Solid-state secondary battery manufacturing equipment
The multi-chamber manufacturing apparatus addresses inefficiencies in solid-state secondary battery production by automating the process and maintaining vacuum conditions, resulting in high-yield, cost-effective batteries with minimal impurity exposure.
Patent Information
- Application Number
- JP2021517128
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-04-30
- Filing Date
- 2020-04-16
- Publication Date
- 2024-10-24
- Estimated Expiration
- 2040-04-16
AI Technical Summary
Existing manufacturing methods for solid-state secondary batteries are inefficient, lack automation, and expose the batteries to the atmosphere, leading to impurity mixing and increased costs.
A multi-chamber manufacturing apparatus with precise control of vacuum levels and sputtering techniques forms solid-state secondary batteries without atmospheric exposure, using the same targets for conductive layers to reduce costs and improve yield.
The apparatus enables high-yield, automated production of solid-state secondary batteries with improved characteristics by minimizing impurity exposure, reducing manufacturing costs, and ensuring efficient film formation.
Smart Images

Figure 0007572949000001 
Figure 0007572949000002 
Figure 0007572949000003
Abstract
Description
[Technical Field]
[0001] One aspect of the present invention relates to an object, a method, or a manufacturing method. Alternatively, the present invention relates to a process, a machine, a manufacture, or a composition of matter. One aspect of the present invention relates to a semiconductor device, a display device, a light-emitting device, a power storage device, a lighting device, an electronic device, or a manufacturing method thereof. In particular, the present invention relates to a manufacturing method and manufacturing apparatus for a power storage device.
[0002] In this specification, the term "electronic device" refers to any device having a power storage device, and includes electro-optical devices having a power storage device, information terminal devices having a power storage device, and the like. [Background technology]
[0003] 2. Description of the Related Art Electronic devices that are carried by users or worn by users have been actively developed.
[0004] Electronic devices carried by users or worn by users operate using primary or secondary batteries, which are examples of power storage devices, as their power source. It is desirable for electronic devices carried by users to be used for long periods of time, and for this reason, large-capacity secondary batteries are used. However, incorporating a large-capacity secondary battery into an electronic device poses the problem of its large size and weight. Therefore, development is underway to develop small or thin, large-capacity secondary batteries that can be incorporated into portable electronic devices.
[0005] Lithium-ion secondary batteries, which use an electrolyte such as an organic solvent as a medium for transporting lithium ions, the carrier ions, are widely used. However, secondary batteries using a liquid have problems such as the decomposition reaction of the electrolyte depending on the operating temperature range and operating potential, and leakage to the outside of the secondary battery. In addition, secondary batteries using an electrolyte have a risk of fire due to leakage.
[0006] Fuel cells are a type of secondary battery that does not use liquid, but they are devices that use precious metals for the electrodes and the solid electrolyte material is also expensive.
[0007] Furthermore, a power storage device called a solid-state battery that uses a solid electrolyte as a secondary battery that does not use a liquid is known. For example, Patent Document 1 discloses such a device.
[0008] Patent Document 1 describes an example in which a lithium cobalt oxide film is formed on a positive electrode current collector by sputtering. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] U.S. Patent No. 8,404,001 Summary of the Invention [Problem to be solved by the invention]
[0010] The present invention aims to realize a manufacturing device capable of fully automating the production of solid-state secondary batteries. Another object is to realize a manufacturing device capable of producing solid-state secondary batteries in a short time. Another object is to realize a manufacturing device capable of producing solid-state secondary batteries with a high yield.
[0011] Another issue is how to fabricate solid-state secondary batteries without exposing them to the atmosphere. [Means for solving the problem]
[0012] The manufacturing apparatus disclosed in the present specification has a configuration including a mask alignment chamber, a first transfer chamber connected to the mask alignment chamber, a second transfer chamber connected to the first transfer chamber, a first film formation chamber connected to the second transfer chamber, a third transfer chamber connected to the first transfer chamber, and a second film formation chamber connected to the third transfer chamber, and the first film formation chamber forms a positive electrode active material layer or a negative electrode active material layer by a sputtering method, and the second film formation chamber forms a positive electrode active material layer or a negative electrode active material layer by a sputtering method. XA solid electrolyte layer is formed by co-evaporation with (0 < X ≤ 2), and it is a manufacturing apparatus for a solid secondary battery in which the substrate is transported without being exposed to the atmosphere between the first film formation chamber and the mask alignment chamber, and between the mask alignment chamber and the second film formation chamber.
[0013] In the above configuration, it may also be configured to have a heating chamber connected to the second transport chamber. The heating chamber is preferably maintained under a pressure lower than the atmospheric pressure (reduced pressure atmosphere) by an exhaust mechanism before and after the heat treatment. The higher the degree of vacuum, the more efficiently water adsorbed on the surface of the insulating film can be desorbed. For example, the pressure at the time of inserting the substrate inside the chamber where the heat treatment is performed is 1 × 10 -7 Pa or more and 1 × 10 -3 Pa or less, preferably 1 × 10 -6 Pa or more and 1 × 10 -4 Pa or less.
[0014] In the above configuration, a solid secondary battery having good characteristics can be produced by maintaining the cleanliness of the film formation chamber and the transport chamber.
[0015] The back pressure (total pressure) of the above-described first film formation chamber is 1 × 10 -4 Pa or less, preferably 3 × 10 -5 Pa or less, more preferably 1 × 10 -5 Pa or less. The partial pressure of gas molecules (atoms) having a mass-to-charge ratio (m / z) of 18 in the above-described first film formation chamber is 3 × 10 -5 Pa or less, preferably 1 × 10 -5 Pa or less, more preferably 3 × 10 -6 Pa or less. Also, the partial pressure of gas molecules (atoms) having an m / z of 28 in the above-described first film formation chamber is 3 × 10 -5 Pa or less, preferably 1 × 10 -5 Pa or less, more preferably 3 × 10 -6 Pa or less. Also, the partial pressure of gas molecules (atoms) having an m / z of 44 in the above-described first film formation chamber is 3 × 10 -5 Pa or less, preferably 1 × 10 -5 Pa or less, more preferably 3 × 10 -6 Pa or less.
[0016] In addition, the total pressure and partial pressure in the vacuum chamber such as the first film-forming chamber can be measured using a mass spectrometer. For example, the quadrupole mass spectrometer manufactured by ULVAC, Inc. (also referred to as Q-mass, Qulee CGM-051) may be used.
[0017] In addition, in the above configuration, the transfer chamber is evacuated from atmospheric pressure to low vacuum or medium vacuum (from several 100 Pa to about 0.1 Pa) using a vacuum pump, and the valve is switched to evacuate from medium vacuum to high vacuum or ultra-high vacuum (from 0.1 Pa to 1×10 -7 Pa) using a cryopump.
[0018] The manufacturing method is also one of the inventions disclosed in this specification. The configuration is to form a first conductive layer in contact with an insulating surface, form a negative electrode active material layer on the first conductive layer, and form a lithium organic complex and SiO X (0 < X ≤ 2) by co-evaporation on the negative electrode active material layer to form a solid electrolyte layer, form a first positive electrode active material layer on the solid electrolyte layer, form a second conductive layer in contact with the insulating surface and on the first positive electrode active material layer, form a second positive electrode active material layer on the second conductive layer, the solid electrolyte layer is in contact with the side surface of the negative electrode active material layer, the second conductive layer is in contact with a part of the side surface of the solid electrolyte layer, and the first positive electrode active material layer and the second positive electrode active material layer do not overlap. This is a method for manufacturing a solid secondary battery.
[0019] In the above manufacturing method, the first positive electrode active material layer and the second positive electrode active material layer can reduce the manufacturing cost by using the same sputtering target.
[0020] In the above manufacturing method, the first conductive layer and the second conductive layer can reduce the manufacturing cost by using the same sputtering target.
[0021] In the above structure, the organic complex of lithium is any one of a simple substance, an organic complex or a compound of an alkali metal or an alkaline earth metal, and examples thereof include Li, Li2O, etc. In particular, an organic complex of lithium is preferable, and among them, lithium 8-hydroxyquinolinate (abbreviation: Liq) is preferable because of its good characteristics. SiO X As other organic materials to be co-evaporated with (0 < X ≤ 2), dilithium phthalocyanine (lithium phthalocyanine), lithium 2-(2-pyridyl)phenolate (abbreviation: Lipp), lithium 2-(2’,2’’-bipyridin-6’-yl)phenolate (abbreviation: Libpp) can also be used.
Effects of the Invention
[0022] By manufacturing a solid secondary battery in an environment where it is not exposed to the atmosphere and is less likely to be contaminated with impurities, a solid secondary battery having good characteristics can be manufactured.
Brief Description of the Drawings
[0023] Figure 1 is a schematic top view of a manufacturing apparatus showing one aspect of the present invention. Figure 2 is a partial cross-sectional view of a manufacturing apparatus showing one aspect of the present invention. Figure 3A is a top view of a secondary battery showing one aspect of the present invention, and Figure 3B is a cross-sectional view. Figure 4A is a top view of a secondary battery during manufacturing showing one aspect of the present invention, and Figure 4B is a top view after completion. Figure 5 is a cross-sectional view showing one aspect of the present invention. Figure 6 is a manufacturing flow chart showing one aspect of the present invention. Figure 7A is a perspective view of a battery cell, and Figure 7B is a view showing an example of an electronic device. Figures 8A, 8B, and 8C are views showing an example of an electronic device.
Modes for Carrying Out the Invention
[0024] Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings. However, the present invention is not limited to the following description, and it will be readily understood by those skilled in the art that various modifications can be made to the embodiments and details. Furthermore, the present invention should not be interpreted as being limited to the description of the embodiments shown below.
[0025] (Embodiment 1) In this embodiment, an example of a multi-chamber manufacturing apparatus capable of fully automating the manufacturing process from the first electrode to the second electrode of a secondary battery is shown in FIG.
[0026] Figure 1 shows an example of a multi-chamber manufacturing apparatus equipped with gates 80, 81, 82, 83, 84, 85, 86, 87, 88, a load lock chamber 70, a mask alignment chamber 91, a first transfer chamber 71, a second transfer chamber 72, a third transfer chamber 73, multiple film formation chambers (first film formation chamber 92, second film formation chamber 74), a heating chamber 93, a second material supply chamber 94, a first material supply chamber 95, and a third material supply chamber 96.
[0027] The mask alignment chamber 91 includes at least a stage 51 and a substrate transport mechanism 52 .
[0028] The first transfer chamber 71 has a substrate cassette lifting mechanism, the second transfer chamber 72 has a substrate transfer mechanism 53, and the third transfer chamber has a substrate transfer mechanism .
[0029] The first film formation chamber 92, the second film formation chamber 74, the second material supply chamber 94, the first material supply chamber 95, the third material supply chamber 96, the mask alignment chamber 91, the first transfer chamber 71, the second transfer chamber 72, and the third transfer chamber 73 are each connected to an exhaust mechanism. As the exhaust mechanism, an appropriate exhaust device may be selected depending on the intended use of each chamber, and examples include an exhaust mechanism equipped with a pump having an adsorption means, such as a cryopump, a sputter ion pump, or a titanium sublimation pump, and an exhaust mechanism equipped with a turbomolecular pump and a cold trap.
[0030] The procedure for forming a film on a substrate is as follows: substrate 50 or a substrate cassette is placed in load lock chamber 70 and then transported to mask alignment chamber 91 by substrate transport mechanism 52. In mask alignment chamber 91, a mask to be used is picked up from a plurality of masks that have been set up in advance, and aligned with the substrate on stage 51. After alignment is complete, gate 80 is opened, and the substrate is transported to first transport chamber 71 by substrate transport mechanism 52. The substrate is transported to first transport chamber 71, and gate 81 is opened, and the substrate is transported to second transport chamber 72 by substrate transport mechanism 53.
[0031] The first film formation chamber 92, which is connected to the second transfer chamber 72 via a gate 82, is a sputtering film formation chamber. The sputtering film formation chamber is equipped with a mechanism that can switch between an RF power supply and a pulsed DC power supply to apply voltage to the sputtering target. Two or three types of sputtering targets can be set. In this embodiment, a single crystal silicon target, a sputtering target mainly composed of lithium cobalt oxide (LiCoO2), and a titanium target are installed. A substrate heating mechanism is installed in the first film formation chamber 92, and it is also possible to perform film formation while the heater temperature is kept at 700°C.
[0032] The negative electrode active material layer can be formed by sputtering using a single crystal silicon target. Also, SiO2 can be formed as a negative electrode by reactive sputtering using Ar gas and O2 gas. X A film made of titanium can be used as the negative electrode active material layer. A silicon nitride film can also be used as a sealing film by reactive sputtering using Ar gas and N2 gas. A positive electrode active material layer can also be formed by sputtering using a sputtering target whose main component is lithium cobalt oxide (LiCoO2). A conductive film that serves as a current collector can be formed by sputtering using a titanium target. A titanium nitride film can also be formed by reactive sputtering using Ar gas and N2 gas, and used as a diffusion prevention layer between the current collector layer and the active material layer.
[0033] When forming a positive electrode active material layer, the substrate is transported from the second transport chamber 72 to the first film formation chamber 92 with the mask and substrate stacked on top of each other by the substrate transport mechanism 53, and then gate 82 is closed and film formation is performed by sputtering. After film formation is completed, gates 82 and 83 are opened, the substrate is transported to the heating chamber 93, and after gate 83 is closed, heating can be performed. For the heating treatment in the heating chamber 93, an RTA (Rapid Thermal Anneal) device, a resistance heating furnace, or a microwave heating device can be used. For the RTA device, a GRTA (Gas Rapid Thermal Anneal) device or an LRTA (Lamp Rapid Thermal Anneal) device can be used. The heating treatment in the heating chamber 93 can be performed in an atmosphere of nitrogen, oxygen, a rare gas, or dry air. The heating time is from 1 minute to 24 hours.
[0034] After the film formation or heat treatment is completed, the substrate and mask are returned to the mask alignment chamber 91, and a new mask is aligned. After alignment, the substrate and mask are transferred to the first transfer chamber 71 by the substrate transfer mechanism 52. The substrate is transported by the lifting mechanism of the first transfer chamber 71, and after the gate 84 is opened, the substrate is transferred to the third transfer chamber 73 by the substrate transfer mechanism 54.
[0035] The second film formation chamber 74, which is connected to the third transfer chamber 73 via a gate 85, performs film formation by evaporation.
[0036] An example of the cross-sectional structure of the second film formation chamber 74 is shown in Figure 2. Figure 2 is a schematic cross-sectional view taken along the dotted line in Figure 1. The second film formation chamber 74 is connected to an exhaust mechanism 49, and the first material supply chamber 95 is connected to an exhaust mechanism 48. The second material supply chamber 94 is connected to an exhaust mechanism 47. The second film formation chamber 74 shown in Figure 2 is an evaporation chamber that performs evaporation using an evaporation source 56 moved from the first material supply chamber 95. Evaporation sources can be moved from multiple material supply chambers, and multiple substances can be vaporized and evaporated simultaneously to perform evaporation, i.e., co-evaporation. Figure 2 shows an evaporation source having an evaporation boat 58 that is also moved from the second material supply chamber 94.
[0037] The second film formation chamber 74 is connected to a second material supply chamber 94 via a gate 86. The second film formation chamber 74 is connected to a first material supply chamber 95 via a gate 88. The second film formation chamber 74 is connected to a third material supply chamber 96 via a gate 87. Therefore, the second film formation chamber 74 is capable of three-source co-evaporation.
[0038] In the deposition process, the substrate is placed on the substrate holder 45. The substrate holder 45 is connected to a rotation mechanism 65. Then, the first deposition material 55 is heated to a certain extent in the first material supply chamber 95, and when the deposition rate stabilizes, the gate 88 is opened and the arm 62 is extended to move the deposition source 56 to a position below the substrate. The deposition source 56 is composed of the first deposition material 55, a heater 57, and a container for storing the first deposition material 55. Similarly, the second deposition material is heated to a certain extent in the second material supply chamber 94, and when the deposition rate stabilizes, the gate 86 is opened and the arm 61 is extended to move the deposition source to a position below the substrate.
[0039] Thereafter, the shutter 68 and the deposition source shutter 69 are opened to perform co-evaporation. During the evaporation, the rotation mechanism 65 is rotated to improve the uniformity of the film thickness. After the evaporation, the substrate is transported along the same route to the mask alignment chamber 91. When the substrate is to be removed from the manufacturing equipment, it is transported from the mask alignment chamber 91 to the load lock chamber 70 and then removed.
[0040] 2 shows an example in which the substrate 50 and the mask are held by the substrate holder 45. By rotating the substrate 50 (and the mask) using a substrate rotation mechanism, the uniformity of the film formation can be improved. The substrate rotation mechanism may also serve as a substrate transport mechanism.
[0041] Furthermore, the second film formation chamber 74 may be provided with an imaging means 63 such as a CCD camera. By providing the imaging means 63, the position of the substrate 50 can be confirmed.
[0042] In the second film formation chamber 74, the thickness of the film formed on the substrate surface can be predicted based on the measurement results of the film thickness measurement mechanism 67. The film thickness measurement mechanism 67 may include, for example, a quartz oscillator.
[0043] In order to control the deposition of the vaporized deposition material, a shutter 68 that overlaps with the substrate until the evaporation rate of the deposition material stabilizes, and a deposition source shutter 69 that overlaps with the deposition source 56 and the deposition boat 58 are provided.
[0044] Although an example of a resistance heating type of evaporation source 56 is shown, an EB (Electron Beam) evaporation type may also be used. Furthermore, although a crucible is shown as an example of a container for evaporation source 56, an evaporation boat may also be used. An organic material is placed as first evaporation material 55 in the crucible heated by heater 57. Furthermore, when pellets or particulate SiO or the like are used as the evaporation material, an evaporation boat 58 is used. The evaporation boat 58 consists of three parts: a member with a concave surface, an inner lid with two holes, and an upper lid with one hole, which are stacked one on top of the other. Note that the inner lid may be removed during evaporation. When electricity is applied, the evaporation boat 58 acts as a resistor, and the evaporation boat itself heats up.
[0045] Furthermore, although the present embodiment has been described as an example of a multi-chamber system, the present invention is not particularly limited thereto, and an in-line type manufacturing apparatus may also be used.
[0046] An example of fabricating a secondary battery using the manufacturing apparatus shown in Figures 1 and 2 will be described below with reference to Figures 3A and 3B. Figure 3A is a top view of the secondary battery, and Figure 3B corresponds to a cross-sectional view taken along line AA' in Figure 3A.
[0047] 3B, a negative electrode current collector 203 is formed on a substrate 50, and a negative electrode active material layer 205, a solid electrolyte layer 202, a positive electrode active material layer 204, a positive electrode current collector 201, and a protective layer 206 are laminated in this order on the negative electrode current collector 203. The thickness of each layer is 10 nm to 10 μm, preferably 100 nm to 2 μm.
[0048] These films can be formed using metal masks. By using a common metal mask for the negative electrode current collector 203 and the negative electrode active material layer 205 and a common metal mask for the positive electrode current collector 201 and the positive electrode active material layer 204, a secondary battery can be fabricated using four different metal masks.
[0049] First, the substrate 50 is set in the load lock chamber 70 shown in Fig. 1 and transferred to the mask alignment chamber 91. In the mask alignment chamber 91, the substrate is aligned with a first metal mask. Then, the substrate is transferred to the first film formation chamber 92 via the transfer chamber 71 and the transfer chamber 72, where a titanium film serving as the negative electrode current collector 203 and a silicon film serving as the negative electrode active material layer 205 are selectively formed by sputtering.
[0050] The substrate 50 may be a substrate having an insulating surface, such as a quartz substrate, a glass substrate, or a plastic substrate. Alternatively, a semiconductor substrate having an insulating surface may be used. Circuits such as semiconductor elements may be formed on the semiconductor substrate in advance, and the semiconductor substrate may be electrically connected to a secondary battery to be formed later.
[0051] After the formation of the negative electrode current collector 203 and the negative electrode active material layer 205 is completed, the substrate is returned to the mask alignment chamber 91 and aligned with the second metal mask. Then, the substrate is transported to the second film formation chamber 74 via the transfer chamber 71 and the transfer chamber 73, where the solid electrolyte layer 202 is selectively formed by vapor deposition.
[0052] In the second film-forming chamber 74, the solid electrolyte layer 202 is formed by co-evaporating Si powder (SiO, SiO2, a mixture of SiO and SiO2, etc.) and Liq powder. Liq is an organic complex of lithium, and refers to 8-hydroxyquinolinato-lithium. Co-evaporation is performed using a resistance heating source or an electron beam evaporation source. The material is not limited to Si powder (SiO), and pellet or particulate powder may also be used.
[0053] After the formation of the solid electrolyte layer 202 is completed, the substrate is returned to the mask alignment chamber 91 and aligned with the third metal mask. Then, the substrate is transferred to the first film formation chamber 92 via the transfer chamber 71 and the transfer chamber 72, where a LiCoO film serving as the positive electrode active material layer 204 and a titanium film serving as the positive electrode current collector 201 are selectively formed by sputtering.
[0054] After the formation of the positive electrode active material layer 204 and the positive electrode current collector 201 is completed, the substrate is returned to the mask alignment chamber 91 and aligned with a fourth metal mask. Then, the substrate is transferred to the first film formation chamber 92 via the transfer chamber 71 and the transfer chamber 72, and a silicon nitride film (also referred to as a SiN film) that will become the protective layer 206 is selectively formed by sputtering using a single crystal silicon target in a nitrogen atmosphere.
[0055] 3A, a portion of the negative electrode current collector 203 is exposed to form a negative electrode terminal portion. The area other than the negative electrode terminal portion is covered with a protective layer 206. Furthermore, a portion of the positive electrode current collector 201 is exposed to form a positive electrode terminal portion. The area other than the positive electrode terminal portion is covered with a protective layer 206.
[0056] After the formation of the protective layer 206 is completed, the substrate is returned to the mask alignment chamber 91 and then transported to the load lock chamber 70, after which the substrate on which the secondary battery has been formed is taken out.
[0057] Using the manufacturing apparatus shown in FIGS. 1 and 2, the thin-film solid secondary battery shown in FIGS. 3A and 3B can be manufactured by the series of steps described above.
[0058] Furthermore, stacking solid-state secondary batteries can increase the capacity, and it is also possible to manufacture thin-film solid-state secondary batteries connected in parallel. When stacking solid-state secondary batteries, positive electrode active material layers are formed so as to be in contact with both surfaces of the positive electrode, and negative electrode active material layers are formed so as to be in contact with both surfaces of the negative electrode.
[0059] (Embodiment 2) In order to increase the output voltage of a solid secondary battery, the solid secondary batteries can be connected in series. While the example of a single-layer cell was shown in the first embodiment, the present embodiment shows an example of fabricating a solid secondary battery connected in series.
[0060] Fig. 4A shows a top view of the first solid secondary battery immediately after its formation, and Fig. 4B shows a top view of two solid secondary batteries connected in series. In Fig. 4A and Fig. 4B, the same reference numerals are used for the same parts as in Fig. 3 shown in embodiment 1.
[0061] 4A shows the state immediately after deposition of the positive electrode current collector 201. The shape of the top surface of the positive electrode current collector 201 differs from that shown in FIG. 3. The positive electrode current collector 201 shown in FIG. 4A is in contact with a portion of the side surface of the solid electrolyte layer and also with the insulating surface of the substrate. This insulating surface is also in contact with the first negative electrode.
[0062] Then, a second positive electrode active material layer is formed on a region of the positive electrode current collector 201 that does not overlap with the first positive electrode active material. Then, a second solid electrolyte layer 212 is formed, and a second negative electrode active material layer and a second negative electrode current collector 213 are formed thereon. Finally, a protective layer 206 is formed, as shown in FIG. 4B.
[0063] FIG. 4B shows a configuration in which two solid-state secondary batteries are arranged on a plane and connected in series.
[0064] A plurality of thin-film solid-state secondary batteries connected in series can also be fabricated without exposure to the atmosphere by using the manufacturing apparatus shown in FIGS.
[0065] (Embodiment 3) While an example of a single-layer cell was shown in Embodiment 1, an example of a multi-layer cell is shown in this embodiment. Figures 5 and 6 show one embodiment of a multi-layer cell of a thin-film solid secondary battery.
[0066] FIG. 5 shows an example of a cross section of a three-layer cell.
[0067] A positive electrode current collector 201 is formed on a substrate 50, and a positive electrode active material layer 204, a solid electrolyte layer 202, a negative electrode active material layer 205, and a negative electrode current collector 203 are sequentially formed on the positive electrode current collector 201 to form a first cell.
[0068] Furthermore, a second negative electrode active material layer, a second solid electrolyte layer, a second positive electrode active material layer, and a second positive electrode are sequentially formed on the negative electrode current collector 203 to form a second cell.
[0069] Furthermore, a third positive electrode active material layer, a third solid electrolyte layer, a third negative electrode active material layer, and a third negative electrode are sequentially formed on the second positive electrode layer to form a third cell.
[0070] In Figure 5, a protective layer 206 is formed last. The three-layer stack shown in Figure 5 is configured to be connected in series to increase voltage, but it can also be connected in parallel with external wiring. Also, series and parallel or series-parallel can be selected with external wiring.
[0071] It is preferable to use the same material for the solid electrolyte layer 202, the second solid electrolyte layer, and the third solid electrolyte layer, as this reduces manufacturing costs.
[0072] FIG. 6 shows an example of a manufacturing flow for obtaining the structure shown in FIG.
[0073] In Figure 6, to reduce the number of manufacturing steps, an LCO film is used as the positive electrode active material layer, and a titanium film is used as the current collector (conductive layer), with the titanium film considered to be the positive electrode. A silicon film is used as the negative electrode active material layer, and a titanium film is used as the current collector (conductive layer), with the titanium film considered to be the negative electrode. By using the titanium film as the common electrode, a three-layer stacked cell can be realized with a small configuration.
[0074] Multilayer cells of thin-film solid secondary batteries can also be produced without exposure to the atmosphere by using the production apparatus shown in FIGS.
[0075] This embodiment mode can be freely combined with Embodiment Mode 1 or 2.
[0076] (Fourth embodiment) In this embodiment, examples of electronic devices using a thin-film secondary battery will be described with reference to FIGS.
[0077] 7A is a perspective view of the appearance of a thin-film secondary battery 3001. A positive electrode lead electrode 510 electrically connected to the positive electrode of the solid secondary battery and a negative electrode lead electrode 511 electrically connected to the negative electrode are sealed with a laminate film or an insulating film so as to protrude.
[0078] 7B shows a card including an IC, which is an example of an application device using a thin-film secondary battery according to the present invention. Electric power obtained by power supply from radio waves 3005 can be charged into thin-film secondary battery 3001. An antenna, IC 3004, and thin-film secondary battery 3001 are arranged inside IC-containing card 3000. ID 3002 and photo 3003 of the worker wearing the management badge are attached to IC-containing card 3000. The power charged in thin-film secondary battery 3001 can also be used to transmit signals such as authentication signals from the antenna.
[0079] Also, an active matrix display device may be provided in place of the photograph 3003. Examples of active matrix display devices include reflective liquid crystal display devices, organic EL display devices, and electronic paper. The active matrix display device can also display images (moving or still images) and time. Power for the active matrix display device can be supplied from a thin-film secondary battery 3001.
[0080] Since a plastic substrate is used for a card including an IC, an organic EL display device using a flexible substrate is preferred.
[0081] A solar cell may be provided in place of the photo 3003. When irradiated with external light, the solar cell absorbs the light, generates electricity, and the electricity can be used to charge the thin-film secondary battery 3001.
[0082] Furthermore, thin-film secondary batteries are not limited to cards containing ICs, but can also be used as power sources for wireless sensors used in vehicles, secondary batteries for MEMS devices, and the like.
[0083] Figure 8A shows an example of a wearable device. The wearable device uses a secondary battery as a power source. To improve water resistance for everyday use or outdoor use, there is a demand for wearable devices that can be charged wirelessly as well as via wired charging, with the connector exposed.
[0084] For example, a secondary battery can be mounted on a glasses-type device 400 as shown in FIG. 8A. The glasses-type device 400 has a frame 400a and a display unit 400b. By mounting a secondary battery on the temples of the curved frame 400a, the glasses-type device 400 can be made lightweight, have a good weight balance, and have a long continuous use time. The thin-film secondary battery shown in embodiment 1 may also be provided, thereby realizing a configuration that can accommodate space savings associated with a smaller housing.
[0085] Furthermore, a secondary battery can be mounted in headset type device 401. Headset type device 401 has at least microphone unit 401a, flexible pipe 401b, and earphone unit 401c. A secondary battery can be provided in flexible pipe 401b or earphone unit 401c. The thin-film secondary battery shown in embodiment 1 may also be provided, making it possible to realize a configuration that can accommodate space savings associated with a smaller housing.
[0086] Furthermore, a secondary battery can be mounted on device 402 that can be directly attached to the body. Secondary battery 402b can be provided in thin housing 402a of device 402. The thin-film secondary battery described in Embodiment 1 may be provided, and a configuration that can accommodate space saving due to miniaturization of the housing can be realized.
[0087] Furthermore, a secondary battery can be mounted on device 403 that can be attached to clothing. Secondary battery 403b can be provided in thin housing 403a of device 403. The thin-film secondary battery shown in Embodiment 1 may be provided, and a configuration that can accommodate space saving due to miniaturization of the housing can be realized.
[0088] Furthermore, a secondary battery can be mounted on the belt type device 406. The belt type device 406 has a belt portion 406a and a wireless power receiving portion 406b, and a secondary battery can be mounted inside the belt portion 406a. The belt type device 406 may be provided with the thin-film secondary battery described in Embodiment 1, and a configuration that can accommodate space saving due to the miniaturization of the housing can be realized.
[0089] Furthermore, a secondary battery can be mounted on the wristwatch device 405. The wristwatch device 405 has a display portion 405a and a belt portion 405b, and a secondary battery can be provided on the display portion 405a or the belt portion 405b. The thin-film secondary battery described in Embodiment 1 may be provided, and a configuration that can accommodate space saving due to miniaturization of the housing can be realized.
[0090] The display unit 405a can display not only the time but also various other information such as incoming emails and phone calls.
[0091] Furthermore, since the wristwatch device 405 is a wearable device that is worn directly on the wrist, it may be equipped with sensors that measure the user's pulse, blood pressure, etc. Data on the user's exercise volume and health can be accumulated and used to help maintain health.
[0092] A detailed description of the wristwatch type device 405 shown in FIG. 8A will be given below.
[0093] FIG. 8B shows a perspective view of the wristwatch type device 405.
[0094] 8C shows a side view of wristwatch device 405. FIG. 8C shows that thin-film secondary battery 913 is built in. Thin-film secondary battery 913 is the secondary battery shown in FIG. 7A. Thin-film secondary battery 913 is provided in a position overlapping display unit 405a, and is small and lightweight. [Explanation of symbols]
[0095] 45: substrate holder, 47: exhaust mechanism, 48: exhaust mechanism, 49: exhaust mechanism, 50: substrate, 51: stage, 52: substrate transport mechanism, 53: substrate transport mechanism, 54: substrate transport mechanism, 55: evaporation material, 56: evaporation source, 57: heater, 58: evaporation boat, 61: arm, 62: arm, 63: imaging means, 65: rotation mechanism, 67: film thickness measurement mechanism, 68: shutter, 69: evaporation source shutter, 70: load lock chamber, 71: transfer chamber, 72: transfer chamber, 73: transfer chamber, 74: film formation chamber, 80: gate, 81: gate, 82: gate, 83: gate, 84: gate, 85: gate, 86: gate, 87: gate, 88: gate, 91: mask alignment chamber, 92: film formation chamber, 93: heating chamber, 94: second material supply chamber, 95: first material supply chamber, 96: third material supply chamber, 201: positive electrode current collector, 202: solid electrolyte layer, 203: negative electrode current collector, 204: positive electrode active material layer, 205: negative electrode active material layer, 206: protective layer, 212: solid electrolyte layer, 213: negative electrode current collector, 400: eyeglass-type device, 400a: frame, 400b: display unit, 401: headset-type device, 401a: microphone unit, 401b: flexible pipe, 401c: earphone unit, 402: device, 402a: housing, 402b: secondary battery, 403: device chair, 403a: housing, 403b: secondary battery, 405: wristwatch type device, 405a: display unit, 405b: belt unit, 406: belt type device, 406a: belt unit, 406b: wireless power supply receiving unit, 510: positive electrode lead, 511: negative electrode lead, 913: secondary battery, 3000: card, 3001: thin film secondary battery, 3002: ID, 3003: photo, 3004: IC, 3005: radio wave
Claims
1. a mask alignment room; a first transfer chamber connected to the mask alignment chamber; a second transfer chamber connected to the first transfer chamber; a first film formation chamber connected to the second transfer chamber; a third transfer chamber connected to the first transfer chamber; a second film forming chamber connected to the third transfer chamber, the first film-forming chamber has a function of forming a positive electrode active material layer or a negative electrode active material layer by a sputtering method, The second film formation chamber contains an organic complex of lithium and SiO X (0<X≦2) to form a solid electrolyte layer, The solid-state secondary battery manufacturing apparatus, wherein a substrate is transported between the mask alignment chamber and the first film formation chamber, and between the mask alignment chamber and the second film formation chamber, without being exposed to air.
2. 2. The apparatus for manufacturing a solid secondary battery according to claim 1, further comprising a heating chamber connected to the second transfer chamber.
3. 3. The apparatus for producing a solid secondary battery according to claim 1, wherein the organic complex of lithium is 8-hydroxyquinolinato-lithium.
Citation Information
Patent Citations
Secondary battery and electric circuit board using it
JP2001076710A
Thin film laminate, thin film battery, capacitor, and manufacturing method and device of thin film laminate
JP2003282142A
Apparatus and method for forming film, and method for cleaning
JP2003313654A
Manufacturing apparatus
JP2004079528A
Vacuum processing apparatus
JP2011192922A
Cited By
All-solid-state battery production method
WO2026121204A1