and second width direction side faces.

[0025] The ceramic body 110 may be composed of an active portion 115 that contributes to the formation of the capacitance of the capacitor, and upper and lower cover portions 112, 113 that are formed on the upper and lower parts of the active portion 115, respectively, as upper and lower margin portions.

[0026] The active part 115 may be formed by repeatedly stacking a plurality of first and second internal electrodes 121 and 122 with the dielectric layer 111 interposed therebetween so that the electrodes are alternately exposed to both end surfaces of the ceramic body 110 .

[0027] In this case, the thickness of the dielectric layer 111 may be changed as desired depending on the capacitance design of the multilayer ceramic capacitor 100, and may be preferably configured so that the thickness of one layer after firing is 0.01 to 1.00 μm, but the present invention is not limited to this.

[0028] In addition, the dielectric layer 111 may contain a ceramic material with a high dielectric constant, for example, a barium titanate (BaTiO3)-based or strontium titanate (SrTiO3)-based ceramic powder, but the present invention is not limited thereto as long as sufficient capacitance is obtained.

[0029] In addition to the ceramic powder, the dielectric layer 111 may further contain various ceramic additives such as transition metal oxides or carbides, rare earth elements, magnesium (Mg) or aluminum (Al), organic solvents, plasticizers, binders, dispersants, etc., if necessary.

[0030] The upper and lower cover parts 112, 113 may have the same material and structure as the dielectric layer 111, except that they do not include internal electrodes.

[0031] In addition, the upper and lower cover parts 112, 113 may be formed by stacking a single dielectric layer or two or more dielectric layers in the thickness direction on the upper and lower surfaces of the active part 115, respectively, and may basically serve to prevent damage to the first and second internal electrodes 121, 122 due to physical or chemical stress.

[0032] In this case, the lower cover part 113 may be formed to have a greater thickness than the upper cover part 112 by increasing the number of laminated dielectric layers more than that of the upper cover part 112 .

[0033] The first and second internal electrodes 121, 122 are electrodes having different polarities from each other, and may be formed by printing a conductive paste containing a conductive metal to a predetermined thickness on the dielectric layer 111 so as to be alternately exposed to the first and second end surfaces of the ceramic body 110 along the lamination direction of the dielectric layer 111, and may be electrically insulated from each other by the dielectric layer 111 disposed therebetween.

[0034] The conductive metal may be, for example, one of silver (Ag), palladium (Pd), platinum (Pt), nickel (Ni) and copper (Cu) or an alloy thereof, but the present invention is not limited thereto. Also, the conductive paste may be printed by screen printing or gravure printing, but the present invention is not limited thereto.

[0035] In addition, the first and second internal electrodes 121 and 122 may be electrically connected to the first and second external electrodes 131 and 132, respectively, through portions alternately exposed on the first and second side surfaces forming both end surfaces in the longitudinal direction of the ceramic body 110.

[0036] Therefore, when a voltage is applied to the first and second external electrodes 131, 132, charges are accumulated between the opposing first and second internal electrodes 121, 122. At this time, the capacitance of the multilayer ceramic capacitor 100 is proportional to the area of ​​the region where the first and second internal electrodes 121, 122 overlap each other in the active portion 115.

[0037] The thickness of the first and second internal electrodes 121, 122 may be determined depending on the application. For example, the thickness may be determined to be within a range of 0.2 to 1.0 μm in consideration of the size of the ceramic body 110, but the present invention is not limited to this.

[0038] The first and second external electrodes 131, 132 may include first and second electrode layers 131a, 132a.

[0039] The first and second electrode layers 131a, 132a are disposed on both longitudinal side surfaces and a bottom surface of the ceramic body 110 so as to cover and electrically connect a plurality of first and second internal electrodes 121, 122 alternately exposed on the first and second side surfaces forming both end surfaces in the longitudinal direction of the ceramic body 110.

[0040] In this case, the first and second electrode layers 131a and 132a may be formed using, for example, a copper-glass (Cu-Glass) paste in order to provide high reliability such as excellent moisture resistance as well as good electrical characteristics, but the present invention is not limited thereto.

[0041] According to an embodiment of the present invention, the first and second electrode layers 131a and 132a may be disposed on both side surfaces forming both end surfaces in the length direction of the ceramic body 110 up to both corners in the width direction.

[0042] That is, the first and second electrode layers 131a and 132a are disposed on both side surfaces and a lower surface that form both end surfaces in the length direction of the ceramic body 110, but are not disposed on an upper surface.

[0043] Meanwhile, the first and second electrode layers 131a and 132a may be disposed to extend on both end surfaces of the ceramic body 110 that face each other in a width direction.

[0044] That is, the first and second electrode layers 131a and 132a may have extensions extending to both end surfaces of the ceramic body 110 that face each other in a width direction.

[0045] Conventionally, the main method for forming external electrodes has been to dip a ceramic body into a paste containing a metal component.

[0046] When the external electrodes are formed by a dipping method, the external electrodes are not uniformly applied due to the fluidity and viscosity of the paste, and a difference in the application thickness occurs between the center and corners of the external electrodes.

[0047] If the thickness of the external electrodes is not uniform, glass beading or blisters may occur in the thickly coated central portion, causing plating defects and defective shapes, and the thinly coated corner portions may be vulnerable to the penetration of plating solution, resulting in reduced reliability.

[0048] In addition, in order to fill in the weak corners of the plating solution, the only way is to increase the coating thickness in the center, and there is a limit to increasing the size of the ceramic capacitor to increase the capacitance.

[0049] The first and second electrode layers 131a and 132a are not formed by the conventional dipping method, and are formed on the head surfaces, which are both end surfaces facing each other in the length L direction of the ceramic body 110, and are not formed or are formed to a minimum on any of the four band surfaces in contact with the head surfaces, except for the lower surface, which is the mounting surface of the substrate. This allows the thickness of the external electrodes to be formed thin and uniform.

[0050] As a result, the area in which the internal electrodes are formed can be increased, and the overlap area of ​​the internal electrodes can be maximized, thereby realizing a high-capacity multilayer ceramic capacitor.

[0051] According to an embodiment of the present invention, the first and second electrode layers 131a and 132a may be formed by a sheet transfer or pad transfer method, unlike the conventional dipping method.

[0052] 1 and 2, it can be seen that the first and second electrode layers 131a, 132a are arranged on the side surfaces that form both end faces in the longitudinal direction of the ceramic body 110, and are formed extending in the thickness direction from the upper corner portions to the lower surface, which is the mounting surface of the substrate, but are not formed on the entire remaining three band surfaces that contact the head surface.

[0053] The first and second electrode layers 131a and 132a may be formed by transferring a sheet including a conductive metal.

[0054] According to one embodiment of the present invention, since the external electrodes have an L-shape, no separate markings are required to distinguish the top and bottom surfaces, and there is no problem of reduced reliability, such as cracks, which may occur when different colors are used for the top and bottom of the body for separate markings.

[0055] In other words, since the external electrodes 131, 132 are arranged on both side surfaces and the bottom surface that form both end surfaces in the longitudinal direction of the ceramic body 110, but not on the top surface, no separate markings are required to distinguish the top and bottom surfaces, and therefore there is no problem of reduced reliability, such as cracks, that can occur when the top and bottom of the body are made different colors.

[0056] In addition, since the external electrodes are L-shaped and formed only on the longitudinal sides of the ceramic body 110 and on the bottom surface, which is the mounting surface, a structure is realized in which the solder creeps up only on one side of the body, which has the effect of reducing acoustic noise.

[0057] FIG. 3 is an enlarged view of area “A” in FIG.

[0058] Referring to FIG. 3, when the thickness of the first and second electrode layers 131a, 132a in the central region in the thickness direction of the ceramic body 110 is T1 and the thickness of the first and second electrode layers 131a, 132a at a height position where the internal electrode stacked at the top of the internal electrodes 121, 122 in the thickness direction of the ceramic body 110 is located is T2, the relationship 0.8≦T2 / T1≦1.2 can be satisfied.

[0059] The thickness T1 of the first and second electrode layers 131a and 132a at the central region in the thickness direction of the ceramic body 110 may refer to the thickness of the external electrode corresponding to the length of a virtual line drawn in the length direction of the ceramic body 110 at the central point in the thickness direction of the ceramic body 110 and crossing the external electrode.

[0060] Similarly, the thickness T2 of the first and second electrode layers 131a, 132a at a point where the upper outermost internal electrode of the internal electrodes 121, 122 in the thickness direction of the ceramic body 110 is located may refer to the thickness of an external electrode corresponding to the length of a virtual line drawn in the length direction of the ceramic body 110 at the position of the internal electrode arranged outermost in the thickness direction of the ceramic body 110, the virtual line crossing the external electrode.

[0061] When the ratio of T2 / T1 satisfies 0.8≦T2 / T1≦1.2, the deviation between the thickness T1 of the first and second electrode layers 131a, 132a in the central region in the thickness direction of the ceramic body 110 and the thickness T2 of the first and second electrode layers 131a, 132a at the point where the outermost internal electrode of the internal electrodes 121, 122 is located is reduced, thereby preventing a decrease in reliability.

[0062] If the above T2 / T1 ratio is less than 0.8 or exceeds 1.2, the thickness deviation of the external electrodes will be large, which may cause the plating solution to penetrate into the thinner parts, resulting in reduced reliability.

[0063] According to one embodiment of the present invention, insulating layers 131b, 132b may be further disposed on the first and second electrode layers 131a, 132a, and the insulating layers 131b, 132b may be disposed from an upper corner portion of the ceramic body 110 in a thickness direction to within a region adjacent to the internal electrodes when the lower cover portion 113 is divided into three equal parts in a thickness direction.

[0064] The insulating layers 131b and 132b are disposed on the first and second electrode layers 131a and 132a disposed on the first and second side surfaces forming both end surfaces in the length direction of the ceramic body 110. This is to prevent or minimize the formation of solder on the mounting surfaces of the first and second external electrodes 131 and 132, i.e., the bottom surface and on portions other than predetermined regions of the first and second side surfaces forming both end surfaces in the length direction of the ceramic body 110, when the multilayer ceramic capacitor 100 is mounted on a printed circuit board.

[0065] Specifically, the insulating layers 131b, 132b are arranged from the upper corner portion in the thickness direction of the ceramic body 110 to within the area adjacent to the internal electrodes when the lower cover portion 113 is divided into three equal parts in the thickness direction, so that solder is not formed at a position horizontally corresponding to the internal electrodes arranged at the bottom of the stacking direction.

[0066] By arranging the insulating layers 131b and 132b as described above, the height of the solder formed on the external electrodes when mounting the multilayer ceramic capacitor on a printed circuit board can be lowered, thereby reducing the transmission of vibration generated from the multilayer ceramic capacitor to the printed circuit board via the external electrodes and solder, thereby reducing acoustic noise.

[0067] On the other hand, if the insulating layers 131b and 132b are formed on the entire side surfaces forming both end surfaces in the length direction, except for the lower surface which is the mounting surface of the ceramic body 110, the area in which the solder is formed is reduced, and mounting defects may occur due to impact when the multilayer ceramic capacitor is mounted on a printed circuit board.

[0068] In other words, by arranging the insulating layers 131b, 132b up to the area adjacent to the internal electrodes when the lower cover portion 113 is divided into three equal parts in the thickness direction, it is possible to reduce acoustic noise and reduce mounting defects when mounting the board.

[0069] Meanwhile, the first and second external electrodes 131, 132 may further include first and second plating layers 131c, 132c disposed on the first and second electrode layers 131a, 132a and disposed to cover lower surfaces of the first and second electrode layers 131a, 132a and ends of the insulating layers 131b, 132b.

[0070] In this case, the first and second plating layers 131c, 132c may include a nickel (Ni) plating layer arranged to cover the lower surfaces of the first and second electrode layers 131a, 132a and the ends of the insulating layers 131b, 132b, and a tin (Sn) plating layer formed on the nickel plating layer.

[0071] The first and second plating layers 131c, 132c are intended to increase the adhesive strength between the multilayer ceramic capacitor 100 when the multilayer ceramic capacitor 100 is mounted on a printed circuit board or the like by soldering. The plating process may be performed by a known method, and it is preferable to perform lead-free plating in consideration of environmental friendliness, but the present invention is not limited thereto.

[0072] Hereinafter, the relationship between the dimensions of the components included in the multilayer ceramic capacitor according to the present embodiment and the acoustic noise will be described.

[0073] FIG. 4 is a cross-sectional view showing a schematic longitudinal section of the multilayer ceramic capacitor shown in FIG. 1, for explaining the dimensional relationship between components included in the multilayer ceramic capacitor of the present embodiment.

[0074] Referring to FIG. 4, half the total thickness of the ceramic body 110 is defined as A, the thickness of the lower cover portion 113 is defined as B, half the total thickness of the active portion 115 is defined as C, and the thickness of the upper cover portion 112 is defined as D.

[0075] Here, the total thickness of the ceramic body 110 means the distance from the top surface to the bottom surface of the ceramic body 110, and the total thickness of the active portion 115 means the distance from the top surface of the second internal electrode 122 formed at the top of the active portion 115 to the bottom surface of the first internal electrode 121 formed at the bottom of the active portion 115.

[0076] In addition, the thickness B of the lower cover part 113 means the distance from the lower surface of the first internal electrode 121 formed at the bottom of the active part 115 in the thickness direction to the lower surface of the ceramic body 110, and the thickness D of the upper cover part 112 means the distance from the upper surface of the second internal electrode 122 formed at the top of the active part 115 in the thickness direction to the upper surface of the ceramic body 110.

[0077] When voltages of opposite polarities are applied to the first and second external electrodes 131, 132 arranged on the first and second side surfaces forming both end surfaces in the longitudinal direction of the multilayer ceramic capacitor 100, the ceramic body 110 expands and contracts in the thickness direction due to the inverse piezoelectric effect of the dielectric layer 111, and the two side surfaces forming both end surfaces in the longitudinal direction of the ceramic body 110 contract and expand in the opposite direction to the expansion and contraction of the ceramic body 110 in the thickness direction due to the Poisson effect.

[0078] Here, the center of the active portion 115 is a portion where contraction and expansion occur significantly on both side surfaces forming both end faces in the longitudinal direction where the first and second external electrodes 131 and 132 are formed. When solder is bonded to this portion, the contraction and expansion behavior of both side surfaces forming both end faces in the longitudinal direction of the ceramic body 110 is mostly transmitted to the printed circuit board via the solder, resulting in a significant increase in acoustic noise.

[0079] However, in this embodiment, due to the insulating layers 131b, 132b, the solder is formed only on the lower end of the ceramic body 110 and on the lower parts of the side surfaces that form both end faces in the longitudinal direction corresponding to the lowest layer internal electrode, and the lower cover part 113 is formed to have a greater thickness than the upper cover part 112.

[0080] Therefore, when a voltage is applied, the central portion CL of the active portion 115 A The difference between the deformation rate of the lower cover portion 113 and the deformation rate of the lower cover portion 114 causes inflection points formed on both side surfaces of the ceramic body 110 that form both end surfaces in the length direction of the ceramic body 110 to be in the center CL C Since the following is formed, acoustic noise can be reduced.

[0081] At this time, in order to further reduce acoustic noise, the central portion CL of the active portion 115 is A is the center CL of the ceramic body 110. C The ratio (B+C) / A away from the above can satisfy the range of 1.050≦(B+C) / A≦1.764.

[0082] Furthermore, the ratio D / B of the thickness D of the upper cover portion 112 to the thickness B of the lower cover portion 113 can satisfy the range of 0.021≦D / B≦0.545.

[0083] Furthermore, the ratio B / A of the thickness B of the lower cover portion 113 to A, which is half the thickness of the ceramic body 110, can more preferably satisfy the range of 0.331≦B / A≦1.537.

[0084] Furthermore, the ratio C / B, which is half the thickness of the active portion 115 relative to the thickness B of the lower cover portion 113, can more preferably satisfy the range of 0.148≦C / B≦2.441.

[0085] Experimental Example The multilayer ceramic capacitors according to the embodiments and comparative examples of the present invention were fabricated as follows.

[0086] A slurry formed by mixing powder such as barium titanate (BaTiO3), a polymer, and a solvent is applied onto a carrier film using a method such as a doctor blade, and then dried to prepare a number of ceramic green sheets manufactured to a thickness of several μm.

[0087] The ceramic sheet is for forming the dielectric layer 111 of the ceramic body 110 .

[0088] Next, a conductive paste for internal electrodes is applied to a predetermined thickness on the ceramic green sheets to form first and second internal electrodes 121 and 122 so as to be exposed on both end surfaces facing each other in the longitudinal direction of the ceramic green sheets.

[0089] The conductive paste may be applied by screen printing, gravure printing or the like, but the present invention is not limited to this method.

[0090] Next, the plurality of ceramic green sheets are laminated such that the plurality of first and second internal electrodes 121, 122 are arranged to face each other with the ceramic sheets interposed therebetween, to form a laminate.

[0091] At this time, the ceramic green sheets on which the first and second internal electrodes 121, 122 are not formed are laminated below the ceramic green sheets on which the first and second internal electrodes 121, 122 are formed in a larger number than the upper portions.

[0092] The laminate thus formed was subjected to a test at approximately 85°C and a pressure of approximately 1,000 kgf / cm 2 Isostatic pressing is performed under the pressure conditions.

[0093] Next, the laminate that has been pressure-bonded is cut into individual regions corresponding to individual capacitors, and the cut chips are maintained in an air atmosphere at about 230° C. for about 60 hours to remove the binder.

[0094] Next, in order to prevent the first and second internal electrodes 121 and 122 from being oxidized at about 1,200° C., the oxygen partial pressure was set at 10 -11 ~10 -10 The ceramic body 110 is produced by firing in a reducing atmosphere under an oxygen partial pressure of atm.

[0095] Next, the first and second external electrodes 131 and 132 are formed on the thickness-width end surfaces of the ceramic body 110 so as to be electrically connected to the exposed portions of the first and second internal electrodes 121 and 122 .

[0096] Hereinafter, a method for forming the first and second external electrodes 131 and 132 will be described in detail.

[0097] First, a seed layer may be formed using a conductive paste on the lower surface of the ceramic body 110. The conductive metal contained in the conductive paste forming the seed layer may be the same as that of the internal electrodes, but is not limited thereto, and may be, for example, copper (Cu), nickel (Ni), palladium (Pd), platinum (Pt), gold (Au), silver (Ag), lead (Pb), or the like, alone or in combination with an alloy of these.

[0098] The method of forming the seed layer 135 using the conductive paste may be, for example, a screen printing method or a gravure printing method, but is not limited thereto, and may be a sputtering method or a vapor deposition method.

[0099] Next, first and second electrode layers 131a and 132a may be formed to be in contact with and electrically connected to the internal electrodes 121 and 122 exposed on both sides forming both end faces in the length direction of the ceramic body 110. The first and second electrode layers 131a and 132a may be formed of the same conductive metal as the internal electrodes, but are not limited thereto, and may be, for example, copper (Cu), silver (Ag), nickel (Ni), or the like, or an alloy thereof.

[0100] As a method for forming the first and second electrode layers 131a and 132a on both side surfaces that form both end surfaces in the longitudinal direction of the ceramic body 110, a sheet transfer method or a pad transfer method may be used instead of the conventional dipping method.

[0101] Specifically, a sheet or pad for forming the first and second electrode layers is placed on a pressure-bonding rubber on a platen, and the ceramic body is pressed against the sheet or pad to adhere the sheet or pad to the ceramic body.

[0102] At this time, heat is applied to the base plate to increase the flexibility of the sheet, and the sheet is attached so as to extend from the head surface, which is the side surface that forms both end faces in the longitudinal direction of the ceramic body, to the underside on which the seed layer is formed, while increasing the adhesive strength between the body and the sheet.

[0103] Next, in order to remove the unnecessary parts of the sheet attached to the ceramic body, the ceramic body with the sheet attached is pressed against a punching rubber on a platen, and the elasticity of the rubber removes the parts of the sheet that are not attached to the body.

[0104] Meanwhile, as another method, a sheet for forming the first and second electrode layers with a PET film attached thereto is placed on a pressure-bonding rubber on a platen, and the ceramic body 110 is pressed against the sheet to adhere the sheet to the ceramic body, thereby attaching the sheet for forming the first electrode layer to the ceramic body.

[0105] At this time, the sheet is cut at the corners of the ceramic body 110 by the PET film, and when the pressure is removed, the sheet is attached only to the head surface of the ceramic body.

[0106] In this case, the portion of the sheet that is not attached to the ceramic body remains on the PET film, and a separate process of removing the unnecessary sheet can be omitted.

[0107] According to the above method, the first and second electrode layers are formed only on the head surfaces, which are both side surfaces that form both end surfaces in the length direction of the ceramic body, and are connected to the seed layer formed on the lower surface of the ceramic body, which further reduces the thickness of the external electrodes, thereby realizing a high-capacity multilayer ceramic capacitor.

[0108] Next, the insulating layers 131b, 132b are formed on the first and second electrode layers 131a, 132a using an epoxy resist or the like.

[0109] In this case, the insulating layers 131b and 132b may be formed up to within a region adjacent to the internal electrodes when the lower cover portion 113 is divided into three equal parts in the thickness direction.

[0110] The epoxy resist may be applied by dipping or various printing methods, but the present invention is not limited thereto. After the application process, a heat treatment process is performed to solidify the applied epoxy resist.

[0111] Meanwhile, if necessary, after the step of forming the insulating layers 131b, 132b, a plating process such as electroplating can be performed on the area from the lower surface of the ceramic body on which the first and second electrode layers 131a, 132a are arranged to the ends of the insulating layers 131b, 132b arranged on the side surfaces that form both end faces in the longitudinal direction, to form the first and second plating layers 131c, 132c.

[0112] The material used for the plating may be nickel, tin, nickel-tin alloy, etc., but the present invention is not limited thereto.

[0113] Furthermore, if necessary, the first and second plating layers 131c, 132c can be formed by applying a nickel plating layer and a tin plating layer in sequence to the region from the lower surface of the ceramic body on which the first and second electrode layers 131a, 132a are arranged to the ends of the insulating layers 131b, 132b arranged on the side surfaces that form both end faces in the longitudinal direction.

[0114] Multilayer ceramic capacitors were manufactured using the above manufacturing method, and the manufacturing tolerance was set to within ±0.1 mm in length x width (L x W). When this tolerance was met, experiments were conducted and acoustic noise was measured.

[0115] [Table 1] Here, * is a comparative example, and AN is acoustic noise.

[0116] The data in Table 1 above was obtained by measuring the dimensions of a cross section taken with a scanning electron microscope (SEM) of the ceramic body 110 of the multilayer ceramic capacitor 100 cut in the length direction L and thickness direction T from the center of the width direction W of the ceramic body 110 as shown in FIG. 4.

[0117] Here, A, B, C, and D are defined as 1 / 2 the total thickness of the ceramic body 110, B the thickness of the lower cover portion 113, C the half the total thickness of the active portion 115, and D the thickness of the upper cover portion 112, as described above.

[0118] To measure acoustic noise, one sample (multilayer ceramic capacitor) per acoustic noise measurement board was mounted on a printed circuit board by dividing it vertically, and the board was then attached to a measurement jig.

[0119] In addition, DC voltage and voltage fluctuation were applied to both terminals of the sample attached to the measurement jig using a DC power supply and a signal generator. Acoustic noise was measured using a microphone installed directly above the printed circuit board.

[0120] In Table 1 above, samples 1 to 3 are comparative examples having a symmetrical cover structure in which the thickness B of the lower cover part 113 and the thickness D of the upper cover part 112 are approximately similar, and samples 4 to 13 are comparative examples having a structure in which the thickness D of the upper cover part 112 is thicker than the thickness B of the lower cover part 113.

[0121] Samples 14 and 35 to 37 are comparative examples having a structure in which thickness B of lower cover portion 113 is greater than thickness D of upper cover portion 112, and Samples 15 to 34 are examples according to the embodiment of the present invention.

[0122] Here, when the (B+C) / A value is approximately 1, it means that the center of the active part 115 is not far from the center of the ceramic body 110. The (B+C) / A value is approximately 1 for Samples 1 to 3, which have a symmetrical cover structure in which the thickness B of the lower cover part 113 and the thickness D of the upper cover part 112 are approximately similar.

[0123] When the value of (B+C) / A is greater than 1, it may mean that the center of the active portion 115 is separated from the center of the ceramic body 110 in an upward direction, and when the value of (B+C) / A is less than 1, it may mean that the center of the active portion 115 is separated from the center of the ceramic body 110 in a downward direction.

[0124] Referring to Table 1 above, it can be seen that in samples 15 to 34, which are embodiments in which the ratio (B+C) / A of the distance between the center of the active portion 115 and the center of the ceramic body 110 satisfies the range of 1.050≦(B+C) / A≦1.764, the acoustic noise was significantly reduced to less than 25 dB.

[0125] In addition, samples 1 to 14, in which the ratio (B+C) / A of the distance between the center of the active portion 115 and the center of the ceramic body 110 is less than 1.050, have a structure in which the center of the active portion 115 is hardly separated from the center of the ceramic body 110 or is separated downward from the center of the ceramic body 110.

[0126] It can be seen that samples 1 to 14, in which the (B+C) / A ratio is less than 1.050, have acoustic noise of 25 to 31 dB, and thus have no effect in reducing acoustic noise compared to the examples of the present invention.

[0127] In addition, in the case of samples 35 to 37 in which the ratio (B+C) / A of the distance between the center of the active portion 115 and the center of the ceramic body 110 exceeded 1.764, the capacitance was low relative to the target capacitance, resulting in capacitance failure.

[0128] In Table 1 above, a capacity realization rate (i.e., the ratio of capacitance to the target capacitance) indicated as "NG" means that when the target capacitance value is 100%, the capacitance value relative to the target capacitance is less than 80%.

[0129] Also, in the embodiment in which the ratio (D / B) of the thickness D of the upper cover part 112 to the thickness B of the lower cover part 113 satisfies the range of 0.021≦D / B≦0.545, it can be seen that the acoustic noise is significantly reduced.

[0130] On the other hand, in the comparative example in which the ratio (D / B) of the thickness D of the upper cover part 112 to the thickness B of the lower cover part 113 exceeds 0.545, there is no effect of reducing acoustic noise.

[0131] If the ratio (D / B) of the thickness D of the upper cover part 112 to the thickness B of the lower cover part 113 is less than 0.021, the thickness B of the lower cover part 113 will be too large compared to the thickness D of the upper cover part 112, which may cause cracks or delamination, and the electrostatic capacitance may be low relative to the target capacitance, resulting in capacitance failure.

[0132] On the other hand, in samples 19 to 34, which are examples in which the ratio (B / A) of the thickness B of the lower cover part 113 to A, which is 1 / 2 the thickness of the ceramic body 110, and the ratio (C / B) of C, which is 1 / 2 the thickness of the active part 115 to the thickness B of the lower cover part 113, respectively, satisfy the ranges of 0.331≦B / A≦1.537 and 0.148≦C / B≦2.441, respectively, it can be seen that the acoustic noise was further reduced to less than 18 dB.

[0133] On the other hand, in the case of samples 35 to 37 in which the ratio (B / A) of the thickness B of the lower cover part 113 to A (half the thickness of the ceramic body 110) exceeded 1.537 or the ratio (C / B) of C (half the thickness of the active part 115) to the thickness B of the lower cover part 113 was less than 0.148, there was a problem that the electrostatic capacitance was low relative to the target capacitance, resulting in capacitance failure.

[0134] Multilayer ceramic capacitor mounting board FIG. 5 is a perspective view showing a state in which the multilayer ceramic capacitor in FIG. 1 is mounted on a printed circuit board, with a portion of the multilayer ceramic capacitor cut away, and FIG. 6 is a cross-sectional view showing the multilayer ceramic capacitor and the printed circuit board in FIG. 5 cut in the longitudinal direction.

[0135] 5 and 6, the mounting substrate 200 of the multilayer ceramic capacitor 100 according to the present embodiment includes a printed circuit board 210 on which the multilayer ceramic capacitor 100 is mounted, and first and second electrode pads 221 and 222 formed spaced apart from each other on an upper surface of the printed circuit board 210.

[0136] In addition, the multilayer ceramic capacitor 100 is mounted such that the lower surfaces of the first and second external electrodes 131 and 132, on which the insulating layers 131b and 132b are not formed and on which the first and second electrode layers 131a and 132a are exposed, face the printed circuit board 210.

[0137] In addition, the multilayer ceramic capacitor 100 may be electrically connected to the printed circuit board 210 by the solder 230 with the lower cover part 113 disposed on the lower side and the first and second plating layers 131c, 132c formed on the first and second electrode layers 131a, 132a, respectively, positioned to contact the first and second electrode pads 221, 222.

[0138] When a voltage is applied to the multilayer ceramic capacitor 100 mounted on the printed circuit board 210 as described above, acoustic noise may be generated.

[0139] In this case, the size of the first and second electrode pads 221, 222 may be an index for determining the amount of solder 230 connecting the first and second external electrodes 131, 132 of the multilayer ceramic capacitor 100 to the first and second electrode pads 221, 222, and the magnitude of acoustic noise may be adjusted according to the amount of solder 230.

[0140] In this embodiment, the solder 230 is formed only up to the end of the insulating layer on the side surfaces that form both end faces in the longitudinal direction of the ceramic body 110, and therefore, by reducing the amount of solder 230 as described above, the magnitude of acoustic noise can be reduced.

[0141] FIG. 7 is a cross-sectional view illustrating a state in which the multilayer ceramic capacitor in FIG. 5 is deformed when a voltage is applied to the multilayer ceramic capacitor mounted on a printed circuit board.

[0142] Referring to FIG. 7, when voltages of opposite polarities are applied to the first and second external electrodes 131, 132 of the multilayer ceramic capacitor 100 mounted on the printed circuit board 210, the ceramic body 110 expands and contracts in the thickness direction due to the inverse piezoelectric effect of the dielectric layer 111, and both side surfaces forming both end faces in the length direction of the ceramic body 110 on which the first and second external electrodes 131, 132 are formed contract and expand in the opposite direction to the expansion and contraction in the thickness direction of the ceramic body 110 due to the Poisson effect.

[0143] Here, the center of the active portion 115 is a portion where significant contraction and expansion occur at both ends in the longitudinal direction where the first and second external electrodes 131, 132 are formed. When the solder 230 is joined to this portion, the contraction and expansion behavior of both ends in the longitudinal direction of the ceramic body 110 is mostly transmitted to the printed circuit board 210 via the solder 230, which may significantly increase the generation of acoustic noise.

[0144] However, according to the present embodiment, the mounting surfaces of the first and second external electrodes 131 and 132 are formed at a position where the ceramic body 110 is less displaced and vibration is not easily transmitted, that is, on the lower surface.

[0145] Therefore, when a voltage is applied, the central portion CL of the active portion 115 A The inflection points formed on both sides of the length of the ceramic body 110 due to the difference in the deformation rate between the upper cover part 112 and the lower cover part 113 are formed below the height of the solder 230, thereby reducing acoustic noise.

[0146] In addition, the first and second external electrodes 131, 132 are not formed on both side surfaces in the width direction, but rather in a predetermined region on both side surfaces in the length direction of the ceramic body 110, i.e., from the upper corner portion in the thickness direction of the ceramic body 110 to the region adjacent to the internal electrodes when the lower cover portion 113 is divided into three equal parts in the thickness direction, the solder 230 is not formed due to the insulating layers 131b, 132b, so that the height of the solder 230 can be minimized.

[0147] By reducing the volume of the solder 230 formed around the first and second external electrodes 131, 132 in this manner, it is possible to reduce acoustic noise transmitted through the first and second external electrodes 131, 132 and the solder 230. Furthermore, even when a plurality of multilayer ceramic capacitors 100 are mounted on the printed circuit board 210 at a narrow pitch, i.e., even when the multilayer ceramic capacitors 100 are mounted at high density, no solder bridges are formed between the respective multilayer ceramic capacitors 100, thereby improving the reliability of the components.

[0148] Although the embodiments of the present invention have been described in detail above, it will be apparent to those skilled in the art that the scope of the present invention is not limited thereto, and that various modifications and variations are possible within the scope of the technical idea of ​​the present invention described in the claims. [Explanation of symbols]

[0149] 100 Multilayer ceramic capacitor 110 Ceramic body 111 Dielectric layer 121, 122 First and second internal electrodes 131, 132 First and second external electrodes 131a, 132a First and second electrode layers 131b, 132b Insulating layer 131c, 132c First and second plating layers 200 Mounting Board 210 Printed Circuit Board 221, 222 First and second electrode pads 230 Solder

Claims

1. a ceramic body including a plurality of dielectric layers; an active portion including a plurality of first and second internal electrodes that are stacked in the ceramic body with the plurality of dielectric layers interposed therebetween and that are alternately exposed at both end faces that face each other in a longitudinal direction of the ceramic body; an upper cover portion formed on an upper portion of the active portion; a lower cover portion formed under the active portion and having a thickness greater than that of the upper cover portion; a first external electrode electrically connected to the first internal electrode and a second external electrode electrically connected to the second internal electrode, the first and second external electrodes include first and second electrode layers disposed on both side surfaces and a bottom surface of the ceramic body that define both end surfaces in a longitudinal direction of the ceramic body, but not disposed on a top surface of the ceramic body; a first insulating layer is further disposed on the first electrode layer, and a second insulating layer is further disposed on the second electrode layer, and the first insulating layer and the second insulating layer are disposed from a horizontal point corresponding to an upper corner portion in a thickness direction of the ceramic body to a horizontal point corresponding to an upper portion when the lower cover portion is divided into three equal parts in a thickness direction; the first insulating layer and the second insulating layer are spaced apart from each other and are not disposed on an upper surface of the ceramic body; The first and second external electrodes further include first and second plating layers disposed on the first and second electrode layers to ends of the first and second insulating layers in the thickness direction. Multilayer ceramic electronic components.

2. 2. The multilayer ceramic electronic component according to claim 1, wherein the first and second electrode layers are disposed on both side surfaces that define both end faces in the length direction of the ceramic body, extending in the width direction to both corner portions.

3. 3. The multilayer ceramic electronic component according to claim 1, wherein the first and second electrode layers are disposed so as to extend to both end faces opposed to each other in a width direction of the ceramic body.

4. 4. The multilayer ceramic electronic component according to claim 1, wherein when half of a total thickness of the ceramic body is defined as A, the thickness of the lower cover portion is defined as B, half of a total thickness of the active portion is defined as C, and the thickness of the upper cover portion is defined as D, a ratio (B+C) / A of a distance between a center of the active portion and a center of the ceramic body satisfies a range of 1.050≦(B+C) / A≦1.

764.

5. 5. The multilayer ceramic electronic component according to claim 1, wherein a ratio D / B of a thickness D of the upper cover portion to a thickness B of the lower cover portion satisfies a range of 0.021≦D / B≦0.

545.

6. 6. The multilayer ceramic electronic component according to claim 1, wherein a ratio B / A of a thickness B of the lower cover portion to A, which is 1 / 2 of an entire thickness of the ceramic body, satisfies a range of 0.331≦B / A≦1.

537.

7. 7. The multilayer ceramic electronic component according to claim 1, wherein a ratio C / B of C, which is 1 / 2 of a total thickness of the active portion, to a thickness B of the lower cover portion satisfies a range of 0.148≦C / B≦2.

441.

8. 8. The multilayer ceramic electronic component according to claim 1 , wherein when a thickness of the first and second electrode layers in a central region in a thickness direction of the ceramic body is T1 and a thickness of the first and second electrode layers at a point where an outermost internal electrode is located at an upper portion of the ceramic body in the thickness direction of the ceramic body is T2, 0.8≦T2 / T1≦1.2 is satisfied.

9. a printed circuit board having electrode pads thereon; The multilayer ceramic electronic component according to claim 1 , which is disposed on the electrode pads; and solder connecting the electrode pad and the multilayer ceramic electronic component, A mounting board for a multilayer ceramic electronic component, wherein the solder is disposed on side surfaces that form both end faces in the longitudinal direction and a mounting surface of the ceramic body.

10. 10. The mounting board for a multilayer ceramic electronic component according to claim 9, wherein the first insulating layer and the second insulating layer are disposed up to a horizontal point corresponding to an upper portion when the lower cover portion is divided into three equal parts in a thickness direction.

11. 11. The mounting substrate for a multilayer ceramic electronic component according to claim 9, wherein the solder is disposed up to lower parts of the first insulating layer and the second insulating layer in a thickness direction of the ceramic body.

12. 12. The mounting substrate for a multilayer ceramic electronic component according to claim 9, wherein, when a thickness of the first and second electrode layers in a central region in a thickness direction of the ceramic body is T1 and a thickness of the first and second electrode layers at a point where an upper outermost internal electrode in the thickness direction of the ceramic body is located among the internal electrodes is T2, 0.8≦T2 / T1≦1.2 is satisfied.

13. A printed circuit board; Two or more electrode pads disposed on the printed circuit board; A ceramic body; first and second external electrodes each having an L-shape and disposed on both end surfaces in a length direction and on a bottom surface in a thickness direction of the ceramic body, respectively; solder connecting the electrode pads to the first and second external electrodes, the ceramic body includes an active portion having first and second internal electrodes connected to the first and second external electrodes; an upper cover portion disposed on an upper portion of the active portion; a lower cover part disposed under the active part and having a thickness greater than that of the upper cover part; the ceramic body further includes first and second insulating layers disposed from upper portions of the first and second external electrodes disposed on both end surfaces of the ceramic body to horizontal points corresponding to upper portions when the lower cover part is divided into three equal parts in a thickness direction of the ceramic body, the first insulating layer is disposed on a first electrode layer of the first external electrode, and the second insulating layer is disposed on a second electrode layer of the second external electrode; the first insulating layer and the second insulating layer are spaced apart from each other and are not disposed on an upper surface of the ceramic body; The first and second external electrodes further include first and second plating layers disposed on the first and second electrode layers to ends of the first and second insulating layers in the thickness direction. A mounting board for multilayer ceramic electronic components.

14. 14. The mounting substrate for a multilayer ceramic electronic component according to claim 13, wherein the solder is disposed in a thickness direction of the ceramic body up to a lower portion of a horizontal region corresponding to the active portion.

Citation Information

Patent Citations

  • Manufacturing method of electronic component and electronic component

    JP2012119616A

  • Multilayer capacitor and manufacturing method of multilayer capacitor

    JP2012248581A

  • Multilayer ceramic electronic component and fabrication method thereof

    JP2013149939A

  • Multilayer capacitor

    JP2014017470A

  • Laminated ceramic capacitor and mounting board of the same

    JP2014132633A