Film Capacitors
The film capacitor design addresses thermal stress issues by structuring the laminate with protruding dielectric films and connected metal layers, improving reliability in varying temperatures.
Patent Information
- Application Number
- JP2023533528
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-07-09
- Filing Date
- 2022-06-23
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2042-06-23
AI Technical Summary
Film capacitors used in low and high temperature conditions experience thermal stress concentration due to differences in thermal shrinkage rates between the film, external electrode, and exterior body, leading to reliability issues.
The film capacitor design includes a laminate structure where the dielectric films protrude more at the outer periphery than the center, with the metal layers connected to external electrodes, allowing for improved joint strength and stress relief.
This design effectively relieves thermal stress at concentrated areas, enhancing the capacitor's reliability under temperature fluctuations.
Smart Images

Figure 0007568109000006 
Figure 0007568109000007 
Figure 0007568109000008
Abstract
Description
[Technical field]
[0001] The present invention relates to a film capacitor. [Background technology]
[0002] One type of capacitor known is a film capacitor, which uses a flexible film as a dielectric film and has a first metal layer and a second metal layer sandwiched between them to face each other. A capacitor element constituting a film capacitor is manufactured, for example, by winding or laminating a film on which a first metal layer is formed and a film on which a second metal layer is formed to produce a laminate, and then forming external electrodes on both end faces of the laminate.
[0003] Such a film capacitor is used, for example, with the outer periphery of the capacitor element covered with an exterior body. For the exterior of a film capacitor, the capacitor element is generally covered with a thermosetting resin such as epoxy resin, or with a case filled with a thermosetting resin such as epoxy resin. Resins such as polyphenylene sulfide are used as the material for the case.
[0004] Patent Document 1 discloses a film capacitor comprising a metallized film formed by superimposing a first film member having a metal film formed on at least one surface thereof and a second film member, the film capacitor being formed by rolling the metallized film, and an electrode member being connected to each of both ends in the width direction of the rolled metallized film, the first film member being arranged so as to protrude in the width direction relative to the second film member, the rolled metallized film being configured so that a first protruding end and a first recessed end are repeated in the stacking direction, and the metal film is configured so as to be exposed at a portion of the first protruding end that protrudes in the width direction from the first recessed end. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2013-4916 A Summary of the Invention [Problem to be solved by the invention]
[0006] In the film capacitor described in Patent Document 1, the first protruding end and the first recessed end are configured to be repeated, which makes it easier to connect the electrode member to the metal film, and therefore it is said that the mechanical strength of the contact area between the metallized film and the electrode member can be improved without processing the first film member.
[0007] However, the film capacitor described in Patent Document 1 is not designed to be used in a manner that repeatedly changes between low and high temperature conditions, and if used in a manner that repeatedly changes between low and high temperature conditions, it will repeatedly shrink and expand. When the film capacitor repeatedly shrinks and expands in this manner, there is a difference in the thermal shrinkage rate between the film included in the laminate, the external electrode, and the exterior body, and therefore thermal stress is concentrated in the area where these three points are close to each other. Therefore, it can be said that there is room for improvement in terms of improving reliability against stress loads.
[0008] The present invention has been made to solve the above problems, and aims to provide a film capacitor that is capable of alleviating thermal stress in areas where thermal stress is concentrated, even when used in conditions that repeatedly involve low and high temperatures. [Means for solving the problem]
[0009] The film capacitor of the present invention includes a capacitor element. The capacitor element includes a laminate having a first end face and a second end face opposing each other in a width direction, a first external electrode connected to the first end face of the laminate, and a second external electrode connected to the second end face of the laminate. The laminate includes a first dielectric film, a second dielectric film, a first metal layer, and a second metal layer. The first dielectric film has a first main surface and a second main surface opposing each other in a thickness direction perpendicular to the width direction. The second dielectric film has a third main surface and a fourth main surface opposing each other in the thickness direction. In the laminate, the second main surface of the first dielectric film and the third main surface of the second dielectric film oppose each other in the thickness direction. The first metal layer is connected to the first external electrode. The second metal layer is connected to the second external electrode. In the first dielectric film and the second dielectric film adjacent to each other in the thickness direction, the first dielectric film protrudes toward the first external electrode side relative to the second dielectric film, and when a length in the width direction by which the first dielectric film protrudes from the second dielectric film is defined as a first protrusion width, at an outer periphery of the laminate in the thickness direction, the first protrusion width is larger than a central portion of the laminate in the thickness direction and increases toward the outermost periphery of the laminate in the thickness direction. In the first dielectric film and the second dielectric film adjacent to each other in the thickness direction, the second dielectric film protrudes toward the second external electrode side relative to the first dielectric film, and when a length in the width direction by which the second dielectric film protrudes from the first dielectric film is defined as a second protrusion width, at an outer periphery of the laminate in the thickness direction, the second protrusion width is larger than a central portion of the laminate in the thickness direction and increases toward the outermost periphery of the laminate in the thickness direction. Effect of the Invention
[0010] According to the present invention, it is possible to provide a film capacitor capable of alleviating thermal stress at locations where thermal stress is concentrated, even when the film capacitor is used in such a way that low and high temperature conditions are repeatedly exposed to each other. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a cross-sectional view illustrating an example of a film capacitor of the present invention. [Diagram 2] FIG. 2 is a schematic cross-sectional view showing another example of the film capacitor of the present invention. [Diagram 3] FIG. 3 is a cross-sectional schematic diagram showing an example of a capacitor element constituting the film capacitor of the present invention. [Figure 4] FIG. 4 is a schematic perspective view showing a step of producing a first metallized film in one example of a method for producing a film capacitor of the present invention. [Diagram 5] FIG. 5 is a schematic perspective view showing a step of producing a second metallized film in one example of a method for producing a film capacitor of the present invention. [Figure 6] FIG. 6 is a schematic cross-sectional view showing a process for producing a laminate in one example of a method for producing a film capacitor of the present invention. [Figure 7] FIG. 7 is a schematic diagram showing a top view of the first metallized film being unwound from the first film reel in FIG. [Figure 8] FIG. 8 is a schematic cross-sectional view showing a capacitor element constituting the film capacitor in accordance with Example 1. As shown in FIG. [Figure 9] FIG. 9 is a cross-sectional schematic diagram showing a capacitor element constituting the film capacitor in accordance with Reference Example 1. As shown in FIG. [Figure 10] FIG. 10 is a schematic cross-sectional view showing a capacitor element constituting the film capacitor in accordance with Comparative Example 1. As shown in FIG. [Figure 11] FIG. 11 is a cross-sectional schematic diagram showing a capacitor element constituting the film capacitor in accordance with Comparative Example 2. As shown in FIG. [Figure 12] FIG. 12 is a schematic cross-sectional view showing an example of a film capacitor model that is modeled and analyzed based on the film capacitor in accordance with Example 1. [Figure 13] FIG. 13 is a schematic cross-sectional view showing the film capacitor model of Example 1. [Figure 14]FIG. 14 is a cross-sectional schematic diagram showing a film capacitor model of Reference Example 1. As shown in FIG. [Figure 15] FIG. 15 is a schematic cross-sectional view showing a film capacitor model of Comparative Example 1. As shown in FIG. [Figure 16] FIG. 16 is a schematic cross-sectional view showing a film capacitor model of Comparative Example 2. As shown in FIG. [Figure 17] FIG. 17 is a schematic cross-sectional view showing a first modified example of the film capacitor model that is modeled and analyzed based on the film capacitor in accordance with Example 1. [Figure 18] FIG. 18 is a schematic cross-sectional view showing a second modified example of the film capacitor model that is modeled and analyzed based on the film capacitor in accordance with Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The film capacitor of the present invention will be described below. Note that the present invention is not limited to the following configurations, and may be modified as appropriate within the scope of the present invention. In addition, a combination of multiple individual preferred configurations described below also constitutes the present invention.
[0013] As an example of the film capacitor of the present invention, a so-called wound film capacitor in which a film including a metallized film having a metal layer provided on a main surface of a dielectric film is laminated and wound will be described below. The film capacitor of the present invention may be a so-called laminated film capacitor in which a film including a metallized film having a metal layer provided on a main surface of a dielectric film is laminated.
[0014] FIG. 1 is a cross-sectional view illustrating an example of a film capacitor of the present invention.
[0015] The film capacitor 1 shown in Fig. 1 includes a capacitor element 10. The capacitor element 10 includes a laminate 20, a first external electrode 51, and a second external electrode 52. In Fig. 1, a first lead wire 61 is electrically connected to the first external electrode 51, and a second lead wire 62 is electrically connected to the second external electrode 52.
[0016] 1 further includes an exterior resin 70, which is an example of an exterior body. The exterior resin 70 covers the outer periphery of the capacitor element 10.
[0017] FIG. 2 is a schematic cross-sectional view showing another example of the film capacitor of the present invention.
[0018] The film capacitor 2 shown in Fig. 2 includes a capacitor element 10. The capacitor element 10 includes a laminate 20, a first external electrode 51, and a second external electrode 52. In Fig. 2, a first lead wire 61 is electrically connected to the first external electrode 51, and a second lead wire 62 is electrically connected to the second external electrode 52.
[0019] 2 further includes a filling resin 71, which is an example of an exterior body, and an exterior case 72. Exterior case 72, with filling resin 71 filled between it and capacitor element 10, covers the outer periphery of capacitor element 10.
[0020] The material for the exterior resin 70 or the filling resin 71 may be, for example, a thermosetting resin such as an epoxy resin, a silicone resin, or a urethane resin. An amine hardener or an imidazole hardener may be used as a hardener for the epoxy resin. The exterior resin 70 or the filling resin 71 may be made of resin alone, or a reinforcing agent may be added to improve strength. Examples of the reinforcing agent that may be used include silica and alumina.
[0021] The exterior case 72 is made of a resin such as polyphenylene sulfide (PPS) or liquid crystal polymer (LCP).
[0022] When LCP is used as the material for the exterior case 72, for example, an LCP having p-hydroxybenzoic acid and 6-hydroxy-2-naphthoic acid groups as a skeleton can be used. Also, an LCP formed as a polycondensate using various components other than p-hydroxybenzoic acid and 6-hydroxy-2-naphthoic acid groups, such as phenol, phthalic acid, and ethylene terephthalate, can be used.
[0023] It is preferable that the exterior case 72 further contains an inorganic filler in addition to the resin. In this case, the inorganic filler contained in the exterior case 72 is preferably a material having a higher melting point than LCP, and more preferably a material having a melting point of 680° C. or higher.
[0024] The form of the inorganic filler is not particularly limited, and examples thereof include those having a longitudinal direction such as fiber or plate. Two or more of these inorganic fillers may be used in combination.
[0025] In this specification, "fibrous" means that the relationship between the longitudinal length of the filler and the cross-sectional diameter in a cross section perpendicular to the longitudinal direction is longitudinal length÷cross-sectional diameter≧5 (i.e., aspect ratio is 5:1 or more). Here, the cross-sectional diameter is the longest distance between two points on the outer periphery of the cross section. When the cross-sectional diameter varies in the longitudinal direction, the measurement is performed at the point where the cross-sectional diameter is maximum. In addition, "plate-like" means that the relationship between the cross-sectional diameter of the surface with the largest projected area and the maximum height in the direction perpendicular to this cross section is cross-sectional diameter÷height≧3.
[0026] The inorganic filler preferably has a size of at least 5 μm in diameter and 50 μm in length.
[0027] Specifically, the inorganic filler may be a material such as a fibrous glass filler or a plate-like talc or mica. In particular, the inorganic filler preferably contains a glass filler as a main component.
[0028] The exterior case 72 containing resin can be manufactured by a method such as injection molding.
[0029] The surface free energy of the outer surface of the outer case 72 is preferably 34 mN / m or more and 40 mN / m or less. In this case, an additional member can be firmly fixed to the outer surface of the outer case 72 with an adhesive force of 400 N or more using a pressure sensitive adhesive, adhesive tape, or the like. In addition, a model number, characteristics, and the like can be printed on the outer surface of the outer case 72 with ink having high surface tension.
[0030] The surface free energy of the outer surface of the outer case 72 can be changed by the composition of the outer case 72 (type of resin, filler content) or the injection molding method of the outer case 72. These are only examples, and the surface free energy of the outer surface of the outer case 72 can also be controlled by other methods.
[0031] The surface free energy of the outer surface of the outer case 72 can be measured as the wetting tension when a liquid is applied onto the outer case 72 .
[0032] The wet tension of the outer surface of the outer case 72 can be measured using, for example, Tension Checker TC-B-30 to 56 (film wet tension check pen) manufactured by Pacific Chemical Co., Ltd. Specifically, a line is drawn on the outer surface of the outer case 72 with a pen having a certain number among the above pens, and if the ink line does not turn into a water droplet and does not change for two seconds, the wet tension of the outer case 72 is judged to be the same as or higher than the number of that pen. On the other hand, if the liquid film breaks or the entire film shrinks within about two seconds, the wet tension of the outer case 72 is judged by repeating the same judgment with a check pen having the next lowest number.
[0033] The adhesive strength of the adhesive to the outer surface of the exterior case 72 can be measured, for example, by the following method. After applying 0.1 g of silicone adhesive TSE322 manufactured by Momentive Corp. to the outer surface of the exterior case 72, the side of the exterior case 72 on which the adhesive is applied is pressed against a glass epoxy board R-1705 (1.6 mm thick) manufactured by Panasonic Electric Works Co., Ltd. After thermal curing at 80°C for 2 hours, a digital force gauge manufactured by Imada Corp. is used to measure the strength at which the exterior case 72 is pressed and peeled off, thereby measuring the adhesive strength of the adhesive to the outer surface of the exterior case 72.
[0034] FIG. 3 is a cross-sectional schematic diagram showing an example of a capacitor element constituting the film capacitor of the present invention.
[0035] In this specification, the thickness direction and width direction of the capacitor element are defined as directions T and W, respectively, as shown in Fig. 3. Here, the thickness direction T and the width direction W are perpendicular to each other.
[0036] The capacitor element 10 shown in FIG. 3 includes a laminate 20, a first external electrode 51, and a second external electrode 52.
[0037] The laminate 20 has a first end surface 20a and a second end surface 20b opposed to each other in the width direction W.
[0038] Laminate 20 is a roll in which first metallized film 21 and second metallized film 22 are rolled in a stacked state in thickness direction T.
[0039] From the viewpoint of reducing the height of capacitor element 10, it is preferable that laminate 20 has a flat cross-sectional shape when viewed in a cross section perpendicular to the winding axis direction (width direction W in FIG. 3) of laminate 20. More specifically, it is preferable that laminate 20 is pressed into a flat shape such as an ellipse or oval, and that the cross-sectional shape of laminate 20 is thinner than when it is a perfect circle.
[0040] Whether or not the laminate has been pressed to have a flat cross-sectional shape can be confirmed, for example, by checking whether or not there are press marks on the laminate.
[0041] Capacitor element 10 may have a cylindrical winding axis. The winding axis is disposed on the central axis of first metallized film 21 and second metallized film 22 in a wound state, and serves as the winding axis when first metallized film 21 and second metallized film 22 are wound.
[0042] First metallized film 21 includes a first dielectric film 31 and a first metal layer 41 .
[0043] The first dielectric film 31 has a first main surface 31a and a second main surface 31b that face each other in the thickness direction T.
[0044] The first metal layer 41 is provided on the first main surface 31a of the first dielectric film 31. More specifically, the first metal layer 41 is provided on the first main surface 31a of the first dielectric film 31 so as to reach one side edge of the first dielectric film 31 in the width direction W but not to reach the other side edge of the first dielectric film 31.
[0045] Second metallized film 22 includes a second dielectric film 32 and a second metal layer 42 .
[0046] The second dielectric film 32 has a third main surface 32a and a fourth main surface 32b that face each other in the thickness direction T.
[0047] The second metal layer 42 is provided on the third main surface 32a of the second dielectric film 32. More specifically, the second metal layer 42 is provided on the third main surface 32a of the second dielectric film 32 so as to not reach one side edge of the second dielectric film 32 in the width direction W but to reach the other side edge of the second dielectric film 32.
[0048] In laminate 20, first metallized films 21 and second metallized films 22 adjacent in thickness direction T are shifted in width direction W so that an end of first metal layer 41 that reaches the side edge of first dielectric film 31 is exposed at first end face 20a of laminate 20, and an end of second metal layer 42 that reaches the side edge of second dielectric film 32 is exposed at second end face 20b of laminate 20. That is, in first metallized film 21 and second metallized film 22 adjacent in thickness direction T, first metallized film 21 protrudes toward first external electrode 51 relative to second metallized film 22. In addition, in first metallized film 21 and second metallized film 22 adjacent in thickness direction T, second metallized film 22 protrudes toward second external electrode 52 relative to first metallized film 21. In this state, the first metal layer 41 is connected to the first external electrode 51, and the second metal layer 42 is connected to the second external electrode 52. In addition, the first metal layer 41 is not connected to the second external electrode 52, and the second metal layer 42 is not connected to the first external electrode 51.
[0049] In laminate 20, first metallized film 21 and second metallized film 22 adjacent in thickness direction T are shifted in width direction W as described above, so that in first dielectric film 31 and second dielectric film 32 adjacent in thickness direction T, first dielectric film 31 protrudes toward first external electrode 51 relative to second dielectric film 32. Also, in first dielectric film 31 and second dielectric film 32 adjacent in thickness direction T, second dielectric film 32 protrudes toward second external electrode 52 relative to first dielectric film 31.
[0050] Since laminate 20 is formed by winding first metallized film 21 and second metallized film 22 in a stacked state in thickness direction T, it can be said that laminate 20 includes first dielectric film 31, first metal layer 41, second dielectric film 32, and second metal layer 42, in that order, in thickness direction T. It can also be said that laminate 20 is a wound body formed by winding first dielectric film 31, first metal layer 41, second dielectric film 32, and second metal layer 42, in that order, in thickness direction T.
[0051] In the laminate 20, the second main surface 31b of the first dielectric film 31 and the third main surface 32a of the second dielectric film 32 face each other in the thickness direction T. In addition, the first main surface 31a of the first dielectric film 31 and the fourth main surface 32b of the second dielectric film 32 face each other in the thickness direction T. In this manner, in the laminate 20, the first metallized film 21 and the second metallized film 22 are wound in a state in which they are stacked in the thickness direction T. In other words, in the laminate 20, the first metallized film 21 is on the inside of the second metallized film 22, more specifically, the first metal layer 41 is on the inside of the first dielectric film 31 and the second metal layer 42 is on the inside of the second dielectric film 32, so that the first metallized film 21 and the second metallized film 22 are wound in a state in which they are stacked in the thickness direction T. That is, in the laminate 20, the first metal layer 41 and the second metal layer 42 face each other with the first dielectric film 31 or the second dielectric film 32 sandwiched therebetween.
[0052] When the length in the width direction W that the first dielectric film 31 protrudes relative to the second dielectric film 32 is defined as the first protrusion width, as shown in Figure 3, at the outer periphery of the laminate 20 in the thickness direction T, the first protrusion width is larger than that at the central portion of the laminate 20 in the thickness direction T, and also becomes larger toward the outermost periphery of the laminate 20 in the thickness direction T.
[0053] Furthermore, when the length in the width direction W that the second dielectric film 32 protrudes from the first dielectric film 31 is defined as the second protrusion width, as shown in Figure 3, at the outer periphery of the laminate 20 in the thickness direction T, the second protrusion width is larger than that at the central portion of the laminate 20 in the thickness direction T, and also becomes larger toward the outermost periphery of the laminate 20 in the thickness direction T.
[0054] As described above, when a film capacitor is used in a manner that repeatedly changes between low-temperature and high-temperature conditions, there is a difference in the thermal shrinkage rate between the film included in the laminate, the external electrodes, and the exterior body, and therefore thermal stress concentrates at the locations where these three points are close to each other. In the film capacitor of the present invention, the protruding width of the film at the outer periphery of the laminate is larger than that at the center of the laminate, and is shaped so as to become larger toward the outermost periphery of the laminate, thereby improving the bonding shape between the film and the external electrodes. This makes it possible to alleviate thermal stress at the locations where thermal stress concentrates.
[0055] At the center of the laminate 20 in the thickness direction T, the first protruding width is preferably constant as shown in Fig. 3, but may have a height difference of 50 µm or less. Similarly, at the center of the laminate 20 in the thickness direction T, the second protruding width is preferably constant as shown in Fig. 3, but may have a height difference of 50 µm or less.
[0056] When a cross section along the thickness direction T and the width direction W is viewed, the end of the first dielectric film 31 that is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest first protruding width is defined as point X1, and the end of the first dielectric film 31 that is closest to point X1 and has the smallest first protruding width is defined as point Y1. The angle (the angle indicated by θ1 in FIG. 3, also referred to as the first pitch angle θ1) formed by a line passing between point X1 and point Y1 and a line passing between the ends of the first dielectric film 31 with the smallest first protruding width is preferably 50° or more and 80° or less. In this case, the effect of alleviating the thermal stress at point X1 is high.
[0057] When a cross section along the thickness direction T and the width direction W is viewed, the end of the first dielectric film 31 that is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest first protruding width is defined as point X1, and the end of the first dielectric film 31 that is closest to point X1 and has the smallest first protruding width is defined as point Y1. The length in the width direction W between point X1 and point Y1 (length indicated by H1 in FIG. 3, also referred to as first pitch height H1) is preferably 5% to 50% of the length in the width direction W between the outer end of the first external electrode 51 and point X1 (length indicated by T1 in FIG. 3, also referred to as first electrode thickness T1). In this case, the effect of alleviating thermal stress at point X1 is high.
[0058] The second main surface 31b of the first dielectric film 31, which is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest first protruding width, may or may not be covered by the first external electrode 51 as shown in Fig. 3. In other words, when the outer periphery of the capacitor element 10 is covered by an exterior body, the end of the first dielectric film 31, which is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest first protruding width, may or may not be in contact with the exterior body.
[0059] When a cross section along the thickness direction T and the width direction W is viewed, the end of the second dielectric film 32 that is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest second protruding width is defined as point X2, and the end of the second dielectric film 32 that is closest to point X2 and has the smallest second protruding width is defined as point Y2. The angle (the angle indicated by θ2 in FIG. 3, also referred to as the second pitch angle θ2) formed by a line passing through points X2 and Y2 and a line passing between the ends of the second dielectric films 32 with the smallest second protruding width is preferably 50° or more and 80° or less. In this case, the effect of alleviating the thermal stress at point X2 is high.
[0060] When a cross section along the thickness direction T and the width direction W is viewed, the end of the second dielectric film 32 that is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest second protruding width is defined as point X2, and the end of the second dielectric film 32 that is closest to point X2 and has the smallest second protruding width is defined as point Y2. The length in the width direction W between point X2 and point Y2 (the length indicated by H2 in FIG. 3, also referred to as the second pitch height H2) is preferably 5% to 50% of the length in the width direction W between the outer end of the second external electrode 52 and point X2 (the length indicated by T2 in FIG. 3, also referred to as the second electrode thickness T2). In this case, the effect of alleviating the thermal stress at point X2 is high.
[0061] The fourth main surface 32b of the second dielectric film 32, which is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest second protruding width, may or may not be covered by the second external electrode 52 as shown in Fig. 3. In other words, when the outer periphery of the capacitor element 10 is covered by an exterior body, the end of the second dielectric film 32, which is closest to the outermost periphery of the laminate 20 in the thickness direction T and has the largest second protruding width, may or may not be in contact with the exterior body.
[0062] It is preferable that the end of the first dielectric film 31, the end of the second dielectric film 32, the outer end of the first external electrode 51, and the outer end of the second external electrode 52 are each flat, but may have a height difference of 50 μm or less.
[0063] The lengths of the first pitch height H1, the second pitch height H2, the first electrode thickness T1, and the second electrode thickness T2, etc., can be measured, for example, by preparing a cross section shown in FIG. 3 using a rotary polisher or the like and using a microscope with a length measurement function.
[0064] The first dielectric film 31 may contain a curable resin as a main component.
[0065] In this specification, the term "major component" means the component having the highest weight percentage, and preferably means the component having a weight percentage greater than 50% by weight.
[0066] The curable resin may be a thermosetting resin or a photocurable resin.
[0067] In this specification, the term "thermosetting resin" refers to a resin that can be cured by heat, but does not limit the curing method. Therefore, the term "thermosetting resin" includes resins that can be cured by methods other than heat (for example, light, electron beam, etc.) as long as they are resins that can be cured by heat. In addition, depending on the material, a reaction may start due to the reactivity of the material itself, and resins that proceed to cure without necessarily applying heat from the outside are also considered to be thermosetting resins. The same applies to photocurable resins, and as long as they are resins that can be cured by light, they also include resins that can be cured by methods other than light (for example, heat, etc.).
[0068] The curable resin is preferably a cured product of a first organic material having a hydroxyl group (OH group) and a second organic material having an isocyanate group (NCO group). In this case, the curable resin is a cured product having a urethane bond obtained by reacting the hydroxyl group of the first organic material with the isocyanate group of the second organic material.
[0069] The presence of urethane bonds in the first dielectric film 31 can be confirmed by analysis with a Fourier transform infrared spectrophotometer (FT-IR).
[0070] When the curable resin is obtained by the above-mentioned reaction, an uncured portion of the starting material may remain in the first dielectric film 31. For example, the first dielectric film 31 may contain at least one of a hydroxyl group and an isocyanate group. In this case, the first dielectric film 31 may contain one of a hydroxyl group and an isocyanate group, or may contain both a hydroxyl group and an isocyanate group.
[0071] The presence of hydroxyl groups and / or isocyanate groups in the first dielectric film 31 can be confirmed by FT-IR analysis.
[0072] Examples of the first organic material include a phenoxy resin, a polyvinyl acetoacetal resin, and a polyvinyl butyral resin.
[0073] As the first organic material, a plurality of types of organic materials may be used in combination.
[0074] Examples of the second organic material include aromatic polyisocyanates such as diphenylmethane diisocyanate (MDI) and tolylene diisocyanate (TDI), and aliphatic polyisocyanates such as hexamethylene diisocyanate (HDI), etc. As the second organic material, at least one modified product of these polyisocyanates may be used, or a mixture of at least one of these polyisocyanates and its modified product may be used.
[0075] As the second organic material, a plurality of types of organic materials may be used in combination.
[0076] The first dielectric film 31 may contain a thermoplastic resin as a main component.
[0077] Examples of the thermoplastic resin include polypropylene, polyethersulfone, polyetherimide, and polyarylate.
[0078] The first dielectric film 31 may contain additives to impart various functions.
[0079] The additives include, for example, a leveling agent for imparting smoothness.
[0080] The additive preferably has a functional group that reacts with a hydroxyl group and / or an isocyanate group and forms a part of the crosslinked structure of the cured product. Examples of such additives include resins having at least one functional group selected from the group consisting of a hydroxyl group, an epoxy group, a silanol group, and a carboxyl group.
[0081] The second dielectric film 32 may contain a curable resin as a main component, or may contain a thermoplastic resin as a main component, similar to the first dielectric film 31. Furthermore, the second dielectric film 32 may contain an additive, similar to the first dielectric film 31.
[0082] The first dielectric film 31 and the second dielectric film 32 may have different compositions, but preferably have the same composition.
[0083] The thickness of the first dielectric film 31 and the second dielectric film 32 is preferably 1 μm or more and 10 μm or less, and more preferably 3 μm or more and 5 μm or less.
[0084] The first dielectric film 31 and the second dielectric film 32 may have different thicknesses, but preferably have the same thickness.
[0085] The thickness of the first dielectric film 31 and the second dielectric film 32 can be measured using an optical film thickness meter.
[0086] The first dielectric film 31 and the second dielectric film 32 are each preferably produced by forming a resin solution containing the above-mentioned resin material into a film and then curing it by heat treatment.
[0087] Examples of materials constituting the first metal layer 41 and the second metal layer 42 include metals such as aluminum, zinc, titanium, magnesium, tin, and nickel.
[0088] The first metal layer 41 and the second metal layer 42 may have different compositions, but preferably have the same composition.
[0089] The thickness of the first metal layer 41 and the second metal layer 42 is preferably not less than 5 nm and not more than 40 nm.
[0090] The first metal layer 41 and the second metal layer 42 may have different thicknesses, but preferably have the same thickness.
[0091] The thickness of first metal layer 41 can be measured by observing a cut surface in the thickness direction of first metallized film 21 with a transmission electron microscope (TEM). The thickness of second metal layer 42 can be measured in the same manner as the thickness of first metal layer 41.
[0092] The first metal layer 41 and the second metal layer 42 are preferably formed by vapor deposition of a metal, such as those described above, onto the major surfaces of the first dielectric film 31 and the second dielectric film 32, respectively.
[0093] A fuse portion may be provided in the first metal layer 41. The fuse portion provided in the first metal layer 41 is a portion that connects a divided electrode portion in which a portion of the first metal layer 41 that faces the second metal layer 42 is divided into multiple portions, and an electrode portion that is a portion that does not face the second metal layer 42. Examples of the electrode pattern of the first metal layer 41 provided with the fuse portion include the electrode patterns disclosed in JP-A-2004-363431 and JP-A-5-251266.
[0094] Similar to the first metal layer 41, the second metal layer 42 may also be provided with a fuse portion.
[0095] The first external electrode 51 is connected to the first end surface 20a of the laminate 20. More specifically, the first external electrode 51 is connected to the first metal layer 41 by contacting an end of the first metal layer 41 exposed at the first end surface 20a of the laminate 20. On the other hand, the first external electrode 51 is not connected to the second metal layer 42.
[0096] The second external electrode 52 is connected to the second end surface 20b of the laminate 20. More specifically, the second external electrode 52 is connected to the second metal layer 42 by contacting an end of the second metal layer 42 exposed at the second end surface 20b of the laminate 20. On the other hand, the second external electrode 52 is not connected to the first metal layer 41.
[0097] Examples of materials for the first external electrode 51 and the second external electrode 52 include metals such as zinc, aluminum, tin, and zinc-aluminum alloys.
[0098] The first external electrode 51 and the second external electrode 52 may have different compositions, but preferably have the same composition.
[0099] The first external electrode 51 and the second external electrode 52 are preferably formed on the first end face 20a and the second end face 20b of the laminate 20 by thermal spraying a metal such as those described above.
[0100] Capacitor element 10 is manufactured, for example, by the following method.
[0101] <Metallized film manufacturing process> Fig. 4 is a schematic perspective view showing a step of producing a first metallized film in one example of a method for producing a film capacitor of the present invention. Fig. 5 is a schematic perspective view showing a step of producing a second metallized film in one example of a method for producing a film capacitor of the present invention.
[0102] First, for example, a resin solution is prepared by mixing the above-mentioned first organic material, second organic material, additives, etc. Then, the obtained resin solution is formed into a film and then cured by heat treatment to prepare a first dielectric film 31 and a second dielectric film 32 as shown in Figs.
[0103] 4, a metal such as aluminum, zinc, titanium, magnesium, tin, or nickel is vapor-deposited on first main surface 31a of first dielectric film 31 to form first metal layer 41, thereby producing first metallized film 21. At this time, first metal layer 41 is formed so as to reach one side edge of first dielectric film 31 but not to reach the other side edge of first dielectric film 31 in the width direction.
[0104] 5, a metal such as aluminum, zinc, titanium, magnesium, tin, or nickel is vapor-deposited on third main surface 32a of second dielectric film 32 to form second metal layer 42, thereby producing second metallized film 22. In this case, second metal layer 42 is formed so as to not reach one side edge of second dielectric film 32 in the width direction, but to reach the other side edge of second dielectric film 32.
[0105] <Laminate manufacturing process> FIG. 6 is a schematic cross-sectional view showing a process for producing a laminate in one example of a method for producing a film capacitor of the present invention.
[0106] First, as shown in FIG. 6, a first film reel 101 having a first metallized film 21 wound around a first reel shaft 111, and a second film reel 102 having a second metallized film 22 wound around a second reel shaft 112 are prepared.
[0107] Next, first metallized film 21 is unwound from first film reel 101, and second metallized film 22 is unwound from second film reel 102. At this time, first metallized film 21 and second metallized film 22 are unwound so that second main surface 31b of first dielectric film 31 and third main surface 32a of second dielectric film 32 face each other.
[0108] Then, first metallized film 21 and second metallized film 22 that have been unwound are wound around winding shaft 200 in an overlapping state with a shift in the width direction.
[0109] FIG. 7 is a schematic diagram showing a top view of the first metallized film being unwound from the first film reel in FIG.
[0110] 7, when first metallized film 21 is unwound, first reel shaft 111 can swing in a width direction (direction indicated by a double arrow) perpendicular to the unwinding direction. As first reel shaft 111 swings in the width direction, first metallized film 21 moves in the same width direction while being unwound.
[0111] Similarly, when second metallized film 22 is unwound, second reel shaft 112 can swing in the width direction perpendicular to the unwinding direction, whereby second metallized film 22 is unwound while moving in the same width direction.
[0112] Therefore, when swinging the first reel shaft 111 and the second reel shaft 112, the first protruding width and the second protruding width can be adjusted by adjusting the swing conditions such as the swing timing and the swing distance. As a result, the laminate 20 having the structure shown in FIG. 3 can be produced in a state where it is wound around the winding shaft 200.
[0113] Moreover, the first protruding width and the second protruding width can also be adjusted by adjusting the winding speed of the winding shaft 200 in combination with the swing conditions of the first reel shaft 111 and the second reel shaft 112.
[0114] Instead of oscillating first reel shaft 111 and second reel shaft 112 in the width direction, laminate 20 having the structure shown in FIG. 3 can be produced in a wound state around winding shaft 200 by oscillating winding shaft 200 in the width direction or by oscillating the running rollers that run first metalized film 21 and second metalized film 22 in the width direction.
[0115] Thereafter, if necessary, the obtained laminate 20 may be sandwiched from a direction perpendicular to the width direction and pressed into an elliptical cylindrical shape.
[0116] <External electrode formation process> A metal such as zinc, aluminum, tin, or a zinc-aluminum alloy is sprayed onto the first end surface 20a of the laminate 20 to form a first external electrode 51 shown in FIG. 3 so as to be connected to the first metal layer 41.
[0117] In addition, a metal such as zinc, aluminum, tin, or a zinc-aluminum alloy is sprayed onto the second end surface 20b of the laminate 20 to form the second external electrode 52 shown in FIG. 3 so as to be connected to the second metal layer 42.
[0118] In this manner, capacitor element 10 shown in FIG. 3 is manufactured.
[0119] Thereafter, if necessary, a conductor terminal such as a lead wire may be connected to each of the obtained first external electrode 51 and second external electrode 52, and the outer periphery of capacitor element 10 may then be covered with an exterior body.
[0120] Through the above steps, the film capacitor 1 shown in FIG. 1 or the film capacitor 2 shown in FIG. 2 is manufactured. EXAMPLES
[0121] EXAMPLES Hereinafter, examples of the film capacitor of the present invention will be described more specifically. However, the present invention is not limited to these examples.
[0122] Fig. 8 is a cross-sectional view showing a capacitor element constituting the film capacitor according to Example 1. Fig. 9 is a cross-sectional view showing a capacitor element constituting the film capacitor according to Reference Example 1. Fig. 10 is a cross-sectional view showing a capacitor element constituting the film capacitor according to Comparative Example 1. Fig. 11 is a cross-sectional view showing a capacitor element constituting the film capacitor according to Comparative Example 2.
[0123] In Example 1, Reference Example 1, Comparative Example 1, and Comparative Example 2, a film capacitor model obtained by modeling a film capacitor was used as an analysis target, and stress analysis was performed by FEM (finite element method).
[0124] Fig. 12 is a schematic cross-sectional view showing an example of a film capacitor model that is an analysis target obtained by modeling the film capacitor according to Example 1. Fig. 13 is a schematic cross-sectional view showing the film capacitor model of Example 1.
[0125] As shown in Fig. 12, the width and thickness of film part A and external electrode part C were 30 mm and 5 mm, respectively, and the entire structure was covered with a 1 mm-thick exterior part B. The point where film part A, exterior part B, and external electrode part C contact each other was designated as point X1, and the point closest to point X1 and lowest on film part A was designated as point Y1.
[0126] In FIG. 12, the first pitch angle θ1 is 71°, and the first pitch height H1 is 1.5 mm (the ratio of the first pitch height H1 to the first electrode thickness T1 is 30%).
[0127] Fig. 14 is a cross-sectional view showing a film capacitor model of Reference Example 1. Fig. 15 is a cross-sectional view showing a film capacitor model of Comparative Example 1. Fig. 16 is a cross-sectional view showing a film capacitor model of Comparative Example 2.
[0128] In the film capacitor models of Example 1, Reference Example 1, Comparative Example 1, and Comparative Example 2, the film part A is a thermosetting resin film (linear expansion coefficient: 60×10 -6 / ℃), and exterior B is epoxy resin (linear expansion coefficient: 27×10 -6 / ℃), and external electrode C is an Al-Zn electrode (linear expansion coefficient: 30.2×10 -6 The properties of the thermosetting resin film, the epoxy resin, and the Al-Zn electrodes are shown in Table 1.
[0129] [Table 1]
[0130] The maximum thermal stress applied to the X1 point was confirmed for the film capacitor models of Example 1, Reference Example 1, Comparative Example 1, and Comparative Example 2 when the ambient temperature was changed from 25°C to 125°C. Furthermore, the maximum thermal stress applied to the X2 point on the opposite side to the X1 point was confirmed. The results are shown in Table 2.
[0131] [Table 2]
[0132] As can be seen from Table 2, in Example 1, the thermal stress at points X1 and X2 is alleviated compared to Reference Example 1, Comparative Example 1 and Comparative Example 2.
[0133] For the film capacitor model of Example 1, the first pitch angle θ1 and the first pitch height H1 were changed to the values shown in Table 3, and the maximum thermal stress applied to points X1 and X2 was confirmed by the same method as above. Using Reference Example 1 in Table 2 as a standard, if the maximum thermal stress applied to points X1 and X2 was less than 20 MPa, it was evaluated as ○, and if it was 20 MPa or more and less than 25 MPa, it was evaluated as △. The results are shown in Table 3.
[0134] [Table 3]
[0135] From Table 3, it can be seen that the thermal stress at points X1 and X2 is reduced more than that of Reference Example 1 in Table 2 when the first pitch angle θ1 and the ratio of the first pitch height H1 to the first electrode thickness T1 are within a predetermined range.
[0136] In the film capacitor model of Example 1, a polypropylene film, which is a thermoplastic resin film, was used instead of the thermosetting resin film (linear expansion coefficient: 100×10 -6 / ℃) to construct a film capacitor model with the same shape as in Table 3. The properties of the polypropylene film are shown in Table 4.
[0137] [Table 4]
[0138] The maximum thermal stress applied to points X1 and X2 was confirmed by the same method as above. The results are shown in Table 5.
[0139] [Table 5]
[0140] Table 5 shows that for all ranges shown in Table 5 for the first pitch angle θ1 and the ratio of the first pitch height H1 to the first electrode thickness T1, the thermal stress at points X1 and X2 is reduced more than in Reference Example 1 in Table 2.
[0141] FIG. 17 is a schematic cross-sectional view showing a first modified example of the film capacitor model that is modeled and analyzed based on the film capacitor in accordance with Example 1.
[0142] In FIG. 17, the thickness of the external electrode part C is 5 mm, the first pitch angle θ1 is 71°, and the first pitch height H1 is 2.5 mm (the ratio of the first pitch height H1 to the first electrode thickness T1 is 50%). In this case, the thermal stress at point X1 was 5.7 MPa. The thermal stress at point X2 opposite to point X1 was also 5.7 MPa.
[0143] FIG. 18 is a schematic cross-sectional view showing a second modified example of the film capacitor model that is modeled and analyzed based on the film capacitor in accordance with Example 1.
[0144] In FIG. 18, the thickness of the external electrode part C is 1 mm, the first pitch angle θ1 is 71°, and the first pitch height H1 is 0.5 mm (the ratio of the first pitch height H1 to the first electrode thickness T1 is 50%). In this case, the thermal stress at point X1 was 5.7 MPa. The thermal stress at point X2 opposite to point X1 was also 5.7 MPa.
[0145] From the above, it is considered that the thermal stress applied to points X1 and X2 depends on the first pitch angle θ1 and the ratio of the first pitch height H1 to the first electrode thickness T1. [Explanation of symbols]
[0146] 1, 2 Film capacitor 10 Capacitor element 20 Laminate 20a: first end surface of laminate 20b: second end surface of laminate 21 First metallized film 22 Second metallized film 31 First dielectric film 31a: First main surface of first dielectric film 31b: second main surface of first dielectric film 32 Second dielectric film 32a: third main surface of second dielectric film 32b: fourth main surface of second dielectric film 41 1st metal layer 42 Second metal layer 51 1st external electrode 52 2nd external electrode 61 First lead wire 62 Second Lead Wire 70 Exterior resin (exterior body) 71 Filling resin (outer body) 72 Exterior case (exterior body) 101 1st film reel 102 2nd film reel 111 1st reel axis 112 Second reel axis 200 winding shaft H1 First pitch height H2 Second pitch height T1 First electrode thickness T2 Second electrode thickness θ1 First pitch angle θ2 Second pitch angle
Claims
1. A film capacitor including a capacitor element, the capacitor element comprises a laminate having a first end face and a second end face opposing each other in a width direction, a first external electrode connected to the first end face of the laminate, and a second external electrode connected to the second end face of the laminate, the laminate includes a first dielectric film, a second dielectric film, a first metal layer, and a second metal layer; the first dielectric film has a first main surface and a second main surface opposed to each other in a thickness direction perpendicular to the width direction, the second dielectric film has a third main surface and a fourth main surface opposed to each other in the thickness direction, In the laminate, the second main surface of the first dielectric film and the third main surface of the second dielectric film face each other in the thickness direction, the first metal layer is connected to the first external electrode; the second metal layer is connected to the second external electrode; the first dielectric film and the second dielectric film adjacent to each other in the thickness direction, the first dielectric film protrudes toward the first external electrode relative to the second dielectric film, when a length in the width direction by which the first dielectric film protrudes from the second dielectric film is defined as a first protrusion width, the first protrusion width is larger at an outer periphery of the laminate in the thickness direction than at a central portion of the laminate in the thickness direction and increases toward the outermost periphery of the laminate in the thickness direction, the first dielectric film and the second dielectric film adjacent to each other in the thickness direction, the second dielectric film protruding toward the second external electrode side relative to the first dielectric film, a film capacitor, wherein when a length in the width direction by which the second dielectric film protrudes from the first dielectric film is defined as a second protrusion width, the second protrusion width at the outer periphery of the laminate in the thickness direction is larger than that at a central portion of the laminate in the thickness direction and becomes larger toward the outermost periphery of the laminate in the thickness direction.
2. 2. The film capacitor according to claim 1, wherein, when viewed in a cross section along the thickness direction and the width direction, an end of the first dielectric film that is closest to an outermost periphery of the laminate in the thickness direction and has the largest first protrusion width is defined as point X1, and an end of the first dielectric film that is closest to point X1 and has the smallest first protrusion width is defined as point Y1, an angle formed by a straight line passing through point X1 and point Y1 and a straight line passing between the ends of the first dielectric film having the smallest first protrusion width is greater than or equal to 50° and less than 80°.
3. 3. The film capacitor according to claim 1, wherein, when viewed in a cross section along the thickness direction and the width direction, an end of the first dielectric film that is closest to an outermost periphery of the laminate in the thickness direction and has the largest first protruding width is defined as point X1, and an end of the first dielectric film that is closest to point X1 and has the smallest first protruding width is defined as point Y1, and a length in the width direction between point X1 and point Y1 is 5% to 50% of a length in the width direction between an outer end of the first external electrode and point X1.
4. 3. The film capacitor according to claim 1, wherein, when viewed in a cross section along the thickness direction and the width direction, an end of the second dielectric film that is closest to the outermost periphery of the laminate in the thickness direction and has the largest second protrusion width is defined as point X2, and an end of the second dielectric film that is closest to point X2 and has the smallest second protrusion width is defined as point Y2, an angle formed by a straight line passing through point X2 and point Y2 and a straight line passing between the ends of the second dielectric film having the smallest second protrusion width is greater than or equal to 50° and less than 80°.
5. 3. The film capacitor according to claim 1, wherein, when viewed in a cross section along the thickness direction and the width direction, an end of the second dielectric film that is closest to an outermost periphery of the laminate in the thickness direction and has the largest second protruding width is defined as point X2, and an end of the second dielectric film that is closest to point X2 and has the smallest second protruding width is point Y2, a length in the width direction between point X2 and point Y2 is 5% to 50% of a length in the width direction between an outer end of the second external electrode and point X2.
6. the first metal layer is not connected to the second external electrode; The film capacitor according to claim 1 , wherein the second metal layer is not connected to the first external electrode.
7. the first metal layer is provided on the first major surface of the first dielectric film; The film capacitor according to claim 1 , wherein the second metal layer is provided on the third main surface of the second dielectric film.
8. The film capacitor according to claim 1 , wherein the first dielectric film and the second dielectric film contain a curable resin as a main component.
9. The film capacitor according to claim 1 , wherein the first dielectric film and the second dielectric film contain a thermoplastic resin as a main component.
10. The film capacitor according to claim 1 , further comprising an exterior body covering an outer periphery of the capacitor element.
Citation Information
Patent Citations
Film capacitor
JP1992057311A
Film capacitor
JP1992057312A
Film capacitor
JP2012182352A
Film capacitor
JP2013004916A