Sealed battery

The sealed battery design with curved side walls and optimized ratios in the laminate film structure addresses electrode body movement issues, enhancing battery reliability and sealing performance.

JP7569496B2Active Publication Date: 2024-10-18TOYOTA JIDOSHA KK
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2020106749
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-22
Publication Date
2024-10-18
Estimated Expiration
2040-06-22

AI Technical Summary

Technical Problem

The movement of the electrode body inside the housing part of a sealed battery with a laminate film exterior body can cause deformation or damage, leading to short circuits.

Method used

The housing portion of the laminate exterior body is designed with curved side walls that approach the electrode body, and the ratio of long sides to short sides is optimized to suppress movement, along with a specific curvature ratio and laminate film structure to prevent deformation and wrinkles.

Benefits of technology

This configuration effectively prevents electrode body movement, deformation, and terminal structure damage, ensuring reliable sealing and performance of the sealed battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569496000001
    Figure 0007569496000001
  • Figure 0007569496000002
    Figure 0007569496000002
  • Figure 0007569496000003
    Figure 0007569496000003
Patent Text Reader

Abstract

To provide a technology that can suppress the movement of an electrode body inside an exterior body.SOLUTION: A hermetically sealed battery 100 includes an electrode body 1 having a rectangular wide surface 11, an exterior body 2 made of a laminated film, and positive and negative electrode collecting terminals 3, 4. The exterior body 2 includes a housing unit 30, which houses the electrode body 1, and a seal unit formed around the housing unit 30 to shut off the interior of the exterior body 2 from the exterior. The housing unit 30 has a flat surface 31, which faces the wide surface 11 of the electrode body 1 and four side walls 32 to 35, which are formed to rise from the sealing unit toward the flat surface 31 and correspond to the four sides of the wide face 11, respectively. A set of side walls 32, 34 corresponding to the long sides of the wide surface 11 are curved toward the electrode body 1, in the inward direction of the exterior body 2, until they are close to the electrode body 1.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sealed battery having an exterior body made of a laminate film, and more particularly to a structure of an electrode assembly housing portion formed in the exterior body. [Background technology]

[0002] In recent years, research and development of various batteries has been actively conducted. In particular, secondary batteries such as lithium-ion secondary batteries are becoming increasingly important as power sources for vehicles or for personal computers, mobile terminals, etc. In particular, lithium-ion secondary batteries, which are lightweight and have high energy density, are preferably used as high-output power sources for vehicles. This type of secondary battery is typically a sealed battery in which an electrode assembly, which is a power generating element having a positive electrode and a negative electrode, is housed and sealed inside an exterior body.

[0003] In recent years, there has been an increasing demand for smaller batteries, and the development of sealed batteries with an exterior body made of a laminate film has been actively carried out. In a sealed battery with an exterior body made of a laminate film, typically, an electrode assembly is sandwiched between two laminate films, and the laminate films are sealed together at the periphery of the electrode assembly, thereby being housed inside the exterior body. Regarding the arrangement of the electrode body inside the exterior body, Patent Documents 1 and 2 describe a method of embossing a laminate film in advance and arranging the electrode body in the internal space of the embossed part. In this way, by providing a housing part for housing the electrode body in the laminate film, the electrode body can be arranged at an appropriate position inside the exterior body. On the other hand, when the sealed battery is a so-called all-solid-state battery that includes a solid electrolyte as an electrolyte, the electrode body is generally sandwiched between two laminate films, and then the exterior body is sealed in a state in which the inside of the exterior body is depressurized, thereby holding the electrode body inside the exterior body. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2005-285506 A [Patent Document 2] International Publication No. 2015 / 151580 Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, when the electrode body is disposed inside a housing part previously formed in a laminate film, if there is a distance between the laminate film (i.e., the housing part) and the electrode body, the electrode body may move inside the housing part. The movement of the electrode body inside the housing part is undesirable because it may cause deformation or damage to the edge of the electrode body, leading to the occurrence of a short circuit.

[0006] The present invention has been made in consideration of these points, and its main objective is to provide a technology that can suppress movement of an electrode body inside an outer casing in a sealed battery equipped with an outer casing having a storage section as described above. [Means for solving the problem]

[0007] The present inventors focused on the structure of the housing part of the laminate exterior body and discovered that movement of the electrode body inside the housing part can be suppressed by curving a part of the housing part toward the electrode body, which led to the completion of the present invention.

[0008] According to the technology disclosed herein, there is provided a sealed battery comprising: an electrode body having a positive electrode and a negative electrode and having a rectangular wide surface; an exterior body made of a laminate film that houses the electrode body; and positive and negative electrode current collecting terminals for external connection that are provided on the positive electrode and the negative electrode, with at least a portion of the positive and negative electrode current collecting terminals being disposed outside the exterior body. The exterior body includes a housing portion that houses the electrode assembly, and a seal portion formed around the housing portion to isolate the inside and outside of the exterior body. The housing portion has a flat surface facing the wide surface of the electrode body, and four side walls that rise from the seal portion toward the flat surface and correspond to the four sides of the wide surface. Of the four side walls, a set of side walls that correspond to the long sides of the wide surface are curved inwardly of the exterior body toward the electrode body until they approach the electrode body. According to this configuration, the side wall of the housing portion is curved and comes close to the electrode body, thereby suppressing movement of the electrode body inside the exterior body, thereby making it possible to prevent deformation and damage of the electrode body due to movement of the electrode body.

[0009] The periphery of the exterior body, when the electrode body is housed therein, has two long sides corresponding to the long sides of the wide surface and two short sides corresponding to the short sides of the wide surface. Preferably, the ratio of the length of the long side to the length of the short side is 2 or greater. With this configuration, in addition to the effect of suppressing movement of the electrode body, the effect of preventing deformation of the terminal structure can be achieved.

[0010] In one embodiment of the sealed battery disclosed herein, the ratio of the length of the long side to the width of the seal portion at the long side is 15 or greater. According to the technology disclosed herein, even in a sealed battery having an exterior body having such a dimensional relationship, in addition to the effect of suppressing movement of the electrode body, the effect of preventing the occurrence of wrinkles and distortion can be suitably exerted.

[0011] In another aspect, the positive electrode current collector terminal and the negative electrode current collector terminal are both disposed on the short side of the rectangular wide surface of the electrode body. With this configuration, in addition to the effect of suppressing movement of the electrode body, the effect of preventing deformation of the terminal structure can be more suitably achieved.

[0012] In another embodiment, the laminate film is a laminated structure having a metal layer and a resin layer, and the thickness of the metal layer is 100 μm or less. According to the technology disclosed herein, even in a sealed battery having an outer casing made of such a laminate film, in addition to the effect of suppressing movement of the electrode body, the effect of preventing the occurrence of wrinkles and distortion and the effect of preventing deformation of the terminal structure can be suitably exerted.

[0013] For the two long sides and two short sides of the flat surface of the storage section, the ratio of the distance between the apex of curvature of one of the two long sides and the apex of curvature of the other long side to the length of the short sides is 0.9 or more and 0.99 or less. In a sealed battery having such a configuration, the internal space of the storage portion is appropriately provided compared to the size of the electrode body contained in the storage portion, and when the above ratio is in the range of 0.9 or more and 0.99 or less, it is possible to achieve a high level of effect in preventing the electrode body from moving, as well as a high level of effect in preventing deformation of the terminal structure and the occurrence of wrinkles and distortion. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 is a perspective view showing a schematic structure of a sealed battery according to one embodiment. [Diagram 2] FIG. 1 is a plan view illustrating a schematic structure of a sealed battery according to one embodiment. [Diagram 3] FIG. 2 is a plan view illustrating a process for producing a sealed battery according to an embodiment. [Figure 4] FIG. 2 is a plan view illustrating a process for producing a sealed battery according to an embodiment. [Diagram 5] FIG. 2 is a plan view illustrating a process for producing a sealed battery according to an embodiment. [Figure 6] FIG. 2 is a plan view illustrating a process for producing a sealed battery according to an embodiment. [Figure 7]1 is a graph showing the relationship between the ratio (L2 / W1) of the width W1 of a seal portion on a long side of an exterior body to the length L2 of the long side, and the magnitude of stress that may occur on the long side during a decompression process. [Figure 8] 1 is a graph showing the relationship between the ratio (L2 / L1) of the short side length L1 to the long side length L2 of the exterior body and the magnitude of stress that may occur in the terminal structure of the exterior body during a decompression process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] An embodiment of the present invention will be described below. In the following drawings, the same reference numerals are used to denote components and parts that perform the same function. The dimensional relationships (length, width, thickness, etc.) in each drawing do not reflect the actual dimensional relationships. Furthermore, matters other than those specifically mentioned in this specification that are necessary for implementing the present invention (for example, the detailed structure and materials of the electrode body) can be understood as design matters of a person skilled in the art based on the prior art in the field. In this specification, the notation "A to B" indicating a numerical range means A or more and B or less, and includes values ​​greater than A and less than B. In this specification, the term "secondary battery" refers generally to an electricity storage device that can be repeatedly charged and discharged, and includes so-called storage batteries (i.e., chemical batteries) such as lithium ion secondary batteries, nickel-metal hydride batteries, and nickel-cadmium batteries, as well as capacitors (i.e., physical batteries) such as electric double layer capacitors. Hereinafter, a sealed battery to which the technology disclosed herein is applicable will be described in detail, taking as an example an all-solid-state lithium ion secondary battery including a laminated electrode body.

[0016] 1 and 2, a sealed battery 100 roughly comprises an electrode assembly 1, an exterior body 2, a positive electrode current collector terminal 3, and a negative electrode current collector terminal 4. The electrode assembly 1 is housed inside the exterior body 2 with its periphery heat-sealed. The positive electrode current collector terminal 3 and the negative electrode current collector terminal 4 are partially disposed outside the exterior body 2. The electrode body 1 has two flattened rectangular wide faces, these two wide faces serving as bases, and is in the shape of a rectangular parallelepiped having four side faces.

[0017] Although detailed illustration is omitted, the electrode assembly 1 includes a positive electrode, a negative electrode, and a solid electrolyte layer. The electrode body 1 in this embodiment is a laminated electrode body, and includes a positive electrode sheet having a rectangular sheet-shaped positive electrode collector and a positive electrode composite layer coated on the surface (one side or both sides) of the positive electrode collector as a positive electrode. The electrode body 1 includes a negative electrode sheet having a rectangular sheet-shaped negative electrode collector and a negative electrode composite layer coated on the surface (one side or both sides) of the negative electrode collector as a negative electrode. Both the positive electrode sheet and the negative electrode sheet have a collector exposed portion on which no composite layer is formed at one end in the sheet long side direction (i.e., the long side direction Y of the wide surface of the electrode body 1 in the figure). The collector exposed portion is formed in a tab shape and protrudes outward from the short side of the sheet. The positive electrode sheets and the negative electrode sheets are alternately laminated with a solid electrolyte layer interposed therebetween to form the electrode body 1. The region including the center of the electrode body 1 is a core portion where the electrode composite layers are laminated. At one end of the sheet in the long side direction, a current collector exposed portion (current collector) is laminated, and the current collector exposed portions are gathered in the sheet lamination direction to form a current collector terminal joint for external connection.

[0018] A positive current collector terminal 3 is joined to the positive current collector terminal joint, and a negative current collector terminal 4 is joined to the negative current collector terminal joint. As shown in the figure, the positive current collector terminal 3 and the negative current collector terminal 4 are both arranged on the short side 19 side of the wide surface 11 of the electrode body 1 and are drawn from the inside to the outside of the exterior body 2. The positive current collector terminal 3 and the negative current collector terminal 4 are covered with heat-sealed films 5 and 6, respectively. The heat-sealed films 5 and 6 are sandwiched between the current collector terminals and the exterior body 2.

[0019] The electrode body 1 is not particularly limited in its detailed structure, so long as it has a current collector terminal joint formed therein as described above and a current collector terminal of the same electrode is joined thereto. As the members and materials (e.g., current collector foil, composite layer, solid electrolyte layer, etc.) constituting the electrode body 1, those typically used in this type of lithium ion secondary battery can be used without particular limitation, and detailed description is omitted since they do not characterize the present invention. The positive electrode current collector terminal 3 and the negative electrode current collector terminal 4 are conductive members that electrically connect the electrode body 1 to an external device. Although not particularly limited, such current collector terminals are made of a conductive material such as aluminum, copper, nickel, etc. The heat-sealing films 5 and 6 are members for suitably welding the current collecting terminals and the exterior body 2. The material of the heat-sealing films 5 and 6 may be a resin material that melts at approximately the same temperature as the exterior body 2 (specifically, the first resin layer described later) and exhibits suitable welding properties to both resin materials and metal materials. Although not particularly limited, the heat-sealing films 5 and 6 may be, for example, modified polypropylene or a film with a multilayer structure including a polyolefin layer.

[0020] The exterior body 2 is a battery case made of a laminate film, and is formed by folding a sheet of laminate film and fusing the laminate films together at the periphery as shown in the figure. The exterior body 2 houses the electrode assembly 1 inside. As shown in the figure, the exterior body 2 is rectangular (rectangle in the figure) and has two long sides 22, 24 and two short sides 23, 25. The two long sides 22, 24 correspond to the long sides 16, 18 of the electrode body 1. The two short sides 23, 25 correspond to the short sides 17, 19 of the electrode body 1.

[0021] Furthermore, the exterior body 2 is formed with a housing portion 30 for housing the electrode body 1, and seal portions 41, 42, and 43 around the housing portion 30. The inside and outside of the exterior body 2 are isolated from each other by these seal portions. The housing portion 30 has a flat surface 31 and four side walls 32, 33, 34, and 35. The flat surface 31 faces the wide surface 11 of the electrode body 1. The side walls 32, 33, 34, and 35 are formed to rise from the seal portion 40 toward the flat surface 31 so as to surround the periphery of the electrode body 1. 1, the side wall 33 and the side wall 35 face each other. When the electrode body 1 is housed inside, the side wall 33 and the side wall 35 face each other, respectively, with the side surface 13 and the side surface 15 on the short side of the wide surface 11 of the electrode body 1. Moreover, the side walls 32 and 34 face each other. When the electrode body 1 is housed therein, the side walls 32 and 34 face each other, respectively, with the side surfaces 12 and 14 on the longer sides of the wide surface 11 of the electrode body 1. The side walls 32 and 34 curve inwardly of the exterior body 2 toward the electrode body 1, and are close to the side surfaces 12 and 14. The side walls 32 and 34 may be in contact with the electrode body 1 (i.e., the side surfaces 12 and 14), and are preferably in contact from the viewpoint of suppressing movement of the electrode body 1.

[0022] Since the exterior body made of a laminate film is highly flexible, problems may occur during the process of manufacturing the battery. For example, when manufacturing an all-solid-state battery, in the process of reducing the pressure inside the exterior body, stress may be generated in the periphery of the exterior body, causing the periphery to bend. It is not preferable that the periphery of the exterior body bends because wrinkles or distortion may occur during welding, causing poor welding and reducing the sealing property of the sealed battery, or reducing the folding processability of the seal part. In addition, if the part where the current collecting terminal is arranged is bent and the terminal structure is deformed, it may cause damage to the electrode body or a short circuit, which is not preferable.

[0023] From the viewpoint of preventing deformation of the terminal structure, the ratio (L2 / L1) of the length L2 of the long side portions 22, 24 to the length L1 of the short side portions 23, 25 of the exterior body 2 is greater than 1, more preferably the ratio (L2 / L1) is 1.5 or more, and even more preferably the ratio (L2 / L1) is 2 or more. The ratio (L2 / L1) can typically be 10 or less, for example, 5 or less, 3 or less. 2, L1 is the length of the side of the exterior body 2 on which the current collecting terminals are arranged, and L2 is the length of the side of the exterior body 2 on which the current collecting terminals are not arranged. In other words, the above ratio (L2 / L1) can also be said to be the ratio between the length L1 of the side on which the current collecting terminals are arranged and the length L2 of the side on which the current collecting terminals are not arranged. As described in Test Example 1 below, when the ratio (L2 / L1) is within the above range, the stress that may occur in the peripheral portion of the outer casing 2 where the current collecting terminal is arranged (in Figure 2, the short side portion 25 of the outer casing 2) during the decompression process described below is reduced, thereby suppressing deformation of the terminal structure.

[0024] As described in the following Test Example 2, the larger the length L2 of the long side portions 22, 24 of the exterior body 2 is relative to the width W1 of the seal portions 41, 43 at the long side portions 22, 24 (i.e., the length in the short side direction X of the exterior body 2), the more likely it is that stress will be generated in the long side portions in the decompression process described later, and wrinkles, distortion, etc. will be generated. Since the laminate film is a material with low rigidity, it is easily deformed, and if deformation occurs in the storage portion in the decompression process described later, this may cause excessive deformation in the seal portion. In particular, in a sealed battery in which the ratio (L2 / W1) of the length L2 of the long side portions 22, 24 to the width W1 of the seal portions 41, 43 at the long side portions 22, 24 is 15 or more, wrinkles, distortion, etc. will be generated easily due to the decompression process. It is preferable to apply the technology disclosed herein to such a sealed battery 100.

[0025] With regard to the two long sides 36, 38 and short sides 37, 39 on the flat surface 31 of the housing section 30, it is preferable that the ratio (L4 / L3) of the distance L4 between the curved vertex 36a of the long side 36 and the curved vertex 38a of the long side 38 to the length L3 of the short side is 0.9 or more and 0.99 or less. By having the ratio (L4 / L3) within the above range, movement of the electrode body 1 inside the exterior body 2 can be suitably suppressed.

[0026] Although not shown in the figure, the exterior body 2 typically includes a first resin layer, a metal layer, and a second resin layer, and these layers are laminated in this order from the inside to the outside of the exterior body 2. The first resin layer is the innermost layer of the exterior body 2 and is the layer closest to the electrode body 1. The first resin layer is a layer for enabling welding of laminate films to each other, and is typically made of a thermoplastic resin. Examples of the thermoplastic resin include crystalline resins such as polyolefins such as polyethylene (PE) and polypropylene (PP); polyesters such as polyethylene terephthalate (PET); and non-crystalline resins such as polystyrene and polyvinyl chloride.

[0027] The metal layer is a layer that imparts strength to the exterior body 2. The metal layer can also have a function of blocking the movement of gas between the inside and outside of the exterior body 2. Examples of materials that form the metal layer include aluminum, iron, and stainless steel. By adjusting the thickness of the metal layer, it is possible to adjust the rigidity of the exterior body 2. Although not particularly limited, the thickness of the metal layer is typically 0.01 μm or more and 200 μm or less. The effect of the technology disclosed herein can be preferably achieved even in the case of using a laminate film having a metal layer with a thickness of 0.01 μm or more and 100 μm or less and having a relatively low rigidity.

[0028] The second resin layer is located closer to the outer surface than the metal layer and may be the outermost layer of the exterior body 2. The second resin layer can improve, for example, the durability of the exterior body 2. Examples of materials constituting such a second resin layer include polyethylene terephthalate (PET) and polyamide.

[0029] The number of layers constituting the exterior body 2 is not particularly limited, and may be 3 or more, or 4 or more (for example, 4 or more and 10 or less). Also, an adhesive layer may be provided between the layers, and a printed layer or the like may be provided as the outermost layer.

[0030] The method for producing a sealed battery disclosed herein broadly includes an electrode body preparation step, a current collecting terminal attachment step, an arrangement step, a first heating step, a decompression step, a second heating step, and a cutting step (see FIGS. 3 to 6). First, the electrode assembly 1 is constructed (electrode assembly preparation step). The method for constructing the electrode assembly 1 may be the same as in the conventional method, and is not a feature of the present invention, so a detailed description thereof will be omitted. Next, the positive electrode current collector terminal 3 and the negative electrode current collector terminal 4 are attached to the current collector terminal joint of the electrode body 1 (terminal attachment process). At this time, heat-sealing films 5, 6 are placed on the positive electrode current collector terminal 3 and the negative electrode current collector terminal 4. Note that as a means for joining the current collector terminals to the current collector terminal joint, any conventionally known joining means such as ultrasonic welding, laser welding, resistance welding, etc. can be used without any particular limitation.

[0031] Next, as shown in Fig. 3, the electrode body 1 with the current collector terminals attached and the laminate film 7 are placed in a predetermined position (placement step). Specifically, first, a laminate film 7 with a storage section 71 formed in advance, for example, by embossing is prepared. Next, the electrode body 1 is placed inside the storage section 71, and the laminate film 7 is folded to encase the electrode body 1. At this time, the electrode body 1 is placed such that the positive electrode current collector terminal 3 and the negative electrode current collector terminal 4 are at least partially pulled out to the outside of the laminate film. In addition, the thermally welded films 5 and 6 are placed such that at least partially pulled out to the outside of the laminate film. The accommodation section 71 may be formed so as to be disposed on both sides of the electrode body 1 when the laminate film 7 is disposed to encase the electrode body 1 as described above. The accommodation section 71 may also be formed so as to be disposed on only one side (the wide surface 11a side in FIG. 3) of the electrode body 1. That is, in this case, the laminate film 7 disposed on the wide surface side different from the wide surface 11a side is flat, and no accommodation section is formed therein.

[0032] 4, the overlapped laminate films 7 are heat-sealed to each other at an edge 73 on the long side of the wide surface 11a of the electrode body 1 in the laminate film 7 and an edge 72 on the short side where the current collecting terminals 3, 4 and the heat-sealing films 5, 6 are arranged (first heating step). In the sandwiching direction of the electrode body 1, the edges 72, 73 are sandwiched from both sides by a heating part of a heat sealing device (also called a "heat sealer"), and a predetermined amount of heat is applied to the edges 72, 73, thereby heat-sealing the laminate films 7 to each other. The order in which the edges 72, 73 are heat-sealed is not particularly limited, but from the viewpoint of fixing the current collecting terminals 3, 4 and the heat-sealing films 5, 6, it is preferable to heat-seal the edges 72 and then the edges 73. In this step, the laminate film 7 is not heat-welded to each other at another edge 75 on the long side of the wide surface 11a, which is different from the edge 72, but is left open. The other edge 74 on the short side of the wide surface 11a, which is different from the edge 72, is a folded portion of the laminate film 7, so there is no need to heat-weld it.

[0033] Next, the inside of the laminate film 7 that has been formed into a bag shape by the above-mentioned heat welding is depressurized to a vacuum state (about several tens to 99 kPa) (depressurization process). As a result, as shown in FIG. 5, the side walls 71b and 71d on the long side (i.e., the long side of the wide surface 11a) of the housing portion 71 are curved toward the electrode body 1 until they approach the electrode body 1. The edge portion 73 and the edge portion 75 on the long side of the wide surface 11a of the electrode body 1 in the laminate film 7 may be curved inward. On the other hand, in this embodiment, the seal portion formed on the edge portion 72 where the current collecting terminals 3 and 4 are arranged corresponds to the seal portion 42 on the short side portion 25 in FIG. 2. As described above, since it is not preferable for the terminal structure to be deformed, the depressurized state is adjusted to such an extent that the side walls 71a and 71c on the short side of the housing portion 71 are not curved. Furthermore, from the viewpoint of the sealing performance of the sealed battery and the folding workability of the sealed portion, the reduced pressure state is adjusted so that even if side walls 71b and 71d are curved as described above, wrinkles or distortions do not occur around the side walls. Furthermore, the laminate films 7 are heat-welded to each other at the edges 75 that were not heat-welded in the first heating step. As a result, there is no opening in the laminate film 7, and the laminate film 7 is sealed with the electrode body 1 housed inside.

[0034] 6, the overlapping laminate films 7 are heat-sealed to each other around the long side of the housing section 71 (second heating step). The laminate films 7 are sandwiched from both sides by the heating section of a heat sealer in the sandwiching direction of the electrode body 1, and a predetermined amount of heat is applied to heat-seal the laminate films 7 to form the seal section 76 and the seal section 77. As shown in the figure, the seal section 76 and the seal section 77 are straight and not curved. That is, no wrinkles or distortions are formed in the seal section 76 and the seal section 77. Next, the laminate film 7 is cut along the seal portion 76 and the seal portion 77 (cutting step). In this way, a sealed battery is produced. The seal portion 76 and the seal portion 77 correspond to the seal portion 43 and the seal portion 41 in the sealed battery 100 in FIG. 2.

[0035] The manufacturing method disclosed herein can suppress the movement of the electrode body inside the exterior body. In addition to the effect of suppressing the movement of the electrode body, the method can also achieve the effect of suppressing deformation in the short side portion of the exterior body where the current collecting terminal is arranged, and the effect of preventing the occurrence of wrinkles and distortion in the long side portion of the exterior body. Therefore, although not particularly limited, the manufacturing method disclosed herein can be particularly preferably used in the manufacture of a sealed battery including an exterior body having the above-mentioned dimensional relationship. Furthermore, although not particularly limited, the manufacturing method disclosed herein can be particularly preferably used in the case where a laminate film having a relatively low rigidity as described above is used as the exterior body.

[0036] <Variation 1> In the above manufacturing method, the side walls 32 and 34 (see FIG. 1) on the long sides of the housing section 30 are curved by carrying out a decompression step, but the present invention is not limited to this. For example, when forming a housing section in a laminate film, a housing section with curved side walls on the long sides may be formed, and such a laminate film may be used as an exterior body. In this case, the decompression step of the above manufacturing method is not essential. When the decompression step is not carried out, a sealed battery having an electrolytic solution as an electrolyte can be manufactured by the manufacturing method.

[0037] <Variation 2> In addition, by appropriately adjusting the reduced pressure state in the depressurization step, the thermal welding of the edge portion 73 and the edge portion 75 in the above embodiment can be omitted (see Figs. 4 to 6). That is, the electrode body 1 is wrapped in the laminate film 7, a seal portion is formed at the edge portion 72 on the short side of the housing portion 71 in the laminate film 7, and a seal portion 76 is formed along the side wall 71b of the housing portion 71. Next, the inside of the bag-shaped laminate film 7 is depressurized. Here, the reduced pressure state is adjusted to such an extent that the edge portion 72 and the edge portion 74 on the short side of the laminate film 7 and the seal portion 76 are not curved, and the side wall 71b and the side wall 71d on the long side of the housing portion 71 are curved toward the electrode body 1. Then, the seal portion 77 is formed along the side wall 71d of the housing portion 71 to seal the laminate film 7.

[0038] <Variation 3> In the above embodiment, one laminate film is folded to encase the electrode body, and seal portions are formed on three sides, but this is not limited to this, and two laminate films may be used. In the first heating step of this modification, a seal portion is formed on the edge portion 74 (see FIG. 4) on the short side of the laminate film 7.

[0039] <Test Example> The test examples described below were carried out by the present inventors when conceiving the technology disclosed herein. <<Test Example 1: Examination of deformation of the long side of the exterior body>> The correlation between the ratio of the width of the seal portion at the long side of the exterior body to the length of the long side and the magnitude of stress that may occur at the long side in the decompression process was examined. Specifically, the present test was performed on the assumption that the exterior body has an aluminum layer as a metal layer, and the sealed battery 100 is manufactured while changing the ratio (L2 / W1) of the width W1 of the seal portion 41, 43 at the long side portions 22, 24 of the exterior body 2 shown in FIG. 2 to the length L2 of the long side. In the present test, first, an electrode body 1 having a rectangular wide surface was manufactured by a conventional method. The electrode body 1 was accommodated in the accommodation portion 30 of the exterior body 2 made of a laminate film. The inside of the exterior body 2 was made into a vacuum state by the above-mentioned method, and the sealed battery 100 in which the seal portions 41, 42, 43 were formed was manufactured. Here, the sealed batteries 100 having different widths W1 of the seal portions 41, 43 at the long side portions 22, 24 of the exterior body 2 were prepared. That is, sealed batteries 100 were prepared with different ratios (L2 / W1) of the width W1 of the seal portions 41, 43 to the length L2 of the long sides 22, 24 of the exterior body 2. Then, for each sealed battery 100, the stress σ generated in the seal portions 41, 43 was calculated based on the degree of curvature (the degree to which the sealed battery is bent inward). The results of Test Example 1 are shown in Figure 7. The X-axis "L2 / W1" in Figure 7 indicates the ratio (L2 / W1), and the Y-axis "stress [MPa]" indicates the magnitude of stress that can occur in the long side of the exterior body. The straight line A in the figure indicates the yield strength of aluminum, and indicates that when the stress is below A, the long side does not deform, and when the stress is A or more, the long side can deform.

[0040] As shown in the figure, it was found that the larger the ratio (L2 / W1), the greater the stress generated in the long side portion of the exterior body. When the ratio (L2 / W1) is greater than 15, the stress becomes A or more, and therefore it was found that the sealed battery 100 having an exterior body having the above-mentioned dimensional relationship for the length L2 and width W1 is prone to wrinkles and distortion in the long side portion during the decompression process. Therefore, it was found that such a sealed battery 100 is suitable as an application subject of the technology disclosed herein.

[0041] <<Test Example 2: Consideration of the arrangement of current collecting terminals>> The correlation between the dimensional relationship (aspect ratio) of the exterior body and the magnitude of stress that may occur in the terminal structure during the decompression process was examined. Specifically, this test was performed on the assumption that a sealed battery 100 was manufactured while changing the ratio (L2 / L1) of the length L1 to the length L2 shown in FIG. 2. That is, in this test, for the exterior body 2, the length L1 represents the length of the side on which the current collector terminals 3 and 4 are arranged (the length of the short side portions 23 and 25 in FIG. 2), and the length L2 represents the length of the side on which the current collector terminals 3 and 4 are not arranged (the length of the long side portions 22 and 24 in FIG. 2). In addition, the specific procedure of this test was as follows: first, an electrode body 1 having a rectangular wide surface was manufactured by a conventional method. The electrode body 1 was accommodated in the accommodation portion 30 of the exterior body 2 made of a laminate film. The inside of the exterior body 2 was evacuated by the above-mentioned method, and the sealed battery 100 was manufactured in which the seal portions 41, 42, and 43 were formed. Here, sealed batteries 100 were prepared with different ratios (L2 / L1) of the length L1 of the side on which the current collecting terminals 3, 4 are arranged to the length L2 of the side on which the current collecting terminals 3, 4 are not arranged. For each sealed battery 100, the stress σ generated on the side on which the current collecting terminals 3, 4 are arranged was calculated based on the degree of curvature (the degree of bending inward of the sealed battery) on that side. The results of Test Example 2 are shown in Figure 8. Note that the X-axis "L2 / L1" in Figure 8 indicates the ratio (L2 / L1), and the Y-axis "stress [MPa]" indicates the magnitude of stress that may occur on the side on which the current collecting terminal is arranged.

[0042] As shown in the figure, it was found that the larger the ratio (L2 / L1), the smaller the stress generated in the terminal structure. It was found that when the ratio (L2 / L1) is smaller than 1, that is, when the length L1 of the side on which the current collecting terminal is arranged is longer than the length L2 of the side on which the current collecting terminal is not arranged, the terminal structure may be deformed by the stress generated in the depressurization process. On the other hand, when the ratio (L2 / L1) is larger than 1, that is, when the length L1 of the side on which the current collecting terminal is arranged is shorter than the length L2 of the side on which the current collecting terminal is not arranged, it was found that stress is less likely to be generated in the part by the depressurization process. In other words, it was found that it is preferable to arrange the current collecting terminal on the short side of the exterior body. In addition, it was found that from the viewpoint of preventing deformation of the terminal structure, it is preferable that the ratio (L2 / L1) is 1.5 or more, and more preferably 2 or more. [Explanation of symbols]

[0043] 100 sealed battery 1 Electrode body 2 Exterior body 3,4 Current collector terminal 5,6 Heat-sealing film 7 Laminating film 11 Wide surface 12~15 Side 22,24 Long side 23,25 Short side 30 Storage unit 31 Flat surface 32~35 side wall 36,38 Long side 36a,38a curved apex 37,39 Short side 41~43 Seal part 71 Storage unit 71a~71d Side wall 72~75 Edge 76,77 Seal part

Claims

1. An electrode body having a positive electrode and a negative electrode and a rectangular wide surface; an exterior body made of a laminate film that houses the electrode body; a positive electrode current collecting terminal and a negative electrode current collecting terminal for external connection provided on the positive electrode and the negative electrode, at least a portion of which is disposed outside the exterior body; A sealed battery comprising: the exterior body includes a housing portion that houses the electrode assembly, and a seal portion that is formed around the housing portion to isolate the inside and the outside of the exterior body, A sealed battery, wherein the storage portion has a flat surface facing the wide surface of the electrode body, and four side walls corresponding to the four sides of the wide surface and formed to rise from the sealing portion toward the flat surface, and one set of the side walls corresponding to the long sides of the wide surface are curved inwardly of the outer casing toward the electrode body until they contact the electrode body.

2. a periphery of the exterior body has two long side portions corresponding to the long side sides of the wide surface and two short side portions corresponding to the short side sides of the wide surface when the electrode assembly is housed therein; 2. The sealed battery according to claim 1, wherein the ratio of the length of said long side portion to the length of said short side portion is 2 or more.

3. a periphery of the exterior body has two long side portions corresponding to the long side sides of the wide surface and two short side portions corresponding to the short side sides of the wide surface when the electrode assembly is housed therein; 3. The sealed battery according to claim 1, wherein a ratio of the length of the long side portion to the width of the seal portion at the long side portion is 15 or more.

4. 4. The sealed battery according to claim 1, wherein the positive electrode current collector terminal and the negative electrode current collector terminal are both disposed on the short side of the rectangular wide surface of the electrode body.

5. 5. The sealed battery according to claim 1, wherein the laminate film is a laminated structure having a metal layer and a resin layer, and the thickness of the metal layer is 100 μm or less.

6. 6. The sealed battery according to claim 1, wherein, for each of the two long sides and two short sides of the flat surface of the housing portion, a ratio of a distance between an apex of curvature of one of the two long sides and an apex of curvature of the other long side to a length of the short side is 0.9 or more and 0.99 or less.

Citation Information

Patent Citations

  • Battery

    JP2005174680A

  • Manufacturing method of laminated battery and laminated battery

    JP2005285506A

  • Battery pack and manufacturing method thereof

    JP2014238912A

  • Staircase structure battery cell

    JP2015508223A

  • Flexible secondary battery

    JP2016149349A