METHOD FOR PREPARING MEASUREMENT SAMPLE FOR MALDI MASS ANALYSIS, APPARATUS FOR PREPARING MEASUREMENT SAMPLE FOR MALDI MASS ANALYSIS, AND SUBSTRATE FOR PREPARING MEASUREMENT SAMPLE FOR MALDI MASS ANALYSIS

By applying a laser beam with a wavelength of 400 nm or more to a base material with a laser energy-absorbing material and matrix, multiple matrices can be precisely placed on a sample for MALDI mass spectrometry, addressing inefficiencies in conventional methods and enhancing sensitivity and accuracy.

JP7567562B2Active Publication Date: 2024-10-16RICOH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021033985
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-03-23
Filing Date
2021-03-04
Publication Date
2024-10-16
Estimated Expiration
2041-03-04

AI Technical Summary

Technical Problem

Conventional MALDI mass spectrometry methods are limited to using a single type of matrix on a sample, which is inefficient for samples with multiple components, and rely heavily on operator skill, leading to non-uniform matrix crystal diameters and low quantitative performance.

Method used

A method for preparing a measurement sample for MALDI mass spectrometry involves using a base material with a laser energy-absorbing material and a matrix, where a laser beam with a wavelength of 400 nm or more is applied to the opposite side of the matrix, causing it to fly and be placed at predetermined positions on the sample, allowing multiple types of matrices to be used.

Benefits of technology

This approach enables precise placement of matrices suitable for different targets, such as proteins, lipids, and nucleotides, facilitating highly sensitive imaging mass spectrometry with reduced sample alteration and variation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567562000004
    Figure 0007567562000004
  • Figure 0007567562000005
    Figure 0007567562000005
  • Figure 0007567562000006
    Figure 0007567562000006
Patent Text Reader

Abstract

To provide a measurement sample preparation method for MALDI mass spectroscopy that, in performing mass spectroscopy with MALDI, can arrange two or more types of matrices in one sample and further can perform MALDI mass spectroscopy with a small variation.SOLUTION: A measurement sample preparation method for MALDI mass spectroscopy includes: irradiating, with a laser beam, a surface of a substrate having matrices arranged on its surface used for preparation of a measurement sample for MALDI mass spectroscopy, the surface of the substrate on the opposite side of the surface having the matrices, to cause the matrices to fly from the substrate to be arranged at a predetermined position of a sample to be subjected to the MALDI mass spectroscopy. The substrate has a laser energy absorbing material, and the wavelength of laser energy for the laser beam is 400 nm or more.SELECTED DRAWING: Figure 4A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for preparing a measurement sample for MALDI mass spectrometry, an apparatus for preparing a measurement sample for MALDI mass spectrometry, and a substrate for preparing a measurement sample for MALDI mass spectrometry. [Background technology]

[0002] Mass spectrometry is an analytical technique that can obtain information regarding the specific chemical structure of a target molecule by ionizing a sample containing the target molecule, and then separating and detecting the ions derived from the target molecule based on their mass-to-charge ratio (m / z).

[0003] In mass spectrometry, sample ionization is a factor that determines the quality of the analysis, and many methods have been developed for this purpose, such as MALDI (Matrix Assisted Laser Desorption / Ionization) and ESI (Electrospray ionization). These methods are used in biotechnology, medical technology, and other technical fields because they are easy to ionize even with a small amount of sample.

[0004] In MALDI, a pulsed laser beam is irradiated onto a portion of a sample where a matrix, a substance that assists in ionizing the sample, has been applied, thereby ionizing the sample together with the matrix. The pulsed laser beam is often in the ultraviolet region, and it is preferable to use a wavelength that matches the light absorption characteristics of the matrix. The matrix is ​​a crystalline organic low-molecular-weight material, and it is said that it must be co-crystallized or mixed with the sample. Since it is believed that the uniformity and degree of mixing of the co-crystal affect the sensitivity and accuracy of the analysis, lasers are being developed according to the sample.

[0005] Various methods for applying these matrices to samples have also been proposed, including a method for preparing samples for mass spectrometry in which a matrix is ​​evaporated to form microcrystals, and then a matrix solution is sprayed to grow matrix crystals on the microcrystals (see, for example, Patent Document 1). Summary of the Invention [Problem to be solved by the invention]

[0006] The present invention aims to provide a method for preparing a measurement sample for MALDI mass spectrometry, which enables two or more types of matrices to be placed in one sample when performing MALDI mass spectrometry, and further enables MALDI mass spectrometry to be performed with little variation. [Means for solving the problem]

[0007] As a means for solving the above-mentioned problems, the method of preparing a measurement sample for MALDI mass spectrometry of the present invention includes irradiating a laser beam onto a surface of a substrate opposite to the side having a matrix used in preparing a measurement sample for MALDI mass spectrometry, causing the matrix to fly from the substrate and be placed at a predetermined position of a sample to be subjected to MALDI mass spectrometry, wherein the substrate has a laser energy absorbing material, and the laser energy of the laser beam has a wavelength of 400 nm or more. Effect of the Invention

[0008] According to the present invention, there is provided a method for preparing a measurement sample for MALDI mass spectrometry, which enables two or more types of matrices to be placed in one sample when performing MALDI mass spectrometry, and further enables MALDI mass spectrometry to be performed with little variation. [Brief description of the drawings]

[0009] [Figure 1A] FIG. 1A is a schematic diagram showing an example of the entire powder forming apparatus. [Figure 1B]FIG. 1B is a schematic diagram showing a droplet forming head in the droplet forming unit of FIG. 1A. [Figure 1C] FIG. 1C is a cross-sectional view of the droplet forming unit of FIG. 1A taken along line AA'. [Figure 1D] FIG. 1D is a schematic diagram showing an example of applying a matrix onto a substrate by electrostatic application. [Diagram 2] FIG. 2 is a schematic diagram showing an example of a laser beam irradiation means that can be used in the method of the present invention for preparing an measurement sample for MALDI mass spectrometry. [Figure 3A] FIG. 3A is a block diagram showing an example of hardware of a measurement sample preparation device for MALDI mass spectrometry. [Figure 3B] FIG. 3B is a block diagram showing an example of the functions of the measurement sample preparation device for MALDI mass spectrometry. [Figure 3C] FIG. 3C is a flow chart showing an example of the processing procedure of the measurement sample preparation program for MALDI mass spectrometry of the present invention. [Figure 4A] FIG. 4A is a schematic diagram showing a layer structure of a matrix plate in an example. [Figure 4B] FIG. 4B is a schematic diagram showing a layer structure of a matrix plate in a comparative example. [Figure 5A] FIG. 5A is a diagram showing an example of a base material used in the examples and comparative examples. [Figure 5B] FIG. 5B is a diagram showing an example of a base material on which a sample used in the examples and comparative examples is placed. [Figure 6A] FIG. 6A is a schematic diagram showing the preparation of a measurement sample for MALDI mass spectrometry in an example. [Figure 6B] FIG. 6B is a schematic diagram showing the preparation of a measurement sample for MALDI mass spectrometry in the example. [Figure 6C] FIG. 6C is a schematic diagram showing the preparation of a measurement sample for MALDI mass spectrometry in the example. [Figure 7A] FIG. 7A is a graph showing an example of the results of MALDI mass spectrometry in an example. [Figure 7B]FIG. 7B is a graph showing an example of the results of MALDI mass spectrometry in an example. [Figure 7C] FIG. 7C is a graph showing an example of the results of MALDI mass spectrometry in an example. [Figure 8A] FIG. 8A is a graph showing an example of the results of MALDI mass spectrometry in a comparative example. [Figure 8B] FIG. 8B is a graph showing an example of the results of MALDI mass spectrometry in a comparative example. [Figure 8C] FIG. 8C is a graph showing an example of the results of MALDI mass spectrometry in a comparative example. [Figure 9A] FIG. 9A is a conceptual diagram showing a method for preparing a measurement sample for MALDI mass spectrometry when a general laser beam is used. [Figure 9B] FIG. 9B is a photograph showing an example of a method for preparing a measurement sample for MALDI mass spectrometry when a general laser beam is used. [Figure 9C] Figure 9C is a conceptual diagram showing a method of preparing a measurement sample for MALDI mass spectrometry when an optical vortex laser beam is used. [Figure 9D] Figure 9D is a photograph showing an example of a method for preparing a measurement sample for MALDI mass spectrometry when an optical vortex laser beam is used. [Figure 10A] FIG. 10A is a schematic diagram showing an example of a wavefront (equal phase surface) in a typical laser beam. [Figure 10B] FIG. 10B is a diagram showing an example of a light intensity distribution in a typical laser beam. [Figure 10C] FIG. 10C is a diagram showing an example of a phase distribution in a typical laser beam. [Figure 11A] FIG. 11A is a schematic diagram showing an example of a wavefront (equal phase surface) in an optical vortex laser beam. [Figure 11B] FIG. 11B is a diagram showing an example of the light intensity distribution in an optical vortex laser beam. [Figure 11C] FIG. 11C is a diagram showing an example of a phase distribution in an optical vortex laser beam. [Figure 11D]FIG. 11D is a diagram showing an example of the results of interference measurement of an optical vortex laser beam. [Figure 11E] FIG. 11E is a diagram showing an example of the result of interference measurement of a laser beam having a point of zero light intensity at its center. [Figure 12A] FIG. 12A is a diagram showing an example of a simulation image in which the temperature (energy) distribution of a Gaussian laser beam is represented by contour lines. [Figure 12B] FIG. 12B is a diagram showing an example of an image showing the temperature (energy) distribution of the uniform heating irradiation laser beam. [Figure 13] FIG. 13 is a diagram showing an example of the cross-sectional intensity distribution of a Gaussian laser beam (dotted line) and a uniform heat irradiation laser beam (solid line). [Figure 14A] FIG. 14A is a schematic diagram showing an example of a cross-sectional intensity distribution of a uniform thermal irradiation laser beam. [Figure 14B] FIG. 14B is a schematic diagram showing another example of the cross-sectional intensity distribution of the uniform thermal irradiation laser beam. [Figure 15A] FIG. 15A is a schematic diagram showing an example of the conventional LIFT method using a Gaussian laser beam. [Figure 15B] FIG. 15B is a schematic diagram showing another example of the conventional LIFT method using a Gaussian laser beam. [Figure 15C] FIG. 15C is a schematic diagram showing another example of the conventional LIFT method using a Gaussian laser beam. [Figure 15D] FIG. 15D is a schematic diagram showing an example of the LIFT method using a uniform heat irradiation laser beam in the present invention. [Figure 15E] FIG. 15E is a schematic diagram showing another example of the LIFT method using a uniform heat irradiation laser beam in the present invention. [Figure 15F] FIG. 15F is a schematic diagram showing another example of the LIFT method using a uniform heat irradiation laser beam in the present invention. [Figure 16A] FIG. 16A is a schematic diagram showing an example of adjusting a soaking irradiation laser beam by a geometrical method using an aspheric lens. [Figure 16B] FIG. 16B is a schematic diagram showing an example of adjusting a uniform thermal irradiation laser beam by a wave optics technique using a DOE. [Figure 16C] FIG. 16C is a schematic diagram showing an example of adjusting the uniform heating irradiation laser beam by a combination of a reflective liquid crystal phase conversion element and a prism. [Figure 17A] FIG. 17A is a schematic diagram showing an example of a projectile generating device for carrying out the method of preparing an measurement sample for MALDI mass spectrometry of the present invention. [Figure 17B] FIG. 17B is a schematic diagram showing another example of a projectile generating device for carrying out the method of preparing a measurement sample for MALDI mass spectrometry of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] (Method of preparing a measurement sample for MALDI mass spectrometry and device for preparing a measurement sample for MALDI mass spectrometry) The method for preparing a measurement sample for MALDI mass spectrometry of the present invention includes irradiating a laser beam onto a surface of a substrate opposite to the side having a matrix used in preparing a measurement sample for MALDI mass spectrometry, causing the matrix to fly from the substrate and be placed at a predetermined position of a sample to be subjected to MALDI mass spectrometry, wherein the substrate has a laser energy absorbing material, the laser energy of the laser beam has a wavelength of 400 nm or more, and further includes other steps as necessary. The MALDI mass spectrometry measurement sample preparation device of the present invention is a MALDI mass spectrometry measurement sample preparation device used in the MALDI mass spectrometry measurement sample preparation method of the present invention, and has a laser beam irradiation means for irradiating a laser beam onto the surface of the substrate, and further has other means as necessary.

[0011] MALDI is an abbreviation for Matrix Assisted Laser Desorption / Ionization, and is a method of mass spectrometry known as matrix-assisted laser desorption / ionization. In mass spectrometry using MALDI (hereinafter referred to as "MALDI mass spectrometry"), a pulsed laser is irradiated onto the portion of the sample where a matrix, a material that assists ionization, has been applied, thereby ionizing the sample together with the matrix and performing mass analysis. The matrix is ​​used differently depending on the components to be analyzed in the sample.

[0012] The method and device for preparing a measurement sample for MALDI mass spectrometry of the present invention are based on the finding that conventional methods such as applying a matrix to a sample with a spray gun or applying a matrix by vapor phase spraying or deposition can only provide one type of matrix for one sample. In other words, the present invention is based on the finding that, although there is an optimal matrix depending on the component to be analyzed, conventional methods cannot apply optimal matrices to one sample even if there are multiple components to be analyzed. Furthermore, in such conventional methods for preparing measurement samples for MALDI mass spectrometry, only one type of matrix is ​​applied to the entire sample, and therefore, for a sample containing multiple measurement targets, the same number of samples as the corresponding matrices are required, which is inefficient. The method of the present invention for preparing a measurement sample for MALDI mass spectrometry is based on the knowledge that conventional methods are often dependent on the skill of the operator, which can easily result in non-uniform crystal sizes in the matrix and low quantitative accuracy, which can affect the sensitivity and accuracy of the analysis.

[0013] The method of the present invention for preparing an measurement sample for MALDI mass spectrometry involves irradiating a laser beam having a wavelength of 400 nm or more onto the surface of a substrate having a laser energy absorbing material and a matrix arranged on its surface, the surface of the substrate being opposite the side on which the matrix is ​​arranged, to cause the matrix to fly from the substrate and be placed at a predetermined position in the sample to be subjected to MALDI mass spectrometry. As a result, the method for preparing a sample for MALDI mass spectrometry of the present invention can place matrices suitable for targets to be analyzed, such as proteins, lipids, nucleotides, etc., at their respective predetermined positions even if there is only one sample. Therefore, the method for preparing a sample for MALDI mass spectrometry of the present invention can perform high-sensitivity imaging mass spectrometry for each target to be analyzed, even if there are multiple targets to be analyzed for one sample. Furthermore, the method for preparing a measurement sample for MALDI mass spectrometry of the present invention has a laser energy absorbing material, and can cause the matrix to fly from the substrate by irradiating a laser beam with a wavelength of 400 nm or more (visible light wavelength region), so that it is possible to prevent the target to be analyzed from being altered (damaged) by irradiating it with a high-energy laser beam. This makes it possible to perform MALDI mass spectrometry with little variation. Here, "alteration" means that the structure, molecular weight, etc. of the substance change. The alteration can be confirmed, for example, by checking whether the proportion of low molecular weight components has increased by mass spectrometry.

[0014] <Substrate with laser energy absorbing material and matrix on its surface> The substrate having the laser energy absorbing material and the matrix disposed on the surface thereof is not particularly limited and can be appropriately selected depending on the purpose. In the following, the "substrate having the laser energy absorbing material and the matrix disposed on the surface thereof" is referred to as a "matrix plate." The matrix plate includes a laser energy absorbing material, a matrix, and a substrate.

[0015] <<Laser energy absorbing materials>> The laser energy absorbing material is not particularly limited as long as it can absorb the energy of a laser beam having a wavelength of 400 nm or more, and can be appropriately selected according to the purpose, and examples thereof include those having a transmittance of 60% or less at the wavelength of the laser beam. The transmittance of the wavelength of the laser beam can be measured using a spectrophotometer such as the UV-Vis-Infrared Spectrophotometer V-660 (manufactured by JASCO Corporation). The shape of the laser energy absorbing material is not particularly limited and may be appropriately selected depending on the purpose, and is preferably a thin film with an average thickness of 3 μm or less.

[0016] The material of the laser energy absorbing material is preferably a material that is inactive to the matrix and has a conductive surface when the matrix is ​​formed on the laser energy absorbing material. If the material is inactive to the matrix, there is no risk of chemical reaction with the matrix when irradiated with a laser beam. In addition, if the material has a conductive surface when the matrix is ​​formed on the laser energy absorbing material, the matrix can be electrostatically applied, making it possible to form a more uniform matrix and improve the matrix application yield.

[0017] The material of the laser energy absorbing material is not particularly limited and can be appropriately selected depending on the purpose. For example, metals and the like can be mentioned. Examples of metals include gold, platinum, palladium, silver, etc. Among these, gold is preferred because it absorbs a wide range of laser beam wavelengths and is inactive.

[0018] When the laser energy absorbing material is a metal thin film, its average thickness is preferably 20 nm or more and 200 nm or less. When the laser energy absorbing material is a metal thin film with an average thickness of 20 nm or more and 200 nm or less, the occurrence of variation in surface conductivity can be suppressed, and when the matrix is ​​applied by electrostatic application, the occurrence of variation in matrix thickness can be suppressed. Methods for forming the laser energy absorbing material on the substrate include, for example, vacuum deposition and sputtering.

[0019] <<Matrix>> There are no particular limitations on the matrix, so long as it is a material that can suppress photolysis and thermal decomposition of the sample and can suppress fragmentation (cleavage) of the sample, and the matrix can be appropriately selected depending on the purpose. Examples of the matrix include known matrices, such as 1,8-diaminonaphthalene (1,8-DAN), 2,5-dihydroxybenzoic acid (hereinafter sometimes abbreviated as "DHBA"), 1,8-anthracenedicarboxylic acid dimethyl ester, and the like. ester), Leucoquinizarin, Anthrarobin, 1,5-Diaminonaphthalene (1,5-DAN), 6-Aza-2-thiothymine, 1,5-Diaminoanthraquinone, 1,6-Diaminopyrene, 3,6-Diaminocarbazole, 1,8-Anthracenedicarboxylic Acid, Norharmane, 1-Pyrenepropylamine hydrochloride, 9-Aminofluorene Hydrochloride, Ferulic Acid acid), Dithranol, 2-(4-Hydroxyphenylazo)benzoic acid (HABA), trans-2-[3-(4-tert-butylphenyl)-2-methyl-2-propenylidene]malononitrile (DCTB), trans-4-Phenyl-3-buten-2-one (TPBO), trans-3-Indoleacrylic acid (IAA), 1,10-Phenanthroline (1,10-phenanthroline, 5-Nitro-1,10-phenanthroline, α-Cyano-4-hydroxycinnamic acid (CHCA), Sinapic acid (SA), 2,4,6-Trihydroxyacetophenone (THAP), 3-Hydroxypicolinic acid (HPA), Anthranilic acid, Nicotinic acid, 3-Aminoquinoline, 2-Hydroxy-5-methoxybenzoic acid, 2,5-Dimethoxybenzoic acid Examples of suitable matrices include 1-pyrenebutanoic acid, 4,7-phenanthroline, p-coumaric acid, 1-isoquinolinol, 2-picolinic acid, 1-pyrenebutanoic acid, hydrazide (PBH), 1-pyrenebutyric acid (PBA), and 1-pyrenemethylamine hydrochloride (PMA). Among these, matrices that have the property of crystallizing into needles are preferred, and for example, 2,5-dihydroxybenzoic acid (DHBA) is preferred.

[0020] In this method for preparing a measurement sample for MALDI mass spectrometry, the matrix to be ejected from the matrix plate containing the base material can be one of the various matrices described above, but it is preferable to select two or more types. In addition, it is preferable that the two or more types of matrices ejected from the matrix plate containing the substrate are arranged at different predetermined positions in the sample to be subjected to MALDI mass spectrometry, which is advantageous in that two or more types of matrices can be applied separately in one measurement sample, and two or more types of imaging mass spectrometry can be performed in one measurement sample.

[0021] The region where the matrix is ​​formed is not particularly limited as long as it exists on the laser energy absorbing material, and the shape and structural size thereof can be appropriately selected. The matrix may be fully or partially coated on the laser energy absorbing material. When a matrix coats the laser energy absorbing material, the area where the matrix is ​​present may be referred to as the matrix layer. The average thickness of the matrix is ​​not particularly limited and can be appropriately selected depending on the purpose, and is preferably 3 μm to 50 μm, more preferably 5 μm to 30 μm. When the average thickness of the matrix is ​​5 μm to 50 μm, a sufficient amount of the matrix can be accurately attached to the measurement sample in one flight.

[0022] <<Base material>> The substrate is not particularly limited in terms of shape, structure, size, material, etc., and can be appropriately selected depending on the purpose.

[0023] The shape of the substrate is not particularly limited as long as it can support a matrix on the surface and can be irradiated with a laser beam or an optical vortex laser beam from the back side, and can be appropriately selected according to the purpose. In addition, examples of the shape of the flat substrate include a slide glass.

[0024] The material of the substrate is not particularly limited as long as it transmits the laser beam or optical vortex laser beam, and can be appropriately selected according to the purpose. Among the materials that transmit the laser beam or optical vortex laser beam, inorganic materials such as various glasses mainly composed of silicon oxide, transparent heat-resistant plastics, organic materials such as elastomers are preferable in terms of transmittance and heat resistance.

[0025] The surface roughness Ra of the substrate is not particularly limited and can be appropriately selected depending on the purpose, but it is preferable that both the front and back surfaces are 1 μm or less in order to suppress refraction and scattering of the laser beam or the optical vortex laser beam and not to reduce the energy imparted to the matrix. In addition, if the surface roughness Ra is within the preferred range, it is advantageous in that the variation in the average thickness of the matrix attached to the sample can be suppressed and the desired amount of matrix can be attached. The surface roughness Ra can be measured in accordance with JIS B0601, for example, using a confocal laser microscope (manufactured by Keyence Corporation) or a stylus-type surface profiler (Dektak150, manufactured by Bruker AXS K.K.).

[0026] [How to make a matrix plate] The method for producing the matrix plate is not particularly limited and can be appropriately selected depending on the purpose. For example, a method for producing a matrix plate includes placing a matrix layer crystallized by a powder forming device described below on a slide glass.

[0027] In the method for producing the exemplified matrix layer, first, a matrix solution is prepared by mixing a matrix in a solvent. The solvent is not particularly limited and can be appropriately selected depending on the purpose. Examples of the solvent include TFA, TFA-acetonitrile, THF, and methanol. Next, the prepared matrix solution is contained in the raw material container 13 of the powder forming apparatus 1 shown in FIGS. 1A to 1C.

[0028] Fig. 1A is a schematic diagram showing an example of an entire powder forming apparatus, Fig. 1B is a schematic diagram showing a droplet forming head in a droplet forming unit of Fig. 1A, Fig. 1C is a cross-sectional view of the droplet forming unit of Fig. 1A taken along line AA'. 1A mainly includes a droplet formation unit 10 and a drying and collecting unit 30. The droplet formation unit 10 is a liquid chamber having a liquid ejection region communicating with the outside through an ejection hole, and is arranged with a plurality of droplet ejection heads 11 which are droplet forming means for ejecting, from the ejection hole, a matrix solution in the liquid column resonance liquid chamber as droplets, where a liquid column resonance standing wave is generated under predetermined conditions. On both sides of each droplet ejection head 11, airflow passages 12 are provided through which airflow generated by airflow generating means passes so that droplets of the matrix solution ejected from the droplet ejection head 11 flow out to the drying and collecting unit 30 side. The droplet forming unit 10 also includes a raw material container 13 that contains a matrix solution 14, which is a matrix raw material, and a liquid circulation pump 15 that supplies the matrix solution 14 contained in the raw material container 13 to a liquid common supply path 17 described later in the droplet discharge head 11 through a liquid supply pipe 16, and further pressurizes the matrix solution 14 in the liquid supply pipe 16 to return it to the raw material container 13 through a liquid return pipe 22. As shown in FIG. 1B, the droplet discharge head 11 also includes a liquid common supply path 17 and a liquid column resonance liquid chamber 18. The liquid column resonance liquid chamber 18 is connected to the liquid common supply path 17 provided in one of the wall surfaces at both ends in the longitudinal direction. The liquid column resonance liquid chamber 18 also has a matrix discharge hole 19 that discharges matrix droplets 21 in one of the wall surfaces connected to the wall surfaces at both ends, and a vibration generating means 20 that is provided in the wall surface facing the matrix discharge hole 19 and generates high-frequency vibration to form a liquid column resonance standing wave. The vibration generating means 20 is connected to a high-frequency power source.

[0029] The drying and collecting unit 30 shown in FIG. 1A includes a chamber 31 and a matrix collecting section 32. In the chamber 31, a large downward air current is formed by the joining of the air current generated by the air current generating means and the downward air current 33. The matrix droplets 21 ejected from the droplet ejection head 11 of the droplet forming unit 10 are transported downward not only by gravity but also by the downward air current 33, so that the ejected matrix droplets 21 can be prevented from being decelerated by air resistance. As a result, when the matrix droplets 21 are continuously ejected, the matrix droplets 21 ejected earlier are decelerated by air resistance, and the matrix droplets 21 ejected later catch up with the matrix droplets 21 ejected earlier, so that the matrix droplets 21 are prevented from coalescing together and the crystal diameter of the matrix droplets 21 varies. As the air current generating means, either a method of pressurizing by providing a blower in the upstream portion or a method of reducing pressure by suction from the matrix collecting section 32 can be adopted. A rotating airflow generator that generates a rotating airflow that rotates around an axis parallel to the vertical direction is disposed in matrix collecting section 32. Then, the dried and crystallized matrix powder is supported on substrate 201 disposed below chamber 31.

[0030] The matrix powder thus obtained has little variation in crystal size, enabling highly reproducible analysis. In addition, since the matrix powder contains almost no solvent, as the solvent is evaporated by drying, the matrix solution is hardly applied to the sample and the biological tissue of the measurement sample is hardly destroyed by the solvent, as in the conventional method using spraying. Furthermore, since the solvent is hardly evaporated by mass spectrometry, the matrix powder can be used in medical settings and clinical trials, and is advantageous in that the analysis results can be obtained on the spot.

[0031] Similarly, as a method for forming the matrix layer, an electrostatic coating device (Micro Mist Coater, manufactured by Nagase Techno Engineering) shown in FIG. 1D can be suitably used. The electrostatic application device (micro-mist coater) has a power source 41, a syringe 42, and a coating stage 44. The electrostatic coating device (micro-mist coater) uses a phenomenon called electrospray to turn the liquid in the syringe 42 into mist 42-2 (Rayleigh breakup). More specifically, electrospray is a phenomenon in which a voltage of several thousand volts is applied to the liquid in the nozzle 42-1 to turn it into mist. The charged liquid 43 is turned into fine mist by electrostatic repulsion, and advances toward and adheres to the conductive surface 46 (laser energy absorbing material) on the substrate 45 on the coating stage 44. By using such electrostatic coating, the finely misted matrix solution or powder is attracted to the substrate by electrostatic force, so scattering of the matrix solution or powder can be minimized and the utilization rate of the matrix solution can be significantly improved. In addition, the mist hits the substrate softly and does not bounce back after impact, making it possible to form a more uniform matrix layer. Furthermore, the matrix layer can be formed by vacuum deposition or sputtering, which can form a uniform matrix layer.

[0032] The shape of the matrix arranged on the surface of the substrate is not particularly limited and can be appropriately selected depending on the purpose. For example, a single layer, multiple layers, dots, etc. can be mentioned. Among these, when the matrix absorbs the laser wavelength, it is preferable that the matrix is ​​at least one of a single layer and a dot shape. When the matrix is ​​in the shape of at least one of a single layer and a dot shape, it is advantageous in that the matrix can be easily disposed on the surface of the sample. In the present invention, in order to prevent the laser that propels the matrix from damaging the sample, a matrix layer is formed on a laser energy absorbing layer that absorbs laser light of a wavelength that is not absorbed by the matrix layer.

[0033] [Method of irradiating a matrix plate with a laser beam (laser beam irradiation means)] The method of irradiating the matrix plate with a laser beam (laser beam irradiation means) is not particularly limited and can be appropriately selected depending on the purpose. For example, a method performed by the following laser beam irradiation means is preferred.

[0034] -Laser beam irradiation means- Examples of the laser beam irradiation means include means for irradiating an optical vortex laser beam, a uniform heat irradiation laser beam, a Gaussian laser beam, and the like.

[0035] FIG. 2 is a schematic diagram showing an example of a laser beam irradiation means that can be used in the method of the present invention for preparing an measurement sample for MALDI mass spectrometry. In FIG. 2, the laser beam irradiation means 140 irradiates the matrix 202 and the laser energy absorbing material supported on the substrate 201 with a laser beam L, causing the matrix 202 and the laser energy absorbing material to fly by the energy of the laser beam L and adhere to a sample slice 301 on a slide glass 302.

[0036] The laser beam irradiation means 140 includes, for example, a laser light source 141, a beam diameter changing means 142, a beam wavelength changing means 143, an energy adjustment filter 144, and a beam scanning means 145. The matrix plate 200 is made of a base material 201, a matrix 202, and a laser energy absorbing material, and the measurement sample 300 is made of a sample slice 301 and a slide glass 302.

[0037] The laser light source 141 generates a pulsed laser beam L and irradiates the beam diameter changing means 142 with the laser beam L. Examples of the laser light source 141 include a solid-state laser, a gas laser, and a semiconductor laser.

[0038] The beam diameter changing means 142 is disposed downstream of the laser light source 141 in the optical path of the laser beam L generated by the laser light source 141, and changes the diameter of the laser beam L. The beam diameter changing means 142 is, for example, a condenser lens. The beam diameter of the laser beam L is not particularly limited and can be appropriately selected depending on the purpose, but is preferably 20 μm or more and 300 μm or less. If the beam diameter of the laser beam L is within the preferred range, it is advantageous in that it is possible to arrange a matrix corresponding to the beam diameter of the existing MALDI.

[0039] The beam wavelength changing means 143 is disposed downstream of the beam diameter changing means 142 in the optical path of the laser beam L, and changes the wavelength of the laser beam L to a wavelength that can be absorbed by the matrix 202 and the laser energy absorbing material. In the present invention, the wavelength of the laser beam L is not absorbed by the matrix 202 but is absorbed by the laser energy absorbing layer.

[0040] As a beam wavelength changing means, for example, when an optical vortex laser beam described below is used, the total rotation moment J expressed by the following formula (1) is increased by giving circular polarization to the laser beam. L,S But, |J L,S As long as the condition |≧0 is satisfied, there is no particular limitation, and it can be appropriately selected according to the purpose. Examples of the beam wavelength changing means include a quarter-wave plate. In the case of a quarter-wave plate, the optical axis may be set at an angle other than +45° or -45° to give elliptical circular polarization (elliptical polarization) to the optical vortex laser beam described below, but it is preferable to set the optical axis at +45° or -45° to give a perfect circular circular polarization to the laser beam and satisfy the above condition. This allows the image forming apparatus to stably fly the light absorbing material and increase the effect of attaching it to the object in a shape that suppresses scattering.

[0041]

number

number

[0042] L is a parameter determined by the number of turns of the helical wavefront in the wave plate. S is a parameter determined by the direction of the circularly polarized light in the wave plate. Both L and S are integers. The signs of L and S indicate the direction of the helix (clockwise, counterclockwise), respectively. If the total rotational moment in the laser beam is J, it can be expressed as J=L+S. The beam wavelength changing means 143 may be, for example, a KTP crystal, a BBO crystal, an LBO crystal, or a CLBO crystal.

[0043] The energy adjusting filter 144 is disposed downstream of the beam wavelength changing means 143 in the optical path of the laser beam L, and when the laser beam L is transmitted, it changes the energy of the laser beam L to an appropriate energy for flying the matrix 202. Examples of the energy adjusting filter 144 include an ND filter and a glass plate.

[0044] The beam scanning means 145 is disposed downstream of the energy adjusting filter 144 in the optical path of the laser beam L, and includes a reflecting mirror 146 . The reflecting mirror 146 is movable in the scanning direction indicated by the arrow S in FIG. 2 by a reflecting mirror driving means, and reflects the laser beam L onto any desired position of the matrix 202 and the laser energy absorbing material carried by the base material 201 .

[0045] The matrix 202 and the laser energy absorbing material are irradiated with the laser beam L that has passed through the energy adjusting filter 144 , receive the energy within the diameter range of the laser beam L, fly, and adhere to the sample slice 301 .

[0046] The laser beam L is not particularly limited and can be appropriately selected according to the purpose, and examples thereof include an optical vortex laser beam, a uniform heat irradiation laser beam, a Gaussian laser beam, etc. Among these, an optical vortex laser beam is preferred because the laser characteristics can improve the robustness of the conditions for transferring the matrix to the sample without scattering it. When the laser beam L is an optical vortex laser beam, it is advantageous in that the flying matrix 202 and the laser energy absorption layer are adhered to the sample slice 301 while being suppressed from scattering to the surroundings by the gyro effect imparted by the optical vortex laser beam. An optical vortex laser beam can be obtained by converting a Gaussian laser beam. For example, a diffractive optical element, a multimode fiber, a liquid crystal phase modulator, etc. can be used to convert the Gaussian laser beam into an optical vortex laser beam.

[0047] --Optical vortex laser beam-- Here, an optical vortex laser beam will be described. A typical laser beam has a uniform phase, and therefore has a planar equiphase surface (wavefront) as shown in FIG. 10A. The direction of the Poynting vector of the laser beam is perpendicular to the planar equiphase surface, and therefore the direction is the same as the direction of the laser beam irradiation. Therefore, when the laser beam is irradiated onto a light absorbing material, a force acts on the light absorbing material in the irradiation direction. However, since the light intensity distribution on the cross section of the laser beam is a normal distribution (Gaussian distribution) with the strongest intensity at the center of the beam as shown in FIG. 10B, the light absorbing material is likely to scatter. In addition, when the phase distribution is observed, it is confirmed that there is no phase difference as shown in FIG. 10C. In contrast, an optical vortex laser beam has a spiral equiphase surface as shown in FIG. 11A. Since the direction of the Poynting vector of the optical vortex laser beam is perpendicular to the spiral equiphase surface, when the optical vortex laser beam is irradiated to a light absorbing material, a force acts in the perpendicular direction. Therefore, as shown in FIG. 11B, the light intensity distribution becomes a concave donut-shaped distribution with zero at the center of the beam, and the donut-shaped energy is applied as radiation pressure to the light absorbing material irradiated with the optical vortex laser beam. Then, the light absorbing material irradiated with the optical vortex laser beam flies along the irradiation direction of the optical vortex laser beam and adheres to the object in a state where it is unlikely to scatter. In addition, when the phase distribution is observed, it is confirmed that a phase difference occurs as shown in FIG. 11C.

[0048] There are no particular limitations on the method for determining whether or not an optical vortex laser beam is present, and it can be selected appropriately depending on the purpose. For example, the method can include the aforementioned observation of the phase distribution and interferometry, with interferometry being the most common. The interference measurement can be observed using a laser beam profiler (such as a laser beam profiler manufactured by Spiricon or a laser beam profiler manufactured by Hamamatsu Photonics KK), and examples of the results of the interference measurement are shown in FIGS. 11D and 11E. FIG. 11D is an explanatory diagram showing an example of the results of interferometry on an optical vortex laser beam, and FIG. 11E is an explanatory diagram showing an example of the results of interferometry on a laser beam having a point with zero light intensity at its center. When an optical vortex laser beam is subjected to interferometric measurement, it can be confirmed that the energy distribution is donut-shaped, as shown in Figure 11D, and that the laser beam has a point of zero light intensity in the center, as in Figure 9C. On the other hand, when an interferometric measurement of a typical laser beam with a point of zero light intensity at the center is performed, as shown in Figure 11E, it is similar to the interferometric measurement of the optical vortex laser beam shown in Figure 11D. However, the energy distribution in the donut-shaped part is not uniform, indicating a difference from the optical vortex laser beam.

[0049] When the laser beam L is an optical vortex laser beam, the flying matrix 202 has the advantage that it adheres to the sample slice 301 while being prevented from scattering to the surrounding area by the gyro effect imparted by the optical vortex laser beam. Conversion into an optical vortex laser beam can be achieved, for example, by using a diffractive optical element, a multimode fiber, a liquid crystal phase modulator, or the like.

[0050] --Uniform heat irradiation laser beam-- Next, the uniform heating irradiation laser beam will be described below. The uniform heating irradiation laser beam is a laser beam that creates a uniform heating region at the interface between the substrate and the target material (laser energy absorbing material and matrix) that exhibits a substantially uniform temperature distribution above the melting point of the target material (laser energy absorbing material and matrix). By irradiating the interface between the substrate and the material to be flown (particularly the laser energy absorbing material) with a laser beam so as to create a region where the temperature is above the melting point of the material to be flown (laser energy absorbing material), the bonding force (intermolecular force) at the interface between the substrate and the material to be flown decreases, and the material to be flown flies as powder or small fragments.

[0051] Here, the "generation of a uniformly heated region exhibiting a substantially uniform temperature distribution above the melting point of the target material at the interface between the base material and the target material" by the uniformly heated irradiation laser beam will be described in detail with reference to the drawings. The term "uniformly heated region" refers to a region in which the temperature distribution of the flying object material is approximately uniform. The term "region in which the temperature distribution of the flying material is approximately uniform" means that within a region in which the flying material is disposed on the base material, the temperature of the flying material is uniform and approximately the same temperature. When the target material is a homogeneous material, it is important that the temperature (energy) distribution of the irradiated laser beam is approximately uniform in order to generate a "region in which the temperature distribution of the target material is approximately uniform." The approximately uniform temperature (energy) distribution of the irradiated laser beam will be explained with reference to the drawings. In the following, a laser beam with an approximately uniform temperature (energy) distribution may be referred to as a "uniformly heated laser beam."

[0052] FIG. 12A is a diagram showing an example of a simulation image in which the temperature (energy) distribution of a Gaussian laser beam, which is a commonly used laser beam, is expressed by contour lines in a cross section perpendicular to the laser beam traveling direction. As shown in FIG. 12A, the Gaussian laser beam has a temperature (energy) distribution in which the energy intensity is maximum at the center (optical axis) of the laser beam in a cross section perpendicular to the laser beam traveling direction, and the energy intensity decreases toward the edge. FIG. 13 is a diagram showing an example of the energy intensity distribution of a Gaussian laser beam (dotted line) and a uniform heat irradiation laser beam (solid line) in a cross section perpendicular to the laser beam traveling direction. As shown in FIG. 13, as in FIG. 12A, it can be seen that the energy intensity of the Gaussian laser beam (dotted line) is maximum at the center (optical axis) of the laser beam, and the energy intensity decreases toward the edge. Note that the "energy intensity distribution of the laser beam in a cross section perpendicular to the laser beam traveling direction" may be simply referred to as the "cross-sectional intensity distribution of the laser beam". Fig. 12B is a diagram showing an example of an image showing the temperature (energy) distribution of the uniform thermal irradiation laser beam. As shown in Fig. 12B, in the uniform thermal irradiation laser beam, the area having energy (black area in the figure) and the area not having energy (gray area in the figure) are clearly separated. Also, as shown in Fig. 13, the uniform thermal irradiation laser beam (solid line) does not have the maximum energy value on the optical axis like a Gaussian laser beam, but has an energy intensity distribution in which the energy intensity of the laser beam is approximately the same. Note that such a laser beam having a cross-sectional intensity distribution in which the energy intensity of the laser beam is approximately the same is sometimes called a top hat laser beam. Conventionally, it is known that a top hat laser beam is used for thin film laser patterning, but its application to the LIFT method is not known (see, for example, JP 2012-143787 A).

[0053] In the uniform heat irradiation laser beam, it is ideal that the energy intensity of the laser beam is uniform. In other words, it is ideal that the energy of the laser beam is approximately uniform (approximately constant) in a cross section perpendicular to the traveling direction of the laser beam. Here, FIG. 14A is a schematic diagram showing an example of the cross-sectional intensity distribution of the uniform thermal irradiation laser beam, and FIG. 14B is a schematic diagram showing another example of the cross-sectional intensity distribution of the uniform thermal irradiation laser beam. For example, as shown in FIG. 14A, in a cross section perpendicular to the traveling direction of the laser beam, the ideal uniform thermal irradiation laser beam appears to have the same energy intensity of the laser beam. However, in reality, the energy intensity of the laser beam is not completely constant as shown in FIG. 14A, and the value of the energy intensity of the laser beam oscillates, and an energy distribution that appears to be wavy is shown as shown in FIG. 14B. Therefore, there are three or more points where the energy intensity of the uniform thermal irradiation laser beam is the same in a cross section perpendicular to the traveling direction of the laser beam. For example, in the cross-sectional intensity distribution of the uniform thermal irradiation laser beam shown in FIG. 14B, there are six points where the energy intensity of the laser beam is the same. In contrast, in the cross-sectional intensity distribution of the ideal Gaussian laser beam shown in FIG. 13, the distribution of the energy intensity is a Gaussian distribution, so there are only a maximum of two points where the energy intensity of the laser beam is the same. Therefore, in other words, when the laser beam has three or more points where the energy intensity of the laser beam is the same in the cross-sectional intensity distribution of the laser beam, the energy distribution of the laser beam can be said to be substantially uniform. In the present invention, the uniform heating irradiation laser beam that produces the "uniform heating region" means a laser beam having three or more points where the energy intensity of the laser beam is the same in the cross-sectional intensity distribution of the laser beam.

[0054] Whether a laser beam is a uniform heat irradiation laser beam can be determined by measuring the energy distribution of the irradiated laser beam with a beam profiler and determining whether the cross-sectional intensity distribution of the laser beam has three or more points with the same laser beam energy intensity.

[0055] Next, the advantages of carrying out the LIFT method using a uniform heat irradiation laser beam will be described with reference to the drawings. 15A to 15C are schematic diagrams showing an example of the LIFT method using a conventional Gaussian laser beam, and 15D to 15F are schematic diagrams showing an example of the LIFT method using a uniform heat irradiation laser beam in the present invention. In Fig. 15A to Fig. 15F, a case will be described in which a transparent substrate 411 is used as the substrate and a solid film 421 is used as the target material. 15A is a schematic diagram showing an example of a case where a Gaussian laser beam 431 is irradiated onto a substrate 411 having a flying object material 421 arranged on at least a part of its surface, from a surface side opposite to the surface on which the flying object material 421 is arranged. As shown in FIG. 15A, when a Gaussian laser beam 431 is irradiated onto the substrate 411 from a surface side opposite to the surface on which the flying object material 421 is arranged, the Gaussian laser beam 431 is irradiated onto the flying object material 421 through the substrate 411. When the Gaussian laser beam 431 is irradiated onto the flying object material 421, the flying object material 421 is heated to a melting point or higher by the energy of the laser beam, and the bonding force (intermolecular force) at the interface between the substrate 411 and the flying object material 421 is reduced. The cross-sectional intensity distribution 432 of the Gaussian laser beam 431 has a maximum value at the center of the Gaussian laser beam 431, and the intensity gradually decreases toward the edge. Therefore, as shown in Fig. 15B, a force in the direction from the center of the Gaussian laser beam 431 toward the outside is easily generated in the flying target material 421. As a result, as shown in Fig. 15C, the flying target material 421 scatters and ends up adhering to the target 441 in pieces. Figure 15D is a schematic diagram showing an example of a substrate 411 having a flying target material 421 arranged on at least a portion of its surface, in which a uniform heat irradiation laser beam 433 is irradiated onto the substrate 411 from the surface side opposite to the surface on which the flying target material 421 is arranged. In the case of the uniform heat irradiation laser beam, the laser beam is irradiated onto the flying object material 421 through the substrate 411, the flying object material 421 is heated to the melting point or higher by the energy of the laser beam, and the bonding force at the interface between the substrate 411 and the flying object material 421 is reduced, similarly to the case of the Gaussian laser beam. However, in the present invention, the laser beam is irradiated to generate a uniform heat region on the flying object material 421. That is, as described above, the flying object material 421 is irradiated with the uniform heat irradiation laser beam 433 having a substantially uniform cross-sectional intensity distribution 434, so that a force in the same direction as the irradiation direction of the uniform heat irradiation laser beam 433 is generated in the flying object material 421, as shown in FIG. 15E. As a result, as shown in FIG. 15F, the flying object material 421 flies in the same direction as the irradiation direction of the laser beam, and the flying object material 421 can be attached to the object 441 while suppressing scattering.

[0056] In addition, as an index of the size (width) of a laser beam, "Full Width at Half Maximum (FWHM)" and "1 / e 2 There is a "width". "Full width at half maximum (FWHM)" refers to the spectral width of a laser beam at half the maximum intensity of the laser beam (eg, the spectral width at intensity A in FIG. 13). "1 / e 2 "Width" refers to an index that regards the distance between two points of intensity values ​​equivalent to 13.5% of the maximum intensity in the cross-sectional intensity distribution of the laser beam as the laser beam diameter (for example, the spectral width at the intensity of B in Figure 13). This "full width at half maximum (FWHM)" and "1 / e 2 The ratio of "FWHM" to "1 / e 2 When the laser beam is an ideal Gaussian laser beam, ho is 0.6, and when the laser beam is an ideal top hat beam, ho is 1. In the case of a Gaussian laser beam, as the energy intensity of the laser beam increases, the irradiation area at that intensity decreases. Also, the intensity of the Gaussian laser beam increases as it approaches the center. That is, the energy intensity in the irradiation area of the Gaussian laser beam becomes non-uniform. On the other hand, for a uniform heating irradiation laser beam, the top-hat beam having the maximum intensity has a ratio ho (Full Width at Half Maximum (FWHM) / (1 / e 2 width)) that theoretically becomes "1", and the energy intensity of the laser beam in the irradiation area (1 / e 2 width) is uniform. 2 By the inventors, the ratio ho (FWHM / (1 / e 2 width)) of the Full Width at Half Maximum (FWHM) of the energy intensity distribution of the laser beam in the cross section orthogonal to the traveling direction of the laser beam and the 1 / e 2 width is preferably irradiated onto the flying target material so as to satisfy 0.6 < ho < 1, and more preferably to satisfy 0.7 ≤ ho ≤ 0.9. Incidentally, ho (FWHM / (1 / e 2 width)) of the uniform heating irradiation laser beam shown in FIG. 12B above was 0.85.

[0057] In the cross section orthogonal to the traveling direction of the laser beam, the shape of the energy intensity distribution of the uniform heating irradiation laser beam with the 1 / e 2 width as the base is not particularly limited and can be appropriately selected according to the purpose. Examples include a square, a rectangle, a parallelogram, a circle, an ellipse, and the like.

[0058] The method for generating the uniform heating irradiation laser beam is not particularly limited and can be appropriately selected according to the purpose. Examples include a uniform heating irradiation laser beam conversion means and the like. ​The uniformly heated irradiation laser beam conversion means is not particularly limited as long as it can generate the uniformly heated region described above, and examples thereof include aspherical lenses, phase masks such as diffractive optical elements (DOEs), phase conversion means such as liquid crystal phase conversion elements (SLMs), etc. These may be used alone or in combination of two or more.

[0059] The method using an aspheric lens is a method for geometrically converting a Gaussian laser beam into a uniformly heated irradiation laser beam. Fig. 16A is a schematic diagram showing an example of adjusting the uniform thermal irradiation laser beam by a geometrical method using an aspherical lens. As shown in Fig. 16A, by passing a Gaussian laser beam through an aspherical lens 511, a laser beam having a cross-sectional intensity distribution 432 of a Gaussian laser beam is expanded at a central portion 521 of the laser beam by a concave lens effect, and a peripheral portion 522 of the laser beam is converged by a convex lens effect, so that a laser beam having a cross-sectional intensity distribution 434 of the uniform thermal irradiation laser beam can be adjusted on an irradiation surface (substrate) 512.

[0060] The method using a phase mask such as a diffractive optical element (DOE) is a method for converting a Gaussian laser beam into a uniformly heated irradiation laser beam using wave optics. Fig. 16B is a schematic diagram showing an example of adjusting a uniformly heated irradiation laser beam by a wave optics technique using a DOE. As shown in Fig. 16B, by passing a Gaussian laser beam through a DOE 531, the central part of the laser beam is given a phase distribution that produces a concave lens effect, and the peripheral part of the laser beam is given a phase distribution that produces a convex lens effect, and the wavefront is controlled to produce a uniformly heated irradiation laser beam. In Fig. 16B, 541 denotes a condenser lens, and 551 denotes a substrate.

[0061] A method using a phase conversion means such as a liquid crystal phase shifter (SLM) can convert the phase distribution of a laser beam (temporal spatial light modulation), so that the superimposed wavefront can be changed over time.

[0062] As an example other than the above, a combination of a reflective liquid crystal phase conversion element and a prism can also be used. FIG. 16C is a schematic diagram showing an example of adjusting the uniform heating irradiation laser beam by a combination of a reflective liquid crystal phase conversion element 561 and a prism 562. In FIG.

[0063] The laser beam is converted into a uniform heat irradiation laser beam by the laser beam conversion optical system and the fθ lens, and the uniform heat irradiation laser beam is irradiated onto the target material. The size of the laser beam irradiated onto the substrate (diameter, 1 / e 2 The width is preferably from 20 μm to 200 μm, and more preferably from 30 μm to 150 μm. By setting the size of the laser beam to be between 20 μm and 200 μm, it becomes possible to maintain quality by laser scanning, and to realize high-resolution two-dimensional drawing or three-dimensional printing.

[0064] The energy of the uniform heat irradiation laser beam is expressed as the fluence of the laser beam on the surface on which the target material is placed, F B (J / cm 2 ) is the fluence F of the laser beam at the surface of the substrate where the laser beam is irradiated. F (J / cm 2 ) is preferably 20% or more, and more preferably 20% or more and 80% or less. In addition, the fluence (J / cm 2 ) usually refers to the fluence on the incident side (front side fluence, F F ) and is often discussed in terms of the absorption coefficient of the material. However, the fluence on the film surface opposite the light irradiation of the light absorbing film (backside fluence, F B The inventors' investigations revealed that controlling the .DELTA..times ...

[0065] Next, an embodiment of a projectile generating device for carrying out the method of preparing a measurement sample for MALDI mass spectrometry of the present invention will be described with reference to the drawings. FIG. 17A is a schematic diagram showing an example of a projectile generating device for carrying out the method of preparing an measurement sample for MALDI mass spectrometry of the present invention. As shown in FIG. 17A, the flying object generating device 700 of the present invention has a laser beam 711 irradiated from a light source (not shown), a beam conversion optical system 721, and a focusing optical system 731, and is used together with a substrate 741, a flying object material 751, and a medium to be attached 761. In the flying object generating device 700, the laser beam 711 irradiated from a light source (not shown) passes through the beam conversion optical system 721 and an fθ lens as the focusing optical system 731 to convert it into a desired beam profile, and is irradiated to the flying object material 751 through the substrate 741. The flying object material 751 irradiated with the laser beam 711 flies toward the medium to be attached 761 arranged so as to face the flying object material 751 arranged on the substrate 741 through a gap 771, and is attached (flying object material 752 after attachment). The gap 771 between the flying object material 751 and the attachment medium 761 is adjusted by a gap holding means (not shown), and the position of the attachment medium 761 in the planar direction can be adjusted by a position adjusting means (not shown). FIG. 17B is a schematic diagram showing another example of the flying object generating device of the present invention. As shown in FIG. 17B, the figure is an axisymmetric model for convenience. As shown in FIG. 17B, the flying object generating device has a light source 811, a beam conversion optical system 821, an (XY) galvano scanner 831 which is a scanning optical system, and a condenser lens 841 which is a condensing optical system, and is capable of placing a transparent body (base material) 851 on which a flying object material 853 and a laser energy absorbing material (assist film) 852 are arranged on at least a part of the surface on a sample stage 881. Also, a gap (gap) holding member 871 for providing a gap between the transparent body (base material) 851 and the object to be attached (acceptor substrate) 861 is provided. The flying object generating device converts a Gaussian laser beam 812 irradiated from the light source 811 into a uniform heat irradiation laser beam 813 in the beam conversion optical system 821. 17B, ​​a flying object flying means having a light source 811, a beam conversion optical system 821, a galvano scanner 831 as a scanning optical system, and a condenser lens 841 irradiates a transparent body (substrate) 851 with a laser beam 813 from a surface side opposite to the surface on which the flying object material 853 is arranged, thereby flying the flying object material 853 in the irradiation direction of the laser beam 813. Then, in the example of the flying object generating device shown in FIG. 17B, the flying object material 853 (flying object) that is flown adheres to a target object (target) 861.

[0066] (Substrate for preparing measurement samples for MALDI mass spectrometry) The substrate for preparing a measurement sample for MALDI mass spectrometry of the present invention has, on a substrate, a laser energy absorbing material capable of absorbing the energy of a laser beam having a wavelength of 400 nm or more, and a matrix, in that order, and further has other materials as necessary. The substrate for preparing a sample for measurement by MALDI mass spectrometry of the present invention is the same as the matrix plate in the method for preparing a sample for measurement by MALDI mass spectrometry of the present invention.

[0067] (MALDI mass spectrometry measurement sample) The measurement sample for MALDI mass spectrometry is not particularly limited, and can be appropriately selected according to the purpose, as long as it has a sample to be subjected to MALDI mass spectrometry and one or more matrices arranged at predetermined positions on the sample. When performing MALDI mass spectrometry, the measurement sample for MALDI mass spectrometry needs to be placed on a conductive substrate.

[0068] As a measurement sample for MALDI mass spectrometry, a matrix can be ejected from a substrate multiple times to a predetermined position of a sample to be subjected to MALDI mass spectrometry. If the matrix can be ejected from a substrate multiple times to be ejected, this is advantageous in that the amount of the matrix can be adjusted.

[0069] <Sample> The sample to be subjected to MALDI mass spectrometry is not particularly limited as long as it can be analyzed by MALDI mass spectrometry, and can be appropriately selected depending on the purpose. Examples of the sample include frozen brain tissue, whole animal sections, seeds, and printed images.

[0070] (MALDI mass spectrometry method) The MALDI mass spectrometry method of the present invention is not particularly limited, so long as MALDI mass spectrometry is carried out using the measurement sample for MALDI mass spectrometry of the present invention, and can be appropriately selected depending on the purpose. MALDI mass spectrometry can be performed, for example, by MALDI-TOF-MS (manufactured by Bruker Daltonics).

[0071] (Sample preparation program for MALDI mass spectrometry) The measurement sample preparation program for MALDI mass spectrometry of the present invention causes a computer to execute a process of irradiating a laser beam onto the surface of a substrate having a matrix used in preparing a measurement sample for MALDI mass spectrometry arranged on its surface, on the side opposite to the side on which the matrix is ​​arranged, thereby causing the matrix to fly from the substrate and be arranged at a predetermined position on the sample to be subjected to MALDI mass spectrometry, based on positional information of the sample to be subjected to MALDI mass spectrometry.

[0072] The program for preparing a measurement sample for MALDI mass spectrometry of the present invention is suitably executed for carrying out the method for preparing a measurement sample for MALDI mass spectrometry of the present invention. In other words, the MALDI mass spectrometry measurement sample preparation program of the present invention can execute the MALDI mass spectrometry measurement sample preparation method of the present invention by using a computer or the like as a hardware resource. Furthermore, the MALDI mass spectrometry measurement sample preparation program of the present invention may be executed by at least one of one or a plurality of computers and servers.

[0073] Processing using the measurement sample preparation program for MALDI mass spectrometry of the present invention is performed with multiple matrix plates, each with a different type of matrix arranged thereon, pre-installed at predetermined positions and an ITO-coated slide glass carrying a measurement sample fixed in place.

[0074] The processing according to the program for preparing a measurement sample for MALDI mass spectrometry of the present invention can be executed by, for example, an apparatus for preparing a measurement sample for MALDI mass spectrometry as shown in FIG. 3A and FIG. 3B.

[0075] FIG. 3A is a block diagram showing an example of hardware of a measurement sample preparation device for MALDI mass spectrometry. 3A, this measurement sample preparation device 100 for MALDI mass spectrometry has a mouse 110, a CPU 120, a display 130, a laser beam irradiation means 140, a plate replacement mechanism 150, and a storage means 160. The CPU 120 is connected to each section.

[0076] The mouse 110 receives irradiation data from a user, which corresponds information on the "type of matrix" and the "position of the measurement sample to be irradiated with the laser beam" through an input unit 110a described later. The mouse 110 also receives other inputs to the measurement sample preparation device 100 for MALDI mass spectrometry.

[0077] The CPU 120 is a type of processor, and is a processing device that performs various controls and calculations. The CPU 120 realizes various functions by executing firmware stored in the storage unit 160. The CPU 120 corresponds to a control unit 120a described later.

[0078] The display 130 displays a screen for accepting various instructions via an output unit 130a, which will be described later.

[0079] The laser beam irradiation means 140 is, for example, the same as the laser beam irradiation means shown in FIG. 2, and can irradiate a laser beam to a predetermined position on the matrix plate by an output section 130a described later.

[0080] The plate exchanging mechanism 150 is a mechanism for exchanging matrix plates on which various matrices stored in the apparatus are arranged, by a plate exchanging section 150a described later.

[0081] The storage means 160 stores various programs for operating the measurement sample preparation device 100 for MALDI mass spectrometry.

[0082] FIG. 3B is a block diagram showing an example of the functions of the measurement sample preparation device for MALDI mass spectrometry. 3B, the MALDI mass spectrometry measurement sample preparation device 100 includes an input unit 110a, a control unit 120a, an output unit 130a, an irradiation unit 140a, a plate replacement unit 150a, and a storage unit 160a. The control unit 120a is connected to each unit.

[0083] The input unit 110a receives, from the user via the mouse 110, irradiation data that associates information on the "type of matrix" with the "position on the measurement sample to be irradiated with the laser beam" in accordance with instructions from the control unit 120a. The irradiation data may be received, for example, by inputting the type of matrix and the irradiation position on an image of a measurement sample placed on an ITO-coated slide glass. The input unit 110a also accepts other inputs from the user.

[0084] The control unit 120a stores the irradiation data received by the input unit 110a in the storage unit 160a. The control unit 120a also controls the operation of the entire measurement sample preparation apparatus 100 for MALDI mass spectrometry.

[0085] The output unit 130a displays a screen for accepting various instructions on the display 130 in accordance with instructions from the control unit 120a.

[0086] The irradiation unit 140a operates the laser beam irradiation means 140 according to an instruction from the control unit 120a, and can irradiate the matrix plate arranged by the plate exchange unit 150a with a laser beam.

[0087] The plate exchanging unit 150a exchanges the matrix plate according to an instruction from the control unit 120a based on the irradiation data. A plurality of matrix plates are stored in the device, and different types of matrix powder are arranged on the plate. The matrix plates are exchanged by the plate exchanging mechanism 150.

[0088] The storage unit 160a stores the irradiation data and various programs received by the input unit 110a in the storage means 160 in accordance with instructions from the control unit 120a.

[0089] FIG. 3C is a flow chart showing an example of the processing procedure of the measurement sample preparation program for MALDI mass spectrometry of the present invention.

[0090] In step S101, when the input unit 110a receives irradiation data, which associates information on the "type of matrix" with information on the "position on the measurement sample to be irradiated with the laser beam", from the user via the mouse 110, the process proceeds to S102.

[0091] In step S102, the control unit 120a moves the irradiation position of the laser beam irradiation means 140 based on the irradiation data, and then shifts the process to S103.

[0092] In step S103, the irradiation unit 140a causes the laser beam irradiation means 140 to eject the matrix arranged on the matrix plate, and when the matrix is ​​arranged on the sample slice, the process proceeds to S104.

[0093] In step S104, the control unit 120a judges whether or not the contents of the irradiation data are all complete. If the control unit 120a judges that the contents of the irradiation data are all complete, the control unit 120a ends this process. If the control unit 120a judges that the contents of the irradiation data are not all complete, the control unit 120a shifts the process to S105.

[0094] In step S105, the control unit 120a determines whether or not the matrix plate needs to be replaced based on the irradiation data. If the control unit 120a determines that the matrix plate needs to be replaced, the process proceeds to S106. If the control unit 120a determines that the matrix plate does not need to be replaced, the process returns to S102.

[0095] In step S106, the exchanging unit 120 exchanges the matrix plate and then returns the process to S102.

[0096] In this way, the MALDI mass spectrometry measurement sample preparation program used in the present invention causes a computer to execute a process of irradiating a laser beam onto the surface of a substrate having a matrix used in preparing a measurement sample for MALDI mass spectrometry arranged on its surface, on the side opposite to the side on which the matrix is ​​arranged, thereby causing the matrix to fly from the substrate and be arranged at a predetermined position on the sample to be subjected to MALDI mass spectrometry, based on position information of the sample to be subjected to MALDI mass spectrometry. EXAMPLES

[0097] Examples of the present invention will be described below, but the present invention is not limited to these examples. In the following, an embodiment and a comparative example will be described in which a pulsed laser beam is irradiated onto two types of matrices A and B, respectively, by the laser beam irradiation means 140 shown in FIG. 2, thereby arranging dots of the two types of matrices on one sample slice.

[0098] Example 1 [Preparation of matrix solution] <Preparation of matrix solution A> Sinapic acid (SA) serving as matrix A was dissolved in THF (manufactured by Tokyo Chemical Industry Co., Ltd.) as a solvent to prepare a matrix solution A having a solid content of 1 mass % in THF.

[0099] <Preparation of matrix solution B> Next, α-cyano-4-hydroxycinnamic acid (HCCA), which serves as matrix B, was dissolved in a solvent, THF (Tokyo Chemical Industry Co., Ltd.), to prepare a THF solution of α-cyano-4-hydroxycinnamic acid with a solid content of 1% by mass as matrix solution B.

[0100] <Preparation of matrix solution C> Next, 2,5-dihydroxybenzoic acid (DHB) serving as matrix C was dissolved in THF (Tokyo Chemical Industry Co., Ltd.) as a solvent to prepare a matrix solution C containing 2,5-dihydroxybenzoic acid in THF with a solid content of 1 mass %.

[0101] [Matrix plate preparation] <Creating matrix plate A> Gold was vacuum-deposited on one surface of a slide glass (S2441, Superfrost White, manufactured by Matsunami Glass Industry Co., Ltd.) as a substrate, so that the average thickness was 50 nm. The prepared matrix solution A was applied to the gold-deposited paper surface, and matrix A powder with an average primary particle size of 20 μm on the long side of the needle-shaped crystals was formed using the powder formation technique shown in Figures 1A to 1C, forming a powder layer of matrix A to an average thickness of 5 μm, thereby producing matrix plate A with the configuration shown in Figure 4A.

[0102] <Creating matrix plate B> Matrix plate B was produced in the same manner as matrix plate A, except that matrix solution A was changed to matrix solution B. Matrix B powder having an average primary particle size of 10 μm was formed, and a powder layer of matrix B was formed to an average thickness of 5 μm.

[0103] <Creating matrix plate C> Same as matrix plate A except that matrix solution A was replaced with matrix solution C. Similarly, matrix C powder having an average primary particle size of 15 μm was formed, and a powder layer of matrix C was formed to an average thickness of 5 μm to prepare matrix plate C.

[0104] <Creating matrix plate D> The prepared matrix solution A was applied to the surface of a slide glass (S2441, Superfrost White, manufactured by Matsunami Glass Industry Co., Ltd.) as a substrate, and using the powder formation technology shown in Figures 1A to 1C, a powder of matrix A with a primary average particle size of 20 μm was formed. A powder layer of matrix A was then formed to an average thickness of 5 μm, thereby producing matrix plate D with the configuration shown in Figure 4B.

[0105] <Creating matrix plate E> Matrix B powder with an average primary particle size of 10 μm was formed in the same manner as for matrix plate D, except that matrix solution A was changed to matrix solution B. A powder layer of matrix B was then formed to an average thickness of 5 μm, thereby producing matrix plate E having the configuration shown in Figure 4B.

[0106] <Creating matrix plate F> Matrix C powder having an average primary particle size of 15 μm was formed in the same manner as in matrix plate D, except that matrix solution A was changed to matrix solution C. A powder layer of matrix C was then formed to an average thickness of 5 μm, thereby producing matrix plate F having the configuration shown in FIG. 4B.

[0107] <Creating matrix plate G> The substrate was a slide glass (S2441, Superfrost White, Matsunami Glass Industry Co., Ltd.) on one side of which gold was vacuum-deposited to an average thickness of 50 nm. The prepared matrix solution A was applied to the substrate using the electrostatic coating technique shown in Figure 1D to form a matrix A powder having an average primary particle size of 10 μm, and a powder layer of matrix A was formed to an average thickness of 5 μm, producing matrix plate G with the configuration shown in Figure 4A.

[0108] <Creating matrix plate H> Matrix B powder having an average primary particle size of 10 μm was formed in the same manner as for matrix plate G, except that matrix solution A was changed to matrix solution B. A powder layer of matrix B was then formed to an average thickness of 5 μm, thereby producing matrix plate H having the configuration shown in FIG. 4A.

[0109] [Preparation of standard samples] First, the contents of one bottle of Peptide Calibration Standard II as a standard sample is dissolved in 125 μL of 0.1% THF solvent, and the solution is shaken and stirred for several seconds. This solution 53 was dropped at 1 μL each into the circles arranged from vertical A to vertical P and horizontal 1 to horizontal 24 of "MTP384 Targret Ground SteelBC" 51 shown in Figure 5A using a microsyringe 52 (Figure 5B), and dried to prepare a standard sample group. The same standard sample group was prepared by the same procedure, and two standard sample groups (standard sample group 1 and standard sample group 2) were prepared.

[0110] [Preparation of laser beam irradiation means] <Preparation of Laser Beam Irradiation Means A> The laser beam irradiation means used was the laser beam irradiation means 140 shown in FIG. Specifically, the laser beam source (YAG) used was a YAG laser that excites a YAG crystal to generate laser oscillation. This laser beam source was used to generate a single-pulse laser beam with a wavelength of 1,064 nm, a beam diameter of 1.25 mm×1.23 mm, a pulse width of 2 nanoseconds, and a pulse frequency of 20 Hz. The single-pulse laser beam was irradiated onto a condenser lens (manufactured by Sigma Koki Co., Ltd., YAG laser condenser lens) as a beam diameter changing member, so that the beam diameter when irradiated onto the matrix was 100 μm×100 μm. The laser beam that passed through the beam diameter changing member was irradiated onto an LBO crystal (manufactured by CESTEC Co., Ltd.) used as the beam wavelength changing element, so that the wavelength was changed from 1,064 nm to 532 nm. The laser beam was passed through an energy adjustment filter (manufactured by Sigma Koki Co., Ltd., ND filter) to adjust the laser output when irradiated onto the matrix to 50 μJ / dot.

[0111] <Preparation of Laser Beam Irradiation Means B> In the laser beam irradiation means B, the laser beam changed by the wavelength changing means in the laser beam irradiation means A was passed through a spiral phase plate (Vortex phase plate, manufactured by Luminex) to convert it into an optical vortex laser beam. Next, the optical vortex laser beam converted by the spiral phase plate was passed through a quarter-wave plate (QWP; manufactured by Kogaku Giken Co., Ltd.) arranged downstream of the spiral phase plate. At this time, the optical axes of the spiral phase plate and the quarter-wave plate were set to +45° so that the total rotation moment J expressed by formula (1) was 2. The converted optical vortex laser beam was passed through an energy adjustment filter (ND filter, manufactured by Sigma Koki Co., Ltd.) to adjust the laser output when irradiated onto the matrix to 50 μJ / dot. Other than this change, it is the same as the laser beam irradiation means A.

[0112] <Preparation of laser beam irradiation means C> The laser beam irradiation means C is the same as the laser beam irradiation means B, except that a 1,064 nm laser beam and a 532 nm laser beam are further used with an LBO crystal, and a wavelength changing means for generating a sum frequency is used to change the laser beam to a 355 nm laser beam.

[0113] <Preparation of Laser Beam Irradiation Means D> The laser beam irradiation means D used was the laser irradiation means shown in Figs. 17A and 17B as an example. The laser emitted from the Nd:YAG laser light source unit with a wavelength of 1064 nm was passed through a spatial isolator, a λ / 4 plate, and a collimating lens. The acousto-optic deflection element (AOM) controlled the frequency of the laser light source by temporally separating the zeroth-order light and the first-order light based on the ON / OFF signal from the PC and controller. The zeroth-order light was cut when passing through the mirror and lens, and only the first-order light passed through the nonlinear optical crystal (SHG element), and the nonlinear optical effect generated second harmonic waves (SHG), generating green light with a wavelength of 532 nm. Next, the fundamental wave and the second harmonic were separated by a harmonic separator HS to obtain a green monochromatic laser beam (green light). The obtained green light has its phase distribution and intensity distribution corrected by an aberration correction and vertical / horizontal variable magnification element, passes through a zoom lens, and is made to enter the laser beam conversion means shown in Figure 16A, which converts it into a uniformly heated irradiation laser beam. The light then passed through a mirror, ND, and other optical elements, was reflected by an optical deflector such as a galvanometer mirror, and was irradiated onto the matrix via a focusing lens (focal length: 100 mm), resulting in a laser output of 50 μJ / dot.

[0114] [Preparation of samples for MALDI mass spectrometry] Example 1 As shown in Fig. 6A, the matrix A powder layer (202) formed on the surface of the matrix plate A (200) was placed opposite the sample surface of the standard sample group 1, and the matrix plate A was set so that a Gaussian laser beam could be irradiated vertically from the rear surface (surface not having a matrix) of the matrix plate A by the laser beam irradiation means A. Although not shown in Fig. 6A, a laser energy absorbing material is disposed between the powder layer (202) of the matrix A and the substrate 201 in the matrix plate A (200). The gap G between the standard sample slice and the powder layer of the matrix A was set to 100 µm. 6B and 6C, matrix A powder was ejected from the rear surface of matrix plate A by laser beam irradiation means A to arrange matrix dots at sample position A-1 in a square shape with 10 dots in each direction, with a matrix dot diameter of 200 μm and a dot-to-dot distance of 10 μm. Further, dots of matrix A were formed in the same manner from A-2 to A-12 to obtain a measurement sample group A for MALDI mass spectrometry.

[0115] Example 2 Similarly to the MALDI mass spectrometry measurement sample group A, the matrix plate A was changed to the matrix plate B, and matrix dots B-1 to B-12 were formed to obtain the MALDI mass spectrometry measurement sample group B.

[0116] Example 3 Similarly to the MALDI mass spectrometry measurement sample group A, the matrix plate A was replaced with matrix plate C, and matrix dots were formed on C-1 to C-12 to obtain the MALDI mass spectrometry measurement sample group C.

[0117] Example 4 As shown in Figure 6A, the powder layer of matrix A formed on the surface of matrix plate A was placed opposite the sample surface of standard sample group 1, and the matrix plate was set up so that an optical vortex laser beam could be irradiated vertically from the back surface (surface not having the matrix) of matrix plate A by laser beam irradiation means B. The gap between the standard sample slice and the powder layer of matrix A was set to 100 μm. 6B and 6C, matrix A powder was ejected from the rear surface (surface not having the matrix) of matrix plate A by laser beam irradiation means B, and arranged in a square shape of 10 dots vertically and horizontally at sample position D-1, with a matrix dot diameter of 200 μm and a dot-to-dot distance of 10 μm. Further, dots of matrix A were formed in the same manner from D-2 to D-12, and a measurement sample group D for MALDI mass spectrometry was obtained.

[0118] Example 5 Similarly to MALDI mass spectrometry measurement sample group D, matrix plate A was changed to matrix plate B, and matrix dots were formed in E-1 to E-12, thereby obtaining MALDI mass spectrometry measurement sample group E.

[0119] Example 6 Similarly to MALDI mass spectrometry measurement sample group D, matrix plate A was replaced with matrix plate C, and matrix dots were formed in F-1 to F-12 to obtain MALDI mass spectrometry measurement sample group F.

[0120] Example 7 Similarly to MALDI mass spectrometry measurement sample group D, matrix plate A was replaced with matrix plate G, and matrix dots were formed on G-1 to G-12 to obtain MALDI mass spectrometry measurement sample group G.

[0121] Example 8 Similarly to the MALDI mass spectrometry measurement sample group D, the matrix plate A was replaced with the matrix plate H, and matrix dots were formed on H-1 to H-12, thereby obtaining the MALDI mass spectrometry measurement sample group H.

[0122] Example 9 As shown in Fig. 6A, the powder layer of matrix A formed on the surface of matrix plate A was placed opposite the standard sample on standard sample group 2, and was set up so that the back surface (surface not having the matrix) of matrix plate A could be irradiated vertically with a uniform heat irradiation laser beam by laser beam irradiation means D. The gap between the standard sample slice and the powder layer of matrix A was set to 100 µm. 6B and 6C, matrix A powder was ejected from the rear surface (surface not having the matrix) of matrix plate A by laser beam irradiation means D to arrange matrix dots at sample position A-1 in a square shape with 10 dots vertically and horizontally, with a matrix dot diameter of 200 μm and a dot-to-dot distance of 10 μm. Further, dots of matrix A were formed in the same manner from A-2 to A-12, and a measurement sample group Q for MALDI mass spectrometry was obtained.

[0123] Example 10 Similarly to the MALDI mass spectrometry measurement sample group Q, the matrix plate A was changed to the matrix plate B, and matrix dots B-1 to B-12 were formed to obtain the MALDI mass spectrometry measurement sample group R.

[0124] Comparative Example 1 As shown in Figure 6A, the powder layer of matrix A formed on the surface of matrix plate D was placed opposite the sample surface of standard sample group 1, and the matrix plate was set up so that an optical vortex laser beam could be irradiated vertically from the back surface (surface not having a matrix) of matrix plate D by laser beam irradiation means B. The gap between the standard sample slice and the powder layer of matrix A was set to 100 μm. Next, as shown in Figures 6B and 6C, an attempt was made to form a matrix dot dot with a diameter of 200 μm at sample position K-1 by using laser beam irradiation means A to eject matrix A powder from matrix plate A from the back surface (the surface not having the matrix) of matrix plate D; however, matrix A did not eject from matrix plate D, and a matrix dot could not be formed at sample position K-1. However, this was designated as measurement sample group K for MALDI mass spectrometry.

[0125] Comparative Example 2 Matrix plate D was changed to matrix plate E, and an attempt was made to form a matrix dot with a diameter of 200 μm at sample position L-1 in a similar manner; however, matrix B did not fly from matrix plate E, and it was not possible to form a matrix dot at sample position L-1. However, this was designated as measurement sample group L for MALDI mass spectrometry.

[0126] Comparative Example 3 Matrix plate D was changed to matrix plate F, and an attempt was made to form a matrix dot with a diameter of 200 μm at sample position M-1 in a similar manner; however, matrix C did not fly from matrix plate F, and it was not possible to form a matrix dot at sample position M-1. However, this was designated as measurement sample group M for MALDI mass spectrometry.

[0127] Comparative Example 4 As shown in Figure 6A, the powder layer of matrix A formed on the surface of matrix plate D was placed opposite the sample surface of standard sample group 1, and the matrix plate D was set up so that an optical vortex laser beam could be irradiated vertically from the back surface (the surface not having the matrix) of the matrix plate D by laser beam irradiation means C. The gap between the standard sample slice and the powder layer of matrix A was set to 100 μm. 6B and 6C, matrix A powder was ejected from the rear surface (surface not having the matrix) of matrix plate A by laser beam irradiation means A to arrange matrix dots at sample position N-1 in a square shape with 10 dots vertically and horizontally, with a matrix dot diameter of 200 μm and a dot-to-dot distance of 10 μm. Further, dots of matrix A were formed in the same manner from N-2 to N-12, and a measurement sample group N for MALDI mass spectrometry was obtained.

[0128] Comparative Example 5 Similarly to the MALDI mass spectrometry measurement sample group N, the matrix plate D was changed to the matrix plate E and matrix dots were formed on O-1 to O-12 to obtain the MALDI mass spectrometry measurement sample group O.

[0129] Comparative Example 6 Similarly to the MALDI mass spectrometry measurement sample group N, matrix plate D was replaced with matrix plate F, and matrix dots were formed on P-1 to P-12 to obtain a MALDI mass spectrometry measurement sample group P.

[0130] Next, the presence or absence of matrix scattering and the detection sensitivity of MALDI mass spectrometry were evaluated as follows.

[0131] [Matrix flight comparison using lasers] The matrix flying by the laser beam irradiation means A and the laser beam irradiation means B of the present invention was compared. In order to make the matrix fly, a dye plate was used in which the matrix layer was replaced with the red organic dye Acid Red 151, which is an organic low molecular weight substance that can be visualized and has crystallinity like the matrix of the present invention, instead of the colorless and transparent matrix that cannot be visualized. The results of comparing flight are shown in Figures 9B and 9D. When placing the matrix in a designated position, the Gaussian laser 91 of laser beam application means A requires that the gap between the standard sample slice and the matrix layer be narrowed because a wide gap between them is likely to generate dust (Figure 9B). However, by using the optical vortex laser beam 92 of laser beam application means B, dust is less likely to be generated (Figure 9D), making it possible to widen the gap between the standard sample slice and the matrix layer, further reducing the risk of damage (e.g., changes in molecular weight) when the matrix is ​​sprayed onto the sample slice. In experiments using the present invention, laser beam irradiation means B was able to form accurate dots without dust when the distance between the matrix layer and the standard sample was 200 μm, but with laser beam irradiation means A, dust occurred unless the distance was 100 μm, and it was not possible to form dots as accurate as those formed by laser beam irradiation means B.

[0132] [MALDI mass spectrometry] MALDI mass spectrometry was performed on the MALDI mass spectrometry measurement samples A to P, each containing a matrix powder, using a MALDI-TOF-MS (autoflex III LRF200-CID, manufactured by Bruker Daltonics, Inc.). Representative examples of the results are shown in Figures 7A to 7C and 8A to 8C. In Figures 7A to 7C and 8A to 8C, the horizontal axis indicates mass (m / z) and the vertical axis indicates detection intensity. [Evaluation method] The data obtained from the measurements was evaluated as follows. -Effects on samples- The detection data for 12 points of each MALDI mass spectrometry measurement sample group was scanned with a laser energy intensity of 50% per point, and the detection peak of the detection target was measured after 1500 shots. The detection peak value differs depending on the type of matrix, but components with relatively large molecular weights are more susceptible to the effects of the laser when the matrix flies, and the greater the damage, the more the molecular chains are broken and the detection peak ratio tends to decrease. The damage to the standard sample was evaluated based on the ratio (Y / X) of the detected peak intensity X of somatostatin 28 (peak indicated by the arrow in a1 in the figure), which has a relatively small molecular weight of about 759 among the representative peaks of the standard sample, to the detected peak intensity Y of bradykinin (1-7) (peak indicated by the arrow in a2 in the figure), which has a relatively large molecular weight of about 3149. [Evaluation Criteria] When matrices A and B were used, the minimum detection intensity ratio (Y / X) in the 12 points of detection data was used for evaluation based on the following evaluation criteria. Good: The minimum detection intensity ratio (Y / X) is 3 or more. Detectable: The minimum detection intensity ratio (Y / X) is 1 or more and less than 3. Undetectable: The minimum detection intensity ratio (Y / X) is less than 1. In the case of matrix C, the minimum detection intensity ratio Y / X among the 12 detection data points was used to evaluate the matrix C according to the following criteria. Note that matrix C is a matrix type that is difficult to detect high molecular weight components. Good: The minimum detection intensity ratio (Y / X) is 0.1 or more. Detectable: The minimum detectable intensity ratio (Y / X) is 0.05 or more and less than 0.1. Undetectable: The minimum detection intensity ratio (Y / X) is less than 0.05. - Detection variation (amplitude) - The average value Ave, maximum value Max, and minimum value Min of the detection intensity ratio (Y / X) for the 12 detection data points of each MALDI mass spectrometry measurement sample group were evaluated based on the following evaluation criteria. The results are shown in Table 1. The detection variation (amplitude) was evaluated using a value calculated from the following formula, {(Max-Min) / (2×Ave)}×100, described in the evaluation criteria below. [Evaluation Criteria] When matrix A and matrix B are used Excellent: {(Max-Min) / (2×Ave)}×100 is less than 10% Good: {(Max-Min) / (2×Ave)}×100 is 10% or more and less than 15% Acceptable: {(Max-Min) / (2×Ave)}×100 is 15% or more and less than 20% Not possible: {(Max-Min) / (2×Ave)}×100 is 20% or more When matrix C is used Excellent: {(Max-Min) / (2×Ave)}×100 is less than 10% Good: {(Max-Min) / (2×Ave)}×100 is between 10% and 20% Acceptable: {(Max-Min) / (2×Ave)}×100 is between 20% and 40% Not possible: {(Max-Min) / (2×Ave)}×100 is 40% or more

[0133] [Table 1]

[0134] For example, aspects of the present invention are as follows. <1> a substrate having a matrix used for preparing a measurement sample for MALDI mass spectrometry arranged on its surface, the substrate being irradiated with a laser beam on a surface opposite to the side having the matrix, thereby causing the matrix to fly from the substrate and be disposed at a predetermined position of a sample to be analyzed by MALDI mass spectrometry; the substrate having a laser energy absorbing material; The method for preparing an assay sample for MALDI mass spectrometry is characterized in that the wavelength of the laser energy of the laser beam is 400 nm or more. <2> The laser energy absorbing material and the matrix are disposed on the substrate in this order. <1> This is a method for preparing a measurement sample for MALDI mass spectrometry described in the above. <3> The transmittance of the laser beam from the laser energy absorbing material is 60% or less. <1> from <2> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <4> The laser energy absorbing material is a thin film of metal. <1> from <3> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <5> The metal is gold. <4> This is a method for preparing a measurement sample for MALDI mass spectrometry described in the above. <6> The matrix to be ejected from the substrate is of two or more types. <1> from <5> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <7> The two or more types of matrices ejected from the substrate are disposed at different predetermined positions in the sample to be subjected to the MALDI mass spectrometry. <1> from <6> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <8> The matrix is ​​placed at a predetermined position of the sample to be analyzed by MALDI mass spectrometry by flying the matrix from the substrate a plurality of times. <1> from <7> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <9> The laser beam is an optical vortex laser beam. <1> from <8> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <10> The laser beam is a uniform heat irradiation laser beam. <1> from <8> 1 is a method for preparing a measurement sample for MALDI mass spectrometry according to any one of the above. <11> The above <1> from <10> A MALDI mass spectrometry measurement sample preparation apparatus used in any one of the MALDI mass spectrometry measurement sample preparation methods, The measurement sample preparation device for MALDI mass spectrometry is characterized by having a laser beam irradiation means for irradiating a surface of the base material with a laser beam. <12> The substrate for preparing a measurement sample for MALDI mass spectrometry is characterized by having, on a substrate, a laser energy absorbing material capable of absorbing the energy of a laser beam having a wavelength of 400 nm or more, and a matrix, in that order. <13> The laser energy absorbing material is a thin film of metal. <12> The present invention relates to a substrate for preparing a measurement sample for MALDI mass spectrometry. <14> The metal is gold. <13> The present invention relates to a substrate for preparing a measurement sample for MALDI mass spectrometry.

[0135] The above <1> from <10> The method for preparing a measurement sample for MALDI mass spectrometry according to any one of the preceding claims. <11> The measurement sample preparation device for MALDI mass spectrometry described in <12> from <14> According to the substrate for preparing an measurement sample for MALDI mass spectrometry described in any one of the above, the above-mentioned conventional problems can be solved and the above-mentioned object of the present invention can be achieved. [Explanation of symbols]

[0136] 100 MALDI mass spectrometry sample preparation device 140 Laser beam irradiation means 200 Matrix Plate 201 Base material 202 Matrix 203 Laser Energy Absorbing Materials 301 Sample section (sample) L Laser beam [Prior art documents] [Patent documents]

[0137] [Patent Document 1] JP 2014-206389 A

Claims

1. A method for preparing a sample for MALDI mass spectrometry comprising: irradiating a surface of a substrate opposite to a side having a matrix used for preparing a sample for MALDI mass spectrometry with a laser beam, thereby causing the matrix to fly from the substrate and be disposed at a predetermined position of a sample to be subjected to MALDI mass spectrometry; the substrate having a laser energy absorbing material; The method for preparing an assay sample for MALDI mass spectrometry, wherein the wavelength of the laser energy of the laser beam is 400 nm or more.

2. 2. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, comprising the steps of: providing the laser energy absorbing material and the matrix in this order on the substrate.

3. 3. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the transmittance of the laser beam from the laser energy absorbing material is 60% or less.

4. 4. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the laser energy absorbing material is a thin metal film.

5. 5. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 4, wherein the metal is gold.

6. 6. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the matrix to be ejected from the substrate is of two or more types.

7. 7. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the two or more types of matrices ejected from the substrate are disposed at different predetermined positions in the sample to be analyzed by MALDI mass spectrometry.

8. 8. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the matrix is ​​jetted from the base material a plurality of times to be disposed at a predetermined position of the sample to be subjected to MALDI mass spectrometry.

9. 9. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the laser beam is an optical vortex laser beam.

10. 9. The method for preparing a measurement sample for MALDI mass spectrometry according to claim 1, wherein the laser beam is a uniformly heated irradiation laser beam.

11. 11. A MALDI mass spectrometry measurement sample preparation apparatus used in the MALDI mass spectrometry measurement sample preparation method according to claim 1 , A measurement sample preparation device for MALDI mass spectrometry, comprising a laser beam irradiation means for irradiating a surface of the base material with a laser beam.

12. A laser energy absorbing material capable of absorbing the energy of a laser beam having a wavelength of 400 nm or more and a matrix are provided on a substrate in this order; A substrate for preparing a measurement sample for MALDI mass spectrometry, characterized in that the matrix is ​​ejected from the substrate and placed at a predetermined position of a sample to be analyzed by MALDI mass spectrometry.

13. The substrate for preparing a measurement sample for MALDI mass spectrometry according to claim 12, wherein the laser energy absorbing material is a thin metal film.

14. The substrate for preparing a measurement sample for MALDI mass spectrometry according to claim 13, wherein the metal is gold.

Citation Information

Patent Citations

  • Sample adjustment method for mass spectrometric analysis, and mass spectrometry

    JP2014206389A

  • Generation of viable cell active biomaterial patterns by laser transfer

    US20020122898A1

  • Method and apparatus of uniform gas-phase molecular matrix deposition for imaging mass spectrometry

    US20100090099A1

  • Soft ablative desorption method and system

    US20100213367A1

  • Light-absorbing material jetting device, light-absorbing material jetting method, and applications using same

    WO2016136722A1