Method, program, and device for predicting crack growth in plastic processing

The crack growth prediction method in plastic working processes addresses the challenge of inaccurate crack prediction by using simulation to identify initiation and track progression, ensuring high accuracy and efficiency in predicting crack locations and sizes.

JP7571664B2Active Publication Date: 2024-10-23PROTERIAL LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021091354
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-05-31
Publication Date
2024-10-23
Estimated Expiration
2041-05-31

AI Technical Summary

Technical Problem

Existing methods for predicting crack growth in plastic working processes, such as forging and rolling, fail to accurately account for plastic deformation, leading to inaccurate and time-consuming crack predictions in materials like super heat-resistant alloys used in aircraft engines and gas turbines.

Method used

A crack growth prediction method using plastic working simulation to identify crack initiation, specify the normal vector at initiation, and predict crack progression by determining the normal vector in subsequent simulation steps, incorporating finite element methods and crack growth models.

Benefits of technology

Enables precise and timely prediction of crack location and progression, reducing the need for extensive modifications and defects by accurately tracking crack growth during plastic deformation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007571664000019
    Figure 0007571664000019
  • Figure 0007571664000020
    Figure 0007571664000020
  • Figure 0007571664000021
    Figure 0007571664000021
Patent Text Reader

Abstract

To provide a method for predicting a crack initiation location and its propagation behavior with high accuracy in a short period of time in consideration of a plastic deformation state of a workpiece.SOLUTION: Based on plastic working simulation, the method S1 calculates a fracture value of a workpiece, S2 determines a position where the fracture value exceeds a preset threshold as a crack generation position, S3 identifies a simulation step in which the fracture value exceeds the threshold for the first time as a cracking generation step, S4 identifies the normal direction of crack generation in the crack generation step at the crack generation position, step S5 identifies the normal direction of the crack in each simulation step after the crack generation step, and S6 calculates a crack growth evaluation value for the workpiece.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method, a program, and an apparatus for predicting the growth of a crack that occurs in a workpiece during plastic processing, which includes hot processing such as forging and rolling. [Background technology]

[0002] Nowadays, plastic processing is being carried out on workpieces in various fields. It is necessary to analyze and consider measures against cracks in workpieces in this plastic processing. For example, superalloys used in aircraft engines and power generation gas turbines have the property of becoming embrittled at low temperatures, and their workability is highly dependent on temperature. For this reason, in the hot processing process of superalloys, there is a risk that cracks will occur during processing if the mold shape and processing conditions are not appropriate, which will increase the number of correction steps for the processed product and cause defects. Therefore, in order to achieve shorter delivery times and stable quality of products, it is necessary to predict the location and size of cracks at the design stage and consider measures to suppress cracks in advance.

[0003] Conventionally, a method for predicting cracks is generally known in which, for example, an index for evaluating fracture is calculated by the finite element method, and the index is compared with a threshold value to predict the crack occurrence position. Regarding prediction of crack growth, Patent Document 1 discloses a method for determining the stress state under a predetermined load condition in a state where no crack occurs, and then, in a state where a virtual crack exists that connects the end position and the tip position of the crack with a straight line, a stress intensity factor is determined reflecting the stress state in a state where no crack exists, and the direction of crack growth is determined. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2008-216184 A Summary of the Invention [Problem to be solved by the invention]

[0005] Here, Patent Document 1 describes a method for predicting the progress of a crack, but does not describe how to handle the crack when the material in the vicinity of the crack undergoes plastic deformation, so it is not possible to track the change in the direction of the crack due to plastic deformation. Therefore, it is not possible to grasp the stress components acting on the crack, and it is not possible to apply the method to a situation in which the crack progresses along with the plastic deformation of the workpiece material.

[0006] As described above, in Patent Document 1, it was not possible to predict the growth of a crack accompanying plastic deformation of a workpiece material with high accuracy and in a short period of time.

[0007] Therefore, an object of the present invention is to make it possible to predict the location of crack initiation and its propagation with high accuracy and in a short period of time, taking into account the state of plastic deformation of a workpiece when plastic processing is performed. [Means for solving the problem]

[0008] In order to achieve the above object of the present invention, the present invention provides a crack growth prediction method for predicting the growth of a crack that occurs in a workpiece during plastic processing, the method comprising the steps of: Determining the occurrence of cracks in the workpiece; Identifying a crack occurrence position where the crack has occurred; After the plastic deformation simulation: Identifying a crack initiation step in the plastic processing simulation in which a crack occurs at the identified crack initiation position; Identifying an initial crack initiation normal vector indicating a normal direction of the crack at the crack initiation step and the crack initiation position; predicting the growth of the crack by identifying a crack normal vector in a simulation step after the crack generation step based on the initial crack generation normal vector; This is a method for predicting crack growth.

[0009] The present invention also includes a crack growth prediction device that executes the crack growth prediction method, and a crack growth prediction program itself, which is a computer program that causes a computer to execute the crack growth prediction method, or a storage medium that stores the program. Effect of the Invention

[0010] According to the present invention, the progression of defects in plastic working can be predicted more easily, that is, with a smaller amount of calculation and with high accuracy. [Brief description of the drawings]

[0011] [Figure 1] 1 is a diagram showing the configuration of a crack growth prediction device according to one embodiment of the present invention; [Diagram 2] 1 is a flowchart showing an overall flow of a crack growth prediction method according to one embodiment of the present invention. [Diagram 3] 4 is a flowchart showing details of step S1 of the crack growth prediction method in one embodiment of the present invention. [Figure 4] FIG. 4 is a diagram showing processing condition information used in one embodiment of the present invention. [Diagram 5] FIG. 13 is a diagram showing the relationship between a breakdown value and a simulation step when one embodiment of the present invention is applied. [Figure 6] FIG. 13 is a diagram showing the arrangement of vectors that crack a crack surface when one embodiment of the present invention is applied. [Figure 7] FIG. 2 is a diagram for explaining a process of rolling a ring with a cylindrical main roll and a cylindrical mandrel to which one embodiment of the present invention is applied. [Figure 8] FIG. 13 is a diagram showing fracture values ​​and crack growth evaluation values ​​to which one embodiment of the present invention is applied. [Figure 9] FIG. 13 is a diagram showing the normal direction identified in the crack generation step in step S4 of one embodiment of the present invention. [Figure 10] FIG. 13 shows the normal directions identified in the simulation step following the crack initiation step in step S5 of one embodiment of the present invention. [Figure 11] FIG. 11 illustrates the normal directions identified in the next simulation step of FIG. 10 in step S5 of one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In this embodiment, a process in a simulation of plastic processing of a workpiece (plastic processing simulation) will be described. Here, a crack in this embodiment refers to a defect that progresses over time, such as a crack, a split, a tear, a fracture, or a breakage. Furthermore, progress refers to a state in a crack that changes over time, regardless of whether it is expressed as "progress" or "advancement," and may include the amount of progress or direction of progress, which indicates the size or length, as well as the shape. <System configuration> First, FIG. 1 shows the configuration of a crack growth prediction device 100 for predicting crack growth in this embodiment. The crack growth prediction device 100 can be realized by a so-called computer. For this reason, the crack growth prediction device 100 has a processing unit 1100 that can be realized by an arithmetic device such as a CPU. The processing unit 1100 executes various calculations according to a plastic processing simulation program 1210 stored in a memory 1200. The contents of this will be described later. In addition, the plastic processing simulation program 1210 can be distributed via a network (not shown) or stored in the crack growth prediction device 100 via a storage medium that stores the program. In addition, the plastic processing simulation program 1210 is, for example, a set of a solver program and a post-processor program. However, the plastic processing simulation program 1210 may be another program, and may be a set of other programs such as a pre-processor program. In addition, since the plastic processing simulation program is used in this embodiment for the purpose of predicting the growth of a crack, it may be called a crack growth prediction program.

[0013] The crack growth prediction device 100 also has an output unit 1300 that provides information to a user. This can be realized by a display monitor or the like. The crack growth prediction device 100 also has an input unit 1400 that accepts operations from a user. This can be realized by a pointing device such as a keyboard or a mouse. Here, the output unit 1300 and the input unit 1400 may be realized by a terminal device in a separate housing from the crack growth prediction device 100. In this case, the terminal device can be realized by a tablet, a smartphone, or the like in addition to a PC.

[0014] Furthermore, the crack growth prediction device 100 includes a storage device that stores various information. The storage device stores workpiece material property information 1001, processing condition information 1002, and simulation result information 1003. The contents of these will be described later. The storage device may be realized by a file system in a separate housing from the crack growth prediction device 100.

[0015] In this embodiment, the crack growth prediction device 100 is described as a computer that executes processing according to software. However, the entire software or a part of it may be realized by hardware such as a dedicated circuit or an FPGA (Field Programmable Gate Array). <Crack growth prediction method> Fig. 2 is a flowchart showing the overall process of the crack growth prediction method for predicting crack growth according to this embodiment. The crack growth prediction method will be described below with reference to Fig. 2. Note that, in this case, the subject of each process is described as a processing unit 1100, but this is processing according to the plastic processing simulation program 1210 as described above.

[0016] In the following, first, an overview of the entire flowchart in Fig. 2 will be described, and then each step will be described in detail. In step S1, the processing unit 1100 starts a plastic processing simulation that reproduces a predetermined processing method. To this end, the processing unit 1100 accepts a simulation instruction input by a user via the input unit 1400. Then, the processing unit 1100 calculates a fracture value of the processed material included in the simulation instruction.

[0017] Next, in step S2, the processing unit 1100 identifies as candidate positions material points (positions) where the fracture value calculated in step S1 exceeds a preset threshold value in the final step of the plastic processing simulation. Then, the processing unit 1100 determines, from among these identified candidate positions, a candidate position selected by the user via the input unit 1400 as the crack occurrence position. Note that the processing unit 1100 may identify one candidate position and determine this as the crack occurrence position.

[0018] Next, in step S3, the processing unit 1100 identifies, as a crack occurrence step, the simulation step in which the fracture value exceeds the threshold value for the first time at the crack occurrence position determined in step S2.

[0019] Next, in step S4, the processing unit 1100 identifies the normal direction in which the crack occurred in the crack occurrence step at the crack occurrence position. This normal direction is the normal direction to the crack surface, and can be realized by identifying the crack normal vector (the same applies below).

[0020] Next, in step S5, the processing unit 1100 specifies the normal direction of the crack in each simulation step after the crack generation step. That is, the processing unit 1100 specifies the normal direction of the crack in each simulation step after the simulation step in which the fracture value exceeds the threshold value for the first time. This makes it possible to predict the crack in the workpiece.

[0021] Then, in step S6, the processing unit 1100 calculates an evaluation value of crack growth for the workpiece using the processing results up to step S6. This evaluation value is a parameter that indicates the degree of crack growth, and is correlated with the depth of crack growth. The calculation of the evaluation value in step S6 may be omitted. This completes the explanation of the entire crack growth prediction method. Below, each step in the crack growth prediction method will be explained in detail. Each step will be explained in detail in the following order. First, step S1 will be explained in detail using FIG. 3. Next, steps S2 to S6 will be explained in detail. <<Step S1: Breakdown value calculation process>> In step S1, the processing unit 1100 calculates a fracture value in the workpiece according to the flowchart showing the details of step S1 of the crack growth prediction method in this embodiment shown in Fig. 3. This fracture value is an evaluation index for crack generation. Therefore, by using this fracture value, it is possible to determine whether or not a crack will occur.

[0022] First, in step S1001, the processing unit 1100 reads the shape of the workpiece before processing and the die shape included in the simulation instruction from the workpiece characteristic information 1001. For example, if the processing is rolling, the roll shape is read as the die shape. Thus, in this step, the processing unit 1100 reads information indicating the processing characteristics of the workpiece.

[0023] Next, in step S1002, the processing unit 1100 reads the stress-strain curve and thermal properties of the workpiece from the workpiece characteristic information 1001. For example, the thermal properties may be the density, thermal conductivity, emissivity, etc. of the workpiece. Thus, in this step, the processing unit 1100 reads information indicating the characteristics of the workpiece itself. Furthermore, the workpiece characteristic information 1001 includes information indicating the processing characteristics of the workpiece and information indicating the characteristics of the workpiece itself.

[0024] Next, in step S1003, the processing unit 1100 reads a crack growth prediction model from the workpiece material property information 1001. The information on this crack growth prediction model includes a calculation formula for a fracture value C that is an index for evaluating the occurrence of a crack, a threshold value C0 that is a threshold value of an index used in determining the occurrence of a crack, and a calculation formula for crack growth.

[0025] Next, in step S1004, the processing unit 1100 reads the processing conditions of the workpiece from the processing condition information 1002. This processing condition information 1002 is shown in FIG. 4. As shown in FIG. 4, the processing conditions can include the heating temperature of the workpiece, the time from when the workpiece is removed from the heating furnace to when it is placed in the processing machine, the reduction speed during processing, the reduction amount, and the like. Also, if the processing is rolling, the number of rotations of the rolls can be used. Note that in this embodiment, at least one of these can be used as the processing condition.

[0026] Next, in step S1005, the processing unit 1100 divides the shape of the workpiece and the shape of the die read in step S1001 into elements of the finite element method.

[0027] Next, in step S1006, the processing unit 1100 divides the processing time into a plurality of time segments, that is, into each simulation step in the plastic processing simulation.

[0028] Next, in step S1007, the processing unit 1100 calculates state information (more specifically, state information of elements in the finite element method obtained by the plastic processing simulation) in each simulation step i divided in step S1006 by the finite element method based on each piece of information read in steps S1001 to 1005. As the state information, for example, the maximum principal stress σ_max, the von Mises equivalent stress σ_eff, the equivalent plastic strain ε, and the stress component σ are calculated. Note that examples of the stress component σ include σ_xx, σ_yy, σ_zz, σ_xy, σ_yz, and σ_xz. Then, the processing unit 1100 stores the resultant state information in the storage device or memory 1200.

[0029] Next, in step S1008, the processing unit 1100 calculates C(i), the fracture value at each simulation step i divided in step S1006. To do this, the processing unit 1100 applies the state information of each simulation step i to the crack propagation prediction model read in step S1003 for calculation. Further, the processing unit 1100 calculates this fracture value C(i) for each element in the finite element method. Then, the processing unit 1100 records the calculated fracture value C(i) in the memory 1200. Thus, the processing of step S1 ends. <<Step S2: Process of determining crack generation position>> In step S2, the processing unit 1100 identifies C(n), the fracture value of each element at the final simulation step of the plastic working simulation, from each fracture value C(i) calculated in step S1. Then, the processing unit 1100 compares the fracture value C(n) with a threshold value C0 set in advance in the storage device. As a result, the position indicating the fracture value C(n) equal to or greater than the threshold value C0 is identified as a candidate position. Then, the output unit 1300 outputs this candidate position and the corresponding fracture value C(n). The processing unit 1100 determines, as the crack generation position, one or more candidate positions specified by the user via the input unit 1400 in response to this output. As described above, the processing unit 1100 may automatically determine the crack generation position.

[0030] As a result, it is desirable for the processing unit 1100 to record the determined crack generation position in the memory 1200. Note that the crack generation position in the present embodiment indicates the element itself of the finite element method, the position within the element, or the contact point on the interface between elements, where the crack occurs, that is, the fracture value C(n) is equal to or greater than the threshold value C0. <<S3: Process of specifying crack generation step>> In step S3, the processing unit 1100 advances the plastic working simulation and obtains the relationship between C(i), the fracture value at the crack generation position determined in step S2, and each simulation step i divided in step S1006. As a result, the processing unit 1100 obtains the relationship between the fracture value and the simulation step shown in FIG. 5.

[0031] Then, the processing unit 1100 identifies the simulation step i at which the fracture value C(i) at the crack generation position first becomes equal to or greater than the threshold value C0. That is, the processing unit 1100 identifies the simulation step i that satisfies the relationships of (Equation 1) and (Equation 2). Note that the fracture value C(i) has the property of monotonically increasing in accordance with the passage of time, that is, the progress of the simulation step.

[0032]

Equation

[0033]

Equation

[0034] <<S4: Step for Identifying the Normal Direction of the Crack at the Crack Generation Step>> Next, step S4 will be described with reference to FIG. 9 as well. FIG. 9 is a diagram showing the normal direction specified in the crack generation step in step S4. Among FIGS. 9, (a) schematically shows the workpiece as a cube, and is composed of each element (shown in FIG. 9(a) as a region separated by a solid line that divides the cube; the same applies hereinafter). Note that in FIG. 9(a), there are 25 elements exposed on the front of the paper surface. Among these, taking cross-section A as an example, that is, using (b), the identification of the normal direction in the crack generation step will be described.

[0035] First, in step S4, the processing unit 1100 uses the state information regarding the crack generation position at the crack generation position determined in step S2 to identify the crack normal vector N0 at the simulation step at which the fracture value C(i) first becomes equal to or greater than the threshold value C0. In the present embodiment, the case where the crack occurs perpendicular to the maximum principal stress direction is taken as an example to identify the crack normal vector N0. Note that the crack normal vector N0 is also referred to as the crack generation normal vector.

[0036] In the example shown in FIG. 9(b), the simulation step i=10 is the crack occurrence step. Also, it is assumed that the crack occurrence position determined in step S2 is located at the upper center of cross section A. Furthermore, tension (stress), which is the cause of crack occurrence, is applied to cross section A. Therefore, at the crack occurrence position, maximum principal stress corresponding to the tension occurs in opposite directions. Note that the coordinate axes in FIG. 9(b) are as shown. Using state information regarding the crack including this maximum stress, the processing unit 1100 identifies the crack normal vector N0 at the crack occurrence step shown in FIG. 9(b).

[0037] Then, the processing unit 1100 records the crack normal vector N0 in the memory 1200. Note that, although an example is shown here assuming that the crack occurs perpendicular to the maximum principal stress direction, if there is another method for determining the crack initiation normal direction of the crack surface in the crack initiation step, that method may be used. In this way, the processing unit 1100 can specify the normal direction of the crack in the crack initiation step.

[0038] Then, the processing unit 1100 can identify the crack in-plane vector U0 and the crack in-plane vector V0 that define the crack normal vector N0 from the crack normal vector N0. Here, in this embodiment, the identification of the crack in-plane vector U0 and the crack in-plane vector V0 is performed in step S5. In FIG. 9(b), the crack in-plane vector U0 is oriented perpendicular to the plane of the drawing.

[0039] In this embodiment, the crack in-plane vector V0 is a vector whose end point is another adjacent element as shown in the figure. However, the end point is not limited to another element, and may be within the same element as the starting point.

[0040] In the examples of Figures 9 to 11, for the sake of simplicity, the crack in-plane vector U0 is perpendicular to the paper surface of the drawing, and is omitted in Figures 10 and 11. Various methods for identifying the crack in-plane vector U0 and the crack in-plane vector V0 can be assumed, and an example of such a method will be described in the detailed description of step S5. <<Calculation Process of Normal Direction of Crack after Crack Generation Step S5>> In step S5, the normal direction of the crack after crack generation at the crack generation position is obtained. First, the processing unit 1100 identifies an in-plane crack vector U0 and an in-plane crack vector V0 that are perpendicular to the crack normal vector N0 identified in step S4 and have different directions from each other. For this purpose, an example of this is shown in FIG. 6. Here, since the starting points of the vectors U0 and V0 are at the crack generation position, the crack plane can be defined by the starting and ending points of the in-plane crack vector U0 and the in-plane crack vector V0.

[0041] Here, the method for identifying these in-plane crack vectors U0 and in-plane crack vectors V0 will be described. By determining the in-plane crack vector U0 and the in-plane crack vector V0 such that the processing unit 1100 satisfies the relationship of (Equation 3), it is perpendicular to the crack normal vector N0 and is not in the same direction (including not being in the 180-degree opposite direction), so it can be used as a vector that defines the crack plane. That is, the crack normal vector N0 can be defined as the cross product of the in-plane crack vector U0 and the in-plane crack vector V0.

[0042]

Equation

[0043] In addition, the in-plane crack vector U0 and the in-plane crack vector V0 also need to satisfy the following (Equation 4) and (Equation 5).

[0044]

Equation

[0045]

Equation

[0046] Here, although there are an infinite number of solutions for (Equation 4) and (Equation 5), the processing unit 1100 can identify a solution that uniquely indicates the crack in-plane vector U0 and the crack in-plane vector V0 by establishing rules for how to determine the crack in-plane vector U0 and the crack in-plane vector V0. In this embodiment, the processing unit 1100 sets the rules shown in the following (Equation 6) to (Equation 8).

[0047]

number

[0048]

number

[0049]

number

[0050] Note that N0x, N0y, and N0z are the x-, y-, and z-components of the crack normal vector N0, and U0x, U0y, and U0z are the x-, y-, and z-components of the crack in-plane vector U0, respectively. Here, the processing unit 1100 calculates the x-, y-, and z-components of the crack in-plane vector U0 using Equations 6 to 8.

[0051] Then, the processing unit 1100 uses the crack normal vector N0 as a rotation axis and repeatedly rotates the vector U0 by the angle θ to obtain a vector that is perpendicular to the crack normal vector N0 and does not have the same direction as the vector U0. In this way, the processing unit 1100 can obtain candidates for the crack in-plane vector U0 and the crack in-plane vector V0. The angle θ can be set as an input condition, and can be input via the input unit 1400 and recorded in the memory 1200 when reading the crack growth prediction model in step S1003, for example. In addition, when determining the crack in-plane vector U0 and the crack in-plane vector V0, other examples may be used as long as the relationship shown in (Equation 3) is satisfied.

[0052] Furthermore, the end points of the crack in-plane vector U0 and the crack in-plane vector V0 define the crack surface in each simulation step from the crack generation step to the final step of the plastic processing simulation. For this reason, it is necessary to set positions inside the workpiece as the end points. Therefore, the processing unit 1100 judges whether the candidate end points of the crack in-plane vector U0 and the crack in-plane vector V0 are points inside the workpiece. Then, the processing unit 1100 selects two candidate positions inside the workpiece from among the candidate end points. In other words, the processing unit 1100 specifies one end point each for the crack in-plane vector U0 and the crack in-plane vector V0.

[0053] Furthermore, the processing unit 1100 may select the candidate end points by, for example, selecting the candidate end points in ascending order of distance from the start point.

[0054] Since the direction of the crack normal vector N0 depends on the magnitude of the crack in-plane vector U0 and the in-plane vector V0, it is preferable that the processing unit 1100 sets these to a predetermined magnitude, which are set in advance. That is, the processing unit 1100 uses the magnitudes du and dv of the crack in-plane vector U0 and the crack in-plane vector V0 as input conditions. Then, the processing unit 1100, which is recorded in advance in the memory 1200, calculates the crack in-plane vector U0 and the crack in-plane vector V0 so that they are the same magnitude as the input conditions du and dv. In the following description, each vector and position in the crack generation step may be called with the word "initial". For example, they may be called the initial crack in-plane vectors U0 and V0, and the initial crack normal vector N0.

[0055] Next, the processing unit 1100 identifies the crack in-plane vector U(i) and the crack in-plane vector V(i) in each simulation step from the crack generation step to the final step of the plastic processing simulation. The identification is performed by identifying the positions after displacement of the end points of the initial crack in-plane vectors U0 and V0 in each simulation step, and calculating the crack in-plane vector whose end point is the position after the displacement. The displacement of the end point position is obtained by utilizing the fact that in the plastic processing simulation by the finite element method, the deformation and displacement of each element are calculated for each simulation step.

[0056] Then, the processing unit 1100 uses these to identify the normal vector N(i) of the crack surface in each simulation step by (Equation 9), and records it in the memory 1200.

[0057]

number

[0058] Here, a specific example of specifying the crack in-plane vector U(i) and the crack in-plane vector V(i) will be described with reference to Figures 10 and 11. Figure 10 is a diagram showing the normal direction specified in the simulation step (i=11) following the crack generation step in step S5.

[0059] In the simulation step (i=11), cross section A is deformed by tension. The processing unit 1100 then identifies a crack in-plane vector U (i=11) and a crack in-plane vector V (i=11) in accordance with the deformation of cross section A. In other words, cross section A is crushed in the vertical direction on the drawing from FIG. 9 to FIG. 10. Therefore, the processing unit 1100 identifies a crack in-plane vector V whose end point is a position displaced by the deformation amount of the crack in-plane vector V0. Note that the processing unit 1100 identifies the end point of the crack in-plane vector U (i=11) as being the same as the end point of the crack in-plane vector U0, since the crack in-plane vector U0 is in a direction that is not affected by tension.

[0060] In this way, in step S5, the processing unit 1100 identifies the end point of the crack in-plane vector according to the cause of the crack such as tension, and uses this to identify the crack surface or the crack normal vector N(i). Note that this identification of the crack surface or the crack normal vector N(i) is merely an example, and is not limited to this.

[0061] Then, the processing unit 1100 applies the crack in-plane vector V(i=11) and the crack in-plane vector U(i=11) to the equation 9 to identify the crack normal vector N(i=11). In this way, the processing unit 1100 can identify the propagation direction of the crack. This crack normal vector N(i=11) is in the direction shown in FIG. 10.

[0062] Furthermore, the processing unit 1100 calculates the amount of crack growth by using (Equation 10) and (Equation 11).

[0063]

number

[0064]

number

[0065] As a result, the processing unit 1100 can predict that the crack has progressed to the crack progress tip indicating the tip of the crack progress direction by the progress amount indicated by D (i=11) in FIG.

[0066] Note that (Equation 10) and (Equation 11) are merely examples, and other equations or other conditions may be used.

[0067] Subsequently, the above processing is executed in each simulation step. FIG. 11 is a diagram showing the normal direction identified in the simulation step following FIG. 10. In FIG. 11, the cross section A is further crushed than the cross section shown in FIG. 10 due to tension. Therefore, the processing unit 1100 identifies the crack in-plane vector V(i=12) that is more horizontal (parallel) on the figure than the crack in-plane vector V(i=11) in response to this deformation. As a result, the processing unit 1100 identifies the normal vector N(i=12) that is more downward on the figure than the normal vector N(i=11). In addition, the processing unit 1100 identifies the crack advance destination in the simulation step i=12 as a position advanced from i=11 as shown in the figure.

[0068] Thus, in this embodiment, in steps S4 and S5, the processing unit 1100 executes the following processes. (1) In the crack initiation step, identify the normal vector N0 from the state information. (2) From this normal vector N0, identify the crack in-plane vector U0 and the crack in-plane vector V0. (3) The crack in-plane vector U(i) and crack in-plane vector V(i) in the next simulation step are determined from the crack in-plane vector U0 and crack in-plane vector V0, taking into account deformation and displacement due to factors such as tension. (4) Next, identify the normal vector N(i) from the crack in-plane vector U(i) and the crack in-plane vector V(i) at each simulation step. (5) (3) and (4) are repeated for each simulation step to continuously and propagate the normal vectors of each simulation step. Moreover, as described above, the processing unit 1100 calculates the crack normal vector in each simulation step from the crack generation step to the final step of the plastic processing simulation using the start point and end point of the crack in-plane vector U0 and the crack in-plane vector V0. Then, the processing unit 1100 records this in the memory 1200. Note that the processing unit 1100 may calculate the start points of the crack in-plane vector Ui and the crack in-plane vector Vi in each simulation step, or may reuse the start points of the crack in-plane vector U0 and the crack in-plane vector V0. Furthermore, in this embodiment, the end points of the crack in-plane vector U0 and the crack in-plane vector V0 are set to be within a different element from the start points, but they may be within the same element.

[0069] In addition, in step S4, the processing unit 1100 can also identify the local deformation and rotation of the workpiece in the vicinity of the crack initiation position by, for example, the deformation gradient tensor or the displacement gradient tensor of continuum mechanics. This allows the processing unit 1100 to identify the normal direction of the crack after the crack initiation step, that is, the crack normal vector N(i), in step S5.

[0070] For example, the deformation gradient tensor when the shape of the workpiece in simulation step i=1 is set as the reference arrangement and the shape of the workpiece in simulation step i=2 is set as the current arrangement is set as F, and the tensor obtained by transposing the deformation gradient tensor and taking the inverse matrix is ​​set as F^(-T). At this time, the crack normal vector N(i=2) at i=2 can be expressed by applying F^(-T) to the crack normal vector N(i=1) at i=1. Specifically, the processing unit 1100 identifies the normal vector N(i=2) using the history of the following fracture condition formula (Equation 12).

[0071]

number

[0072] In the present embodiment, although the parameter related to time is defined in the simulation step (i), time or time (t) may also be used. <<S6: Calculation Step of Evaluation Value of Crack Propagation>> In step S6, the processing unit 1100 obtains a unit normal vector from the normal vector N(i) of the crack at each simulation step up to the final step of the plastic working simulation at the crack generation position. Then, the processing unit 1100 calculates the stress vector acting on the crack surface from the stress components σ_xx, σ_yy, σ_zz, σ_xy, σ_yz, σ_xz at the crack generation position and the unit normal vector. Then, using the crack propagation calculation formula read in step S1003, the evaluation value of crack propagation is calculated. It is desirable that the processing unit 1100 records the evaluation value in the memory 1200. Then, it is desirable that the processing unit 1100 records the results of each step (process) including the evaluation value as simulation result information 1003. Further, it is desirable that the output unit 1300 outputs the simulation result information 1003. <Verification Example> The present embodiment is applicable to ring rolling. Among these, in the hot ring rolling process, an example of applying the present embodiment to a Ni-based alloy in which cracks are relatively likely to occur is shown.

[0073] After heating a rectangular workpiece 1 made of Ni-based alloy to 900 °C, the occurrence of cracks was determined by plastic working simulation of the process of rolling a ring with the cylindrical main roll 2 and the cylindrical mandrel 3 shown in FIG. 7. The dimensions of the workpiece 1 are an inner diameter of 450 mm, an outer diameter of 600 mm, and a height of 500 mm.

[0074] Here, the following (Equation 13) to (Equation 18) were used as the calculation formula for the fracture value C and the calculation formula for crack propagation, respectively. Here, the threshold value C0 is equal to 1, and when the fracture value C exceeds 1, it is determined that a crack has occurred. This determination can be executed by the processing unit 1100 of the crack propagation prediction device 100 of the present embodiment.

[0075]

Equation

[0076]

number

[0077]

number

[0078] where Cc is the temperature-dependent characteristic threshold.

[0079]

number

[0080]

number

[0081]

number

[0082] Here, σ_c is the normal stress component acting on the crack surface.

[0083] In the final step of the simulation, point P1 on the inside corner of the upper end face of the ring was selected from the points where the fracture value C exceeded the threshold value C0, and crack growth was evaluated at P1. Figure 8 shows the history of fracture value C and crack growth evaluation value at P1. It was confirmed that the evaluation value of crack growth could be calculated after the time when the fracture value exceeded the threshold, and crack growth could be easily predicted without modifying the finite element model.

[0084] The present invention is not limited to the above-described embodiment, and includes various modified examples. For example, the above-described embodiment has been described in detail to easily explain the present invention, and is not necessarily limited to an embodiment having all of the configurations described. In addition, it is possible to replace a part of a certain configuration of the present embodiment with another configuration. It is also possible to add another configuration to the configuration of the present embodiment. In other words, it is possible to add, delete, or replace a part of the configuration of the present embodiment with another configuration.

[0085] According to one embodiment of the present invention, the crack normal direction at the time of crack occurrence is identified and the coordinates of the vector defining the crack surface at that time are recorded, making it possible to track the normal direction of the crack surface after crack occurrence and evaluate the crack progression. [Explanation of symbols]

[0086] 1 Workpiece, 2 Main roll, 3 Mandrel, 100 Crack growth prediction device, 1100 Processing section, 1200 Memory, 1210 Plastic processing simulation program, 1300 Output section, 1400 Input section, 1001 Workpiece characteristic information, 1002 Processing condition information, 1003 Simulation result information

Claims

1. A method for predicting the progress of a crack that occurs in a workpiece during plastic processing, comprising: Simulation of the plastic processing for the above-mentioned plastic processing: Determining the occurrence of cracks in the workpiece; Identifying a crack occurrence position where the crack has occurred; After the plastic processing simulation: Identifying a crack initiation step in the plastic processing simulation in which a crack occurs at the identified crack initiation position; Identifying an initial crack initiation normal vector indicating a normal direction of the crack at the crack initiation step and the crack initiation position; predicting the growth of the crack by identifying a crack normal vector in a simulation step after the crack generation step based on the initial crack generation normal vector; Crack growth prediction method.

2. The crack growth prediction method according to claim 1, The crack initiation step is identified based on a history of a fracture condition formula. Crack growth prediction method.

3. The crack growth prediction method according to claim 1, With respect to the crack generating step: Identifying the initial crack initiation normal vector using state information on the crack initiation position obtained by the plastic processing simulation; Identifying multiple in-plane vectors of the initial crack that satisfy all of the following requirements: is perpendicular to the crack initiation normal vector, The crack initiation position is the starting point, and the end point is within the workpiece, Each is in a different direction, Crack growth prediction method.

4. The crack growth prediction method according to claim 3, For each simulation step after the crack initiation step: Identifying a position after displacement of an end point of the initial crack in-plane vector in the simulation step; Identifying a crack in-plane vector whose end point is the position after the displacement; Identifying a crack normal vector based on the crack in-plane vector; A prediction of the growth of the crack is performed based on the crack normal vector. Crack growth prediction method.

5. The crack growth prediction method according to claim 3, In the plastic processing simulation, the workpiece is divided into a plurality of elements using a wire element method; A method for predicting crack growth during plastic processing, wherein the end points and start points of the multiple initial crack in-plane vectors are within the same element.

6. The crack growth prediction method according to claim 3, A method for predicting crack propagation during plastic processing, in which a pre-specified crack in-plane vector is repeatedly rotated a predetermined angle around the crack initiation normal vector as a rotation axis, thereby specifying the multiple candidate positions.

7. A crack growth prediction program that causes a computer to execute the crack growth prediction method according to any one of claims 1 to 6.

8. A crack growth prediction device having a processing unit and a memory storing a plastic processing simulation program, which predicts the growth of a crack that occurs in a workpiece during plastic processing, The processing unit executes the plastic working simulation program to: Simulation of the plastic processing for the above-mentioned plastic processing: Determining the occurrence of cracks in the workpiece; Identifying a crack occurrence position where the crack has occurred; After the plastic processing simulation: Identifying a crack occurrence step in the plastic processing simulation in which a crack occurs at the identified crack occurrence position; Identifying an initial crack initiation normal vector indicating a normal direction of the crack at the crack initiation step and the crack initiation position; predicting the growth of the crack by identifying a crack normal vector in a simulation step after the crack generation step based on the initial crack generation normal vector; Crack growth prediction device.

9. 9. The crack growth prediction device according to claim 8, The processing unit identifies the crack occurrence step based on a history of a fracture condition equation. Crack growth prediction device.

10. 9. The crack growth prediction device according to claim 8, The processing unit, in relation to the crack generating step, Identifying the initial crack initiation normal vector using state information on the crack initiation position obtained by the plastic processing simulation; Identifying multiple in-plane vectors of the initial crack that satisfy all of the following requirements: is perpendicular to the crack initiation normal vector, The crack initiation position is the starting point, and the end point is within the workpiece, Each is in a different direction, Crack growth prediction device.

11. The crack growth prediction device according to claim 10, The processing unit, for each simulation step after the crack initiation step, Identifying a position after displacement of an end point of the initial crack in-plane vector in the simulation step; Identifying a crack in-plane vector whose end point is the position after the displacement; Identifying a crack normal vector based on the crack in-plane vector; A prediction of the growth of the crack is performed based on the crack normal vector. Crack growth prediction device.

12. The crack growth prediction device according to claim 10, The processing unit includes: In the plastic processing simulation, the workpiece is divided into a plurality of elements using a wire element method; A crack propagation prediction device in plastic processing, wherein the end point and start point of the multiple initial crack in-plane vectors are within the same element.

13. The crack growth prediction device according to claim 10, The processing unit includes: A crack propagation prediction device for plastic processing that identifies the multiple candidate positions by repeatedly rotating a pre-specified crack in-plane vector by a specified angle around the crack initiation normal vector as a rotation axis.

Citation Information

Patent Citations

  • Bilinear adaptive phase field method for simulating brittle material damage

    CN112036060A

  • Method for predicting crack development of elasto-plastic body and deformation predicting method

    JP2004069638A

  • Crack progress prediction method

    JP2008216184A

  • Information processing apparatus, information processing method, and program

    JP2015111098A